Flame-retardant low-VOC (volatile organic compound) double-sided tape and preparation method thereof

By using specific material combinations and processes in automotive double-sided tape, adhesives with good flame retardant properties and low VOC emissions are prepared, which solves the problem of smoke and toxic gases in the prior art, and improves bonding strength and temperature resistance. Performance enhances the safety and service life of the car.

CN119060649AInactive Publication Date: 2024-12-03CROWN NEW MATERIALS TECHNOLOGY CO LTD

Patent Information

Application Number
CN202411188924.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-12-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

When the flame retardant performance of existing automobile double-sided tape is improved, it is prone to generate a large amount of smoke and toxic gases, affecting the environment and human health, and has poor effect on low VOC emissions.

Method used

The basic adhesive is prepared using polyurethane, epoxy resin, silane coupling agent and vinyl acetate, and mixed with acrylate polymers, aluminum hydroxide, antimony trioxide and phosphate to form flame retardant and low VOC adhesive. , through uniform coating and curing technology, double-sided tape with good flame retardant properties and low VOC emissions were prepared.

Benefits of technology

It achieves good flame retardant performance and low VOC emissions of double-sided tape, improves bonding strength and temperature resistance, reduces the impact on the environment and human health, and enhances the safety and service life of the car.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119060649A_ABST
    Figure CN119060649A_ABST
Patent Text Reader

Abstract

The invention discloses a flame-retardant low-VOC (volatile organic compound) double-sided adhesive tape and a preparation method thereof. The preparation method comprises the following steps: S1, preparing a basic adhesive; s2, preparing a combustion improver; s3, preparing the flame-retardant low-VOC adhesive; and S4, coating and curing. The special flame retardant and the low-VOC material are adopted, and the specific stabilizer and the modifier are added to optimize and improve the materials and the formula of the adhesive, so that the adhesive has good flame retardant property, can effectively reduce the emission of volatile organic compounds, can meet the flame retardant requirement of the double-sided adhesive tape, and can reduce the influence on the environment and human health; meanwhile, the bonding strength of the double-sided adhesive tape on a low-surface-energy material and a rough material is also improved, so that the performance and the safety of an automobile are improved; the performance stability of the double-sided adhesive tape in high-temperature and low-temperature environments is improved, and good bonding performance can be kept in extreme environments, so that the using effect of an automobile is improved, and the service life of the automobile is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of double-sided adhesive tapes, in particular to a flame-retardant low-VOC double-sided adhesive tape and a preparation method thereof. Background Art

[0002] With the rapid development of the automotive industry, automobile safety and environmental friendliness have become increasing concerns. Flame retardancy in automotive materials and the control of volatile organic compounds (VOCs) have become two key research areas. Flame retardancy refers to the ability of a material to prevent the spread of flames when exposed to a fire source, thereby protecting the vehicle and its passengers. VOCs, on the other hand, are harmful gases released during the use of a material, which can impact the environment and human health. Therefore, how to reduce VOC emissions while ensuring flame retardancy has become a pressing issue for the automotive industry, particularly in the production of double-sided automotive tape.

[0003] Existing solutions primarily involve improving adhesive formulations by adding flame retardants and low-VOC raw materials to achieve flame retardancy and low-VOC properties. For example, some adhesive manufacturers add halogenated flame retardants to enhance the flame retardancy of double-sided tapes. However, these halogenated flame retardants produce large amounts of smoke and toxic gases during combustion, posing a threat to the environment and human health. Summary of the Invention

[0004] In order to overcome the deficiencies of the prior art, the present invention provides a flame retardant low-VOC double-sided adhesive tape and a preparation method thereof.

[0005] The technical solution adopted by the present invention to solve its technical problem is:

[0006] A method for preparing a flame-retardant, low-VOC double-sided adhesive tape comprises the following steps:

[0007] S1. Preparation of base adhesive: polyurethane, epoxy resin, silane coupling agent and vinyl acetate are mixed in a weight ratio of 100:50:20:10 to obtain a mixed solution A, and the mixed solution A is stirred at 50-70° C. for 30-90 minutes to obtain a base adhesive;

[0008] S2. Preparation of flame retardant: Mixing an acrylic polymer, aluminum hydroxide, antimony trioxide, and a phosphate in a weight ratio of 100:30:10:5 to obtain a mixed solution B, and stirring the mixed solution B at 70-100° C. for 100-150 minutes to obtain a flame retardant;

[0009] S3. Preparation of a flame-retardant low-VOC adhesive: The base adhesive prepared in step S1 and the flame retardant prepared in step S2 are mixed in a weight ratio of 180:145 to obtain a mixed solution C, and the mixed solution C is stirred at 60-80° C. for 30-90 minutes to obtain a flame-retardant low-VOC adhesive;

[0010] S4, coating and curing: The flame retardant low VOC adhesive prepared in step S3 is evenly coated on the substrate, and then the substrate coated with the flame retardant low VOC adhesive is placed at 70-90° C. for curing for 150-200 minutes to obtain a flame retardant low VOC double-sided tape.

