In-situ infrared spectrum test tool and test method for organic electroluminescent material during electrical excitation
By using potassium bromide wafer substrate and spacer pad structure plated with micro-nano conductive film in OLED material testing, the problem of substrate interference and response rate mismatch in infrared spectroscopy test is solved, and the in-position of OLED material during electrical excitation is achieved Infrared spectral tests provide real-time data on structure-effect relationships.
Patent Information
- Application Number
- CN202411205530.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-12-03
AI Technical Summary
In the prior art, when testing OLED materials, there are problems such as glass substrate interference, potassium bromide substrate not conducting, and the infrared spectrum response rate does not match the electrical response rate of electroluminescent materials, making it difficult to realize in-situ infrared spectrum testing during electrical excitation of OLED materials. .
The micro-nano-thick elemental material conductive film is plated on the surface of the potassium bromide wafer as an anode and cathode substrate to form a plane electric field, and a cavity is formed through a thin spacer pad to place the sample, realizing infrared light transmission and electrical excitation, and ensuring the response rate Consistent.
In-situ infrared spectral test during electrical excitation of OLED materials is realized, with a response rate of milliseconds. It can obtain the infrared spectral pattern changes under powered operation conditions in real time, judge the changes in chemical structures, and optimize the structural design of electroluminescent devices.
Smart Images

Figure CN119064338A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of photoelectric testing of organic electroluminescent materials, relates to in-situ infrared spectrum testing of organic electroluminescent materials during electrical excitation, and specifically relates to an in-situ infrared spectrum testing tool and a testing method of organic electroluminescent materials during electrical excitation. Background Art
[0002] Organic light-emitting diode (OLED) materials are display materials that can generate radiant light when driven by voltage. In-situ and real-time testing of the molecular structure changes of devices made of OLED materials when excited by current can provide basic data for structure-activity relationship research and guide the design of molecular structure and formulation.
[0003] At present, the main means of studying the structure and efficiency of OLED materials are luminescence characteristics testing under current excitation, static chemical structure characterization, and electrochemical theoretical research. There is a gap in the in-situ and real-time characterization of the chemical structure of the electroluminescence process. Therefore, establishing an in-situ infrared spectroscopy test method for organic electroluminescent materials during electrical excitation can improve the technical system for structure and efficiency research of OLED materials.
[0004] Electrochemical theory holds that under the action of an electric field, holes enter the device from the anode and pass through the hole injection / transport layer, while electrons enter the device from the cathode and pass through the electron injection / transport layer. The two eventually reach the organic light-emitting layer, where holes and electrons meet and recombine. The molecular structure of the electron transfer recombination process in the light-emitting layer has an electron cloud offset. The infrared spectrum is the resonant absorption of chemical bond stretching and bending vibrations produced by molecules excited by infrared light. The electron cloud offset can cause the infrared resonance absorption peak to shift or change in intensity on the original basis. In order to test the infrared spectrum signal during the power-on process, the OLED device is placed in the infrared light path. It is necessary to solve the problems of interference from the glass substrate of conventional OLED devices, the non-conductivity of the potassium bromide substrate during conventional infrared spectrum testing, and the mismatch between the infrared spectrum response rate and the electrical response rate of the electroluminescent material. Summary of the invention
[0005] In view of the shortcomings of the prior art, the purpose of the present invention is to provide an in-situ infrared spectroscopy testing tool and testing method for organic electroluminescent materials when electrically excited. A layer of micro-nanometer-thick conductive film of a single substance material is plated on the surface of a potassium bromide wafer as positive and negative pole plates, which can both transmit infrared light and be energized to form a planar electric field. The infrared response rate is consistent with the response rate of the sample when electrically excited, thereby realizing in-situ and real-time testing of the structure-activity relationship of the organic electroluminescent material.
[0006] In order to achieve the above object, the present invention adopts the following technical solutions:
[0007] An in-situ infrared spectrum testing tool for an organic electroluminescent material during electrical excitation, comprising an anode substrate having a conductive coating formed by coating micro-nano carbon on one side of a potassium bromide wafer and a cathode substrate having a conductive coating formed by coating micro-nano gold or aluminum on one side of a potassium bromide wafer;
[0008] Two thin spacers are arranged between the anode substrate and the cathode substrate in parallel with their long sides; a cavity for filling the sample is formed between the anode substrate, the cathode substrate and the two thin spacers;
[0009] The conductive coatings on the anode substrate and the cathode substrate are arranged facing each other.
