Semiconductor structure and manufacturing method thereof
By designing a light control layer containing quantum dots and porous structures in LED microdisplay technology, the problems of light crosstalk and performance improvement are solved, and uniform exit and full color display of light are achieved, which simplifies the process and reduces costs.
Patent Information
- Application Number
- CN202310637539.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-31
- Publication Date
- 2024-12-03
AI Technical Summary
In the existing LED microdisplay technology, the small distance between the core particles leads to a large angle of emitted light, which easily causes light crosstalk, and the manufacturing cost and performance (such as the directionality and uniformity of light) need to be further improved.
Design a semiconductor structure, including a light emitting structure and a light control layer located on one side of the light emitting structure. The light control layer consists of a plurality of regularly arranged light control regions and substrate structures. The light control region includes quantum dots and porous structures and porous structures. The structure is used to adsorb quantum dots, realize wavelength conversion, and improve the uniformity and directionality of light through the substrate structure and light reflective layer.
The uniform light exit is achieved, the light extraction rate is improved, the light crosstalk is avoided, and the full color display is realized through the porous structure, which simplifies the process and reduces costs.
Smart Images

Figure CN119069604A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the field of semiconductor technology, and in particular to a semiconductor structure and a method for manufacturing the same. Background Art
[0002] Micro-LED (Micro Light Emitting Diode) technology is also known as LED micro-display technology. Compared with traditional LED display technology, LED micro-display can reduce the overall system volume and weight, and has a large room for reducing manufacturing costs. At the same time, it has the advantages of low power consumption, high light energy utilization, fast response speed, wide operating temperature range, and strong anti-interference ability.
[0003] However, there are still some technical difficulties in LED micro-display technology: for example, in order to increase the pixel, the distance between the core particles is very small, and the angle of light emission is very large, which easily causes crosstalk between the light of each core particle. In addition, the manufacturing cost and various performances (directivity and uniformity of light, etc.) of LED micro-display technology also need to be further improved. Summary of the invention
[0004] In view of this, an embodiment of the present disclosure provides a semiconductor structure and a method for manufacturing the same.
[0005] According to one aspect of the present disclosure, an embodiment of the present disclosure provides a semiconductor structure, characterized in that it includes:
[0006] Light-emitting structure;
[0007] A light control layer located on one side of the light emitting structure, the light control layer comprising a plurality of regularly arranged light control regions and a substrate structure located between the light control regions;
[0008] The light control region includes a wavelength conversion structure, and the wavelength conversion structure includes quantum dots and a porous structure on which the quantum dots are adsorbed.
[0009] As an optional embodiment, the material of the substrate structure includes silicon, and the material of the porous structure includes porous silicon oxide.
[0010] As an optional embodiment, the porous structure has holes capable of adsorbing quantum dots, and the holes are columnar, and the angle between the holes and the plane where the substrate is located is 60° to 120°.
[0011] As an optional embodiment, the light control region further includes an opening penetrating the light control region, and the opening and the wavelength conversion structure are arranged in a horizontal direction and separated by the substrate structure.
[0012] As an optional embodiment, the light control layer, the light control area and the substrate structure have the same thickness.
[0013] As an optional embodiment, the thickness of the light control layer is less than or equal to 50 μm.
[0014] As an optional embodiment, the light control area includes a first color light area, a second color light area and a third color light area which are spaced apart in the horizontal direction.
[0015] As an optional embodiment, the aperture ratios of the first color light area, the second color light area, and the third color light area are the same or different.
[0016] As an optional embodiment, a light reflecting layer is provided on the side wall of the light control area.
[0017] As an optional embodiment, the sidewalls of the light control area are inclined sidewalls, so that the equivalent diameter of the light control area increases in the direction in which light travels.
[0018] As an optional embodiment, the light emitting structure includes: a first semiconductor layer, an active layer, a second semiconductor layer, and at least one group of a first electrode and a second electrode;
[0019] The first electrode is connected to the first semiconductor layer and is blocked from the second semiconductor layer and the active layer by an insulating material;
[0020] The second electrode is connected to the second semiconductor layer and is blocked from the first electrode by an insulating material.
[0021] As an optional embodiment, the light-emitting structure has a plurality of light-emitting units, an insulating structure is provided between two adjacent light-emitting units, and a thickness of the insulating structure is less than or equal to a thickness of the light-emitting structure.
