Online maintenance treatment process for cold leakage of LNG (Liquefied Natural Gas) low-temperature pipeline
By detecting and repairing the cold leakage problem of LNG low-temperature pipelines online, and using detection instruments and protective materials to repair the pipelines, the problems of inaccurate cold leakage detection and damage to the insulation layer in the existing technology have been solved, and energy consumption is reduced, equipment life is extended and equipment life is reduced. The effect of safety accidents.
Patent Information
- Application Number
- CN202411482964.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-23
- Publication Date
- 2024-12-03
AI Technical Summary
The existing LNG low-temperature pipe cold leakage maintenance and treatment process is not accurate and efficient in early detection and positioning, which makes it difficult to detect and deal with cold leakage problems in time, increasing the probability of safety accidents, and not timely repairing the insulation layer after it is damaged will aggravate the condensation water. Accumulate and pipe corrosion, shorten the service life of the equipment.
A LNG low-temperature pipe cold leakage online maintenance and treatment process, including removing external guard plates, checking the status of the pipeline, using infrared thermometers, hygrometers, ultrasonic thickness gauge and other detection instruments to determine the status of the pipeline, and selecting the corresponding maintenance and treatment method according to the status , including removing the icy part, repairing the cold-proof layer, installing protective materials, applying isolation paint and vacuum silicon to repair the pipe.
By timely repairing the problem of cold leakage in pipelines, reducing cooling consumption losses, optimizing the insulation structure significantly reduces the energy consumption of the cooling system, reducing condensate erosion on the equipment, extending the service life of the equipment, reducing maintenance costs and failure rates, improving conveying efficiency, and reducing safety accidents and environmental pollution.
Smart Images

Figure CN119062860A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of cryogenic pipeline maintenance, and in particular relates to an online maintenance and treatment process for cold leakage of an LNG cryogenic pipeline. Background Art
[0002] In the field of cryogenic transportation of LNG (liquefied natural gas), the operational safety and efficiency of LNG cryogenic pipelines, as key infrastructure, are directly related to the stability and economy of the entire energy supply chain. However, the existing LNG cryogenic pipeline leakage repair and treatment processes still have some significant deficiencies in practical applications, which not only affect the overall performance of the pipeline system, but also increase operational risks and maintenance costs.
[0003] First, the existing technology is not accurate and efficient enough in the early detection and location of cooling leakage problems. It often relies on manual inspections and indirect parameter judgment, which makes it difficult to find and deal with cooling leakage problems in a timely manner, increasing the probability of safety accidents. The temperature of LNG fluctuates greatly during transportation, which not only reduces transportation efficiency, but also increases energy consumption and operating costs. At the same time, if the insulation layer is damaged but not repaired in time, it will aggravate the accumulation of condensate and pipeline corrosion, shortening the service life of the equipment.
[0004] In view of this, the inventors proposed an online repair and treatment process for LNG cryogenic pipeline leakage to solve the above problems. Summary of the invention
[0005] The purpose of the present invention is to provide an online repair and treatment process for LNG cryogenic pipeline leakage to solve the problems raised in the above background technology.
[0006] To achieve the above object, the present invention provides the following technical solutions:
[0007] An online repair and treatment process for LNG cryogenic pipeline leakage includes the following steps:
[0008] S1. Remove the outer protective plate, remove the external protective layer, and expose the failed pipe insulation layer;
[0009] S2. Check the status of the pipeline. First, conduct a visual inspection to see if there are visible problems such as ice, condensation water dripping, and insulation material damage on the surface of the existing cold insulation layer of the pipeline. If it is not directly observed, use a detection instrument to obtain the status data of the existing cold insulation layer of the pipeline to determine the current status of the pipeline and whether there are hidden dangers of ice, condensation water, or cold insulation failure;
[0010] S3. Select a corresponding maintenance method according to the current state of the pipeline in step S2.
[0011] Preferably, the detection instrument in step S2 includes an infrared thermometer or temperature sensor, a hygrometer, an ultrasonic thickness gauge, a pressure gauge and an infrared thermal imager.
[0012] Preferably, the maintenance treatment method in step S3 includes processing the frozen part caused by failure of the cold insulation material due to reaching the service life, the cold loss caused by pipeline condensation and condensation due to damage to the LNG cold insulation process or material consumption reduction, and processing the LNG pipeline part with double or multiple layers of pipeline cold insulation.
