Bonding method for electronic components and method for mass transfer of electronic components
By using heating and ultrasonic oscillation assisted laser welding during electronic component jointing and massive transfer, the problems of uneven welding and low transfer rates are solved, efficient electronic component jointing and transfer are achieved, and production efficiency and quality are improved .
Patent Information
- Application Number
- CN202410547511.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-06-02
- Filing Date
- 2024-05-06
- Publication Date
- 2024-12-03
AI Technical Summary
The existing electronic component bonding methods and huge transfer methods have short circuits or air soldering problems caused by uneven welding, insufficient or excessive solder paste, and insufficient transfer rate and yield, which affects the production capacity for a long laser welding time.
Using a carrier table equipped with heating equipment and ultrasonic oscillation equipment, the welding pad temperature is controlled between 30℃ and 300℃ through heating and ultrasonic oscillation, and the bonding of electronic components is completed in a short time by using laser welding technology, and the bonding of electronic components is completed in a short time. Temporary substrates achieve huge transfer.
It effectively reduces the limit time of laser welding, improves the efficiency and quality of electronic components bonding, improves the transfer rate and yield, and improves production capacity.
Smart Images

Figure CN119069370A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for joining electronic components and a method for mass transferring electronic components. Background Art
[0002] Light-emitting diodes have the advantages of active light emission, high brightness, and energy saving. Therefore, they have been widely used in technical fields such as lighting, display, and projector, and micro-LED display has gradually become a new generation of display technology. However, a high-density (FHD) display has 1920 rows x 1080 columns, about 2 million pixels, and each pixel is further divided into three sub-pixels (Sub pixel) of red, green, and blue. Therefore, a high-density light-emitting diode display (FHD LED Display) has a total of about 6 million LED dies. To cut and paste these 6 million dies on the substrate of the display panel, the key technology lies in how to accurately transfer a certain amount of micro-LEDs to the substrate of the display panel and fix them together.
[0003] Conventional electronic component joining methods mainly utilize reflow soldering, whereby electronic components are soldered to a target substrate after solder paste is heated and reflowed. However, the disadvantages of reflow soldering are that during the reflow process, electronic components may drift due to uneven heating, short circuits may occur due to excessive solder paste, empty soldering may occur due to insufficient solder paste, or cold soldering may occur due to too low a reflow temperature.
[0004] In addition, conventional methods for mass transferring electronic components mainly include electrostatic transfer, magnetic transfer, micro-transfer printing, and fluid assembly, etc. However, the transfer rate and yield of these methods for mass transferring electronic components still need to be further improved.
[0005] Although the description of Taiwan invention patent application No. TW112112737 of the applicant in this case discloses a novel electronic component joining method and a method for mass transferring electronic components using laser welding to improve the shortcomings of conventional electronic component joining methods and conventional methods for mass transferring electronic components, laser welding is usually performed in a fixed temperature environment, and there is a limit time to achieve good laser welding. How to shorten this limit time to increase production capacity is what the industry is eagerly looking forward to. Summary of the invention
[0006] The present invention discloses a method for joining electronic components, which is characterized by comprising the following steps: providing a carrier, the carrier being equipped with a heating device and / or an ultrasonic oscillation device; providing a target substrate, and placing the target substrate on the carrier, the target substrate having a first upper surface and a first lower surface opposite to each other, and the first upper surface comprising a joining area, and the joining area comprising at least one welding pad, wherein when the heating device of the carrier is turned on and operated, at least one welding pad of the joining area of the target substrate can be heated to 30°C to 300°C, and when the ultrasonic oscillation device ... Ultrasonic oscillation of 5 kHz to 2 MHz; providing an electronic component, the electronic component comprising an electronic component body and at least one electrode, the electronic component body having a second upper surface and a second lower surface relative to each other, the at least one electrode being formed on the second lower surface of the electronic component body and electrically connected to the electronic component body, wherein the electronic component is aligned with the bonding area of the target substrate, and the at least one electrode is aligned with at least one welding pad in the bonding area; and providing a laser, and when the heating device of the support platform and / or the ultrasonic oscillation device are turned on, the electronic component is welded to at least one welding pad in the bonding area of the target substrate by the laser through the at least one electrode.
[0007] In the aforementioned method for bonding electronic components, the aforementioned target substrate is a semiconductor substrate, a ceramic substrate, a metal substrate, a glass substrate, a printed circuit board, or a flexible printed circuit board.
[0008] The aforementioned method for joining electronic components, wherein the aforementioned flexible printed circuit board comprises: a flexible insulating substrate; a circuit formed on the surface of the aforementioned flexible insulating substrate; and an insulating layer covering the aforementioned circuit; wherein the aforementioned solder pad is formed on the surface of the aforementioned insulating layer and is electrically connected to the aforementioned circuit.
[0009] In the aforementioned method for bonding electronic components, the electronic components are selected from a group consisting of light emitting diodes, laser diodes and semiconductor components.
[0010] In the aforementioned method for bonding electronic components, the light emitted by the aforementioned light emitting diode is red light, green light, blue light, yellow light, white light, infrared light or ultraviolet light.
[0011] In the aforementioned method for bonding electronic components, the wavelength of the aforementioned laser diode is between 390 nanometers and 1700 nanometers.
[0012] The aforementioned method for bonding electronic components, wherein the aforementioned semiconductor component is selected from a group consisting of a processor, a memory integrated circuit, a microcomponent integrated circuit, a logic integrated circuit and an analog integrated circuit.
[0013] In the aforementioned method for bonding electronic components, the material of the aforementioned at least one electrode and / or the aforementioned at least one welding pad is metal, metal alloy or metal oxide respectively.
[0014] The aforementioned method for joining electronic components further includes the step of forming a solder on the aforementioned at least one soldering pad and / or the aforementioned at least one electrode, so that the at least one electrode of the aforementioned electronic component is indirectly in contact with the at least one electrode of the aforementioned target substrate through the aforementioned solder, and the aforementioned solder is directly or indirectly heated by the aforementioned laser to obtain a heated solder, thereby allowing the at least one electrode of the aforementioned electronic component to be joined to the at least one soldering pad of the joining area of the aforementioned target substrate through the aforementioned heated solder.
[0015] In the aforementioned method for bonding electronic components, the wavelength of the aforementioned laser is between 190 nanometers and 11000 nanometers.
[0016] The aforementioned semiconductor bonding method further includes the step of disposing a transparent or semi-transparent dielectric layer on the second upper surface of the aforementioned electronic component body, wherein the aforementioned laser is irradiated toward the aforementioned electronic component body from above the aforementioned electronic component through the aforementioned transparent or semi-transparent dielectric layer.
[0017] The aforementioned semiconductor bonding method further includes the step of disposing a transparent or semi-transparent medium layer on the first lower surface of the target substrate, wherein the aforementioned laser is irradiated toward the aforementioned target substrate from below the aforementioned target substrate through the aforementioned transparent or semi-transparent medium layer.
[0018] The present invention further discloses a method for mass transfer of electronic components, characterized in that it includes the following steps: providing a carrier, the carrier is equipped with a heating device and / or an ultrasonic oscillation device; providing a target substrate, and placing the target substrate on the carrier, the target substrate having a first upper surface and a first lower surface relative to each other, and the first upper surface includes a plurality of bonding areas, and each of the plurality of bonding areas includes at least one welding pad, wherein when the heating device of the carrier is turned on, at least one welding pad of each of the plurality of bonding areas of the target substrate can be heated to 30°C to 300°C, and when the ultrasonic oscillation device is turned on, at least one welding pad of the bonding area of the target substrate can be oscillated by an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz; providing a temporary substrate above the target substrate, forming a There are multiple electronic components, each of the multiple electronic components includes an electronic component body and at least one electrode, the electronic component body has a second upper surface and a second lower surface relative to each other, the at least one electrode is formed on the second lower surface of the electronic component body and is electrically connected to the electronic component body, wherein the second lower surface of the multiple electronic component bodies faces the first upper surface of the target substrate, and each of the multiple electronic components is respectively aligned with each of the multiple bonding areas of the target substrate, and at least one electrode of each of the multiple electronic components is aligned with at least one welding pad of each of the multiple bonding areas; and a laser is provided, and when the heating device of the support platform and / or the ultrasonic oscillation device are turned on, each of the multiple electronic components is respectively welded by the laser on at least one welding pad of each of the multiple bonding areas of the target substrate through the at least one electrode.
[0019] In the aforementioned method for mass transferring electronic components, the aforementioned target substrate is a semiconductor substrate, a ceramic substrate, a metal substrate, a glass substrate, a printed circuit board, or a flexible printed circuit board.
[0020] The aforementioned method for mass transferring electronic components, wherein the aforementioned flexible printed circuit board comprises: a flexible insulating substrate; a circuit formed on the surface of the aforementioned flexible insulating substrate; and an insulating layer covering the aforementioned circuit; wherein the aforementioned solder pad is formed on the surface of the aforementioned insulating layer and is electrically connected to the aforementioned circuit.
[0021] In the aforementioned method for mass transferring electronic components, the aforementioned plurality of electronic components are selected from one or more groups consisting of light emitting diodes, laser diodes and semiconductor components.
[0022] In the aforementioned another method for mass transfer of electronic components, the light emitted by the aforementioned multiple light emitting diodes is red light, and / or green light, and / or blue light, and / or yellow light, and / or white light, and / or infrared light, and / or ultraviolet light.
[0023] In the aforementioned method for mass transferring electronic components, the wavelengths of the aforementioned plurality of laser diodes are between 390 nanometers and 1700 nanometers.
[0024] The aforementioned method for mass transfer of electronic components, wherein the aforementioned plurality of semiconductor components are selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits and analog integrated circuits.
