Silicon carbide split trench gate MOSFET (Metal-Oxide-Semiconductor Field Effect Transistor) device with enhanced short-circuit tolerance and manufacturing method thereof
By designing the current limiting secondary channel and secondary gate shielding structure in the silicon carbide MOSFET device, the high power density and drain-source voltage problems of the device in the short-circuit state are solved, the short-circuit withstandability and switching speed are improved, and the loss is reduced .
Patent Information
- Application Number
- CN202411145330.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-12-03
AI Technical Summary
The power density of silicon carbide MOSFET devices is high in the short-circuit state and the temperature rises sharply. The short-circuit withstand time is short, and the drain-source voltage is high in the saturated on state, resulting in the failure and burnout of the device.
Design a SiC trench split gate MOSFET device with enhanced short-circuit withstandability. By forming a current limiting sub-channel in the source secondary gate and Nbase region, the device saturation current is reduced, and the main gate is shielded through the source secondary gate to reduce the Small drain-source voltage improves the device's short-circuit withstandability.
Without increasing the on-resistance, the current and power density during short-circuiting of the device is significantly reduced, the device's short-circuit withstandability, the device's switching loss is reduced, and the device's reverse voltage withstandability is improved.
Smart Images

Figure CN119069530A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor devices, and in particular to a silicon carbide split trench gate MOSFET device with enhanced short-circuit tolerance and a manufacturing method thereof. Background Art
[0002] Silicon Carbide (SiC) is a third-generation wide bandgap semiconductor material with excellent material properties such as large bandgap width, high breakdown field strength, high thermal conductivity, and high carrier saturation mobility. It is very suitable for high-temperature and high-power applications. It can significantly improve the efficiency of power electronic systems, reduce system losses, increase power density, reduce system volume, and improve system high-temperature stability. Therefore, SiC MOSFET is currently the most important device among SiC power devices. It can maintain a low on-resistance while reaching a withstand voltage of several kV. In addition, as a unipolar device, it naturally has the advantages of fast switching speed and low switching loss compared to bipolar switching devices such as Si IGBT. However, the biggest problem of SiC MOSFET devices is that the SiC / SiO2 interface state density is too high, resulting in a very low channel mobility of SiC MOSFET (about 20cm 2 V –1 s –1 ), which brings about a large channel resistance and seriously affects the performance of SiC MOSFET devices. In the prior art, a trench gate structure is usually used to improve this problem.
[0003] For example, the patent document with publication number CN114597130B discloses a split-gate silicon carbide MOSFET device and its manufacturing method, wherein a first trench structure is etched in the middle area of the first conductive type heavily doped region; a second conductive type body region is deeply etched into the first conductive type epitaxial layer to form a second trench structure, and the width of the second trench structure is less than the width of the first trench structure; the first conductive type heavily doped region is deeply etched into the second conductive type body region; silicon dioxide is formed on the inner surface of the first trench structure and the second trench structure; polysilicon is deposited on the silicon dioxide to form a polysilicon gate. The T-type split-gate trench structure of the MOSFET is formed by the first trench structure and the second trench structure, which reduces the size of the MOSFET device cell, effectively eliminates the JFET resistance, improves the mobility of the channel, reduces the loss of the silicon carbide MOSFET device, and the vertical conductive channel improves the device integration and current conduction density.
[0004] For example, the patent document with publication number CN117457739A discloses a trench gate SiC MOSFET device structure and preparation method, which forms a gate oxide layer with a sandwich structure of a first gate dielectric layer, a second gate dielectric layer and a third gate dielectric layer by inserting hafnium oxide (HfO2) in the middle of the gate dielectric layer; due to the addition of hafnium oxide (HfO2), a high dielectric constant material, the gate oxide capacitance (C ox ), effectively reducing the channel resistance (R ch ); due to the addition of a second gate dielectric layer including hafnium oxide, which serves as a portion of the gate oxide thickness, the thickness of the first gate dielectric layer can be reduced while ensuring the overall thickness of the gate oxide layer is constant, thereby reducing SiC / SiO2 interface defects and improving the gate oxide withstand voltage capability of the device; at the same time, HfO2 does not directly contact the gate polysilicon layer, but the third gate dielectric layer on its surface serves as a transition between the two, avoiding the "Fermi pinning phenomenon" that would be caused by direct contact between the two.
