Sodium-ion battery hard carbon negative electrode material preparation device

By using photomultiplier tubes and color development reactions in the pickling liquid testing mechanism, the problem of degradation of cleaning effect caused by the accumulation of metal ions in the pickling liquid is solved, automatic detection is achieved, and production efficiency is improved and product quality.

CN119064323AInactive Publication Date: 2024-12-03ANHUI XIONGCHU ENERGY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411302641.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-18
Publication Date
2024-12-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the prior art, during the preparation of hard carbon anode materials of sodium ion batteries, the accumulation of metal ions such as iron ions will lead to a decrease in cleaning effect, lack of automated and high-precision detection methods, which will affect production efficiency and product quality.

Method used

A pickling liquid testing mechanism including lamp tube, bottom tube, photomultiplier tube and color developer was designed. The metal ion content in the pickling liquid was automatically detected through monochromatic light irradiation and color development reaction, and the photomultiplier tube and The comparator implements automated detection.

Benefits of technology

It realizes automatic detection of metal ion content in the pickling liquid, improves detection efficiency and accuracy, ensures the stability of the pickling process and material performance, and improves production efficiency and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119064323A_ABST
    Figure CN119064323A_ABST
Patent Text Reader

Abstract

The invention discloses a sodium ion battery hard carbon negative electrode material preparation device, and belongs to the technical field of hard carbon negative electrode material preparation, the sodium ion battery hard carbon negative electrode material preparation device comprises a pickling tank for containing a pickling solution and a pickling solution testing mechanism connected with the pickling tank, the pickling solution testing mechanism comprises a lamp tube, a bottom tube and a photomultiplier which are arranged in sequence; a monochromator is fixedly arranged on the peripheral surface of the lamp tube; monochromatic light emitted by the lamp tube is irradiated to the photomultiplier after passing through the bottom tube; and a pickling solution and a color developing agent which are mixed are accommodated in the bottom tube. A top pipe is fixedly arranged at the top of the bottom pipe; a partition plate is fixedly arranged in the top pipe in the vertical direction, and a pickling solution and a color developing agent are injected into liquid injection chambers on the two sides of the partition plate respectively; a valve plate is fixedly arranged between the top pipe and the bottom pipe; two liquid outlet through holes are formed in the valve plate; a liquid outlet plate is slidably arranged in the liquid outlet through hole in the vertical direction; a liquid outlet is formed in the liquid outlet plate; a liquid inlet groove is formed in the top face of the liquid outlet plate and communicates with the liquid outlet. The device has the effect of automatically detecting the content of the metal ions in the pickling solution.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of hard carbon negative electrode material preparation, and in particular relates to a device for preparing hard carbon negative electrode materials for sodium ion batteries. Background Art

[0002] In the preparation process of hard carbon negative electrode materials for sodium ion batteries, the use of pickling solution is one of the key steps. Pickling solution can effectively remove impurities and defects on the surface of the material and improve the performance of the material. However, during repeated use, the pickling solution will gradually accumulate metal ions, especially iron ions, that fall off during the treatment process. When the content of these metal ions exceeds a certain standard, the cleaning effect of the pickling solution will be significantly reduced, and may even cause secondary pollution to the material. Therefore, the pickling solution needs to be regenerated or replaced regularly to maintain its cleaning effect. At present, the judgment of whether the metal ions in the pickling solution exceed the standard mainly relies on manual detection. This process is not only time-consuming and labor-intensive, but also lacks accuracy and real-time performance, and cannot meet the requirements of efficiency and precision in industrial production. Therefore, the development of an automated and high-precision method for detecting the metal ion content of the pickling solution is of great significance for improving production efficiency and ensuring product quality. Summary of the invention

[0003] The purpose of the present invention is to overcome the above problems existing in the prior art and provide a device for preparing hard carbon negative electrode materials for sodium ion batteries.