[0013] Preferably, the steps of treating the leaking ice part are:
[0014] The steps of treating the leakage and icing part are as follows:
[0015] S21. Remove all internal cold-insulation tube shells inside the frozen area;
[0016] S22. The construction plan for completely removing the first insulation layer of the insulation layer pipe includes the following five methods S231~S235:
[0017] S221. Install fixed foam external support, calculate the amount of black and white materials used, and pour foam for the first layer of failed pipes. The minimum thickness of the foam is 50mm and the maximum thickness is 80mm. The thickness is adjusted according to the pipe diameter and the original design documents;
[0018] S222. Use low-temperature cotton or aerogel for the first two-layer installation protection. The minimum thickness of low-temperature cotton or aerogel is 20mm and the maximum thickness is 50mm. The thickness is adjusted according to the pipe diameter and the original design documents.
[0019] S223, PIR or foam glass is used for wrapping. The minimum thickness of PIR or foam glass is 50mm and the maximum thickness is 100mm. The thickness is adjusted according to the pipe diameter and the original design documents.
[0020] S224, using composite porous vacuum silicon for wrapping, the minimum thickness of vacuum silicon is 2mm, the maximum thickness is 10mm, and the thickness is adjusted according to the pipe diameter and the original design documents;
[0021] S225; It is wrapped with composite low-temperature nitrile rubber products. The minimum thickness of the nitrile rubber products is 25mm and the maximum thickness is 70mm. The thickness is adjusted according to the pipe diameter and the original design documents.
[0022] S23. Clean the pipeline surface. Use nitrogen to purge or alcohol to brush the exposed low-temperature pipeline surface to prevent ice from forming on the pipeline surface. Use air blocking to isolate the pipeline in sections at the pipe support.
[0023] S24: Apply a moisture-proof layer or bond aluminum foil to the surface of the first cold-insulation pipe, and isolate the first and second cold-insulation materials from air and condensate, which includes the following three solutions: S241 to S243:
[0024] S241, apply a layer of isolation coating, the coating layer is a polyurethane waterproof coating layer, the minimum thickness of the coating layer is 50 microns, and the maximum thickness is 80 microns;
[0025] S242, install a layer of composite porous vacuum silicon, the minimum thickness of the composite porous vacuum silicon is 2 mm, and the maximum thickness is 10 mm;
[0026] Apply a layer of isolation paint, the minimum thickness of the isolation paint layer is 50 microns and the maximum thickness is 80 microns;
[0027] S243, install a layer of thick composite vacuum silicon, the minimum thickness of the composite vacuum silicon is 2mm, the maximum thickness is 10mm;
[0028] Apply a layer of isolation coating, which is polyurethane waterproof coating. The minimum thickness of the isolation coating is 50 microns and the maximum thickness is 80 microns;
[0029] S25. Install the exterior guard plate and conduct acceptance inspection.
[0030] Preferably, the steps for processing the pipeline portion of condensed water caused by the failure of LNG refrigeration are:
[0031] S31, apply a layer of isolation coating, the minimum thickness of the coating layer is 50 microns and the maximum thickness is 80 microns;
[0032] S32, install a layer of composite porous vacuum silicon, the minimum thickness of the composite porous vacuum silicon is 2 mm, and the maximum thickness is 10 mm;
[0033] S33, applying a layer of isolation coating, the minimum thickness of the isolation coating layer is 50 microns and the maximum thickness is 80 microns;
[0034] S34, install a layer of 2mm thick composite vacuum silicon, the minimum thickness of the composite vacuum silicon is 2mm, and the maximum thickness is 10mm;
[0035] S35, apply a layer of isolation coating, the minimum thickness of the isolation coating is 50 microns and the maximum thickness is 80 microns;
[0036] S36. Install the outer guard plate and carry out acceptance inspection.
[0037] Preferably, the double-layer or multi-layer LNG pipeline portion processing steps are:
[0038] S41. Remove the outermost layer of PIR insulation material that has failed;
[0039] S42, apply a layer of isolation coating, the minimum thickness of the coating layer is 50 microns and the maximum thickness is 80 microns;
[0040] S43, install a layer of composite porous vacuum silicon, the minimum thickness of the composite porous vacuum silicon is 2 mm, and the maximum thickness is 10 mm;
[0041] S44, apply a layer of isolation coating, the minimum thickness of the isolation coating layer is 50 microns and the maximum thickness is 80 microns;
[0042] S45, apply a layer of isolation coating, the minimum thickness of the isolation coating is 50 microns and the maximum thickness is 80 microns;
[0043] S46, install a layer of 2mm thick composite vacuum silicon, the minimum thickness of the composite vacuum silicon is 2mm, and the maximum thickness is 10mm;
[0044] S46. Install the exterior panel and conduct acceptance inspection.
