CMOS device manufacturing process and CMOS device prepared based on process
Through the second step annealing process in the exchange of nickel silicide process in the manufacturing of CMOS devices and the sequence of contact etching barrier layers, the peak annealing is used as the protective layer to perform peak annealing, which solves the device performance caused by nickel silicide defects. The problem has achieved improvements in yield and reliability, while avoiding nickel metal pollution and cost increase.
Patent Information
- Application Number
- CN202411171358.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-23
- Publication Date
- 2024-12-03
AI Technical Summary
In the manufacturing of CMOS devices, nickel silicide defects lead to increased leakage current of the device, increased static power consumption, reduced yield and reliability. The prior art is difficult to effectively suppress the abnormal diffusion of nickel atoms, and the introduction of spike annealing may lead to nickel metal contamination. Increase process complexity and cost.
Through the second step annealing process in the exchange nickel silicide process and the sequence of deposition of contact etching barrier layers, the contact etching barrier layer is used as a protective layer to perform peak annealing to avoid nickel metal contamination and without adding new equipment and processes In the case of steps, the diffusion and defect generation of nickel atoms are controlled.
It effectively suppresses the occurrence of nickel silicide erosion defects, improves the leakage current and reliability of the device, reduces production costs, and improves the performance and carrier mobility of the device.
Smart Images

Figure CN119069426A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a CMOS device manufacturing process. Background Art
[0002] The self-aligned metal silicide process plays a very important role in ultra-large-scale integrated circuits and is one of the key manufacturing processes for high-performance devices. This process reduces the series parasitic resistance of the gate and source / drain and shortens the RC delay of the device. In addition, due to the use of a self-aligned process, this technology does not require additional lithography and etching steps, thus greatly reducing the complexity of the process. Nickel silicide technology is widely used in 65nm and below nodes due to its advantages such as low silicon consumption, low thermal budget, no wireless bandwidth effect and bridge failure. A typical self-aligned nickel silicide process includes the following steps: depositing a nickel-containing metal layer and a capping layer on a substrate; performing a first step of rapid thermal annealing to form a high-resistance nickel silicide layer; selectively etching to remove the capping layer and unreacted metal; performing a second step of rapid thermal annealing to form a low-resistance nickel silicide layer.
[0003] Nickel atoms are always the main diffusing species during the silicidation reaction, and their diffusion rate in silicon is very fast (diffusion coefficient is ∼10 at 500°C). -14 m 2 / s), so nickel atoms are prone to uneven and abnormal diffusion, resulting in rough silicide / silicon interface or corrosion defects. With the continuous miniaturization of technology nodes, device size is getting smaller and smaller. Even if the nickel silicide defect is only a few nanometers, it will cause a sharp increase in device leakage current, resulting in increased static power consumption, reduced yield and reliability of the product, which limits its further application.
[0004] In order to suppress the abnormal diffusion of nickel atoms, people have tried many methods. Among them, the introduction of spike annealing process is widely adopted as a convenient and effective method. As the extreme of rapid thermal annealing, spike annealing was first applied to the activation of doped ions and the repair of lattice damage after source / drain ion implantation in the front-end process of CMOS. It has a higher heating and cooling speed and a shorter heating time. Applying it to the second-step annealing process of nickel silicide can effectively reduce the thermal budget, and its short time scale helps to control the diffusion of nickel atoms. The machine for spike annealing is usually basically the same as that for rapid thermal annealing. Therefore, spike annealing can be achieved on the rapid thermal annealing machine after simple debugging and calibration, without adding new equipment, which greatly reduces production costs. In order to ensure that the thermal budget of spike annealing is sufficient to completely convert high-resistance nickel silicide into low-resistance nickel silicide, the temperature setting of spike annealing is usually 100℃-200℃ higher than that of rapid thermal annealing. Considering the rapid diffusion of nickel atoms at high temperatures, there is a potential risk of nickel metal contaminating the machine chamber, which will affect the subsequent operation of the machine and thus affect the yield of the product. To prevent the escape of nickel atoms, a protective layer can be covered on the nickel metal layer, but adding an additional protective layer will increase the process steps, cost and process complexity.
