Corrosion-resistant ceramic corrugated packing and preparation method thereof
The ceramic corrugated packing design with staggered plates and porous anti-corrosion layers addresses dead corners by facilitating material flow and optimizing filtration, enhancing corrosion resistance and service life.
Patent Information
- Application Number
- CN202411583279.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-07
- Publication Date
- 2024-12-06
AI Technical Summary
Traditional ceramic corrugated packing suffers from dead corners where material flow is restricted, leading to adsorbent retention and accelerated corrosion, reducing its performance and service life.
A corrosion-resistant ceramic corrugated packing design featuring staggered ceramic corrugated plates with a porous anti-corrosion layer having sparse and dense pore parts, where sparse pores are large but less dense on ridges and dense pores are small but more dense in valleys, eliminating dead corners and optimizing material processing.
The design effectively reduces adsorbent retention and enhances corrosion resistance by allowing smooth material flow through large sparse pores and concentrating filtration in non-dead corner areas, improving the packing's service life and efficiency.
Smart Images

Figure CN119075895A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to packing technology used in the fields of chemical industry and environmental protection, and in particular to the problem of dead corners in traditional ceramic corrugated packing. A corrosion-resistant ceramic corrugated packing and a preparation method thereof are proposed, aiming to effectively eliminate the dead corners of the packing and improve the corrosion resistance and service life of the packing through innovations in structural design and preparation process. Background Art
[0002] In traditional ceramic corrugated packing, a significant technical problem exists in the areas where adjacent ceramic corrugated plate corrugation ridges and corrugation valleys contact each other. Due to the structural characteristics of these areas, two angles are formed, and these angle areas often become packing dead corners. In these dead corners, the flow of materials is restricted, which easily leads to the retention and accumulation of adsorbents (such as corrosive media, impurities, etc.). Over time, these retained adsorbents will accelerate the corrosion of the area, resulting in a decrease in the overall performance of the packing and a shortened service life. Therefore, how to effectively eliminate these packing dead corners and reduce the retention and corrosion of adsorbents has become a technical problem that needs to be solved urgently. Summary of the invention
[0003] In view of the deficiencies in the prior art, the present invention provides a corrosion-resistant ceramic corrugated packing and a preparation method thereof, which effectively eliminates packing dead corners through unique design and preparation process, improves the packing's corrosion resistance and high-efficiency material processing capability.
[0004] The above technical objectives of the present invention are achieved through the following technical solutions: a corrosion-resistant ceramic corrugated packing, comprising a plurality of stacked ceramic corrugated plates, wherein the upper surface of each layer of ceramic corrugated plates is paved with a porous anti-corrosion layer adapted to the shape of the ceramic corrugated plates; The ceramic corrugated plates are staggered with convex corrugated ridges and concave corrugated valleys, and the corrugated ridges and corrugated valleys of adjacent layers of ceramic corrugated plates abut against each other; The porous anti-corrosion layer is also staggered with sparse pore parts and dense pore parts. The pore density in the sparse pore part is smaller than that in the dense pore part, but the size of a single pore in the sparse pore part is larger than that in the dense pore part. Each sparse hole portion is arranged on each corrugated ridge of the ceramic corrugated plate in a one-to-one correspondence, and each dense hole portion is arranged in each corrugated valley in a one-to-one correspondence; On both sides of the contact position between the corrugation ridge and the corrugation valley, the corrugation ridge and the corrugation valley of adjacent ceramic corrugated plates are away from each other, forming a large space channel for materials to pass through.
[0005] A method for preparing a packing, which is used to prepare the above-mentioned corrosion-resistant ceramic corrugated packing, comprises the following steps: S1. preparing ceramic slurry: finely grinding and mixing ceramic raw materials, and adding appropriate amounts of additives to form ceramic slurry; S2, preparing a dry sponge and immersing it in the ceramic slurry until the sponge absorbs the ceramic slurry to a saturated state; S3, covering the upper surface of the ceramic corrugated plate to be sintered but already formed with the sponge fully soaked with ceramic slurry; S4, let it stand for adjustment, during which, under the influence of gravity, the ceramic slurry in the sponge covered on the corrugated ridge will tend to flow slowly down along the slopes on both sides and gather in the sponge in the corrugated valley; S5. Sintering: After the sponge is melted and volatilized at high temperature, the space originally occupied by the sponge will become a number of holes.
