Method for detecting deviation of PCB (Printed Circuit Board) molding routing board

By making detection units and forming detection slots on PCB production boards, efficient early warning and rapid screening of gong biases are achieved, and the treatment of defective products is solved, which is the problem of low efficiency and high cost caused by gong biases in the existing technology is improved. Production efficiency and product quality.

CN119072011AActive Publication Date: 2024-12-03JIANGMEN SUNTAK CIRCUIT TECH
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411176102.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-12-03
Estimated Expiration
2044-08-26

AI Technical Summary

Technical Problem

During the PCB manufacturing process, due to the material and process characteristics, the shrinkage coefficient of the gong plate is mismatched, which is easy to cause the gong to deviate. The existing technology lacks methods to early warning and efficient screening of unqualified products, resulting in low efficiency and high cost.

Method used

The detection unit is made on the production board, including two parallel first PADs and a vertically extended second PAD, to form a detection groove, and during the molding process, the gong passes through the detection groove to visually check whether there is copper exposed on the groove wall. Identify gong bias, replace equipment measurement, improve efficiency and reduce costs.

Benefits of technology

Through visual inspection of the detection slot, the gong deviation can be quickly identified and early warning can be made, which improves production efficiency and reduces labor costs. The deviation direction is confirmed through the exposed copper position of the groove wall, adjusts the processing parameters of the gong plate, and improves product quality .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119072011A_ABST
    Figure CN119072011A_ABST
Patent Text Reader

Abstract

The invention discloses a PCB forming routing deviation detection method, which comprises the following steps that when each layer of circuit is manufactured on a production board, a detection unit is manufactured on a process edge, the detection unit comprises two first PADs which are arranged in parallel and a second PAD which is arranged at one end of the first PADs at an interval, and the second PAD is perpendicular to the first PADs; manufacturing a solder mask layer on the production board, and windowing the solder mask layer at a position corresponding to the detection unit so as to expose the detection unit; in the process of forming and milling the board, milling grooves between the two first PADs and between the first PADs and the second PADs together so as to mill through the production board to form a detection groove; the vertical distance between the groove edge of the detection groove and the first PAD and the vertical distance between the groove edge of the detection groove and the second PAD are both smaller than the minimum vertical distance between in-board copper and the appearance edge. Whether the board is deviated is determined by observing whether copper is exposed on the groove wall. According to the method, visual inspection can be used for replacing quadratic element machine equipment to measure, inspect and screen products, the product disposal efficiency is improved, and the cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of printed circuit board manufacturing, and in particular to a method for detecting the deviation of a PCB forming gong plate. Background Art

[0002] PCB gong board forming is a common machining method. The board from the previous process is placed on the gong machine, and the SET board or PCS board on the circuit board is separated from the substrate by the high-speed rotation and vacuum adsorption of the gong cutter, thereby realizing the forming of the circuit board; in the PCB industry, the distance from the outer edge (i.e. the cutting edge) to the copper inside the board is designed to be ≤0.2mm, and the outer dimension tolerance from edge to edge is ±0.1mm. The outer dimension requirements are high, and the gong is not allowed to be offset and the copper is exposed. When the gong board is made in the forming process, the gong board operation is generally performed according to the expansion and contraction coefficient provided by the previous process. This processing method has the advantages of high efficiency and low cost, and is widely used in the PCB manufacturing industry.

[0003] However, the above production method has the following disadvantages:

[0004] During the PCB manufacturing process, due to the characteristics of materials, processes, etc., some processes produce different amounts of expansion and shrinkage. If the operation is only based on the expansion and shrinkage coefficient of the previous process, there is a large mismatch between the expansion and shrinkage coefficient of the previous process and the actual expansion and shrinkage coefficient during the PCB manufacturing process. If the production process is completely in accordance with the expansion and shrinkage coefficient provided by the previous process, it is very easy to cause the product to be scrapped due to PCB deviation. When the board is PCB-deflected and copper is exposed, there is a lack of a method that can warn of the risk of PCB deviation in advance, and use visual inspection after the PCB deviation is found to be exposed, and quickly screen out unqualified products. Usually, the entire outer shape of each molded board is measured with a two-dimensional measuring equipment for product selection and disposal, which is inefficient and has high labor costs. It is also impossible to give a warning of PCB deviation in advance, and the problem can only be dealt with after the PCB deviation and copper exposure occurs. Summary of the invention

[0005] In view of the above-mentioned existing technical defects, the present invention provides a method for detecting the deviation of a PCB forming gong plate, which can replace equipment measurement with visual inspection, thereby improving efficiency and reducing costs.