[0010] The present invention also has the following technical features:
[0011] Preferably, the thickness of the conductive coating is 5-10 nm.
[0012] Preferably, the two ends of the anode substrate and the cathode substrate along the short sides are placed flush, and the two ends along the long sides are staggered with extended electrode clamp loading sections.
[0013] Furthermore, the potassium bromide wafer is a rectangle with a size of 20 mm×30 mm and a thickness of 1 to 10 mm.
[0014] Furthermore, the thin strip spacer is a plastic film thin strip spacer, which has the same length as the long side of the potassium bromide wafer, a width of 0.5 mm, and a thickness of 20 μm.
[0015] Furthermore, the width of the electrode clamp loading section is 10 mm.
[0016] The present invention also protects an in-situ infrared spectrum testing method for an organic electroluminescent material during electrical excitation, comprising the following steps:
[0017] Step 1: prepare the in-situ infrared spectrum test tooling for the organic electroluminescent material when electrically excited as described above, drop 1-2 drops of 502 glue on the overlapping of one short side of the cathode substrate or the anode substrate located at the lower side, and cure for 2-3 minutes to seal the edge; turn over the cured and sealed tooling, and drop 2-3 drops of OLED sample close to the gap of the unsealed short side, and the sample is automatically sucked into the spacer layer between the two substrates due to capillary action, and then laid flat and left to stand;
[0018] Step 2: Test the electro-optical characteristics of the sample on a liquid crystal comprehensive parameter tester to determine the infrared acquisition rate;
[0019] Step 3: Determine the infrared spectrum test parameters and set the infrared spectrum acquisition rate to match the sample current excitation response rate;
[0020] Step 4: Test the static infrared spectrum of the sample and the in-situ infrared spectrum of the sample during electrical excitation;
[0021] Step 5. Analyze the spectrum changes according to the power-on time point, and compare and analyze the infrared absorption spectra of single components and complex components under static and power-on conditions. The changes in chemical structure after power-on are judged by the peak displacement and intensity changes.
[0022] Compared with the prior art, the present invention has the following technical effects:
[0023] The in-situ infrared spectrum testing tool for organic electroluminescent materials during electrical excitation of the present invention is used to make the substrate for preparing the sample conductive and transmit infrared light. A layer of single-substance conductive film with a micro-nanometer thickness is plated on the surface of a potassium bromide wafer as an anode substrate and a cathode substrate, which can transmit infrared light and form a planar electric field when powered on. The in-situ infrared spectrum testing method for organic electroluminescent materials during electrical excitation of the present invention has the function of in-situ obtaining the change law of the infrared spectrum of the organic electroluminescent material under power-on conditions, with the fastest response rate being at the millisecond level. The photoelectric response is made consistent with the infrared spectrum testing rate through calculation. By comparing and analyzing the infrared spectrum under static conditions and power-on conditions, the chemical structure change after power-on is judged by the spectrum peak displacement and intensity change, so as to realize the in-situ and real-time testing of the structure-activity relationship of the organic electroluminescent material, and is used to study the change law of the complexation, crystal transformation, molecular arrangement and the like of the sample molecules, so as to provide an in-situ and real-time testing method for further studying the structure-activity relationship, and to provide chemical structure information for optimizing the structural design and stable use of electroluminescent devices. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 This is a schematic diagram of the in-situ infrared spectrum test tooling structure when the organic electroluminescent material is electrically excited;
[0025] Figure 2 The schematic diagram is a principle diagram of coating micro-nano carbon on one side of a potassium bromide wafer using a pulsed carbon filament evaporation method;
[0026] Figure 3 The schematic diagram is a principle diagram of coating micro-nano metal on one side of a potassium bromide wafer by vacuum magnetron ion sputtering coating method;
[0027] Figure 4 It is a schematic diagram of the infrared spectrum diagram and the in-situ infrared spectrum diagram test of the sample electrical excitation process of the present invention;
[0028] Figure 5 Comparison of typical infrared spectra with and without power in the high frequency area;
[0029] Figure 6 Comparison of typical infrared spectra with and without power on the low-frequency fingerprint area;
[0030] Figure 7 This is the infrared spectrum interference test chart caused by glass and ITO conductive film;
[0031] The meanings of the numbers in the figure are: 1-potassium bromide wafer, 2-conductive coating, 3-thin strip spacer. DETAILED DESCRIPTION
[0032] The specific contents of the present invention are further explained in detail below in conjunction with embodiments.
