Converter high-temperature high-carbon low-nitrogen production control method

By detecting and controlling the nitrogen content, adding calcium silicate and predicting the scrap steel output, and monitoring key parameters in real time, the problem of inaccurate nitrogen content control in the existing technology is solved, and more efficient nitrogen content control and energy utilization are achieved.

CN119061229APending Publication Date: 2024-12-03SHANDONG IRON & STEEL GRP YONGFENG LINGANG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411337454.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-25
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The existing converter high-temperature, high-carbon, low-nitrogen production control methods cannot accurately predict and calculate the addition of auxiliary materials, resulting in insufficient control of nitrogen content and easy control errors.

Method used

By detecting nitrogen content, controlling oxygen supply and fuel combustion conditions, setting the smelting temperature between 1600°C and 1700°C, adding calcium silicate when the nitrogen content exceeds the threshold, predicting the nitrogen in the next time period based on the existing nitrogen content The content is calculated and the scrap steel is discharged, and the key parameters during the smelting process are monitored in real time and timely adjusting operating parameters.

Benefits of technology

It achieves more precise control of nitrogen content, improves energy utilization, reduces the occurrence of control errors, and improves production stability and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119061229A_ABST
    Figure CN119061229A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of steel smelting, in particular to a converter high-temperature high-carbon low-nitrogen production control method which comprises the steps of detecting the nitrogen content, controlling oxygen supply and fuel combustion conditions in a converter and monitoring the nitrogen content. The smelting temperature is set, and the temperature is controlled between 1600 DEG C and 1700 DEG C; when it is detected that the nitrogen content exceeds a threshold value, the slag component of calcium silicate is added to reduce the nitrogen content in the slag; on the basis of the existing nitrogen content, the nitrogen content of the next time period is predicted, the required waste steel feeding amount is calculated, and waste steel feeding is conducted; key parameters including temperature, pressure and gas components in the smelting process are monitored in real time, and operation parameters are adjusted in time. According to the method, by predicting the nitrogen content and calculating the addition amount of the waste steel, the utilization rate of energy is higher, control over the nitrogen content is more accurate, control errors are not likely to be generated, and better use prospects and commercial value are brought.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of steel smelting, and in particular relates to a converter high-temperature high-carbon low-nitrogen production control method. Background Art

[0002] The high-temperature, high-carbon, low-nitrogen production control method of the converter refers to a technical solution in the steel smelting process, which aims to achieve high-efficiency, low-carbon and low-nitrogen production goals by optimizing the charge ratio, operating parameters and smelting process. The converter is an important industrial equipment used for steelmaking. It is mainly used to convert molten iron, that is, liquid iron obtained from smelting equipment such as blast furnaces, into various grades of steel. It adjusts the content of carbon and other alloy elements in the molten iron by blowing in oxygen and fuel to achieve the desired chemical composition and physical properties.

[0003] The existing converter high-temperature, high-carbon, low-nitrogen production control method cannot accurately predict and calculate the addition of auxiliary materials, resulting in inaccurate control of nitrogen content and easy control errors. Summary of the invention

[0004] In view of the deficiencies in the prior art, the present invention provides a converter high-temperature, high-carbon, low-nitrogen production control method to solve the above technical problems.

[0005] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a converter high-temperature, high-carbon, low-nitrogen production control method, characterized in that the control method comprises: S1: detecting the nitrogen content, controlling the oxygen supply and fuel combustion conditions in the furnace, and monitoring the nitrogen content; S2: setting the smelting temperature, and controlling the temperature between 1600°C and 1700°C; S3: when it is detected that the nitrogen content exceeds the threshold, adding calcium silicate slag components to reduce the nitrogen content in the slag; S4: based on the existing nitrogen content, predicting the nitrogen content in the next time period, calculating the required amount of scrap steel to be put in, and putting in the scrap steel; S5: real-time monitoring of key parameters in the smelting process, including temperature, pressure and gas composition, and timely adjusting the operating parameters.

[0006] Preferably, the step of S1 is: Before smelting begins, check the working status of the nitrogen analyzer, calibrate and verify the accuracy of the instrument; take samples from the furnace and obtain samples directly from the molten iron through the sampling device; The sample is sent into the analysis chamber of the nitrogen analysis instrument and the sample is heated to release the nitrogen in the sample; The nitrogen analyzer uses the absorption method to measure the nitrogen content in the sample, and then analyzes the absorption spectrum of nitrogen to determine the concentration of nitrogen; According to the results of nitrogen content analysis, adjust the oxygen supply and fuel combustion conditions in the furnace, including adjusting the position of the fuel nozzle and increasing the reducing gas; Record the analysis results, including sample identification, sampling time and analysis time, and record the operating parameters and instrument status during the analysis.

