Electronic device and manufacturing method thereof
A two-step cutting method with a protective layer and distinct cutting conditions addresses the cracking issue in low dielectric constant material layers, enhancing the structural stability and reliability of electronic devices.
Patent Information
- Application Number
- CN202410186853.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-30
- Filing Date
- 2024-02-20
- Publication Date
- 2024-12-03
AI Technical Summary
Low dielectric constant material layers in electronic devices are prone to chipping or cracking during the cutting process, affecting the structural stability and reliability of the devices.
A manufacturing method involving two distinct cutting steps with different conditions is employed, where a protective layer is first applied to the circuit structure, followed by a first cutting step to expose the base layer, and a second cutting step to form crystal grains, reducing the likelihood of cracking.
The method enhances the structural stability and reliability of electronic devices by minimizing cracking and chipping of dielectric layers, improving bonding quality and reducing the risk of defects during the cutting process.
Smart Images

Figure CN119069425A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to an electronic device and a manufacturing method thereof, and in particular to an electronic device and a manufacturing method thereof which can improve the structural stability and reliability thereof. Background Art
[0002] During the manufacturing process of electronic devices, the insulating layer or dielectric layer is cut through the cutting area. According to the development trend of electronic devices, low dielectric constant material layers are beneficial for electronic devices to exhibit electronic properties such as lower leakage current. However, the material properties of the low dielectric constant material layer itself are relatively fragile, so when the low dielectric constant material layer is cut, the low dielectric constant material layer is prone to chipping or cracking defects. The chipped or cracked dielectric layer will affect the structural stability and reliability of the electronic device after cutting.
[0003] In view of this, the art needs to continue to study the manufacturing method of electronic devices to improve the problem that the dielectric constant material layer in the cut electronic devices is prone to cracking or breaking, which helps to further enhance the structural stability and reliability of the electronic devices after cutting. Summary of the invention
[0004] The purpose of the present invention is to provide an electronic device and a manufacturing method thereof, which is conducive to improving the problem that the dielectric constant material layer in the electronic device is prone to fragmentation or cracking after cutting, thereby further enhancing the structural stability and reliability of the electronic device after cutting.
[0005] According to some embodiments of the present invention, the present invention provides a method for manufacturing an electronic device. First, a base layer is provided, the base layer including a circuit structure disposed on one side of the base layer. Second, a protective layer is attached to the circuit structure. Next, a first cutting step is performed to cut the protective layer to expose a portion of the base layer. After that, a second cutting step is performed to cut the base layer to form a plurality of crystal grains, wherein the first cutting step is different from the second cutting step.
[0006] According to some other embodiments of the present invention, an electronic device provided by the present invention includes a chip, a protective layer, a packaging layer and a redistribution structure layer. The chip has an active surface and a first side surface connected to the active surface. The protective layer is arranged on the active surface of the chip, and the protective layer has a second side surface. The packaging layer surrounds the chip and the protective layer. The redistribution structure layer is arranged on the packaging layer and the protective layer, and the redistribution structure layer is electrically connected to the chip. Wherein, the roughness of the first side surface is different from the roughness of the second side surface. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figure 1 , Figure 1A , Figure 1B, Figure 1C A schematic diagram of a process of forming an electronic device according to an embodiment of the present invention is shown respectively. Figure 1 , Figure 1A , Figure 1B , Figure 1C The component structures are shown in cross-sectional schematic diagrams. Figure 1C A cross-sectional schematic diagram of a modified embodiment of a component structure of an electronic device is shown.
[0008] Figure 2 , Figure 2A , Figure 2B , Figure 2C A process schematic diagram of a modified embodiment of a method for forming an electronic device according to the present invention is respectively shown. Figure 2 , Figure 2A , Figure 2B , Figure 2C The component structures are shown in cross-sectional schematic diagrams.
[0009] Figure 3 , Figure 3A , Figure 3B , Figure 3C , Figure 3D , Figure 3E The process diagrams of an embodiment of a method for forming an electronic device by sequentially packaging and manufacturing a redistribution structure layer according to the present invention are respectively shown. Figure 3 , Figure 3A , Figure 3B , Figure 3C , Figure 3D , Figure 3E The component structures are shown in cross-sectional schematic diagrams.
[0010] Figure 4 Plot corresponding to Figure 3A A cross-sectional schematic diagram of a modified embodiment of the packaging structure in FIG.
[0011] Figure 5 Plot corresponding to Figure 3E A cross-sectional schematic diagram of a variant embodiment of the electronic device in FIG.
[0012] Description of reference numerals: 100 ~ electronic device; 101 ~ electronic device; 102 ~ laser; 103 ~ diamond knife; 104 ~ laser; 105 ~ laser; 110 ~ base layer; 111 ~ first side; 112 ~ second side; 113 ~ cutting line area; 114 ~ groove; 115 ~ first side; 116 ~ surface; 117 ~ third side; 118 ~ opening; 118A ~ notch; 120 ~ circuit structure; 1 21~metal layer; 121A~metal pad; 122~insulating layer; 122A~through hole; 123~insulating layer; 123A~through hole; 124~side surface; 130~protective layer; 130T~top surface; 131~second side surface; 132~through hole; 141~wafer; 142~crystal grain; 143~crystal grain; 144~electronic unit; 145~bottom filling layer; 150~encapsulation layer; 150-1~first side ; 150-2 ~ second side; 150' ~ packaging material; 151 ~ packaging structure; 152 ~ second carrier; 153 ~ debonding layer; 160 ~ first redistribution structure layer; 160' ~ second redistribution structure layer; 161 ~ first metal layer; 161' ~ first metal layer; 161A ~ cavity; 161A' ~ seed layer; 162 ~ second metal layer; 162' ~ second metal layer; 162B ~ top surface; 16 3~first insulating layer; 163'~second insulating layer; 163A~recess; 163B~top surface; 170~joining element; 171~solder ball; 172~solder ball; D~distance; G~step difference; G1~step difference; O~opening; P1~junction point; P2~junction point; T~thickness; W1~width; W118~width; W114~width; W2~width; θ1~angle; θ2~angle; θ3~angle. DETAILED DESCRIPTION
[0013] The present invention can be understood by referring to the following detailed description in conjunction with the accompanying drawings. It should be noted that in order to make it easier for readers to understand and for the simplicity of the drawings, the multiple drawings in the present invention only depict a portion of the electronic device, and specific elements in the drawings are not drawn according to the actual scale. In addition, the number and size of each element in the figure are only for illustration and are not intended to limit the scope of the present invention.
[0014] Certain words are used throughout the specification and the appended claims to refer to specific components. It should be understood by those skilled in the art that electronic equipment manufacturers may refer to the same components by different names. The present invention is not intended to distinguish between components that have the same function but different names.
[0015] In the present specification and claims, the words “including” and “comprising” are open-ended words, and thus should be interpreted as meaning “including but not limited to…”.
