Production method of stitch-bonded non-woven fabric

Through the seam knitting machine, and combined with hot melt film fusion technology, the problem of narrow application range of seam knitting non-woven fabrics is solved, the weight and thickness are expanded, the strength is improved, and the application field is expanded.

CN119058218APending Publication Date: 2024-12-03ZHEJIANG INST OF STANDARDIZATION (ZIS) +1
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410997200.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The existing stitching non-woven fabric has a narrow application range, a narrow range of weight, a thin thickness, and insufficient strength and elongation performance, which limits its application in multiple fields.

Method used

The combed fibers are sewn into fabrics with a preset sewing length through a sewing machine, and dried to adjust the softness and hardness. A hot melt film is set between the upper and lower fabrics. The hot melt film and the fabric are fused by an oven to expand the weight Range, increase product thickness and increase strength.

Benefits of technology

The weight range of stitched non-woven fabrics has been expanded, the product thickness has been increased, and the strength has been improved, which has achieved the expansion of the application field of stitched non-woven fabrics has been solved, and the problem of narrow application range has been solved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119058218A_ABST
    Figure CN119058218A_ABST
Patent Text Reader

Abstract

The invention relates to a stitch-bonded non-woven fabric production method, which comprises the following steps of: sewing carded fibers into cloth with a preset sewing length through a stitch-bonded machine; drying the stitched and knitted cloth, wherein the drying is used for adjusting the hardness of the cloth; the wound upper cloth is placed on an upper unwinding device, the wound lower cloth is placed on a lower unwinding device, and a hot melting film is arranged between the upper cloth and the lower cloth; and fusing the hot melt film with the upper cloth and the lower cloth through a drying oven to obtain the stitch-bonded non-woven fabric. The gram weight range is greatly expanded, the product thickness is increased, and the strength is improved. And the application field of the stitch-bonded non-woven fabric is expanded. The problem that an existing stitch-bonded non-woven fabric is narrow in application range in the prior art is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of nonwoven fabric production, and in particular to a method for producing stitch-bonded nonwoven fabric. Background Art

[0002] In recent years, the stitched non-woven fabric industry has developed rapidly. Through the introduction of foreign advanced equipment and technology, domestic stitched non-woven fabric technology has developed rapidly, various new processes have emerged one after another, and the successful combination of various equipment technologies and process technologies has opened up the bottlenecks that restrict production capacity, variety, and energy consumption. The application areas of products have been greatly broadened, which has promoted the upgrading of the overall industry.

[0003] At present, although the application of stitch-bonded nonwoven fabrics is becoming more and more extensive, due to the limitations of stitch-bonded nonwoven fabrics, the existing stitch-bonded nonwoven fabrics have a problem of narrow application range. Summary of the invention

[0004] The embodiment of the present application provides a method for producing a stitch-bonded nonwoven fabric, so as to at least solve the problem that the existing stitch-bonded nonwoven fabric in the related art has a narrow application range.

[0005] The present application provides a method for producing a stitch-bonded nonwoven fabric, the method comprising:

[0006] The carded fibers are stitched into fabrics of a preset stitching length by a stitch-bonding machine;

[0007] Drying the stitched fabric, wherein the drying is used to adjust the softness and hardness of the fabric;

[0008] Placing the wound upper fabric on an upper unwinder, and placing the wound lower fabric on a lower unwinder, wherein a hot melt film is provided between the upper fabric and the lower fabric;

[0009] The hot melt film is fused with the upper fabric and the lower fabric through an oven to obtain a stitch-bonded nonwoven fabric.

[0010] In one embodiment, the hot melt film is fused with the upper fabric and the lower fabric through an oven to obtain a stitch-bonded nonwoven fabric, comprising:

[0011] According to the melting point of the hot melt film and the heat resistance of the fabric, the internal temperature of the oven is preset, wherein the preset internal temperature of the oven is 50°C-250°C;

[0012] The upper fabric is 100gsm-300gsm with a thickness of 1mm-4mm, and the lower fabric is 100gsm-300gsm with a thickness of 1mm-4mm;

[0013] The nonwoven fabric is dried in an oven to obtain a 2mm-8mm stitched nonwoven fabric, wherein the drying time is 6min-15min.

[0014] In one embodiment, after fusing the hot melt film with the upper fabric and the lower fabric through an oven to obtain a stitch-bonded nonwoven fabric, the method includes:

[0015] The stitched nonwoven fabric is subjected to product index testing, and relevant adjustments are made to the stitched nonwoven fabric that does not meet the product index to obtain the stitched nonwoven fabric that meets the product index, wherein the product index testing includes gram weight index, softness and hardness index, metal residue rate, strength index and thickness index testing.

[0016] In one embodiment, the stitch-bonded nonwoven fabric that does not meet the product specifications is adjusted to obtain the stitch-bonded nonwoven fabric that meets the product specifications, including:

[0017] When the weight and thickness of the stitch-bonded nonwoven fabric do not meet the product specifications, adjusting the oven spacing and the oven temperature;

[0018] When the hardness and strength index of the fabric do not meet the quality standards, adjusting the oven temperature of the upper area and the lower area of ​​the fabric;

[0019] In the case that the metal residue rate of the cloth does not meet the quality standard, the metal in the cloth is filtered and metal residue detection is performed on each device.