[0004] In order to achieve the above technical objectives and the above technical effects, the present invention is implemented through the following technical solutions:

[0005] A device for preparing hard carbon negative electrode materials for sodium ion batteries comprises a pickling tank for containing pickling solution and a pickling solution testing mechanism connected to the pickling tank, wherein the pickling solution testing mechanism comprises a lamp tube, a bottom tube and a photomultiplier tube arranged in sequence; a monochromator is fixedly arranged on the outer peripheral surface of the lamp tube; the monochromatic light emitted by the lamp tube passes through the bottom tube and irradiates the photomultiplier tube; the bottom tube contains mixed pickling solution and a developer.

[0006] Optionally, a top tube is fixedly provided on the top of the bottom tube; a partition is fixedly provided vertically inside the top tube, and the pickling liquid and the color developer are respectively injected into the injection chambers on both sides of the partition; a valve plate is fixedly provided between the top tube and the bottom tube; two liquid outlet holes are provided on the valve plate; a liquid outlet plate is vertically slidably provided inside the liquid outlet holes; a liquid outlet port is provided on the liquid outlet plate; a liquid inlet groove is provided on the top surface of the liquid outlet plate, and the liquid inlet groove is connected with the liquid outlet port.

[0007] Optionally, a support plate is fixedly provided on the outer peripheral surface of the valve plate; a plate groove is opened in the liquid outlet hole; the support plate is slidably arranged in the plate groove along the height direction of the top tube; a tension spring and an electromagnet are fixedly provided in the plate groove; a metal sheet that can be magnetically attracted to the electromagnet is fixedly provided on the bottom surface of the support plate; the tension spring provides elastic force for the support plate to reset upward.

[0008] Optionally, a vertical plate is fixedly provided in the liquid injection chamber; the vertical plate divides the liquid injection chamber into a liquid inlet chamber and a liquid level chamber; a floating plate is vertically slidably provided in the liquid level chamber.

[0009] Optionally, a slide groove is provided on the top surface of the top tube, and a slide plate is slidably arranged in the slide groove along the height direction of the top tube; a contact switch is arranged between the slide groove and the slide plate; a compression spring is arranged in the slide groove, and the compression spring is used to push the slide plate to reset downward.

[0010] Optionally, a second electromagnet is fixedly provided on the bottom surface of the top tube; and a metal sheet that can be adsorbed by the second electromagnet is fixedly provided on the top surface of the floating plate.

[0011] Optionally, a second slide groove is provided on the side wall of the vertical plate, and a second slider is provided in the second slide groove for sliding along the width direction of the vertical plate; a chamfer is provided on the second end of the slider, and a second contact switch is provided between the slider and the second slide groove; and the second electromagnet is connected to the second contact switch.

[0012] Optionally, a compression spring 2 is fixedly disposed in the second slide groove, and the compression spring 2 is used to drive the second slide block to reset outward.

[0013] The beneficial effects of the present invention are:

[0014] 1. Through the automated design of the pickling liquid testing mechanism, the metal ion content in the pickling liquid can be tested without manual intervention, which improves the detection efficiency and accuracy. The automated detection process reduces manual operations and improves production efficiency.

[0015] 2. By precisely controlling the metal ion content of the pickling solution, the stability and consistency of the pickling process are ensured, thereby improving the performance and quality of the hard carbon negative electrode material for sodium ion batteries. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] The drawings described herein are used to provide a further understanding of the present invention and constitute a part of this application. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:

[0017] Figure 1 It is a cross-sectional view of the pickling liquid testing mechanism according to an embodiment of the present invention.

[0018] Figure 2 It is a cross-sectional view of a top pipe according to an embodiment of the present invention.

[0019] Figure 3 yes Figure 2 A magnified schematic diagram of center A.