[0022] According to another aspect of the present disclosure, an embodiment of the present disclosure provides a method for manufacturing a semiconductor structure, characterized in that it includes the following steps:
[0023] S1. Provide a silicon substrate;
[0024] S2, forming a light emitting structure on one side of the silicon substrate;
[0025] S3, thinning the silicon substrate from the other side away from the light emitting structure;
[0026] S4, forming a plurality of regularly arranged light control regions in the remaining silicon substrate to form a light control layer, wherein the light control layer further comprises a substrate structure located between the light control regions;
[0027] The light control region includes a wavelength conversion structure, and the wavelength conversion structure includes quantum dots and a porous structure on which the quantum dots are adsorbed.
[0028] As an optional embodiment, the method for preparing the porous structure is to thin the silicon substrate and then perform etching on a side of the silicon substrate away from the light-emitting structure.
[0029] As an optional embodiment, the step S4 further includes:
[0030] S41, oxidizing the porous structure;
[0031] S42, filling quantum dots in the oxidized porous structure to form a wavelength conversion structure.
[0032] As an optional embodiment, the step S1 further includes:
[0033] S11, providing a silicon substrate;
[0034] S12, preparing holes on a side of the silicon substrate away from the growth surface to form a plurality of regularly arranged porous structures.
[0035] As an optional embodiment, the step S2 is to form a light-emitting structure on one side of the silicon substrate including the porous structure, and the step S3 is to thin the silicon substrate from the other side away from the light-emitting structure until the porous structure is exposed.
[0036] As an optional embodiment, the step S3 further includes:
[0037] S31, thinning the silicon substrate from the other side away from the light emitting structure;
[0038] S32, preparing holes on a side of the thinned silicon substrate away from the light-emitting structure to form a plurality of regularly arranged porous structures.
[0039] As an optional embodiment, the step S2 further includes:
[0040] S21, sequentially growing a first semiconductor layer, an active layer, and a second semiconductor layer on one side of the silicon substrate;
[0041] S22, forming at least one filling groove on a side of the second semiconductor layer away from the silicon substrate, wherein the filling groove completely penetrates the second semiconductor layer and the active layer, and partially penetrates the first semiconductor layer;
[0042] S23, manufacturing a first electrode in the filling groove, wherein the first electrode is insulated and blocked from the second semiconductor layer and the active layer, and the first electrode is connected to the first semiconductor layer;
[0043] S24. Fabricate a second electrode on a side of the second semiconductor layer away from the active layer, wherein the second electrode is insulated and blocked from the first electrode.
[0044] As an optional embodiment, the step S21 further includes:
[0045] S211. Form an insulating structure between two adjacent light-emitting units on a side of the second semiconductor layer away from the silicon substrate, wherein a thickness of the insulating structure is less than or equal to a thickness of the light-emitting structure.
[0046] The present disclosure provides a semiconductor structure and a manufacturing method thereof, wherein the semiconductor structure includes a light-emitting structure; a light-control layer located on one side of the light-emitting structure, the light-control layer includes a plurality of regularly arranged light-control regions and a substrate structure located between the light-control regions; wherein the light-control region includes a wavelength conversion structure, the wavelength conversion structure includes quantum dots and a porous structure adsorbed with the quantum dots. In the present disclosure, a plurality of light-control regions and a substrate structure are provided, so that the light output of each light-control region is uniform, has good directionality, and has a high light extraction rate, thereby avoiding light crosstalk; the porous structure is used to adsorb quantum dots to achieve full-color display, which can improve resolution, simplify the process, and save costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] Figures 1a to 1f Shown is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure;
[0048] Figure 2 Shown is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure;
[0049] Figure 3 Shown is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure;
[0050] Figure 4 Shown is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure;
[0051] Figure 5 Shown is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure;
[0052] Figure 6 Shown is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure;
[0053] Figure 7 Shown is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure;
[0054] Figure 8 Shown is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure;
[0055] Fig. 9 Shown is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure;
[0056] Fig.10 Shown is a flow chart of a semiconductor structure manufacturing method provided by an embodiment of the present disclosure;
[0057] Figure 11-21 The figure shows a schematic diagram of the decomposition of a semiconductor structure provided by an embodiment of the present disclosure during the preparation process. DETAILED DESCRIPTION
[0058] The following will be combined with the drawings in the embodiments of the present disclosure to clearly and completely describe the technical solutions in the embodiments of the present disclosure. Obviously, the described embodiments are only part of the embodiments of the present disclosure, not all of the embodiments. Based on the embodiments in the present disclosure, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present disclosure.