[0016] It should be understood that when an element or film layer is referred to as being "on" or "connected to" another element or film layer, it may be directly on or directly connected to the other element or layer, or there may be an intervening element or film layer between the two (indirect case). Conversely, when an element is referred to as being "directly" "on" or "directly connected to" another element or film layer, there may be no intervening element or film layer between the two.
[0017] In some embodiments of the present invention, terms such as "connection" and "interconnection" related to bonding and connection, unless otherwise defined, may refer to two structures being in direct contact, or may also refer to two structures not being in direct contact, wherein another structure is disposed between the two structures. Such terms related to bonding and connection may also include situations where both structures are movable, or where both structures are fixed. In addition, the terms "electrically connected" or "electrically coupled" include any direct and indirect electrical connection means.
[0018] Although the terms first, second, third, etc. can be used to describe a variety of components, the components are not limited to these terms. These terms are only used to distinguish a single component from other components in the specification. The same terms may not be used in the claims, but may be replaced by first, second, third, etc. according to the order in which the components are declared in the claims. Therefore, in the specification of the present invention, the first component may be the second component in the claims.
[0019] The term “disposed on” is only used to facilitate description of the manufacturing method and does not limit the process steps or sequence.
[0020] In the present invention specification, roughness is defined as: on the surface of a given component, such as a stud, observed by a scanning electron microscope (SEM), the peaks and valleys of the surface undulations can be seen to have a distance difference of 0.15 microns to 1 micron. The measurement of roughness determination may include using a scanning electron microscope, a transmission electron microscope (TEM), etc., to observe the surface undulations at the same appropriate magnification. And the undulations are compared by capturing a unit length (e.g., 10 microns). Here, "appropriate magnification" means that at least one surface can see at least 10 undulating peaks under this magnification. According to some embodiments, the stud can be used to contact the solder ball, but is not limited to this.
[0021] It should be noted that the following embodiments may replace, reorganize, or mix the technical features in several different embodiments to complete other embodiments without departing from the spirit of the present invention.
[0022] Figure 1 , Figure 1A , Figure 1B , Figure 1C A schematic diagram of a process of forming an electronic device according to an embodiment of the present invention is shown respectively. Figure 1 , Figure 1A , Figure 1B , Figure 1C The component structures are shown in cross-sectional schematic diagrams. Figure 1CA cross-sectional schematic diagram of a modified embodiment of the component structure of an electronic device is depicted. In the present invention, the electronic device can be applied to a power module, a semiconductor packaging device, a display device, a light-emitting device, a backlight device, an antenna device, a sensing device, a splicing device or a flexible / bendable device, but is not limited thereto. The electronic device may also include semiconductor grains, or a functional stack formed by staggered stacking of multiple metal layers (copper layers and seed layers) and multiple insulating layers, such as a redistribution layer (RDL), but the present invention is not limited thereto. "Flexible / bendable" here means that the material can be bent, bent, folded, rolled, flexed, stretched and / or other similar deformations to represent at least one of the above possible deformation modes, and "flexible / bendable" is not limited to the above deformation modes. The antenna device may be a liquid crystal type antenna device or a non-liquid crystal type antenna device. In the present invention, the electronic components may include passive components, active components or a combination thereof, such as capacitors, resistors, inductors, varactor diodes, variable capacitors, filters, diodes, transistors, sensors, micro-electromechanical system components (MEMS), liquid crystal chips, etc., but are not limited thereto. The diode may include a light-emitting diode or a non-light-emitting diode. The diode may include a PN junction diode, a PIN diode or a constant current diode. The light-emitting diode may include, for example, an organic light emitting diode (OLED), a sub-millimeter light-emitting diode (mini LED), a micro LED, a quantum dot light-emitting diode (quantum dot LED), a fluorescence diode, a phosphor diode or other suitable materials, or a combination thereof, but is not limited thereto. The electronic component may include a die or a light emitting diode die, which may be a crystal made of silicon (Si), gallium arsenide (GaAs), gallium nitride (GaN), silicon carbide (SiC), sapphire or a glass substrate, but is not limited thereto. In another embodiment, the die may include a semiconductor package component, such as a chip size package (CSP) component, but is not limited thereto.In another embodiment, the chip can be any flip chip bonding component, such as integrated circuits (IC), transistors, thyristors, valves, thin film transistors, capacitors, inductors, variable capacitors, filters, resistors, diodes, micro-electromechanical system components (MEMS), liquid crystal chips, etc., but not limited thereto. In addition, the grains can include, for example, diodes or semiconductor chips (semiconductor dies), but not limited thereto. The chip can be a known good die (KGD), which can include various electronic components, such as (but not limited to) wires, transistors, circuit boards, etc. Adjacent chips can have different functions from each other, such as integrated circuits, RFICs, D-RAMs, but not limited thereto. If the electronic device is used in packaging, for example, it can be applied to packaging such as wafer-level package (WLP) and panel-level packaging (PLP), and may include chip-first or chip last RDL first packaging methods, but the present invention is not limited thereto. It should be noted that the electronic device may be any of the aforementioned arrangements and combinations, but the present invention is not limited thereto. The various embodiments of the present invention illustrate a combination of a plurality of electronic units, a rewiring structure, a metal layer, an insulating layer, a connector, a bonding element, and an input / output bonding pad (I / O pad) encapsulated by a packaging insulating layer, wherein the electronic unit of the present invention may be an electronic device of a fan-out package, but the present invention is not limited thereto. The following will illustrate the content of the present invention by taking a packaging device as an example of an electronic device, but it is not limited thereto. The dielectric material of the rewiring structure layer may include an organic dielectric material, an inorganic dielectric material, or a combination of the above dielectric materials that can be used for packaging, but it is not limited thereto. The organic dielectric material may include, for example, polybenzoxazole (PBO), benzocyclobutene (BCB), acrylic, ABF (Ajinomoto build-up film) material, polyimide (PI), polyamide, other suitable materials, or combinations thereof, etc., which may be used for encapsulation of organic dielectric materials, but the present invention is not limited thereto.The inorganic dielectric material may include, for example, silicon oxide, silicon nitride, aluminum oxide, siloxane, other suitable materials, or combinations thereof, which may be used for packaging, but the present invention is not limited thereto.
[0023] Figures 1 to 1C The X direction and the Y direction represent the plane direction of the base layer 110, and the Z direction is the normal direction of the base layer 110, or can be regarded as the stacking direction of the material layers of the multiple metal layers and the insulating layer in the base layer 110, and the X direction and the Y direction are respectively perpendicular to the Z direction. Please refer to Figure 1 The manufacturing method of the electronic device of the present invention includes first providing a base layer 110. The base layer 110 may include a wafer, and the wafer may include, for example, a silicon base material, a doped silicon material, a gallium nitride (GaN) material or other semiconductor material, glass, ceramic, organic material, a combination of the above or other suitable materials, but the present invention is not limited thereto. The base layer 110 has two sides arranged opposite to each other, such as a first side 111 and a second side 112 opposite to the first side 111. According to some embodiments, a circuit structure 120 is arranged on the first side 111 of the base layer 110, and the side of the base layer 110 having the circuit structure 120 may be called an active surface. Therefore, the wafer 141 may include the base layer 110 and the circuit structure 120 arranged on one side of the base layer 110. The circuit structure 120 may be provided with a cutting line region 113. According to some embodiments, a cutting step may be performed in the cutting line region 113 by some suitable cutting methods to separate the base layer 110 and the circuit structure 120, thereby obtaining a plurality of grains.