[0033] like Figure 1 As shown, this embodiment provides an in-situ infrared spectrum test tool for an organic electroluminescent material when electrically excited, comprising an anode substrate having a conductive coating 2 formed by coating micro-nano carbon on one side of a potassium bromide wafer 1 and a cathode substrate having a conductive coating 2 formed by coating micro-nano gold or aluminum on one side of the potassium bromide wafer 1;
[0034] Since potassium bromide and single-substance materials have no infrared signals, in order to form positive and negative electric fields and to be used as infrared "transparent" substrates, a single-substance conductive film with a micro-nanometer thickness is plated on the surface of the potassium bromide wafer 1 as an anode substrate and a cathode substrate, which can both transmit infrared light and be energized to form a planar electric field. In the tooling of the present invention, the potassium bromide wafer 1 and the conductive coating 2 have no infrared signals and do not interfere with the sample test; the anode substrate and the cathode substrate are transparent or weakly absorbing in the mid-infrared region and can be used as conductive electrode bases for electroluminescent devices; the thickness of the conductive coating 2 is 5 to 10 nm. The potassium bromide wafer 1 is a rectangle of 20 mm × 30 mm and a thickness of 1 to 10 mm.
[0035] like Figure 2 As shown, a pulsed carbon filament evaporation method is used to plate micro-nano carbon on one side of a potassium bromide wafer 1. The specific operation is as follows:
[0036] Under normal pressure, the sharpened carbon rods are respectively mounted on the positive and negative electrodes of the pulsed carbon filament evaporation carbon plating device, with the sharpened parts facing each other and the distance between the two tips visually about 10mm. A white paper is placed under the potassium bromide wafer 1 under the electrode, and a 5-10nm conductive carbon layer can be formed on the potassium bromide wafer 1 at a pressure of 10-4Pa, a current of 30-40A, and an action time of 10-20s. When the wafer is taken out, the white outline of the wafer on the white paper below also indicates that a coating has been produced.
[0037] like Figure 3 As shown, a vacuum magnetron ion sputtering coating method is used to coat micro-nano-level metal gold or aluminum on one side of the potassium bromide wafer 1. The specific operation is as follows:
[0038] The ion sputtering coating method is to fill argon gas in a medium vacuum atmosphere, add 1-2.5kV DC high voltage between the anode and the cathode, and use gold or aluminum target as the cathode electrode. The argon gas is ionized into Ar + ,Ar - , and under the action of the electric field, Ar +The target is accelerated to the cathode. When the wafer is placed above the target, the sputtered metal atoms will fall onto the wafer surface. The sputtering time is 120 seconds to form a 5-10nm metal film.
[0039] Two thin strip spacers 3 are arranged between the anode substrate and the cathode substrate in parallel with their long sides; the thin strip spacers 3 are plastic film thin strip spacers, with the same length as the long side of the potassium bromide wafer 1, a width of 0.5 mm and a thickness of 20 μm.
[0040] A cavity for filling the sample is formed between the anode substrate, the cathode substrate and the two thin spacers 3;
[0041] The conductive coating films 2 on the anode substrate and the cathode substrate are arranged facing each other, and the sample is placed between the anode substrate and the cathode substrate to manufacture an in-situ test device.
[0042] The anode substrate and the cathode substrate are placed flush along the two ends of the short side, and the two ends of the long side are staggered with each other to provide extended electrode clamp loading sections; the width of the electrode clamp loading section is 10 mm.
