Preparation method of LED chip release paper
Through ultrasonic cleaning and surface treatment, nanostructure design, automated coating and process simulation optimization, combined with online monitoring and intelligent temperature control, the unstable surface treatment of release paper, uneven coating thickness and temperature control in the existing technology, is solved. The problem of precision has achieved the uniformity and performance improvement of LED chip release paper.
Patent Information
- Application Number
- CN202411390813.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-08
- Publication Date
- 2024-12-03
AI Technical Summary
In the existing LED chip release paper preparation methods, the surface treatment effect is unstable, the coating thickness is not easy to control, and the drying and curing temperature control is not accurate, resulting in poor uniformity of release performance and poor final performance.
Ultrasonic cleaning and surface treatment are used to improve the surface energy of the substrate, design nanostructured coatings and ensure uniform thickness through automated coating systems, optimize process parameters using computer simulation and big data, and install online monitoring and intelligent temperature control systems to control the production process in real time.
The surface energy and coating uniformity of the substrate are significantly improved, the uniformity and final performance of the release paper are ensured, and the stability and consistency of the product are improved by precise control of process parameters and temperature.
Smart Images

Figure CN119056722A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of LED chips, and in particular to a method for preparing release paper for LED chips. Background Art
[0002] LED chip release paper is a specialized material used to protect LED chips from damage during manufacturing and transportation. It's typically made from a polymer material and offers excellent release properties and durability. Its primary function is to form a barrier between the LED chip and the packaging material, preventing adhesion and ensuring smooth release of the LED chip during the packaging process.
[0003] The existing method for preparing release paper for LED chips primarily involves the following steps: substrate selection, surface treatment, coating, drying, and curing. First, a suitable substrate, such as polyester film or polyimide film, is selected. The surface energy of the substrate is then increased through corona or plasma treatment. Next, a coating machine is used to evenly apply the release coating to the substrate. After drying and curing, the final product is the LED chip release paper.
[0004] While existing methods for preparing release paper for LED chips have achieved some success, they still suffer from some significant drawbacks. First, the surface treatment effect is unstable, resulting in poor uniformity in release performance. Second, the coating thickness is difficult to control during the coating process, which can easily lead to uneven thickness. Furthermore, imprecise temperature control during the drying and curing processes affects the release paper's ultimate performance. Summary of the Invention
[0005] The object of the present invention is to provide a method for preparing release paper for LED chips to solve the problems raised in the above background technology.
[0006] To achieve the above object, the present invention provides the following technical solutions:
[0007] A method for preparing LED chip release paper comprises the following steps:
[0008] Step S1: Place the substrate in an ultrasonic cleaning machine and clean it with pure water or an organic solvent for 10-15 minutes.
[0009] Step S2: corona treatment or plasma treatment is performed, and the treatment time is controlled within 5-10 minutes to ensure that the surface energy of the substrate is significantly improved;
[0010] Step S3, using computer simulation technology to design the nanostructured coating and optimize the distribution and arrangement of the nanoparticles;
[0011] Step S4: Using an automated coating system, the nanostructured coating is applied layer by layer, and online thickness monitoring is performed after each layer is applied to ensure uniform coating thickness.
[0012] The present invention further comprises the following steps:
[0013] Step S5, using computer simulation technology to simulate the coating, drying and curing processes and optimize process parameters;
[0014] Step S6: Collect data from the production process, analyze it using big data and artificial intelligence technology, and optimize production parameters;
[0015] Step S7, installing sensors and monitoring equipment to monitor key parameters of the production process in real time, including but not limited to coating thickness, drying temperature and curing time;
[0016] Step S8: Using an intelligent temperature control system to control the temperature during the drying and curing process to ensure that the coating is completely cured.
[0017] In the present invention, in step S1, the organic solvent used is ethanol or acetone;
[0018] Cleaning time calculation formula:
[0019] t=k·PV
[0020] Wherein, t represents the cleaning time, k represents the cleaning efficiency coefficient, V represents the volume of the cleaning liquid, and P represents the ultrasonic power.
[0021] In the present invention, in step S2, the corona treatment time is 5 minutes and the plasma treatment time is 10 minutes;
[0022] Surface energy increment calculation formula:
[0023] Δγ=γ0·et / T
[0024] Where Δγ represents the surface energy increment, γ0 represents the initial surface energy, t represents the processing time, and T represents the time constant.
