MRAM memory bit and memory array
By using the inverse piezoelectric effect of the piezoelectric layer to change the stress state in the MRAM memory bit, the uncompensated magnetic moment flip of the antiferromagnetic metal layer is driven, and the electric field driving magnetic moment flip is achieved without current, which solves the SOT-MRAM memory device The problems of high power consumption and low write speed efficiency improve write efficiency.
Patent Information
- Application Number
- CN202310652680.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-06-02
- Publication Date
- 2024-12-03
AI Technical Summary
SOT-MRAM memory devices consume a large power during the writing process and have low write speed efficiency, making it difficult to achieve below 5ns. The write current flowing into the heavy metal layer is large, and the spin Hall angle needs to be increased to improve the writing efficiency.
Design an MRAM memory bit, including a piezoelectric layer, an antiferromagnetic metal layer and a magnetic tunnel junction, changes the stress state under different voltages through the inverse piezoelectric effect, and transfers it to the interface of the antiferromagnetic metal layer, and flips the uncompensated magnetic moment. and exchange bias field to drive the free layer magnetic moment flip, realize the electric field driving magnetic moment flip, and reduce power consumption.
In the absence of an external magnetic field, the electric field drives the free layer magnetic moment flip is realized, and there is no current during the writing process, reducing device power consumption, maintaining storage density, and improving writing efficiency.
Smart Images

Figure CN119068935A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of MRAM memory, and in particular to an MRAM storage bit and a storage array. Background Art
[0002] Magnetic random access memory (MRAM) is a new type of non-volatile memory with excellent characteristics such as nanosecond high-speed reading and writing, nearly unlimited service life, and data retention time of more than 10 years. It has become the most promising technology for the next generation of memory. The current mainstream mechanisms of MRAM include spin transfer torque mechanism (STT-MRAM) and spin orbit torque mechanism (SOT-MRAM). STT-MRAM can be mass-produced, but the balance between the write speed and breakdown voltage of STT-MTJ limits the write speed efficiency of STT-MTJ (it is difficult to reach below 5ns). As a three-terminal device, SOT-MRAM can realize read-write separation and improve erase and write life. However, SOT-MRAM still faces a problem: the write current passed into the heavy metal layer is large, and the spin Hall angle of the heavy metal layer needs to be increased to obtain higher write efficiency, which consumes a lot of power. Summary of the invention
[0003] In view of this, the present invention provides an MRAM storage bit cell and a storage array, which can reduce device power consumption.
[0004] In a first aspect, the present invention provides an MRAM storage bit cell, comprising:
[0005] Piezoelectric layer;
[0006] an antiferromagnetic metal layer, located above the piezoelectric layer;
[0007] A magnetic tunnel junction, located above the antiferromagnetic metal layer, comprising a stacked free layer, a tunnel layer and a reference layer, wherein the free layer is close to the antiferromagnetic metal layer, and the free layer and the reference layer have perpendicular magnetic anisotropy;
[0008] Wherein, the piezoelectric layer has an inverse piezoelectric effect and has different stress states under different voltages;
[0009] The antiferromagnetic metal layer has a reversible uncompensated magnetic moment at the interface close to the free layer, and the uncompensated magnetic moment generates an exchange bias field. When the stress provided by the piezoelectric layer is transmitted to the interface of the antiferromagnetic metal layer close to the free layer, the uncompensated magnetic moment is reversed, and the direction of the exchange bias field is reversed, thereby driving the magnetic moment of the free layer to be reversed.
[0010] Optionally, the piezoelectric layer is non-conductive, and the material is selected from any one of lead zirconate titanate (PZT), barium titanate (BaTiO3), lead magnesium niobate-lead titanate (PMN-PT) and lead zinc niobate-lead titanate (PZN-PT).
[0011] Optionally, the material of the antiferromagnetic metal layer is conductive and is selected from any one of IrMn, PtMn and FeMn.