[0059] In order to solve the technical problem of light crosstalk in the prior art, the present disclosure provides a semiconductor structure and a manufacturing method thereof, wherein the semiconductor structure includes a light-emitting structure; a light-control layer located on one side of the light-emitting structure, the light-control layer includes a plurality of regularly arranged light-control regions and a substrate structure located between the light-control regions; wherein the light-control region includes a wavelength conversion structure, the wavelength conversion structure includes quantum dots and a porous structure adsorbed with quantum dots. In the present disclosure, multiple light-control regions and substrate structures are provided, so that the light output of each light-control region is uniform, has good directionality, and has a high light extraction rate, thereby avoiding light crosstalk; the porous structure is used to adsorb quantum dots to achieve full-color display, which can improve resolution, simplify the process, and save costs.
[0060] Below is a combination of Figures 1 to Fig.21 A semiconductor structure and a manufacturing method thereof mentioned in the present disclosure are further illustrated by way of example.
[0061] Figures 1a to 1f FIG. 1 is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure. Figure 1a As shown, the semiconductor structure includes: a light-emitting structure 200; a light-control layer 300 located on one side of the light-emitting structure 200, the light-control layer 300 includes a plurality of regularly arranged light-control regions 301 and a substrate structure 101 located between the light-control regions 301; wherein the light-control regions 301 include a wavelength conversion structure, the wavelength conversion structure includes quantum dots and a porous structure on which the quantum dots are adsorbed.
[0062] In this embodiment, Figure 1aAs shown, the light-emitting structure 200 includes a first semiconductor layer 201, an active layer 202, a second semiconductor layer 203, at least one group of first electrodes 205 and second electrodes 206; the first electrode 205 is connected to the first semiconductor layer 201, and is blocked from the second semiconductor layer 203 and the active layer 202 by an insulating material 207; the second electrode 206 is connected to the second semiconductor layer 203, and is blocked from the first electrode 205 by an insulating material 207; the light-emitting structure 200 has a plurality of light-emitting units, an insulating structure 204 is provided between two adjacent light-emitting units, the thickness of the insulating structure 204 is less than or equal to the thickness of the light-emitting structure 200, and each light control area 301 corresponds to at least one light-emitting unit.
[0063] In this embodiment, Figure 1a As shown, the insulating structure 204 completely penetrates the first semiconductor layer 201 from the side of the second semiconductor layer 203 away from the light control layer 300, so that the light-emitting units are isolated from each other and the edge non-radiative recombination is reduced. Other embodiments can also achieve the same technical effect. The insulating structure 204 can partially penetrate the first semiconductor layer 201, such as Figure 1b As shown; the insulating structure 204 may completely penetrate the active layer 202, such as Figure 1c As shown; the insulating structure 204 may partially penetrate the active layer 202, such as Figure 1d As shown; the insulating structure 204 may completely penetrate the second semiconductor layer 203, such as Figure 1e As shown; the insulating structure 204 may partially penetrate the second semiconductor layer 203, such as Figure 1f shown.
[0064] In this embodiment, the materials of the first semiconductor layer 201 and the second semiconductor layer 203 are group III nitride materials, and the materials of the first semiconductor layer 201 and the second semiconductor layer 203 can be the same or different. The first semiconductor layer 201 is an n-type layer, and the doped n-type ions can be at least one of Si ions, Ge ions, Sn ions, Se ions or Te ions. The second semiconductor layer 203 is a p-type layer, and the doped p-type ions can be at least one of Mg ions, Zn ions, Ca ions, Sr ions or Ba ions. The active layer 202 includes a barrier layer and a potential well layer, and the bandgap width of the barrier layer is greater than the bandgap width of the potential well layer. For example, the material of the barrier layer is GaN, and the material of the potential well layer is InGaN.
[0065] In this embodiment, the material of the substrate structure 101 includes silicon, the material of the porous structure includes silicon oxide, the porous structure is prepared in the silicon material, and the quantum dots are filled in the porous structure after oxidation to form an intermittently arranged and transparent light control area 301, and there is no need to peel off the substrate and re-prepare the transparent light control area, which simplifies the process. The light control layer 300, the light control area 301 and the substrate structure 101 have the same thickness, and the thickness of the light control layer 300 is less than or equal to 50μm.