[0011] The method for preparing a flame-retardant, low-VOC double-sided adhesive tape as described above further comprises, after step S4, performing the following steps:

[0012] S5. Performance test: The flame retardant low-VOC double-sided tape prepared in step S4 is tested in terms of flame retardancy, low VOC emissions, bonding strength, and temperature resistance in accordance with the corresponding national industry standards, and the flame retardant low-VOC double-sided tape that does not meet the standards is discarded.

[0013] In the method for preparing a flame-retardant, low-VOC double-sided tape as described above, in step S4, the flame-retardant, low-VOC adhesive is applied to a thickness of 0.1-0.3 mm.

[0014] In the method for preparing a flame-retardant, low-VOC double-sided tape as described above, in step S4, the thickness of the flame-retardant, low-VOC adhesive coating is 0.2 mm.

[0015] In the method for preparing a flame-retardant, low-VOC double-sided tape as described above, in step S4, the flame-retardant, low-VOC adhesive is evenly coated on the upper and lower surfaces of the substrate.

[0016] In the method for preparing a flame-retardant, low-VOC double-sided tape as described above, in step S1, the mixed solution A is stirred at 60° C. for 60 minutes to prepare a basic adhesive.

[0017] In the method for preparing a flame-retardant low-VOC double-sided adhesive tape as described above, in step S2, the mixed solution B is stirred at 80° C. for 120 minutes to prepare a flame retardant.

[0018] In the method for preparing a flame-retardant, low-VOC double-sided adhesive tape as described above, in step S3, the mixed solution C is stirred at 70° C. for 60 minutes to obtain a flame-retardant, low-VOC adhesive.

[0019] In the method for preparing a flame-retardant, low-VOC double-sided tape as described above, in step S4, the substrate coated with the flame-retardant, low-VOC adhesive is placed at 80° C. and cured for 180 minutes to obtain the flame-retardant, low-VOC double-sided tape.

[0020] The present application also discloses a flame-retardant low-VOC double-sided adhesive tape, which is prepared using the flame-retardant low-VOC double-sided adhesive tape preparation method described above.

[0021] The beneficial effects of the present invention are: by adopting special flame retardants and low-VOC materials, adding specific stabilizers and modifiers, to optimize and improve the materials and formula of the adhesive, the adhesive has good flame retardant properties and can effectively reduce the emission of organic volatiles, which not only meets the flame retardant requirements of double-sided tapes, but also reduces the impact on the environment and human health; at the same time, it also improves the bonding strength of the double-sided tape on low surface energy materials and rough materials, thereby improving the performance and safety of the car; and improves the performance stability of the double-sided tape in high and low temperature environments, and can maintain good bonding properties in extreme environments, thereby improving the use effect and life of the car. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without any creative work.

[0023] Figure 1 This is a flow chart of the steps of a method for preparing a flame-retardant, low-VOC double-sided tape according to an embodiment of the present invention.

[0024] Figure 2 It is a structural schematic diagram of a flame-retardant low-VOC double-sided tape according to an embodiment of the present invention.

[0025] Label: 1. Base material; 2. Flame retardant low VOC adhesive; 3. Release material. DETAILED DESCRIPTION

[0026] The technical solution of the present invention is described in detail below with reference to the accompanying drawings and embodiments.

[0027] See Figure 1 and Figure 2 As shown, the embodiment of the present application provides a method for preparing a flame retardant low VOC double-sided tape, comprising performing the following steps:

[0028] S1. Preparation of base adhesive: polyurethane, epoxy resin, silane coupling agent and vinyl acetate are mixed in a weight ratio of 100:50:20:10 to obtain a mixed solution A, and the mixed solution A is stirred at 50-70° C. for 30-90 minutes to obtain a base adhesive;

[0029] S2. Preparation of flame retardant: Mixing an acrylic polymer, aluminum hydroxide, antimony trioxide, and a phosphate in a weight ratio of 100:30:10:5 to obtain a mixed solution B, and stirring the mixed solution B at 70-100° C. for 100-150 minutes to obtain a flame retardant;

[0030] S3. Preparation of a flame-retardant low-VOC adhesive: The base adhesive prepared in step S1 and the flame retardant prepared in step S2 are mixed in a weight ratio of 180:145 to obtain a mixed solution C, and the mixed solution C is stirred at 60-80° C. for 30-90 minutes to obtain a flame-retardant low-VOC adhesive;

[0031] S4, coating and curing: The flame retardant low VOC adhesive prepared in step S3 is evenly coated on the substrate, and then the substrate coated with the flame retardant low VOC adhesive is placed at 70-90° C. for curing for 150-200 minutes to obtain a flame retardant low VOC double-sided tape.