[0006] In order to solve the above technical problems, the present invention provides a method for detecting the deviation of a PCB forming gong plate, comprising the following steps:

[0007] S1. When making each layer of circuits on the production board, a detection unit is made on the process edge at the same time, wherein the detection unit includes two first PADs arranged in parallel and a second PAD arranged at an interval at one end of the first PAD, and the extension direction of the second PAD is perpendicular to the extension direction of the first PAD;

[0008] S2. Making a solder resist layer on the production board, and opening a window in the solder resist layer at a position corresponding to the detection unit to expose the detection unit;

[0009] S3, in the process of forming the gong board, gong grooves are simultaneously performed between the two first PADs and between the first PAD and the second PAD to gong through the production board to form a detection groove; the vertical distance between the groove edge of the detection groove and the first PAD and the second PAD is less than the minimum vertical distance between the copper in the board and the outer shape edge;

[0010] S4. Observe and inspect whether there is exposed copper on the groove wall to determine whether the board is deflected.

[0011] Furthermore, in step S1, when manufacturing each layer of circuits on the production board, at least one detection unit is manufactured on the process edge of each set board.

[0012] Furthermore, in step S1, when manufacturing each layer of circuits on the production board, at least one detection unit is manufactured on the process edge of each PCS board.

[0013] Furthermore, in step S1, two ends of the second PAD are respectively located on one side of the ends of the two first PADs, so that the area between the two first PADs and the second PAD forms a T-shaped area.

[0014] Furthermore, in step S2, a window is opened in the solder resist layer at the middle position corresponding to the T-shaped area to form a T-shaped groove area, and the outer periphery of the groove area is retracted by 1-2 mm relative to the outer periphery of the T-shaped area.

[0015] Furthermore, in step S3, during the process of forming the gong plate, the plate at the gong groove area is cut and removed to form a T-shaped detection groove.

[0016] Furthermore, in step S3, the vertical distance between the groove edge of the detection groove and the first PAD and the second PAD is 0.025 mm smaller than the minimum vertical distance between the copper inside the board and the outer shape edge.

[0017] Furthermore, in step S1, the second PAD is located on one side of an end portion of one of the first PADs, and the length of the second PAD is ≥ the width of the first PAD.

[0018] Furthermore, the lengths of the first PAD and the second PAD are both 3 mm, and the widths are both 0.7 mm.

[0019] Furthermore, the production board is a multi-layer board in which an inner core board and an outer copper foil are pressed together by a semi-cured sheet, and the multi-layer board has been sequentially subjected to the processes of drilling, copper deposition, full-board electroplating and outer layer circuit production.

[0020] Compared with the prior art, the present invention has the following beneficial effects:

[0021] In the present invention, firstly, when making each layer of circuit, a detection unit including a first PAD and a second PAD is made in the process edge, and then a groove is made in the inner area of ​​the detection unit in the molding process to form a detection groove, so that the exposed copper condition of the groove wall of the detection groove can be visually inspected to identify whether the product has the risk of exposed copper, instead of the existing method of using equipment measurement, thereby improving the inspection efficiency and reducing the cost; and because the vertical distance between the groove edge of the detection groove and the first PAD and the second PAD is less than the minimum vertical distance between the copper in the board and the outer shape edge, when the detection groove is found When there is exposed copper on the groove wall, it means that the board has a problem of gong deviation and is judged to be a risky product, which serves as an early warning of gong deviation. However, it does not mean that there is exposed copper on the outer edge of the board. Further visual inspection is required to determine whether there is exposed copper on the entire outer edge, and a full inspection should be conducted on the outer edges of all the gonged boards to determine whether there is exposed copper. The defective products should be picked out and disposed of, and the product can be quickly inspected and disposed of after gong deviation and copper exposure occurs, thereby improving efficiency. In addition, the direction of deviation can be confirmed by detecting whether the exposed copper on the groove wall deviates from the position of the first PAD or the second PAD, and the subsequent gong board processing parameters can be adjusted according to the deviation direction. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a schematic diagram of a detection unit manufactured on the process edge of each circuit layer of a production board in an embodiment;

[0023] Figure 2 This is a schematic diagram of a process in which a solder mask layer is formed on a production board and a window is opened in the middle of a detection unit to form a gong groove area in an embodiment;

[0024] Figure 3 It is a schematic diagram of the detection groove after the groove area of ​​the production board is gonged out in the embodiment;

[0025] Figure 4 is a schematic diagram of a detection unit when the second PAD does not cover two ends of the first PAD in another embodiment;

[0026] Figure 5 It is a schematic diagram of a detection unit in another embodiment when a second PAD is disposed on one side of both ends of the first PAD. DETAILED DESCRIPTION

[0027] In order to more fully understand the technical content of the present invention, the technical solution of the present invention will be further introduced and illustrated in conjunction with specific embodiments below.