[0005] However, when a circuit fails and shorts, the above-mentioned prior art silicon carbide MOSFET devices all have the following problems:
[0006] (1) The on-resistance of SiC trench MOSFET devices is very low. When a circuit fails and the device is in a short-circuit working state, the power density of the SiC trench MOSFET device is very high, the temperature rises very sharply, and the device quickly reaches the thermal breakdown temperature. Therefore, the short-circuit withstand time of SiC trench MOSFET devices is very short, generally only 1 to 2 microseconds, and the short-circuit protection capability of the device and power electronic system is poor;
[0007] (2) In the short-circuit state, when the gate of the SiC trench MOSFET device is turned on, it is also subjected to a very high drain-source voltage (i.e., the system power supply voltage). The device enters a saturated conduction state, and the drain-source current is extremely high, causing the device temperature to rise sharply, ultimately leading to failure and burning. Summary of the invention
[0008] In view of the problems existing in the prior art, the present invention provides a silicon carbide split trench gate MOSFET device with enhanced short-circuit tolerance and a method for manufacturing the same. Under the action of the source sub-gate and the current-limiting sub-channel, the saturation current of the device is significantly reduced without affecting the on-resistance of the device, the short-circuit tolerance of the device is improved, and the switching loss of the device is effectively reduced.
[0009] The present invention is implemented as follows: a SiC trench split-gate MOSFET device with enhanced short-circuit tolerance comprises a drain metal layer, a silicon carbide N+ substrate and a silicon carbide N-epitaxial layer are sequentially arranged above the drain metal layer, a first Pbase region is arranged above the silicon carbide N-epitaxial layer, a second Pbase region is arranged above the first Pbase region, a second Nwell region and an Nbase region are arranged at the upper right corner and the lower right corner of the first Pbase region respectively, a trench region is arranged on the right side of the silicon carbide N-epitaxial layer, the first Pbase region and the second Pbase region, a main gate and a source sub-gate are arranged in the trench region from top to bottom, and a current-limiting sub-channel is formed between the Nbase region and the source sub-gate;
[0010] The upper left corner and the upper right corner of the silicon carbide N-epitaxial layer are respectively provided with a Pshield region and a first Nwell region;
[0011] The source sub-gate, the main gate, the silicon carbide N-epitaxial layer, the first Pbase region and the second Pbase region are isolated by a gate oxide layer;
[0012] A P+ ohmic contact region and an N+ ohmic contact region are respectively provided on the left and right sides of the upper end of the second Pbase region;
[0013] The upper end surfaces of the P+ ohmic contact area and the N+ ohmic contact area are covered with a source metal layer, and a gate metal layer is provided above the main gate. The source metal layer and the gate metal layer are not in contact with each other and are isolated by a field oxide dielectric layer.
[0014] Further: The peak concentration of the Pshield region is 5e18cm -3 , width is 0.5~0.6μm, and depth is 0.4~0.6μm.
[0015] Further: The peak concentration of the first Nwell region is 8e17cm -3 , width is 0.5~1μm, and depth is 0.3~0.4μm.
[0016] Further: In the second Nwell region, the peak concentration is 8e17cm -3 , width is 0.5~1μm, and depth is 0.4~0.5μm.
[0017] Further: the first Pbase region and the second Pbase region are both formed by epitaxy, and the epitaxial concentration of the first Pbase region is ≥ 2e17 cm -3 , thickness 0.9~1μm, second Pbase region epitaxial ≥ concentration 8e16cm -3 , thickness 0.9~1μm.
[0018] Further: the concentration of the P+ ohmic contact area is ≥ 1e19cm-3 , depth 0.2-0.3 μm, width 0.5-0.6 μm, the concentration of the N+ ohmic contact area ≥ 1e19 cm -3 , depth 0.2~0.3μm, width 0.9~1μm.
[0019] Further: The peak concentration of the Nbase region is 3e17cm -3 , width 0.2~0.4μm, thickness 0.5~0.6μm.
[0020] Further: the drain metal layer, the source metal layer and the gate metal layer are made of nickel, titanium, aluminum or their alloys.
[0021] Furthermore, the width of the main gate and the source sub-gate is 0.4-0.5 μm, the thickness is 0.9-1 μm, and the thickness of the gate oxide layer between the main gate and the source sub-gate is 0.2-0.3 μm.