[0025] In the aforementioned method for mass transferring electronic components, the material of at least one electrode of each of the aforementioned plurality of electronic components and / or at least one pad of each of the aforementioned plurality of bonding regions is respectively metal, metal alloy or metal oxide.
[0026] The aforementioned method for mass transfer of electronic components further includes the step of forming a solder on at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate and / or on at least one electrode of each of the aforementioned multiple electronic components, so that at least one electrode of each of the aforementioned multiple electronic components and at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate are indirectly in contact with each other through the aforementioned solder, and the aforementioned solder is directly or indirectly heated by the aforementioned laser to obtain a heated solder, thereby allowing at least one electrode of each of the aforementioned multiple electronic components to be joined to at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate through the aforementioned heated solder.
[0027] In the aforementioned method for mass transferring electronic components, the wavelength of the aforementioned laser is between 190 nanometers and 11,000 nanometers.
[0028] The aforementioned method for mass transfer of electronic components, wherein the aforementioned temporary substrate can be removed by being simultaneously photolyzed or thermally decomposed when the aforementioned laser is irradiated toward the aforementioned temporary substrate from above the aforementioned temporary substrate, or can be directly peeled off and removed after at least one electrode of each of the aforementioned multiple electronic components is respectively bonded to at least one solder pad of each of the aforementioned multiple bonding areas of the aforementioned target substrate.
[0029] The aforementioned method for mass transfer of electronic components further includes the step of setting a transparent or semi-transparent medium layer on the aforementioned temporary substrate, wherein the aforementioned laser is irradiated from above the aforementioned multiple electronic components toward the aforementioned temporary substrate and each of the aforementioned multiple electronic component bodies through the aforementioned transparent or semi-transparent medium layer.
[0030] The present invention discloses another method for mass transfer of electronic components, characterized in that it includes the following steps: providing a carrier, the carrier is equipped with a heating device and / or an ultrasonic oscillation device; providing a target substrate, and placing the target substrate on the carrier, the target substrate has a first upper surface and a first lower surface relative to each other, and the first upper surface includes a plurality of bonding areas, and each of the plurality of bonding areas includes at least one welding pad, wherein when the heating device of the carrier is turned on, at least one welding pad of each of the plurality of bonding areas of the target substrate can be heated to 30°C to 300°C by the carrier, and when the ultrasonic oscillation device is turned on, at least one welding pad of each of the plurality of bonding areas of the target substrate can be oscillated by an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz; providing a temporary substrate above the target substrate, the temporary A plurality of electronic components are formed on a target substrate, each of the plurality of electronic components comprises an electronic component body and at least one electrode, the electronic component body has a second upper surface and a second lower surface relative to each other, the at least one electrode is formed on the second lower surface of the electronic component body and is electrically connected to the electronic component body, wherein the second lower surface of the plurality of electronic component bodies faces the first upper surface of the target substrate, and each of the plurality of electronic components is respectively aligned with each of the plurality of bonding areas of the target substrate, and at least one electrode of each of the plurality of electronic components is aligned with at least one welding pad of each of the plurality of bonding areas; a first laser is provided, and when the heating device of the carrier and / or the ultrasonic oscillation device are turned on, each of the plurality of electronic components is respectively welded by the laser on at least one welding pad of each of the plurality of bonding areas of the target substrate through the at least one electrode.
[0031] In the aforementioned another method for mass transferring electronic components, the target substrate is a semiconductor target substrate, a ceramic target substrate, a metal target substrate, a glass target substrate, a printed circuit board, or a flexible printed circuit board.
[0032] In the aforementioned method for mass transferring electronic components, the aforementioned flexible printed circuit board comprises: a flexible insulating substrate; a circuit formed on the surface of the aforementioned flexible insulating substrate; and an insulating layer covering the aforementioned circuit; wherein the aforementioned solder pad is formed on the surface of the aforementioned insulating layer and is electrically connected to the aforementioned circuit.
[0033] In the aforementioned another method for mass transferring electronic components, the aforementioned multiple electronic components are selected from one or more groups consisting of light emitting diodes, laser diodes and semiconductor components.
[0034] In the aforementioned another method for mass transfer of electronic components, the light emitted by the aforementioned multiple light emitting diodes is red light, and / or green light, and / or blue light, and / or yellow light, and / or white light, and / or infrared light, and / or ultraviolet light.
[0035] In the aforementioned another method for mass transferring electronic components, the wavelengths of the aforementioned multiple laser diodes are between 390 nanometers and 1700 nanometers.
[0036] In the aforementioned method for mass transfer of electronic components, the aforementioned plurality of semiconductor components are selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, and analog integrated circuits.
[0037] In the aforementioned another method for mass transferring electronic components, the material of at least one electrode of each of the aforementioned plurality of electronic components and / or at least one pad of each of the aforementioned plurality of bonding regions is respectively metal, metal alloy or metal oxide.
[0038] The aforementioned another method for mass transfer of electronic components further includes the step of forming a solder on at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate and / or on at least one electrode of each of the aforementioned multiple electronic components, so that at least one electrode of each of the aforementioned multiple electronic components and at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate are indirectly in contact with each other through the aforementioned solder, and the aforementioned solder is directly or indirectly heated by the aforementioned first laser to obtain a heated solder, thereby allowing at least one electrode of each of the aforementioned multiple electronic components to be joined to at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate through the aforementioned heated solder.
[0039] Another method for mass transfer of electronic components as mentioned above, wherein the temporary substrate can be irradiated from above by a second laser toward the temporary substrate after each of the aforementioned multiple electronic components is joined to at least one pad of each of the aforementioned multiple joining areas of the aforementioned target substrate by means of the aforementioned at least one electrode, so that the aforementioned temporary substrate is removed after being photolyzed or pyrolyzed, or the aforementioned temporary substrate is directly peeled off and removed.
[0040] In the aforementioned method for mass transferring electronic components, the wavelength of the first laser is between 190 nanometers and 11,000 nanometers.
[0041] In the aforementioned method for mass transferring electronic components, the wavelength of the second laser is between 190 nanometers and 11,000 nanometers.
[0042] The aforementioned another method for mass transfer of electronic components further includes the step of setting a transparent or semi-transparent medium layer on the first lower surface of the target substrate, wherein the aforementioned first laser is irradiated toward the aforementioned target substrate from below the aforementioned target substrate through the aforementioned transparent or semi-transparent medium layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0043] Figure 1A-1B The cross-sectional schematic diagram is an electronic component bonding process disclosed according to the first embodiment of the present invention.
[0044] Figure 2A-2B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed in the second embodiment of the present invention.
[0045] Figure 3A-3B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed in the third embodiment of the present invention.
[0046] Figures 4A to 4B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed in the fourth embodiment of the present invention.
[0047] Figures 5A-5B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed in the fifth embodiment of the present invention.
[0048] Figures 6A-6B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed in the sixth embodiment of the present invention.
[0049] Figures 7A-7B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed in the seventh embodiment of the present invention.
[0050] Figures 8A-8B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed in the eighth embodiment of the present invention.
[0051] Figures 9A to 9B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed in the ninth embodiment of the present invention.
[0052] Figures 10A to 10B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed according to the tenth embodiment of the present invention.
[0053] Figures 11A to 11B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed according to the eleventh embodiment of the present invention.
[0054] Figures 12A to 12B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed according to the twelfth embodiment of the present invention.
[0055] Figures 13A to 13BThe cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed according to the thirteenth embodiment of the present invention.
[0056] Figures 14A to 14B The cross-sectional schematic diagram is a schematic diagram of an electronic component bonding process disclosed according to a fourteenth embodiment of the present invention.
[0057] Figures 15A to 15B The cross-sectional schematic diagram is a schematic diagram of the electronic component bonding process disclosed according to the fifteenth embodiment of the present invention.
[0058] Figures 16A to 16B The cross-sectional schematic diagram is a schematic diagram of an electronic component bonding process disclosed according to the sixteenth embodiment of the present invention.
[0059] Figures 17A to 17B The cross-sectional schematic diagram is a schematic diagram of an electronic component bonding process disclosed according to the seventeenth embodiment of the present invention.
[0060] Figures 18A to 18C The cross-sectional schematic diagram is a mass transfer electronic component manufacturing process disclosed according to the eighteenth embodiment of the present invention.
[0061] Figures 19A to 19C The cross-sectional schematic diagram is a mass transfer electronic component manufacturing process disclosed according to the nineteenth embodiment of the present invention.
[0062] Figures 20A to 20D The cross-sectional schematic diagram is a mass transfer electronic component manufacturing process disclosed according to the twentyth embodiment of the present invention.
[0063] Figures 21A to 21D The cross-sectional schematic diagram is a mass transfer electronic component manufacturing process disclosed according to embodiment 21 of the present invention.
[0064] Among them, the simple description of the symbols in the accompanying drawings is as follows:
[0065] 10 Loading platform
[0066] 20 Heating equipment
[0067] 30 Ultrasonic oscillation equipment
[0068] 100 Target substrate
[0069] 100A First upper surface
[0070] 100B First lower surface
[0071] 110 Junction area
[0072] 120 Solder pad
[0073] 200 Electronic components
[0074] 210 Electronic components
[0075] 210A Second upper surface
[0076] 210B Second lower surface
[0077] 220 Electrode
[0078] 150, 250 thermal conductive material
[0079] 300 Solder
[0080] 300' Heated solder
[0081] 400 Transparent or semi-transparent dielectric layer
[0082] 500 Temporary substrate DETAILED DESCRIPTION
[0083] In order to make the description of the disclosed content of the present invention more detailed and complete, the following is an illustrative description of the implementation and specific embodiments of the present invention; however, this is not the only form of implementing or using the specific embodiments of the present invention. The various embodiments disclosed below can be combined or replaced with each other under beneficial circumstances, and other embodiments can be added to one embodiment without further recording or explanation.