[0020] In one embodiment, the stitched fabric is dried, and the drying is used to adjust the softness and hardness of the fabric, including:

[0021] Electric heating is used in a closed space to control the oven temperatures of the upper area and the lower area of ​​the fabric respectively, wherein the oven temperatures of the upper area and the lower area of ​​the fabric are controlled according to the characteristics of the fabric, the oven temperature of the upper area of ​​the fabric includes 50°C-250°C, and the oven temperature of the lower area of ​​the fabric includes 50°C-250°C.

[0022] In one embodiment, the hot melt film is 40gsm-60gsm.

[0023] In one embodiment, it is characterized in that before stitching the combed fibers into a cloth of a preset stitching length by a stitching machine, the method further comprises:

[0024] Different types of fibers are fed into different bale opening machines according to the production formula, and the proportion of input materials is controlled;

[0025] The different types of fibers that pass through the bale opener are subjected to metal detection, and the raw materials after detection are initially mixed and loosened through the mixing bin;

[0026] Further mixing and finely opening the fibers after mixing in the large bin;

[0027] The mixed and opened fibers are sucked into a cotton storage box through a fan for storage and standby;

[0028] The fibers in the cotton storage box are sent to the air pressure cotton box by a powerful fan, and the fibers are accurately weighed by a belt scale.

[0029] In one embodiment, after the fibers in the cotton storage box are sent to the air pressure cotton box by a powerful fan and the fibers are accurately weighed by a belt scale, the method further comprises:

[0030] The weighed different fibers are combed into a cross-arranged, evenly mixed single-layer fiber web through a carding machine.

[0031] In one embodiment, before placing the wound upper fabric on the upper unwinder, the method comprises:

[0032] The fabric is wound up by a winder to obtain a fabric roll.

[0033] In one embodiment, the stitch-bonded nonwoven fabric is subjected to product index detection, and the stitch-bonded nonwoven fabric that does not meet the product index is adjusted accordingly, and after the stitch-bonded nonwoven fabric that meets the product index is obtained, the method further includes:

[0034] The slitting machine is used to cut the stitched nonwoven fabric into preset width and remove the excess waste edges.

[0035] A method for producing a stitch-bonded nonwoven fabric provided in an embodiment of the present application has at least the following technical effects.

[0036] The combed fibers are sewn into fabrics of preset sewing lengths through a sewing machine; the sewing fabrics are dried to adjust the softness and hardness of the fabrics; the wound upper fabric is placed on an upper unwinder, and the wound lower fabric is placed on a lower unwinder, with a hot melt film between the upper and lower fabrics; the hot melt film is fused with the upper and lower fabrics through an oven to obtain a sewing non-woven fabric. The weight range is expanded, the product thickness is increased, the strength is improved, the application field of sewing non-woven fabrics is expanded, and the problem of narrow application range of existing sewing non-woven fabrics in related technologies is solved.

[0037] Details of one or more embodiments of the present application are set forth in the following drawings and description to make other features, objects, and advantages of the present application more readily apparent. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:

[0039] Figure 1 It is a flow chart of stitch-bonded nonwoven production;

[0040] Figure 2 is a flowchart of steps S107-S108 and steps S113-S114 according to an exemplary embodiment;

[0041] Figure 3 is a flowchart of steps S101 to S105 according to an exemplary embodiment. DETAILED DESCRIPTION

[0042] In order to make the purpose, technical solutions and advantages of the present application clearer, the present application is described and illustrated below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not intended to limit the present application. Based on the embodiments provided in the present application, all other embodiments obtained by ordinary technicians in the field without making creative work are within the scope of protection of the present application.

[0043] Obviously, the drawings described below are only some examples or embodiments of the present application. For ordinary technicians in this field, the present application can also be applied to other similar scenarios based on these drawings without creative work. In addition, it can also be understood that although the efforts made in this development process may be complicated and lengthy, for ordinary technicians in this field related to the content disclosed in this application, some changes in design, manufacturing or production based on the technical content disclosed in this application are just conventional technical means, and should not be understood as insufficient content disclosed in this application.

[0044] Reference to "embodiments" in this application means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those of ordinary skill in the art that the embodiments described in this application may be combined with other embodiments without conflict.

[0045] Unless otherwise defined, the technical terms or scientific terms involved in this application should be understood by people with ordinary skills in the technical field to which this application belongs. The words "one", "a", "a", "the" and the like involved in this application do not indicate a quantitative limitation, and may represent the singular or plural. The terms "include", "comprise", "have" and any of their variations involved in this application are intended to cover non-exclusive inclusions; for example, a process, method, system, product or device that includes a series of steps or modules (units) is not limited to the listed steps or units, but may also include steps or units that are not listed, or may also include other steps or units inherent to these processes, methods, products or devices. The words "connect", "connected", "coupled" and the like involved in this application are not limited to physical or mechanical connections, but may include electrical connections, whether direct or indirect. The "multiple" involved in this application refers to two or more. "And / or" describes the association relationship of associated objects, indicating that there may be three relationships, for example, "A and / or B" can represent: A exists alone, A and B exist at the same time, and B exists alone. The character " / " generally indicates that the objects before and after are in an "or" relationship. The terms "first", "second", "third", etc. involved in this application are only used to distinguish similar objects and do not represent a specific ordering of the objects.

