Spunlace non-woven fabric coating process

Through online monitoring and dynamic spraying, heating and stirring emulsion, fan-shaped cross-spraying and ultrasonic maturation, combined with the recycling device, the problems of poor uniformity and material waste in the coating process of spunlace nonwovens are solved, and production efficiency and environmental protection are improved .

CN119061704APending Publication Date: 2024-12-03YIXIANG HEALTH TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411489742.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-24
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

In the coating process, spunlace non-woven fabrics have problems such as poor uniformity, high material waste, high production costs, and environmental pollution, which are difficult to effectively solve in the existing technology.

Method used

The online monitoring device and dynamic spraying device are used for real-time detection and spraying. Combined with the heating and stirring of the emulsion, the fan-shaped cross-spraying process and ultrasonic maturation, a recycling device is set up to achieve uniform coating and emulsion recycling.

Benefits of technology

Improve coating quality, reduce material waste and production costs, shorten maturation time, and protect the environment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119061704A_ABST
    Figure CN119061704A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of spunlace non-woven fabric coating production, in particular to a spunlace non-woven fabric coating process. Comprising the following steps that S1, spunlace non-woven fabric spraying preparation is conducted, and emulsion in an emulsion tank is homogenized; s2, spraying the spunlace non-woven fabric by a spraying device; s3, the sprayed spunlace non-woven fabric is detected through an online monitoring device; s4, local supplementary spraying is conducted on the positions which are detected to be unqualified through a dynamic supplementary spraying device; s5, rechecking the spunlace non-woven fabric subjected to supplementary spraying; S6, curing a spunlace non-woven fabric coating semi-finished product subjected to rechecking; according to the spunlace non-woven fabric coating device, the uniformity in the spunlace non-woven fabric coating production process is monitored in real time, the missing part is compensated in time, the coating quality is improved, meanwhile, the problem that materials are wasted due to repeated coating is solved, and in addition, the problem of environmental pollution is also solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of spunlace nonwoven fabric coating production, in particular to a spunlace nonwoven fabric coating process. Background Art

[0002] Spunlace nonwoven fabric is a kind of nonwoven fabric, which is formed by spraying high-pressure fine water flow onto one or more layers of fiber webs, so that the fibers are entangled with each other, thereby strengthening the fiber web. It has the advantages of softness, strength, durability, etc., and is widely used in various fields. However, with the improvement of people's living standards, in addition to the requirements for the material of spunlace nonwoven fabrics, the requirements for various functions of spunlace nonwoven fabrics are also increasing; at present, some solutions with functional substances added are often coated on spunlace nonwoven fabrics through coating equipment to increase some of the functions of spunlace nonwoven fabrics. Spunlace nonwovens are generally coated by roller coating. Due to the uneven surface of spunlace nonwovens, the uniformity of the spunlace nonwovens coated by this coating method is poor. Repeated coating will not only waste materials (the proportion of wasted materials is as high as 35%) but also significantly increase production costs. On the other hand, the aging time of the semi-finished spunlace nonwovens is relatively long, which seriously affects production efficiency. In addition, in the prior art, spunlace nonwovens often have problems of excessive spraying, splashing, and incomplete adhesion to the surface of the substrate during the coating process, resulting in a large amount of emulsion waste. At the same time, the direct discharge of the waste emulsion without treatment will pollute the environment. Summary of the invention

[0003] In order to solve the above technical problems, the present invention provides a spunlace non-woven fabric coating process, which realizes real-time monitoring of the uniformity of the spunlace non-woven fabric coating production process and timely compensates for the missing parts, which not only improves the coating quality, but also solves the problem of repeated coating and waste of materials, and also solves the problem of environmental pollution.

[0004] To achieve the above object, the present invention proposes the following technical solution: a spunlace nonwoven fabric coating process, characterized in that it comprises the following steps: S1: Preparation for spraying spunlace nonwoven fabrics, homogenizing the emulsion in the emulsion tank; S2: The spraying device sprays the spunlace nonwoven fabric; S3: Testing the spunlace nonwoven fabric after spraying through an online monitoring device; S4: Use the dynamic re-spraying device to perform local re-spraying on the locations that failed the test S5: Re-inspect the spunlace nonwoven fabric after re-spraying: S6: Curing the re-inspected spunlace nonwoven coated semi-finished product.

[0005] Furthermore, homogenizing the emulsion in step S1 includes heating and stirring the emulsion in the emulsion tank to maintain the uniformity of the emulsion.

