MIM capacitor device and manufacturing method thereof
By depositing the buffer dielectric layer and the second metal layer interlayer dielectric layer in the MIM capacitor device and flattening the top surface, the problem of uncontrollable resistance of the lower plate metal wire and the upper plate resistance is solved, and the reliability of the device is improved and stability of metal wire.
Patent Information
- Application Number
- CN202310651603.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-06-02
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2043-06-02
AI Technical Summary
The problem that existing MIM capacitor devices cannot accurately control the lower plate metal wire and the surrounding metal wire and the upper plate metal wire resistance Rs affects the device reliability.
By depositing the second inter-metal dielectric layer and the buffer dielectric layer in sequence on the MIM capacitance structure and flattening the top surface, the first opening and the second opening are formed to lead out the lower plate and the upper plate metal wires to ensure the metal wires. Stability of thickness and precise control of resistance.
It provides a safer process window, avoids the problems of metal wire bridging and uncontrollable resistance, and improves the reliability of MIM capacitor devices, the stability and low resistance characteristics of the upper plate metal wire.
Smart Images

Figure CN119069463A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of integrated circuit manufacturing, and in particular to a MIM capacitor device and a manufacturing method thereof. Background Art
[0002] Capacitors are widely used in integrated circuits. In the current CMOS (Complementary Metal Oxide Semiconductor) process and the ferroelectric storage process of eFRAM, the industry's popular capacitors are MIM (Metal-Insulator-Metal) structures manufactured through the BEOL (Backend of Line) process.
[0003] Please refer to Figure 1 The MIM capacitor structure in the MIM capacitor device generally includes a lower plate 11, an upper plate 13, and a capacitor dielectric layer 12 therebetween (the material of which is oxide, silicon nitride SiN, ferroelectric material, or high-K material, etc.). The upper plate 13 is led out through the upper plate lead-out structure above it (i.e., the upper through hole 14a and the upper plate metal wire 15a), and the lower plate 11 is led out through the lower plate lead-out structure above it (i.e., the through hole 14b and the metal wire 15b).
[0004] However, current MIM capacitor devices have problems such as the lower plate metal wire bridging with the surrounding metal wires and the upper plate metal wire resistance Rs cannot be precisely controlled, which affects the device reliability. Summary of the invention
[0005] The object of the present invention is to provide a MIM capacitor device and a manufacturing method thereof, which can provide a safer process window, thereby solving the problems of bridging of the lower plate metal wire with the surrounding metal wires and the inability to accurately control the resistance Rs of the upper plate metal wire, and improving the device reliability.
[0006] To achieve the above object, the present invention provides a method for manufacturing a MIM capacitor device, which includes but is not limited to the following steps:
[0007] Providing a substrate, and sequentially depositing a lower electrode layer, a capacitor dielectric layer, and an upper electrode layer on the substrate;
[0008] The lower plate layer is etched by etching the stop layer, and the upper plate layer and the capacitor dielectric layer are etched to form an upper plate;
[0009] Etching the lower electrode layer around the upper electrode to form a lower electrode, wherein the lower electrode, the upper electrode and the capacitor dielectric layer sandwiched therebetween together constitute a MIM capacitor structure;
[0010] sequentially conformally depositing a second metal interlayer dielectric layer and a buffer dielectric layer on the MIM capacitor structure and the substrate around it, and planarizing the top surface of the buffer dielectric layer;
[0011] A first opening and a second opening are formed respectively, wherein the first opening penetrates the buffer dielectric layer and the second metal interlayer dielectric layer to expose a portion of the top surface of the lower electrode plate, and the second opening penetrates the buffer dielectric layer and the second metal interlayer dielectric layer to expose a portion of the top surface of the upper electrode plate;
[0012] Metal is deposited and the top surface is planarized to form a lower electrode plate lead-out structure filled in the first opening and an upper electrode plate lead-out structure filled in the second opening.
[0013] Optionally, the buffer dielectric layer is made of a material different from that of the second intermetallic dielectric layer, and both are removed after the top surface of the deposited metal is planarized.
[0014] Optionally, the lower portion of the first opening is a first through hole aligned with and exposing a portion of the top surface of the lower electrode plate, the upper portion of the first opening is a first groove connected to the first through hole, and the lower electrode plate lead-out structure includes but is not limited to a plug filled in the first through hole and a lower electrode plate metal wire filled in the first groove; the second opening is a second groove aligned with and exposing a portion of the top surface of the upper electrode plate, and the upper electrode plate lead-out structure includes but is not limited to an upper electrode plate metal wire filled in the second groove.
[0015] Optionally, the steps of forming the first opening and the second opening include but are not limited to:
[0016] Sequentially etching the buffer dielectric layer and the second metal interlayer dielectric layer at the periphery of the upper electrode plate to form the first through hole;
[0017] The upper electrode layer is used as an etching stop layer, and the buffer dielectric layer and the second metal interlayer dielectric layer are etched in sequence to form the first trench and the second trench simultaneously.
[0018] Optionally, a common thickness of the capacitor dielectric layer and the upper electrode plate matches a height of the first through hole below the first groove.
[0019] Optionally, the substrate also has a first metal interlayer dielectric layer and a lower metal interconnection line formed in the first metal interlayer dielectric layer; while forming the first through hole, a second through hole aligned with and exposing a portion of the top surface of the lower metal interconnection line is also formed; while forming the first groove and the second groove, a third groove aligned with and connected to the second through hole is also formed; while forming the lower plate lead-out structure and the upper plate lead-out structure, an upper metal interconnection line filled in the third groove and a plug located between the upper metal interconnection line and the lower metal interconnection line are also formed.
[0020] Optionally, before depositing the lower electrode layer on the substrate, a first metal barrier layer is also deposited on the first metal interlayer dielectric layer and the lower metal interconnect line; before conformally depositing the second metal interlayer dielectric layer, a second metal barrier layer is also conformally deposited on the surface of the first metal barrier layer of the MIM capacitor structure and its periphery.