[0022] To achieve the purpose of the present invention, the present invention also provides a method for manufacturing the SiC trench split-gate MOSFET device with enhanced short-circuit withstand capability, comprising the following steps:
[0023] S1: After cleaning the silicon carbide N+ substrate sheet, a silicon carbide N- epitaxial layer is formed on the silicon carbide N+ substrate sheet by epitaxy;
[0024] S2: forming a Pshield region by ion implantation at the upper left corner of the silicon carbide N-epitaxial layer, and forming a first Nwell region by ion implantation at the upper right corner of the silicon carbide N-epitaxial layer;
[0025] S3: forming a first Pbase region on the silicon carbide N-epitaxial layer by epitaxy again;
[0026] S4: forming an Nbase region with uniform concentration distribution and a box-shaped distribution by ion implantation at the lower right corner of the first Pbase region, and forming a second Nwell region with uniform concentration distribution and a box-shaped distribution by ion implantation at the upper right corner of the first Pbase region;
[0027] S5: forming a second Pbase region on the first Pbase region again by epitaxy;
[0028] S6: forming a P+ ohmic contact region by ion implantation at the upper left corner inside the second Pbase region, and forming an N+ ohmic contact region by ion implantation at the upper right corner inside the second Pbase region, wherein the left boundary of the N+ ohmic contact region contacts the right boundary of the P+ ohmic contact region;
[0029] S7: growing and patterning field oxide on the surface of silicon carbide, and etching from the upper right corner of the second Pbase region to the silicon carbide N-epitaxial layer to form a trench region;
[0030] S8: growing the silicon carbide N-epitaxial layer, the first Pbase region and the second Pbase region on the outer surface of the trench to form a gate oxide layer through a dry oxygen process;
[0031] S9: forming a source sub-gate above the gate oxide layer at the bottom of the trench by depositing polysilicon;
[0032] S10: forming an insulating medium by depositing an oxide layer above the source sub-gate;
[0033] S11: forming a main gate by depositing polysilicon on the insulating medium;
[0034] S12: an insulating medium is formed by depositing an oxide layer above the main gate, a source ohmic contact hole is opened, an ohmic contact metal is sputtered, and annealing is performed to form a source ohmic contact;
[0035] S13: opening holes above the main gate and the source sub-gate respectively;
[0036] S14: thickening the front metal to form ohmic contacts between the main gate and the source sub-gate, and patterning the metal to form source and drain electrodes;
[0037] S15: sputtering of back ohmic contact metal, laser annealing to form drain ohmic contact, and thickening of back metal to form drain electrode.
[0038] In summary, the beneficial effects of the present invention are:
[0039] (1) The present invention utilizes the current-limiting sub-channel formed by the source sub-gate and the Nbase region to reduce the current and power density of the device under short-circuit conditions without increasing the on-resistance, thereby improving the short-circuit tolerance of the device, while reducing the gate-drain capacitance of the device and increasing the switching speed of the device.
[0040] (2) When the device of the present invention is in a short-circuit state, that is, in a saturated conduction state, since the secondary gate potential is lower than the secondary channel potential, the N-type secondary channel will be depleted, so that the saturated conduction current of the device is limited, thereby reducing the power density of the device when it is short-circuited.
[0041] (3) The source sub-gate of the present invention has a good shielding effect on the main gate. In the linear region, the drain-source voltage is very low, and the potential in the sub-gate and the sub-channel is very close. The current path formed by the sub-channel makes the current in the linear region unaffected, and very low gate-drain capacitance and switching loss can be achieved, and there will be no obvious impact on the reverse withstand voltage.
[0042] (4) The manufacturing method adopted by the present invention can achieve its technical effect without using complicated process technology, and the formation process of each part has less interference and has little impact on the overall performance of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0043] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for describing the embodiments are briefly introduced below.