[0007] Preferably, the step of S2 is: Set the target temperature and control the smelting temperature between 1600°C and 1700°C; Use infrared temperature measuring instruments outside the furnace to monitor the temperature inside the furnace in real time; According to the real-time monitoring of the furnace temperature, the fuel supply is adjusted, and the amount of fuel input is increased or decreased to control the combustion heat in the furnace, thereby controlling the furnace temperature; Adjust combustion conditions, including air supply, fuel distribution and control of combustion area; Maintain and adjust the reducing atmosphere in the furnace to reduce the oxide content in the slag; Continuously monitor furnace temperature changes and adjust fuel supply and combustion conditions based on real-time data; Record each furnace temperature measurement data and adjustment operation to form a data record of the smelting process.

[0008] Preferably, the step of S3 is: Based on the data from the nitrogen analyzer, the nitrogen content in the slag has exceeded the set threshold; Prepare calcium silicate as a conditioning agent, calcium silicate is supplied in the form of powder and granules; According to the amount of slag and the degree of excess nitrogen content, calcium silicate is added to the slag and is placed on the surface of the slag through the furnace top hopper; After adding calcium silicate, the slag is fully mixed and stirred to promote the reaction of calcium silicate with nitrogen compounds in the slag, convert the nitrogen compounds into non-volatile compounds, and reduce the nitrogen content in the slag; The chemical composition of the slag changes after calcium silicate reacts with nitrogen compounds in the slag. The chemical composition and nitrogen content of the slag are continuously monitored; Record the operation time, quality and effect of adding calcium silicate.

[0009] Preferably, the step of S4 is: Data collection and analysis: Collect and analyze key data from the current smelting process, including the chemical composition of the current slag and metal, and the current nitrogen content; Use historical and current data to develop a predictive model for nitrogen levels; The prediction model formula is: ; in, is the predicted value for the next time period, is the observed value of nitrogen content at the current time point, and α is the smoothing coefficient; The amount of scrap steel that needs to be added is calculated based on the predicted nitrogen content target that needs to be adjusted in the next time period, which is determined by calculating the difference between the total amount of nitrogen in the current slag and the target nitrogen content; Preferably, the calculation formula for the amount of scrap steel added is: ; Among them, N c is the total amount of nitrogen in the current slag, N t is the predicted target nitrogen content, S add is the amount of scrap steel to be added, S g is the nitrogen content of nitrogen-containing scrap steel; Scrap steel is added according to the calculated scrap steel amount.

[0010] Calculate the amount of scrap steel to be added and add the scrap steel.

[0011] Preferably, the operation steps of putting in scrap steel are: Prepare scrap steel: Prepare scrap steel according to the calculated scrap steel input quantity. The scrap steel is pre-sorted, cut and processed; Putting scrap steel: Put the prepared scrap steel into the furnace at the set time and method, and put it through the furnace top hopper; Monitor reaction: After adding scrap steel, monitor the reaction in the furnace and the changes in slag composition, pay attention to the changes in nitrogen content, and ensure that it meets the expected adjustment target; Adjustment and recording: Adjustment is made based on the actual amount of scrap steel put in and the changes in the monitored slag composition; Record the amount of scrap steel added, the reaction effect and the final slag composition changes for future production process optimization and quality control.

[0012] Preferably, the step of S5 is: Clearly define the key parameters that need to be monitored, including furnace temperature, pressure and gas concentration; Install sensors and instruments in smelting equipment and systems to monitor these parameters in real time; Sensors can collect and transmit data to monitoring systems; Establish a dedicated monitoring system and integrate it with the existing automation control system to display and record the changes of various parameters in real time; According to process requirements and safety standards, set the alarm threshold of each parameter. When any parameter exceeds the preset safety and process range, the system will sound an alarm and prompt the operator. Operators can view the status and trends of key parameters in real time through the monitoring interface, which clearly displays current values, historical data and predicted changes; Use historical data and trend analysis tools to identify periodic changes or anomalies in key parameters for more accurate adjustments and forecasts; Adjust based on monitoring results: Based on real-time monitoring data and preset process goals, operators take measures to adjust operating parameters.

[0013] Preferably, the parameter adjustment measures include: Temperature regulation: adjust fuel supply and cooling medium flow rate according to furnace temperature changes; Pressure management: Adjust gas and liquid pressure control devices to ensure pressure is maintained within safe and operational specifications; Gas composition control: Adjust the supply of oxygen and other gases to maintain the desired atmosphere and chemical reaction conditions.