[0066] In this embodiment, Figure 2 FIG. 1 is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure, such as Figure 2 As shown, the porous structure has holes 302 that can absorb quantum dots. The holes 302 are columnar, and the angle between them and the plane where the substrate 100 is located is 60° to 120°. The holes 302 can be columnar perpendicular to the plane where the silicon substrate 100 is located, or they can be inclined columns at a certain angle to the plane where the silicon substrate 100 is located. By adjusting the angle of the holes 302, the light output direction is adjusted, the light output angle is increased, and the light output efficiency of the device is improved. The projection shape of the holes 302 on the plane where the silicon substrate 100 is located can be any one or more of a circle, an ellipse, a polygon, a strip, or a mesh.
[0067] In this embodiment, Figure 3 FIG. 1 is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure, such as Figure 3 As shown, the light control area 301 includes a first color light area 3011, a second color light area 3012 and a third color light area 3013 which are spaced apart in the horizontal direction. Optionally, the first color light is red, the second color light is green, and the third color light is blue, but it is not limited thereto.
[0068] Specifically, Figure 3 As shown, the light emitted by the light emitting structure 200 can be white light, and red quantum dots are filled in the porous structure of the first color light region 3011 to form a red light region, green quantum dots are filled in the porous structure of the second color light region 3012 to form a green light region, and blue quantum dots are filled in the porous structure of the third color light region 3013 to form a blue region, thereby forming three primary colors and realizing full-color LED. By using the porous structure to adsorb quantum dots, there is no need to fill photoresist, which simplifies the process and saves costs.
[0069] Optionally, the light control region 301 further includes an opening penetrating the light control region 301, and the opening and the wavelength conversion structure are arranged in a horizontal direction and separated by the substrate structure 101. Figure 4 As shown, the light emitted by the light emitting structure 200 may also be blue light, the first color light region 3011 is a wavelength conversion structure, red quantum dots are filled in the porous structure of the first color light region 3011 to form a red light region, the second color light region 3012 is a wavelength conversion structure, green quantum dots are filled in the porous structure of the second color light region 3012 to form a green light region, and the third color light region 3013 is an opening filled with photoresist to form a blue light region, thereby forming three primary colors to realize a full-color LED; Figure 5As shown, the light emitted by the light-emitting structure 200 can also be blue light and green light. The first color light region 3011 is a wavelength conversion structure. Red quantum dots are filled in the porous structure of the first color light region 3011 to form a red light region. The second color light region 3012 is an opening filled with photoresist to form a green light region. The third color light region 3013 is an opening filled with photoresist to form a blue light region, thereby forming three primary colors to realize a full-color LED.
[0070] In this embodiment, Figure 6 The figure shows a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure, in which the hole ratios of the first color light region 3011, the second color light region 3012, and the third color light region 3013 are the same or different. In the green light spectrum region near the wavelength of 555nm, the sensitivity of the human eye is the highest, while in regions with longer wavelengths (such as red light) or shorter wavelengths (such as blue light), the sensitivity of the human eye decreases, which means that higher radiation power is required in these wavelength regions to obtain the same brightness perception. By changing the hole ratios of different color light regions, the quantum dot content of different color light regions can be changed, thereby adjusting the brightness perception of different luminous wavelength regions. Figure 6 As shown, the hole ratios of the first color light region 3011 emitting red light and the third color light region 3013 emitting blue light are designed to be greater than the hole ratio of the second color light region 3012 emitting green light, thereby improving the brightness perception of red light and blue light.
[0071] In this embodiment, one light control area 301 corresponds to one light emitting unit, that is, Figure 1a As shown. In other embodiments, one light control area 301 may correspond to multiple light emitting units. When one light emitting unit is disconnected, other light emitting units can still emit light normally, avoiding the common "bad pixel" problem in the display field. The number of light emitting units corresponding to the light control area 301 is not particularly limited, and at least one light emitting unit is sufficient. The number of light emitting units corresponding to the light control area 301 can be selected according to the specific device application requirements.
[0072] In some embodiments, Figure 7 FIG. 1 is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure, such as Figure 7 As shown, the side wall of the light control area 301 is provided with a light reflecting layer 102. The material of the reflecting layer 102 can be silver, aluminum, nickel or one of other metals that reflect light, or a metal alloy or metal combination layer composed of multiple metals, or an alloy superlattice structure.
[0073] In some embodiments, Figure 8 FIG. 1 is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure, such as Figure 8As shown, the sidewall of the light control region 301 is an inclined sidewall, so that the equivalent diameter of the light control region 301 increases in the direction of light travel. The sidewall of the light control region 301 is formed as an inclined sidewall. Since the sidewall is inclined, the equivalent diameter of the space surrounded by the inclined sidewall can be increased in the direction of light travel, thereby improving the light extraction efficiency of the semiconductor device.