[0005] Therefore, a method that does not require adding new process steps and equipment and can suppress the generation of nickel silicide defects is desired to improve the yield and reliability of CMOS devices. Summary of the invention
[0006] A series of simplified concepts are introduced in the Summary of the Invention, which will be further described in detail in the Detailed Description of the Invention. The Summary of the Invention does not mean to attempt to define the key features and essential technical features of the claimed technical solution, nor does it mean to attempt to determine the scope of protection of the claimed technical solution.
[0007] The object of the present invention is to provide a CMOS device manufacturing process to solve the increasingly serious yield and reliability problems caused by nickel silicide defects in small-size CMOS devices.
[0008] The present invention adopts the following technical solution:
[0009] The first aspect of the present invention provides a CMOS device manufacturing process, comprising: depositing a nickel-containing metal layer and a covering layer on a substrate, performing a first step of rapid thermal annealing process to form a high-resistance nickel silicide layer, selectively etching away the covering layer and unreacted metal, first depositing a contact etch barrier layer, and then performing a second step of spike annealing process to form a low-resistance nickel silicide layer.
[0010] The present invention exchanges the order of the second annealing process step and the contact etch barrier layer deposition step, uses the contact etch barrier layer as a protective layer, and enables the second step of spike annealing to be completed on the same machine as the first step of rapid thermal annealing without causing additional nickel metal pollution, without adding new process steps and equipment, thereby reducing production costs. At the same time, the introduction of spike annealing can effectively control the diffusion of nickel atoms, inhibit the generation of nickel silicide corrosion defects, and significantly improve the leakage current of the device.
[0011] Optionally, the substrate is single crystal silicon, silicon on insulator, laminated silicon on insulator, silicon germanium on insulator, laminated germanium silicon on insulator or germanium on insulator, etc. The substrate can be selected according to actual needs.
[0012] Optionally, before depositing the nickel-containing metal layer and covering layer on the substrate, the substrate is further processed as follows: forming a gate and source / drain structure of a CMOS device on the substrate, depositing a nickel silicide barrier layer, etching the barrier layer, and exposing a window area of the deposited metal layer and covering layer.
[0013] Optionally, the nickel-containing metal layer is pure nickel or an alloy of nickel and other metals.
[0014] Optionally, the covering layer is metallic titanium or titanium nitride.
[0015] Optionally, the deposition process of the nickel-containing metal layer and the covering layer is physical vapor deposition.
[0016] Optionally, the rapid thermal annealing process in the first step uses a rapid thermal annealing furnace, and the process parameters are: annealing temperature is 200°C-350°C, annealing time is 15s-45s, and heating and cooling rates are less than 50°C / s.
[0017] Optionally, the selective etching is wet etching, and the etchant is a mixed solution of a strong oxidant and a strong acid.
[0018] Optionally, the contact etch barrier layer is silicon nitride or silicon nitride oxide.
[0019] Optionally, the deposition process of the contact etch barrier layer is plasma enhanced chemical vapor deposition, and the deposition temperature is 200° C.-350° C., which matches the rapid thermal annealing temperature of the first step.
[0020] Optionally, the spike annealing process in the second step adopts the same rapid thermal annealing furnace as the rapid thermal annealing process in the first step, and the process parameters are: annealing temperature is 500°C-650°C, no holding time, and the heating and cooling rates are greater than 50°C / s.
[0021] A second aspect of the present invention provides a CMOS device, which is manufactured based on the CMOS device manufacturing process described in the first aspect of the present invention.
[0022] The beneficial effects of the present invention are:
[0023] As an inherent process in the manufacturing process of CMOS devices, contact etch barrier layer deposition is usually carried out after the completion of the metal silicide process. It serves as a barrier layer for etching to form contact holes, prevents etching damage to the gate and source / drain, and eliminates the adverse effects caused by different etching heights of the gate and source / drain. At the same time, depending on the choice of contact etch barrier layer material, different stresses can be introduced into CMOS devices, thereby improving the carrier mobility of the device. Generally, the lower the deposition temperature of the contact etch barrier layer, the looser the texture, the smaller the introduced stress, and the more limited the improvement in device performance. Annealing the deposited contact etch barrier layer can make it denser and increase the introduced stress. The CMOS device manufacturing process proposed in the present invention uses the contact etch barrier layer as a protective layer by exchanging the second annealing process and the contact etch barrier layer deposition in the nickel silicide process. Without adding new process steps and equipment, on the one hand, a spike annealing is completed in a rapid thermal annealing machine as the second annealing step of the nickel silicide process, which effectively controls the diffusion of nickel atoms and improves the yield and reliability of the device without causing additional nickel metal contamination. On the other hand, the contact etch barrier layer also becomes dense during the spike annealing process, which can introduce greater stress and help improve the performance of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 A typical process flow chart is shown below;
[0025] Figure 2 is a process flow chart of the present invention;
[0026] FIG3 is a schematic cross-sectional view of a CMOS device manufacturing process according to an embodiment of the present invention.