[0084] In the following description, many specific details will be described in detail to enable the reader to fully understand the following embodiments. However, embodiments of the present invention can be practiced without these specific details. In other cases, well-known structures and devices are only schematically depicted in the figures to simplify the drawings.
[0085] Example
[0086] Embodiment 1
[0087] First, see Figure 1A .like Figure 1AAs shown, a carrier 10 is provided, the carrier 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and then a target substrate 100 is provided and placed on the carrier, and an electronic component 200 is provided. The target substrate 100 has a first upper surface 100A and a first lower surface 100B opposite to each other, and the first upper surface 100A includes a bonding area 110, and the bonding area includes at least one pad 120. The aforementioned electronic component 200 includes an electronic component body 210 and at least one electrode 220, the aforementioned electronic component body 210 has a second upper surface 210A and a second lower surface 210B relative to each other, the aforementioned at least one electrode 220 is formed on the second lower surface 210B of the aforementioned electronic component body 210 and is electrically connected to the aforementioned electronic component body 210, wherein the aforementioned electronic component 200 is aligned with the bonding area 110 of the aforementioned target substrate 100, and the aforementioned at least one electrode 220 is aligned with at least one solder pad 120 in the aforementioned bonding area 110.
[0088] According to the present embodiment, the target substrate 100 may be, for example but not limited to, a semiconductor substrate, a ceramic substrate, a metal substrate, a glass substrate, a printed circuit board, or a flexible printed circuit board.
[0089] According to the present embodiment, the target substrate 100 is illustrated as a flexible printed circuit board, and the flexible printed circuit board may include a flexible insulating substrate, a circuit formed on the surface of the flexible insulating substrate, and an insulating layer covering the circuit, wherein the solder pad is formed on the surface of the insulating layer and is electrically connected to the circuit.
[0090] According to this embodiment, the electronic component 200 is, for example, but not limited to, a light emitting diode, a laser diode, or a semiconductor component, wherein the light emitted by the light emitting diode is, for example, but not limited to, red light, green light, blue light, yellow light, white light, infrared light, or ultraviolet light; the wavelength of the laser diode is, for example, but not limited to, between 390 nanometers and 1700 nanometers; the semiconductor component is, for example, but not limited to, a processor, a memory integrated circuit, a micro-component integrated circuit, a logic integrated circuit, or an analog integrated circuit. The electronic component 200 of the first embodiment is illustrated by taking a light emitting diode as an example.
[0091] According to the present embodiment, the material of the at least one electrode 220 and / or the at least one bonding pad 120 may be, for example but not limited to, metal, metal alloy or metal oxide.
[0092] Next, see Figure 1A-1B .like Figure 1A-1BAs shown, a laser is provided, the wavelength of the laser is, for example but not limited to, between 190 nanometers and 11000 nanometers, and when the heating device 20 of the aforementioned carrier 10 and / or the aforementioned ultrasonic oscillation device 30 are turned on, the aforementioned laser is irradiated from the top of the aforementioned electronic component 200 toward the aforementioned electronic component body 210, so that the aforementioned laser can be concentrated on the second upper surface 210A of the aforementioned electronic component body 210, the inside of the aforementioned electronic component body 210, the second lower surface 210B of the aforementioned electronic component body 210, the aforementioned at least one electrode 220 or the aforementioned at least one welding pad 120, and a eutectic layer (not shown) is generated between the at least one electrode 220 of the aforementioned electronic component 200 and the at least one welding pad 120 of the bonding area 110 of the aforementioned target substrate 100, so that the aforementioned electronic component 200 is welded to the at least one welding pad 120 of the bonding area 110 of the aforementioned target substrate 100 by the aforementioned laser through the aforementioned at least one electrode 220. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 toward the aforementioned target substrate 100. At least one pad 120 of the joint area 110 of the target substrate 100 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0093] Embodiment 2
[0094] First, see Figure 2A .like Figure 2A As shown, a carrier platform 10 is provided, and the carrier platform 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and then a target substrate 100 is provided, and the target substrate 100 is placed on the carrier platform 10, and an electronic component 200 is provided. The structures of the target substrate 100 and the electronic component 200 are the same as those described in Example 1, and are not repeated here.
[0095] Next, see Figure 2A-2B .like Figure 2A-2BAs shown, a laser is provided, the wavelength of the laser is, for example but not limited to, between 190 nanometers and 11000 nanometers, and when the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the laser is irradiated toward the target substrate 100 from below the target substrate 100, so that the laser can be concentrated on the first upper surface 100A of the target substrate 100, the inside of the target substrate 100, the first lower surface 100B of the target substrate 100, the at least one welding pad 120 or the at least one electrode 220, and a eutectic layer (not shown) is generated between the at least one electrode 220 of the electronic component 200 and the at least one welding pad 120 of the bonding area 110 of the target substrate 100, so that the electronic component 200 is welded to the at least one welding pad 120 of the bonding area 110 of the target substrate 100 by the laser through the at least one electrode 220. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 toward the aforementioned target substrate 100. At least one pad 120 of the joint area 110 of the target substrate 100 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0096] Embodiment 3
[0097] First, see Figure 3A .like Figure 3A As shown, a carrier 10 is provided, the carrier 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and then a target substrate 100 is provided, and the target substrate 100 is placed on the carrier 10, and an electronic component 200 is provided, and the structures of the target substrate 100 and the electronic component 200 are the same as those described in the first embodiment, and are not repeated here. In addition, as Figure 3AAs shown, a solder 300 is further formed on the at least one pad 120 and / or the at least one electrode 220 , so that the at least one electrode 220 of the electronic component 200 and the at least one electrode 120 of the target substrate 100 are indirectly contacted via the solder 300 .
[0098] Next, see Figure 3A-3B .like Figure 3A-3B As shown, a laser is provided, the wavelength of the laser being, for example but not limited to, between 190 nanometers and 11000 nanometers, and when the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the laser is irradiated from above the electronic component 200 toward the electronic component body 210, so that the laser can be concentrated on the second upper surface 210A of the electronic component body 210, the inside of the electronic component body 210, the second lower surface 210B of the electronic component body 210, the at least one electrode 220, the solder 300 or the at least one pad 120, and the solder 300 is directly or indirectly heated by the laser to obtain a heated solder 300', so that the at least one electrode 220 of the electronic component 200 is bonded to the at least one pad 120 of the bonding area 110 of the target substrate 100 through the heated solder 300'. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 to the aforementioned target substrate 100. At least one pad 120 of the joint area 110 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200, the heated solder 300' and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0099] Embodiment 4
[0100] First, see Figure 4A .like Figure 4AAs shown, a carrier 10 is provided, the carrier 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and then a target substrate 100 is provided, and the target substrate 100 is placed on the carrier 10, and an electronic component 200 is provided, and the structures of the target substrate 100 and the electronic component 200 are the same as those described in the first embodiment, and are not repeated here. In addition, as Figure 4A As shown, a solder 300 is further formed on the at least one pad 120 and / or the at least one electrode 220 , so that the at least one electrode 220 of the electronic component 200 and the at least one electrode 120 of the target substrate 100 are indirectly contacted via the solder 300 .