[0045] Preferably, the detection instrument includes an infrared thermometer or temperature sensor, a hygrometer, a pressure gauge and an ultrasonic thickness gauge, wherein the measured temperature T using the infrared thermometer needs to be compared with the set safe temperature range Tsafe. If the measured temperature exceeds the set value, the integrity of the insulation layer needs to be further analyzed, and the expression is:
[0046] T<Tsafe。
[0047] Preferably, the hygrometer is used to measure the relative humidity RH of the air near the pipeline, and the expression is:
[0048]
[0049] Where Td is the dew point temperature;
[0050] T is the temperature measured by the infrared thermometer;
[0051] If the dew point temperature Td is close to the pipe surface temperature T, there is a risk of condensation.
[0052] Preferably, the pressure gauge is used for pipeline pressure testing to ensure that the pipeline has no leakage, and the calculation expression is:
[0053] P=F / A
[0054] Where F is the force acting on the pipe, and A is the cross-sectional area of the pipe;
[0055] If the test pressure is lower than the design standard, it indicates leakage or damage.
[0056] Preferably, the ultrasonic thickness gauge detects the pipe wall thickness, identifies corrosion or wear conditions, and calculates the wall thickness d by the speed of sound and the echo time, expressed as:
[0057]
[0058] Where v is the propagation speed of the sound wave in the material, and t is the echo time.
[0059] Compared with the prior art, the present invention has the following beneficial effects:
[0060] (1) The present invention can effectively reduce the cooling loss caused by the failure of pipeline cooling insulation by timely repairing the pipeline cooling leakage problem.
[0061] (2) The optimized insulation structure in the present invention can significantly reduce the energy consumption of the cooling system, thereby saving operating costs; through effective insulation and isolation measures, the erosion of pipes and equipment by condensed water is reduced, thereby extending the service life of the equipment; regular repairs and maintenance can reduce the failure rate of equipment and reduce maintenance costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0062] Figure 1 This is a process flow chart of online repair and treatment of LNG cryogenic pipeline leakage according to the present invention;
[0063] Figure 2 It is a block diagram of the detection instrument of the present invention;
[0064] Figure 3 It is a block diagram of the maintenance processing method of the present invention;
[0065] Figure 4 This is a flow chart of the process of cooling leakage and icing of the present invention;
[0066] Figure 5 This is a flow chart of the pipeline portion processing of condensed water caused by LNG refrigeration failure of the present invention;
[0067] Figure 6 This is a partial processing flow chart of a double-layer or multi-layer LNG pipeline according to the present invention. DETAILED DESCRIPTION
[0068] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0069] Embodiment 1:
[0070] See also Figures 1 to 6As shown, during the maintenance of the connecting pipeline of a certain LNG storage tank, icing was found, and it was suspected that the thermal insulation had failed. The outer protection board was removed, the external protective layer was removed, and the cold insulation layer of the failed pipeline was exposed. The specific inspection of the pipeline status is as follows:
[0071] Visual inspection
[0072] Result:疑似结冰现象 was found at the connection.
[0073] Temperature measurement
[0074] Equipment: Infrared thermometer.
[0075] Measured data: The surface temperature of the pipeline T = -160°C
[0076] Ambient temperature Tenv = 25°C
[0077] Safe temperature range: Set as Tsafe = -130°C;
[0078] Judgment: Since T < Tsafe, there is a risk of cold leakage;
[0079] Humidity measurement
[0080] Equipment: Digital hygrometer.
[0081] Measured data: Relative humidity RH = 90%
[0082] Calculate the dew point temperature:
[0083] Judgment: The dew point temperature is higher than the surface temperature of the pipeline, there is a risk of condensation;
[0084] Pressure test
[0085] Equipment: Pressure gauge.
[0086] Test data: Test pressure P = 0.6 MPa
[0087] Design standard pressure Pdesign = 0.8 MPa
[0088] Judgment: The test pressure is lower than the design standard, indicating a leak;
[0089] Ultrasonic testing
[0090] Equipment: Ultrasonic thickness gauge.