[0006] In some embodiments, the specific steps of step S1 are as follows: a. Raw material selection and pretreatment: Alumina and silicon oxide with a purity of not less than 98% are selected as the main raw materials, and the raw materials are vibrated, screened and ground; b. Additive ratio and mixing: Add polyvinyl alcohol as a binder, glycerol as a plasticizer, sodium tripolyphosphate as a dispersant, and mix all the raw materials and additives; c. Slurry preparation and homogenization: Deionized water is added during the stirring process to adjust the solid content of the slurry, and the slurry is homogenized using an ultrasonic disperser while the slurry temperature is controlled not to exceed 40°C.
[0007] In some embodiments, the sponge in step S2 is an open-pore sponge made of polyester or polyurethane, with a porosity controlled between 70% and 90%, a density maintained at 15-30 kg / m³, and an average pore size controlled between 0.5 and 2 mm.
[0008] In some embodiments, in step S3, after covering the upper surface of the ceramic corrugated plate with the sponge soaked with ceramic slurry, the step of appropriately pressing and shaping the sponge is also included, using a soft and flat tool to evenly and appropriately press and shape the sponge.
[0009] In some embodiments, in step S4, during the static adjustment period, a step of accelerating the redistribution of the ceramic slurry in the sponge by using vibration-assisted means is also included, and slight and uniform vibration is applied to the ceramic corrugated plate covered with the sponge soaked with the ceramic slurry.
[0010] In some embodiments, in step S5, after sintering is completed, a step of cleaning the sponge residue that has not been completely melted and volatilized is included, and the surface of the sintered ceramic corrugated plate is cleaned using a high-pressure air gun or a special cleaning tool.
[0011] Compared with the prior art, the present invention has the following beneficial effects: 1. The present invention provides a porous portion at the contact position between the corrugated ridges and corrugated valleys of adjacent ceramic corrugated plates, thereby effectively eliminating dead corners of the packing, reducing the retention and accumulation of adsorbents, and improving the corrosion resistance and service life of the packing.
[0012] 2. The synergistic effect of the sparse pore part and the dense pore part, as well as the corrugated structural characteristics of the ceramic corrugated plate itself, achieves efficient processing of materials.
[0013] 3. The preparation method is simple and feasible. By using the sponge as a template, the porous anti-corrosion layer is perfectly fitted with the surface of the ceramic corrugated plate, thereby improving the overall consistency and stability of the filler.
[0014] 4. By utilizing the natural flow of slurry under the action of gravity and vibration as an auxiliary means, hole structures of different densities can be formed at the corrugation ridges and corrugation valleys without complicated processes, which simplifies the production process and accurately controls the performance distribution of the porous anti-corrosion layer.
[0015] In summary, the present invention provides a corrosion-resistant ceramic corrugated packing and a preparation method thereof. Through a unique design and preparation process, the dead corner problem existing in traditional ceramic corrugated packing is effectively solved, the corrosion resistance of the packing and the efficient processing capacity of materials are improved, and it has broad application prospects. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a schematic diagram of the structure of the filler of the present invention; Figure 2 A detailed structural diagram of a ceramic corrugated plate as a filler of the present invention; Figure 3 This is a detailed structural diagram of the porous anti-corrosion layer of the filler of the present invention.
[0017] In the figure: 100, ceramic corrugated plate; 200, porous anti-corrosion layer; 1, corrugation ridge; 2, corrugation valley; 3, sparse pore part; 4, dense pore part. DETAILED DESCRIPTION
[0018] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention.