[0024] The circuit structure 120 may include at least one metal layer 121, at least one insulating layer 122, and at least one insulating layer 123. The metal layer 121 may also include a metal pad 121A located on the top layer and used as an input / output pad (I / O pad). According to some embodiments, the circuit structure 120 may include a transistor, for example, including a gate, a drain, and a source, but not limited thereto. For example, the transistor may be a metal oxide semiconductor field effect transistor (MOSFET). In other words, the die may output or receive a signal, such as an output voltage or current, through the circuit structure 120. According to some embodiments, the metal layer may be used as an alignment mark to facilitate alignment in a cutting step, a wafer transfer step, or other steps. According to some embodiments, stacked metal layers or metal layers overlapping each other may be disposed adjacent to a cutting area, and metal layers overlapping each other may be used as a retaining wall, for example, to buffer the stress generated in the cutting step and reduce the risk of cracking of the circuit structure, but not limited thereto. Figure 1 , two metal layers 121 and a metal pad 121A are respectively embedded in three insulating layers 123, but the present invention is not limited thereto. An insulating layer 122 is provided between adjacent metal layers 121 to form a circuit structure 120. The metal layer 121 may include copper, nickel, gold, titanium, molybdenum, aluminum, tantalum or other suitable materials, but the present invention is not limited thereto. The materials of the insulating layer 122 and the insulating layer 123 may be the same or different, and may include organic dielectric materials, inorganic dielectric materials, or a combination of the above dielectric materials that can be used for packaging, but the present invention is not limited thereto. For details, please refer to the above description. The insulating layer 122 and the insulating layer 123 may include porous materials with low dielectric constants, such as porous materials with dielectric constants lower than 2.4, porous materials with dielectric constants lower than 2.0, and porous materials with dielectric constants lower than 1.9, but the present invention is not limited thereto. The metal pad 121A used as an input and output terminal bonding pad can be electrically connected to the metal layer 121, and serves as an input and output terminal for the metal layer 121 to be electrically connected to the outside. According to some embodiments, the metal layer 121 may be disposed in the cutting line region 113. The formation process of the circuit structure 120 may include processes such as lithography, etching, cleaning, impurity diffusion, ion implantation, and thin film deposition, and the metal layers 121 and / or metal pads 121A in different layers may be electrically connected to each other through the through holes 122A or the through holes 123A, but the present invention is not limited thereto.
[0025] Secondly, if Figure 1As shown, a protective layer 130 is formed on the circuit structure 120, for example, the protective layer 130 can be formed on the circuit structure 120 by attachment, deposition or coating, but it is not limited thereto. For example, the protective layer 130 can completely cover the surface of the circuit structure 120. For example, the protective layer 130 can cover the surface of the circuit structure 120 along the topography of the circuit structure 120. The protective layer 130 can, for example, include an organic material with a filler. The particle size of the filler can be 0.05 micrometers (micrometer, μm) to 10 micrometers. The thickness of the protective layer 130 can be 10 micrometers to 30 micrometers. The organic material can, for example, include photosensitive polyimide (PSPI), polyimide, epoxy resin (epoxy), polymer (polymer), a combination of the above or other suitable materials, but the present invention is not limited thereto. The coefficient of thermal expansion (CTE) of the protective layer 130 may be, for example, 20 ppm / °C to 40 ppm / °C, the Young's modulus of the protective layer 130 may be, for example, 3 GPa to 15 GPa, and the tensile strength of the protective layer 130 may be, for example, 50 MPa to 110 MPa, but the present invention is not limited thereto. According to some embodiments, along the Z direction, the thickness of the protective layer 130 may be greater than the thickness of the circuit structure 120. For example, in a same cross-sectional view, the maximum thickness of the protective layer 130 may be greater than the maximum thickness of the circuit structure 120. According to some embodiments, a ratio of the thickness of the protective layer 130 to the thickness of the circuit structure 120 may be greater than or equal to 1.1 and less than or equal to 2.5, or according to some embodiments, a ratio of the thickness of the protective layer 130 to the thickness of the circuit structure 120 may be greater than or equal to 1.3 and less than or equal to 2.3. By forming the protective layer 130 on the circuit structure 120 through the above design, the damage to the circuit structure 120 caused by the cutting step or other steps can be reduced, but the invention is not limited thereto. The thickness referred to in the present invention can be measured along the normal direction of the base layer 110, that is, the Z direction indicated in the figure. In addition, the X direction and the Y direction are respectively perpendicular to the Z direction, and the X direction is perpendicular to the Y direction.
[0026] Please continue to refer to Figure 1A, and then patterning the protective layer 130 to expose the side surface of the circuit structure 120 and a portion of the base layer 110. In detail, the first cutting step is performed after the surface of the circuit structure 120 is covered with the protective layer 130. The first cutting step can cut the protective layer 130 from the cutting line area 113, cut the insulating layer 122 and the insulating layer 123 of the circuit structure 120, and cut a portion of the base layer 110. After the first cutting step, a portion of the base layer 110 located in the cutting line area 113 can be exposed, and the exposed portion of the base layer 110 can form a groove 114. According to some embodiments of the present invention, the first cutting step can cut the protective layer 130 into an inclined second side 131, cut the circuit structure 120 into a continuously inclined side 124, and cut the exposed part of the base layer 110 into a groove 114 with a curved concave surface 116, and form a curved edge (edge) adjacent to the circuit structure 120, called the first side 115, wherein the first side 115 is connected to the concave surface 116, wherein the first side 115 can have a wavy profile. The second side 131 of the protective layer 130 forms a continuous inclined surface with the inclined side 124 of the insulating layer 122 in the circuit structure 120. According to some embodiments of the present invention, the first cutting step can reduce the possibility of forming undesirable cracks or fractures on the side 124 of the exposed insulating layer 122. The wavy in the present invention means that the line connecting the position of each point is not a straight line, for example, the line connecting each point is not along the X direction, the Y direction, and the Z direction.