[0027] Figure 3a A schematic diagram of a CMOS device substrate provided in an embodiment of the present invention;
[0028] Figure 3b A schematic diagram of depositing a nickel-containing metal layer and a capping layer on a CMOS device substrate in an embodiment of the present invention;
[0029] Figure 3c A schematic diagram of performing the first step of rapid thermal annealing process in an embodiment of the present invention to form a high-resistance nickel silicide layer, and selectively etching away the covering layer and unreacted metal;
[0030] Figure 3dIt is a schematic diagram of depositing a contact etch barrier layer and performing a second step of spike annealing process to form a low-resistance nickel silicide layer in an embodiment of the present invention.
[0031] In FIG3 , the reference numerals are as follows:
[0032] Semiconductor substrate 301, isolation structure 302, gate dielectric layer 303, P-type doped gate material layer 304, N-type doped gate material layer 305, sidewall 306, P-type source / drain 307, N-type source / drain 308, nickel silicide barrier layer 309, nickel-containing metal layer 310, covering layer 311, high-resistance nickel silicide layer 312, contact etching barrier layer 313, and low-resistance nickel silicide layer 314. DETAILED DESCRIPTION
[0033] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments.
[0034] The drawings are only for illustrative purposes and cannot be construed as limiting the present invention. To better illustrate the present embodiment, some parts of the drawings may be omitted, enlarged, or reduced, and do not represent the size of the actual product. It is understandable to those skilled in the art that some well-known structures and their descriptions may be omitted in the drawings. The positional relationships described in the drawings are only for illustrative purposes and cannot be construed as limiting the present invention.
[0035] Figure 1 This is a typical CMOS device manufacturing process flow chart, including:
[0036] Step 201, providing a patterned substrate;
[0037] Step 202, depositing a nickel-containing metal layer and a covering layer on a substrate;
[0038] Step 203, performing the first step of rapid thermal annealing process on the structure to form a high-resistance nickel silicide layer;
[0039] Step 204, selectively etching to remove the cover layer and unreacted metal;
[0040] Step 205, performing a second rapid annealing process on the structure to form a low-resistance nickel silicide layer;
[0041] Step 206 , depositing a contact etch stop layer.
[0042] Figure 2 The CMOS device manufacturing process flow chart proposed by the present invention is used to briefly illustrate the process of the entire manufacturing process, including:
[0043] Step 101, providing a patterned substrate;
[0044] Step 102, depositing a nickel-containing metal layer and a covering layer on the substrate;
[0045] Step 103, performing the first step of rapid thermal annealing process on the structure to form a high-resistance nickel silicide layer;
[0046] Step 104, selectively etching to remove the cover layer and unreacted metal;
[0047] Step 105, exchanging the order of the second annealing process step and the contact etch barrier layer deposition step, first depositing the contact etch barrier layer, and then performing the second spike annealing process on the structure to form a low-resistance nickel silicide layer.
[0048] The biggest difference between the CMOS device manufacturing process proposed in the present invention and the conventional process is that the order of the second annealing process and the contact etch barrier layer deposition in the nickel silicide process is exchanged, so that the contact etch barrier layer acts as a protective layer to prevent nickel metal from contaminating the chamber in the second step of the spike annealing process. Without adding new process steps and equipment, the diffusion of nickel atoms can be effectively controlled and the generation of nickel silicide defects can be suppressed.
[0049] Figure 3a to Figure 3d 3 is a schematic cross-sectional view of the CMOS device manufacturing process in the embodiment of the present invention.