[0020] Figure numerals: 1, top pipe; 11, bottom pipe; 12, partition; 13, liquid injection chamber; 14, vertical plate; 15, liquid inlet chamber; 16, liquid level chamber; 17, floating plate; 18, valve plate; 19, liquid outlet hole; 2, liquid outlet plate; 21, support plate; 22, plate groove; 23, tension spring; 24, slide groove one; 25, slide plate one; 26, slide groove two; 27, slide block two. DETAILED DESCRIPTION

[0021] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0022] In the description of the present invention, it should be understood that the terms "opening", "upper", "lower", "thickness", "top", "middle", "length", "inside", "all around" and the like indicating orientation or positional relationship are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the components or elements referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0023] like Figure 1 A sodium ion battery hard carbon negative electrode material preparation device shown includes a pickling tank for containing pickling solution and a pickling solution testing mechanism connected to the pickling tank. The pickling solution testing mechanism includes a top tube 1 and a bottom tube 11 fixed to each other. A partition 12 is fixed vertically inside the top tube 1, and the partition 12 divides the top tube 1 into two semicircular injection chambers 13 isolated from each other; the pickling tank is connected to the injection chamber 1 through a liquid inlet pipe 1, and the liquid inlet pipe 1 is used to inject the pickling solution into the liquid injection chamber 1; a liquid inlet pipe 2 is fixed on the second side of the injection chamber, and the liquid inlet pipe 2 is used to inject a color developer into the liquid injection chamber 2. Liquid pumps are provided on the liquid inlet pipe 1 and the liquid inlet pipe 2, respectively.

[0024] In this embodiment, the color developer is ammonium thiocyanate; ammonium thiocyanate reacts with iron ions in the pickling solution to generate a red iron thiocyanate complex; which is used for the subsequent color development reaction.

[0025] A vertical plate 14 is fixedly arranged in the first or second liquid injection chamber along the vertical direction; the vertical plate 14 divides the first or second liquid injection chamber into a liquid inlet chamber 15 and a liquid level chamber 16 which are isolated from each other. A floating plate 17 is vertically slidably arranged in the liquid level chamber 16; preferably, the cross-sectional shape of the floating plate 17 is equivalent to the cross-sectional shape of the liquid level chamber 16, and the floating plate 17 is slidably connected to the vertical plate 14 through a dovetail block, so that the floating plate 17 can only move along the height direction of the top pipe 1.

[0026] The bottom tube 11 is fixed to the bottom of the top tube 1; a valve plate 18 is fixed between the top tube 1 and the bottom tube 11. Two liquid outlet holes 19 are symmetrically provided on the valve plate 18; the two liquid outlet holes 19 are respectively connected to the two liquid inlet chambers 15. A liquid outlet plate 2 is vertically slidably arranged in the liquid outlet hole 19; the liquid outlet plate 2 is consistent in shape with the liquid outlet hole 19 and is used to block the liquid outlet hole 19. Liquid outlets are respectively provided on the opposite side walls of the two liquid outlet plates 2. A liquid inlet groove is provided on the top surface of the liquid outlet plate 2, and the liquid inlet groove is connected to the liquid outlet.

[0027] An annular support plate 21 is fixedly arranged on the outer circumference of the valve plate 18; a plate groove 22 for accommodating the support plate 21 is opened on the wall of the liquid outlet through hole 19; the support plate 21 is slidably arranged in the plate groove 22 along the height direction of the top pipe 1. A tension spring 23 and an electromagnet 1 are fixedly arranged on the inner wall of the plate groove 22; a metal sheet that can be magnetically attracted to the electromagnet 1 is fixedly arranged on the bottom surface of the support plate 21; the electromagnet 1 drives the support plate 21 to move downward by attracting the metal sheet; the tension spring 23 provides an elastic force for the support plate 21 to return upward.

[0028] Specifically, when the electromagnet is powered on, the valve plate 18 moves downward by adsorbing the metal sheet, so that the liquid outlet is located below the liquid outlet through hole 19, and the liquid in the liquid inlet chamber 15 flows out from the liquid outlet through hole 19. When the electromagnet is powered off, the valve plate 18 is reset under the action of the tension spring 23, and the liquid outlet is blocked by the hole wall of the liquid outlet through hole 19, so that the liquid in the liquid inlet chamber 15 cannot flow out. It should be noted that the bottom of the vertical plate 14 does not contact the valve plate 18, and the liquid in the liquid outlet chamber and the liquid level chamber 16 is connected through the gap between the vertical plate 14 and the valve plate 18.