[0014] Preferably, all monitoring data and changes in operating parameters are recorded and archived, and the effects of adjusting operating parameters are regularly evaluated to ensure that the stability of the smelting process, production efficiency and product quality meet the expected standards.

[0015] Compared with the prior art, the present invention has the following beneficial effects: This application predicts the nitrogen content and calculates the amount of scrap steel to be added, thereby making energy utilization more efficient, making the control of nitrogen content more precise, and being less likely to cause control errors, thereby bringing better usage prospects and commercial value. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a flow chart of the steps of the present invention. DETAILED DESCRIPTION

[0017] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0018] Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in the field without making any creative work shall fall within the scope of protection of the present invention.

[0019] The present invention provides a technical solution: a converter high-temperature, high-carbon, low-nitrogen production control method, the control method comprising: S1: Detect nitrogen content, control oxygen supply and fuel combustion conditions in the furnace, and monitor nitrogen content; S2: Set the smelting temperature and control the temperature between 1600°C and 1700°C; S3: When it is detected that the nitrogen content exceeds a threshold value, a slag component of calcium silicate is added to reduce the nitrogen content in the slag; S4: Based on the existing nitrogen content, the nitrogen content in the next time period is predicted, the required amount of scrap steel to be put in is calculated, and the scrap steel is put in; S5: Real-time monitoring of key parameters in the smelting process, including temperature, pressure and gas composition, and timely adjustment of operating parameters.

[0020] Furthermore, the steps of S1 are: Before smelting begins, check the working status of the nitrogen analyzer, calibrate and verify the accuracy of the instrument; take samples from the furnace and obtain samples directly from the molten iron through the sampling device; The sample is sent into the analysis chamber of the nitrogen analysis instrument and the sample is heated to release the nitrogen in the sample; The nitrogen analyzer uses the absorption method to measure the nitrogen content in the sample, and then analyzes the absorption spectrum of nitrogen to determine the concentration of nitrogen; According to the results of nitrogen content analysis, adjust the oxygen supply and fuel combustion conditions in the furnace, including adjusting the position of the fuel nozzle and increasing the reducing gas; Record the analysis results, including sample identification, sampling time and analysis time, and record the operating parameters and instrument status during the analysis.

[0021] Furthermore, the steps of S2 are: Set the target temperature and control the smelting temperature between 1600°C and 1700°C; Use infrared temperature measuring instruments outside the furnace to monitor the temperature inside the furnace in real time; According to the real-time monitoring of the furnace temperature, the fuel supply is adjusted, and the amount of fuel input is increased or decreased to control the combustion heat in the furnace, thereby controlling the furnace temperature; Adjust combustion conditions, including air supply, fuel distribution and control of combustion area; Maintain and adjust the reducing atmosphere in the furnace to reduce the oxide content in the slag; Continuously monitor furnace temperature changes and adjust fuel supply and combustion conditions based on real-time data; Record each furnace temperature measurement data and adjustment operation to form a data record of the smelting process.

[0022] Furthermore, the steps of S3 are: Based on the data from the nitrogen analyzer, the nitrogen content in the slag has exceeded the set threshold; Prepare calcium silicate as a conditioning agent, calcium silicate is supplied in the form of powder and granules; According to the amount of slag and the degree of excess nitrogen content, calcium silicate is added to the slag and is placed on the surface of the slag through the furnace top hopper; After adding calcium silicate, the slag is fully mixed and stirred to promote the reaction of calcium silicate with nitrogen compounds in the slag, convert the nitrogen compounds into non-volatile compounds, and reduce the nitrogen content in the slag; The chemical composition of the slag changes after calcium silicate reacts with nitrogen compounds in the slag. The chemical composition and nitrogen content of the slag are continuously monitored; Record the operation time, quality and effect of adding calcium silicate.

[0023] Furthermore, the steps of S4 are: Data collection and analysis: Collect and analyze key data from the current smelting process, including the chemical composition of the current slag and metal, and the current nitrogen content; Use historical and current data to develop a predictive model for nitrogen levels; The prediction model formula is: ; in, is the predicted value for the next time period, is the observed value of nitrogen content at the current time point, and α is the smoothing coefficient; The amount of scrap steel that needs to be added is calculated based on the predicted nitrogen content target that needs to be adjusted in the next time period, which is determined by calculating the difference between the total amount of nitrogen in the current slag and the target nitrogen content; Calculate the amount of scrap steel to be added and add the scrap steel.