[0012] Optionally, it also includes:
[0013] A bottom electrode, located below the piezoelectric layer;
[0014] The antiferromagnetic metal layer serves as the top electrode of the piezoelectric layer, and a voltage is applied to the piezoelectric layer through the bottom electrode and the antiferromagnetic metal layer to control the stress state of the piezoelectric layer.
[0015] Optionally, the material of the bottom electrode is selected from any one of Cu, Ag, Au, Al, Ti, and W.
[0016] Optionally, an angle between the bottom electrode and the antiferromagnetic metal layer is θ, 0°≤θ≤90°.
[0017] Optionally, it also includes:
[0018] A first side electrode, located at one side of the piezoelectric layer;
[0019] The second side electrode is located on the other side of the piezoelectric layer opposite to the first side electrode, and a voltage is applied to the piezoelectric layer through the first side electrode and the second side electrode to control the stress state of the piezoelectric layer.
[0020] Optionally, a material of the first side electrode and the second side electrode is selected from any one of Cu, Ag, Au, Al, Ti, and W.
[0021] Optionally, it also includes:
[0022] A magnetic hard mask layer is located above the magnetic tunnel junction, and the magnetic hard mask layer has perpendicular magnetic anisotropy and is used to provide an equivalent magnetic field in the opposite direction to the exchange bias field at the interface of the antiferromagnetic metal layer close to the free layer. When the equivalent magnetic field is greater than the exchange bias field, the magnetic moment of the free layer is along the direction of the equivalent magnetic field; when the exchange bias field is greater than the equivalent magnetic field, the magnetic moment of the free layer is along the direction of the exchange bias field.
[0023] In a second aspect, the present invention provides an MRAM storage array, comprising the above-mentioned MRAM storage bit.
[0024] The MRAM storage bit provided by the present invention applies different voltages to the piezoelectric layer, and different stress states can be obtained due to the inverse piezoelectric effect and transmitted to the interface of the antiferromagnetic metal layer near the free layer, and the stress is used to change the direction of the uncompensated magnetic moment at the interface of the antiferromagnetic metal layer, thereby changing the direction of the exchange bias field, and then driving the magnetic moment of the free layer to flip. Compared with the prior art, the electric field can drive the magnetic moment flip of the free layer in the absence of an external magnetic field, and there is no current during the writing process, which reduces the power consumption of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 A schematic cross-sectional structure diagram of an MRAM storage bit cell according to an embodiment of the present invention;
[0026] Figure 2 for Figure 1 A schematic diagram of the three-dimensional structure of an MRAM storage bit is shown;
[0027] Figure 3 for Figure 1 A top view of an MRAM storage bit cell is shown;
[0028] Figure 4 A schematic diagram of the stress state of an MRAM storage bit according to an embodiment of the present invention;
[0029] Figure 5 A top view of an MRAM storage bit cell according to an embodiment of the present invention;
[0030] Figure 6 A schematic cross-sectional structure diagram of an MRAM storage bit cell according to an embodiment of the present invention;
[0031] Figure 7 for Figure 6 A top view of an MRAM storage bit cell is shown;
[0032] Figure 8 A schematic cross-sectional structure diagram of an MRAM storage bit cell according to an embodiment of the present invention;
[0033] Fig. 9 A schematic cross-sectional structure diagram of an MRAM storage bit cell according to an embodiment of the present invention;
[0034] Fig.10 FIG. 4 is a schematic diagram of the structure of an MRAM storage array according to an embodiment of the present invention. DETAILED DESCRIPTION
[0035] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0036] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequential order. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present application described here. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.
[0037] In the present application, the terms "upper", "lower", "left", "right", "front", "back", "top", "bottom", "inner", "outer", "middle", "vertical", "horizontal", "lateral", "longitudinal" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings. These terms are mainly used to better describe the present application and its embodiments, and are not used to limit the indicated devices, elements or components to have a specific orientation, or to be constructed and operated in a specific orientation.
