Novel film laminating process of zipper
Through the new coating process, laser laser and hot pressing technology, the problem of poor combination of zipper and fabric is solved, efficient sealing effect and waterproof performance are achieved, and the overall quality and service life of the jacket are improved.
Patent Information
- Application Number
- CN202411264049.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-10
- Publication Date
- 2024-12-03
AI Technical Summary
When ordinary zippers are sewn onto the fabric of the jacket, they are layered due to improper handling of the high and low seams, and they are prone to flashing and glue opening in extreme weather, which affects the waterproof performance and service life of the clothing.
Using a new film coating process, laser processing of zippers and fabric cutting sheets is combined with an iron and a repair press to ensure the tight fit of the adhesive film and zippers and seamless connection of the fabric, and hot air reinforcement is carried out at the end of the zipper. Treatment to form a stable combination.
It achieves the perfect integration of zippers and fabrics, enhances the firmness of the connection and sealing effect, prevents the phenomenon of flashing glue, improves the waterproof performance and overall aesthetics of the clothing, and extends the service life.
Smart Images

Figure CN119055020A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of zipper production, and in particular to a new type of zipper laminating process. Background Art
[0002] Zippers are commonly used accessories for clothing, bags and other products, especially in the production process of jackets. However, ordinary zippers have some obvious design defects. Specifically, when the zipper is sewn to the jacket fabric, the overall appearance often has a layered look due to improper handling of the high and low seams, which not only affects the aesthetics of the jacket, but also reduces its grade as outdoor clothing to a certain extent.
[0003] More importantly, the processing of the joints between ordinary zippers and fabrics is often unsatisfactory. Under long-term use and the influence of the external environment, the joints between the zipper and the fabric are prone to flaking, which not only affects the overall appearance of the jacket, but also greatly shortens the service life of the clothing. Especially in extreme weather conditions, the problem of flaking may cause the waterproof performance of the jacket to be greatly reduced, allowing rainwater or other liquids to penetrate into the interior of the clothing, thus seriously affecting the comfort and safety of the wearer.
[0004] Therefore, in order to solve the problems existing in the prior art and improve the overall quality and waterproof performance of the jacket, it is necessary to improve and optimize the zippers on the jackets, and by improving the lamination process and improving the bonding method between the zipper and the fabric, the durability and waterproof performance of the jackets can be effectively improved, providing consumers with a better outdoor wearing experience. Summary of the invention
[0005] In order to solve the above technical problems, the present invention discloses a novel laminating process for a zipper, comprising the following steps: S1: First, prepare the zipper, film, tape, and cut fabric pieces, and laser the above materials to the required standard parts specifications through the laser process; S2: Use an electric iron to tightly fit the film and the zipper. Control the temperature of the electric iron equipment at 180-220℃. According to the specific specifications of the film and the zipper, control the ironing time at 5-15s to ensure a firm and uniform fitting effect. S3: Use a pressing machine to press the zipper with the film fixed on it and the fabric piece together. Set the temperature of the pressing machine to 140-180℃ and adjust the pressure to 2-4kg to achieve seamless connection between the zipper and the fabric piece. S4: Use the electric iron again to preliminarily fix the rubber strip and the head and tail of the zipper that has been pressed together with the fabric piece. Control the temperature of the electric iron at 180-220℃ and the ironing time at 8-15s to ensure uniform and stable fixing effect. S5: Use the pressing machine again to perform hot air reinforcement treatment on the rubber strip. Set the temperature of the pressing machine to 140-180℃. When pressing, press the zipper head and tail for 10-30s each to ensure the firmness and stability of the key parts.
[0006] Furthermore, in step S1, the zipper with a laser-marked length is placed on a sewing machine, and the chain teeth are positioned and sewn to form a knot, with the knot being 1.2-1.8 cm away from the zipper head and tail edges.
[0007] Furthermore, in step S2, the zipper is first placed in the mold with the front side facing upward to position the zipper, and then the adhesive film is covered on the zipper according to the position of the mold, and the two are fixed together using an electric iron.
[0008] Furthermore, in step S3, the fabric piece is first placed on the template with the reverse side facing upward, and then the cover of the template is closed, and the zipper is placed with the reverse side facing upward according to the zipper position reserved on the cover.
[0009] Furthermore, in step S4, the fabric pieces are first placed with the reverse side facing upwards, and then the adhesive strips are placed in the middle of the head and tail of the zipper, and it is ensured that the adhesive strips cover the head and tail of the zipper by 0.4-0.6 cm respectively.