[0044] Figure 1 It is a schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance according to the present invention;
[0045] Figure 2 This is a comparison chart of the simulation results of the forward output characteristics of the present invention and the traditional device;
[0046] Figure 3 It is a comparison of the heat generation power density of the present invention and the conventional device when a short circuit occurs;
[0047] Figure 4 This is a comparison chart of the reverse breakdown characteristics simulation results of the present invention and the traditional device;
[0048] Figure 5 This is a comparison chart of the simulation results of gate-drain capacitance of the present invention and traditional devices;
[0049] Figure 6 It is a process flow chart of a method for manufacturing a SiC split trench gate MOSFET device with enhanced short circuit tolerance according to the present invention;
[0050] Figure 7 Schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance in step S1 of the present invention;
[0051] Figure 8 Schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance in step S2 of the present invention;
[0052] Fig. 9 Schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance in step S3 of the present invention;
[0053] Fig.10 Schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance in step S4 of the present invention; Figure 8-4 yes
[0054] Fig.11 Schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance in step S5 of the present invention;
[0055] Fig.12 Schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance in step S6 of the present invention;
[0056] Fig.13Schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance in step S7 of the present invention;
[0057] Fig.14 Schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance in step S8 of the present invention;
[0058] Fig.15 Schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance in step S9 of the present invention;
[0059] Fig.16 Schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance in step S10 of the present invention;
[0060] Fig.17 (a) is a schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short-circuit tolerance in step S11 of the present invention;
[0061] Fig.17 (b) Fig.17 (a) is a schematic diagram of the cross-sectional structure along the dotted line AA' perpendicular to the image direction;
[0062] Fig.18 (a) is a schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short-circuit tolerance in step S12 of the present invention;
[0063] Fig.18 (b) Fig.18 (a) is a schematic diagram of the cross-sectional structure along the dotted line AA' perpendicular to the image direction;
[0064] Fig.19 (a) is a schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short-circuit tolerance in step S13 of the present invention;
[0065] Fig.19 (b) Fig.19 (a) is a schematic diagram of the cross-sectional structure along the dotted line AA' perpendicular to the image direction;
[0066] Fig. 20 (a) is a schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short-circuit tolerance in step S14 of the present invention;
[0067] Fig. 20 (b) Fig. 20 (a) is a schematic diagram of the cross-sectional structure along the dotted line AA' perpendicular to the image direction;
[0068] Fig.21 Schematic diagram of the structure of a SiC split trench gate MOSFET device with enhanced short circuit tolerance in step S15 of the present invention;
[0069] Explanation of the accompanying drawings: 1. drain metal layer; 2. silicon carbide N+ substrate; 3. silicon carbide N- epitaxial layer; 4. Pshield region; 5. first Pbase region; 6. second Pbase region; 7. first Nwell region; 8. Nbase region; 9. second Nwell region; 10. P+ ohmic contact region; 11. N+ ohmic contact region; 12. source sub-gate; 13. gate oxide layer; 14. main gate; 15. gate metal layer; 16. field oxygen medium; 17. source metal layer. DETAILED DESCRIPTION
[0070] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0071] The present invention provides a specific embodiment of a silicon carbide split trench gate MOSFET device with enhanced short circuit tolerance and a manufacturing method thereof, the specific contents of which are as follows:
[0072] Combination Figure 1The embodiment of the present invention provides a silicon carbide split trench gate MOSFET device with enhanced short-circuit tolerance, comprising: a drain metal layer 1, a silicon carbide N+ substrate 2 and a silicon carbide N-epitaxial layer 3 are sequentially arranged above the drain metal layer 1, a first Pbase region 5 is arranged above the silicon carbide N-epitaxial layer 3, a second Pbase region 6 is arranged above the first Pbase region 5, a second Nwell region 9 and an Nbase region 8 are arranged at the upper right corner and the lower right corner of the first Pbase region 5, respectively, a trench region is arranged on the right side of the silicon carbide N-epitaxial layer 3, the first Pbase region 5 and the second Pbase region 6, a main gate 14 and a source sub-gate 12 are arranged in the trench region from top to bottom, and the Nbase region 8 and the source sub-gate 12 are arranged at the upper right corner and the lower right corner of the first Pbase region 5, respectively. A current limiting auxiliary channel is formed between the gates 12, and a Pshield region 4 and a first Nwell region 7 are respectively arranged at the upper left corner and the upper right corner of the silicon carbide N-epitaxial layer 3; the source auxiliary gate 12, the main gate 14 are isolated from the silicon carbide N-epitaxial layer 3, the first Pbase region 5 and the second Pbase region 6 by a gate oxide layer 13; the left and right sides of the upper end of the second Pbase region 6 are respectively provided with a P+ ohmic contact region 10 and an N+ ohmic contact region 11; the upper end surfaces of the P+ ohmic contact region 10 and the N+ ohmic contact region 11 are covered with a source metal layer 17, and a gate metal layer 15 is provided above the main gate 14, and the source metal layer 17 and the gate metal layer 15 are not in contact and are isolated by a field oxygen dielectric layer 16. The current limiting auxiliary channel formed by the source auxiliary gate 12 and the Nbase region 8 reduces the current and power density of the device under short-circuit conditions without increasing the on-resistance, improves the short-circuit tolerance of the device, and reduces the gate-drain capacitance of the device, thereby improving the switching speed of the device.