[0046] In recent years, the stitched non-woven fabric industry has developed rapidly. Through the introduction of foreign advanced equipment and technology, domestic stitched non-woven fabric technology has developed rapidly, various new processes have emerged one after another, and the successful combination of various equipment technologies and process technologies has opened up the bottlenecks that restrict production capacity, variety, and energy consumption. The application field of products has been greatly broadened, which has promoted the upgrading of the overall industry. The production process of stitched non-woven fabrics mainly includes the following steps: ① Raw material preparation. Chemical fibers such as polyester and polypropylene are usually used as raw materials. ② Fine opening and combing. The fiber material is combed to remove impurities and make it into a continuous fiber web. ③ Stitching. The fiber web is preliminarily reinforced through the stitching process. ④ Heat setting. The stitched non-woven fabric is heat treated to fix its structure and increase its strength. ⑤ Rolling. After inspection, the non-woven fabric is rolled and packaged.

[0047] Stitched nonwoven fabrics are widely used, mainly in the following aspects:

[0048] First, in terms of home fabrics, stitched non-woven fabrics can be used to make curtains, sofa covers, carpets, etc. Its softness and comfortable touch make the home environment more warm and comfortable. In addition, stitched non-woven fabrics are also widely used in clothing, shoes and hats, etc., providing convenience and comfort for people's lives.

[0049] Second, stitched non-woven fabrics are also widely used in the agricultural field. Due to its superior air permeability and moisture retention properties, stitched non-woven fabrics can be used as greenhouse covering materials and an excellent protective layer for the growth of fruits and vegetables. It can effectively control temperature and humidity, create good environmental conditions for the growth of crops, and thus increase yields. At the same time, stitched non-woven fabrics can also be used to make agricultural tools, plant bags, etc., to facilitate farmers' labor.

[0050] Third, stitched non-woven fabrics play an irreplaceable role in the medical and health field. In medical supplies, stitched non-woven fabrics can be used to make disposable masks, medical surgical gowns and other protective supplies. Its material is waterproof and antibacterial, which can provide good protection and protect the lives of medical staff and patients. In addition, stitched non-woven fabrics can also be used to make wound dressings, sanitary napkins, etc., with good moisture absorption and breathability, which can effectively prevent bacterial infection and maintain hygiene and comfort.

[0051] Fourth, stitched nonwoven fabrics have applications in other fields. They can be used to make filter materials and sound insulation materials, and are widely used in industrial production and construction. In the industrial field, stitched nonwoven fabrics can be used in environmental protection projects such as oil-water separation and dust filtration. In the construction field, stitched nonwoven fabrics can be used for roof waterproofing, sound insulation walls, etc., providing a safer and more comfortable building environment.

[0052] Fifth, stitched nonwoven fabrics are increasingly used in automotive interiors and ceilings. Because the fabric has a certain texture, better scratch resistance than ordinary nonwoven fabrics, and the price is much lower than knitted fabrics, it has gradually been recognized by many automakers in recent years and its application has become more and more extensive.

[0053] At present, stitch-bonded nonwoven fabrics have problems such as a narrow range of final product weights, thin thickness, insufficient strength and elongation, and poor air permeability. These problems seriously hinder the application scope and scenarios of stitch-bonded nonwoven fabrics, making stitch-bonded nonwoven fabrics insufficient in product strength and difficult to be applied in multiple fields like needle-punched nonwoven fabrics, limiting the further development and market of stitch-bonded nonwoven fabrics. The existing stitch-bonded nonwoven fabrics in the related art have the problem of a narrow application scope.

[0054] Therefore, the embodiment of the present application proposes a method for producing a stitch-bonded nonwoven fabric to solve the above-mentioned problem.

[0055] The present application provides a method for producing a stitch-bonded nonwoven fabric. Figure 1 This is a flow chart of stitch-bonded nonwoven production. Figure 2 is a flowchart of steps S107-step S108 and steps S113-step S114 according to an exemplary embodiment. Figure 1 , Figure 2 As shown, a method for producing a stitch-bonded nonwoven fabric comprises:

[0056] Step S107: stitching the combed fibers into a cloth with a preset stitching length by a stitching machine.

[0057] Step S108, drying the stitched fabric, wherein the drying is used to adjust the hardness of the fabric.

[0058] Step S113: the wound upper fabric is placed on an upper unwinder, and the wound lower fabric is placed on a lower unwinder, with a hot melt film being provided between the upper fabric and the lower fabric.

[0059] Step S114: fusing the hot melt film with the upper fabric and the lower fabric in an oven to obtain a stitch-bonded nonwoven fabric.