[0074] In some embodiments, Fig. 9 FIG. 1 is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure, such as Fig. 9 As shown, the sidewalls of the light control region 301 are inclined sidewalls, so that the equivalent diameter of the light control region 301 increases in the direction of light travel, and the sidewalls of the light control region 301 are provided with a light reflection layer 102, further improving the light extraction efficiency of the device.
[0075] According to another aspect of the present disclosure, Fig.10 FIG. 1 is a flow chart of a semiconductor structure manufacturing method provided by an embodiment of the present disclosure. Figure 11-21 FIG. 1 is a schematic diagram of a semiconductor structure provided by an embodiment of the present disclosure during the preparation process. Fig.10 As shown, a semiconductor structure manufacturing method provided by an embodiment of the present disclosure includes the following steps:
[0076] Step S1: Fig.11 As shown, a silicon substrate 100 is provided.
[0077] Step S2: forming a light emitting structure 200 on one side of the silicon substrate 100. The light emitting structure 200 includes a first semiconductor layer 201, an active layer 202, a second semiconductor layer 203, and at least one set of a first electrode 205 and a second electrode 206. Specifically:
[0078] Step S21: Fig.12 As shown, a first semiconductor layer 201, an active layer 202, and a second semiconductor layer 203 are sequentially grown on one side of a silicon substrate.
[0079] The formation process of the first semiconductor layer 201, the active layer 202, and the second semiconductor layer 203 may include: atomic layer deposition (ALD), chemical vapor deposition (CVD), molecular beam epitaxy (MBE), plasma enhanced chemical vapor deposition (PECVD), low pressure chemical vapor deposition (LPCVD), metal-organic chemical vapor deposition (MOCVD), or a combination thereof.
[0080] Step S211: Fig.13 As shown, an insulating structure 204 is formed between two adjacent light-emitting units on the side of the second semiconductor layer 203 away from the silicon substrate 100, and the thickness of the insulating structure 204 is less than or equal to the thickness of the light-emitting structure 200. The insulating structure 204 can be formed by ion implantation, and the implanted ions include at least one of hydrogen ions, helium ions, nitrogen ions, and fluorine ions. Optionally, the method for forming the insulating structure 204 between two adjacent light-emitting units may be to etch a groove between the two adjacent light-emitting units and then fill it with an insulating material 207. The method for forming the insulating structure 204 is not limited thereto.
[0081] Step S22: Fig.14 As shown, at least one filling groove 2051 is formed on a side of the second semiconductor layer 203 away from the silicon substrate 100 , and the filling groove 2051 completely penetrates the second semiconductor layer 203 and the active layer 202 , and partially penetrates the first semiconductor layer 201 .
[0082] Step S23 : manufacturing a first electrode 205 in the filling groove 2051 , wherein the first electrode 205 is insulated and blocked from the second semiconductor layer 203 and the active layer 202 , and the first electrode 205 is connected to the first semiconductor layer 201 .
[0083] Step S24 : forming a second electrode 206 on a side of the second semiconductor layer 203 away from the active layer 202 , and the second electrode 206 is insulated and blocked from the first electrode 205 .
[0084] In this embodiment, Fig.15As shown, an insulating material 207 is provided between the first electrode 205 and the side wall of the filling groove 2051 , thereby achieving insulation blocking between the first electrode 205 and the second semiconductor layer 203 and the active layer 202 , and connecting the first electrode 205 to the first semiconductor layer 201 .
[0085] In this embodiment, the insulating material 207 may be silicon dioxide or silicon nitride, but is not limited thereto and may be any other suitable insulating material. Specifically, the insulating material 207 that can play a role of electrical disconnection may be formed directly in the filling groove 2051 by chemical vapor deposition or the like, without having to achieve the necessary electrical disconnection through filling, etching or the like processes.
[0086] Furthermore, the electrode materials for making the first electrode 205 and the second electrode 206 may be metals or multilayer metals such as gold, copper, silver, zinc, platinum, tantalum, titanium, aluminum, tungsten, and nickel, and the embodiments of the present disclosure are not limited thereto.
[0087] Step S3: Fig.16 As shown, the silicon substrate 100 is thinned from the other side away from the light emitting structure 200. After the silicon substrate 100 is thinned, the thickness of the remaining silicon substrate is less than or equal to 50 μm.
[0088] Step S4: Fig.17 As shown, a plurality of regularly arranged light control regions 301 are formed in the remaining silicon substrate to form a light control layer 300. The light control layer 300 also includes a substrate structure 101 located between the light control regions 301. The light control regions 301 include a wavelength conversion structure. The wavelength conversion structure includes quantum dots and a porous structure on which the quantum dots are adsorbed.