[0019] In the description of the present invention, it should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
[0020] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0021] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0022] like Figure 1-3 As shown, this embodiment provides a corrosion-resistant ceramic corrugated packing, comprising a plurality of stacked ceramic corrugated plates 100, wherein the upper surface of each layer of ceramic corrugated plates 100 is paved with a porous anti-corrosion layer 200 that matches the shape of the ceramic corrugated plates 100; The ceramic corrugated plate 100 is staggered with convex corrugated ridges 1 and concave corrugated valleys 2, and the corrugated ridges 1 and corrugated valleys 2 of adjacent layers of the ceramic corrugated plate 100 abut against each other. The porous anti-corrosion layer 200 is also staggered with sparse pores 3 and dense pores 4, wherein the hole density at the sparse pores 3 is smaller than that at the dense pores 4, but the size of a single hole at the sparse pores 3 is larger than that at the dense pores 4. The sparse pores 3 have large hole sizes but low density, which is convenient for materials to pass through, and the dense pores 4 have small hole sizes but high density, which has strong adsorption and filtration capabilities; The sparse pore portions 3 of the porous anti-corrosion layer 200 are fitted one-to-one on the corrugated ridges 1 of the ceramic corrugated plate 100, while the dense pore portions 4 are fitted one-to-one in the corrugated valleys 2. The sparse pore portions 3 of the porous anti-corrosion layer 200 are deliberately arranged at the contact position between the corrugated ridge 1 and the corrugated valley 2. Since the hole size of the sparse pore portion 3 is large, the material can pass through easily, thereby reducing the retention of the adsorbate in these dead corners and effectively eliminating the dead corners of the packing. On both sides of the contact position between the corrugated ridge 1 and the corrugated valley 2, that is, on both sides of the dead corner, the corrugated ridges 1 and the corrugated valleys 2 of adjacent ceramic corrugated plates 100 are far away from each other, forming a large space channel for the material to pass through. The dense pore portions 4 of the porous anti-corrosion layer 200 are arranged in these large space channels, and use their powerful adsorption and filtration capabilities to achieve efficient processing of materials. This design sets the structure with a heavy adsorption and filtration burden in a non-dead corner area, optimizing the position of the adsorption and filtration process in the packing.
[0023] The present invention sets a sparse hole portion 3 at the contact position between the corrugated ridge 1 and the corrugated valley 2 of adjacent ceramic corrugated plates 100, that is, the traditional dead corner area. Since the hole size of the sparse hole portion 3 is relatively large, the material can pass smoothly, thereby reducing the retention and accumulation of adsorbates in these areas, effectively eliminating the dead corner, and setting a dense hole portion 4 in the large space channel formed on both sides of the contact position between the corrugated ridge 1 and the corrugated valley 2. The dense hole portion 4 uses its dense holes and smaller hole size to efficiently adsorb and filter the material. This design concentrates the adsorption and filtration process mainly in the non-dead corner area, optimizes the position of the adsorption and filtration process in the filler, and through the synergistic effect of the sparse hole portion 3 and the dense hole portion 4, as well as the corrugated structural characteristics of the ceramic corrugated plate 100 itself, the present invention realizes efficient processing of materials and effective elimination of dead corners of fillers.
[0024] In summary, the contact area between the corrugated ridge 1 and the corrugated valley 2 of the adjacent ceramic corrugated plate 100 is a packing dead angle, where two angles are formed, and it is very easy to retain adsorbed materials, resulting in that the corrosion at this location is usually more serious. In the present invention, the sparse hole portion 3 of the porous anti-corrosion layer 200 is arranged at the contact area between the corrugated ridge 1 and the corrugated valley 2. The sparse hole portion 3 is easy for materials to pass through, which is conducive to reducing retention, thereby playing a role in eliminating the dead angle. Since the ceramic corrugated plate 100 is corrugated, there are two sides of the contact position between the corrugated ridge 1 and the corrugated valley 2, that is, the two sides of the dead angle. On the other side, the corrugated ridges 1 and corrugated valleys 2 of adjacent ceramic corrugated plates 100 will move away from each other to form a large space channel for materials to pass through, and the dense pore portion 4 of the porous anti-corrosion layer 200 is arranged in the large space channel. Since the holes in the dense pore portion 4 are densely distributed and the hole size is small, its adsorption and filtration ability is the strongest. Therefore, arranging the structure with a heavy adsorption and filtration burden in the large space channel is beneficial to reducing the retention and accumulation of adsorbates, and realizing that most of the adsorption and filtration process is concentrated in non-dead angle areas, thereby realizing the optimization of the position of the adsorption and filtration process in the filler.