[0021] Based on the same inventive concept, the present invention also provides a MIM capacitor device, which includes but is not limited to:
[0022] A substrate having a first metal interlayer dielectric layer and a lower metal interconnection line formed in the first metal interlayer dielectric layer;
[0023] The MIM capacitor structure comprises a lower plate, a capacitor dielectric layer and an upper plate which are sequentially formed on a portion of the top surface of the first metal interlayer dielectric layer;
[0024] A second metal interlayer dielectric layer with a flat top surface, the second metal interlayer dielectric layer is formed on the MIM capacitor structure and the first metal interlayer dielectric layer around it, the second metal interlayer dielectric layer has a first through hole, a second through hole, a first groove, a second groove and a third groove, wherein the first through hole is aligned with and exposes a portion of the top surface of the lower electrode plate, the second through hole is aligned with and exposes a portion of the top surface of the lower metal interconnection line, the first groove is aligned with and connected to the first through hole, the second groove is aligned with and exposes a portion of the top surface of the upper electrode plate, and the third groove is aligned with and connected to the second through hole;
[0025] A lower plate metal line filled in the first trench and electrically connected to the lower plate via a plug filled in the first through hole;
[0026] An upper plate metal wire filled in the second trench and electrically connected to the upper plate;
[0027] An upper metal interconnection line is filled in the third trench and electrically connected to the lower metal interconnection line through a plug filled in the second through hole.
[0028] Optionally, the first through hole and the second through hole are formed by a same through hole etching process, and the lower plate metal line, the upper plate metal line and the upper metal interconnection line are formed by a same metal deposition process.
[0029] Optionally, the material of the first metal interlayer dielectric layer or the second metal interlayer dielectric layer includes but is not limited to a low-K dielectric with a dielectric constant K less than 3, the material of the capacitor dielectric layer includes but is not limited to at least one of silicon oxide, silicon nitride, silicon oxynitride, a high-K dielectric with a dielectric constant K greater than 7 and a ferroelectric dielectric material, the material of the upper plate or the lower plate includes but is not limited to at least one of Ti, TiN, Ta, TaN, AL and W, and the material of the lower metal interconnect line or the upper metal interconnect line includes but is not limited to at least one of Cu, W, AL and Au.
[0030] Compared with the prior art, the technical solution of the present invention has at least one of the following beneficial effects:
[0031] 1. Because a buffer dielectric layer is first deposited on the second metal interlayer dielectric layer and its top surface is flattened before etching the second metal interlayer dielectric layer to form the first opening and the second opening, on the one hand, a safer process window can be provided to ensure the process effects of lithography and etching when manufacturing the first opening and the second opening; on the other hand, it can ensure that after the first opening and the second opening are filled with metal and the top surface is flattened, a stable thickness of the upper plate metal wire can be left, thereby solving the problem of directly depositing metal on the second metal interlayer dielectric layer due to process limitations and causing metal residue after flattening, which in turn causes the lower plate metal wire to bridge with the surrounding metal wires. It can also solve the problem that the resistance Rs of the upper plate metal wire cannot be accurately controlled due to the uncontrollable thickness of the upper plate metal wire (for example, the thickness is too thin), and ultimately improve the reliability of the MIM capacitor device.
[0032] 2. The upper electrode plate is led out through the upper electrode plate metal wire, omitting the through hole between the upper electrode plate metal wire and the upper electrode plate in the prior art, making the process simpler, and the resistance Rs of the upper electrode plate metal wire is more stable and lower.
[0033] 3. The grooves used to form the upper plate metal wire and the lower plate metal wire are formed simultaneously with the grooves used to form the upper metal interconnection lines at the corresponding positions in the back-end process, which simplifies the process steps. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Those skilled in the art will appreciate that the accompanying drawings are provided for a better understanding of the present invention and do not constitute any limitation on the scope of the present invention.
[0035] Figure 1 It is a schematic diagram of the cross-sectional structure of an existing MIM capacitor device.
[0036] Figure 2 It is a kind of Figure 1 A schematic diagram of the device cross-sectional structure in the manufacturing method of the MIM capacitor device is shown.
[0037] Figure 3A yes Figure 2 The manufacturing method of the MIM capacitor device shown is for the case where the upper electrode plate after the filled copper is planarized is too thin.
[0038] Figure 3B yes Figure 2 The manufacturing method of the MIM capacitor device shown in the figure has the problem that the upper electrode plate is too thick after the copper filling is planarized.
[0039] Figure 4 It is a schematic flow chart of a method for manufacturing a MIM capacitor device according to a specific embodiment of the present invention.
[0040] Figure 5 It is a schematic diagram of the device cross-sectional structure in the method for manufacturing a MIM capacitor device according to a specific embodiment of the present invention.
[0041] The reference numerals in the accompanying drawings are as follows:
[0042] 10a, 20a, first metal interlayer dielectric layer; 10b, 20b, lower metal interconnection line; 10c, 20c, first metal barrier layer; 11, 21, lower plate; 11a, 21a, lower plate layer; 12, 22, capacitor dielectric layer; 13a, 23a, upper plate layer; 14a, 14b, 14c, through hole; 15a, 15b, 15c, groove; 16, 26, second metal barrier layer; 17, 27a, second metal interlayer dielectric layer; 18a, 28a, upper plate metal line; 18b, 28b, lower plate metal line; 18c, 28c, upper metal interconnection line; 24b, first through hole; 24c, second through hole; 25a, second groove; 25b, first groove; 25c, third groove; 27b, buffer dielectric layer. DETAILED DESCRIPTION
[0043] In the following description, a large number of specific details are given in order to provide a more thorough understanding of the present invention. However, it is obvious to those skilled in the art that the present invention can be implemented without one or more of these details. In other examples, in order to avoid confusion with the present invention, some technical features known in the art are not described. It should be understood that the present invention can be implemented in different forms and should not be interpreted as being limited to the embodiments proposed here. On the contrary, providing these embodiments will make the disclosure thorough and complete, and the scope of the present invention will be fully conveyed to those skilled in the art. The same reference numerals represent the same elements from beginning to end. It should be understood that when an element is referred to as "connected to", "coupled" other elements, it can be directly connected to other elements, or there can be intervening elements. On the contrary, when an element is referred to as "directly connected to" other elements, there is no intervening element. When used here, the singular forms of "one", "an" and "said / the" are also intended to include plural forms, unless the context clearly indicates another way. It should also be understood that the term "comprising" is used to identify the presence of features, steps, operations, elements and / or components, but does not exclude the presence or addition of one or more other features, steps, operations, elements, components and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.