[0101] Next, see Figures 4A to 4B .like Figures 4A to 4B As shown, a laser is provided, the wavelength of the laser is, for example but not limited to, between 190 nanometers and 11000 nanometers, and when the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the laser is irradiated toward the target substrate 100 from below the target substrate 100, so that the laser can be concentrated on the first upper surface 100A of the target substrate 100, the inside of the target substrate 100, the first lower surface 100B of the target substrate 100, the at least one pad 120, the solder 300 or the at least one electrode 220, and the solder 300 is directly or indirectly heated by the laser to obtain a heated solder 300', so that the at least one electrode 220 of the electronic component 200 is bonded to the at least one pad 120 of the bonding area 110 of the target substrate 100 through the heated solder 300'. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 to the aforementioned target substrate 100. At least one pad 120 of the joint area 110 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200, the heated solder 300' and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0102] Embodiment 5
[0103] See also Figures 5A-5B The electronic component bonding process disclosed in the fifth embodiment is generally similar to that disclosed in the first embodiment, and the only difference is that the fifth embodiment further includes disposing a transparent or semi-transparent dielectric layer 400 on the second upper surface 210A of the electronic component body 210, and the transparent or semi-transparent dielectric layer 400 and the target substrate 100 are sequentially placed on the carrier 10, and when the heating device 20 and / or the ultrasonic oscillation device 30 of the carrier 10 are turned on, the laser is irradiated from the upper side of the electronic component 200 toward the electronic component body 210 through the transparent or semi-transparent dielectric layer 400. The laser beam can be concentrated on the second upper surface 210A of the electronic component body 210, the inside of the electronic component body 210, the second lower surface 210B of the electronic component body 210, the at least one electrode 220 or the at least one welding pad 120, and a eutectic layer (not shown) is generated between the at least one electrode 220 of the electronic component 200 and the at least one welding pad 120 of the bonding area 110 of the target substrate 100, so that the electronic component 200 is welded on the at least one welding pad 120 of the bonding area 110 of the target substrate 100 by the laser beam through the at least one electrode 220. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 toward the aforementioned target substrate 100. At least one pad 120 of the joint area 110 of the target substrate 100 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0104] Embodiment 6
[0105] See also Figures 6A-6BThe electronic component bonding process disclosed in the sixth embodiment is substantially similar to that disclosed in the second embodiment, except that the sixth embodiment further includes the step of disposing a transparent or semi-transparent medium layer 400 on the first lower surface 100B of the target substrate 100, and the transparent or semi-transparent medium layer 400 and the target substrate 100 are sequentially placed on the carrier 10, and when the heating device 20 and / or the ultrasonic oscillation device 30 of the carrier 10 are turned on, the laser is irradiated from the bottom of the target substrate 100 toward the target substrate 100 through the transparent or semi-transparent medium layer 400. The laser beam is irradiated so that the laser beam can be concentrated on the first upper surface 100A of the target substrate 100, the inside of the target substrate 100, the first lower surface 100B of the target substrate 100, the at least one welding pad 120 or the at least one electrode 220, and a eutectic layer (not shown) is generated between the at least one electrode 220 of the electronic component 200 and the at least one welding pad 120 of the bonding area 110 of the target substrate 100, so that the electronic component 200 is welded on the at least one welding pad 120 of the bonding area 110 of the target substrate 100 by the laser beam through the at least one electrode 220. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 toward the aforementioned target substrate 100. At least one pad 120 of the joint area 110 of the target substrate 100 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0106] Embodiment 7
[0107] See also Figures 7A-7BThe electronic component bonding process disclosed in the seventh embodiment is generally similar to that disclosed in the third embodiment, and the only difference is that the seventh embodiment further includes disposing a transparent or semi-transparent dielectric layer 400 on the second upper surface 210A of the electronic component body 210, and the transparent or semi-transparent dielectric layer 400 and the target substrate 100 are sequentially placed on the carrier 10, and when the heating device 20 and / or the ultrasonic oscillation device 30 of the carrier 10 are turned on, the laser is transmitted from the upper side of the electronic component 200 toward the electronic component body through the transparent or semi-transparent dielectric layer 400. 210 is irradiated, and the laser can be concentrated on the second upper surface 210A of the electronic component body 210, the inside of the electronic component body 210, the second lower surface 210B of the electronic component body 210, the solder 300, the at least one electrode 220 or the at least one pad 120, and the solder 300 is directly or indirectly heated by the laser to obtain a heated solder 300', so that the at least one electrode 220 of the electronic component 200 is bonded to the at least one pad 120 of the bonding area 110 of the target substrate 100 through the heated solder 300'. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 toward the aforementioned target substrate 100. At least one pad 120 of the joint area 110 of the target substrate 100 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0108] Embodiment 8
[0109] See also Figures 8A-8BThe electronic component bonding process disclosed in the eighth embodiment is generally similar to that disclosed in the fourth embodiment, and the only difference is that the eighth embodiment further includes the step of disposing a transparent or semi-transparent medium layer 400 on the first lower surface 100B of the target substrate 100, and the transparent or semi-transparent medium layer 400 and the target substrate 100 are sequentially placed on the carrier 10, and when the heating device 20 and / or the ultrasonic oscillation device 30 of the carrier 10 are turned on, the laser is transmitted from the bottom of the target substrate 100 toward the target substrate through the transparent or semi-transparent medium layer 400. 100 irradiation, so that the aforementioned laser can be concentrated on the first upper surface 100A of the aforementioned target substrate 100, the inside of the aforementioned target substrate 100, the first lower surface 100B of the aforementioned target substrate 100, the aforementioned at least one welding pad 120, the aforementioned solder 300 or the aforementioned at least one electrode 220, and the aforementioned solder 300 is directly or indirectly heated by the aforementioned laser to obtain a heated solder 300', and then the at least one electrode 220 of the aforementioned electronic component 200 is joined to the at least one welding pad 120 of the joining area 110 of the aforementioned target substrate 100 through the aforementioned heated solder 300'. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 toward the aforementioned target substrate 100. At least one pad 120 of the joint area 110 of the target substrate 100 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0110] Embodiment 9
[0111] First, see Fig. 9A .like Fig. 9AAs shown, a carrier platform 10 is provided, and the carrier platform 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and then a target substrate 100 is provided, and the target substrate 100 is placed on the carrier platform 10, and an electronic component 200 and a solder 300 are provided. The structures of the target substrate 100, the electronic component 200, and the solder are the same as those described in Example 3, and are not repeated here.
[0112] Next, see Figures 9A to 9B .like Figures 9A to 9B As shown, a laser is provided, the wavelength of the laser being, for example but not limited to, between 190 nanometers and 11000 nanometers, and when the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the laser is directly irradiated on the solder 300 from the side, so that the solder 300 is directly heated by the laser to obtain a heated solder 300', thereby allowing at least one electrode 220 of the electronic component 200 to be bonded to at least one pad 120 of the bonding area 110 of the target substrate 100 through the heated solder 300'. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 toward the aforementioned target substrate 100. At least one pad 120 of the joint area 110 of the target substrate 100 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0113] Embodiment 10
[0114] First, see Fig. 10A .like Fig. 10AAs shown, a carrier 10 is provided, the carrier 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and then a target substrate 100 is provided, and the target substrate 100 is placed on the carrier 10, and an electronic component 200 is provided. The structure of the target substrate 100 is the same as that described in the first embodiment, and will not be repeated here. The structure of the electronic component 200 is generally similar to that described in the first embodiment, but the electronic component body 210 of the tenth embodiment further has a through hole (not marked) penetrating the second upper surface 210A and the second lower surface 210B, and the through hole (not marked) is filled with a heat conductive material 250, and the heat conductive material 250 is connected to at least one electrode 220 of the electronic component 200. Among them, the electronic component 200 is also aligned with the bonding area 110 of the target substrate 100, and the at least one electrode 220 is aligned with at least one pad 120 in the bonding area 110.
[0115] Next, see Figures 10A to 10B .like Figures 10A to 10BAs shown, a laser is provided, the wavelength of the laser is, for example but not limited to, between 190 nanometers and 11000 nanometers, and when the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the laser is irradiated from above the electronic component 200 toward the electronic component body 210, so that the laser can be concentrated on the upper surface (not marked) of the thermal conductive material 250, inside the thermal conductive material 250, the lower surface (not marked) of the thermal conductive material 250, the at least one electrode 220 or the at least one welding pad 120, and a eutectic layer (not shown) is generated between the at least one electrode 220 of the electronic component 200 and the at least one welding pad 120 of the bonding area 110 of the target substrate 100, so that the electronic component 200 is welded to the at least one welding pad 120 of the bonding area 110 of the target substrate 100 by the laser through the at least one electrode 220. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 toward the aforementioned target substrate 100. At least one pad 120 of the joint area 110 of the target substrate 100 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0116] Embodiment 11
[0117] First, see Fig.11A .like Fig.11AAs shown, a carrier 10 is provided, the carrier 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and then a target substrate 100 is provided, and the target substrate 100 is placed on the carrier 10, and an electronic component 200 is provided. The structure of the electronic component 200 is the same as that described in the first embodiment, and will not be repeated here. The structure of the target substrate 100 is generally similar to that described in the first embodiment, but the target substrate 100 of the eleventh embodiment further has a through hole (not marked) penetrating the first upper surface 100A and the first lower surface 100B, and the through hole (not marked) is filled with a heat conductive material 150, and the heat conductive material 150 is connected to at least one pad 120 in the bonding area 110 of the target substrate 100. Among them, the electronic component 200 is also aligned with the bonding area 110 of the target substrate 100, and the at least one electrode 220 is aligned with at least one pad 120 in the bonding area 110.
[0118] Next, see Figures 11A to 11B .like Figures 11A to 11BAs shown, a laser is provided, the wavelength of the laser is, for example but not limited to, between 190 nanometers and 11000 nanometers, and when the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the laser is irradiated toward the target substrate 100 from the bottom of the target substrate 100, so that the laser can be concentrated on the upper surface (not marked) of the thermal conductive material 150, inside the thermal conductive material 150, the lower surface (not marked) of the thermal conductive material 150, the at least one welding pad 120 or the at least one electrode 220, and a eutectic layer (not shown) is generated between the at least one electrode 220 of the electronic component 200 and the at least one welding pad 120 of the bonding area 110 of the target substrate 100, so that the electronic component 200 is welded to the at least one welding pad 120 of the bonding area 110 of the target substrate 100 by the laser through the at least one electrode 220. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 toward the aforementioned target substrate 100. At least one pad 120 of the joint area 110 of the target substrate 100 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0119] Embodiment 12
[0120] First, see Fig. 12A .like Fig. 12A As shown, a carrier 10 is provided, the carrier 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and then a target substrate 100 is provided, and the target substrate 100 is placed on the carrier 10, and an electronic component 200 is provided, and the structures of the target substrate 100 and the electronic component 200 are the same as those described in the tenth embodiment, and are not repeated here. In addition, as Fig. 12AAs shown, a solder 300 is further formed on the at least one pad 120 and / or the at least one electrode 220 , so that the at least one electrode 220 of the electronic component 200 and the at least one electrode 120 of the target substrate 100 are indirectly contacted via the solder 300 .
[0121] Next, see Figures 12A to 12B .like Figures 12A to 12B As shown, a laser is provided, the wavelength of the laser is, for example but not limited to, between 190 nanometers and 11000 nanometers, and when the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the laser is irradiated from above the electronic component 200 toward the electronic component body 210, and the laser can be concentrated on the upper surface (not marked) of the thermal conductive material 250, the inside of the thermal conductive material 250, the lower surface (not marked) of the thermal conductive material 250, the at least one electrode 220, the solder 300 or the at least one pad 120, and the solder 300 is directly or indirectly heated by the laser to obtain a heated solder 300', so that the at least one electrode 220 of the electronic component 200 is bonded to the at least one pad 120 of the bonding area 110 of the target substrate 100 through the heated solder 300'. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 to the aforementioned target substrate 100. At least one pad 120 of the joint area 110 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200, the heated solder 300' and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0122] Embodiment 13
[0123] First, see Fig.13A .like Fig.13AAs shown, a carrier 10 is provided, the carrier 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and then a target substrate 100 is provided, and the target substrate 100 is placed on the carrier 10, and an electronic component 200 is provided, and the structures of the target substrate 100 and the electronic component 200 are the same as those described in the eleventh embodiment, and are not repeated here. In addition, as Fig.13A As shown, a solder 300 is further formed on the at least one pad 120 and / or the at least one electrode 220 , so that the at least one electrode 220 of the electronic component 200 and the at least one electrode 120 of the target substrate 100 are indirectly contacted via the solder 300 .