[0025] This embodiment also provides a method for preparing a packing, which is used to prepare the above-mentioned corrosion-resistant ceramic corrugated packing, comprising the following steps: S1. Preparation of ceramic slurry: This step involves finely grinding and mixing the ceramic raw materials, adding appropriate amounts of additives such as binders, plasticizers, etc., and forming a uniform ceramic slurry with a certain fluidity through sufficient stirring. This step is the basis for the subsequent preparation of the porous anti-corrosion layer 200. Ensuring the quality of the ceramic slurry directly affects the performance and durability of the final product. S2. Prepare a dry sponge and immerse it in the ceramic slurry until the sponge absorbs the ceramic slurry to a saturated state: select a dry sponge with appropriate porosity and water absorption, immerse it completely in the prepared ceramic slurry, and make the sponge fully absorb the ceramic slurry through physical adsorption until it reaches saturation. The key to this process is to control the adsorption amount of the sponge to ensure that the sponge can evenly release the ceramic slurry in the subsequent steps to form an ideal porous structure; S3, covering the upper surface of the ceramic corrugated plate 100 to be sintered but already formed with the sponge fully absorbed with the ceramic slurry, because the sponge is fully absorbed with the ceramic slurry, it can bend in a corrugated shape and thus fit on the ceramic corrugated plate 100: this step utilizes the flexibility of the sponge and the plasticity after being fully absorbed with the ceramic slurry, so that the sponge can fit tightly on the complex surface of the ceramic corrugated plate 100, including the corrugated ridges 1 and the corrugated valleys 2. This fitting method ensures that the porous anti-corrosion layer 200 can accurately replicate the shape of the ceramic corrugated plate 100, laying a good foundation for the subsequent sintering process; S4, static adjustment, during which, under the influence of gravity, the ceramic slurry in the sponge covered on the corrugated ridge 1 will tend to flow slowly down along the slopes on both sides and converge into the sponge in the corrugated valley 2. This process causes the ceramic slurry in the sponge in the corrugated ridge 1 area to gradually decrease, while the sponge in the corrugated valley 2 area has a relatively increased content due to the continuous reception of the flowing slurry. This natural flow and redistribution of the ceramic slurry on the corrugated ridge 1 causes the slurry in this area to form a dispersed, small-strand distribution pattern, which is different from the more concentrated and rich slurry layer in the corrugated valley 2. This natural phenomenon lays the foundation for the formation of large-sized but fewer holes (i.e., sparse pore section 3) at the corrugated ridge 1 and small and dense holes (i.e., dense pore section 4) at the corrugated valley 2 during the subsequent sintering process, and the differentiated layout of hole size and density can be cleverly achieved without human intervention; S5, sintering. After the sponge is melted and volatilized at high temperature, the space originally occupied by the sponge will become a number of holes: during the high-temperature sintering process, the sponge is completely melted and volatilized, leaving behind a porous structure formed by the solidification of the ceramic slurry. This process not only removes the sponge, but also makes the porous anti-corrosion layer 200 firmly bonded to the ceramic corrugated plate 100. At the same time, due to the previous differential distribution of the slurry, the structural difference between the sparse pore part 3 and the dense pore part 4 is formed, which meets the design requirements.
[0026] This method uses sponge as a template to achieve perfect fit between the porous anti-corrosion layer 200 and the surface of the ceramic corrugated plate 100, and both the corrugated ridge 1 and the corrugated valley 2 can be evenly covered, thereby improving the overall consistency and stability of the filler. In addition, the natural flow of the slurry under the action of gravity can be used to form hole structures of different densities at the corrugated ridge 1 and the corrugated valley 2 without complicated processes, which not only simplifies the production process, but also accurately controls the performance distribution of the porous anti-corrosion layer 200.
[0027] In some embodiments, the specific steps of step S1 are as follows: a. Raw material selection and pretreatment: Raw material selection: Alumina (Al2O3) and silicon oxide (SiO2) with a purity of not less than 98% are selected as the main raw materials to ensure the high purity and excellent performance of the slurry; Pretreatment: The raw materials need to be vibrated and screened to remove particles larger than 0.5 mm, and then ground in a ball mill for no less than 4 hours until the particle size reaches D50≤0.05 mm to ensure the fineness and uniformity of the slurry; b. Additive ratio and mixing: Binder: Polyvinyl alcohol (PVA) is used as a binder, and the addition amount is 3%-5% of the total weight of the raw materials to improve the adhesion and plasticity of the slurry; Plasticizer: Glycerol is used as plasticizer, and the addition amount is 1%-2% of the total weight of the raw materials to improve the fluidity and processability of the slurry; Dispersant: Sodium tripolyphosphate is used as the dispersant, and the addition amount is 0.5%-1% of the total weight of the raw materials to promote the uniform dispersion of the raw material particles; Mixing: Add all raw materials and additives into a container with a stirring device and stir at a speed of 500-800 rpm for 30-60 minutes to ensure that all components are fully blended to form a uniform slurry; c. Slurry preparation and homogenization: Modulation: During the stirring process, gradually add an appropriate amount of deionized water to adjust the solid content of the slurry to 40%-50% to ensure that the slurry has appropriate fluidity and plasticity; Homogenization: Use an ultrasonic disperser to homogenize the slurry, with the power set to 1-2kW and the processing time not less than 10 minutes to eliminate local concentration differences and agglomeration of tiny particles in the slurry and ensure the uniformity of the slurry quality; Temperature control: During the entire slurry preparation process, the slurry temperature must be strictly controlled not to exceed 40°C to avoid overheating of the slurry, resulting in performance changes or bubbles.