[0091] Measured data: The wall thickness of the pipeline d = 3.5 mm (the normal thickness should be 5.5 mm)
[0092] Judgment: The wall thickness is lower than the normal value.
[0093] Infrared thermal imaging: It should be noted that the text "疑似结冰现象" in the original Chinese is an incomplete or inaccurate expression. It is translated as "疑似结冰现象" here for the purpose of literal translation, but it may need to be adjusted according to the actual situation to make the expression more accurate and clear.
[0094] Use an infrared thermal imager to detect the temperature distribution of the pipeline and identify abnormal cold spots.
[0095] Analyze the temperature difference based on the thermal map to determine whether the insulation layer has failed.
[0096] Specifically, the steps for handling the leakage and icing are as follows:
[0097] Remove all internal cold-insulation tubes and shells inside the iced area;
[0098] The construction method of the first insulation layer of the completely removed insulation layer pipe includes but is not limited to:
[0099] Install fixed foam external support, calculate the amount of black and white materials used, and pour foam for the first layer of failed pipes. The minimum thickness of the foam is 50mm and the maximum thickness is 80mm. The thickness is adjusted according to the pipe diameter and the original design documents;
[0100] Alternatively, use low-temperature cotton or aerogel for the first two-layer installation protection. The minimum thickness of low-temperature cotton or aerogel is 20mm and the maximum thickness is 50mm. The thickness can be adjusted according to the pipe diameter and the original design documents.
[0101] Or use PIR or foam glass for wrapping. The minimum thickness of PIR or foam glass is 50mm and the maximum thickness is 100mm. The thickness can be adjusted according to the pipe diameter and the original design documents.
[0102] Alternatively, composite porous vacuum silicon is used for wrapping. The minimum thickness of vacuum silicon is 2 mm and the maximum thickness is 10 mm. The thickness can be adjusted according to the pipe diameter and the original design documents.
[0103] Alternatively, composite low-temperature nitrile rubber products can be used for wrapping. The minimum thickness of nitrile rubber products is 25mm and the maximum thickness is 70mm. The thickness can be adjusted according to the pipe diameter and the original design documents.
[0104] Clean the pipeline surface, purge the exposed low-temperature pipeline surface with nitrogen or apply alcohol to prevent the pipeline surface from freezing, and use air blocking to isolate the pipeline in sections at the pipe support;
[0105] Apply a moisture-proof layer or bond aluminum foil to the surface of the first cold insulation pipe to isolate the first layer of cold insulation material from the second layer of cold insulation material to prevent air and condensation, including the following steps:
[0106] Apply a layer of polyurethane waterproof coating with a thickness of 50 microns;
[0107] Install a layer of composite porous vacuum silicon, the thickness of the composite porous vacuum silicon is 2 mm;
[0108] Apply a layer of polyurethane waterproof coating with a thickness of 50 microns.
[0109] Install a 2-mm-thick composite vacuum silicon layer with a thickness of 2 mm.
[0110] Apply a layer of polyurethane waterproof coating with a thickness of 50 microns.
[0111] Install the outer protection board and conduct acceptance inspection upon completion.
[0112] Example 2:
[0113] Reference Figures 1 to 6 As shown, for the cold loss caused by the breakage of the LNG cold insulation process or the reduction of material consumption, resulting in condensate water and dew condensation in the pipeline:
[0114] Remove the outer protection board, remove the external protection layer, and expose the failed pipeline cold insulation layer.
[0115] During the regular inspection of a certain LNG transportation pipeline, condensate water was found on the outside, suspecting cold leakage.
[0116] 1. Check the pipeline status:
[0117] Visual inspection:
[0118] Result: Obvious condensate water droplets were found dripping on the pipeline surface.
[0119] Temperature measurement:
[0120] Equipment: Infrared thermometer.
[0121] Measured data:
[0122] The pipeline surface temperature T = -150 °C
[0123] The ambient temperature Tenv = 20 °C
[0124] Safe temperature range: Set as Tsafe = -120 °C
[0125] Judgment: Since T < Tsafe, there is a risk of cold leakage.
[0126] Humidity measurement:
[0127] Equipment: Digital hygrometer.