[0044] As described in the background technology section, current MIM capacitor devices have problems such as the lower plate metal wire bridging with the surrounding metal wires and the upper plate metal wire resistance Rs cannot be accurately controlled, which affects the device reliability. Figures 1 to 3B The defects of the prior art are further described in detail with respect to the manufacturing method of the existing MIM capacitor device.
[0045] Specifically, an existing one has Figure 1 The manufacturing method of the MIM capacitor device shown generally includes but is not limited to the following steps:
[0046] S1.1, please refer to Figure 2 In (A), a first metal interlayer dielectric layer 10a (which may be a low dielectric constant material) and a lower metal interconnection line 10b (which may be a material such as copper Cu) are formed by a preparation process of a metal interconnection structure of a certain layer (e.g., Mn layer) of the back-end process BEOL. The lower metal interconnection line 10b is specifically formed by filling a metal material such as copper Cu in the groove of the first metal interlayer dielectric layer 10a and performing chemical mechanical polishing (CMP).
[0047] S1.2, please continue to refer to Figure 2In (A), a first metal barrier layer 10c, a lower electrode layer 11a, a capacitor dielectric layer 12, and an upper electrode layer 13a are sequentially deposited on the first metal interlayer dielectric layer 10a and the lower metal interconnection line 10b by any appropriate deposition process.
[0048] S1.3, please continue to refer to Figure 2 In (B), a photoresist layer (not shown) is coated on the upper electrode layer 13a, and the photoresist layer is exposed and developed to define the layout of the upper electrode 13 of the MIM capacitor structure, and the developed photoresist layer is used as a mask, and the lower electrode layer 11 is used as an etching stop layer to etch the upper electrode layer 13a and the capacitor dielectric layer 12, and the etching stops at the surface or corresponding depth of the lower electrode layer 11a, thereby transferring the layout of the upper electrode to the upper electrode layer 13a and the capacitor dielectric layer 12 to form the upper electrode 13 of the MIM capacitor structure.
[0049] S1.4, please continue to refer to Figure 2 In (C), the above-mentioned photoresist layer is removed, and the photoresist layer is re-coated, and the re-coated photoresist layer is exposed and developed, thereby defining the layout of the lower plate 11 of the MIM capacitor structure, using the developed photoresist layer as a mask, using the first metal barrier layer 10c as an etching stop layer, etching the lower plate layer 11a outside the upper plate 13, and the etching stops on the surface or corresponding depth of the first metal barrier layer 10c, thereby transferring the layout of the lower plate 11 to the lower plate layer 11a, and the remaining lower plate layer 11a is used as the lower plate 11 of the MIM capacitor structure, which has a portion extending relative to the edge of the remaining upper plate 13, for subsequent external lower plate lead-out structure. At this time, a MIM capacitor structure consisting of the upper plate 13, the lower plate 11 and the capacitor dielectric layer 12 sandwiched therebetween is formed, and the first metal barrier layer 10c, the lower plate 11 and the upper plate 13 form a continuous step.
[0050] S1.5, please refer to Figure 2 In (D), a second metal barrier layer 16 and a second metal interlayer dielectric layer 17 are deposited in sequence, and the second metal barrier layer 16 conformally covers the surface of the first metal barrier layer 10c, the lower electrode 11, the capacitor dielectric layer 12 and the upper electrode 13, and the second metal interlayer dielectric layer 17 conformally covers the surface of the second metal barrier layer 16.
[0051] S1.6, please continue to refer to Figure 2In (D), a through hole preparation process (including photolithography and etching) of another layer (e.g., Mn+1 layer) of the metal interconnection structure of the back-end process BEOL is used to etch the second metal interlayer dielectric layer 17, and the etching stops in the second metal barrier layer 16 to form a through hole (via) 14a for leading out the upper electrode plate 13, a through hole 14b for leading out the lower electrode plate 11, and a through hole 14c for leading out the lower metal interconnection line 10b in the second metal interlayer dielectric layer 17.
[0052] S1.7, please refer to Figure 2 In (E), through the metal line preparation process (including photolithography and etching) of another layer (e.g., Mn+1 layer) of the metal interconnection structure of the above-mentioned back-end process BEOL, the second metal interlayer dielectric layer 17 is etched to form a trench 15a for leading out the upper electrode plate 13, a trench 15b for leading out the lower electrode plate 11, and a trench 15c for leading out the lower metal interconnection line 10b in the top of the second metal interlayer dielectric layer 17.
[0053] S1.8, please continue to refer to Figure 2 (F) and Figure 3A to Figure 3B , through the preparation process of the metal wire of another layer (for example, Mn+1 layer) of the metal interconnection structure of the back-end process BEOL, a blocking seed layer (not shown) is deposited, and metal materials such as copper are filled into the through holes 14a-14c and the grooves 15a-15c through electroplating and other processes, and the filled metal materials are chemically mechanically polished on the top, thereby forming an upper plate metal wire 18a for leading out the upper plate 13, a lower plate metal wire 18b for leading out the lower plate 11, and an upper metal interconnection line 18c, and the upper metal interconnection line 18c is electrically connected to the lower metal interconnection line 10b of the lower layer through the plug in the through hole 14c. The upper plate metal wire 18a and the plug in the through hole 14a constitute the upper plate lead-out structure, and the lower plate metal wire 18b and the plug in the through hole 14b constitute the lower plate lead-out structure.