[0073] In this embodiment, the peak concentration of the Pshield region 4 is 5e18cm -3 , the width is 0.5-0.6 μm, and the depth is 0.4-0.6 μm. The best effect is achieved when the width is 0.5 μm.
[0074] In this embodiment, the peak concentration of the first Nwell region 7 is 8e17cm -3 , the width is 0.5-1 μm, and the depth is 0.3-0.4 μm. Preferably, the width is 0.5-1 μm and the depth is 0.3 μm for the best effect.
[0075] In this embodiment, the second Nwell region 9 has a peak concentration of 8e17 cm -3 , the width is 0.5-1 μm, and the depth is 0.4-0.5 μm. Preferably, the width is 0.5 μm and the depth is 0.4 μm for the best effect.
[0076] In this embodiment, the first Pbase region 5 and the second Pbase region 6 are both formed by epitaxy, and the epitaxial concentration of the first Pbase region 5 is ≥ 2e17 cm-3 , thickness 0.9~1μm, second Pbase region 6 epitaxial ≥ concentration 8e16cm -3 , thickness 0.9 to 1 μm. The preferred first Pbase region 5 epitaxial concentration is 2e17 cm -3 , thickness 1μm, second Pbase region 6 epitaxial concentration 8e16cm -3 , the best effect is achieved with a thickness of 0.9μm.
[0077] In this embodiment, the concentration of the P+ ohmic contact region 10 is ≥ 1e19 cm -3 , depth 0.2-0.3 μm, width 0.5-0.6 μm, the concentration of the N+ ohmic contact region 11 is ≥1e19 cm -3 , depth 0.2-0.3 μm, width 0.9-1 μm. Preferably, the width of the P+ ohmic contact region is 0.5 μm, and the width of the N+ ohmic contact region is 1 μm for best results.
[0078] In this embodiment, the peak concentration of Nbase region 8 is 3e17cm -3 , width 0.2-0.4 μm, thickness 0.5-0.6 μm. Preferably, the width is 0.2 μm and the thickness is 0.5 μm for best effect.
[0079] In this embodiment, the drain metal layer 1, the source metal layer 17, and the gate metal layer 15 are made of nickel, titanium, aluminum, or an alloy thereof to improve electrical performance, enhance conductivity, and high-temperature stability.
[0080] In this embodiment, the main gate 14 and the source sub-gate 12 have a width of 0.4-0.5 μm and a thickness of 0.9-1 μm, and the gate oxide layer thickness between the main gate and the source sub-gate is 0.2-0.3 μm. Preferably, the main gate 14 and the source sub-gate 12 have a width of 0.5 μm and a height of 1 μm, and the gate oxide layer thickness between the main gate and the source sub-gate is 0.2 μm for the best effect, and together form a trench region, providing conditions for the source sub-gate 12 and the Nbase region 8 to form a current-limiting sub-channel.
[0081] During operation, when the device is in a short-circuit state, that is, in a saturated conduction state, the drain-source voltage is high, and the potential gradually increases from the source to the drain. At this time, the sub-channel is at a positive potential, and it increases with the increase of the drain-source voltage, while the source sub-gate is grounded. At this time, the source sub-gate potential is lower than the sub-channel potential, and the potential difference increases with the increase of the source-drain voltage. As the potential difference increases, the originally N-type sub-channel will be depleted when the drain-source voltage is large, pinching off the device current path, so that the device saturation conduction current is limited, thereby reducing the power density of the device when it is short-circuited.