[0027] Please continue to refer to Figure 1B , after the first cutting step, a second cutting step can be performed. The second cutting step can be performed from Figure 1A The base layer 110 is cut along the cutting line area 113 in the groove 114 formed by the first cutting step, and the base layer 110 is completely cut to form an opening 118. That is, the base layer 110, the circuit structure 120 disposed on the base layer 110, and the protection layer 130 disposed on the circuit structure are disconnected through the singulation step to form a plurality of dies 142, such as Figure 1CAs shown. According to some embodiments of the present invention, the opening 118 is completely located in the groove 114, so the width W118 of the opening 118 along the X direction is smaller than the width W114 of the groove 114 along the X direction. According to other embodiments of the present invention, the second cutting step can cut the base layer 110 into a continuous third side 117, and the third side 117 is connected to the second side 131 via the first side 115 and the side 124, which can be defined as a side edge of the die 142. According to some embodiments, the step of forming the circuit structure 120 can define at least one opening O through a patterning process, so that the protective layer 130 attached to the surface of the circuit structure 120 extends into the opening O. Through the above design, the contact area between the protective layer 130 and the circuit structure 120 can be increased, thereby improving the bonding quality, but it is not limited to this. Figure 1C As shown, each insulating layer 122 / 123 of the circuit structure 120 contacting the protection layer 130 may have an arc-shaped corner, which can reduce the risk of cracking of the protection layer 130 or improve the interface bonding quality, but is not limited thereto.
[0028] Different cutting conditions may be used to perform the first cutting step and the second cutting step, respectively. That is, in some embodiments of the present invention, the first cutting step is different from the second cutting step, so the roughness of the first side 115, the side 124, and the second side 131 formed by the first cutting step may be different from the roughness of the third side 117 formed by the second cutting step. According to some embodiments of the present invention, the cutting conditions of the first cutting step may be milder than the cutting conditions of the second cutting step, thereby reducing the possibility of forming undesirable cracking or breaking defects on the side 124 of the exposed circuit structure 120. The cutting steps referred to in the present invention are different, for example, the first cutting step may include a laser 102, and the second cutting step may include physical cutting, such as cutting with a diamond knife (saw) 103, but the present invention is not limited thereto. Alternatively, the laser 102 used for cutting may have different wavelengths or widths, for example, a laser with a wavelength of 355 nanometers (nanometer, nm) may be used to cut the protective layer 130.
[0029] The laser cutting method is advantageous for cutting the insulating layer 122 under low cutting stress conditions, thereby reducing the possibility of forming undesirable cracking or breaking defects on the exposed side 124 of the insulating layer 122. The knife cutting method is advantageous for cutting the base layer 110 having a higher material strength than the insulating layer 122. According to some embodiments of the present invention, the roughness of the third side 117 of the base layer 110 formed by the second cutting step may be smaller than the roughness of the side 124, the second side 131, and the first side 115 of the base layer 110 formed by the first cutting step. The width W118 of the opening 118 being smaller than the width W114 of the groove 114 is advantageous for reducing the probability of affecting the protective layer 130 and the circuit structure 120 when cutting the base layer 110, for example, not affecting the profile formed by the first side 115, the side 124, and the second side 131 through the first cutting step.
[0030] The circuit structure 120 may have an inclined side surface 124, indicating that there is an angle θ1 between the side surface 124 of the circuit structure 120 and the normal direction (i.e., the Z direction) of the substrate layer 110. For example, in a cross-sectional schematic diagram, the side surface 124 contacts a junction point P1 on the surface of the substrate layer 110, and an extension line perpendicular to the surface of the substrate layer 110 is drawn along the normal direction (i.e., the Z direction) of the substrate layer 110, and the extension line passes through the junction point P1, then the angle between the extension line and the side surface 124 is the angle θ1. According to some embodiments of the present invention, θ1 may be 5° to 45°, that is, 5°≤θ1≤45°. There is another angle θ2 between the third side surface 117 of the substrate layer 110 and the normal direction of the substrate layer 110. For example, in a cross-sectional view, the third side surface 117 of the base layer 110 and the bottom surface 112 of the base layer 110 have a junction point P2, and an extension line perpendicular to the surface of the base layer 110 is drawn along the normal direction of the base layer 110 (i.e., the Z direction), and the extension line passes through the junction point P2, then the angle between the extension line and the third side surface 117 is the angle θ2. In some embodiments of the present invention, θ2 may be smaller than θ1, that is, θ2<θ1.
[0031] Figure 2 , Figure 2A , Figure 2B , Figure 2C A process schematic diagram of a modified embodiment of a method for forming an electronic device according to the present invention is respectively shown. Figure 2 , Figure 2A , Figure 2B , Figure 2C The component structures are shown in cross-sectional schematic diagrams. Figure 2 , Figure 2A , Figure 2B , Figure 2C The components shown in the figure roughly correspond to the axial direction. Figure 1 , Figure 1A , Figure 1B , Figure 1C The components shown in FIG. are axially related, so similar components are labeled with the same reference numerals. Figure 2 The method for manufacturing an electronic device of the present invention includes first providing a substrate layer 110. The substrate layer 110 may include a wafer, and the wafer may include, for example, a silicon-based material, a doped silicon material, a gallium nitride material or other semiconductor material, glass, ceramic, organic material, a combination of the above or other suitable materials, but the present invention is not limited thereto. The substrate layer 110 has two sides arranged opposite to each other, for example, a first side 111 as an active surface and an opposite second side 112. According to some embodiments, a circuit structure 120 is arranged on one side of the substrate layer 110. Figure 2 In the figure, two groups of circuit structures 120 are respectively arranged on the first side 111 of the base layer 110, but the present invention is not limited thereto. A cutting line area 113 is arranged between the circuit structures 120 to define the cutting positions of adjacent circuit structures 120. According to some embodiments, a cutting step can be performed in the cutting line area 113 by some suitable cutting method to separate the base layer 110 and the circuit structure 120, thereby obtaining a plurality of dies.
[0032] The circuit structure 120 may include at least one metal layer 121, at least one insulating layer 122, and at least one insulating layer 123. The metal layer 121 may further include a metal pad 121A located at the top layer and used as an input / output terminal bonding pad. Figure 2 The figure shows two metal layers 121 and one metal pad 121A embedded in three insulating layers 123, but the invention is not limited thereto. The details of the metal layer 121, the insulating layer 122, or the insulating layer 123 are as mentioned above, so they will not be described in detail. Figures 2 to 2C It is shown that the cutting line region 113 only passes through the insulating layer 123 of the circuit structure 120 but does not pass through the metal layer 121 .
[0033] Secondly, if Figure 2AAs shown, the first cutting step can be performed without the presence of a protective layer. The first cutting step can cut the insulating layer 122 and the insulating layer 123 of the circuit structure 120 from the cutting line area 113 and completely expose part of the insulating layer 122, cut part of the base layer 110 and expose part of the base layer 110 located in the cutting line area 113 to form a groove 114 and a first side 115. For example, the circuit structure 120 can be cut by laser. The groove 114 has a width W1 along the X direction. According to some embodiments of the present invention, the first cutting step can cut the circuit structure 120 into a continuously inclined side 124, and cut the exposed part of the base layer 110 into a groove 114 with a curved concave surface 116, and form a curved edge adjacent to the metal layer 121, which is called the first side 115, wherein the first side 115 can have a wavy profile. According to some embodiments of the present invention, the first cutting step can reduce the possibility of forming undesirable cracking or breaking defects on the exposed side 124 of the insulating layer 122.