[0060] In summary, the embodiment of the present application provides a method for producing a stitched non-woven fabric, which uses a stitching machine to stitch the combed fibers into a fabric of a preset stitching length; the stitched fabric is dried, and the drying is used to adjust the softness and hardness of the fabric; the wound upper fabric is placed on an upper unwinder, and the wound lower fabric is placed on a lower unwinder, and a hot melt film is provided between the upper fabric and the lower fabric; the hot melt film is fused with the upper fabric and the lower fabric through an oven to obtain a stitched non-woven fabric. The gram weight range is expanded, the product thickness is increased, and the strength is improved. The application field of stitched non-woven fabrics is expanded. The problem of narrow application range of existing stitched non-woven fabrics in the related art is solved.

[0061] Figure 3 is a flowchart of steps S101 to S105 according to an exemplary embodiment, as shown in FIG. Figure 3 As shown, before stitching the combed fibers into a cloth of a preset stitching length by a stitching machine, the method further includes:

[0062] Step S101: different types of fibers are fed into different bag opening machines according to production formulas, and the proportion of the input materials is controlled.

[0063] Optionally, different fibers (such as cotton, polyester, nylon, etc.) are mixed in precise proportions to achieve specific performance requirements, such as strength, hygroscopicity, softness, etc. For example, adding a certain proportion of polyester fibers can improve the wear resistance and elasticity of the fabric, while cotton fibers can enhance comfort and moisture absorption and breathability. By controlling the proportions through the bag opener, the precise delivery of raw materials can be achieved, ensuring the consistency of subsequent product quality.

[0064] Step S102: metal detection is performed on different types of fibers that have passed through the bag opener, and the raw materials after detection are initially mixed and loosened through a mixing bin.

[0065] Optionally, metal detection is an important part of ensuring safe production, which can prevent metal foreign matter from mixing into the production process, damaging equipment or affecting product quality. Once metal impurities are detected, measures are taken immediately to remove them to ensure the purity of the fibers. Subsequently, through the mixing and opening process in the mixing bin, different fibers are fully contacted and mixed evenly, and fiber clumps are opened at the same time, improving the uniformity and efficiency of subsequent processing.

[0066] Step S103, mixing and loosening the fibers after being mixed in the large bin.

[0067] Optionally, the mixing uniformity and opening degree of the fibers are further enhanced to ensure sufficient interweaving between the fibers, improve the fluffiness of the fiber layer and the uniformity of the subsequent web formation. This step helps to improve the uniformity and overall strength of the nonwoven fabric, and also provides a good fiber state for the subsequent molding process.

[0068] Step S104, the mixed and opened fibers are sucked into a cotton storage box through a fan for storage and standby use.

[0069] Optionally, the negative pressure of the fan can be used to transport the fibers to a cotton storage box, which reduces the labor intensity of manual handling and improves production efficiency. The cotton storage box serves as a temporary storage, which is convenient for timely supply of fiber raw materials according to production needs and ensures the continuity of the production process. At the same time, the cotton storage box can also isolate external pollution to a certain extent and keep the fibers clean.

[0070] Step S105: Send the fibers in the cotton storage box to the air pressure cotton box through a powerful fan, and accurately weigh the fibers through a belt scale.

[0071] Optionally, two powerful fans are used to send the fibers from the cotton storage box to the pneumatic cotton box, and the fibers are accurately weighed by a belt scale to ensure the uniformity of the product weight across the entire width. Specifically, the powerful fans ensure the continuity and speed of fiber transmission, and the pneumatic cotton box uses air flow pressure to maintain the loose state of the fibers, creating good conditions for the next processing (such as combing and web forming). The use of a belt scale enables accurate measurement of fiber weight, which is crucial for controlling the weight and cost of finished products and ensuring the accuracy of the formula. Accurate weighing helps standardize production, reduce raw material waste, and ensure the stability of product quality.

[0072] Step S101 to step S105 constitute a fiber pretreatment process, which not only ensures product quality, but also improves production efficiency and economic benefits, laying a solid foundation for subsequent non-woven fabric manufacturing.

[0073] In one embodiment, in step S105, after the fibers in the cotton storage box are sent to the air pressure cotton box by a powerful fan and the fibers are accurately weighed by a belt scale, the method further comprises:

[0074] Step S106: The weighed different fibers are combed by a combing machine into a cross-arranged and evenly mixed single-layer fiber web.

[0075] Optionally, the carding machine combs, mixes and cross-arranges the delivered fibers through the coordinated movement of a series of carding elements (such as carding rollers, fixed needle plates and movable needle plates). This process can effectively open the fiber bundles, remove impurities and lumps in the fibers, and make the fibers looser and more uniform. The fibers are transferred and combed multiple times during the carding process, achieving full mixing between the fibers and cross-arrangement of the fibers, which is conducive to improving the uniformity of subsequent web formation and the bonding force between the fibers. The staggered arrangement of the fibers increases the physical connection points, which improves the stability and strength of the fiber web.

[0076] In one embodiment, step S107, stitching the combed fibers into a cloth of a preset stitching length by a stitching machine, specifically includes:

[0077] The combed fibers are stitched together by a stitch-bonding machine to form a fiber web with the same or different stitching lengths on both sides.