[0006] Furthermore: in step S2, the spunlace nonwoven fabric is sprayed using a fan-shaped cross-spraying process.

[0007] Further: the online monitoring device in step S3 includes a monitoring light emitting device and a monitoring light receiving device. The detection value is Umeasure. A standard value Ustandard is set in the online monitoring device. When Umeasure ≤Ustandard, the monitoring result is sent to the supplementary spraying device in step S4. The dynamic supplementary spraying device performs appropriate supplementary spraying on the missing position according to the difference between Umeasure and Ustandard.

[0008] Further: the monitoring light emitting device and the monitoring light receiving device are respectively located on both sides of the spunlace non-woven fabric, and the monitoring light emitting device corresponds to the spunlace non-woven fabric on the side with the cream attached, so as to detect its uniformity.

[0009] Furthermore: in step S5, the online monitoring device in S3 is used to re-inspect the spunlace nonwoven fabric after the re-spraying.

[0010] Further: U mark is 10-300g / m².

[0011] Furthermore: in step S6, the re-inspected spunlace nonwoven fabric is aged by ultrasonic high-frequency vibration.

[0012] Furthermore: during the spraying process in step S2, a recovery device is provided below the spunlace nonwoven fabric to recover excess emulsion.

[0013] Furthermore: the recovery device includes a pair of stainless steel baffles, a filter plate and a recovery tank, and the stainless steel baffles are fixedly connected to the top of the recovery tank; the stainless steel baffles are located on both sides of the spunlace non-woven fabric, and the dripping emulsion passes through the stainless steel baffles and the filter plate and is collected in the recovery tank, and the recovery tank is connected to the emulsion tank.

[0014] Compared with the prior art, the gain effect of the present invention is: 1. Heating and stirring the emulsion in the emulsion tank can make the temperature and viscosity of the added emulsion more uniform, so that the emulsion can be coated on the surface of the spunlace non-woven fabric more evenly.

[0015] 2. The fan-shaped cross-spraying process adopted by the spraying device replaces the existing roller coating process. The spraying peaks and valleys are staggered, which can make the spraying more uniform and reduce the number of spraying times.

[0016] 3. The cooperation between the online monitoring device and the dynamic compensation device realizes the effective monitoring and compensation of coating uniformity. The dynamic compensation device can perform appropriate replenishment spraying in a range according to the specific difference between U measurement and U mark, thus avoiding the occurrence of production losses, effectively reducing production costs, and saving energy and being efficient.

[0017] 4. Ultrasonic high-frequency vibration can accelerate the movement of glycerol molecules in the emulsion, promote the maturation of spunlace non-woven fabric coating semi-finished products, and reduce the maturation time.

[0018] 5. The setting of the recovery device effectively realizes the recovery of excess coating emulsion, which not only solves the problem of emulsion waste, but also protects the environment. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is the process diagram of the present invention.

[0020] In the figure: 1. Spraying device, 2. Monitoring light emitting device, 3. Monitoring light receiving device, 4. Dynamic supplementary spraying device. DETAILED DESCRIPTION

[0021] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0022] The specific implementation of the present invention is described in detail below in conjunction with the accompanying drawings. It should be understood that the specific implementation described here is only used to illustrate and explain the present invention, and is not used to limit the present invention. Example 1

[0023] like Figure 1 As shown: A spunlace nonwoven coating process, comprising the following steps: S1: Preparation for spraying spunlace nonwoven fabrics, homogenizing the emulsion in the emulsion tank; Homogenizing the emulsion includes heating and stirring the emulsion in the emulsion tank to maintain the uniformity of the emulsion. S2: The spraying device 1 sprays the spunlace nonwoven fabric; The spraying adopts fan-shaped cross-spraying process; the spraying peaks and valleys are staggered, and the coating amount can reach 25-45%, which can make the spraying more uniform (emulsion viscosity is 26 mPa·s) and reduce the number of spraying times; Coating amount = emulsion / (emulsion+spunlace base fabric)*100%.

[0024] S3: Testing the spunlace nonwoven fabric after spraying through an online monitoring device; S4: local re-spraying of the unqualified positions by the dynamic re-spraying device 4; In step S3, the online monitoring device includes a monitoring light emitting device 2 and a monitoring light receiving device 3. The surface density detection value is U measurement. A standard value U mark is set in the online monitoring device, and U mark is 10g / m². When U measurement ≤ U mark, the monitoring result is sent to the dynamic supplementary spraying device 4 in step S4. The dynamic supplementary spraying device 4 performs appropriate supplementary spraying on the missing position according to the difference between U measurement and U mark. The monitoring light emitting device 2 and the monitoring light receiving device 3 are respectively located on both sides of the spunlace nonwoven fabric, and the monitoring light emitting device 2 corresponds to the spunlace nonwoven fabric on the side where the emulsion is attached, so as to detect its uniformity.