[0038] In addition, some of the above terms may be used to express other meanings in addition to indicating orientation or positional relationship. For example, the term "on" may also be used to express a certain dependency or connection relationship in some cases. For those of ordinary skill in the art, the specific meanings of these terms in this application can be understood according to specific circumstances.
[0039] In addition, the terms "installed", "set", "provided with", "connected", "connected", and "socketed" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral structure; it can be a mechanical connection, or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be an internal connection between two devices, elements, or components. For those of ordinary skill in the art, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0040] Some embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the absence of conflict, the following embodiments and features in the embodiments can be combined with each other.
[0041] An embodiment of the present invention provides an MRAM storage bit, such as Figure 1 As shown, the MRAM storage bit cell includes: a piezoelectric layer 102, an antiferromagnetic metal layer 103 and a magnetic tunnel junction 104.
[0042] The antiferromagnetic metal layer 103 is located above the piezoelectric layer 102, and the magnetic tunnel junction 104 is located above the antiferromagnetic metal layer 103, including a stacked free layer, a tunnel layer and a reference layer, the free layer is close to the antiferromagnetic metal layer 103, and the free layer and the reference layer have perpendicular magnetic anisotropy;
[0043] The piezoelectric layer 102 has an inverse piezoelectric effect and has different stress states under different voltages;
[0044] The antiferromagnetic metal layer 103 has a reversible uncompensated magnetic moment at the interface near the free layer. The uncompensated magnetic moment generates an exchange bias field, which is used to reverse the magnetic moment of the free layer. When the stress provided by the piezoelectric layer 102 is transmitted to the interface of the antiferromagnetic metal layer 103 near the free layer, the uncompensated magnetic moment at the interface of the antiferromagnetic metal layer near the free layer is reversed, and the direction of the exchange bias field is reversed, thereby driving the magnetic moment of the free layer to be reversed.
[0045] The specific description is as follows: The stress state of the piezoelectric material is related to the initial state of the piezoelectric material before the voltage is applied. In one embodiment, the piezoelectric layer is in a polarization saturation state in the initial state, which can be achieved by pre-polarizing the piezoelectric layer, that is, the initial state (domain polarization direction state) of the piezoelectric layer before the voltage is applied is consistent with the state after the saturation electric field strength is applied. In this case, when a first voltage is applied to the piezoelectric layer to form an electric field with an electric field strength greater than or equal to the coercive electric field strength, the polarization direction of the piezoelectric layer domain changes, the piezoelectric layer is in a stress state, and after the voltage is removed, the stress can still be maintained, which is non-volatile. When a second voltage is applied to the piezoelectric layer to form an electric field with an electric field strength greater than or equal to the saturation electric field strength and in the opposite direction of the coercive electric field, the piezoelectric layer will return to the state before the voltage is applied and be in a stress-free state.
[0046] The coercive electric field strength refers to the electric field strength required for the electric domain polarization strength in the piezoelectric material to return to zero, and the saturation electric field strength refers to the electric field strength when the electric domain polarization direction reaches saturation along one direction.
[0047] Figure 1In the bit structure shown, a synthetic antiferromagnetic layer is also provided above the reference layer of the magnetic tunnel junction 104 to pin the magnetization direction of the reference layer. It is also noted that the stacked structure of the magnetic tunnel junction is not limited to the structure given in this embodiment. The free layer and reference layer materials include but are not limited to magnetic materials such as Co, CoFe, CoFeB, etc., and the tunnel layer materials include but are not limited to MgO, MgAl2O4, etc. The top view morphology of the magnetic tunnel junction includes but is not limited to circular, elliptical, rectangular, etc.
[0048] Further, refer to Figure 1 The MRAM storage bit cell further includes a bottom electrode 101 located below the piezoelectric layer 102. Correspondingly, the antiferromagnetic metal layer 103 serves as the top electrode of the piezoelectric layer 102, and a voltage is applied to the piezoelectric layer 102 through the bottom electrode 101 and the antiferromagnetic metal layer 103 to control the stress state of the piezoelectric layer.