[0025] In the present invention, in step S3, the distribution and arrangement of the nanoparticles are optimized using finite element analysis technology;
[0026] Nanoparticle distribution optimization formula:
[0027] D=N1i=1∑N(xi-μ)2
[0028] Where D represents the standard deviation of the distribution, N represents the total number of nanoparticles, xi represents the position of the i-th nanoparticle, and μ represents the average position of the nanoparticles.
[0029] In the present invention, in step S4, online thickness monitoring is performed after each layer is coated to ensure that the coating thickness is uniform and the coating thickness is controlled within 10-20 microns;
[0030] Coating thickness uniformity calculation formula:
[0031] σ=N-11i=1∑N(hi-hˉ)2
[0032] Where σ represents the standard deviation of coating thickness, N represents the number of coating thickness measurement points, hi represents the coating thickness at the i-th measurement point, and hˉ represents the average coating thickness.
[0033] In the present invention, in step S5, finite element analysis technology is used to simulate the coating, drying and curing processes, optimize process parameters, and reduce trial and error costs;
[0034] Simulation error calculation formula:
[0035] E=N1i=1∑N(y iy^i)2
[0036] Where E represents the simulation error, N represents the number of simulation data points, yi represents the actual measured value, and y^i represents the simulation predicted value.
[0037] In the present invention, in step S6, data from the production process is collected and analyzed using big data and artificial intelligence technology to optimize production parameters and improve production efficiency and product quality;
[0038] Optimization parameter calculation
[0039] θ*=argθmini=1∑NL(yi,f(xi;θ))
[0040] Among them, θ* represents the optimized parameters, N represents the number of data points, L represents the loss function, yi represents the actual output, f(xi;θ) represents the model predicted output, and xi represents the input data.
[0041] In the present invention, in step S8, an intelligent temperature control system is used to control the temperature during the drying and curing process to ensure that the coating is completely cured, and the temperature is controlled at 150-200 degrees Celsius.
[0042] Compared with the prior art, the present invention has the following beneficial effects:
[0043] The present invention proposes a new method for preparing release paper for LED chips, which solves the shortcomings of the existing technology through multi-step process optimization. First, through ultrasonic cleaning and surface treatment, the surface energy of the substrate is significantly improved, ensuring the uniformity of the release performance. Secondly, nanostructure design and multi-layer coating technology are adopted to optimize the distribution and thickness of the coating, ensuring the uniformity of the coating. In addition, through process simulation and data-driven optimization, the temperature during the drying and curing processes is precisely controlled, improving the final performance of the release paper. Finally, through an online monitoring system and an intelligent temperature control system, key parameters in the production process are monitored in real time, ensuring the stability and consistency of the process parameters. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] Figure 1 The present invention is a flow chart of a method for preparing a release paper for an LED chip. DETAILED DESCRIPTION
[0045] The following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of the present invention.
[0046] See also Figure 1 , the present invention provides a technical solution:
[0047] A method for preparing LED chip release paper comprises the following steps:
[0048] Step S1: Place the substrate in an ultrasonic cleaning machine and clean it with pure water or an organic solvent for 10-15 minutes.
[0049] In this embodiment, the organic solvent used is ethanol or acetone;
[0050] Cleaning time calculation formula:
[0051] t=k·PV
[0052] Wherein, t represents the cleaning time, k represents the cleaning efficiency coefficient, V represents the volume of the cleaning liquid, and P represents the ultrasonic power.
[0053] During this step, the substrate must first be ultrasonically cleaned during the preparation of LED chip release paper. This cleaning procedure removes impurities and contaminants from the substrate surface, ensuring surface cleanliness. The cleaning time directly impacts the cleaning effect, so the optimal cleaning time is calculated using a cleaning time calculation formula.
[0054] Specifically, the calculation steps are as follows:
[0055] Step S101, inputting the cleaning liquid volume V and ultrasonic power P;
[0056] Step S102, setting the cleaning efficiency coefficient k;
[0057] Step S103, calculating the cleaning time t=k·PV;
[0058] Step S104: output the cleaning time t.
[0059] Through the above calculations, the optimal cleaning time can be obtained. Next, the substrate needs to be surface treated to increase its surface energy.