[0124] Next, see Figures 13A to 13B .like Figures 13A to 13B As shown, a laser is provided, the wavelength of the laser is, for example but not limited to, between 190 nanometers and 11000 nanometers, and when the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the laser is irradiated toward the target substrate 100 from below the target substrate 100, and the laser can be concentrated on the upper surface (not marked) of the thermal conductive material 150, the inside of the thermal conductive material 150, the lower surface (not marked) of the thermal conductive material 150, the at least one welding pad 120 or the at least one electrode 220, and the solder 300 is directly or indirectly heated by the laser to obtain a heated solder 300', so that the at least one electrode 220 of the electronic component 200 is bonded to the at least one welding pad 120 of the bonding area 110 of the target substrate 100 through the heated solder 300'. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 to the aforementioned target substrate 100. At least one pad 120 of the joint area 110 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200, the heated solder 300' and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0125] Embodiment 14
[0126] See also Figures 14A to 14B The electronic component bonding process disclosed in the fourteenth embodiment is substantially similar to that disclosed in the tenth embodiment, except that the fourteenth embodiment further includes disposing a transparent or semi-transparent dielectric layer 400 on the second upper surface 210A of the electronic component body 210, and the transparent or semi-transparent dielectric layer 400 and the target substrate 100 are sequentially placed on the carrier 10, and when the heating device 20 and / or the ultrasonic oscillation device 30 of the carrier 10 are turned on, the laser is transmitted from the upper side of the electronic component 200 toward the target substrate 100 through the transparent or semi-transparent dielectric layer 400. The device body 210 is irradiated, and the aforementioned laser can be concentrated on the upper surface (not marked) of the aforementioned thermal conductive material 150, the inside of the aforementioned thermal conductive material 150, the lower surface (not marked) of the aforementioned thermal conductive material 150, the aforementioned at least one welding pad 120 or the aforementioned at least one electrode 220, and a eutectic layer (not shown) is generated between the at least one electrode 220 of the aforementioned electronic component 200 and the at least one welding pad 120 of the bonding area 110 of the aforementioned target substrate 100, thereby allowing the aforementioned electronic component 200 to be welded to the at least one welding pad 120 of the bonding area 110 of the aforementioned target substrate 100 by the aforementioned laser through the aforementioned at least one electrode 220. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 toward the aforementioned target substrate 100. At least one pad 120 of the joint area 110 of the target substrate 100 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0127] Embodiment 15
[0128] See also Figures 15A to 15BThe electronic component bonding process disclosed in the fifteenth embodiment is substantially similar to that disclosed in the eleventh embodiment, and the only difference is that the fifteenth embodiment further includes the step of disposing a transparent or semi-transparent medium layer 400 on the first lower surface 100B of the target substrate 100, and the transparent or semi-transparent medium layer 400 and the target substrate 100 are sequentially placed on the carrier 10, and when the heating device 20 and / or the ultrasonic oscillation device 30 of the carrier 10 are turned on, the laser is transmitted from the bottom of the target substrate 100 toward the target substrate through the transparent or semi-transparent medium layer 400. The board 100 is irradiated so that the aforementioned laser can be concentrated on the upper surface (not marked) of the aforementioned thermal conductive material 150, the inside of the aforementioned thermal conductive material 150, the lower surface (not marked) of the aforementioned thermal conductive material 150, the aforementioned at least one welding pad 120 or the aforementioned at least one electrode 220, and a eutectic layer (not shown) is generated between the at least one electrode 220 of the aforementioned electronic component 200 and the at least one welding pad 120 of the bonding area 110 of the aforementioned target substrate 100, thereby allowing the aforementioned electronic component 200 to be welded to the at least one welding pad 120 of the bonding area 110 of the aforementioned target substrate 100 by the aforementioned laser through the aforementioned at least one electrode 220. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 toward the aforementioned target substrate 100. At least one pad 120 of the joint area 110 of the target substrate 100 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0129] Embodiment 16
[0130] See also Figures 16A to 16BThe electronic component bonding process disclosed in the sixteenth embodiment is generally similar to that disclosed in the twelfth embodiment, and the only difference is that the sixteenth embodiment further includes disposing a transparent or semi-transparent medium layer 400 on the second upper surface 210A of the electronic component body 210, wherein when the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the laser is irradiated from the upper side of the electronic component 200 toward the electronic component body 210 through the transparent or semi-transparent medium layer 400, so that the laser The laser beam may be concentrated on the upper surface (not shown) of the thermally conductive material 250, the interior of the thermally conductive material 250, the lower surface (not shown) of the thermally conductive material 250, the at least one electrode 220, the solder 300 or the at least one pad 120, and the solder 300 may be directly or indirectly heated by the laser beam to obtain a heated solder 300', thereby allowing the at least one electrode 220 of the electronic component 200 to be bonded to the at least one pad 120 of the bonding area 110 of the target substrate 100 through the heated solder 300'. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 to the aforementioned target substrate 100. At least one pad 120 of the joint area 110 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200, the heated solder 300' and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0131] Embodiment 17
[0132] See also Figures 17A to 17BThe electronic component bonding process disclosed in the seventeenth embodiment is generally similar to that disclosed in the thirteenth embodiment, and the only difference is that the seventeenth embodiment further includes the step of disposing a transparent or semi-transparent medium layer 400 on the first lower surface 100B of the target substrate 100, wherein when the heating device 20 and / or the ultrasonic oscillation device 30 of the aforementioned carrier 10 are turned on, the aforementioned laser is irradiated toward the aforementioned target substrate 100 from the bottom of the aforementioned target substrate 100 through the aforementioned transparent or semi-transparent medium layer 400, and the aforementioned laser is The light can be concentrated on the upper surface (not marked) of the thermally conductive material 150, inside the thermally conductive material 150, the lower surface (not marked) of the thermally conductive material 150, the at least one soldering pad 120 or the at least one electrode 220, and the solder 300 is directly or indirectly heated by the laser to obtain a heated solder 300', thereby allowing the at least one electrode 220 of the electronic component 200 to be bonded to the at least one soldering pad 120 of the bonding area 110 of the target substrate 100 through the heated solder 300'. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 to the aforementioned target substrate 100. At least one pad 120 of the joint area 110 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between the electronic component 200, the heated solder 300' and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0133] Embodiment 18
[0134] The method for mass transferring electronic components disclosed in the eighteenth embodiment is based on Figures 18A to 18C Instructions are as follows.
[0135] First, if Fig.18AAs shown, a carrier 10 is provided, the carrier 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and then a target substrate 100 is provided and placed on the carrier 10. The target substrate 100 has a first upper surface 100A and a first lower surface 100B opposite to each other, and the first upper surface 100A includes a plurality of bonding areas 110, and each of the plurality of bonding areas 110 includes at least one pad 120. In addition, as Fig.18A As shown, a temporary substrate 500 is provided above the target substrate 100. A plurality of electronic components 200 are formed on the temporary substrate 500. Each of the plurality of electronic components 200 includes an electronic component body 210 and at least one electrode 220. The electronic component body 210 has a second upper surface 210A and a second lower surface 210B opposite to each other. The at least one electrode 220 is formed on the second lower surface 210B of the electronic component body 210 and is electrically connected to the electronic component body 210. The second lower surface 210B of the plurality of electronic component bodies 210 faces the first upper surface 100A of the target substrate 100. Each of the plurality of electronic components 200 is respectively aligned with each of the plurality of bonding areas 110 of the target substrate 100. The at least one electrode 220 of each of the plurality of electronic components 200 is aligned with at least one solder pad 120 of each of the plurality of bonding areas 110.
[0136] According to the present embodiment, the target substrate 100 may be, for example but not limited to, a semiconductor substrate, a ceramic substrate, a metal substrate, a glass substrate, a printed circuit board, or a flexible printed circuit board.
[0137] According to the present embodiment, the target substrate 100 is illustrated as a flexible printed circuit board, and the flexible printed circuit board may include a flexible insulating substrate, a circuit formed on the surface of the flexible insulating substrate, and an insulating layer covering the circuit, wherein the solder pad is formed on the surface of the insulating layer and is electrically connected to the circuit.
[0138] According to this embodiment, the aforementioned multiple electronic components 200 are, for example, but not limited to, light emitting diodes, laser diodes, or semiconductor components, wherein the light emitted by the aforementioned light emitting diodes is, for example, but not limited to, red light, green light, blue light, yellow light, white light, infrared light, or ultraviolet light; the wavelength of the aforementioned laser diode is, for example, but not limited to, between 390 nanometers and 1700 nanometers; the aforementioned semiconductor components are, for example, but not limited to, processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, or analog integrated circuits. The electronic components 200 of the first embodiment are illustrated by taking light emitting diodes as an example.
[0139] According to this embodiment, the material of at least one electrode 220 of each of the plurality of electronic components 200 and / or at least one pad 120 of each of the plurality of bonding regions 110 may be, for example but not limited to, metal, metal alloy or metal oxide.