[0078] Optionally, by adjusting the speed of the stitching machine, wherein the speed of the stitching machine can be 1m / min-5m / min, preferably 3m / min, the interweaving density of the fibers and the final form of the fiber web can be flexibly controlled, thereby producing a fiber web with the same or different stitching lengths on both sides. Different stitching lengths will affect the strength, softness, and air permeability of the fabric. The stitching process not only increases the transverse and longitudinal strength of the fiber web, but also improves the overall stability and durability of the fabric. By changing the stitching density and method, the strength in a specific direction can be targeted to meet the needs of different application fields.

[0079] In one embodiment, step S108, drying the stitched fabric, wherein the drying is used to adjust the hardness of the fabric. Specifically, the drying comprises:

[0080] Electric heating is used in a closed space, and the oven temperatures of the upper area and the lower area of ​​the fabric are controlled respectively by upper and lower heating plates, wherein the oven temperatures of the upper area and the lower area of ​​the fabric are controlled according to the characteristics of the fabric, the oven temperature of the upper area of ​​the fabric includes 50°C-250°C, and the oven temperature of the lower area of ​​the fabric includes 50°C-250°C.

[0081] Optionally, upper and lower heating plates are used for electrical heating, and the fabric is heated in the upper and lower high-temperature leather curtains, and a cooling component is provided at the rear of the oven for cooling. This design ensures uniform heat distribution, avoids local overheating, and improves the utilization efficiency of thermal energy. According to the characteristics of the fabric, the oven temperature of the upper and lower areas of the fabric is independently controlled, and the range is set to 50°C to 250°C, preferably 120°C to 200°C. This flexible temperature regulation mechanism is based on the understanding of the water evaporation rate, fiber structure changes, and softness and hardness requirements during the fabric drying process. The upper temperature is often set higher to accelerate water evaporation and promote fiber redirection, and enhance the hardness of the fabric; the lower temperature is relatively low, which helps to maintain the softness and structural stability of the fabric and prevent damage caused by overheating at the bottom. With the heating effect of the upper and lower heating plates, the moisture in the fabric is gradually evaporated, and the fibers undergo physical and chemical changes while losing moisture, which promotes the fixation of the structure and the adjustment of softness and hardness. The differential application of temperature accelerates this process and makes the final properties of the fabric more controllable.

[0082] Step S108 can precisely control the hardness of the fabric after drying by setting the difference in temperature between the upper and lower surfaces to meet the needs of different application scenarios. High temperature promotes tighter bonding between fibers and increases hardness, while low temperature helps to retain the natural softness of the fabric. This not only optimizes the drying effect of the fabric and ensures that the hardness of the product meets specific needs, but also improves production efficiency and energy efficiency.

[0083] In one embodiment, step S109, metal and defect detection: metal detection and defect detection are performed to find metal and remove defects to ensure that the fabric surface quality meets the standards and has no metal and defects. Specifically, it includes:

[0084] Carry out metal detection and defect detection to find out metal and remove defects to ensure that the fabric quality meets the standards and is free of metal and defects.

[0085] Optionally, metal detection includes but is not limited to the use of electromagnetic induction principles or X-ray detection technology. Electromagnetic induction metal detectors generate a magnetic field under the material. When a material containing metal passes through, it interferes with the original magnetic field, causing the current in the induction coil to change, thereby triggering an alarm and locating the metal foreign body. X-ray detection identifies the presence of metal and other high-density foreign matter by analyzing the change in the intensity of the rays after penetrating the material. Defect detection includes but is not limited to high-definition cameras, infrared scanning, laser scanning, etc. These technologies can capture the image information of the fabric, and identify surface defects such as color difference, holes, stains, broken wires, etc. through analysis and comparison by image processing software. By efficiently and accurately identifying and removing fabrics containing metal foreign matter or surface defects, the purity and aesthetics of the final product are ensured, and the overall quality level is improved.

[0086] In one embodiment, step S110, first product index detection: timely adjust the production line quality control parameters if unqualified. Specifically including:

[0087] Optionally, the initial quality inspection of the finished product is carried out, including: gram weight, thickness, strength and elongation index, to ensure that the performance indicators meet the predetermined standards. If unqualified products are found, feedback is immediately given and the quality control parameters on the production line are adjusted to correct the deviation and ensure that the subsequent products meet the requirements.

[0088] In one embodiment, step S111, first slitting: slitting the products into products of a specified width by a slitting machine, and removing the excess waste edges on both sides. Specifically, it includes:

[0089] Optionally, the slitting machine uses a sharp blade or laser cutting technology to accurately cut continuous large-area nonwovens into strips or blocks according to pre-set width dimensions. This process requires high-precision positioning control and stable cutting speed to ensure that the cut edges are flat, burr-free, and accurate in size. Cutting off the excess waste edges on both sides is to remove possible defects or uneven parts on the edges of the fabric, which may not meet the quality requirements due to edge effects in the previous production process. After cutting, the overall quality of the product can be improved.