[0010] Compared with the prior art, the present invention has the following beneficial effects: The present invention achieves perfect fusion of the seam between the fabric and the film by optimizing the zipper laminating process, forming a stable combination, which not only has a firm and reliable connection, but also achieves an excellent sealing effect, effectively prevents the occurrence of flashing and debonding, makes the clothes smoother and more beautiful, and gets rid of the problems of high and low seams and layering left on the fabric by traditional zippers; In addition, the zipper lamination process of the present invention also enhances the waterproof performance of clothing, making the joint between the fabric and the film tighter, effectively preventing the penetration of water or other liquids, which not only improves the waterproof effect of clothing in severe weather conditions, but also enhances the comfort and safety of the wearer. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0012] Figure 1 It is a structural schematic diagram of a zipper in the prior art; Figure 2 It is a schematic diagram of the zipper structure of the present invention; Figure 3 for Figure 2 A magnified view of the local structure at point A in the middle; Figure 4 for Figure 2 A magnified view of the local structure at B in the middle; Figure 5 for Figure 1 A magnified view of the local structure at C in the middle; Figure 6 for Figure 1 Enlarged view of the local structure at point D in the middle. DETAILED DESCRIPTION
[0013] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.
[0014] It should be noted that all directional indications (such as up, down, left, right, front, back, etc.) in the embodiments of the present invention are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.
[0015] In addition, the descriptions of "first", "second", etc. in the present invention are only for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include at least one of the features.
[0016] In the description of the embodiments, unless otherwise clearly specified and limited, the terms "disposed", "connected" and the like should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, or an electrical connection; it can be a direct connection, or it can be connected through an intermediate medium, or it can be a communication between the two components. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances. Embodiment 1:
[0017] like Figure 2 As shown, the novel laminating process of the zipper in this embodiment includes the following steps: S1: First, prepare the zipper, film, tape, and cut fabric pieces, and laser the above materials to the required standard parts specifications through the laser process; S2: Use an electric iron to fit the film and the zipper tightly. First, place the zipper in the mold with the front side facing up to position the zipper. Then, cover the film on the zipper according to the position of the mold. Then, control the temperature of the electric iron at 180°C and the ironing time at 15 seconds to initially fix the two together. S3: Use a pressing machine to press the zipper with the film fixed on it and the fabric piece together. First, place the fabric piece with the reverse side facing up on the template, then close the cover of the template, and place the zipper with the reverse side facing up according to the zipper position reserved on the cover. Then set the temperature of the pressing machine to 140°C and adjust the pressure to 4kg. Use the high temperature of the pressing machine to melt the film into liquid, and then fuse the film and fabric together by squeezing. S4: Use the electric iron again to preliminarily fix the adhesive strip to the head and tail of the zipper that has been pressed together with the fabric piece. First, place the fabric piece with the reverse side facing up, then place the adhesive strip in the middle of the head and tail of the zipper, and make sure that the adhesive strip covers the head and tail of the zipper by 0.4 cm respectively. Then control the temperature of the electric iron to 180℃ and the ironing time to 15s to ensure uniform and stable fixing effect. S5: Use the pressing machine again to perform hot air reinforcement treatment on the rubber strip. Set the temperature of the pressing machine to 140℃. During the pressing process, press the zipper head and tail for 30s each to ensure the firmness and stability of the key parts. Embodiment 2:
[0018] like Figure 2 As shown, the novel laminating process of the zipper in this embodiment includes the following steps: S1: First, prepare the zipper, film, tape, and cut fabric pieces, and laser the above materials to the required standard parts specifications through the laser process; S2: Place the laser-cut zipper on the sewing machine, locate the chain teeth, sew and knot. The knot should be 1.2-1.8cm away from the zipper head and tail edges. S3: Use an electric iron to closely fit the film and the zipper. First, place the zipper in the mold with the front side facing up to position the zipper. Then, cover the film on the zipper according to the position of the mold. Then, control the temperature of the electric iron at 220°C and the ironing time at 5s to preliminarily fix the two together. S4: Use a pressing machine to press the zipper with the film fixed on it and the fabric piece together. First, place the fabric piece with the reverse side facing up on the template, then close the cover of the template, and place the zipper with the reverse side facing up according to the zipper position reserved on the cover. Then set the temperature of the pressing machine to 180°C and adjust the pressure to 2kg. Use the high temperature of the pressing machine to melt the film into liquid, and then fuse the film and the fabric together by squeezing. S5: Use the electric iron again to preliminarily fix the adhesive strip to the head and tail of the zipper that has been pressed together with the fabric piece. First, place the fabric piece with the reverse side facing up, then place the adhesive strip in the middle of the head and tail of the zipper, and make sure that the adhesive strip covers the head and tail of the zipper by 0.6 cm respectively. Then control the temperature of the electric iron at 220℃ and the ironing time at 8s to ensure uniform and stable fixing effect. S6: Use the pressing machine to perform hot air reinforcement treatment on the rubber strip again, set the temperature of the pressing machine to 180℃, and press the zipper head and tail for 10s each to ensure the firmness and stability of the key parts.