[0049] In an embodiment of the present invention, the piezoelectric layer 102 is non-conductive, and the material is selected from any one of lead zirconate titanate (PZT), barium titanate (BaTiO3), lead magnesium niobate-lead titanate (PMN-PT) and lead zinc niobate-lead titanate (PZN-PT). The antiferromagnetic metal layer can select collinear antiferromagnetic materials such as IrMn, PtMn, FeMn, etc. The material of the bottom electrode 101 is selected from any one of Cu, Ag, Au, Al, Ti, and W. It is also noted that the thickness of the piezoelectric layer needs to be controlled so that the voltage control range is within the range that the transistor can provide.
[0050] Figure 2 and Figure 3 Given Figure 1 The three-dimensional view and top view of the bit structure are shown. Figure 2 and 3 As shown in the figure, due to the inverse piezoelectric effect of the piezoelectric layer material, non-volatile stress will be generated in the in-plane direction (tensile stress in the x direction and compressive stress in the y direction). When the stress is transmitted to the antiferromagnetic metal layer / free layer interface, the direction of the uncompensated magnetic moment at the antiferromagnetic metal layer / free layer interface will be changed, and the direction of the exchange bias field will be reversed, thereby driving the direction of the perpendicular magnetic moment of the free layer to be reversed.
[0051] During the film growth process, an auxiliary magnetic field needs to be applied to determine the initial arrangement state of the magnetic moment at the antiferromagnetic metal layer / free layer interface and the direction of the exchange bias field, that is, to determine the initial direction of the uncompensated magnetic moment at the antiferromagnetic interface. In one embodiment, the initial direction of the uncompensated magnetic moment at the interface of the antiferromagnetic metal layer 103 close to the free layer is vertically downward.
[0052] refer to Figure 4First, the direction from the bottom electrode 101 to the antiferromagnetic metal layer 103 is defined as positive, and correspondingly, the direction from the antiferromagnetic metal layer 103 to the bottom electrode 101 is defined as negative. Meanwhile, the initial state of the piezoelectric layer 102 is a polarization saturation state (which can be achieved by pre-polarizing the piezoelectric layer). The writing process is as follows: applying an electric field greater than or equal to the saturation electric field strength (Es) to the piezoelectric layer, such as +Es (positive direction) or -Es (negative direction), and then removing the electric field. The antiferromagnetic metal layer / free layer interface is in a stress-free state, the uncompensated magnetic moment returns to the initial state, the exchange bias field direction is negative, driving the free layer magnetic moment downward, and the free layer and reference layer magnetic moments are arranged in parallel, and it is a low resistance state "0" at this time; applying an electric field greater than or equal to the coercive electric field strength (Ec) to the piezoelectric layer, such as -Ec (negative direction) or +Ec (positive direction), the direction is opposite to the previous saturation electric field strength, and then removing the electric field. The antiferromagnetic metal layer / free layer interface is in a stress state, the direction of the uncompensated magnetic moment is flipped, the exchange bias field direction is positive, driving the free layer magnetic moment upward, and the free layer and reference layer magnetic moments are arranged in antiparallel, and it is a high resistance state "1" at this time. It is worth noting that the antiferromagnetic metal layer 103 can also be used as a bottom electrode layer for reading the MTJ resistance. During the read operation, a read voltage is applied to the top of the MTJ and the antiferromagnetic metal layer 103 .
[0053] In this embodiment, the channel width of the bottom electrode 101 and the antiferromagnetic metal layer 103 needs to be larger than the MTJ diameter (for example, the MTJ diameter is 50nm, and the channel width of the bottom electrode 101 and the antiferromagnetic metal layer 103 is 70nm). The angle between the bottom electrode 101 and the antiferromagnetic metal layer 103 is θ, which can vary within a certain range, 0°≤θ≤90°. Figure 5 The case where the bottom electrode and the antiferromagnetic metal layer are perpendicular to each other is shown.