[0082] In the linear region, the drain-source voltage is very low, the potential in the auxiliary gate and the auxiliary channel is very close, and the current path formed by the auxiliary channel makes the current in the linear region unaffected, so the device can be turned on normally, and the on-resistance is also unaffected. The source auxiliary gate plays a good shielding role on the main gate, and the present invention can achieve very low gate-drain capacitance and switching loss, and will not have a significant impact on reverse withstand voltage.
[0083] The present invention uses TCAD Silvaco numerical simulation tool to compare with the traditional SiC trench gate MOSFET device. The forward output characteristics of the SiC trench split-gate MOSFET device with enhanced short-circuit withstand provided by the present invention and the traditional SiC trench gate MOSFET device are as follows: Figure 2 As shown, it can be seen that the output characteristic curves of the two devices are basically overlapped when the drain-source voltage is low and the device is in the linear region, which indicates that the on-resistance of the two devices is very close; however, when the drain-source voltage continues to increase, the traditional device gradually tends to saturation after the drain-source voltage reaches about 15V, and the current increases at a slower rate with the voltage, but still gradually increases. However, the SiC trench split-gate MOSFET device with enhanced short-circuit tolerance provided by the present invention becomes saturated after the drain-source voltage reaches about 7V, and the saturation current does not increase significantly with the increase of the drain-source voltage.
[0084] The power density of the two devices is compared with the drain-source voltage when the short circuit occurs based on the saturation current. Figure 3 As shown, as the short-circuit voltage increases, the power density difference between the two devices becomes larger and larger. The SiC trench split-gate MOSFET device with enhanced short-circuit tolerance provided by the present invention can significantly reduce the device power density under the short-circuit state, thereby reducing the heat generation of the device and improving the short-circuit tolerance of the device. The improvement effect is more significant as the drain-source voltage increases.
[0085] like Figure 4 The figure shows the reverse withstand voltage characteristics comparison of the two devices, and it can be seen that the reverse withstand voltage of the SiC trench split-gate MOSFET device with enhanced short-circuit withstand capacity proposed by the present invention is not significantly different from that of the traditional device. Figure 5 The figure shows a comparison of the curves of the gate-drain capacitance of the two devices changing with the drain-source voltage. It can be seen that the gate-drain capacitance of the SiC trench split-gate MOSFET device with enhanced short-circuit tolerance proposed in the present invention is very small, significantly lower than that of the traditional device. This is due to the good shielding effect of the source sub-gate on the bottom capacitance of the main gate. The very low gate-drain capacitance indicates that the switching speed and switching loss of the SiC trench split-gate MOSFET device with enhanced short-circuit tolerance proposed in the present invention are better than those of the traditional devices.
[0086] The method for manufacturing a SiC trench split-gate MOSFET device with enhanced short-circuit tolerance provided by an embodiment of the present invention has a process flow as follows: Figure 6As shown, the structural diagram of the process flow is as follows Figures 7 to 21 As shown, the following steps are included:
[0087] Step 1: After cleaning the silicon carbide N+ substrate 2 using conventional RCA standards, a silicon carbide N- epitaxial layer 3 is formed on the silicon carbide N+ substrate 2 by conventional epitaxial means of doping nitrogen or phosphorus;
[0088] Step 2: forming a Pshield region 4 at the upper left corner of the silicon carbide N-epitaxial layer 3 by three ion implantations, and forming a first Nwell region 7 at the upper right corner of the silicon carbide N-epitaxial layer 3 by two ion implantations;
[0089] Step 3: Forming a first Pbase region 5 on the silicon carbide N-epitaxial layer 3 by epitaxy again.