[0054] The inventors have found that the above-mentioned existing manufacturing method has the following defects:
[0055] 1. After the second metal interlayer dielectric layer 17 is conformally deposited, its upper surface is uneven. After the photoresist is coated on the second metal interlayer dielectric layer 17 in step S1.6, the thickness of the photoresist will be uneven. When the photoresist is exposed to define the formation positions of the through holes 14a~14c, the process window of the photolithography exposure will be seriously affected. It may cause the photoresist at some through holes in the through holes 14a~14c to be unable to be fully exposed, resulting in some through holes being unable to be formed, which may eventually cause device failure.
[0056] 2. In step S1.8, the chemical mechanical polishing process for the top of the filled metal material does not have enough process window. On the one hand, it is easy to cause the upper plate metal wire 18a to be ground too thin or even completely ground, such as Figure 3A As shown, the resistance Rs of the upper plate metal line 18a of the MIM capacitor device cannot be accurately controlled; on the other hand, in order to retain a sufficiently thick upper plate metal line 18a, it is easy to generate metal material residue (such as Cu residue) at point P of the second metal interlayer dielectric layer 17, resulting in a bridge between the lower plate metal line 18b and the surrounding upper metal interconnect line 18c.
[0057] Based on this, the present invention provides a method for manufacturing a MIM capacitor device. After forming a MIM capacitor structure, the film stack covering the MIM capacitor structure is optimized, and the upper plate metal connection of the MIM capacitor structure is jointly defined by the metal trench process of the upper metal interconnection line. After filling metal (such as Cu) and CMP, a stable height of the upper plate metal line can be reserved for the MIM capacitor structure, thereby ensuring that the upper plate metal line has a stable resistance, and at the same time solves the problem of preventing the resistance from being unable to be precisely controlled due to the metal line being too thin, and also solves the problem of the risk of metal line bridging caused by the presence of undulating steps on the top surface of the metal interlayer dielectric layer after CMP and metal residues at the steps.
[0058] The technical solution proposed by the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. The advantages and features of the present invention will become clearer according to the following description. It should be noted that the accompanying drawings are all in a very simplified form and are not in precise proportions, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.
[0059] Please refer to Figure 4 An embodiment of the present invention provides a method for manufacturing a MIM capacitor device, which includes but is not limited to the following steps:
[0060] S2.1, providing a substrate, and sequentially depositing a lower electrode layer, a capacitor dielectric layer and an upper electrode layer on the substrate;
[0061] S2.2, etching the stop layer of the lower plate layer, etching the upper plate layer and the capacitor dielectric layer, and forming an upper plate;
[0062] S2.3, etching the lower electrode layer around the upper electrode to form a lower electrode, wherein the lower electrode, the upper electrode and the capacitor dielectric layer sandwiched therebetween together constitute a MIM capacitor structure;
[0063] S2.4, sequentially conformally depositing a second metal interlayer dielectric layer and a buffer dielectric layer on the MIM capacitor structure and the substrate surrounding it, and planarizing the top surface of the buffer dielectric layer;
[0064] S2.5, forming a first opening and a second opening respectively, wherein the first opening penetrates the buffer dielectric layer and the second metal interlayer dielectric layer to expose a portion of the top surface of the lower electrode plate, and the second opening penetrates the buffer dielectric layer and the second metal interlayer dielectric layer to expose a portion of the top surface of the upper electrode plate;
[0065] S2.6, depositing metal and flattening the top surface to form a lower electrode plate lead-out structure filled in the first opening and an upper electrode plate lead-out structure filled in the second opening.
[0066] Please refer to Figure 5 In (A), in step S2.1, first, a substrate may be provided, which may be a substrate for preparing a multilayer metal interconnection structure that has been carried out to the back-end process BEOL of the integrated circuit manufacturing process, wherein a certain layer of metal interconnection line Mn and a first metal interlayer dielectric layer 20a have been manufactured, and the certain layer of metal interconnection line Mn is defined as a lower metal interconnection line 20b hereinafter, and the first metal interlayer dielectric layer 20a at least has a groove (not marked) for filling the lower metal interconnection line 20b. The material of the first metal interlayer dielectric layer 20a may be a low-K dielectric with a dielectric constant lower than 3. The lower metal interconnection line 20b may be formed by filling a metal interconnection material such as copper Cu in the groove of the first metal interlayer dielectric layer 20a and performing top surface flattening, and the top surface flattening process is, for example, a chemical mechanical polishing (CMP) process.
[0067] Please continue to refer to Figure 5 (A) in step S2.1, then, by any suitable deposition process, a first metal barrier layer 20c, a lower electrode layer 21a, a capacitor dielectric layer 22, and an upper electrode layer 23a are sequentially deposited on the first metal interlayer dielectric layer 20a and the lower metal interconnection line 20b. The material of the lower metal interconnection line 20b includes but is not limited to at least one of copper Cu, tungsten W, gold Au, etc. The material of the capacitor dielectric layer 22 includes but is not limited to at least one of silicon oxide, silicon nitride, silicon oxynitride, a high-K dielectric material with a dielectric constant K greater than 7, and a ferroelectric dielectric material, which can be a single-layer film or a plurality of layers of different material films stacked together. High-K dielectric materials include but are not limited to hafnium oxide, zirconium oxide, aluminum oxide, titanium oxide, thallium oxide, and BaTiO 3 The common thickness of the capacitor dielectric layer 22 and the upper plate needs to match the height of the first through hole set for the lower plate in the subsequent step S2.5, so as to ensure that the first groove in the subsequent step S2.5 (used to fill the lower plate metal line, i.e. Figure 5 25b shown in (F)), the second trench (for filling the upper plate metal line, Figure 5 25a) and the third trench (for filling the upper metal interconnection line, Figure 5 25c) shown in (F) is formed simultaneously. As an example, the thickness of the capacitor dielectric layer 22 is 10nm to 100nm. The upper plate layer 23a and the lower plate layer 21a can be formed of the same material, which may include but is not limited to at least one material of Ti, TiN, Ta, TaN, AL and W, or a stacked combination of multiple materials therein. The thickness of the upper plate layer 23a and the lower plate layer 21a can be 10nm to 100nm, respectively, and can be specifically formed by deposition processes such as physical vapor deposition (PVD) or atomic layer deposition (ALD). The first metal barrier layer 20c and the capacitor dielectric layer 22 can be formed by deposition processes such as chemical vapor deposition (CVD). The first metal barrier layer 20c prevents metals such as copper in the lower metal interconnection line 20b from moving or diffusing into the upper plate layer 23a, the lower plate layer 21a, the capacitor dielectric layer 22, and the second metal interlayer dielectric layer 27a formed subsequently during the formation of the MIM capacitor, thereby avoiding adverse effects on the performance of the MIM capacitor such as increased leakage current and reduced breakdown voltage. The material of the first metal barrier layer 20c can be an amorphous metal, including but not limited to TiN or TaN.