[0032] By using special flame retardants and low-VOC materials, and adding specific stabilizers and modifiers to optimize and improve the materials and formula of the adhesive, the adhesive has good flame retardant properties and can effectively reduce the emission of organic volatiles. This not only meets the flame retardant requirements of double-sided tape, but also reduces the impact on the environment and human health. At the same time, it also improves the bonding strength of double-sided tape on low-surface energy materials and rough materials, thereby improving the performance and safety of the vehicle. It also improves the performance stability of double-sided tape in high and low temperature environments, and can maintain good bonding properties in extreme environments, thereby improving the use effect and life of the vehicle.

[0033] Furthermore, after step S4, the following steps are also performed:

[0034] S5. Performance test: The flame retardant low-VOC double-sided tape prepared in step S4 is tested in terms of flame retardancy, low VOC emissions, bonding strength, and temperature resistance in accordance with the corresponding national industry standards, and the flame retardant low-VOC double-sided tape that does not meet the standards is discarded.

[0035] Through rigorous testing in step S5, it is ensured that the performance indicators of the adhesive can meet the requirements of the automotive industry, including flame retardancy, low VOC emissions, bonding strength, temperature resistance, etc.

[0036] Furthermore, in step S4, the flame retardant low VOC adhesive is applied to a thickness of 0.1-0.3 mm.

[0037] In this embodiment, preferably, the thickness of the flame retardant low VOC adhesive coating is 0.2 mm.

[0038] In this embodiment, preferably, in step S4, the substrate coated with the flame-retardant low-VOC adhesive is placed at 80° C. and cured for 180 minutes to obtain a flame-retardant low-VOC double-sided tape.

[0039] Specifically, in step S4, the flame retardant low-VOC adhesive is evenly coated on the upper and lower surfaces of the substrate.

[0040] Through the coating and curing technology of step S4, the adhesive forms a uniform and stable coating on the substrate, further improving the bonding performance and stability of the adhesive.

[0041] In this embodiment, preferably, in step S1, the mixed solution A is stirred at 60° C. for 60 minutes to prepare a basic adhesive.

[0042] By optimizing and controlling the stirring speed and time in step S1, the mixing degree and chemical reaction rate of the raw materials of the base adhesive during the stirring process are maintained within an appropriate range, thereby further reducing the occurrence of chemical reactions, reducing the emission of pollutants such as waste gas and wastewater, and reducing environmental pollution.

[0043] In this embodiment, preferably, in step S2, the mixed solution B is stirred at 80°C for 120 minutes to prepare the flame retardant.

[0044] By optimizing and controlling the stirring speed and time in step S2, the mixing degree and chemical reaction rate of the raw materials of the flame retardant during the stirring process are maintained within an appropriate range, thereby further reducing the occurrence of chemical reactions, reducing the emission of pollutants such as waste gas and wastewater, and reducing environmental pollution.

[0045] In this embodiment, preferably, in step S3, the mixed solution C is stirred at 70° C. for 60 minutes to obtain a flame retardant low-VOC adhesive.

[0046] By optimizing and controlling the stirring speed and time in step S3, the mixing degree and chemical reaction rate of the base adhesive and the flame retardant during the stirring process are maintained within an appropriate range, thereby further reducing the occurrence of chemical reactions, reducing the emission of pollutants such as waste gas and wastewater, and reducing environmental pollution.

[0047] The embodiment of the present application also provides a flame-retardant low-VOC double-sided adhesive tape, which is produced using the flame-retardant low-VOC double-sided adhesive tape preparation method described above.

[0048] The flame-retardant, low-VOC double-sided tape of the present application not only has good flame-retardant properties and can effectively prevent the spread or spread of flames, protecting the safety of vehicles and passengers, but also does not produce a large amount of smoke and toxic gases during the combustion process, and has little impact on the environment and human health;

[0049] At the same time, it has high-strength bonding ability on low surface energy materials and rough materials, which not only improves the performance and safety of the car, but also can be used on a variety of different materials, increasing the flexibility and convenience of use;

[0050] As well as stable performance in high and low temperature environments, this can not only improve the use effect of the car and extend its service life, but also can be used in a variety of environmental conditions, increasing the scope of use and adaptability.