[0019] Compared with the prior art, the present invention has the following beneficial effects: 1. The adhesive on the surface of the zipper of the present invention makes the zipper and the fabric piece completely flush after treatment, and there is no gap or layering between the zipper and the fabric piece (such as Figure 4 As shown); However, there is a height difference between the existing zipper and the fabric piece (such as Figure 6 As shown in the figure), glue overflow, debonding, and flash are likely to occur at the joints, thus shortening the service life.
[0020] Second, the zipper head and tail of the present invention are added with a knotting process (such as Figure 3 As shown in the figure), it prevents the zipper from being over-pulled during opening and closing, reduces the problem of zipper damage and fabric wear during the pulling and closing process; at the same time, glue will also be attached to the knot to ensure the overall waterproof performance of the zipper; the existing zippers do not have this process (such as Figure 5 ), which can easily cause the zipper to be over-zipped and the fabric to be worn.
[0021] Third, the zipper of the present invention can achieve a waterproof effect without a layer of waterproof decorative film, while the existing zipper needs to add a layer of waterproof decorative film on the outer side of the fabric piece to achieve a waterproof effect.
[0022] In summary, the present invention achieves the perfect fusion of the seam between the fabric and the film by optimizing the zipper laminating process, forming a stable combination. Not only is the connection firm and reliable, but also an excellent sealing effect is achieved, effectively preventing the occurrence of burrs and debonding, making the clothes smoother and more beautiful, and getting rid of the problems of high and low seams and layering left on the fabric by traditional zippers.
[0023] In addition, the zipper lamination process of the present invention also enhances the waterproof performance of clothing, making the joint between the fabric and the film tighter, effectively preventing the penetration of water or other liquids, which not only improves the waterproof effect of clothing in severe weather conditions, but also enhances the comfort and safety of the wearer.
[0024] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention. In addition, the technical solutions between the various embodiments can be combined with each other, but it must be based on the ability of ordinary technicians in the field to implement; when the combination of technical solutions is contradictory or cannot be implemented, it should be considered that such a combination of technical solutions does not exist and is not within the protection scope required by the present invention.
Claims
1. A new laminating process for zippers, characterized in that: The following steps are involved: S1: First, prepare the zipper, film, tape, and cut fabric pieces, and laser the above materials to the required standard parts specifications through the laser process; S2: Use an electric iron to tightly fit the film and the zipper. Control the temperature of the electric iron equipment at 180-220℃. According to the specific specifications of the film and the zipper, control the ironing time at 5-15s to ensure a firm and uniform fitting effect. S3: Use a pressing machine to press the zipper with the film fixed on it and the fabric piece together. Set the temperature of the pressing machine to 140-180℃ and adjust the pressure to 2-4kg to achieve seamless connection between the zipper and the fabric piece. S4: Use the electric iron again to preliminarily fix the rubber strip and the head and tail of the zipper that has been pressed together with the fabric piece. Control the temperature of the electric iron at 180-220℃ and the ironing time at 8-15s to ensure uniform and stable fixing effect. S5: Use the pressing machine again to perform hot air reinforcement treatment on the rubber strip. Set the temperature of the pressing machine to 140-180℃. When pressing, press the zipper head and tail for 10-30s each to ensure the firmness and stability of the key parts.
2. The novel zipper laminating process according to claim 1, characterized in that: In step S1, the zipper with a laser-marked length is placed on a sewing machine, and the chain teeth are positioned and sewn to form a knot, with the knot being 1.2-1.8 cm away from the zipper head and tail edges.
3. The novel zipper laminating process according to claim 1 is characterized in that: In step S2, the zipper is first placed in the mold with the front side facing upward to position the zipper, and then the adhesive film is covered on the zipper according to the position of the mold, and the two are fixed together using an electric iron.
4. The novel zipper laminating process according to claim 1 is characterized in that: In step S3, firstly, the fabric piece is placed on the template with the reverse side facing upward, and then the cover of the template is closed, and the zipper is placed with the reverse side facing upward according to the zipper position reserved on the cover.
5. The novel zipper laminating process according to claim 1 is characterized in that: In step S4, the fabric pieces are first placed with the reverse side facing upwards, and then the adhesive strips are placed in the middle of the zipper head and tail, and it is ensured that the adhesive strips cover the zipper head and tail by 0.4-0.6 cm respectively.