[0068] Please refer to Figure 5 (B) in step S2.2, first, a photoresist layer (not shown) is coated on the upper electrode layer 23a, and the photoresist layer is exposed and developed to define the layout of the upper electrode 23 of the MIM capacitor structure; then, the developed photoresist layer is used as a mask, and the lower electrode layer 21a is used as an etching stop layer to etch the upper electrode layer 23a and the capacitor dielectric layer 22, and the etching stops at the surface or corresponding depth of the lower electrode layer 21a, thereby transferring the layout of the upper electrode 23 (i.e., the pattern in the developed photoresist layer) to the upper electrode layer 23a and the capacitor dielectric layer 22, thereby forming the upper electrode 23.
[0069] Please continue to refer to Figure 5(B) in step S2.3, first, remove the above-mentioned photoresist layer, re-coat the photoresist layer, and further expose and develop the re-coated photoresist layer to define the layout of the lower electrode 21 of the MIM capacitor structure; then, use the developed photoresist layer as a mask and the first metal barrier layer 20c as an etching stop layer to etch the lower electrode layer 21a outside the upper electrode 23, and stop etching on the surface or at a corresponding depth of the first metal barrier layer 20c, so that the layout of the lower electrode 21 is transferred to the lower electrode layer 21a, and the remaining lower electrode layer 21a serves as the lower electrode 21 of the MIM capacitor structure, and the lower electrode 21 has a portion extending relative to the edge of the upper electrode 23 for subsequent external lower electrode lead-out structure. At this time, the first metal barrier layer 20c, the lower electrode plate 21 and the upper electrode plate 23 form a continuous step, and the lower electrode plate 21, the upper electrode plate 23 and the remaining capacitor dielectric layer 22 sandwiched therebetween constitute a MIM capacitor structure.
[0070] Please refer to Figure 5(C) in step S2.4, first, by a suitable deposition process such as chemical vapor deposition (CVD), the second metal barrier layer 26, the second metal interlayer dielectric layer 27a and the buffer dielectric layer 27b are sequentially conformally deposited. The second metal barrier layer 26 is relatively thin and conformally covers the exposed surfaces of the first metal barrier layer 20c, the lower plate 21, the capacitor dielectric layer 22 and the upper plate 23. The second metal barrier layer 26 can increase the adhesion between the second metal interlayer dielectric layer 27a and the lower structure on the one hand, and can also prevent the metals such as copper in the lower metal interconnect 20b, the upper plate 23, the lower plate 21 and the subsequently formed metal lines and plugs from moving or diffusing between the corresponding dielectric layers or metal layers during the formation of the MIM capacitor, thereby avoiding adverse effects on the performance of the MIM capacitor device such as increased leakage current and reduced breakdown voltage. The material of the second metal barrier layer 26 can be an amorphous metal, including but not limited to TiN or TaN. The second intermetallic dielectric layer 27a conformally covers the exposed surface of the second metal barrier layer 26, and the thickness is relatively thick, and the thickness can at least meet the sum of the height of the through hole to be formed and the corresponding groove depth. The buffer dielectric layer 27b conformally covers the exposed surface of the second intermetallic dielectric layer 27a, and the thickness can at least compensate for the top surface height difference of the corresponding area of the second intermetallic dielectric layer 27a, so as to provide a flat top surface in the subsequent process. As an example, the buffer dielectric layer 27b is preferably a material with a large etching selectivity ratio with the second intermetallic dielectric layer 27a. For example, when the second intermetallic dielectric layer 27a is a low-K dielectric with a dielectric constant lower than 3, the material of the buffer dielectric layer 27b can be a material with a dielectric constant K greater than 3.0 (such as silicon oxide or silicon oxynitride, etc.), and the thickness is about 30nm to 300nm. In the subsequent process of top surface flattening of the metal layer used to make the upper plate metal line, the buffer dielectric layer 27b is removed and does not remain in the final device structure.
[0071] It should be understood that the second metal barrier layer 26, the second metal interlayer dielectric layer 27a and the buffer dielectric layer 27b can be made of any suitable material, and the deposition process of the three layers can be completed in the same deposition chamber or in different deposition chambers.
[0072] Please continue to refer to Figure 5(D) in step S2.4, then, a chemical mechanical polishing (CMP, also known as chemical mechanical grinding) process can be used to flatten the top surface of the buffer dielectric layer 27b. The flattening process, on the one hand, needs to ensure that there is a sufficiently thick dielectric layer on the top surface of the upper electrode 23 (that is, the stacking thickness of the second metal interlayer dielectric layer 27a and other film layers on the top surface of the upper electrode 23 is thick enough), so as to meet the required thickness of the upper electrode metal wire for leading out the upper electrode 23 formed in the subsequent step S2.6; on the other hand, the remaining buffer dielectric layer 27b is as thin as possible on the top surface of the upper electrode 23, so that the thickness of the dielectric layer on the lower electrode 21 and other areas is as thin as possible (that is, the stacking thickness of the buffer dielectric layer 27b and the second metal interlayer dielectric layer 27a and other film layers on the top surface of the lower electrode 21 is thin enough), thereby reducing the difficulty of the subsequent etching process of the through hole on the lower electrode 21. Optionally, the top surface of the buffer dielectric layer 27 b is planarized until the top surface of the second metal interlayer dielectric layer 27 a above the top surface of the upper electrode plate 23 is exposed.