[0090] Step 4: forming an Nbase region 8 with uniform concentration distribution and a box-shaped distribution at the lower right corner of the first Pbase region 5 by four ion implantations, and forming a second Nwell region 9 with uniform concentration distribution and a box-shaped distribution at the upper right corner of the first Pbase region 5 by three ion implantations;
[0091] Step 5: forming a second Pbase region 6 on the first Pbase region 5 again by epitaxy;
[0092] Step 6: A box-shaped P+ ohmic contact region 10 is formed at the upper left corner of the second Pbase region 6 by four ion implantations, and a box-shaped N+ ohmic contact region 11 is formed at the upper right corner of the second Pbase region 6 by four ion implantations, and the boundary of the N+ ohmic contact region 11 and the P+ ohmic contact region 10 are in contact;
[0093] Step 7: grow and pattern field oxide on the surface of silicon carbide, and form a trench region by etching from the upper right corner of the second Pbase region 6 to the silicon carbide N-epitaxial layer 4;
[0094] Step 8: growing the silicon carbide N-epitaxial layer 3, the first Pbase region 5 and the second Pbase region 6 on the outer surface of the trench to form a gate oxide layer 13 by a dry oxygen process;
[0095] Step 9: forming a source sub-gate 12 above the gate oxide layer at the bottom of the trench by depositing polysilicon;
[0096] Step 10: depositing an oxide layer SiO2 on the source sub-gate 12 to form an insulating medium between split gates of the same material as the gate oxide layer 13;
[0097] Step 11: forming a main gate 14 on the insulating medium by depositing polysilicon;
[0098] Step 12: an oxide layer SiO2 is deposited on the main gate 14 to form an insulating medium between split gates of the same material as the gate oxide layer 13, a source ohmic contact hole is opened, an ohmic contact metal is sputtered, and annealing is performed to form a source ohmic contact;
[0099] Step 13: Open holes above the main gate 14 and the source sub-gate 12 respectively;
[0100] Step 14: thickening the front metal to form ohmic contacts between the main gate 14 and the source sub-gate 12, and patterning the metal to form source and drain electrodes;
[0101] Step 15: Sputtering and laser annealing of the back ohmic contact metal form a drain ohmic contact, and thickening the back metal to form a drain electrode.
[0102] The above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. All equivalent structural changes made by using the contents of the present invention specification and drawings under the concept of the present invention, or directly / indirectly applied in other related technical fields are included in the patent protection scope of the present invention.
Claims
1. A SiC trench split-gate MOSFET device with enhanced short-circuit tolerance, Features: The invention comprises a drain metal layer (1), a silicon carbide N+ substrate (2) and a silicon carbide N-epitaxial layer (3) are sequentially arranged above the drain metal layer (1), a first Pbase region (5) is arranged above the silicon carbide N-epitaxial layer (3), a second Pbase region (6) is arranged above the first Pbase region (5), a second Nwell region (9) and an Nbase region (8) are arranged at the upper right corner and the lower right corner of the first Pbase region (5), respectively, a trench region is arranged on the right side of the silicon carbide N-epitaxial layer (3), the first Pbase region (5) and the second Pbase region (6), a main gate (14) and a source sub-gate (12) are arranged in the trench region from top to bottom, and a current limiting sub-channel is formed between the Nbase region (8) and the source sub-gate (12); A Pshield region (4) and a first Nwell region (7) are respectively arranged at the upper left corner and the upper right corner of the silicon carbide N-epitaxial layer (3); The source sub-gate (12), the main gate (14), the silicon carbide N-epitaxial layer (3), the first Pbase region (5) and the second Pbase region (6) are isolated by a gate oxide layer (13); A P+ ohmic contact region (10) and an N+ ohmic contact region (11) are respectively provided on the left and right sides of the upper end of the second Pbase region (6); The upper end surfaces of the P+ ohmic contact region (10) and the N+ ohmic contact region (11) are covered with a source metal layer (17), a gate metal layer (15) is provided above the main gate (14), and the source metal layer (17) and the gate metal layer (15) are not in contact with each other and are isolated by a field oxide dielectric layer (16).
2. The SiC trench split-gate MOSFET device with enhanced short-circuit withstand capability according to claim 1, Features: The peak concentration of the Pshield region (4) is 5e18cm -3 , width is 0.5~0.6μm, and depth is 0.4~0.6μm.
3. The SiC trench split-gate MOSFET device with enhanced short-circuit withstand capability according to claim 1, Features: The peak concentration of the first Nwell region (7) is 8e17cm -3 , width is 0.5~1μm, and depth is 0.3~0.4μm.
4. The SiC trench split-gate MOSFET device with enhanced short-circuit withstand capability according to claim 1, Features: The second Nwell region (9) has a peak concentration of 8e17 cm -3 , width is 0.5~1μm, and depth is 0.4~0.5μm.
5. The SiC trench split-gate MOSFET device with enhanced short-circuit withstand capability according to claim 1, Features: The first Pbase region (5) and the second Pbase region (6) are both formed by epitaxy, and the epitaxial concentration of the first Pbase region (5) is ≥ 2e17 cm -3 , thickness 0.9~1μm, second Pbase region (6) epitaxial ≥ concentration 8e16cm -3 , thickness 0.9~1μm.