[0128] Measured data:
[0129] The relative humidity RH = 85%
[0130] Calculate the dew point temperature: Td = 20 - (100 - 85) / 5 = 17 °C. Judgment: The dew point temperature is higher than the pipeline surface temperature, there is a risk of condensation.
[0131] Stress Test:
[0132] Equipment: Pressure gauge.
[0133] Test data:
[0134] Test pressure P = 0.5 MPa
[0135] Design standard pressure Pdes i gn=0.7MPa
[0136] Judgment: The test pressure is lower than the design standard, indicating that there is a leak.
[0137] Ultrasonic testing:
[0138] Equipment: Ultrasonic thickness gauge.
[0139] Measured data:
[0140] Pipe wall thickness d = 4.0 mm (normal thickness should be 5.0 mm)
[0141] Judgment: The wall thickness is lower than normal and corrosion exists.
[0142] 2. Repair and treatment process:
[0143] Remove the outermost layer of expired PI R insulation material;
[0144] Apply a layer of polyurethane waterproof coating with a thickness of 50 microns;
[0145] Install a layer of composite porous vacuum silicon with a thickness of 2 mm; apply a layer of polyurethane waterproof coating with a thickness of 50 microns; apply a layer of polyurethane waterproof coating with a thickness of 50 microns;
[0146] Install a layer of 2mm thick composite vacuum silicon, the thickness of the composite vacuum silicon is 2mm;
[0147] Install the exterior panel and submit the project for acceptance.
[0148] Embodiment three:
[0149] This design is specifically used for emergency repairs during the production process. In a liquefaction plant, if a leak or cold leakage occurs in an LNG cryogenic pipeline, it is necessary to quickly initiate an emergency repair procedure, using injection-type sealing repair technology or other rapid plugging methods to ensure production safety. Through regular maintenance and inspection, the insulation layer and seals of the pipeline system are replaced or reinforced to prevent cold leakage.
[0150] For further reference, Figures 1 to 6 As shown, the LNG pipeline with double or multi-layer cold insulation is partially processed:
[0151] The LNG transmission pipeline has a double-layer structure. During regular maintenance inspections, it was found that the outer layer of thermal insulation material had failed, resulting in cold leakage, which caused ice formation and condensate on the pipeline surface.
[0152] 1. Check the pipeline status:
[0153] Visual inspection:
[0154] Result: Cracks were found in the outer layer of thermal insulation material, and obvious ice formation was observed on the surface.
[0155] Temperature measurement:
[0156] Equipment: Infrared thermometer.
[0157] Measured data:
[0158] The temperature of the outer surface of the pipeline T = -155°C
[0159] Ambient temperature Tenv = 18°C
[0160] Safe temperature range: Set as Tsafe = -120°C
[0161] Judgment: Since T < Tsafe, there is a risk of cold leakage.
[0162] Humidity measurement:
[0163] Equipment: Digital hygrometer.
[0164] Measured data:
[0165] Relative humidity RH = 80%
[0166] Calculate the dew point temperature: Td = 18 - (100 - 80) / 5 = 14°C
[0167] Judgment: The dew point temperature is higher than the temperature of the outer layer of the pipeline, so there is a risk of condensation.
[0168] Pressure test:
[0169] Equipment: Pressure gauge.
[0170] Test data:
[0171] Test pressure P = 0.5 MPa
[0172] Design standard pressure Pdesign = 0.7 MPa
[0173] Judgment: The test pressure is lower than the design standard, indicating a leak.
[0174] Ultrasonic testing:
[0175] Equipment: Ultrasonic thickness gauge.
[0176] Measured data:
[0177] Inner pipe wall thickness di nner = 4.0 mm (normal thickness should be 5.0 mm)
[0178] Outer pipe wall thickness douter = 3.5mm (normal thickness should be 4.5mm)
[0179] Judgment: The wall thickness of the inner and outer layers is lower than normal, and corrosion exists.
[0180] 2. Repair and treatment process:
[0181] Apply a layer of polyurethane waterproof coating with a thickness of 50 microns;
[0182] Install a layer of composite porous vacuum silicon, the thickness of the composite porous vacuum silicon is 2 mm;
[0183] Apply a layer of polyurethane waterproof coating with a thickness of 50 microns;
[0184] Install a layer of 2mm thick composite vacuum silicon, the thickness of the composite vacuum silicon is 2mm;
[0185] Apply a layer of polyurethane waterproof coating with a thickness of 50 microns;
[0186] Install the exterior panel and submit the project for acceptance.