[0028] Example

[0029] The present embodiment shows a method for manufacturing a circuit board, which includes a process of solder masking with a variegated ink, and includes the following processing steps in sequence:

[0030] (1) Cutting: Cut the core board according to the panel size of 520 mm × 620 mm. The thickness of the core board is 0.5 mm, and the thickness of the copper layer on both surfaces of the core board is 0.5 oz. Multiple unit boards are formed on the core board according to preset rules.

[0031] (2) Inner layer circuit production (negative film process): Inner layer pattern transfer, use a vertical coating machine to coat the photosensitive film, the film thickness of the photosensitive film is controlled to 8μm, and a fully automatic exposure machine is used to complete the exposure of the inner layer circuit with a 5-6 grid exposure ruler (21 grid exposure ruler). After development, the inner layer circuit pattern is formed, and at least one detection unit pattern is formed on the process edge of each set board or pcs board; inner layer etching, the core board after exposure and development is etched to etch the inner layer circuit and the detection unit on the process edge. The inner layer line width is measured to be 3mil; inner layer AOI, and then check the inner layer circuit for defects such as open short circuit, circuit gap, circuit pinhole, etc. Defective products are scrapped, and non-defective products are sent to the next process.

[0032] Among the above, Figure 1 As shown, the detection unit includes two first PAD1 arranged in parallel and a second PAD2 arranged at an interval at one end of the first PAD1, and the extension direction of the second PAD2 is perpendicular to the extension direction of the first PAD1.

[0033] In one embodiment, two ends of the second PAD are respectively located on one side of the ends of the two first PADs, that is, the second PAD can span and cover the ends of the two first PADs, so that the area between the two first PADs and the second PAD forms a T-shaped area.

[0034] In one embodiment, the lengths of the first PAD1 and the second PAD2 are both 3 mm, and the widths are both 0.7 mm.

[0035] In one embodiment, the set board is the shipping unit after later forming and cutting, which includes at least one unit board (ie, PCS board), so that the detection unit is used to realize the deviation detection of each shipping unit.

[0036] In one embodiment, when the shipping unit after forming and cutting is a pcs board (ie, a unit board), at least one detection unit needs to be manufactured on the process edge of each pcs board.

[0037] In another embodiment, if Figure 4 As shown, the second PAD2 can also be located on one side of the end of one of the first PAD1, and the length of the second PAD ≥ the width of the first PAD, that is, the second PAD does not need to cover the ends of the two first PADs, and the detection groove formed during the subsequent molding is correspondingly L-shaped.

[0038] In yet another embodiment, Figure 5As shown, two second PAD2 can also be set, and the two second PAD2 are respectively arranged on one side of the two ends of the first PAD1, and the length of the second PAD2 covers the ends of the two first PAD1, so that an I-shaped area is formed between the four PADs, and the detection groove gonged out during the subsequent molding is correspondingly I-shaped.

[0039] (3) Lamination: The browning speed is based on the browning thickness of the bottom copper. The core board, prepreg, and outer copper foil are laminated in sequence as required. Then, appropriate lamination conditions are selected according to the Tg of the sheet material to laminate the laminated board to form a production board.

[0040] (4) Drilling: Based on the existing drilling technology, drilling processing is performed on the production board according to the design requirements.

[0041] (5) Copper plating: A thin layer of copper is deposited on the board surface and hole wall by chemical copper plating. The backlight test is level 10, and the thickness of the copper plating in the hole is 0.5μm.

[0042] (6) Full-board electroplating: Full-board electroplating is performed for 120 minutes at a current density of 18 ASF to thicken the copper layer on the hole and the board surface.

[0043] (7) Production of outer circuit (positive film process): Transfer of outer pattern, using fully automatic exposure machine and positive circuit film, with 5-7 grid exposure ruler (21 grid exposure ruler) to complete the exposure of outer circuit, after development, the outer circuit pattern is formed on the production board, and at least one detection unit pattern is formed on the process edge of each set board or pcs board; electroplating of outer pattern, and then copper plating and tin plating respectively on the production board, setting the electroplating parameters according to the required copper thickness, copper plating is 1.8ASD current density electroplating for 60 minutes on the whole board, tin plating is 1.2ASD current density electroplating for 10 minutes, tin thickness 3-5μm; then stripping, etching and tin stripping in turn, etching the outer circuit on the production board and etching the detection unit on the process edge; outer layer AOI, using automatic optical inspection system, by comparing with CAM data, detect whether the outer circuit has defects such as open circuit, gap, incomplete etching, short circuit, etc.