[0054] The MRAM storage bit of the embodiment of the present invention applies different voltages to the piezoelectric layer. Due to the inverse piezoelectric effect, different stress states can be obtained and transmitted to the interface of the antiferromagnetic metal layer near the free layer. The stress is used to change the direction of the uncompensated magnetic moment at the interface of the antiferromagnetic metal layer, thereby changing the direction of the exchange bias field, and then driving the magnetic moment of the free layer to flip. Compared with the prior art, electric field-driven magnetic moment flipping of the free layer can be achieved in the absence of an external magnetic field. There is no current during the writing process, which reduces the power consumption of the device. And compared with the traditional SOT-MRAM device, no additional electrode control terminal is added, and the storage density will not be lost.
[0055] In another embodiment, Figure 6 and Figure 7As shown, the MRAM storage bit includes: a piezoelectric layer 202, an antiferromagnetic metal layer 203 and a magnetic tunnel junction 204, and also includes: a first side electrode 2011 and a second side electrode 2012, the first side electrode 2011 is located on one side of the piezoelectric layer 202; the second side electrode 2012 is located on the other side of the piezoelectric layer 202 opposite to the first side electrode 2011, and a voltage is applied to the piezoelectric layer through the first side electrode 2011 and the second side electrode 2012. The material of the first side electrode and the second side electrode is selected from any one of Cu, Ag, Au, Al, Ti, and W.
[0056] In this embodiment, two electrodes at both ends of the piezoelectric layer for applying voltage are grown on both sides of the piezoelectric layer. This structure can achieve complete independent control of reading and writing, and the writing process can refer to the above embodiment.
[0057] During the reading process, voltage may be applied to the upper and lower ends of the magnetic tunnel junction 204 (the top conductive layer of the MTJ 204 and the antiferromagnetic metal layer 203 ) to read the TMR (tunneling magnetoresistance) value.
[0058] In this embodiment, the antiferromagnetic metal layer 203 and the magnetic tunnel junction 204 can be manufactured together.
[0059] Furthermore, in one embodiment, if the stress provided by the piezoelectric layer is small, the uncompensated magnetic moment at the interface of the antiferromagnetic metal layer close to the free layer cannot be completely flipped 180°, and the uncompensated magnetic moment on its surface can only be tilted, so that the exchange bias field is reduced. At this time, a hard magnet can be set in the storage bit region, such as growing a magnetic hard mask layer with perpendicular magnetic anisotropy (i.e., perpendicular magnetization direction) on the top layer of the MTJ, and the material can be FePt or FePd, Figure 8 Shown in Figure 1 The schematic diagram of the structure of the magnetic hard mask layer 105 disposed on the bit structure is shown. Fig. 9 Shown in Figure 6 The structure schematic diagram of the magnetic hard mask layer 205 disposed on the bit structure is shown.
[0060] The magnetic hard mask layer 105 (205) provides an equivalent magnetic field in a vertical direction to the free layer, and the direction is opposite to the exchange bias field generated at the interface of the antiferromagnetic metal layer / free layer, so that the direction of the magnetic moment of the free layer can be controlled by regulating the relative size of the exchange bias field and the equivalent magnetic field through the stress provided by the piezoelectric layer. When the exchange bias field is greater than the equivalent magnetic field provided by the magnetic hard mask layer, the magnetization direction of the free layer is controlled by the exchange bias field, and when the equivalent magnetic field provided by the magnetic hard mask layer is greater than the exchange bias field, the magnetization direction of the free layer is controlled by the equivalent magnetic field. That is, the exchange bias field size is changed by stress, and the direction of the magnetic moment reversal of the free layer is determined according to the relative size of the exchange bias field and the equivalent magnetic field, so as to achieve pure electric field driven free layer magnetic moment reversal.