[0043] An in-situ infrared spectrum testing method for an organic electroluminescent material during electrical excitation comprises the following steps:
[0044] Step 1: Prepare an in-situ infrared spectrum test tool for organic electroluminescent materials during electrical excitation. The specific operations are as follows:
[0045] Place the coated anode substrate or cathode substrate flat on the table with the coating facing upward, and place a plastic film thin strip spacer 3 close to one long side and 10 mm away from the other long side. The plastic film thin strip spacer 3 is the same length as the long side of the wafer, 0.5 mm wide and 20 μm thick.
[0046] Cover another substrate with the coating facing downward, align the two sides of the short sides so that the long side of one side is close to the plastic film strip spacer 3 at a distance of 10mm, and the distance between the long side of the other side and the other plastic film strip spacer 3 is 10mm, so that the left and right sides of the long sides of the anode substrate and the cathode substrate are extended by 10mm respectively as the positive and negative electrode clamp loading areas, drop 1-2 drops of 502 glue on the overlapping of one short side of the cathode substrate or the anode substrate located on the lower side, and cure for 2-3 minutes to seal the edge; turn over the cured and sealed tooling, and drop 2-3 drops of OLED sample close to the gap of the unsealed short side. The sample is automatically sucked into the spacer layer between the two substrates due to capillary action, and there should be no bubble defects, and it should be placed flat and let stand;
[0047] Step 2: Test the electro-optical characteristics of the sample on a liquid crystal comprehensive parameter tester to determine the infrared acquisition rate;
[0048] The threshold voltage (Fth), saturation voltage (Fsat), 10% transmittance rise time and other data of the sample were tested on a liquid crystal comprehensive parameter tester. The 10% transmittance rise time was used as the electrical excitation response time, and 10% determined the infrared acquisition rate.
[0049] Step 3, determine the infrared spectrum test parameters, set the infrared spectrum acquisition rate to match the sample current excitation response rate, the infrared spectrum acquisition rate is converted from the number of spectra collected per second to the time response time of each spectrum, such as the response time when the transmittance rises by 10% as the basis for setting the infrared spectrum fast scanning parameters, such as the acquisition rate of 10 sheets / second is converted to 6 milliseconds per spectrum, that is, 6 milliseconds response rate;
[0050] The test mode is infrared transmission fast scanning mode, the detector is liquid nitrogen cooled mercury cadmium tellurium A detector (MCT, mercury cadmium tellurium), the test range is 4000~650cm -1 , resolution 4cm -1 . According to the different response rates of OLED electrical excitation or research focus, the number of scans for each spectrum can be selected from 1 to 16 times, the total acquisition time can be selected from more than 1 second, and the moving mirror speed can be selected from 0.6329 to 6.329. For example, when each spectrum is scanned once and the moving mirror speed is 6.329, 10 infrared spectra can be collected per second, and the response time of each spectrum is 6 milliseconds.
[0051] Step 4: Test the static infrared spectrum of the sample and the in-situ infrared spectrum of the sample during electrical excitation;
[0052] Figure 4 The infrared spectrum diagram of the present invention and the schematic diagram of the in-situ infrared spectrum diagram of the sample electrical excitation process test; Figure 4 As shown, scan the air background without placing a sample, and save the air background file as the background when power is turned on. Place the prepared sample in the infrared spectrum sample compartment, scan the background the same number of times as the sample, and obtain a static infrared spectrum of the sample;
[0053] The positive and negative poles of the LCD comprehensive parameter tester power-on device are lengthened, and the electrode clips at the ends of the connection are clamped on the anode substrate and cathode substrate of the sample device. At the same time, the infrared spectrum fast scanning program and the LCD comprehensive parameter tester program are started. All spectrum backgrounds in the fast scanning program use the pre-stored air background to obtain a series of spectra during the power-on process.
[0054] Step 5. Analyze the spectrum changes according to the power-on time point, and compare and analyze the infrared absorption spectra of the power-on process of single components and compound components under static and power-on conditions, and judge the changes in chemical structure after power-on by the peak displacement and intensity change. When comparing the intensity of specific absorption peaks, the comparison must be made under the same baseline, integration range, and the same internal standard peak conditions.