[0044] In the above, the detection pattern in the outer layer circuit is the same as the detection unit in the inner layer and is located at the same vertical projection position.

[0045] In another embodiment, the position of the detection unit in the outer layer circuit may be different from the position of the detection unit in the inner layer.

[0046] (8) Solder mask and silk screen characters: After silk screen printing solder mask ink on the surface of the production board, the solder mask ink is cured into a solder mask layer through pre-curing, exposure, development and heat curing treatment in sequence, and the solder mask layer is opened at the position corresponding to the detection unit and at the middle position corresponding to the T-shaped area to reveal the detection unit and the T-shaped groove area 3 (such as Figure 2 As shown in the figure, the periphery of the gong groove area is retracted by 1-2mm relative to the periphery of the T-shaped area, that is, the distance between the edge of the gong groove area and the detection unit is 1-2mm, and the vertical distances between the edge of the gong groove area and the first PAD and the second PAD are both smaller than the minimum vertical distance between the copper in the board and the outer edge; specifically, the solder resist ink on the TOP surface and the characters on the TOP surface add "UL mark", so that a layer is coated on the circuits and substrates that do not need to be soldered to prevent bridging between circuits during soldering, provide a permanent electrical environment and a protective layer against chemical corrosion, and at the same time beautify the appearance.

[0047] Preferably, the vertical distance between the edge of the groove area and the first PAD and the second PAD is 0.025 mm smaller than the minimum vertical distance between the copper in the board and the outer edge. The minimum vertical distance from the copper in the board to the outer edge is the minimum vertical distance from the circuit copper layer in the set board or pcs board to the outer edge.

[0048] (9) Surface treatment (nickel-gold deposition): The copper surface of the pad at the solder mask opening is chemically deposited with a nickel layer and a gold layer of a certain required thickness. The nickel layer thickness is 3-5 μm; the gold layer thickness is 0.05-0.1 μm.

[0049] In one embodiment, in order to reduce costs, a coating resist may be first made on the detection unit to prevent the first PAD and the second PAD from being plated with a nickel-gold layer; the coating resist may preferably be a dry film, which is formed by sequentially exposing and developing the film after being attached to the board.

[0050] (10) Electrical test: Test the electrical conductivity of the finished board. The test method used for this board is: flying probe test.

[0051] (11) Forming: According to the prior art and the design requirements, the gong shape with a tolerance of + / -0.05mm is used to produce a delivery unit set plate or a PCS plate; in the process of forming the gong plate, cutting is performed along the edge of the gong groove area to cut through the plate and remove the plate at the gong groove area to form a T-shaped detection groove 4 (such as Figure 3 As shown in the figure), the vertical distance between the edge of the detection groove and the first PAD and the second PAD is designed to be 0.025mm smaller than the minimum vertical distance between the copper inside the board and the outer edge.

[0052] In the above, whether there is copper exposure on the groove wall of the detection groove is observed to determine whether there is a problem of plate deviation. When copper exposure is found on the groove wall of the detection groove, it means that the board has a problem of deviation and is judged as a risky product, which serves as an early warning of deviation. However, it does not mean that copper is exposed on the outer edge of the board. Further visual inspection is required to determine whether there is copper exposure on the outer edge, and a full inspection is conducted on the outer edges of all the boards that have been grouted to determine whether there is copper exposure. The defective products are picked out and disposed of, and the product can be quickly inspected and disposed of after deviation and copper exposure occurs, thereby improving efficiency. When no copper exposure is found on the groove wall, the board is not deviated and is judged as an OK product.

[0053] In addition, by cooperating with two parallel first PADs and the detection groove therebetween, by observing which side of the first PAD the groove wall is close to with exposed copper, the deviation direction of the left or right side can be known, thereby realizing the identification of the deviation situation in the left or right direction; and by cooperating with the first PAD and the second PAD and the detection groove therebetween, by observing whether the groove wall is close to the end of the first PAD or the groove wall is close to the second PAD with exposed copper, the deviation direction of the front and rear sides can be known, thereby realizing the identification of the deviation situation in the front and rear sides, thereby finally confirming the deviation direction of the gong shape, and then adjusting the subsequent gong plate processing parameters according to the deviation direction.