[0090] In one embodiment, step S112, first winding: the product is wound into a full roll by a winder.

[0091] Specifically include:

[0092] Optionally, the winder mechanically winds the slit nonwoven strips or block products tightly and evenly into rolls. This process involves speed control, tension control and monitoring of winding diameter to ensure the compactness, flatness and uniformity of the coil. Before winding, there is usually a quality inspection link (including but not limited to defect detection and rejection equipment to remove defects in the product and effectively control defects and stains) to ensure that only qualified products enter the winding process and unqualified products will be rejected.

[0093] Step S111 and step S112 not only complete the transformation of the product from a large area to a specified size, but also ensure the high quality and standardization of the product through strict size control and quality inspection.

[0094] In one embodiment, step S113, the wound upper fabric is placed on an upper unwinder, and the wound lower fabric is placed on a lower unwinder, and a hot melt film is provided between the upper fabric and the lower fabric. Specifically, the process includes:

[0095] Optionally, first, the upper and lower layers of non-woven fabric are respectively wound into rolls by a winder, which is for the convenience of handling and subsequent lamination. The winding process needs to ensure the flatness and uniform tension of the fabric to avoid wrinkles or unevenness during lamination. A hot melt film is placed between the upper and lower layers of non-woven fabric. The hot melt film is a thin film material that can melt at a specific temperature and play a bonding role, usually made of polyethylene, polyurethane or other thermoplastic materials. It is located in the middle of the two layers of fabric so that it can melt and bond the fabric evenly during the subsequent hot pressing process.

[0096] Step S113, by adding hot-melt film, the thickness, strength, waterproofness, insulation and other properties of the non-woven fabric can be significantly enhanced, making it suitable for more diverse application scenarios, such as medical protective clothing, waterproof materials, filter media, etc. By selecting different types of hot-melt films and adjusting the number of composite layers, customized non-woven fabric products that meet the needs of different customers can be flexibly produced, broadening the application field of the product.

[0097] In one embodiment, step S114, fusing the hot melt film with the upper fabric and the lower fabric in an oven to obtain a stitch-bonded nonwoven fabric. Specifically, the step S114 includes:

[0098] According to the melting point of the hot melt film and the heat resistance of the fabric, the internal temperature of the oven is preset, wherein the preset internal temperature of the oven is 50°C-250°C, preferably 120°C-200°C;

[0099] The upper fabric is 100gsm-300gsm, with a thickness of 1mm-4mm, preferably 3mm-4mm; the lower fabric is 100gsm-300gsm, with a thickness of 1mm-4mm, preferably 3mm-4mm;

[0100] The nonwoven fabric is dried in an oven to obtain a 2mm-8mm stitched nonwoven fabric, wherein the drying time is 6min-15min, preferably 12min.

[0101] Optionally, the internal temperature of the oven is preset to 120°C to 200°C, which is a temperature range carefully set based on the melting point of the hot melt film and the heat resistance of the fabric. The temperature is high enough to ensure that the hot melt film can completely melt and flow, but it will not damage the fiber structure of the non-woven fabric, so as to achieve effective bonding between the hot melt film and the two layers of fabric. The weight range of the upper and lower fabrics is 100gsm to 300gsm, and the thickness is 3mm to 4mm. This design is to ensure structural stability and strength while also adapting to physical changes in the hot melt composite process to ensure the comprehensive performance of the final product. The circulating hot air system not only accelerates the melting process of the hot melt film, but also promotes the uniform distribution of heat energy, ensuring that every part of the entire composite material can be fully heat treated, avoiding local overheating or incomplete melting, and helping to form a uniform and consistent 6mm to 8mm thick stitched non-woven fabric. The drying time is set between 6 minutes and 15 minutes, which is long enough for the hot melt film to fully melt and penetrate between the fibers of the two layers of fabric, but not too long to cause overheating and damage to the fabric or increase energy consumption.

[0102] Step S114 achieves efficient and high-quality non-woven fabric hot-melt bonding through temperature, time and wind force control, solving the problems of narrow gram weight range, thin thickness, and insufficient strength and elongation performance.

[0103] In one embodiment, step S115, second product index detection: if the gram weight and thickness exceed the standard, adjust the oven spacing and temperature in time. Specifically include:

[0104] The stitched nonwoven fabric is subjected to product index testing, and relevant adjustments are made to the stitched nonwoven fabric that does not meet the product index to obtain the stitched nonwoven fabric that meets the product index, wherein the product index testing includes gram weight index, softness and hardness index, metal residue rate, strength index and thickness index testing.

[0105] In one embodiment, the stitch-bonded nonwoven fabric that does not meet the product specifications is adjusted to obtain the stitch-bonded nonwoven fabric that meets the product specifications, including:

[0106] When the weight and thickness of the stitch-bonded nonwoven fabric do not meet the product specifications, adjusting the oven spacing and the oven temperature;

[0107] When the hardness and strength index of the fabric do not meet the quality standards, adjusting the oven temperature of the upper area and the lower area of ​​the fabric;

[0108] In the case that the metal residue rate of the cloth does not meet the quality standard, the metal in the cloth is filtered and metal residue detection is performed on each device.