[0089] Specifically, the remaining silicon substrate has a porous structure, and step S4 further includes:
[0090] Step S41: oxidizing the porous structure.
[0091] Step S42: filling quantum dots in the oxidized porous structure to form a wavelength conversion structure 301. The porous structure is formed by oxidizing the silicon material of the silicon substrate 100 into silicon oxide material, which can absorb quantum dots to form a full-color LED, and the porous structure is a transparent silicon oxide material, which does not affect the light emission.
[0092] In some embodiments, the porous structure is prepared before forming the light emitting structure 200. Step S1 further includes:
[0093] S11: Fig.11 As shown, a silicon substrate 100 is provided.
[0094] S12: Fig.18As shown, holes 302 are prepared on a side of the silicon substrate 100 away from the growth surface to form a plurality of regularly arranged porous structures.
[0095] The present embodiment does not limit the preparation method of porous silicon, and any preparation method of porous silicon that can be obtained by a person skilled in the art can be used in the present invention, such as electrochemical etching (or anodic oxidation), chemical vapor etching, hydrothermal etching, chemical etching (or dyeing), etc. Preferably, the method for preparing the hole 302 can be electrochemical etching, using platinum wire or graphite as a cathode and a single crystal silicon wafer as an anode, electrochemical etching is performed in a mixed solution containing HF acid, and after thinning the silicon substrate 100, electrochemical etching is performed on the side of the silicon substrate 100 away from the light-emitting structure 200 to prepare the hole 302. The electrochemical etching method does not require electrodes and autoclaves, and the operation process is safe and convenient, and it is easy to combine with current industrial production equipment.
[0096] In this embodiment, the hole 302 may be a columnar shape perpendicular to the plane where the silicon substrate 100 is located, or may be an inclined columnar shape at a certain angle to the plane where the silicon substrate 100 is located. The projection shape of the hole 302 on the plane where the silicon substrate 100 is located may be any one or more of a circle, an ellipse, a polygon, a strip, or a mesh.
[0097] In this embodiment, Fig.19 As shown, step S2 is to form a light emitting structure 200 on one side of the silicon substrate 100 including the porous structure, such as Fig. 20 As shown, step S3 is to thin the silicon substrate 100 from the other side away from the light emitting structure 200 until the porous structure is exposed.
[0098] In some embodiments, the porous structure is prepared after thinning the silicon substrate 200. Step S3 further includes:
[0099] S31, such as Fig.16 As shown, the silicon substrate 100 is thinned from the other side away from the light emitting structure 200 .
[0100] S32, such as Fig. 20 As shown, holes 302 are prepared on the side of the thinned silicon substrate away from the light emitting structure 200 to form a plurality of regularly arranged porous structures.
[0101] The present embodiment does not limit the preparation method of porous silicon, and any preparation method of porous silicon that can be obtained by a person skilled in the art can be used in the present invention, such as electrochemical etching (or anodic oxidation), chemical vapor etching, hydrothermal etching, chemical etching (or dyeing), etc. Preferably, the method for preparing the hole 302 can be electrochemical etching, using platinum wire or graphite as a cathode and a single crystal silicon wafer as an anode, electrochemical etching is performed in a mixed solution containing HF acid, and after thinning the silicon substrate 100, electrochemical etching is performed on the side of the silicon substrate 100 away from the light-emitting structure 200 to prepare the hole 302. The electrochemical etching method does not require electrodes and autoclaves, and the operation process is safe and convenient, and it is easy to combine with current industrial production equipment.
[0102] In this embodiment, the hole 302 may be a columnar shape perpendicular to the plane where the silicon substrate 100 is located, or may be an inclined columnar shape at a certain angle to the plane where the silicon substrate 100 is located. The projection shape of the hole 302 on the plane where the silicon substrate 100 is located may be any one or more of a circle, an ellipse, a polygon, a strip, or a mesh.
[0103] In some embodiments, the light reflection layer 102 can be prepared between the light control region 301 and the substrate structure 101 by etching a groove and filling the groove. Figure 7 As shown, the material of the reflective layer 102 can be silver, aluminum, nickel or other metals that reflect light, or a metal alloy or metal combination layer composed of multiple metals, or an alloy superlattice structure.