[0187] From the above, it can be seen that by promptly repairing the cold leakage problem, the risk of safety accidents such as freezing, explosion or fire caused by pipeline failure can be effectively reduced, and the safety of personnel and equipment can be guaranteed. The isolation coating and thermal insulation materials during the maintenance process can effectively prevent the formation of condensed water and reduce the risk of slipping and corrosion. Good thermal insulation performance can ensure the low temperature state of LNG during transportation, improve transportation efficiency and reduce energy loss.
[0188] The optimized insulation structure can significantly reduce the energy consumption of the cooling system, thereby saving operating costs; through effective insulation and isolation measures, the erosion of pipes and equipment by condensed water can be reduced, thereby extending the service life of the equipment; regular repairs and maintenance can reduce the failure rate of equipment and reduce maintenance costs;
[0189] Effective cold leak repair can reduce gas leakage during LNG transportation, thereby reducing pollution to the environment. It can promote environmentally friendly operation modes by reducing energy consumption and resource waste. Through timely repair and maintenance, it can reduce emergency repair costs caused by equipment failure. A well-maintained pipeline system can improve production efficiency, thereby increasing the economic benefits of the enterprise.
[0190] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. An online repair process for LNG cryogenic pipeline leakage, characterized in that: The following steps are involved: S1. Remove the outer protective plate, remove the external protective layer, and expose the failed pipe insulation layer; S2. Check the status of the pipeline. First, conduct a visual inspection to see if there are visible problems such as ice, condensation water dripping, and insulation material damage on the surface of the existing cold insulation layer of the pipeline. If it is not directly observed, use a detection instrument to obtain the status data of the existing cold insulation layer of the pipeline to determine the current status of the pipeline and whether there are hidden dangers of ice, condensation water, or cold insulation failure; S3. Select a corresponding maintenance method according to the current state of the pipeline in step S2.
2. The online repair process for LNG cryogenic pipeline leakage according to claim 1 is characterized by: The detection instruments in step S2 include an infrared thermometer or temperature sensor, a hygrometer, an ultrasonic thickness gauge, a pressure gauge and an infrared thermal imager.
3. The online repair process for LNG cryogenic pipeline leakage according to claim 1 is characterized by: The maintenance treatment method in step S3 includes the treatment of the frozen part caused by the failure of the cold insulation material reaching the service life, the cold loss caused by pipeline condensation and condensation due to damage to the LNG cold insulation process or material consumption reduction, and the treatment of the LNG pipeline part with double or multiple layers of pipeline cold insulation.
4. The online repair process for LNG cryogenic pipeline leakage according to claim 3 is characterized by: The steps of treating the leakage and icing part are as follows: S21. Remove all internal cold-insulation tube shells inside the frozen area; S22. The construction plan for completely removing the first insulation layer of the insulation layer pipe includes the following five methods S231~S235: S221. Install fixed foam external support, calculate the amount of black and white materials used, and pour foam for the first layer of failed pipes. The minimum thickness of the foam is 50mm and the maximum thickness is 80mm. The thickness is adjusted according to the pipe diameter and the original design documents; S222. Use low-temperature cotton or aerogel for the first two-layer installation protection. The minimum thickness of low-temperature cotton or aerogel is 20mm and the maximum thickness is 50mm. The thickness is adjusted according to the pipe diameter and the original design documents. S223, PIR or foam glass is used for wrapping. The minimum thickness of PIR or foam glass is 50mm and the maximum thickness is 100mm. The thickness is adjusted according to the pipe diameter and the original design documents. S224, using composite porous vacuum silicon for wrapping, the minimum thickness of vacuum silicon is 2mm, the maximum thickness is 10mm, and the thickness is adjusted according to the pipe diameter and the original design documents; S225; It is wrapped with composite low-temperature nitrile rubber products. The minimum thickness of the nitrile rubber products is 25mm and the maximum thickness is 70mm. The thickness is adjusted according to the pipe diameter and the original design documents. S23. Clean the pipeline surface. Use nitrogen to purge or alcohol to brush the exposed low-temperature pipeline surface to prevent ice from forming on the pipeline surface. Use air blocking to isolate the pipeline in sections at the pipe support. S24, apply a moisture-proof layer or bond aluminum foil to the surface of the first cold-insulation pipe, and isolate the first layer of cold-insulation material from the second layer of cold-insulation material to prevent air and condensation. The steps are as follows: S241, apply a layer of isolation coating, the coating layer is a polyurethane waterproof coating layer, the minimum thickness of the coating layer is 50 microns, and the maximum thickness is 80 microns; S242, install a layer of composite porous vacuum silicon, the minimum thickness of the composite porous vacuum silicon is 2 mm, and the maximum thickness is 10 mm; Apply a layer of isolation paint, the minimum thickness of the isolation paint layer is 50 microns and the maximum thickness is 80 microns; S243, install a layer of thick composite vacuum silicon, the minimum thickness of the composite vacuum silicon is 2mm, the maximum thickness is 10mm; Apply a layer of isolation coating, which is polyurethane waterproof coating. The minimum thickness of the isolation coating is 50 microns and the maximum thickness is 80 microns; S25. Install the exterior guard plate and conduct acceptance inspection.