[0073] Please refer to Figure 5 (E) in step S2.5, first, through the preparation process (including photolithography and etching) of the through hole of another layer (e.g., Mn+1 layer) of the metal interconnection structure of the back-end process BEOL, the buffer dielectric layer 27b and the second metal interlayer dielectric layer 27a above the corresponding area of the lower plate 21 and the lower metal interconnection line 20b in its periphery are etched, and the etching stops in the second metal barrier layer 26, thereby forming a first through hole (via) 24b for leading out the lower plate 21 and a third through hole 24c for leading out the lower metal interconnection line 20b. This process only defines the through hole of the metal interconnection structure of this layer (e.g., Mn+1 layer) and the through hole leading out the lower plate 21 of the MIM capacitor structure, and does not define the through hole leading out the upper plate 23 of the MIM capacitor structure. Moreover, since the top surface of the buffer dielectric layer 27b is flattened in step S2.4, the top surface formed by the remaining buffer dielectric layer 27b and the second metal interlayer dielectric layer 27a is sufficiently flat. Therefore, the thickness of the photoresist applied in this step is uniform, and the photoresist at each through-hole position can be fully exposed, so that the quality of each through-hole formed is reliable.
[0074] Please refer to Figure 5In step (F), in step S2.5, then, through the above-mentioned back-end process BEOL, another layer (e.g., Mn+1 layer) of the metal interconnect structure of the metal wire preparation process (including photolithography and etching), the upper plate 23 is used as the etching stop layer, and the buffer dielectric layer 27b, the second metal interlayer dielectric layer 27b and the second metal barrier layer 26 and the first metal barrier layer 20c at the bottom of the first through hole 24b and the second through hole 24c are etched, and the etching stops at the upper plate 23 On the top surface of the upper plate 23 or in a certain depth of the upper plate 23, a second trench 25a for leading out the upper plate 23, a first trench 25b for leading out the lower plate 21, and a third trench 25c for leading out the lower metal interconnection line 20b are formed, and the bottom of the first through hole 24b exposes the corresponding top surface of the lower plate 21, the bottom of the second through hole 24c exposes the corresponding top surface of the lower metal interconnection line 20b, and the second trench 25a exposes the corresponding top surface of the upper plate 23. The first trench 25b is aligned with and connected to the first through hole 24b below it, so that the first trench 25b and the first through hole 24b form a first opening (not marked); the second trench 25a is aligned with a portion of the top surface of the upper plate 23, as a second opening (not marked).
[0075] Obviously, in the manufacturing method of this embodiment, the first through hole 24b connecting the lower electrode 21 of the MIM capacitor structure is formed together with the through hole process of the upper interconnection metal structure in the multi-layer metal interconnection structure, and the grooves required for leading out the upper electrode 23 and the lower electrode 21 of the MIM capacitor structure are formed together with the groove process for manufacturing the metal interconnection line of the upper interconnection metal structure.
[0076] Please refer to Figure 5 (G) in step S2.6, first, a barrier seed layer (not shown) is deposited through a preparation process of a metal wire of another layer (e.g., Mn+1 layer) of a metal interconnect structure of a back-end process BEOL, and a metal material such as copper is deposited through electroplating and other processes. The deposited metal material not only fills the second groove 25a, but also fills the first through hole 24b and the first groove 25b connected thereto, and also fills the second through hole 24c and the third groove 25c connected thereto.
[0077] Please refer to Figure 5(H) in step S2.6, then, the top surface of the deposited metal material is flattened by chemical mechanical polishing or other processes, thereby forming a lower plate metal wire 28b for leading out the lower plate 21 in the first groove 25b, an upper plate metal wire 28a for leading out the upper plate 23 in the second groove 25a, and an upper metal interconnection line 28c for leading out the lower metal interconnection line 20b in the third groove 25c. The upper metal interconnection line 28c is electrically connected to the lower metal interconnection line 20b through the plug in the second through hole 24c. The lower plate metal wire 28b is electrically connected to the lower plate 21 through the plug in the first through hole 24b, and the upper plate metal wire 28a is directly electrically connected to the upper plate 23 without a plug. At this time, the lower plate metal wire 28b and the plug in the first through hole 24b constitute a lower plate lead-out structure filled in the first opening (not marked in Figure 5 ), the upper plate metal wire 28a is used as the upper plate lead-out structure filled in the second opening (not marked in Figure 5 middle).
[0078] Among them, in the process of flattening the top surface of the deposited metal material through the chemical mechanical polishing process, the remaining buffer dielectric layer 27b can be used to monitor the stopping point of the chemical mechanical polishing process, so that when the buffer dielectric layer 27b is completely removed, the steps on the top of the second metal interlayer dielectric layer 27a are completely removed at the same time, thereby ensuring that the thickness of the upper electrode plate metal wire remaining above the top surface of the upper electrode plate 23 meets the requirements, thereby avoiding the problem of bridging of the lower electrode plate metal wire and other surrounding metal wires due to metal residues at the steps on the upper surface of the second metal interlayer dielectric layer 27a, and also avoiding the problem of bridging of some metal wires due to the upper electrode plate metal wire being too thick or the problem that the resistance of the upper electrode plate metal wire cannot be accurately controlled due to the upper electrode plate metal wire being too thin.
[0079] It should also be understood that the direction of the second groove 25a above the upper plate 23 can be designed to be different from Figure 2 15a in (E), but because there is no plug between the upper electrode metal line 28a in the second groove 25a and the upper electrode 23, the contact area between the two is greatly increased and the contact resistance between the two is reduced.