[0029] A chute 24 is provided on the top surface of the top pipe 1 in the liquid level chamber 16, and a slide plate 25 is slidably provided in the chute 24 along the height direction of the top pipe 1. A contact switch 1 is provided between the chute 24 and the slide plate 25; a compression spring 1 is provided in the chute 24, and the compression spring 1 is used to push the slide plate 25 to reset downward. Specifically, after the floating plate 17 moves upward, it contacts the slide plate 25 and pushes the slide plate 25 to move upward, and the contact switch 1 is in a closed state; when the floating plate 17 moves downward, the slide plate 25 is reset downward under the push of the compression spring 1, and the contact switch 1 is in an open state. The contact switch 1 is connected to the connection circuit between the electromagnet 1 and the power supply. It should be noted that the two contact switches 1 are respectively connected to the two electromagnets 1. After the contact switch 1 is closed, the corresponding liquid injection chamber 1 or liquid injection chamber 2 releases liquid into the bottom pipe 11.

[0030] An electromagnet 2 is fixedly provided on the bottom surface of the top pipe 1; the electromagnet 2 is embedded in the side of the slide groove 24. A metal sheet that can be adsorbed by the electromagnet 2 is fixedly provided on the top surface of the floating plate 17. A slide groove 26 is provided on the side wall of the vertical plate 14, and a slider 27 is slidably provided in the slide groove 26 along the width direction of the vertical plate 14. After the floating plate 17 moves upward, it can contact with the slider 27; a chamfer is provided at the bottom corner position of the end of the slider 27. Specifically, the floating plate 17 contacts with the slider 27 through the chamfer and pushes the slider 27 to move inside the slide groove 26. A contact switch 2 is provided between the slider 27 and the slide groove 26; when the slider 27 moves inside the slide groove 26, the contact switch 2 is closed, the electromagnet 2 is energized, and the electromagnet 2 has an adsorption effect on the floating plate 17; after the floating plate 17 is separated from the slider 27, the contact switch 2 is disconnected and the electromagnet is de-energized. A second compression spring is fixedly arranged in the second slide groove 26, and the second compression spring is used to drive the second slide block 27 to reset outward.

[0031] Solenoid valve 1 and solenoid valve 2 are respectively arranged in liquid inlet pipe 1 and liquid inlet pipe 2; solenoid valve 1 and solenoid valve 2 are respectively connected to two contact switches 1. When contact switch 1 is closed, solenoid valve 1 and solenoid valve 2 are in a closed state; when contact switch 1 is disconnected, solenoid valve 1 and solenoid valve 2 are opened.

[0032] The test structure is arranged in the test box, and a lamp tube and a photomultiplier tube are fixed in the test box. The lamp tube is a tungsten lamp, and a monochromator is fixed on the outer surface of the lamp tube. The light emitted by the lamp tube forms monochromatic light after passing through the monochromator. The bottom tube 11, the photomultiplier tube and the lamp tube are located on the same straight line, and the bottom tube 11 is located between the photomultiplier tube and the lamp tube; the monochromatic light emitted by the lamp tube passes through the bottom tube 11 and irradiates the photomultiplier tube.

[0033] Specifically, when the two valve plates 18 are in the open state, the color developing solution and the pickling solution are mixed in the bottom tube 11, and a red complex precipitate is formed. The monochromatic light emitted by the lamp passes through the bottom tube 11 and is projected onto the photomultiplier tube. A comparator and a relay are provided in the connection circuit of the photomultiplier tube; specifically, the positive input terminal of the comparator is connected to the photomultiplier tube, and the negative input terminal is connected to the reference voltage; the output terminal is connected to the relay; and the normally closed contact of the relay is connected to an indicator light. When the current signal output by the photomultiplier tube is greater than the current signal generated by the reference voltage, the comparator outputs a high level, and the indicator light is in the off state. On the contrary, the comparator outputs a low level, and the indicator light is turned on.

[0034] Specifically, the lower the iron ion content in the pickling solution, the greater the light intensity after the monochromatic light passes through the bottom tube 11, and the stronger the current signal generated after irradiating the photomultiplier tube. When the iron ion content in the pickling solution exceeds the standard, the content of the complex generated after the pickling solution is mixed with the color developing solution increases, the light intensity after the monochromatic light passes through the bottom tube 11 decreases, and the current signal generated by the photomultiplier tube weakens; after the comparator detects that the current signal is less than the current signal formed by the reference voltage, the control indicator light is turned on.