5. The online repair process for LNG cryogenic pipeline leakage according to claim 3 is characterized by: The steps for processing the pipeline portion of condensed water caused by the failure of LNG refrigeration are as follows: S31, apply a layer of isolation coating, the minimum thickness of the coating layer is 50 microns and the maximum thickness is 80 microns; S32, install a layer of composite porous vacuum silicon, the minimum thickness of the composite porous vacuum silicon is 2 mm, and the maximum thickness is 10 mm; S33, applying a layer of isolation coating, the minimum thickness of the isolation coating layer is 50 microns and the maximum thickness is 80 microns; S34, install a layer of thick composite vacuum silicon, the minimum thickness of the composite vacuum silicon is 2mm, and the maximum thickness is 10mm; S35, apply a layer of isolation coating, the minimum thickness of the isolation coating is 50 microns and the maximum thickness is 80 microns; S36. Install the outer guard plate and carry out acceptance inspection.
6. The online repair process for LNG cryogenic pipeline leakage according to claim 3 is characterized by: The steps for processing the double-layer or multi-layer LNG pipeline part are as follows: S41. Remove the outermost layer of PIR insulation material that has failed; S42, apply a layer of isolation coating, the minimum thickness of the coating layer is 50 microns and the maximum thickness is 80 microns; S43, install a layer of composite porous vacuum silicon, the minimum thickness of the composite porous vacuum silicon is 2 mm, and the maximum thickness is 10 mm; S44, apply a layer of isolation coating, the minimum thickness of the isolation coating layer is 50 microns and the maximum thickness is 80 microns; S45, apply a layer of isolation coating, the minimum thickness of the isolation coating is 50 microns and the maximum thickness is 80 microns; S46, install a layer of thick composite vacuum silicon, the minimum thickness of the composite vacuum silicon is 2mm, and the maximum thickness is 10mm; S47. Install the exterior guard plate and carry out acceptance inspection.
7. The online repair process for LNG cryogenic pipeline leakage according to claim 1 is characterized by: The detection instrument includes an infrared thermometer or temperature sensor, a hygrometer, a pressure gauge and an ultrasonic thickness gauge. The infrared thermometer is used to compare the measured temperature T with the set safe temperature range Tsafe. If the measured temperature exceeds the set value, the integrity of the insulation layer needs to be further analyzed. The expression is: T<Tsafe。 8. The online repair process for LNG cryogenic pipeline leakage according to claim 7 is characterized by: The hygrometer is used to measure the relative humidity RH of the air near the pipeline, and the expression is: Where Td is the dew point temperature; T is the temperature measured by the infrared thermometer; If the dew point temperature Td is close to the pipe surface temperature T, there is a risk of condensation.
9. The online repair process for LNG cryogenic pipeline leakage according to claim 7, characterized in that: The pressure gauge is used for pipeline pressure testing to ensure that there is no leakage in the pipeline. The calculation expression is: P=F / A Where F is the force acting on the pipe, and A is the cross-sectional area of the pipe; If the test pressure is lower than the design standard, it indicates leakage or damage.
10. The online repair process for LNG cryogenic pipeline leakage according to claim 7, characterized in that: The ultrasonic thickness gauge detects the wall thickness of the pipeline, identifies corrosion or wear, and calculates the wall thickness d through the sound velocity and echo time, which is expressed as: Where v is the propagation speed of the sound wave in the material, and t is the echo time.