[0080] In summary, in the manufacturing method of this embodiment, firstly, due to the use of buffer dielectric layer deposition and top surface flattening, a flat process window is provided for subsequent steps, so that the grooves required for the upper electrode plate to be led out can be formed synchronously with the grooves required for the lower electrode plate and other positions to be led out, simplifying the process steps, and at the same time avoiding the problem of difficulty in metal filling due to excessive through hole depth; secondly, after the metal is filled in each groove and the top surface is flattened, the remaining buffer dielectric layer and the steps on the top of the second metal interlayer dielectric layer can be removed, thereby solving the problem that the upper electrode plate metal line is too thick due to process limitations, which makes the second There are metal residues at the steps on the upper surface of the metal interlayer dielectric layer, which leads to metal wire bridging and other problems. It can also solve the problem that the upper plate metal wire is too thin due to process limitations, making it impossible to accurately control the resistance Rs of the upper plate metal wire. Furthermore, the upper plate is only led out through the upper plate metal wire, the process is simpler, the resistance value is more stable, and for the capacitor plate, the contact resistance between the upper plate metal wire and the upper plate is much lower than the existing contact resistance between the upper plate and the plug in the through hole, so the contact resistance can be reduced, the parasitic effect of the MIM capacitor device is improved, and the performance of the MIM capacitor device is improved.
[0081] Based on the same inventive concept, an embodiment of the present invention further provides a MIM capacitor device, which can be formed by any suitable manufacturing method, preferably by the manufacturing method of the MIM capacitor device of the present invention. Figure 5 In (E) to (F) and (H), the MIM capacitor device specifically includes but is not limited to the following structure:
[0082] A substrate having a first metal interlayer dielectric layer 20a and a lower metal interconnection line 20b formed in the first metal interlayer dielectric layer 20a;
[0083] The MIM capacitor structure includes a lower plate 21, a capacitor dielectric layer 22 and an upper plate 23 which are sequentially formed on a portion of the top surface of the first metal interlayer dielectric layer 20a;
[0084] A second metal interlayer dielectric layer 27a having a flat top surface, the second metal interlayer dielectric layer 27a is formed on the MIM capacitor structure and the first metal interlayer dielectric layer 20a at its periphery, the second metal interlayer dielectric layer 27a has a first through hole 24b, a second through hole 24c, a first groove 25b, a second groove 25a and a third groove 25c, wherein the first through hole 24b is aligned with and exposes a portion of the top surface of the lower electrode plate 21, the second through hole 24c is aligned with and exposes a portion of the top surface of the lower metal interconnection line 20b, the first groove 25b is aligned with and connected to the first through hole 24b, the second groove 25a is aligned with and exposes a portion of the top surface of the upper electrode plate 23, and the third groove 25c is aligned with and connected to the second through hole 24c;
[0085] A lower plate metal wire 28b is filled in the first groove 25b and is electrically connected to the lower plate 21 through a plug (not marked) filled in the first through hole 24b. Optionally, the lower plate metal wire 28b and the plug of the first through hole 24b are formed by the same metal deposition process, and the lower plate metal wire 28b and the plug of the first through hole 24b constitute a lower plate lead-out structure;
[0086] An upper electrode plate metal wire 28a is filled in the second groove 25a and is electrically connected to the upper electrode plate 23, wherein the upper electrode plate metal wire 28a serves as an upper electrode plate lead-out structure for leading out the upper electrode plate 23;
[0087] The upper metal interconnection line 28c is filled in the third trench 25c and is electrically connected to the lower metal interconnection line 20b through the plug filled in the second through hole 24c. The upper metal interconnection line 28c, the lower metal interconnection line 20b and the plug filled in the second through hole 24c constitute a part of a multi-layer metal interconnection structure.
[0088] Optionally, the first through hole 24b and the second through hole 24c are formed by the same through hole etching process, the grooves where the lower plate metal line 28b, the upper plate metal line 28a and the upper metal interconnection line 28c are located are formed by the same groove etching process, and the lower plate metal line 28b, the upper plate metal line 28a and the upper metal interconnection line 28c are formed by the same metal deposition process and CMP process.
[0089] Optionally, the material of the first metal interlayer dielectric layer 20a or the second metal interlayer dielectric layer 27a includes but is not limited to a low-K dielectric with a dielectric constant K less than 3, the material of the capacitor dielectric layer 22 includes but is not limited to at least one of silicon oxide, silicon nitride, silicon oxynitride, a high-K dielectric with a dielectric constant K greater than 7 and a ferroelectric dielectric material, the material of the upper plate 232 or the lower plate 21 includes but is not limited to at least one of Ti, TiN, Ta, TaN, AL and W, and the material of the lower metal interconnect line 20b or the upper metal interconnect line 28c includes but is not limited to at least one of Cu, W, AL and Au.
[0090] Optionally, a first metal barrier layer 20c may be sandwiched between the lower electrode 21 and the first metal interlayer dielectric layer 20a, and a second metal barrier layer 26 may be sandwiched between the upper electrode 23 and the second metal interlayer dielectric layer 27a. The materials of the first metal barrier layer 20c and the second metal barrier layer 26 may be the same, for example, both include but are not limited to TiN or TaN. The first metal barrier layer 20c and the second metal barrier layer 26 can prevent the corresponding metals from moving and diffusing between the film layers and causing adverse effects on the performance of the device.
[0091] In the MIM capacitor device of this embodiment, the through hole is omitted in the upper plate lead-out structure for leading out the upper plate, so the device performance can be improved by the performance of the lower contact resistance between the upper plate metal wire and the upper plate. In addition, the thickness of the upper plate metal wire is controllable, so that on the one hand, the problem of bridging between the lower plate metal wire and the surrounding metal wires caused by the thick thickness of the upper plate metal wire can be avoided, and on the other hand, the problem of uncontrollable resistance of the upper plate metal wire caused by the thin thickness of the upper plate metal wire can be avoided, thereby improving the reliability of the device.
[0092] The above description is only a description of the preferred embodiment of the present invention, and is not intended to limit the scope of the present invention. Any changes or modifications made by a person skilled in the art in the field of the present invention based on the above disclosure shall fall within the scope of protection of the technical solution of the present invention.