[0024] Furthermore, the calculation formula for the amount of scrap steel added is: ; Among them, N c is the total amount of nitrogen in the current slag, N t is the predicted target nitrogen content, S add is the amount of scrap steel to be added, S g is the nitrogen content of nitrogen-containing scrap steel; Scrap steel is added according to the calculated scrap steel amount.

[0025] Furthermore, the operation steps of scrap steel delivery are as follows: Prepare scrap steel: Prepare scrap steel according to the calculated scrap steel input quantity. The scrap steel is pre-sorted, cut and processed; Putting scrap steel: Put the prepared scrap steel into the furnace at the set time and method, and put it through the furnace top hopper; Monitor reaction: After adding scrap steel, monitor the reaction in the furnace and the changes in slag composition, pay attention to the changes in nitrogen content, and ensure that it meets the expected adjustment target; Adjustment and recording: Adjustment is made based on the actual amount of scrap steel put in and the changes in the monitored slag composition; Record the amount of scrap steel added, the reaction effect and the final slag composition changes for future production process optimization and quality control.

[0026] Furthermore, the steps of S5 are: Clearly define the key parameters that need to be monitored, including furnace temperature, pressure and gas concentration; Install sensors and instruments in smelting equipment and systems to monitor these parameters in real time; Sensors can collect and transmit data to monitoring systems; Establish a dedicated monitoring system and integrate it with the existing automation control system to display and record the changes of various parameters in real time; According to process requirements and safety standards, set the alarm threshold of each parameter. When any parameter exceeds the preset safety and process range, the system will sound an alarm and prompt the operator. Operators can view the status and trends of key parameters in real time through the monitoring interface, which clearly displays current values, historical data and predicted changes; Use historical data and trend analysis tools to identify periodic changes or anomalies in key parameters for more accurate adjustments and forecasts; Adjust based on monitoring results: Based on real-time monitoring data and preset process goals, operators take measures to adjust operating parameters.

[0027] Further, parameter adjustment measures include: Temperature regulation: adjust fuel supply and cooling medium flow rate according to furnace temperature changes; Pressure management: Adjust gas and liquid pressure control devices to ensure pressure is maintained within safe and operational specifications; Gas composition control: Adjust the supply of oxygen and other gases to maintain the desired atmosphere and chemical reaction conditions.

[0028] Furthermore, all monitoring data and changes in operating parameters are recorded and archived, and the effects of adjusting operating parameters are regularly evaluated to ensure that the stability of the smelting process, production efficiency and product quality meet the expected standards.

[0029] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0030] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A converter high temperature, high carbon, low nitrogen production control method, characterized in that: Control methods include: S1: Detect nitrogen content, control oxygen supply and fuel combustion conditions in the furnace, and monitor nitrogen content; S2: Set the smelting temperature and control the temperature between 1600°C and 1700°C; S3: When it is detected that the nitrogen content exceeds a threshold value, a slag component of calcium silicate is added to reduce the nitrogen content in the slag; S4: Based on the existing nitrogen content, the nitrogen content in the next time period is predicted, the required amount of scrap steel to be put in is calculated, and the scrap steel is put in; S5: Real-time monitoring of key parameters in the smelting process, including temperature, pressure and gas composition, and timely adjustment of operating parameters.

2. The converter high temperature, high carbon, low nitrogen production control method according to claim 1, characterized in that: The steps of S1 are: Before smelting begins, check the working status of the nitrogen analyzer, calibrate and verify the accuracy of the instrument; take samples from the furnace and obtain samples directly from the molten iron through the sampling device; The sample is sent into the analysis chamber of the nitrogen analysis instrument and the sample is heated to release the nitrogen in the sample; The nitrogen analyzer uses the absorption method to measure the nitrogen content in the sample, and then analyzes the absorption spectrum of nitrogen to determine the concentration of nitrogen; According to the results of nitrogen content analysis, adjust the oxygen supply and fuel combustion conditions in the furnace, including adjusting the position of the fuel nozzle and increasing the reducing gas; Record the analysis results, including sample identification, sampling time and analysis time, and record the operating parameters and instrument status during the analysis.