[0051] In summary, the flame-retardant, low-VOC double-sided tape prepared by the preparation method of the present application not only meets the requirements of flame retardancy and low VOC, but also has the advantages of high-strength bonding and high and low temperature resistance, which greatly improves the safety, stability and applicability of the double-sided tape and extends its service life.

[0052] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structures made using the contents of the present invention's description and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.

Claims

1. A method for preparing a flame retardant low VOC double-sided tape, characterized in that: This involves performing the following steps: S1. Preparation of base adhesive: polyurethane, epoxy resin, silane coupling agent and vinyl acetate are mixed in a weight ratio of 100:50:20:10 to obtain a mixed solution A, and the mixed solution A is stirred at 50-70° C. for 30-90 minutes to obtain a base adhesive; S2. Preparation of flame retardant: acrylic polymer, aluminum hydroxide, antimony trioxide and phosphate are mixed in a weight ratio of 100:30:10:5 to obtain a mixed solution B, and the mixed solution B is stirred at 70-100° C. for 100-150 minutes to obtain a flame retardant; S3, preparation of flame retardant low VOC adhesive: the base adhesive prepared in step S1 and the flame retardant prepared in step S2 are mixed in a weight ratio of 180:145 to obtain a mixed solution C, and the mixed solution C is stirred at 60-80° C. for 30-90 min to obtain a flame retardant low VOC adhesive; S4, coating and curing: the flame retardant low VOC adhesive prepared in step S3 is evenly coated on the substrate, and then the substrate coated with the flame retardant low VOC adhesive is placed at 70-90° C. for curing for 150-200 minutes to obtain a flame retardant low VOC double-sided tape.

2. The method for preparing a flame retardant low VOC double-sided tape according to claim 1, characterized in that: After step S4, the following steps are also performed: S5. Performance test: The flame retardant low-VOC double-sided tape prepared in step S4 is tested in terms of flame retardancy, low VOC emission, bonding strength, and temperature resistance in accordance with the corresponding national industry standards, and the flame retardant low-VOC double-sided tape that does not meet the standards is discarded.

3. The method for preparing a flame retardant low VOC double-sided adhesive tape according to claim 1, characterized in that: In step S4, the flame retardant low VOC adhesive is coated to a thickness of 0.1-0.3 mm.

4. The method for preparing a flame retardant low VOC double-sided adhesive tape according to claim 3, characterized in that: In step S4, the flame retardant low VOC adhesive is coated to a thickness of 0.2 mm.

5. The method for preparing a flame retardant low VOC double-sided adhesive tape according to claim 1 or 3, characterized in that: In step S4, the flame retardant low VOC adhesive is evenly coated on the upper and lower surfaces of the substrate.

6. The method for preparing a flame retardant low VOC double-sided tape according to claim 1, characterized in that: In step S1, the mixed solution A is stirred at 60° C. for 60 minutes to obtain a basic adhesive.

7. The method for preparing a flame retardant low VOC double-sided tape according to claim 1, characterized in that: In step S2, the mixed solution B is stirred at 80°C for 120 minutes to obtain a flame retardant.

8. The method for preparing a flame retardant low VOC double-sided tape according to claim 1, characterized in that: In step S3, the mixed solution C is stirred at 70° C. for 60 minutes to obtain a flame retardant low-VOC adhesive.

9. The method for preparing a flame retardant low VOC double-sided adhesive tape according to claim 1, characterized in that: In step S4, the substrate coated with the flame retardant low VOC adhesive is placed at 80° C. for curing for 180 minutes to obtain a flame retardant low VOC double-sided tape.

10. A flame retardant low VOC double-sided tape, characterized in that: The flame retardant low VOC double-sided adhesive tape is prepared by the method for preparing the flame retardant low VOC double-sided adhesive tape as described in any one of claims 1 to 9.

Citation Information

Patent Citations

  • Composite flame-retardant film and preparation method thereof

    CN102220093A

  • Flame-retardant adhesive tape with high-temperature color-changing early-warning function and preparation method thereof

    CN110343479A

  • Adhesive and high-viscosity flame-retardant double-sided tape

    CN117186806A

Cited By

  • Low-VOC (volatile organic compound) flame-retardant double-faced adhesive tape for automotive trim and preparation method thereof

    CN120718563A