[0104] In some embodiments, the sidewalls of the light control region 301 may be designed to be inclined sidewalls, so that the diameter of the light control region 301 increases in the direction in which light travels. Figure 8 As shown, the sidewalls of light control region 301 are formed as inclined sidewalls. Since the sidewalls are inclined, the diameter of the space surrounded by the inclined sidewalls can be increased in the direction in which light travels, thereby improving the light extraction efficiency of the semiconductor device.
[0105] In some embodiments, the sidewalls of the light control region 301 can be designed to be inclined sidewalls so that the diameter of the light control region 301 increases in the direction of light travel, and a light reflection layer 102 is prepared between the light control region 301 and the substrate structure 101, such as Fig. 9 As shown, the light extraction efficiency of the device is further improved.
[0106] The semiconductor structure in the embodiment of the present disclosure needs to be driven by an external driving circuit 400 to emit light. Fig.21As shown, specifically, the first electrode 205 and the second electrode 206 can be connected to the electrode bonding pad 402 in the external driving circuit 400 through the conductive structure 401. In addition, the driving circuit 400 can be made into an active drive or a passive drive. The active drive method has a faster response speed and is not limited by the number of scanning electrodes. Each pixel unit can be addressed and controlled independently, which is suitable for most applications. The passive drive method uses a line-by-line scanning method for display, which has a lower production cost and technical threshold, but cannot achieve high-resolution display well.
[0107] According to another aspect of the present disclosure, the present disclosure also provides a display panel, including the above-mentioned semiconductor structure, the holes 302 in the light control area 301 in the middle part of the display panel are columnar and perpendicular to the plane where the silicon substrate 100 is located, and the holes 302 in the light control area 301 at the edge part of the display panel are columnar and form a certain angle with the plane where the silicon substrate 100 is located, and are inclined toward the middle of the display panel, thereby alleviating the problem of uneven display caused by light leakage in the edge area.
[0108] In summary, the present disclosure provides a semiconductor structure and a manufacturing method thereof, wherein the semiconductor structure includes a light-emitting structure; a light-control layer located on one side of the light-emitting structure, the light-control layer includes a plurality of regularly arranged light-control regions and a substrate structure located between the light-control regions; wherein the light-control region includes a wavelength conversion structure, the wavelength conversion structure includes quantum dots and a porous structure adsorbed with quantum dots. In the present disclosure, multiple light-control regions and substrate structures are provided, so that the light output of each light-control region is uniform, has good directionality, and has a high light extraction rate, thereby avoiding light crosstalk; the porous structure is used to adsorb quantum dots to achieve full-color display, which can improve resolution, simplify the process, and save costs.
[0109] It should be understood that the term "including" and its variations used in the present disclosure are open inclusions, that is, "including but not limited to". The term "one embodiment" means "at least one embodiment"; the term "another embodiment" means "at least one other embodiment". In this specification, the schematic expressions of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, unless they are contradictory.
[0110] The above description is only a preferred embodiment of the present disclosure and is not intended to limit the present disclosure. Any modifications, equivalent substitutions, etc. made within the spirit and principles of the present disclosure should be included in the protection scope of the present disclosure.
Claims
1. A semiconductor structure, characterized in that: include: A light emitting structure (200); A light control layer (300) located on one side of the light emitting structure (200), the light control layer (300) comprising a plurality of regularly arranged light control regions (301) and a substrate structure (101) located between the light control regions (301); Wherein, the light control area (301) includes a wavelength conversion structure, and the wavelength conversion structure includes quantum dots and a porous structure on which the quantum dots are adsorbed.
2. The semiconductor structure according to claim 1, characterized in that: The material of the substrate structure (101) includes silicon, and the material of the porous structure includes porous silicon oxide.
3. The semiconductor structure according to claim 1, characterized in that: The porous structure has holes (302) capable of adsorbing quantum dots, and the holes (302) are columnar, and the angle between the holes (302) and the plane where the substrate (100) is located is 60° to 120°.
4. The semiconductor structure according to claim 1, characterized in that: The light control region (301) further comprises an opening penetrating the light control region (301), and the opening and the wavelength conversion structure are arranged in a horizontal direction and separated by the substrate structure (101).
5. The semiconductor structure according to claim 1, characterized in that: The light control layer (300), the light control region (301) and the substrate structure (101) have the same thickness.
6. The semiconductor structure according to claim 1, characterized in that: The thickness of the light control layer (300) is less than or equal to 50 μm.
7. The semiconductor structure according to claim 1, characterized in that: The light control area (301) comprises a first color light area (3011), a second color light area (3012) and a third color light area (3013) which are distributed at intervals in the horizontal direction.