[0060] Step S2: corona treatment or plasma treatment is performed, and the treatment time is controlled within 5-10 minutes to ensure that the surface energy of the substrate is significantly improved;
[0061] In this embodiment, the corona treatment time is 5 minutes and the plasma treatment time is 10 minutes;
[0062] Surface energy increment calculation formula:
[0063] Δγ=γ0·et / T
[0064] Where Δγ represents the surface energy increment, γ0 represents the initial surface energy, t represents the processing time, and T represents the time constant.
[0065] The purpose of this surface treatment step is to significantly increase the substrate's surface energy through corona or plasma treatment, thereby enhancing the adhesion of subsequent coatings to the substrate. The treatment time directly affects the increase in surface energy, so the optimal treatment time is calculated using a surface energy increase formula.
[0066] Specifically, the calculation steps are as follows:
[0067] Step S201, inputting initial surface energy γ0, processing time t and time constant T;
[0068] Step S202, calculating the surface energy increment Δγ=γ0·et / T;
[0069] Step S203: outputting the surface energy increment Δγ.
[0070] Through the above calculations, the optimal surface treatment time can be obtained. Next, nanostructure design is required to optimize the distribution and arrangement of nanoparticles.
[0071] Step S3, using computer simulation technology to design the nanostructured coating and optimize the distribution and arrangement of the nanoparticles;
[0072] In this embodiment, the distribution and arrangement of nanoparticles were optimized using finite element analysis technology;
[0073] Nanoparticle distribution optimization formula:
[0074] D=N1i=1∑N(xi-μ)2
[0075] Where D represents the standard deviation of the distribution, N represents the total number of nanoparticles, xi represents the position of the i-th nanoparticle, and μ represents the average position of the nanoparticles.
[0076] Nanostructure design is a key step in the preparation of LED chip release paper. Computer simulation technology is used to design the nanostructured coating and optimize the distribution and arrangement of nanoparticles, thereby improving the coating's performance. Calculating the distribution standard deviation can assess the uniformity of the nanoparticle distribution.
[0077] Specifically, the calculation steps are as follows:
[0078] Step S301, inputting the total number of nanoparticles N and the nanoparticle positions xi;
[0079] Step S302, calculating the average value μ of the nanoparticle positions;
[0080] Step S303, calculate the distribution standard deviation D = N1∑i = 1N(xi-μ)2;
[0081] Step S304: output the distribution standard deviation D.
[0082] Through the above calculations, the standard deviation of the nanoparticle distribution can be obtained. Next, multi-layer coating technology is required to ensure uniform coating thickness.
[0083] Step S4, using an automated coating system to apply the nanostructured coating layer by layer, and performing online thickness monitoring after each coating to ensure uniform coating thickness;
[0084] In this embodiment, online thickness monitoring is performed after each coating to ensure uniform coating thickness, and the coating thickness is controlled within 10-20 microns;
[0085] Coating thickness uniformity calculation formula:
[0086] σ=N-11i=1∑N(hi-hˉ)2
[0087] Where σ represents the standard deviation of coating thickness, N represents the number of coating thickness measurement points, hi represents the coating thickness at the i-th measurement point, and hˉ represents the average coating thickness.
[0088] In this step, multi-layer coating technology is a key step in the preparation of LED chip release paper. The nanostructured coating is applied layer by layer through an automated coating system, and online thickness monitoring is performed to ensure uniform coating thickness. Calculating the standard deviation of the coating thickness can be used to evaluate the uniformity of the coating.
[0089] Specifically, the calculation steps are as follows:
[0090] Step S401, input the number of coating thickness measurement points N and the coating thickness hi;
[0091] Step S402, calculating the average value hˉ of the coating thickness;
[0092] Step S403, calculating the coating thickness standard deviation σ=N-11∑i=1N(hi-hˉ)2;
[0093] Step S404: outputting the coating thickness standard deviation σ.
[0094] Through the above calculation, the standard deviation of the coating thickness can be obtained. Next, process simulation is required to optimize the process parameters.
[0095] The following steps are also included:
[0096] Step S5, using computer simulation technology to simulate the coating, drying and curing processes and optimize process parameters;
[0097] In this embodiment, finite element analysis technology is used to simulate the coating, drying and curing processes to optimize process parameters and reduce trial and error costs;
[0098] Simulation error calculation formula:
[0099] E=N1i=1∑N(y iy^i)2
[0100] Where E represents the simulation error, N represents the number of simulation data points, yi represents the actual measured value, and y^i represents the simulation predicted value.