[0055] Figure 5 Comparison of typical infrared spectra with and without power in high frequency area; Figure 5 As shown in Figure 2, the intensity of the amine complexation decreases when power is applied, which is reflected in the amine stretching vibration peak at 3409 cm -1 、3203cm -1 The liquid crystal transition phenomenon occurs when the power is turned on, which is manifested at 1000cm -1 Changes in the absorption peak shape in the fingerprint region.
[0056] Figure 6 Comparison of typical infrared spectra with and without power on the low-frequency fingerprint area; Figure 6 As shown, the liquid crystal transition phenomenon is displayed.
[0057] Figure 7 This is the infrared spectrum interference test chart caused by glass and ITO conductive film. Figure 5 , 6 As shown in Figure 7, the potassium bromide wafer substrate coated with a conductive film of the present invention overcomes the interference of the infrared spectrum.
[0058] Although the embodiments of the present invention have been described in conjunction with the accompanying drawings, those skilled in the art may make various modifications and variations without departing from the spirit and scope of the present invention, and such modifications and variations are all within the scope defined by the appended claims.
Claims
1. An in-situ infrared spectrum testing tool for organic electroluminescent materials during electrical excitation, characterized in that: It comprises an anode substrate on one side of a potassium bromide wafer (1) coated with micro-nano carbon to form a conductive coating (2) and a cathode substrate on one side of a potassium bromide wafer (1) coated with micro-nano gold or aluminum to form a conductive coating (2); Two thin spacers (3) are arranged between the anode substrate and the cathode substrate in parallel with their long sides; a cavity for filling a sample is formed between the anode substrate, the cathode substrate and the two thin spacers (3); The conductive coatings (2) on the anode substrate and the cathode substrate are arranged facing each other.
2. The in-situ infrared spectrum testing tool for organic electroluminescent materials during electrical excitation as claimed in claim 1, characterized in that: The thickness of the conductive coating (2) is 5-10 nm.
3. The in-situ infrared spectrum testing tool for organic electroluminescent materials during electrical excitation as claimed in claim 1, characterized in that: The anode substrate and the cathode substrate are placed flush along the two ends of the short sides, and the two ends of the long sides are staggered with each other to provide extended electrode clamp loading sections.
4. The in-situ infrared spectrum testing tool for organic electroluminescent materials during electrical excitation as claimed in claim 3, characterized in that: The potassium bromide wafer (1) is a rectangle with a size of 20 mm×30 mm and a thickness of 1 to 10 mm.
5. The in-situ infrared spectrum testing tool for organic electroluminescent materials during electrical excitation as claimed in claim 4, characterized in that: The thin strip spacer (3) is a plastic film thin strip spacer, which has the same length as the long side of the potassium bromide wafer (1), a width of 0.5 mm and a thickness of 20 μm.
6. The in-situ infrared spectrum testing tool for organic electroluminescent materials during electrical excitation as claimed in claim 4, characterized in that: The width of the electrode clamp loading section is 10 mm.
7. An in-situ infrared spectrum testing method for an organic electroluminescent material during electrical excitation, characterized in that: The following steps are involved: Step 1, prepare an in-situ infrared spectrum test tool for the organic electroluminescent material when electrically excited as described in any one of claims 1 to 6, drop 1 to 2 drops of 502 glue on the overlapping of one short side of the cathode substrate or the anode substrate located on the lower side, and cure for 2 to 3 minutes to seal the edge; turn over the cured and sealed tool, and drop 2 to 3 drops of OLED sample close to the gap of the unsealed short side, and the sample is automatically sucked into the spacer layer between the two substrates due to capillary action, and then laid flat and left to stand; Step 2: Test the electro-optical characteristics of the sample on a liquid crystal comprehensive parameter tester to determine the infrared acquisition rate; Step 3: Determine the infrared spectrum test parameters and set the infrared spectrum acquisition rate to match the sample current excitation response rate; Step 4: Test the static infrared spectrum of the sample and the in-situ infrared spectrum of the sample during electrical excitation; Step 5. Analyze the spectrum changes according to the power-on time point, and compare and analyze the infrared absorption spectra of single components and complex components under static and power-on conditions. The changes in chemical structure after power-on are judged by the peak displacement and intensity changes.
Citation Information
Cited By
System for evaluating spraying effect of semiconductor device in vacuum box based on multi-dimensional data
CN121092924A