[0109] Optionally, by adjusting the spacing and temperature of the ovens, the melting degree of the hot melt film and the bonding effect between the fibers can be controlled, thereby affecting the gram weight and thickness of the final product. The reduction in the spacing of the ovens will increase the pressure of the hot melt film between the fabrics, which will help to increase the melting degree and fabric density, thereby changing the gram weight and thickness; the increase in temperature can accelerate the melting speed of the hot melt film, promote better bonding between the fibers and the hot melt film, and also help to change the gram weight and thickness. On the contrary, increasing the spacing or lowering the temperature can reduce the melting degree, change the gram weight and thickness. The precise control of the gram weight and thickness of the non-woven fabric is achieved to meet the predetermined product specifications, improve the uniformity and consistency of the product, and enhance market competitiveness. The hardness and softness of the fabric are mainly affected by factors such as fiber structure and degree of heat treatment. By adjusting the oven temperature of the upper and lower areas respectively, the degree of heat treatment of the fibers in these areas and the distribution of the hot melt film can be controlled, thereby affecting the hardness of the overall fabric. For example, increasing the temperature of a certain area can make the fibers in that area more relaxed, thereby adjusting the hardness and softness of the fabric as a whole. The hardness and softness of the fabric meet specific application requirements. For the problem of metal residue, dual measures of filtration and equipment testing are adopted. Adding metal filtering devices in the production process can physically intercept metal fragments that may be mixed in the production line and reduce metal residues in the final product. At the same time, regular metal residue testing of production equipment can timely detect and deal with metal debris generated by equipment wear and prevent it from entering the production materials. Significantly reduce the metal residue rate in the product, ensure product safety, and comply with industry safety standards and regulatory requirements.

[0110] In one embodiment, step S116, second slitting: slitting the products into products of a specified width by a slitting machine, and removing the excess waste edges on both sides. Specifically, it includes:

[0111] Optionally, the non-woven fabric material after composite treatment (such as hot melt film lamination, etc.) is further accurately cut into widths that meet customer requirements, and possible unevenness or excess parts at the edges are removed to ensure the quality of the finished product. The second slitting is a key step in non-woven fabric production to ensure that the final product specifications are accurate and the quality meets the standards, which is conducive to improving the quality of stitched products.

[0112] In one embodiment, step S117, second winding: the product is wound into a full roll by a winder.

[0113] Specifically include:

[0114] Optionally, the nonwoven fabric product that has been cut into a specified width is rolled into a roll again for storage, transportation, and subsequent processing or direct use.

[0115] The following are specific practical application examples of the embodiments of this application:

[0116] Example 1: A customer needs a stitched nonwoven fabric with a gram weight of 460gsm-600gsm and a thickness of 6-8mm or more. With a general stitching machine, the gram weight range is up to 350gsm, and we cannot provide samples. We now use this production line to first produce a stitched nonwoven fabric with a gram weight of 200-270gsm and a thickness of 3-4mm, and then add 40-60gsm of hot melt adhesive between the two layers of stitched nonwoven fabric to make the gram weight reach 460-600gsm and the thickness reach 6-8mm or more, meeting the customer's needs.

[0117] Example 2: The customer needs a 150gsm-250gsm stitched nonwoven fabric, one side of which needs to have a hot melt film. Now this production line is used to apply a 50gsm hot melt film on one side of the original stitched nonwoven fabric, which is convenient for customers to heat-fuse other products. This process can be used to fuse 100gsm-200gsm stitched nonwoven fabric and 50gsm hot melt film to meet customer needs. This process provides a nonwoven fabric and hot melt film fusion process.

[0118] In summary, the embodiment of the present application provides a method for producing a stitched non-woven fabric, which uses a stitching machine to stitch the combed fibers into a fabric of a preset stitching length; the stitched fabric is dried, and the drying is used to adjust the softness and hardness of the fabric; the wound upper fabric is placed on an upper unwinder, and the wound lower fabric is placed on a lower unwinder, and a hot melt film is provided between the upper fabric and the lower fabric; the hot melt film is fused with the upper fabric and the lower fabric through an oven to obtain a stitched non-woven fabric. The gram weight range is greatly expanded, the product thickness is increased, and the strength is improved. The application field of stitched non-woven fabrics is expanded. The problem of narrow application range of existing stitched non-woven fabrics in the related art is solved.

[0119] The beneficial effects of the present invention also include: the weight of the final product can be increased by hot melting the stitched nonwoven fabric in an oven, and the original weight of 80gsm-300gsm can be increased to 80gsm-600gsm. The weight range is greatly expanded, the product thickness is increased, the strength is increased, and the elongation and air permeability indicators are improved. This process has brought about the expansion of the application field of stitched nonwoven fabrics, making stitched nonwoven fabrics adaptable to a wider range of application requirements, and laying a solid foundation for the development of new markets in the future.

[0120] This process can bring the following practical benefits:

[0121] 1. The weight range of stitched non-woven fabrics has been expanded, laying a solid foundation for business expansion.