8. The semiconductor structure according to claim 7, characterized in that: The hole ratios of the first color light area (3011), the second color light area (3012) and the third color light area (3013) are the same or different.
9. The semiconductor structure according to claim 1, characterized in that: A light reflecting layer (102) is provided on the side wall of the light control area (301).
10. The semiconductor structure according to claim 1, characterized in that: The sidewalls of the light control region (301) are inclined sidewalls, so that the equivalent diameter of the light control region (301) increases in the direction in which light travels.
11. The semiconductor structure according to claim 1, characterized in that: The light emitting structure (200) comprises: a first semiconductor layer (201), an active layer (202), a second semiconductor layer (203), and at least one group of a first electrode (205) and a second electrode (206); The first electrode (205) is connected to the first semiconductor layer (201), and is blocked from the second semiconductor layer (203) and the active layer (202) by an insulating material (207); The second electrode (206) is connected to the second semiconductor layer (203) and is blocked from the first electrode (205) by an insulating material (207).
12. The semiconductor structure according to claim 1, characterized in that: The light-emitting structure (200) has a plurality of light-emitting units, an insulating structure (204) is provided between two adjacent light-emitting units, and the thickness of the insulating structure (204) is less than or equal to the thickness of the light-emitting structure (200).
13. A method for manufacturing a semiconductor structure, characterized in that: The following steps are involved: S1. providing a silicon substrate (100); S2, forming a light emitting structure (200) on one side of the silicon substrate (100); S3, thinning the silicon substrate (100) from the other side away from the light emitting structure (200); S4, forming a plurality of regularly arranged light control regions (301) in the remaining silicon substrate to form a light control layer (300), wherein the light control layer (300) further comprises a substrate structure (101) located between the light control regions (301); Wherein, the light control area (301) includes a wavelength conversion structure, and the wavelength conversion structure includes quantum dots and a porous structure on which the quantum dots are adsorbed.
14. The method for manufacturing a semiconductor structure according to claim 13, characterized in that: The method for preparing the porous structure comprises: after thinning the silicon substrate (100), etching is performed on a side of the silicon substrate (100) away from the light-emitting structure (200).
15. The method for manufacturing a semiconductor structure according to claim 13, characterized in that: The step S4 further comprises: S41, oxidizing the porous structure; S42, filling quantum dots in the oxidized porous structure to form a wavelength conversion structure.
16. The method for manufacturing a semiconductor structure according to claim 13, characterized in that: The step S1 further comprises: S11, providing a silicon substrate (100); S12, preparing holes (302) on a side of the silicon substrate (100) away from the growth surface to form a plurality of regularly arranged porous structures.
17. A method for manufacturing a semiconductor structure according to claim 16, characterized in that: The step S2 is to form a light emitting structure (200) on one side of the silicon substrate (100) including the porous structure, and the step S3 is to thin the silicon substrate (100) from the other side away from the light emitting structure (200) until the porous structure is exposed.
18. The method for manufacturing a semiconductor structure according to claim 13, characterized in that: The step S3 further comprises: S31, thinning the silicon substrate (100) from the other side away from the light emitting structure (200); S32, preparing holes (302) on a side of the thinned silicon substrate away from the light-emitting structure (200) to form a plurality of regularly arranged porous structures.
19. The method for manufacturing a semiconductor structure according to claim 13, characterized in that: The step S2 further comprises: S21, sequentially growing a first semiconductor layer (201), an active layer (202), and a second semiconductor layer (203) on one side of the silicon substrate (100); S22, forming at least one filling groove (2051) on a side of the second semiconductor layer (203) away from the silicon substrate (100), wherein the filling groove (2051) completely penetrates the second semiconductor layer (203) and the active layer (202), and partially penetrates the first semiconductor layer (201); S23, manufacturing a first electrode (205) in the filling groove (2051), wherein the first electrode (205) is insulated and blocked from the second semiconductor layer (203) and the active layer (202), and the first electrode (205) is connected to the first semiconductor layer (201); S24. A second electrode (206) is fabricated on a side of the second semiconductor layer (203) away from the active layer (202), wherein the second electrode (206) is insulated and blocked from the first electrode (205).
20. The method for manufacturing a semiconductor structure according to claim 19, characterized in that: The step S21 further comprises: S211. An insulating structure (204) is formed between two adjacent light-emitting units on a side of the second semiconductor layer (203) away from the silicon substrate (100), wherein the thickness of the insulating structure (204) is less than or equal to the thickness of the light-emitting structure (200).