[0054] (12) FQC: Inspect the appearance of the circuit board according to the customer's acceptance standards and our inspection standards. If there are any defects, repair them in time to ensure that we provide customers with excellent quality control.

[0055] (13) FQA: Re-test the circuit board’s appearance, hole copper thickness, dielectric layer thickness, green oil thickness, inner layer copper thickness, etc. to see if they meet customer requirements.

[0056] (14) Packaging: According to the packaging method and packaging quantity required by the customer, the circuit boards are sealed and packed with desiccant and humidity card before shipment.

[0057] The technical solutions provided by the embodiments of the present invention are introduced in detail above. Specific examples are used herein to illustrate the principles and implementation methods of the embodiments of the present invention. The description of the above embodiments is only applicable to help understand the principles of the embodiments of the present invention. At the same time, for those skilled in the art, according to the embodiments of the present invention, there will be changes in the specific implementation methods and application scopes. In summary, the content of this specification should not be understood as limiting the present invention.

Claims

1. A method for detecting the deviation of a PCB forming gong plate, characterized in that: The following steps are involved: S1. When making each layer of circuits on the production board, a detection unit is made on the process edge at the same time, wherein the detection unit includes two first PADs arranged in parallel and a second PAD arranged at an interval at one end of the first PAD, and the extension direction of the second PAD is perpendicular to the extension direction of the first PAD; S2. Making a solder resist layer on the production board, and opening a window in the solder resist layer at a position corresponding to the detection unit to expose the detection unit; S3, in the process of forming the gong board, gong grooves are simultaneously performed between the two first PADs and between the first PAD and the second PAD to gong through the production board to form a detection groove; the vertical distance between the groove edge of the detection groove and the first PAD and the second PAD is less than the minimum vertical distance between the copper in the board and the outer shape edge; S4. Observe and inspect whether there is exposed copper on the groove wall to determine whether the board is deflected.

2. The method for detecting the deviation of the PCB forming gong plate according to claim 1, characterized in that: In step S1, when manufacturing each layer of circuits on the production board, at least one detection unit is manufactured on the process edge of each set board.

3. The method for detecting the deviation of the PCB forming gong plate according to claim 1, characterized in that: In step S1, when manufacturing each layer of circuits on the production board, at least one detection unit is manufactured on the process edge of each PCS board.

4. The method for detecting the deviation of the PCB forming gong plate according to claim 1, characterized in that: In step S1 , two ends of the second PAD are respectively located at one side of the ends of the two first PADs, so that the area between the two first PADs and the second PAD forms a T-shaped area.

5. The method for detecting the deviation of the PCB forming gong plate according to claim 4, characterized in that: In step S2, a window is opened in the solder resist layer at the middle position corresponding to the T-shaped area to form a T-shaped groove area, and the outer periphery of the groove area is retracted by 1-2 mm relative to the outer periphery of the T-shaped area.

6. The method for detecting the deviation of the PCB forming gong plate according to claim 5, characterized in that: In step S3, during the process of forming the gong plate, the plate at the gong groove area is cut and removed to form a T-shaped detection groove.

7. The method for detecting the deviation of the PCB forming gong plate according to any one of claims 1 to 6, characterized in that: In step S3, the vertical distance between the groove edge of the detection groove and the first PAD and the second PAD is 0.025 mm smaller than the minimum vertical distance between the copper inside the board and the outer shape edge.

8. The method for detecting the deviation of the PCB forming gong plate according to claim 1, characterized in that: In step S1, the second PAD is located at one side of an end of one of the first PADs, and the length of the second PAD is greater than or equal to the width of the first PAD.

9. The method for detecting the deviation of the PCB forming gong plate according to claim 1, characterized in that: The length of the first PAD and the second PAD are both 3 mm, and the width are both 0.7 mm.

10. The method for detecting the deviation of the PCB forming gong plate according to claim 1, characterized in that: The production board is a multi-layer board in which an inner core board and an outer copper foil are pressed together by a semi-cured sheet, and the multi-layer board has been through the processes of drilling, copper deposition, full-board electroplating and outer layer circuit making in sequence.

Citation Information

Patent Citations

  • Method for preventing milling leakage of milling groove of circuit board

    CN105228358A

  • Method for quickly detecting deviation of PCB (Printed Circuit Board) molding routing board

    CN118158900A

  • Container based method and server for managing artificial intelligence model

    KR102735646B1