[0025] S5: Re-inspect the spunlace nonwoven fabric after re-spraying: The re-inspection uses the online monitoring device in S3 to re-inspect the spunlace non-woven fabric after re-spraying.

[0026] S6: Curing the re-inspected spunlace nonwoven coated semi-finished product.

[0027] The aging process uses ultrasonic high-frequency vibration to accelerate the movement of glycerol molecules in the emulsion, promote the aging of the spunlace non-woven fabric coating semi-finished products, and reduce the aging time.

[0028] During the spraying process in step S2, a recovery device is arranged under the spunlace non-woven fabric to recover excess emulsion; the recovery device includes a pair of stainless steel baffles, a filter plate and a recovery tank, and the stainless steel baffles are fixedly connected to the top of the recovery tank; the stainless steel baffles are located on both sides of the spunlace non-woven fabric, and the dripping emulsion passes through the stainless steel baffles and the filter plate and is collected in the recovery tank, and the recovery tank is connected to the emulsion tank. Example 2

[0029] like Figure 1 As shown: A spunlace nonwoven coating process, comprising the following steps: S1: Preparation for spraying spunlace nonwoven fabrics, homogenizing the emulsion in the emulsion tank; Homogenizing the emulsion includes heating and stirring the emulsion in the emulsion tank to maintain the uniformity of the emulsion. S2: The spraying device 1 sprays the spunlace nonwoven fabric; The spraying adopts fan-shaped cross-spraying process; the spraying peaks and valleys are staggered, and the coating amount can reach 25-45%, which can make the spraying more uniform (emulsion viscosity is 26 mPa·s) and reduce the number of spraying times; Coating amount = emulsion / (emulsion+spunlace base fabric)*100%.

[0030] S3: Testing the spunlace nonwoven fabric after spraying through an online monitoring device; S4: local re-spraying of the unqualified positions by the dynamic re-spraying device 4; In step S3, the online monitoring device includes a monitoring light emitting device 2 and a monitoring light receiving device 3. The surface density detection value is U measurement. A standard value U mark is set in the online monitoring device, and U mark is 300g / m². When U measurement ≤ U mark, the monitoring result is sent to the dynamic supplementary spraying device 4 in step S4. The dynamic supplementary spraying device 4 performs a range of appropriate supplementary spraying on the missing position according to the difference between U measurement and U mark. The monitoring light emitting device 2 and the monitoring light receiving device 3 are respectively located on both sides of the spunlace nonwoven fabric, and the monitoring light emitting device 2 corresponds to the spunlace nonwoven fabric on the side where the emulsion is attached, so as to detect its uniformity.

[0031] S5: Re-inspect the spunlace nonwoven fabric after re-spraying: The re-inspection uses the online monitoring device in S3 to re-inspect the spunlace non-woven fabric after re-spraying.

[0032] S6: Curing the re-inspected spunlace nonwoven coated semi-finished product.

[0033] The aging process uses ultrasonic high-frequency vibration to accelerate the movement of glycerol molecules in the emulsion, promote the aging of the spunlace non-woven fabric coating semi-finished products, and reduce the aging time.

[0034] During the spraying process in step S2, a recovery device is arranged under the spunlace non-woven fabric to recover excess emulsion; the recovery device includes a pair of stainless steel baffles, a filter plate and a recovery tank, and the stainless steel baffles are fixedly connected to the top of the recovery tank; the stainless steel baffles are located on both sides of the spunlace non-woven fabric, and the dripping emulsion passes through the stainless steel baffles and the filter plate and is collected in the recovery tank, and the recovery tank is connected to the emulsion tank.

[0035] During the working process of this scheme: the emulsion in the emulsion tank is stirred and heated to make the emulsion heated evenly, thereby reducing the viscosity of the emulsion and facilitating transportation and spraying; the emulsion is coated on the spunlace non-woven fabric through the spraying device 1, and the fan-shaped cross-spraying process replaces the existing roller coating process. The spraying peaks and valleys are staggered, and the coating amount can reach 25-45%, which can make the spraying more uniform and reduce the number of spraying times; the coating effect of the coated spunlace non-woven fabric is monitored by an online monitoring device.