Claims
1. A method for manufacturing a MIM capacitor device, characterized in that: include: Providing a substrate, and sequentially depositing a lower electrode layer, a capacitor dielectric layer and an upper electrode layer on the substrate; The lower plate layer is etched by etching the stop layer, and the upper plate layer and the capacitor dielectric layer are etched to form an upper plate; Etching the lower electrode layer around the upper electrode to form a lower electrode, wherein the lower electrode, the upper electrode and the capacitor dielectric layer sandwiched therebetween together constitute a MIM capacitor structure; sequentially conformally depositing a second metal interlayer dielectric layer and a buffer dielectric layer on the MIM capacitor structure and the substrate around it, and planarizing the top surface of the buffer dielectric layer; A first opening and a second opening are formed respectively, wherein the first opening penetrates the buffer dielectric layer and the second metal interlayer dielectric layer to expose a portion of the top surface of the lower electrode plate, and the second opening penetrates the buffer dielectric layer and the second metal interlayer dielectric layer to expose a portion of the top surface of the upper electrode plate; Metal is deposited and the top surface is planarized to form a lower electrode plate lead-out structure filled in the first opening and an upper electrode plate lead-out structure filled in the second opening.
2. The manufacturing method according to claim 1, characterized in that The buffer dielectric layer is made of a material different from that of the second intermetallic dielectric layer, and both are removed after the top surface of the deposited metal is planarized.
3. The manufacturing method according to claim 1, characterized in that: The lower portion of the first opening is a first through hole aligned with and exposing a portion of the top surface of the lower electrode plate, the upper portion of the first opening is a first groove connected to the first through hole, and the lower electrode plate lead-out structure includes a plug filled in the first through hole and a lower electrode plate metal wire filled in the first groove; the second opening is a second groove aligned with and exposing a portion of the top surface of the upper electrode plate, and the upper electrode plate lead-out structure includes an upper electrode plate metal wire filled in the second groove.
4. The manufacturing method according to claim 3, characterized in that: The steps of forming the first opening and the second opening include: Sequentially etching the buffer dielectric layer and the second metal interlayer dielectric layer at the periphery of the upper electrode plate to form the first through hole; The upper electrode layer is used as an etching stop layer, and the buffer dielectric layer and the second metal interlayer dielectric layer are etched in sequence to form the first trench and the second trench simultaneously.
5. The manufacturing method according to claim 3 or 4, characterized in that: The common thickness of the capacitor dielectric layer and the upper electrode plate matches the height of the first through hole below the first groove.
6. The manufacturing method according to claim 3 or 4, characterized in that: The substrate also has a first metal interlayer dielectric layer and a lower metal interconnection line formed in the first metal interlayer dielectric layer; while forming the first through hole, a second through hole aligned with and exposing a portion of the top surface of the lower metal interconnection line is also formed; while forming the first groove and the second groove, a third groove aligned with and connected to the second through hole is also formed; while forming the lower electrode plate lead-out structure and the upper electrode plate lead-out structure, an upper metal interconnection line filled in the third groove and a plug located between the upper metal interconnection line and the lower metal interconnection line are also formed.
7. The manufacturing method according to claim 6, characterized in that: Before depositing the lower electrode layer on the substrate, a first metal barrier layer is also deposited on the first metal interlayer dielectric layer and the lower metal interconnection line; before conformally depositing the second metal interlayer dielectric layer, a second metal barrier layer is also conformally deposited on the surface of the first metal barrier layer of the MIM capacitor structure and its periphery.
8. A MIM capacitor device, characterized in that: include: A substrate having a first metal interlayer dielectric layer and a lower metal interconnection line formed in the first metal interlayer dielectric layer; The MIM capacitor structure comprises a lower plate, a capacitor dielectric layer and an upper plate which are sequentially formed on a portion of the top surface of the first metal interlayer dielectric layer; A second metal interlayer dielectric layer with a flat top surface, the second metal interlayer dielectric layer is formed on the MIM capacitor structure and the first metal interlayer dielectric layer around it, the second metal interlayer dielectric layer has a first through hole, a second through hole, a first groove, a second groove and a third groove, wherein the first through hole is aligned with and exposes a portion of the top surface of the lower electrode plate, the second through hole is aligned with and exposes a portion of the top surface of the lower metal interconnection line, the first groove is aligned with and connected to the first through hole, the second groove is aligned with and exposes a portion of the top surface of the upper electrode plate, and the third groove is aligned with and connected to the second through hole; A lower plate metal line filled in the first trench and electrically connected to the lower plate via a plug filled in the first through hole; An upper plate metal wire filled in the second trench and electrically connected to the upper plate; An upper metal interconnection line is filled in the third trench and electrically connected to the lower metal interconnection line through a plug filled in the second through hole.
9. The MIM capacitor device according to claim 8, characterized in that: The first through hole and the second through hole are formed by a same through hole etching process, and the lower plate metal line, the upper plate metal line and the upper metal interconnection line are formed by a same metal deposition process.
10. The MIM capacitor device according to claim 8, characterized in that: The material of the first metal interlayer dielectric layer or the second metal interlayer dielectric layer includes a low-K dielectric with a dielectric constant K less than 3, the material of the capacitor dielectric layer includes at least one of silicon oxide, silicon nitride, silicon oxynitride, a high-K dielectric with a dielectric constant K greater than 7, and a ferroelectric dielectric material, the material of the upper plate or the lower plate includes at least one of Ti, TiN, Ta, TaN, AL and W, and the material of the lower metal interconnect line or the upper metal interconnect line includes at least one of Cu, W, AL and Au.
Citation Information
Patent Citations
Method for fabricating conducting plates for a high-q mim capacitor
CN101523560A
Forming method of rear-end structure comprising MIM capacitor
CN113506769A
Metal-insulator-metal capacitor forming method for semiconductor device
KR100779387B1
Method of manufacturing semiconductor device
KR1020050005972A
Structure and method for integrating MIM capacitor in BEOL wiring levels
US20060189069A1