[0140] Then, if Fig.18B As shown, a laser is provided, the wavelength of the laser is, for example but not limited to, between 190 nanometers and 11000 nanometers. When the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the laser is irradiated from above the temporary substrate 500 toward the temporary substrate 500 and each of the plurality of electronic component bodies 210, so that the laser can be concentrated on the second upper surface 210A of the plurality of electronic component bodies 210, inside the plurality of electronic component bodies 210, and the second lower surface 210 of the plurality of electronic component bodies 210. 210B, at least one electrode 220 of each of the aforementioned multiple electronic components 200 or at least one welding pad 120 of each of the aforementioned multiple bonding areas 110, thereby generating a eutectic layer (not shown) between the at least one electrode 220 of each of the aforementioned multiple electronic components 200 and the at least one welding pad 120 of each of the aforementioned multiple bonding areas 110 of the aforementioned target substrate 100, thereby allowing each of the aforementioned multiple electronic components 200 to be welded to the at least one welding pad 120 of each of the aforementioned multiple bonding areas 110 of the aforementioned target substrate 100 by the aforementioned laser through the aforementioned at least one electrode 220. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 to the aforementioned target substrate 100. At least one pad 120 of the joint area 110 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between at least one electrode 220 of each of the plurality of electronic components 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0141] After removing the temporary substrate 500, Fig.18CAs shown, the plurality of electronic components 200 are transferred in bulk from the temporary substrate 500 to the plurality of bonding areas 110 of the target substrate 100. The temporary substrate 500 can be removed by being photolyzed or pyrolyzed simultaneously when the laser is irradiated from above the temporary substrate 500, or can be directly peeled off and removed after at least one electrode 220 of each of the plurality of electronic components 200 is bonded to at least one pad 120 of each of the plurality of bonding areas 110 of the target substrate 100.
[0142] In addition, according to other embodiments of the present invention, the electronic component joining methods disclosed in embodiments five, ten, fourteen, etc. can also be applied to the method of mass transfer of electronic components disclosed in this embodiment as needed, so that each of the aforementioned multiple electronic components 200 is welded by the aforementioned laser on at least one welding pad 120 of each of the aforementioned multiple joining areas 110 of the aforementioned target substrate 100 through the aforementioned at least one electrode 220.
[0143] Embodiment 19
[0144] The method for mass transferring electronic components disclosed in the nineteenth embodiment is based on Figures 19A to 19C Instructions are as follows.
[0145] First, if Fig.19A As shown, a carrier 10, a target substrate 100 and a temporary substrate 500 as shown in the eighteenth embodiment are provided. The carrier 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and the target substrate 100 is placed on the carrier 10. The structures of the carrier 10, the target substrate 100 and the temporary substrate 500 are the same as those described in the eighteenth embodiment, and are not described in detail here. Fig.19A As shown, a solder 300 is further formed on the aforementioned plurality of pads 120 and / or the aforementioned plurality of electrodes 220 , so that at least one electrode 220 of each of the aforementioned plurality of electronic components 200 and at least one electrode 120 of each of the aforementioned plurality of bonding areas 110 of the aforementioned target substrate 100 are indirectly contacted through the aforementioned solder 300 .
[0146] Then, if Fig.19BAs shown, a laser is provided, the wavelength of the laser is, for example but not limited to, between 190 nanometers and 11000 nanometers. When the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the laser is irradiated from above the temporary substrate 500 toward the temporary substrate 500 and each of the plurality of electronic component bodies 210, so that the laser can be concentrated on the second upper surface 210A of the plurality of electronic component bodies 210, the interior of the plurality of electronic component bodies 210, and the plurality of electronic component bodies 210. The second lower surface 210B of the body 210, at least one electrode 220 of each of the aforementioned multiple electronic components 200, the aforementioned solder 300 or at least one pad 120 of each of the aforementioned multiple bonding areas 110, and the aforementioned solder 300 is directly or indirectly heated by the aforementioned laser to obtain a heated solder 300', so that the at least one electrode 220 of each of the aforementioned multiple electronic components 200 is bonded to the at least one pad 120 of each of the aforementioned multiple bonding areas 110 of the aforementioned target substrate 100 through the aforementioned heated solder 300'. The heating device 20 of the carrier 10 and the ultrasonic oscillating device 30 can be started and operated separately or simultaneously. When the heating device 20 of the carrier 10 is started and operated, at least one pad 120 of the bonding area 110 of the target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the ultrasonic oscillating device 30 is started and operated, the ultrasonic oscillating device 30 can be moved from the carrier 10 to the bonding area 110 of the target substrate 100. At least one welding pad 120 emits an ultrasonic wave with a power of 2W to 750W and a frequency of 15kHz to 2MHz, so that the at least one welding pad 120 is vibrated by the ultrasonic wave with a power of 2W to 750W and a frequency of 15kHz to 2MHz, thereby generating high-speed friction between at least one electrode 220 of each of the plurality of electronic components 200, the solder 300' to be heated and the surface of the welding pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0147] The laser of the nineteenth embodiment irradiates the temporary substrate 500 and each of the plurality of electronic component bodies 210 from above the temporary substrate 500, so that the laser can be concentrated on the second upper surface 210A of the plurality of electronic component bodies 210, the inside of the plurality of electronic component bodies 210, the second lower surface 210B of the plurality of electronic component bodies 210, at least one electrode 220 of each of the plurality of electronic components 200, the solder 300 or at least one pad 120 of each of the plurality of bonding areas 110, and the solder 300 is directly or indirectly heated by the laser to obtain a heated solder 300′. However, according to other embodiments of the present invention, the laser can also be directly irradiated on the solder 300 as needed, for example but not limited to irradiating the solder 300 in a manner substantially parallel to the target substrate 100 and / or the temporary substrate 500, and the solder 300 is directly heated by the laser to obtain a heated solder 300′, which will not be repeated here.
[0148] After removing the temporary substrate 500, Fig.19C As shown, the plurality of electronic components 200 are transferred in bulk from the temporary substrate 500 to the plurality of bonding areas 110 of the target substrate 100. The temporary substrate 500 can be removed by being photolyzed or pyrolyzed simultaneously when the laser is irradiated from above the temporary substrate 500, or can be directly peeled off and removed after at least one electrode 220 of each of the plurality of electronic components 200 is bonded to at least one pad 120 of each of the plurality of bonding areas 110 of the target substrate 100.
[0149] In addition, according to other embodiments of the present invention, the electronic component joining methods disclosed in embodiments seven, twelve, sixteen, etc. can also be applied to the method of mass transfer of electronic components disclosed in this embodiment as needed, so that each of the aforementioned multiple electronic components 200 is welded by the aforementioned laser on at least one welding pad 120 of each of the aforementioned multiple joining areas 110 of the aforementioned target substrate 100 through the aforementioned at least one electrode 220.
[0150] Embodiment 20
[0151] The method for mass transferring electronic components disclosed in the present embodiment 20 is based on Figures 20A to 20C Instructions are as follows.
[0152] First, if Fig. 20AAs shown, a carrier platform 10, a target substrate 100 and a temporary substrate 500 as shown in the eighteenth embodiment are provided, the aforementioned carrier platform 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, the target substrate 100 and the temporary substrate 500, and the aforementioned target substrate 100 is placed on the aforementioned carrier platform 10, and the structures of the carrier platform 10, the target substrate 100 and the temporary substrate 500 are the same as those described in the eighteenth embodiment, and are not repeated here.
[0153] Secondly, if Fig. 20B As shown, a first laser is provided, and the wavelength of the first laser is, for example but not limited to, between 190 nanometers and 11000 nanometers. When the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the first laser is irradiated from the bottom of the target substrate 100 toward the target substrate 100, and the first laser can be concentrated on the first upper surface 100A of the target substrate 100, the inside of the target substrate 100, the first lower surface 100B of the target substrate 100, each of the plurality of bonding At least one welding pad 120 of each of the aforementioned multiple bonding areas 110 or at least one electrode 220 of each of the aforementioned multiple electronic components 200, thereby generating a eutectic layer (not shown) between the at least one electrode 220 of each of the aforementioned multiple electronic components 200 and the at least one welding pad 120 of each of the aforementioned multiple bonding areas 110 of the aforementioned target substrate 100, thereby allowing each of the aforementioned multiple electronic components 200 to be welded to the at least one welding pad 120 of each of the aforementioned multiple bonding areas 110 of the aforementioned target substrate 100 by the aforementioned first laser through the aforementioned at least one electrode 220. The heating device 20 of the aforementioned carrier 10 and the aforementioned ultrasonic oscillating device 30 can be turned on and operated separately or simultaneously. When the heating device 20 of the aforementioned carrier 10 is turned on and operated, at least one pad 120 of the bonding area 110 of the aforementioned target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the aforementioned ultrasonic oscillating device 30 is turned on and operated, the aforementioned ultrasonic oscillating device 30 can be moved from the aforementioned carrier 10 to the aforementioned target substrate 100. At least one pad 120 of the joint area 110 emits an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, so that the at least one pad 120 is vibrated by the ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz, thereby generating high-speed friction between at least one electrode 220 of each of the plurality of electronic components 200 and the surface of the pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0154] Then, if Fig. 20CAs shown, a second laser is provided, the wavelength of the second laser is, for example but not limited to, between 190 nanometers and 11000 nanometers, so that the second laser irradiates the temporary substrate 500 from above the temporary substrate 500, so that the temporary substrate 500 is removed after photolysis or thermal decomposition, and as shown in FIG. Fig.20D As shown, the plurality of electronic components 200 are transferred in bulk from the temporary substrate 500 to the plurality of bonding regions 110 of the target substrate 100 .