[0034] Please continue to refer to Figure 2B Attach the protection layer 130 to the circuit structure 120 and the exposed portion of the curved concave surface 116 of the base layer 110, and make Figure 2A The middle groove 114 is reduced to a notch 118A, and the notch 118A has a width W2 along the X direction. The protective layer 130 can completely fill the groove 114 in a conformal manner, and cover the upper surface of the circuit structure 120 and the continuously inclined side surface 124 to protect the circuit structure 120 on the base layer 110, and cover the curved concave surface 116 exposed by a portion of the base layer 110. For example, the protective layer 130 can cover the surface of the circuit structure 120 and the exposed curved concave surface 116 of the portion of the base layer 110 along the topography of the circuit structure 120. Please refer to the above for details of the protective layer 130, so it will not be repeated.
[0035] After the circuit structure 120 is covered with the protection layer 130, a second cutting step may be continued in the presence of the protection layer 130. The second cutting step may continue to cut the protection layer 130 and the base layer 110 along the cutting line area 113 from the notch 118A, and completely cut the protection layer 130 and the base layer 110, so that the multiple groups of circuit structures 120 disposed on the first side 111 of the base layer 110 are separated from each other through the singulation step, and a plurality of die 143 are formed. Figure 2CAs shown. According to some embodiments of the present invention, the notch 118A is completely located in the groove 114, so the width W2 of the notch 118A along the X direction is less than the width W1 of the groove 114 along the X direction. According to some embodiments of the present invention, the second cutting step can cut the base layer 110 into the third side 117, and cut the protective layer 130 into the second side 131, and the third side 117 is connected to the second side 131. According to other embodiments of the present invention, the second cutting step reduces the influence of the second cutting step on the contours formed by the first side 115 and the side 124 through the first cutting step in the presence of the protective layer 130, but is not limited thereto.
[0036] Different cutting conditions may be used to perform the first cutting step and the second cutting step, respectively. That is, according to some embodiments of the present invention, the first cutting step is different from the second cutting step, for example, the wavelength or energy of the laser 104 used in the first cutting step may be different from the wavelength or energy of the laser 105 used in the second cutting step. For example, the laser 104 used in the first cutting step may be a laser with a wavelength of 540 nanometers, a wavelength of 1075 nanometers, or other suitable wavelengths, and the laser 105 used in the second cutting step may be a laser with a wavelength of 355 nanometers or a wavelength less than 450 nanometers, but the present invention is not limited thereto. Through the above-mentioned step design, cutting debris can be reduced, but it is not limited thereto.
[0037] The circuit structure 120 after cutting may have an inclined side surface 124, indicating that there is an angle θ1 between the side surface 124 of the circuit structure 120 and the normal direction of the substrate layer 110, that is, the Z direction. According to some embodiments of the present invention, θ1 may be 5° to 45°, that is, 5°≤θ1≤45°. For example, in a cross-sectional schematic diagram, the side surface 124 contacts a junction P1 on the surface of the substrate layer 110, and an extension line perpendicular to the surface of the substrate layer 110 is drawn along the normal direction of the substrate layer 110 (that is, the Z direction), and the extension line passes through the junction P1, then the angle between the extension line and the side surface 124 is the angle θ1. The protective layer 130 after cutting may have an inclined second side surface 131, wherein the second side surface 131 may have a stepped profile, that is, in a cross-sectional schematic diagram, as shown Figure 2CAs shown by the dotted line, at least one section of the contour has an extension direction different from that of other contours. Through the above design, the surface area of the protective layer 130 is increased, for example, the bonding force between the protective layer 130 and the subsequent film layer can be improved, but it is not limited to this. The cut base layer 110 can have an inclined third side 117, and there is an angle θ2 between the third side 117 and the normal direction of the base layer 110. For example, in a cross-sectional schematic diagram, the third side 117 of the base layer 110 and the bottom surface 112 of the base layer 110 have an intersection point P2, and an extension line perpendicular to the surface of the base layer 110 is drawn along the normal direction of the base layer 110 (i.e., the Z direction), and the extension line passes through the intersection point P2, then the angle between the extension line and the third side 117 is the angle θ2. In some embodiments of the present invention, θ2 can be less than θ1, that is, θ2<θ1. Through the above cutting method, cutting debris can be reduced, or through the above design, the risk of other film layers being broken in subsequent packaging steps can be reduced.
[0038] The plurality of dies 142 or 143 obtained by the aforementioned method of forming an electronic device may further undergo the steps of packaging and making a redistribution structure layer. The dies 142 or 143 may respectively include a base layer 110, a circuit structure 120 disposed on one side of the active surface of the base layer 110, and a protective layer 130. Figure 3 , Figure 3A , Figure 3B , Figure 3C , Figure 3D , Figure 3E A schematic diagram of a process of connecting a packaging structure and manufacturing a redistribution structure layer to form an electronic device according to an embodiment of the present invention is respectively shown. Figure 3 , Figure 3A , Figure 3B , Figure 3C , Figure 3D , Figure 3E The device structures are shown in cross-sectional schematic diagrams, and the crystal grain 142 is used as an example for illustration, but the present invention is not limited thereto. Figure 3As shown, a packaging material 150' is provided to package a die 142 located on a first carrier (not shown). For example, at least one die 142 is transferred to the first carrier, and the packaging material 150' is provided to package or surround at least one die 142. After the packaging material 150' is cured (or solidified), a packaging layer 150 is formed to cover and directly contact the first carrier and the die 142. According to some embodiments, the packaging layer 150 surrounds the first carrier and the die 142, so that the die 142 is buried in the packaging layer 150. For example, when the die 142 is transferred to the first carrier, the active surface of the die can be directed toward the first carrier. In other words, the protective layer 130 can be arranged toward the first carrier, and then the packaging layer 150 is formed to cover the die 142. In other words, the thickness of the packaging layer 150 can be greater than the thickness of the die 142 to form a packaging structure 151. For example, in the cross-sectional view, the packaging layer 150 is arranged in a manner that directly contacts at least two sides of the die 142 to form a packaging structure 151. Before being provided, the packaging layer 150 can be a soft film-like, powdery or liquid packaging material, for example, it can include a prepolymerized epoxy resin (Epoxy Molding Compound, EMC) packaging material, but the present invention is not limited thereto. After the prepolymerized epoxy resin packaging material is matured, it can become a matured packaging layer 150, but the present invention is not limited thereto. The packaging layer 150 that directly contacts the corresponding component is, for example, helpful in preventing moisture or oxygen from contacting or penetrating the corresponding component, that is, it can improve the weather resistance of the electronic device, but the present invention is not limited thereto.