3. The converter high temperature, high carbon, low nitrogen production control method according to claim 1, characterized in that: The steps of S2 are: Set the target temperature and control the smelting temperature between 1600°C and 1700°C; Use infrared temperature measuring instruments outside the furnace to monitor the temperature inside the furnace in real time; According to the real-time monitoring of furnace temperature, adjust the fuel supply to control the furnace temperature; Adjust combustion conditions, including air supply, fuel distribution and control of combustion area; Maintain and adjust the reducing atmosphere in the furnace to reduce the oxide content in the slag; Continuously monitor furnace temperature changes and adjust fuel supply and combustion conditions based on real-time data; Record each furnace temperature measurement data and adjustment operation to form a data record of the smelting process.

4. The converter high temperature, high carbon, low nitrogen production control method according to claim 1, characterized in that: The steps of S3 are: Based on the data from the nitrogen analyzer, the nitrogen content in the slag has exceeded the set threshold; Prepare calcium silicate as a conditioning agent, calcium silicate is supplied in the form of powder and granules; According to the amount of slag and the degree of excess nitrogen content, calcium silicate is added to the slag and is placed on the surface of the slag through the furnace top hopper; After adding calcium silicate, nitrogen compounds are converted into non-volatile compounds, reducing the nitrogen content in the slag; The chemical composition of the slag changes after calcium silicate reacts with nitrogen compounds in the slag. The chemical composition and nitrogen content of the slag are continuously monitored; Record the operation time, quality and effect of adding calcium silicate.

5. The converter high temperature, high carbon, low nitrogen production control method according to claim 1, characterized in that: The steps of S4 are: Data collection and analysis: Collect and analyze key data from the current smelting process, including the chemical composition of the current slag and metal, and the current nitrogen content; Use historical and current data to develop a predictive model for nitrogen levels; The prediction model formula is: ; in, is the predicted value for the next time period, is the observed value of nitrogen content at the current time point, and α is the smoothing coefficient; The amount of scrap steel that needs to be added is calculated based on the predicted nitrogen content target that needs to be adjusted in the next time period, which is determined by calculating the difference between the total amount of nitrogen in the current slag and the target nitrogen content; Calculate the amount of scrap steel to be added and add the scrap steel.

6. The converter high temperature, high carbon, low nitrogen production control method according to claim 5, characterized in that: The calculation formula for the amount of scrap steel added is: ; Among them, N c is the total amount of nitrogen in the current slag, N t is the predicted target nitrogen content, S add is the amount of scrap steel to be added, S g is the nitrogen content of nitrogen-containing scrap steel; Scrap steel is added according to the calculated scrap steel amount.

7. The converter high temperature, high carbon, low nitrogen production control method according to claim 6, characterized in that: The operation steps of scrap steel delivery are: Prepare scrap steel: Prepare scrap steel according to the calculated scrap steel input quantity. The scrap steel is pre-sorted, cut and processed; Putting scrap steel: Put the prepared scrap steel into the furnace at the set time and method, and put it through the furnace top hopper; Monitor reaction: After adding scrap steel, monitor the reaction in the furnace and the changes in slag composition, pay attention to the changes in nitrogen content, and ensure that it meets the expected adjustment target; Adjustment and recording: Adjustment is made based on the actual amount of scrap steel put in and the changes in the monitored slag composition; Record the amount of scrap steel added, the reaction effect and the final slag composition changes for future production process optimization and quality control.

8. The converter high temperature, high carbon, low nitrogen production control method according to claim 1, characterized in that: The steps of S5 are: Install sensors and instruments in smelting equipment and systems to monitor parameters in real time; Sensors can collect and transmit data to monitoring systems; Establish a dedicated monitoring system and integrate it with the existing automation control system to display and record the changes of various parameters in real time; Set alarm thresholds for each parameter. When any parameter exceeds the preset safety and process range, the system will sound an alarm and prompt the operator. Operators can view the status and trends of key parameters in real time through the monitoring interface; Use historical data and trend analysis tools to identify periodic changes or anomalies in key parameters; Adjust based on monitoring results: Based on real-time monitoring data and preset process goals, operators take measures to adjust operating parameters.

9. The converter high temperature, high carbon, low nitrogen production control method according to claim 8, characterized in that: Parameter adjustment measures include: Temperature regulation: adjust fuel supply and cooling medium flow rate according to furnace temperature changes; Pressure management: Adjust gas and liquid pressure control devices to ensure pressure is maintained within safe and operational specifications; Gas composition control: Adjust the supply of oxygen and other gases to maintain the desired atmosphere and chemical reaction conditions.

10. The converter high temperature, high carbon, low nitrogen production control method according to claim 8, characterized in that: All monitoring data and changes in operating parameters shall be recorded and archived, and the effects of adjusting operating parameters shall be regularly evaluated to ensure that the stability of the smelting process, production efficiency and product quality meet the expected standards.