[0050] like Figure 3a As shown, in step 101, the process of providing a patterned substrate includes:
[0051] A semiconductor substrate 301 is provided, and the substrate is single crystal silicon, silicon on insulator, laminated silicon on insulator, silicon germanium on insulator, laminated silicon germanium on insulator or germanium on insulator. An isolation structure 302 is formed in the semiconductor substrate 301. As an example, in this embodiment, the isolation structure is a shallow trench isolation, which is used to isolate the substrate between transistors to prevent current leakage and mutual interference, thereby improving the performance and reliability of the device. Various well structures are also formed in the semiconductor substrate 301, PMOS is manufactured on N well, and NMOS is manufactured on P well, which are omitted in the figure for simplicity. A gate structure is formed on the semiconductor substrate 301, and the gate structure includes a gate dielectric layer 303, gate material layers 304 and 305, and a sidewall 306. As an example, in this embodiment, the gate dielectric layer 303 is silicon dioxide or nitrogen-doped silicon dioxide, the gate material layers 304 and 305 are respectively P-type doped and N-type doped polysilicon, and the sidewall 306 includes several layers of silicon dioxide layers and / or silicon nitride layers, which are omitted in the figure for simplicity. Source / drain 307, 308 are formed in the semiconductor substrate 301 located on both sides of the gate structure. The P-type source / drain 307 located in the PMOS region is doped with P-type impurities, which can be ion-implanted trivalent elements such as boron; the N-type source / drain 308 located in the NMOS region is doped with N-type impurities, which can be ion-implanted pentavalent elements such as arsenic and phosphorus. A nickel silicide barrier layer 309 and a photoresist are deposited on the substrate structure, and the barrier layer 309 is masked, exposed, and etched to expose the window area. Preferably, the nickel silicide barrier layer 309 can be a silicon dioxide layer or a stack of silicon dioxide and silicon nitride.
[0052] like Figure 3b As shown, in step 102, a nickel-containing metal layer 310 and a covering layer 311 are deposited on the patterned substrate. The covering layer 311 can prevent the rapid flow of nickel atoms during the annealing process. The nickel-containing metal layer 310 is pure nickel or an alloy of nickel and other metals, the covering layer 311 is metal titanium or titanium nitride, and the deposition process of the nickel-containing metal layer 310 and the covering layer 311 is physical vapor deposition. Preferably, the nickel-containing metal layer 310 can be an alloy of nickel and platinum or a laminate of nickel and platinum, and the platinum content is 5%-10%.
[0053] like Figure 3cAs shown, in steps 103 and 104, the structure is subjected to the first step of rapid thermal annealing process to form a high-resistance nickel silicide layer 312, and the covering layer and unreacted metal are selectively etched away. The first step of rapid thermal annealing process uses a rapid thermal annealing furnace, and the process parameters are: annealing temperature is 200°C-350°C, annealing time is 15s-45s, and heating and cooling rates are less than 50°C / s. The selective etching is wet etching, and the etchant is a mixed solution of a strong oxidant and a strong acid. Preferably, the etchant can be a mixed solution of hydrogen peroxide and sulfuric acid and / or hydrochloric acid, etc.
[0054] like Figure 3d As shown, in step 105, the order of the second annealing process step and the contact etch barrier layer 313 deposition step is exchanged, the contact etch barrier layer 313 is deposited first, and then the second step spike annealing process is performed on the above structure to form a low-resistance nickel silicide layer 314. The contact etch barrier layer 313 is silicon nitride or silicon oxynitride, and the deposition process is plasma enhanced chemical vapor deposition, and the deposition temperature is 200°C-350°C, which matches the rapid thermal annealing temperature of the first step. The second step spike annealing process uses the same rapid thermal annealing furnace as the first step rapid thermal annealing process, and the process parameters are: annealing temperature is 500°C-650°C, no holding time, and the heating and cooling rate is greater than 50°C / s. The shorter time scale of the spike annealing can effectively control the diffusion of nickel atoms and reduce the generation of nickel silicide defects. At the same time, the contact etch barrier layer 313, which protects the machine chamber from nickel metal contamination, is also rearranged more closely during the annealing process, thereby applying greater stress to the CMOS device.