[0039] Continue, as Figure 3 As shown, after the die 142 is packaged with the packaging layer 150, the packaging structure 151 can be turned over so that Figure 3The protective layer 130 shown in the figure is arranged upward, that is, after the packaging structure 151 is turned over, the packaging layer 150 exposes the protective layer 130. The step of turning over the packaging structure 151 may include the step of providing a second carrier 152 on a side of the packaging structure 151 relative to the first carrier and the step of removing the first carrier, as needed. For example, in some embodiments, the step of adding the second carrier 152 and turning over the first carrier may be performed before the step of removing the first carrier. The first carrier and the second carrier 152 may be respectively adjacent to one side of the packaging structure, and the second carrier 152 is further provided with a release layer 153, so that the packaging layer 150 is temporarily fixed on the second carrier 152 via the release layer 153. After the step of removing the first carrier, the protective layer 130 may be exposed. Then, a portion of the protective layer 130 is removed through an appropriate patterning step to form a through hole 132, and the metal pad 121A of the metal layer 121 covered by the protective layer 130 and the insulating layer 123 is exposed through the through hole 132. The method of patterning the protective layer 130 includes photolithography, laser, a combination of the above or other suitable methods, but is not limited thereto. According to some embodiments, the step of patterning the protective layer 130 to expose the metal pad 121A can be performed before the singulation step, but is not limited thereto.
[0040] Next, a redistribution structure layer may be provided to electrically connect the metal pad 121A of the circuit structure 120 in the die 142. The method for forming the redistribution structure layer includes providing at least one insulating layer and at least one conductive layer stacked, including processes such as yellow light, etching, surface treatment, laser, and electroplating. The surface treatment includes roughening the surface of the insulating layer or the conductive layer to improve its bonding ability. The following example illustrates the method for forming the redistribution structure layer, but the present invention is not limited thereto.
[0041] like Figure 3AAs shown, in some embodiments, for example, a first metal layer 161 is provided to electrically connect metal pads 121A of the die 142 that serve as input and output bonding pads. For example, a whole seed layer (not shown) may be formed on the surface of the protective layer 130 and the packaging layer 150 by sputtering or deposition. The material of the seed layer may include titanium, copper, tantalum, nickel, a combination of the above or other suitable materials. Then, a photoresist material (not shown) is formed on the whole seed layer. Then, after the photoresist material is patterned by exposure and development (not shown), a conductive layer may be formed by electroplating or chemical plating. The material may include copper, nickel, gold, titanium, molybdenum, aluminum or other suitable materials. After removing the photoresist or etching, the first metal layer 161 is formed. Further, the first metal layer 161 may be a composite layer of a seed layer and a conductive layer. By forming the seed layer between the conductive layer and the protective layer 130, the bonding ability between the first metal layer 161 and the protective layer 130 or between the first metal layer 161 and the packaging layer 150 can be improved. Repeat the above steps to form the second metal layer 162 on the first metal layer 161. The photoresist material may be an attached dry film, or a positive photoresist material or a negative photoresist material patterned by exposure and development to help define the pattern of the first metal layer 161 and the position of the second metal layer 162 used as a stud.
[0042] In some embodiments, after forming the first metal layer 161 and the second metal layer 162, a first etching process may be further performed to roughen the first metal layer 161 and / or the second metal layer 162, for example, to roughen the surface of the first metal layer 161 and / or the surface of the second metal layer 162. For example, the first metal layer 161 and the second metal layer 162 are immersed in an etching solution to perform the first etching process, so that the surface of the first metal layer 161 or the surface of the second metal layer 162 has a rough surface, respectively, and produces uneven protrusions or recesses. The etching process may include chemical etching, laser etching, a combination of the above or other suitable roughening methods, but is not limited thereto.
[0043] Then, if Figure 3BAs shown, a first insulating layer 163 is first provided to cover the protective layer 130, the encapsulation layer 150, the first metal layer 161 and the second metal layer 162. For example, the first insulating layer 163 can directly contact the protective layer 130, the encapsulation layer 150, the first metal layer 161 and the second metal layer 162. The first metal layer 161, the second metal layer 162, and the first insulating layer 163 together form a redistribution structure layer 160. In particular, the first insulating layer 163 directly contacts the roughened surface of the first metal layer 161 or the convex part of the surface of the second metal layer 162 or penetrates into the concave part. For example, the above design can help increase the bonding force of the first metal layer 161 and the second metal layer 162 to the first insulating layer 163, reduce the risk of interlayer cracking caused by the difference in thermal expansion coefficients, or help improve the reliability of the electronic device.
[0044] Continue as Figure 3B As shown, according to some embodiments of the present invention, a portion of the first insulating layer 163 may be removed to expose the second metal layer 162. For example, grinding may be used to remove a portion of the first insulating layer 163, thereby exposing the second metal layer top surface 162B of the second metal layer 162. When the second metal layer top surface 162B is removed by grinding, the roughened convex or concave portions previously formed by etching on the second metal layer top surface 162B are removed, and the second metal layer top surface 162B is polished into a smooth surface and is flush with the ground first insulating layer top surface 163B.
[0045] Afterwards, if Figure 3CAs shown, according to some embodiments of the present invention, after removing part of the first insulating layer 163, a second etching process, such as chemical etching, laser etching, micro-etching process or a combination thereof, can be performed to remove part of the second metal layer 162 to form a cavity 163A, thereby shortening the vertical distance D between the second metal layer top surface 162B and the second carrier 152 along the Z direction, so that there is a step difference (gap) G between the first insulating layer top surface 163B and the second metal layer top surface 162B, such as 1 micron to 10 microns, and increasing the roughness of the second metal layer top surface 162B. Through the second etching process, the second metal layer top surface 162B and the first insulating layer top surface 163B after the grinding step are no longer coplanar, thereby defining the cavity 163A, while increasing the roughness of the second metal layer top surface 162B, and / or making the second metal layer top surface 162B a concave surface. For example, the package structure 151 may be immersed in an etching solution or the etching solution may be applied to the second metal layer top surface 162B to perform a second etching process to selectively remove a portion of the second metal layer top surface 162B, thereby reducing the vertical distance D between the second metal layer top surface 162B and the second carrier 152 along the Z direction. After the second etching process is completed, the first redistribution structure layer 160 may be obtained. For example, the first redistribution structure layer 160 may include a first metal layer 161, a second metal layer 162, and a first insulating layer 163, and is located on the package structure 151. In some embodiments, after the second etching process, the second metal layer top surface 162B may be flat. In other embodiments, after the second etching process, the second metal layer top surface 162B may be a curved surface. In other embodiments, after the second etching process, the second metal layer top surface 162B may be smooth. In other embodiments, after the second etching process, the second metal layer top surface 162B may be a rough surface with unevenness and roughness.