[0101] During this step, process simulation is a crucial step in the preparation of LED chip release paper. Computer simulation technology is used to simulate the coating, drying, and curing processes, optimizing process parameters and reducing trial-and-error costs. Calculating simulation errors can be used to assess the accuracy of simulation results.
[0102] Specifically, the calculation steps are as follows:
[0103] Step S501, input the number of simulation data points N, the actual measurement value yi and the simulation prediction value yi;
[0104] Step S502, calculating the simulation error E = N1∑i = 1N(y iy^i)2;
[0105] Step S503: output simulation error E.
[0106] Through the above calculations, the simulation error can be obtained. Next, data-driven optimization is needed to improve production efficiency and product quality.
[0107] Step S6: Collect data from the production process, analyze it using big data and artificial intelligence technology, and optimize production parameters;
[0108] In this embodiment, data from the production process is collected and analyzed using big data and artificial intelligence technologies to optimize production parameters and improve production efficiency and product quality;
[0109] Optimization parameter calculation
[0110] θ*=argθmini=1∑NL(yi,f(xi;θ))
[0111] Among them, θ* represents the optimized parameters, N represents the number of data points, L represents the loss function, yi represents the actual output, f(xi;θ) represents the model predicted output, and xi represents the input data.
[0112] In this step, data-driven optimization is a key step in the preparation of LED chip release paper. By collecting data from the production process and using big data and artificial intelligence technology for analysis, production parameters can be optimized to improve production efficiency and product quality. The calculation of optimization parameters can find the best production parameters.
[0113] Specifically, the calculation steps are as follows:
[0114] Step S601: input the number of data points N, the actual output yi, the model prediction output f(xi;θ) and the loss function L;
[0115] Step S602 , calculating the optimization parameter θ*=argminθ∑i=1N L(yi,f(xi;θ));
[0116] Step S603: output the optimized parameter θ*.
[0117] Through the above calculations, the optimized parameters can be obtained. Next, an online monitoring system is needed to monitor the key parameters of the production process in real time.
[0118] Step S7, installing sensors and monitoring equipment to monitor key parameters of the production process in real time, including but not limited to coating thickness, drying temperature and curing time;
[0119] During this step, the online monitoring system plays a crucial role in the preparation of LED chip release paper. By installing sensors and monitoring equipment, key parameters in the production process, such as coating thickness, drying temperature, and curing time, are monitored in real time to ensure process stability. Calculating real-time monitoring errors can assess the accuracy of monitoring results.
[0120] Specifically, the calculation steps are as follows:
[0121] Step S701, input monitoring data points N and monitoring data mi;
[0122] Step S702, calculating the average value mˉ of the monitoring data;
[0123] Step S703, calculating the real-time monitoring error ∈=N1∑i=1N|m i-mˉ|;
[0124] Step S704: output the real-time monitoring error ∈.
[0125] Through the above calculations, the real-time monitoring error can be obtained. Next, an intelligent temperature control system is needed to ensure that the coating is completely cured.
[0126] Step S8, using an intelligent temperature control system to control the temperature during the drying and curing process to ensure that the coating is completely cured;
[0127] In this embodiment, an intelligent temperature control system is used to control the temperature during the drying and curing process to ensure that the coating is completely cured, and the temperature is controlled at 150-200 degrees Celsius.
[0128] During this step, the intelligent temperature control system is a key step in the preparation of LED chip release paper. It controls the temperature during the drying and curing process to ensure that the coating is fully cured. Calculating the temperature control error can assess the accuracy of temperature control.
[0129] Specifically, the calculation steps are as follows:
[0130] Step S801, input the number of temperature measurement points N, actual temperature Ti and target temperature Td;
[0131] Step S802 , calculating the temperature control error δ=N1∑i=1N|T iT d|;
[0132] Step S803: outputting the temperature control error δ.
[0133] Through the above calculation, the temperature control error can be obtained to ensure that the coating is completely cured. At this point, the preparation process of the LED chip release paper has been completed.