[0028] In some embodiments, the sponge in step S2 is an open-pore sponge made of polyester (PET) or polyurethane (PU), and its porosity is controlled between 70% and 90% to ensure that the sponge has sufficient water absorption and air permeability. The density of the sponge needs to be maintained at 15-30kg / m³. Such a density can not only ensure that the sponge will not be deformed due to excessive weight when absorbing the ceramic slurry, but also ensure that the sponge can be completely melted and volatilized during the sintering process without leaving any residue. At the same time, the pore size of the sponge should be uniform, and the average pore size should be controlled between 0.5-2mm, so that the ceramic slurry can evenly penetrate and fill the pores of the sponge to form an ideal porous structure. In addition, the sponge must have good resilience and flexibility to ensure that it can fit closely to its complex surface, including the corrugated ridges 1 and the corrugated valleys 2, when covering the ceramic corrugated plate 100, so as to ensure that the porous anti-corrosion layer 200 can accurately replicate the shape of the ceramic corrugated plate 100.
[0029] In some embodiments, in step S3, after the sponge fully absorbed with the ceramic slurry is covered on the upper surface of the ceramic corrugated plate 100 to be sintered but already formed, the step of appropriately pressing and shaping the sponge is also included: specifically, a soft and flat tool, such as a soft scraper or a sponge roller, is used to uniformly and appropriately press the sponge covered on the ceramic corrugated plate 100 to ensure that the sponge is in close contact with every part of the ceramic corrugated plate 100, especially the junction of the corrugated ridge 1 and the corrugated valley 2. At the same time, through gentle shaping operations, the shape of the sponge is adjusted to make it more fit the corrugated profile of the ceramic corrugated plate 100 to avoid wrinkles or gaps. By appropriately pressing and shaping the sponge, it can be ensured that the sponge is in close contact with every part of the ceramic corrugated plate 100, avoiding the problem of uneven or missing porous anti-corrosion layer 200 caused by gaps between the sponge and the ceramic corrugated plate 100. In this way, the porous anti-corrosion layer 200 can be more evenly covered on the ceramic corrugated plate 100, thereby improving the overall consistency and stability of the filler.
[0030] In some embodiments, in step S4, during the static adjustment period, a step of accelerating the redistribution of the ceramic slurry in the sponge by using vibration-assisted means is also included: specifically, a low-frequency vibrator or a vibration platform can be used to apply slight and uniform vibration to the ceramic corrugated plate 100 covered with a sponge full of ceramic slurry. This vibration can produce a tiny mechanical disturbance, promote the flow and redistribution of the ceramic slurry inside the sponge, especially at the junction of the corrugated ridge 1 and the corrugated valley 2, the vibration can help the slurry flow down the slope more smoothly and converge into the corrugated valley 2. The vibration-assisted means can produce a tiny mechanical disturbance, break the static balance of the slurry inside the sponge, and accelerate the flow and redistribution of the slurry in the sponge. This can not only shorten the static adjustment time and improve production efficiency, but also ensure that the slurry is more evenly distributed in the sponge, laying the foundation for the formation of an ideal pore structure in the subsequent sintering process.
[0031] In some embodiments, in step S5, after sintering is completed, a step of cleaning up the sponge residue that has not been completely melted and volatilized is also included: specifically, a high-pressure air gun or a special cleaning tool is used to carefully clean the surface of the sintered ceramic corrugated plate 100 to remove any sponge residue that may be attached to the surface and has not been completely melted and volatilized. During the sintering process, although most of the sponge will melt and volatilize, a small amount of sponge residue that has not been completely melted and volatilized may still be left. If these residues are attached to the surface of the filler, they will not only affect the appearance quality of the filler, but may also become a potential area for the retention and accumulation of adsorbents, thereby accelerating the corrosion of the filler. Through the cleaning step, these residues can be completely removed, the cleanliness of the filler surface can be improved, and the risk of corrosion can be reduced. And the presence of sponge residues may block some holes, affecting the integrity and permeability of the porous structure. The cleaning step can ensure that each hole is unobstructed, so that the porous anti-corrosion layer 200 can give full play to its adsorption and filtration function, and improve the processing efficiency of the filler for the material.