[0046] Then, if Figure 3DAs shown, after the second etching process, the bonding element 170 can be further formed, so that the bonding element 170 is disposed in the cavity 163A defined by the first insulating layer 163 and the second metal layer top surface 162B corresponding to the second metal layer 162. For example, the bonding element 170 can be formed after a ball drop step and a reflow step, so that the bonding element 170 is overlapped and disposed corresponding to the metal layer of the redistribution structure layer 160. According to some embodiments of the present invention, the above-mentioned "corresponding to..." can mean that the bonding element 170 directly contacts at least part of the corresponding element, for example, in the cross-sectional view, the bonding element 170 directly contacts the second metal layer top surface 162B. According to some embodiments, the rough second metal layer top surface 162B can be beneficial to increase the contact area of the bonding surface between the bonding element 170 and the second metal layer top surface 162B. In some embodiments of the present invention, the bonding element 170 may include a bump, which may be, for example, a solder ball. Figure 3D The solder balls 171 and 172 included in the bonding element 170 can be respectively disposed corresponding to different second metal layer top surfaces 162B, but the present invention is not limited thereto. The bonding element 170 can include tin, nickel, gold, a combination thereof, or other suitable materials, but is not limited thereto.
[0047] According to some embodiments of the present invention, solder balls or other bonding elements can be electrically connected to each die or electronic unit through a rewiring structure. The rewiring structure may include at least one conductive layer and at least one insulating layer, or reroute the circuit and / or further increase the circuit fan-out area, or different electronic components can be electrically connected to each other through the rewiring structure. For example, in a cross-sectional view, along a direction perpendicular to the normal direction of the substrate layer 110 (Z direction), the spacing between two adjacent contact pads of the rewiring structure contacting one end of the die is smaller than the spacing between two adjacent contact pads of the circuit structure away from one end of the die, that is, the distance between adjacent first metal layers 161 is smaller than the distance between adjacent second metal layers 162, so the circuit fan-out condition can be adjusted through the circuit structure, but is not limited to this.
[0048] Then, if Figure 3EAs shown, after the bonding element 170 is completed, the second carrier 152 can be removed by removing the release layer 153 by heating, laser, etc. According to some embodiments of the present invention, the redistribution structure 160 and the packaging structure 151 are further cut to obtain the electronic device 100 of the present invention. The electronic device 100 of the present invention may include at least one chip 141, a protective layer 130, a packaging layer 150, a redistribution structure layer 160, and a bonding element 170. The chip 141 may include a substrate layer 110, which may include, for example, a silicon-based material, a doped silicon material, or a gallium nitride material, but the present invention is not limited thereto. The substrate layer 110 may have two sides arranged oppositely, such as a first side 111 of an active surface, a second side 112, and a first side surface 115 connected to the active surface. According to some embodiments, the first side 111 of the active surface of the substrate layer 110 is provided with a circuit structure 120, so that the chip 141 may include a substrate layer 110 and a circuit structure 120 arranged on one side of the substrate layer 110.
[0049] The circuit structure may include at least one metal layer 121, at least one dielectric layer 122, and at least one insulating layer 123. The dielectric layer 122 may include a porous material with a low dielectric constant, such as a porous material with a dielectric constant lower than 2.4, a porous material with a dielectric constant lower than 2.0, or a low dielectric constant layer of a porous material with a dielectric constant lower than 1.9, but the present invention is not limited thereto.
[0050] The protective layer 130 may be disposed on an active surface of the substrate layer 110 of the wafer 141, such as the first side 111. In addition, the protective layer 130 may have a second side 131. The encapsulation layer 150 surrounds the wafer 141 and the protective layer 130. In the cross-sectional view, the encapsulation layer 150 may directly contact at least two sides of the wafer 141, such as the first side 115 and the third side 117 of the substrate layer 110, and the side 124 of the circuit structure 120. According to some embodiments of the present invention, the roughness of the first side 115 and the third side 117 of the wafer 141 is different, the roughness of the first side 115 of the wafer 141 is different from the roughness of the second side 131, and the roughness of the third side 117 of the wafer 141 is different from the roughness of the second side 131. For example, the roughness of the third side 117 is less than the roughness of the first side 115. For example, under observation with an electron microscope, the difference in the undulation of the first side 115 is greater than the difference in the undulation of the third side 117. For example, the roughness of the second side 131 is greater than the roughness of the third side 117, but not limited thereto. For example, the roughness of the second side 131 is less than the roughness of the first side 115, but not limited thereto. According to other embodiments of the present invention, the cut surface of the low dielectric constant layer is aligned with the cut surface of the protective layer. For example, the protective layer 130 has a cut surface of the second side 131, and the dielectric layer 122 in the circuit structure 120 has a cut surface of the side 124, and the two are formed in the same cutting method, so they are aligned with each other. According to some embodiments, the side edges of each film layer may not be aligned with each other.
[0051] The first redistribution structure layer 160 may be disposed on the packaging layer 150 and the protective layer 130. The first redistribution structure layer 160 may include one or more groups of conductor layers, such as one or more groups of first metal layers 161 and one or more groups of second metal layers 162, and one or more groups of first insulating layers 163. The redistribution structure layer may be electrically connected to the chip 141 via the conductor layer, for example, it may be electrically connected to a plurality of metal pads 121A used as input and output terminal bonding pads in the circuit structure 120 via the first metal layer 161, so that the redistribution structure layer is electrically connected to the chip 141. The bonding element 170 may be disposed overlapping with a conductor layer of the redistribution structure layer 160, for example, the bonding element 170 may be disposed corresponding to the second metal layer 162, so that the bonding element 170 may be electrically connected to the chip 141 via the redistribution structure layer 160.
[0052] According to some embodiments of the present invention, the chip 141 further includes a back side, such as the second side 112, relative to the active surface, such as the first side 111. The back side can be connected to the active surface via the third side 117 and the first side 115. According to other embodiments of the present invention, the roughness of the third side 117 is less than the roughness of the first side 115. Through the above design, the bonding strength can be increased, thereby reducing the risk of interface cracking between different film layers, but it is not limited thereto.
[0053] According to some embodiments of the present invention, the surface of the conductor layer in the redistribution structure may not be coplanar with the insulating layer surrounding the conductor layer of the redistribution structure. For example, the second metal layer top surface 162B in the first redistribution structure layer 160 and the first insulating layer top surface 163B surrounding the second metal layer 162 may not be coplanar to define the cavity 163A, but the present invention is not limited thereto.