6. The SiC trench split-gate MOSFET device with enhanced short-circuit withstand capability according to claim 1, Features: The concentration of the P+ ohmic contact area (10) is ≥ 1e19 cm -3 , with a depth of 0.2 to 0.3 μm and a width of 0.5 to 0.6 μm, and the concentration of the N+ ohmic contact region (11) is ≥ 1e19 cm -3 , depth 0.2~0.3μm, width 0.9~1μm.
7. The SiC trench split-gate MOSFET device with enhanced short-circuit withstand capability according to claim 1, Features: The peak concentration of the Nbase region (8) is 3e17cm -3 , width 0.2~0.4μm, thickness 0.5~0.6μm.
8. The SiC trench split-gate MOSFET device with enhanced short-circuit withstand capability according to claim 1, Features: The drain metal layer (1), the source metal layer (17) and the gate metal layer (15) are made of nickel, titanium, aluminum or an alloy thereof.
9. The SiC trench split-gate MOSFET device with enhanced short-circuit withstand capability according to claim 1, Features: The main gate (14) and the source sub-gate (12) have a width of 0.4 to 0.5 μm and a thickness of 0.9 to 1 μm, and the thickness of the gate oxide layer between the main gate and the source sub-gate is 0.2 to 0.3 μm.
10. A method for manufacturing a SiC trench split-gate MOSFET device with enhanced short-circuit tolerance, the method comprising manufacturing the SiC trench split-gate MOSFET device with enhanced short-circuit tolerance according to any one of claims 1 to 9, It is characterized in that The following steps are involved: S1: After cleaning the silicon carbide N+ substrate sheet (2), forming a silicon carbide N- epitaxial layer (3) on the silicon carbide N+ substrate sheet (2) by epitaxy; S2: forming a Pshield region (4) at the upper left corner of the silicon carbide N-epitaxial layer (3) by ion implantation, and forming a first Nwell region (7) at the upper right corner of the silicon carbide N-epitaxial layer (3) by ion implantation; S3: forming a first Pbase region (5) on the silicon carbide N-epitaxial layer (3) by epitaxial growth again, S4: forming an Nbase region (8) with uniform concentration distribution in a box shape at the lower right corner of the first Pbase region (5) by ion implantation, and forming a second Nwell region (9) with uniform concentration distribution in a box shape at the upper right corner of the first Pbase region (5) by ion implantation; S5: forming a second Pbase region (6) on the first Pbase region (5) again by epitaxy; S6: forming a P+ ohmic contact region (10) by ion implantation at the upper left corner inside the second Pbase region (6), and forming an N+ ohmic contact region (11) by ion implantation at the upper right corner inside the second Pbase region (6), wherein the left edge of the N+ ohmic contact region (11) contacts the right edge of the P+ ohmic contact region (10); S7: growing and patterning field oxide on the surface of silicon carbide, and etching from the upper right corner of the second Pbase region (6) to the silicon carbide N-epitaxial layer (3) to form a trench region; S8: growing the silicon carbide N-epitaxial layer (3), the first Pbase region (5) and the second Pbase region (6) on the outer surface of the trench to form a gate oxide layer (13) through a dry oxygen process; S9: forming a source sub-gate (12) above the gate oxide layer at the bottom of the trench by depositing polysilicon; S10: forming an insulating medium by depositing an oxide layer above the source sub-gate (12); S11: forming a main gate (14) on the insulating medium by depositing polysilicon; S12: forming an insulating medium by depositing an oxide layer above the main gate (14), opening a source ohmic contact, sputtering an ohmic contact metal, and annealing to form a source ohmic contact; S13: holes are respectively opened above the main gate (14) and the source sub-gate (12); S14: thickening the front metal to form an ohmic contact between the main gate (12) and the source sub-gate (14), and patterning the metal to form a source metal layer (17) and a gate metal layer (15); S15: sputtering of back ohmic contact metal, laser annealing to form a drain ohmic contact, and thickening of the back metal to form a drain metal layer (1).
Citation Information
Patent Citations
A silicon carbide MOSFET device based on a split gate and its fabrication method
CN114597130B
Trench gate SiC MOSFET device structure and preparation method thereof
CN117457739A
Cited By
Groove type SiC MOSFET and preparation method thereof
CN121240492A