[0134] It should be noted that, in this document, relational terms such as first and second, etc., are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any actual relationship or order between these entities or operations. Moreover, the terms "comprises," "comprising," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that includes a list of elements includes not only those elements but also other elements not explicitly listed, or elements inherent to such process, method, article, or apparatus.
[0135] While embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions, and variations may be made to these embodiments without departing from the principles and spirit of the invention, and that the scope of the invention is defined by the appended claims and their equivalents.
Claims
1. A method for preparing a release paper for an LED chip, characterized in that: The following steps are involved: Step S1, placing the substrate in an ultrasonic cleaning machine and cleaning it with pure water or an organic solvent, and the cleaning time is controlled within 10-15 minutes; Step S2, using corona treatment or plasma treatment, the treatment time is controlled within 5-10 minutes to ensure that the surface energy of the substrate is significantly improved; Step S3, using computer simulation technology to design the nanostructured coating and optimize the distribution and arrangement of the nanoparticles; Step S4, using an automated coating system to apply the nanostructured coating layer by layer, and performing online thickness monitoring after each coating to ensure uniform coating thickness.
2. The method for preparing a release paper for an LED chip according to claim 1, characterized in that: The following steps are also included: Step S5, using computer simulation technology to simulate the coating, drying and curing processes and optimize process parameters; Step S6, collecting data from the production process, analyzing it using big data and artificial intelligence technology, and optimizing production parameters; Step S7, installing sensors and monitoring equipment to monitor key parameters in the production process in real time, including but not limited to coating thickness, drying temperature and curing time; Step S8, using an intelligent temperature control system to control the temperature during the drying and curing process to ensure that the coating is completely cured.
3. The method for preparing a release paper for an LED chip according to claim 1, characterized in that: In step S1, the organic solvent used is ethanol or acetone; Cleaning time calculation formula: t=k·PV Wherein, t represents the cleaning time, k represents the cleaning efficiency coefficient, V represents the volume of the cleaning liquid, and P represents the ultrasonic power.
4. The method for preparing a release paper for an LED chip according to claim 1, characterized in that: In step S2, the corona treatment time is 5 minutes and the plasma treatment time is 10 minutes; Surface energy increment calculation formula: Δγ=γ0·et / T Where Δγ represents the surface energy increment, γ0 represents the initial surface energy, t represents the processing time, and T represents the time constant.
5. The method for preparing a release paper for an LED chip according to claim 1, characterized in that: In step S3, the distribution and arrangement of the nanoparticles are optimized using finite element analysis technology; Nanoparticle distribution optimization formula: D=N1i=1∑N(xi-μ)2 Where D represents the standard deviation of the distribution, N represents the total number of nanoparticles, xi represents the position of the i-th nanoparticle, and μ represents the average position of the nanoparticles.
6. The method for preparing a release paper for an LED chip according to claim 1, characterized in that: In step S4, online thickness monitoring is performed after each layer is coated to ensure that the coating thickness is uniform and the coating thickness is controlled within 10-20 microns; Coating thickness uniformity calculation formula: σ=N-11i=1∑N(hi-hˉ)2 Wherein, σ represents the standard deviation of coating thickness, N represents the number of coating thickness measurement points, hi represents the coating thickness at the i-th measurement point, and hˉ represents the average coating thickness.
7. The method for preparing a release paper for an LED chip according to claim 2, characterized in that: In step S5, finite element analysis technology is used to simulate the coating, drying and curing processes, optimize process parameters, and reduce trial and error costs; Simulation error calculation formula: E=N1i=1∑N(yi-y^i)2 Where E represents the simulation error, N represents the number of simulation data points, yi represents the actual measured value, and y^i represents the simulation predicted value.
8. The method for preparing a release paper for an LED chip according to claim 1, characterized in that: In step S6, data from the production process is collected and analyzed using big data and artificial intelligence technology to optimize production parameters and improve production efficiency and product quality; Optimization parameter calculation θ*=argθmini=1∑NL(yi,f(xi;θ)) Among them, θ* represents the optimized parameters, N represents the number of data points, L represents the loss function, yi represents the actual output, f(xi;θ) represents the model predicted output, and xi represents the input data.
9. The method for preparing a release paper for an LED chip according to claim 1, characterized in that: In step S8, an intelligent temperature control system is used to control the temperature during the drying and curing process to ensure that the coating is completely cured and the temperature is controlled at 150-200 degrees Celsius.