[0155] In addition, in other embodiments of the present invention, the temporary substrate 500 may also be directly peeled off and removed after at least one electrode 220 of each of the plurality of electronic components 200 is respectively bonded to at least one pad 120 of each of the plurality of bonding regions 110 of the target substrate 100 .
[0156] In addition, according to other embodiments of the present invention, the electronic component joining methods disclosed in embodiments six, eleven, fifteen, etc. can also be applied to the method of mass transfer of electronic components disclosed in this embodiment as needed, so that each of the aforementioned multiple electronic components 200 is welded by the aforementioned laser on at least one welding pad 120 of each of the aforementioned multiple joining areas 110 of the aforementioned target substrate 100 through the aforementioned at least one electrode 220.
[0157] Embodiment 21
[0158] First, if Fig.21A As shown, a carrier 10, a target substrate 100 and a temporary substrate 500 as shown in the eighteenth embodiment are provided. The carrier 10 is equipped with a heating device 20 and / or an ultrasonic oscillation device 30, and the target substrate 100 and the temporary substrate 500 are placed on the carrier 10. The structures of the carrier 10, the target substrate 100 and the temporary substrate 500 are the same as those described in the eighteenth embodiment, and are not described in detail here. In addition, Fig.21A As shown, a solder 300 is further formed on the aforementioned plurality of pads 120 and / or the aforementioned plurality of electrodes 220 , so that at least one electrode 220 of each of the aforementioned plurality of electronic components 200 and at least one electrode 120 of each of the aforementioned plurality of bonding areas 110 of the aforementioned target substrate 100 are indirectly contacted through the aforementioned solder 300 .
[0159] Then, if Fig. 21BAs shown, a first laser is provided, and the wavelength of the first laser is, for example but not limited to, between 190 nanometers and 11000 nanometers. When the heating device 20 of the carrier 10 and / or the ultrasonic oscillation device 30 are turned on, the first laser is irradiated toward the target substrate 100 from below the target substrate 100, and the first laser is concentrated on the first upper surface 100A of the target substrate 100, the inside of the target substrate 100, the first lower surface 100B of the target substrate 100, at least one pad 120 of each of the plurality of bonding areas 110, the solder 300, or at least one electrode 220 of each of the plurality of electronic components 200, and the solder 300 is directly or indirectly heated by the laser to obtain a heated solder 300', so that the at least one electrode 220 of each of the plurality of electronic components 200 is bonded to the at least one pad 120 of each of the plurality of bonding areas 110 of the target substrate 100 through the heated solder 300'. The heating device 20 of the carrier 10 and the ultrasonic oscillating device 30 can be started and operated separately or simultaneously. When the heating device 20 of the carrier 10 is started and operated, at least one pad 120 of the bonding area 110 of the target substrate 100 can be heated to 30°C to 300°C, thereby effectively reducing the critical time for achieving good laser welding, for example but not limited to, from 14ms to 8ms; and when the ultrasonic oscillating device 30 is started and operated, the ultrasonic oscillating device 30 can be moved from the carrier 10 to the bonding area 110 of the target substrate 100. At least one welding pad 120 emits an ultrasonic wave with a power of 2W to 750W and a frequency of 15kHz to 2MHz, so that the at least one welding pad 120 is vibrated by the ultrasonic wave with a power of 2W to 750W and a frequency of 15kHz to 2MHz, thereby generating high-speed friction between at least one electrode 220 of each of the plurality of electronic components 200, the heated solder 300' and the surface of the welding pad 120 to assist the laser welding process, thereby effectively reducing the limit time for achieving good laser welding, for example but not limited to reducing it from 14ms to below 7ms.
[0160] The first laser of the twenty-first embodiment irradiates the target substrate 100 from below the target substrate 100, and the first laser can be concentrated on the first upper surface 100A of the target substrate 100, the inside of the target substrate 100, the first lower surface 100B of the target substrate 100, at least one pad 120 of each of the plurality of bonding areas 110, the solder 300 or at least one electrode 220 of each of the plurality of electronic components 200, and the solder 300 is directly or indirectly heated by the first laser to obtain a heated solder 300′. However, according to other embodiments of the present invention, the first laser can also be directly irradiated to the solder 300 as needed, for example but not limited to irradiating the solder 300 in a manner substantially parallel to the target substrate 100 and / or the temporary substrate 500, and the solder 300 is directly heated by the first laser to obtain a heated solder 300′, which will not be repeated herein.
[0161] Then, if Fig. 21C As shown, a second laser is provided, the wavelength of the second laser is, for example but not limited to, between 190 nanometers and 11000 nanometers, so that the second laser irradiates the temporary substrate 500 from above the temporary substrate 500, so that the temporary substrate 500 is removed after photolysis or thermal decomposition, and as shown in FIG. Fig.21D As shown, the plurality of electronic components 200 are transferred in bulk from the temporary substrate 500 to the plurality of bonding regions 110 of the target substrate 100 .
[0162] In addition, in other embodiments of the present invention, the temporary substrate 500 may also be directly peeled off and removed after at least one electrode 220 of each of the plurality of electronic components 200 is respectively bonded to at least one pad 120 of each of the plurality of bonding regions 110 of the target substrate 100 .
[0163] In addition, according to other embodiments of the present invention, the electronic component joining methods disclosed in embodiments eight, thirteen, seventeen, etc. can also be applied to the method of mass transfer of electronic components disclosed in this embodiment as needed, so that each of the aforementioned multiple electronic components 200 is welded by the aforementioned laser on at least one welding pad 120 of each of the aforementioned multiple joining areas 110 of the aforementioned target substrate 100 through the aforementioned at least one electrode 220.
[0164] Although the present invention has been disclosed as above by way of embodiments, it is not intended to limit the present invention. Anyone skilled in the art may make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be determined by the definition of the appended claims.
Claims
1. A method for bonding electronic components, Features The following steps are involved: A carrier is provided, the carrier is equipped with a heating device and / or an ultrasonic oscillation device; a target substrate is provided, and the target substrate is placed on the carrier, the target substrate has a first upper surface and a first lower surface opposite to each other, and the first upper surface includes a bonding area, and the bonding area includes at least one welding pad, wherein when the heating device of the carrier is turned on, the at least one welding pad of the bonding area of the target substrate can be heated to 30°C to 300°C, and when the ultrasonic oscillation device is turned on, the bonding area of the target substrate is heated to 30°C to 300°C. At least one pad can be vibrated by an ultrasonic wave with a power between 2W and 750W and a frequency between 15kHz and 2MHz; an electronic component is provided, the electronic component comprising an electronic component body and at least one electrode, the electronic component body having a second upper surface and a second lower surface opposite to each other, the at least one electrode being formed on the second lower surface of the electronic component body and being electrically connected to the electronic component body, wherein the electronic component is aligned with a bonding area of the target substrate, and the at least one electrode is aligned with at least one pad in the bonding area; and A laser is provided, and when the heating device of the aforementioned carrier and / or the aforementioned ultrasonic oscillation device are turned on, the aforementioned electronic component is welded to at least one pad of the bonding area of the aforementioned target substrate by the aforementioned laser through the aforementioned at least one electrode.
2. The method for bonding electronic components as claimed in claim 1, wherein the target substrate is a semiconductor substrate, a ceramic substrate, a metal substrate, a glass substrate, a printed circuit board, or a flexible printed circuit board.
3. The method for joining electronic components as claimed in claim 2, wherein the flexible printed circuit board include: A soft insulating substrate; A circuit formed on the surface of the aforementioned flexible insulating substrate; as well as an insulating layer covering the aforementioned circuit; The soldering pad is formed on the surface of the insulating layer and is electrically connected to the circuit.
4. The method for bonding electronic components as claimed in claim 1, wherein the electronic components are selected from a group consisting of light emitting diodes, laser diodes and semiconductor components. 5 . The method for bonding electronic components as claimed in claim 4 , wherein the light emitted by the light emitting diode is red light, green light, blue light, yellow light, white light, infrared light or ultraviolet light. 6 . The method for bonding electronic components as claimed in claim 4 , wherein the wavelength of the laser diode is between 390 nanometers and 1700 nanometers.
7. The method for bonding electronic components as described in claim 4, wherein the aforementioned semiconductor component is selected from a group consisting of a processor, a memory integrated circuit, a microcomponent integrated circuit, a logic integrated circuit and an analog integrated circuit. 8 . The method for bonding electronic components as claimed in claim 1 , wherein the material of the at least one electrode and / or the at least one soldering pad is metal, metal alloy or metal oxide respectively.
9. The method for joining electronic components as described in claim 1 further includes the step of forming a solder on the at least one soldering pad and / or the at least one electrode, so that the at least one electrode of the electronic component is indirectly in contact with the at least one electrode of the target substrate through the solder, and the solder is directly or indirectly heated by the laser to obtain a heated solder, thereby joining the at least one electrode of the electronic component to the at least one soldering pad of the joining area of the target substrate through the heated solder.
10. The method for bonding electronic components as claimed in claim 1, wherein the wavelength of the laser is between 190 nanometers and 11000 nanometers.
11. The method for joining electronic components as described in any one of claims 1 to 10 further comprises the step of disposing a transparent or semi-transparent medium layer on the second upper surface of the electronic component body, wherein the laser is irradiated from above the electronic component toward the electronic component body through the transparent or semi-transparent medium layer.
12. The method for joining electronic components as described in any one of claims 1 to 10 further comprises the step of disposing a transparent or semi-transparent medium layer on the first lower surface of the target substrate, wherein the laser is irradiated toward the target substrate from below the target substrate through the transparent or semi-transparent medium layer.