[0036] During the operation of the online monitoring device, the monitoring light emitting device 2 emits light, and the light is received by the monitoring light receiving device 3 after passing through the coated spunlace non-woven fabric, and Umeasure is obtained after data analysis. A standard value Umark is set in the online monitoring device; when Umeasure ≤Umark, the online monitoring device feeds back the monitoring result to the dynamic supplementary spraying device 4; when the spunlace non-woven fabric at this position moves to the dynamic supplementary spraying position, the dynamic supplementary spraying device 4 performs local spraying on the coating missing part, and the dynamic compensation device can perform a range of appropriate supplementary spraying according to the specific difference between Umeasure and Umark; thus avoiding the occurrence of production losses, effectively reducing production costs, and saving energy and being efficient.

[0037] Subsequently, the re-inspection device re-inspects the spunlace non-woven fabric to obtain the spunlace non-woven fabric coated semi-finished product; the high-frequency vibration device accelerates the movement speed of glycerol molecules in the emulsion by means of ultrasonic high-frequency vibration, accelerates the maturation of the spunlace non-woven fabric coated semi-finished product, and reduces the maturation time; it realizes real-time monitoring of the uniformity of the spunlace non-woven fabric coating production process and timely compensates for the missing parts, which not only improves the coating quality, but also solves the problem of repeated coating and waste of materials.

[0038] The recovery device recovers excess emulsion. The stainless steel baffles on both sides of the spunlace non-woven fabric are used to receive the emulsion splashed onto the baffles. The recovered emulsion is collected into the recovery tank through the filter plate and finally flows into the emulsion tank to be reused; it not only solves the problem of emulsion waste, but also protects the environment.

[0039] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.

[0040] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

Claims

1. A spunlace nonwoven fabric coating process, characterized in that: The following steps are involved: S1: Preparation for spraying spunlace nonwovens, homogenizing the emulsion in the emulsion tank; S2: The spraying device (1) sprays the spunlace nonwoven fabric; S3: Testing the sprayed spunlace nonwoven fabric through an online monitoring device; S4: local re-spraying of the locations that failed the test by means of the dynamic re-spraying device (4); S5: Re-inspect the spunlace nonwoven fabric after re-spraying: S6: Curing the re-inspected spunlace nonwoven coated semi-finished product.

2. The spunlace nonwoven fabric coating process according to claim 1, characterized in that: Homogenizing the emulsion in step S1 includes heating and stirring the emulsion in the emulsion tank to maintain the uniformity of the emulsion.

3. The spunlace nonwoven fabric coating process according to claim 1, characterized in that: In step S2, the spunlace nonwoven fabric is sprayed using a fan-shaped cross-spraying process.

4. The spunlace nonwoven fabric coating process according to claim 1, characterized in that: The online monitoring device in step S3 includes a monitoring light emitting device (2) and a monitoring light receiving device (3). The surface density detection value is Umeasure. A standard value Umark is set in the online monitoring device. When Umeasure ≤ Umark, the monitoring result is sent to the dynamic supplementary spraying device (4) in step S4. The dynamic supplementary spraying device (4) performs appropriate supplementary spraying on the missing position according to the difference between Umeasure and Umark.

5. The spunlace nonwoven fabric coating process according to claim 1, characterized in that: The monitoring light emitting device (2) and the monitoring light receiving device (3) are respectively located on both sides of the spunlace non-woven fabric, and the monitoring light emitting device (2) corresponds to the spunlace non-woven fabric on the side where the emulsion is attached, so as to detect its uniformity.

6. The spunlace nonwoven fabric coating process according to claim 1, characterized in that: In step S5, the online monitoring device in S3 is used to re-inspect the spunlace non-woven fabric after the re-spraying.

7. The spunlace nonwoven fabric coating process according to claim 1, characterized in that: U mark is 10-300g / m².

8. The spunlace nonwoven fabric coating process according to claim 1, characterized in that: In step S6, the re-inspected spunlace nonwoven fabric is aged by ultrasonic high-frequency vibration.

9. The spunlace nonwoven fabric coating process according to claim 1, characterized in that: During the spraying process in step S2, a recovery device is provided below the spunlace non-woven fabric to recover excess emulsion.

10. The spunlace nonwoven fabric coating process according to claim 1, characterized in that: The recovery device includes a pair of stainless steel baffles, a filter plate and a recovery tank. The stainless steel baffles are fixedly connected to the top of the recovery tank; the stainless steel baffles are located on both sides of the spunlace non-woven fabric. The dripping emulsion passes through the stainless steel baffles and filter plates and is collected in the recovery tank. The recovery tank is connected to the emulsion tank.