[0035] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.

[0036] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0037] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments, and the above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, and these changes and improvements all fall within the scope of the present invention to be protected.

Claims

1. A device for preparing a hard carbon negative electrode material for a sodium ion battery, comprising a pickling tank for holding a pickling solution and a pickling solution testing mechanism connected to the pickling tank, characterized in that: The pickling liquid testing mechanism comprises a lamp tube, a bottom tube (11) and a photomultiplier tube arranged in sequence; a monochromator is fixedly arranged on the outer peripheral surface of the lamp tube; the monochromatic light emitted by the lamp tube passes through the bottom tube (11) and then irradiates the photomultiplier tube; the bottom tube (11) contains a mixed pickling liquid and a color developer.

2. A sodium ion battery hard carbon negative electrode material preparation device according to claim 1, characterized in that: A top pipe (1) is fixedly arranged on the top of the bottom pipe (11); a partition (12) is fixedly arranged in the top pipe (1) in the vertical direction, and the pickling liquid and the developer are respectively injected into the injection chambers (13) on both sides of the partition (12); a valve plate (18) is fixedly arranged between the top pipe (1) and the bottom pipe (11); two liquid outlet holes (19) are provided on the valve plate (18); a liquid outlet plate (2) is vertically slidably arranged in the liquid outlet holes (19); a liquid outlet port is provided on the liquid outlet plate (2); a liquid inlet groove is provided on the top surface of the liquid outlet plate (2), and the liquid inlet groove is connected to the liquid outlet port.

3. A sodium ion battery hard carbon negative electrode material preparation device according to claim 2, characterized in that: A support plate (21) is fixedly provided on the outer peripheral surface of the valve plate (18); a plate groove (22) is opened in the liquid outlet through hole (19); the support plate (21) is slidably arranged in the plate groove (22) along the height direction of the top tube (1); a tension spring (23) and an electromagnet are fixedly provided in the plate groove (22); a metal sheet that can be magnetically attracted to the electromagnet is fixedly provided on the bottom surface of the support plate (21); the tension spring (23) provides an elastic force for the support plate (21) to return upward.

4. A sodium ion battery hard carbon negative electrode material preparation device according to claim 3, characterized in that: A vertical plate (14) is fixedly arranged in the liquid injection chamber (13); the vertical plate (14) divides the liquid injection chamber (13) into a liquid inlet chamber (15) and a liquid level chamber (16); a floating plate (17) is vertically slidably arranged in the liquid level chamber (16).

5. A sodium ion battery hard carbon negative electrode material preparation device according to claim 3 or 4, characterized in that: The top surface of the top pipe (1) is provided with a slide groove (24), and a slide plate (25) is slidably arranged in the slide groove (24) along the height direction of the top pipe (1); a contact switch (25) is arranged between the slide groove (24) and the slide plate (25); a compression spring (25) is arranged in the slide groove (24), and the compression spring (25) is used to push the slide plate (25) to return downward.

6. A sodium ion battery hard carbon negative electrode material preparation device according to claim 4, characterized in that: A second electromagnet is fixedly provided on the bottom surface of the top pipe (1); and a metal sheet capable of being attracted to the second electromagnet is fixedly provided on the top surface of the floating plate (17).

7. A sodium ion battery hard carbon negative electrode material preparation device according to claim 6, characterized in that: The side wall of the vertical plate (14) is provided with a second slide groove (26), and a second slider (27) is slidably arranged in the second slide groove (26) along the width direction of the vertical plate (14); a chamfer is provided at the end of the second slider (27), and a second contact switch is arranged between the second slider (27) and the second slide groove (26); the second electromagnet is connected to the second contact switch.

8. The device for preparing hard carbon negative electrode material for sodium ion battery according to claim 7, characterized in that: A second compression spring is fixedly arranged in the second slide groove (26), and the second compression spring is used to drive the second slide block (27) to return outward.