13. A method for mass transfer of electronic components, Features The following steps are involved: A carrier is provided, the carrier is equipped with a heating device and / or an ultrasonic oscillation device; a target substrate is provided, and the target substrate is placed on the carrier, the target substrate has a first upper surface and a first lower surface opposite to each other, and the first upper surface includes a plurality of bonding areas, and each of the plurality of bonding areas includes at least one welding pad, wherein when the heating device of the carrier is turned on, at least one welding pad of each of the plurality of bonding areas of the target substrate can be heated to 30°C to 300°C, and when the ultrasonic oscillation device is turned on, at least one welding pad of the bonding area of the target substrate can be heated to 30°C to 300°C, and when the ultrasonic oscillation device is turned on, at least one welding pad of the bonding area of the target substrate can be heated to 30°C to 300°C. Ultrasonic oscillations of kilohertz to 2 megahertz; Providing a temporary substrate above the target substrate, with a plurality of electronic components formed on the temporary substrate, each of the plurality of electronic components comprising an electronic component body and at least one electrode, the electronic component body having a second upper surface and a second lower surface opposite to each other, the at least one electrode being formed on the second lower surface of the electronic component body and electrically connected to the electronic component body, wherein the second lower surfaces of the plurality of electronic component bodies face the first upper surface of the target substrate, and each of the plurality of electronic components is respectively aligned with each of the plurality of bonding areas of the target substrate, and at least one electrode of each of the plurality of electronic components is aligned with at least one pad of each of the plurality of bonding areas; and A laser is provided, and when the heating device of the aforementioned carrier and / or the aforementioned ultrasonic oscillation device are turned on, each of the aforementioned multiple electronic components is welded by the aforementioned laser to at least one welding pad of each of the aforementioned multiple bonding areas of the aforementioned target substrate through the aforementioned at least one electrode. 14 . The method for mass transferring electronic components as claimed in claim 13 , wherein the target substrate is a semiconductor substrate, a ceramic substrate, a metal substrate, a glass substrate, a printed circuit board, or a flexible printed circuit board.
15. The method for mass transfer of electronic components as claimed in claim 14, wherein the flexible printed circuit board include: A soft insulating substrate; A circuit formed on the surface of the aforementioned flexible insulating substrate; as well as an insulating layer covering the aforementioned circuit; The soldering pad is formed on the surface of the insulating layer and is electrically connected to the circuit. 16 . The method for mass transferring electronic components as claimed in claim 13 , wherein the plurality of electronic components are selected from one or more of the group consisting of light emitting diodes, laser diodes and semiconductor components.
17. The method for mass transfer of electronic components as claimed in claim 16, wherein the light emitted by the plurality of light emitting diodes is red light, and / or green light, and / or blue light, and / or yellow light, and / or white light, and / or infrared light, and / or ultraviolet light.
18. The method for mass transfer of electronic components as claimed in claim 16, wherein the wavelengths of the plurality of laser diodes are between 390 nanometers and 1700 nanometers.
19. The method for mass transfer of electronic components as claimed in claim 16, wherein the plurality of semiconductor components are selected from one or more of the group consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits and analog integrated circuits.
20. The method for mass transferring electronic components as claimed in claim 13, wherein the material of at least one electrode of each of the plurality of electronic components and / or at least one pad of each of the plurality of bonding regions is metal, metal alloy or metal oxide.
21. The method for mass transfer of electronic components as described in claim 13 further includes the step of forming a solder on at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate and / or on at least one electrode of each of the aforementioned multiple electronic components, so that at least one electrode of each of the aforementioned multiple electronic components and at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate are indirectly in contact with each other through the aforementioned solder, and the aforementioned solder is directly or indirectly heated by the aforementioned laser to obtain a heated solder, thereby allowing at least one electrode of each of the aforementioned multiple electronic components to be joined to at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate through the aforementioned heated solder.
22. The method for mass transfer of electronic components as claimed in claim 13, wherein the wavelength of the laser is between 190 nanometers and 11000 nanometers.
23. A method for mass transfer of electronic components as described in claim 13, wherein the temporary substrate can be removed by being simultaneously photolyzed or thermally decomposed when the laser is irradiated toward the temporary substrate from above the temporary substrate, or can be directly peeled off and removed after at least one electrode of each of the plurality of electronic components is respectively bonded to at least one pad of each of the plurality of bonding areas of the target substrate.
24. The method for mass transfer of electronic components as described in any one of claims 13 to 23 further comprises the step of setting a transparent or semi-transparent medium layer on the aforementioned temporary substrate, wherein the aforementioned laser is irradiated toward the aforementioned temporary substrate and each of the aforementioned multiple electronic component bodies from above the aforementioned multiple electronic components through the aforementioned transparent or semi-transparent medium layer.
25. A method for mass transfer of electronic components, Features The following steps are involved: A carrier is provided, wherein the carrier is equipped with a heating device and / or an ultrasonic oscillation device; a target substrate is provided, and the target substrate is placed on the carrier, wherein the target substrate has a first upper surface and a first lower surface opposite to each other, and the first upper surface includes a plurality of bonding areas, and each of the plurality of bonding areas includes at least one welding pad, wherein when the heating device of the carrier is turned on, at least one welding pad of each of the plurality of bonding areas of the target substrate can be heated to 30° C. to 300° C. by the carrier, and when the ultrasonic oscillation device is turned on, at least one welding pad of each of the plurality of bonding areas of the target substrate can be oscillated by an ultrasonic wave having a power of 2 W to 750 W and a frequency of 15 kHz to 2 MHz; Providing a temporary substrate above the target substrate, with a plurality of electronic components formed on the temporary substrate, each of the plurality of electronic components comprising an electronic component body and at least one electrode, the electronic component body having a second upper surface and a second lower surface opposite to each other, the at least one electrode being formed on the second lower surface of the electronic component body and being electrically connected to the electronic component body, wherein the second lower surfaces of the plurality of electronic component bodies face the first upper surface of the target substrate, and each of the plurality of electronic components is respectively aligned with each of the plurality of bonding areas of the target substrate, and at least one electrode of each of the plurality of electronic components is aligned with at least one pad of each of the plurality of bonding areas; A first laser is provided, and when the heating device of the aforementioned carrier and / or the aforementioned ultrasonic oscillation device are turned on, each of the aforementioned multiple electronic components is welded by the aforementioned first laser on at least one welding pad of each of the aforementioned multiple joining areas of the aforementioned target substrate through the aforementioned at least one electrode. 26 . The method for mass transferring electronic components as claimed in claim 25 , wherein the target substrate is a semiconductor target substrate, a ceramic target substrate, a metal target substrate, a glass target substrate, a printed circuit board, or a flexible printed circuit board.
27. The method for mass transfer of electronic components as claimed in claim 26, wherein the flexible printed circuit board include: A soft insulating substrate; A circuit formed on the surface of the aforementioned flexible insulating substrate; as well as an insulating layer covering the aforementioned circuit; The soldering pad is formed on the surface of the insulating layer and is electrically connected to the circuit.
28. The method for mass transferring electronic components as claimed in claim 25, wherein the plurality of electronic components are selected from one or more of the group consisting of light emitting diodes, laser diodes and semiconductor components.
29. The method for mass transfer of electronic components as claimed in claim 28, wherein the light emitted by the plurality of light emitting diodes is red light, and / or green light, and / or blue light, and / or yellow light, and / or white light, and / or infrared light, and / or ultraviolet light.
30. The method for mass transfer of electronic components as claimed in claim 28, wherein the wavelengths of the plurality of laser diodes are between 390 nanometers and 1700 nanometers.
31. The method for mass transfer of electronic components as described in claim 28, wherein the plurality of semiconductor components are selected from one or more groups consisting of processors, memory integrated circuits, micro-component integrated circuits, logic integrated circuits, and analog integrated circuits.
32. The method for mass transferring electronic components as claimed in claim 25, wherein the material of at least one electrode of each of the plurality of electronic components and / or at least one pad of each of the plurality of bonding regions is metal, metal alloy or metal oxide.
33. The method for mass transfer of electronic components as described in claim 25 further includes the step of forming a solder on at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate and / or on at least one electrode of each of the aforementioned multiple electronic components, so that at least one electrode of each of the aforementioned multiple electronic components and at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate are indirectly in contact with each other through the aforementioned solder, and the aforementioned solder is directly or indirectly heated by the aforementioned first laser to obtain a heated solder, thereby allowing at least one electrode of each of the aforementioned multiple electronic components to be joined to at least one soldering pad of each of the aforementioned multiple joining areas of the aforementioned target substrate through the aforementioned heated solder.
34. A method for mass transfer of electronic components as described in claim 25, wherein the temporary substrate can be removed by photolysis or thermal decomposition, or the temporary substrate can be directly peeled off and removed by irradiating the temporary substrate from above with a second laser after each of the plurality of electronic components is bonded to at least one pad of each of the plurality of bonding areas of the target substrate by means of the at least one electrode.
35. The method for mass transfer of electronic components as claimed in claim 25, wherein the wavelength of the first laser is between 190 nanometers and 11000 nanometers.
36. The method for mass transfer of electronic components as claimed in claim 34, wherein the wavelength of the second laser is between 190 nanometers and 11000 nanometers.
37. The method for mass transfer of electronic components as described in any one of claims 25 to 36 further includes the step of setting a transparent or semi-transparent medium layer on the first lower surface of the target substrate, wherein the first laser is irradiated toward the target substrate from below the target substrate through the transparent or semi-transparent medium layer.
Citation Information
Patent Citations
Laser bonded devices, laser bonding tools, and related methods
CN113828909A
Micro-LED laser processing system
CN115837518A
Manufacturing method of micro light-emitting element array, transfer carrier, and micro light-emitting element array
TW201916189A
Die bonder
TWI722801B