[0061] On the other hand, an embodiment of the present invention provides an MRAM storage array, including the MRAM storage bit in the above embodiment. Fig.10 As shown, the MRAM storage array is based on Figure 5 The bit structure shown is constructed by applying voltage in the array as follows: the bottom electrode is grounded, a pulse voltage is applied to the antiferromagnetic metal layer, and the bit of the applied electric field is determined by the on-off connection between the bottom electrode and the piezoelectric layer, thereby realizing the write operation on a certain bit structure.
[0062] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.
Claims
1. An MRAM storage bit, It is characterized in that include: Piezoelectric layer; an antiferromagnetic metal layer, located above the piezoelectric layer; A magnetic tunnel junction, located above the antiferromagnetic metal layer, comprising a stacked free layer, a tunnel layer and a reference layer, wherein the free layer is close to the antiferromagnetic metal layer, and the free layer and the reference layer have perpendicular magnetic anisotropy; Wherein, the piezoelectric layer has an inverse piezoelectric effect and has different stress states under different voltages; The antiferromagnetic metal layer has a reversible uncompensated magnetic moment at the interface close to the free layer, and the uncompensated magnetic moment generates an exchange bias field. When the stress provided by the piezoelectric layer is transmitted to the interface of the antiferromagnetic metal layer close to the free layer, the uncompensated magnetic moment is reversed, and the direction of the exchange bias field is reversed, thereby driving the magnetic moment of the free layer to be reversed.
2. The MRAM storage bit cell according to claim 1, It is characterized in that The piezoelectric layer is non-conductive and the material is selected from lead zirconate titanate (PZT), barium titanate (BaTiO 3 ), any one of lead magnesium niobate-lead titanate (PMN-PT) and lead zinc niobate-lead titanate (PZN-PT).
3. The MRAM storage bit cell according to claim 1, It is characterized in that The material of the antiferromagnetic metal layer is conductive and is selected from any one of IrMn, PtMn and FeMn.
4. The MRAM storage bit cell according to claim 1, It is characterized in that Also includes: A bottom electrode, located below the piezoelectric layer; The antiferromagnetic metal layer serves as the top electrode of the piezoelectric layer, and a voltage is applied to the piezoelectric layer through the bottom electrode and the antiferromagnetic metal layer to control the stress state of the piezoelectric layer.
5. The MRAM storage bit cell according to claim 4, It is characterized in that The material of the bottom electrode is selected from any one of Cu, Ag, Au, Al, Ti, and W.
6. The MRAM storage bit cell according to claim 4, It is characterized in that The included angle between the bottom electrode and the antiferromagnetic metal layer is θ, 0°≤θ≤90°.
7. The MRAM storage bit cell according to claim 1, It is characterized in that Also includes: A first side electrode, located at one side of the piezoelectric layer; The second side electrode is located on the other side of the piezoelectric layer opposite to the first side electrode, and a voltage is applied to the piezoelectric layer through the first side electrode and the second side electrode to control the stress state of the piezoelectric layer.
8. The MRAM storage bit cell according to claim 7, It is characterized in that The material of the first side electrode and the second side electrode is selected from any one of Cu, Ag, Au, Al, Ti, and W.
9. The MRAM storage bit cell according to claim 1, It is characterized in that Also includes: A magnetic hard mask layer is located above the magnetic tunnel junction, and the magnetic hard mask layer has perpendicular magnetic anisotropy and is used to provide an equivalent magnetic field in the opposite direction to the exchange bias field at the interface of the antiferromagnetic metal layer close to the free layer. When the equivalent magnetic field is greater than the exchange bias field, the magnetic moment of the free layer is along the direction of the equivalent magnetic field; when the exchange bias field is greater than the equivalent magnetic field, the magnetic moment of the free layer is along the direction of the exchange bias field.
10. An MRAM storage array, It is characterized in that The method comprises the MRAM storage bit cell as claimed in any one of claims 1 to 9.