[0032] This specific embodiment is merely an explanation of the present invention and is not a limitation of the present invention. After reading this specification, those skilled in the art may make non-creative modifications to the present embodiment as needed. However, as long as they are within the scope of the claims of the present invention, they are protected by the patent law.
Claims
1. A corrosion-resistant ceramic corrugated packing, characterized in that: It comprises a plurality of layers of ceramic corrugated plates (100) stacked together, wherein the upper surface of each layer of ceramic corrugated plates (100) is provided with a porous anti-corrosion layer (200) that matches the shape of the ceramic corrugated plates (100); The ceramic corrugated plates (100) are alternately provided with upwardly convex corrugated ridges (1) and downwardly concave corrugated valleys (2), and the corrugated ridges (1) and corrugated valleys (2) of adjacent layers of the ceramic corrugated plates (100) abut against each other; The porous anti-corrosion layer (200) is also staggered with sparse pore parts (3) and dense pore parts (4), the pore density in the sparse pore part (3) is smaller than that in the dense pore part (4), but the size of a single pore in the sparse pore part (3) is larger than that in the dense pore part (4); Each sparse hole portion (3) is arranged one-to-one on each corrugated ridge (1) of the ceramic corrugated plate (100), and each dense hole portion (4) is arranged one-to-one in each corrugated valley (2); On both sides of the contact position between the corrugated ridges (1) and the corrugated valleys (2), the corrugated ridges (1) and the corrugated valleys (2) of adjacent ceramic corrugated plates (100) are spaced away from each other, forming a large space channel for materials to pass through.
2. A method for preparing a packing, the method being used for preparing a corrosion-resistant ceramic corrugated packing as claimed in claim 1, characterized in that: The following steps are involved: S1. preparing ceramic slurry: finely grinding and mixing ceramic raw materials, and adding appropriate amounts of additives to form ceramic slurry; S2, preparing a dry sponge and immersing it in the ceramic slurry until the sponge absorbs the ceramic slurry to a saturated state; S3, covering the upper surface of the ceramic corrugated plate (100) to be sintered but already formed with a sponge fully soaked with ceramic slurry; S4, standing still for adjustment, during which, under the influence of gravity, the ceramic slurry in the sponge covered on the corrugated ridge (1) tends to flow slowly down along the slopes on both sides and gather in the sponge in the corrugated valley (2); S5. Sintering: After the sponge is melted and volatilized at high temperature, the space originally occupied by the sponge will become a number of holes.
3. A filler preparation method according to claim 2, characterized in that: The specific steps of step S1 are as follows: a. Raw material selection and pretreatment: Alumina (Al2O3) and silicon oxide (SiO2) with a purity of not less than 98% are selected as the main raw materials, and the raw materials are vibrated, screened and ground; b. Additive ratio and mixing: Add polyvinyl alcohol (PVA) as a binder, glycerol as a plasticizer, sodium tripolyphosphate as a dispersant, and mix all the raw materials and additives; c. Slurry preparation and homogenization: Deionized water is added during the stirring process to adjust the solid content of the slurry, and the slurry is homogenized using an ultrasonic disperser while the slurry temperature is controlled not to exceed 40°C.
4. A method for preparing a filler according to claim 2, characterized in that: The sponge in step S2 is an open-pore sponge made of polyester or polyurethane, with a porosity controlled between 70% and 90%, a density maintained at 15-30 kg / m³, and an average pore size controlled between 0.5 and 2 mm.
5. A method for preparing a filler according to claim 2, characterized in that: In step S3, after the sponge fully absorbed with the ceramic slurry is covered on the upper surface of the ceramic corrugated plate (100), the step of appropriately pressing and shaping the sponge is also included, using a soft and flat tool to evenly and appropriately press and shape the sponge.
6. A method for preparing a filler according to claim 2, characterized in that: In step S4, during the static adjustment period, a step of accelerating the redistribution of the ceramic slurry in the sponge by using a vibration auxiliary means is also included, wherein a slight and uniform vibration is applied to the ceramic corrugated plate (100) covered with the sponge full of ceramic slurry.
7. A method for preparing a filler according to claim 2, characterized in that: In step S5, after sintering is completed, a step of cleaning the sponge residue that has not been completely melted and volatilized is also included, using a high-pressure air gun or a dedicated cleaning tool to clean the surface of the sintered ceramic corrugated plate (100).
Citation Information
Cited By
Corrosion-resistant ceramic composite material and preparation method thereof
CN121248265A
Corrosion-resistant ceramic composite material and method for manufacturing the same
CN121248265B