[0122] 2. It provides new non-woven products for the company's sales, which is conducive to enriching the product line and broadening the customer base.

[0123] 3. The innovation of this technology has improved the competitiveness of products compared with similar enterprises, indirectly improved the corporate image and competitiveness, and provided a guarantee for the long-term development of the enterprise.

[0124] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0125] The above embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent of the present application shall be subject to the attached claims.

Claims

1. A method for producing a stitch-bonded nonwoven fabric, characterized in that: The method comprises: The carded fibers are stitched into fabrics of a preset stitching length by a stitch-bonding machine; Drying the stitched fabric, wherein the drying is used to adjust the softness and hardness of the fabric; Placing the wound upper fabric on an upper unwinder, and placing the wound lower fabric on a lower unwinder, wherein a hot melt film is provided between the upper fabric and the lower fabric; The hot melt film is fused with the upper fabric and the lower fabric through an oven to obtain a stitch-bonded nonwoven fabric.

2. The method according to claim 1, characterized in that The hot melt film is fused with the upper fabric and the lower fabric through an oven to obtain a stitch-bonded nonwoven fabric, comprising: According to the melting point of the hot melt film and the heat resistance of the fabric, the internal temperature of the oven is preset, wherein the preset internal temperature of the oven is 50°C-250°C; The upper fabric is 100gsm-300gsm with a thickness of 1mm-4mm, and the lower fabric is 100gsm-300gsm with a thickness of 1mm-4mm; The nonwoven fabric is dried in an oven to obtain a 2mm-8mm stitched nonwoven fabric, wherein the drying time is 6min-15min.

3. The method according to claim 1, characterized in that After fusing the hot melt film with the upper fabric and the lower fabric through an oven to obtain a stitch-bonded nonwoven fabric, the method comprises: The stitched nonwoven fabric is subjected to product index testing, and relevant adjustments are made to the stitched nonwoven fabric that does not meet the product index to obtain the stitched nonwoven fabric that meets the product index, wherein the product index testing includes gram weight index, softness and hardness index, metal residue rate, strength index and thickness index testing, etc.

4. The method according to claim 3, characterized in that Make relevant adjustments to the stitched nonwoven fabrics that do not meet the product specifications to obtain stitched nonwoven fabrics that meet the product specifications, including: When the weight and thickness of the stitch-bonded nonwoven fabric do not meet the product specifications, adjusting the oven spacing and the oven temperature; When the hardness and strength index of the fabric do not meet the quality standards, adjusting the oven temperature of the upper area and the lower area of ​​the fabric; In the case that the metal residue rate of the cloth does not meet the quality standard, the metal in the cloth is filtered and metal residue detection is performed on each device.

5. The method according to claim 1, characterized in that The stitched fabric is dried, and the drying is used to adjust the softness and hardness of the fabric, including: Electric heating is used in a closed space, and heat is generated by an electric heating plate to control the oven temperatures of the upper area and the lower area of ​​the cloth respectively, wherein the oven temperatures of the upper area and the lower area of ​​the cloth are controlled according to the characteristics of the cloth, the oven temperature of the upper area of ​​the cloth includes 50°C-250°C, and the oven temperature of the lower area of ​​the cloth includes 50°C-250°C.

6. The method according to claim 1, characterized in that The hot melt film has a thickness of 40 gsm to 60 gsm.

7. The method according to claim 1, characterized in that Before stitching the combed fibers into a cloth of a preset stitching length by a stitching machine, the method further comprises: Different types of fibers are fed into different bale opening machines according to the production formula, and the proportion of input materials is controlled; The different types of fibers that pass through the bale opener are subjected to metal detection, and the raw materials after detection are initially mixed and loosened through the mixing bin; Further mixing and finely opening the fibers after mixing in the large bin; The mixed and opened fibers are sucked into a cotton storage box through a fan for storage and standby; The fibers in the cotton storage box are sent to the air pressure cotton box by a powerful fan, and the fibers are accurately weighed by a belt scale.

8. The method according to claim 7, characterized in that After the fibers in the cotton storage box are sent to the air pressure cotton box by a powerful fan and the fibers are accurately weighed by a belt scale, the method further comprises: The weighed different fibers are combed into a cross-arranged, evenly mixed single-layer fiber web through a carding machine.

9. The method according to claim 1, characterized in that: Before placing the wound upper fabric on the upper unwinder, the following steps are performed: The fabric is wound up by a winder to obtain a fabric roll.

10. The method according to claim 3, characterized in that After testing the stitch-bonded nonwoven fabric for product indicators, making relevant adjustments to the stitch-bonded nonwoven fabric that does not meet the product indicators, and obtaining the stitch-bonded nonwoven fabric that meets the product indicators, the method further includes: The slitting machine is used to cut the stitched nonwoven fabric into preset width and remove the excess waste edges.

Citation Information

Patent Citations

  • Manufacturing method of different-hardness non-woven fabric composite layer product

    CN103507388A

  • Technology for processing natural kapok fiber hot-rolled non-woven cloth

    CN104452102A

  • A filtering material made of non-woven charcoal cloth

    CN1943841A