[0054] Figure 4 Plot corresponding to Figure 3B A cross-sectional schematic diagram of a variant embodiment of the electronic device 100 in FIG. For the convenience of description, some elements are omitted. According to some embodiments of the present invention, the electronic device 100 may further include a first rewiring structure layer 160 and a second rewiring structure layer 160'. The first rewiring structure layer 160 and the second rewiring structure layer 160' may be respectively disposed on opposite sides of the packaging layer 150, such as the first side 150-1 and the second side 150-2. The first rewiring structure layer 160 may include one or more groups of first metal layers 161 and second metal layers 162, and one or more groups of first insulating layers 163 corresponding to the one or more groups of first metal layers 161 and second metal layers 162. The second rewiring structure layer 160' may include one or more groups of first metal layers 161', second metal layers 162', one or more groups of second insulating layers 163' corresponding to the one or more groups of first metal layers 161' and second metal layers 162', and a seed layer 161A'. The first metal layer 161 may further include a cavity 161A. The first metal layer 161 is electrically connected to a plurality of metal pads 121A of the die 142 that are used as input and output terminal bonding pads. The first insulating layer 163 covers the protection layer 130 of the package structure 151 and the first metal layer 161. In addition, the second rewiring structure layer 160' may be electrically connected to the second metal layer 162 of the first rewiring structure layer 160 via the seed layer 161A'. In detail, the second metal layer 162' may be bonded to an external element, such as a printed circuit board, but not limited thereto.
[0055] Figure 5 Plot corresponding to Figure 3E A cross-sectional schematic diagram of a modified embodiment of the electronic device in FIG. For the convenience of description, some components are omitted. Figure 5The electronic device 101 in the embodiment may include an electronic unit 144 in addition to the chip 141. The chip 141 and the electronic unit 144 may be electronic units with different functions, and may be electrically connected to each other via the first metal layer 161 of the first redistribution structure layer 160. In some embodiments, the electronic unit 144 may include an integrated circuit, a memory, a diode, a sensor, a surface mount device (SMD) and / or a large scale integration LSI (large scale integration). The surface mount device may include, for example, passive components such as capacitors and resistors, but is not limited thereto. The chip 141 may be a die, a semiconductor device, a light emitting diode, a variable capacitance diode, etc. As shown in the figure, a glue layer 145 may be selectively provided around the conductive pad to which the electronic unit 144 and the first metal layer 161 are bonded. The glue layer 145 may include a resin, a polymer or other suitable materials. For example, the glue layer 145 may be an underfill layer. The provision of the underfill layer 145 helps to improve the reliability of the electronic unit 144. The electronic unit 144 may include a conductive pad (not shown) contacting the first metal layer 161 so as to electrically connect the electronic unit 144 to the redistribution structure layer 160 , wherein the conductive pad includes copper, tin, silver, alloy, combinations thereof or other suitable conductive materials, but is not limited thereto.
[0056] According to some embodiments of the present invention, the top surface 130T of the protective layer 130 and the first side 150-1 of the packaging layer 150 may not be at the same height and have a step difference G1. For example, along the Z direction, the step difference G1 may be 0.05 microns to 10 microns (0.05m≤G1≤10m), or the step difference G1 may be 1 micron to 5 microns (1m≤G1≤5m), but the present invention is not limited thereto. By having a step difference design between the protective layer 130 and the packaging layer 150, the contact area between the protective layer 130 and the packaging layer 150 can be increased, so that the protective layer 130 and the packaging layer 150 can be engaged with each other, reducing the risk of chip deviation in the packaging step, but not limited thereto. According to other embodiments of the present invention, the bonding element 170 is disposed in the recess 163 and overlaps the second conductor layer 162. There is an angle θ3 between the bonding element 170 and the second conductor layer 162, and the angle θ3 can be 15° to 60°, that is, 15°≤θ3≤60°, but the present invention is not limited thereto. In other words, when there is an angle θ3 between the bonding element 170 and the second conductor layer 162, the first insulating layer 163 is disposed on a portion of the bonding element 170, so that a portion of the bonding element 170 is disposed between the first insulating layer 163 and the second conductor layer 162. Through the above design, the risk of the bonding element 170 breaking can be reduced, but the present invention is not limited thereto.
[0057] Some embodiments of the present invention provide a method for manufacturing an electronic device, which can cut a dielectric layer and a base layer respectively by two different cutting methods. The cutting conditions of the first cutting step can be milder than the cutting conditions of the second cutting step. For example, the dielectric layer is cut under low cutting stress conditions, thereby reducing the possibility of causing undesirable defects such as fragmentation or cracking on the side of the exposed dielectric layer. The second cutting step is beneficial for cutting the base layer whose material strength is higher than that of the dielectric layer, and the roughness of the side formed by the first cutting step may be different from the roughness of the side formed by the second cutting step. The method for manufacturing an electronic device provided by some embodiments of the present invention is beneficial for reducing the possibility of the dielectric constant material layer in the obtained grain, packaging structure, wafer, or electronic device being easily fragmented or cracked, thereby helping to improve the structural stability and reliability of the grain, packaging structure, wafer, or electronic device.
[0058] The above description is only an embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for manufacturing an electronic device, characterized in that: include: providing a base layer; forming a circuit structure on one side of the base layer; forming a protective layer on the circuit structure; Performing a first cutting step to cut the protective layer to expose a portion of the base layer; and performing a second cutting step to cut the base layer into a plurality of grains, The first cutting step is different from the second cutting step.
2. The method for manufacturing an electronic device according to claim 1, wherein: Also includes: Transferring at least one of the plurality of dies to a carrier; as well as providing a packaging layer surrounding at least one of the plurality of dies, The packaging layer exposes the protection layer of at least one of the plurality of dies.
3. The method for manufacturing an electronic device according to claim 2, wherein: Also includes: patterning the protection layer of at least one of the plurality of dies to form a through hole; as well as A redistribution structure layer is formed. The redistribution structure layer includes at least one metal layer and at least one insulating layer, and the at least one metal layer is electrically connected to at least one of the plurality of grains through the through hole.
4. The method for manufacturing an electronic device according to claim 3, wherein: Also includes: grinding the at least one insulating layer to expose the at least one metal layer; as well as A bonding element is provided and disposed corresponding to the at least one metal layer.
5. The method for manufacturing an electronic device according to claim 1, wherein: Performing the first cutting step includes cutting a portion of the base layer.
6. The method for manufacturing an electronic device according to claim 1, wherein: The first cutting step includes laser cutting, and the second cutting step includes knife cutting.
7. An electronic device, characterized in that: include: A chip has an active surface and a first side surface connected to the active surface; A protective layer is disposed on the active surface of the wafer, and the protective layer has a second side surface; A packaging layer surrounds the chip and the protection layer; as well as A redistribution structure layer is disposed on the packaging layer and the protective layer, and the redistribution structure layer is electrically connected to the chip. The first side surface is adjacent to the protection layer, and a roughness of the first side surface is different from a roughness of the second side surface.
8. The electronic device as claimed in claim 7, characterized in that: The chip further includes a back surface and a third side surface opposite to the active surface, the third side surface connects the first side surface and the back surface, and a roughness of the third side surface is smaller than the roughness of the first side surface.
9. The electronic device as claimed in claim 8, characterized in that: Also includes: A bonding element is arranged overlapping with a metal layer of the redistribution structure layer.
10. The electronic device according to claim 9, wherein: A surface of the metal layer is not coplanar with an insulating layer of the redistribution structure surrounding the metal layer.