[0055] After the above process flow is completed, the standard CMOS process is continued to form contact holes and the back-end copper metal interconnection process, and the manufacturing of the complete CMOS device can be completed.
[0056] It can be seen from the embodiments of the present invention that the present invention provides a CMOS device manufacturing process, by exchanging the second annealing process and the contact etch barrier layer in the nickel silicide process, using the contact etch barrier layer as a protective layer, and by introducing spike annealing as the second annealing step of the nickel silicide process without adding new process steps and equipment, the abnormal diffusion of nickel atoms is suppressed, and the yield and reliability of the device are improved without causing additional nickel metal contamination.
[0057] The present invention has been described by the above-mentioned embodiments, but it should be understood that the above-mentioned embodiments are only for the purpose of example and illustration, and are not intended to limit the present invention to the scope of the described embodiments. This application is intended to cover any modification, use or adaptation of the present application, which follows the general principles of the present application and includes common knowledge or customary technical means in the art that are not disclosed in the present application. The description and embodiments are only regarded as exemplary, and the true scope and spirit of the present application are indicated by the claims.
[0058] It should be understood that the present application is not limited to the precise structures that have been described above and shown in the drawings, and that various modifications and changes may be made without departing from the scope thereof. The scope of the present application is limited only by the appended claims.
Claims
1. A CMOS device manufacturing process, characterized in that: include: A nickel-containing metal layer and a capping layer are deposited on the substrate, and a first step of rapid thermal annealing process is performed to form a high-resistance nickel silicide layer; After the capping layer and unreacted metal are removed by selective etching, a contact etching barrier layer is first deposited, and then a second step of spike annealing process is performed to form a low-resistance nickel silicide layer.
2. The CMOS device manufacturing process according to claim 1, characterized in that: The substrate is single crystal silicon, silicon on insulator, stacked silicon on insulator, silicon germanium on insulator, stacked germanium silicon on insulator or germanium on insulator.
3. The CMOS device manufacturing process according to claim 1 or 2, characterized in that: Before depositing the nickel-containing metal layer and the covering layer on the substrate, the substrate is further treated as follows: The gate and source / drain structures of the CMOS device are formed on the substrate, a nickel silicide barrier layer is deposited, and the barrier layer is etched to expose the window area of the deposited metal layer and the cover layer.
4. The CMOS device manufacturing process according to claim 1, characterized in that: The nickel-containing metal layer is pure nickel or an alloy of nickel and other metals.
5. The CMOS device manufacturing process according to claim 1, characterized in that: The cover layer is metal titanium or titanium nitride.
6. The CMOS device manufacturing process according to claim 1, 2 or 4, characterized in that: The deposition process of the nickel-containing metal layer and the covering layer is physical vapor deposition.
7. The CMOS device manufacturing process according to claim 1, characterized in that: The rapid thermal annealing process in the first step adopts a rapid thermal annealing furnace, and the process parameters are: annealing temperature is 200°C-350°C, annealing time is 15s-45s, and heating and cooling rates are less than 50°C / s.
8. The CMOS device manufacturing process according to claim 1, characterized in that: The selective etching is wet etching, and the etchant is a mixed solution of a strong oxidant and a strong acid.
9. The CMOS device manufacturing process according to claim 1, characterized in that: The contact etching barrier layer is silicon nitride or silicon nitride oxide.
10. The CMOS device manufacturing process according to claim 1 or 7, characterized in that: The deposition process of the contact etching barrier layer is plasma enhanced chemical vapor deposition, and the deposition temperature is 200° C.-350° C., which matches the rapid thermal annealing temperature of the first step.
11. The CMOS device manufacturing process according to claim 1, characterized in that: The spike annealing process of the second step adopts the same rapid thermal annealing furnace as the rapid thermal annealing process of the first step, and the process parameters are: annealing temperature is 500°C-650°C, there is no holding time, and the heating and cooling rates are greater than 50°C / s.
12. A CMOS device, characterized in that: The CMOS device is manufactured based on the CMOS device manufacturing process according to any one of claims 1 to 11.
Citation Information
Cited By
Formation method of silicide connection layer and semiconductor device
CN119297082A