Forging die and forging method for aluminum-based composite thin-wall pipe fitting
The forging die and method address the issue of inconsistent forging ratios and defects by using synchronized upper and lower die assemblies with temperature control and a supporting middle assembly, ensuring stable deformation and improved production efficiency for aluminum-based composite pipe fittings.
Patent Information
- Application Number
- CN202411442523.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-16
- Publication Date
- 2024-12-06
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing forging dies for aluminum-based composite thin-walled pipe fittings face challenges such as inconsistent forging ratios leading to quality defects like microcracks due to the excessive height of the suspended section, which causes instability and material waste during the forging process.
A forging die and method utilizing a combination of upper and lower die assemblies with servo forging technology, where the upper and lower forging heads move synchronously, and a middle fixing assembly supports the forging blank, ensuring consistent deformation and temperature-controlled recrystallization to stabilize the lattice size and prevent defects.
The solution stabilizes the forging process, reduces material waste, and enhances production efficiency by achieving consistent deformation and preventing defects like microcracks, resulting in high-quality double-bell-mouth silicon carbide reinforced aluminum-based composite material pipe fittings.
Smart Images

Figure CN119076865A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of forging, and in particular relates to a forging die and a forging method for an aluminum-based composite material thin-wall pipe fitting. Background Art
[0002] Aluminum alloy special-shaped pipe fittings are widely used in industrial production. For example, the lower connector of the aluminum alloy support arm used for the suspension frame of a high-speed maglev vehicle is a key part connecting the support arm parts of the maglev vehicle. This part has a special-shaped hollow thin-walled bidirectional trumpet-shaped structure. The wall thickness of the part is small, and both ends are not only trumpet-shaped, but also have flanges. The shape is very complex, and its forging production is very difficult.
[0003] In terms of forging technology and die design, if solid structural parts are used for forging, the entire hollow structure needs to be hollowed out by machining after forging. The processing volume and difficulty are very large, the material waste is extremely serious, and there is a lack of process innovation. At present, forging dies are used to forge hollow forging blanks of thin-walled aluminum-based composite materials, which saves materials. The forging die is a combination of a fixed die and a movable die. Figure 1 As shown, the blank fixed section 101 of the forging blank 1 is fixed in contact with the mold fixed section 401 of the fixed mold 4. When the suspended height of the blank suspended section 102 of the forging blank 1 is too long, if the movable mold 5 is pressed downward, the first technical difficulty is: the suspended section of the thin-walled aluminum-based composite material of the forging blank 1 has a large convection heat dissipation area, and the suspended end is far away from the heating contact isothermal hot forging (higher than the recrystallization temperature) area of the fixed mold 4, resulting in unstable lattice size of the forging; the second technical difficulty is: the suspended section of the thin-walled aluminum-based composite material of the forging blank 1 is too high, which will lead to crushing instability; the third technical difficulty is: the suspended section of the thin-walled aluminum-based composite material of the forging blank 1 is too high, which will lead to inconsistent forging ratios from the edge to the inside of the bell mouth of the formed forging, and it is easy to produce quality and lattice defects such as microcracks. Summary of the invention
[0004] In view of the above problems, the purpose of the present invention is to provide a forging die and forging method for thin-walled aluminum-based composite material pipes, so as to solve the problem that the existing forging die has an inconsistent forging ratio from the edge to the inside of the bell mouth of the formed forging due to the excessive height of the suspended section of the thin-walled aluminum-based composite material, which easily causes quality and lattice defects such as microcracks.
[0005] In order to achieve the above object, the present invention adopts the following technical solutions:
[0006] On the one hand, the present invention provides a forging die for aluminum-based composite material thin-walled pipe fittings, which is arranged on a press, and the press has an upper forging head and a lower forging head arranged relatively to each other, and the forging die comprises an upper die assembly, a middle fixed assembly, an upper lifting platform, a lower die assembly and a lower lifting platform, wherein the upper lifting platform, the middle fixed assembly and the lower lifting platform are arranged on the press from top to bottom in sequence, the middle fixed assembly is used to fix a cylindrical forging blank, the upper die assembly and the lower die assembly are respectively arranged on the upper lifting platform and the lower lifting platform, the upper lifting platform and the lower lifting platform are respectively used to drive the upper die assembly and the lower die assembly to rise and fall, the upper die assembly and the upper forging head cooperate to realize the expansion forging of the upper port of the forging blank, and the lower die assembly and the lower forging head cooperate to realize the expansion forging of the lower port of the forging blank, so as to obtain a forging with two trumpet-shaped ports.
[0007] In one possible implementation, the upper mold assembly includes an upper mold I, an upper mold II and two groups of upper horizontal drive modules, wherein the upper mold I and the upper mold II are both horizontally slidably connected to the upper lifting platform, the two groups of upper horizontal drive modules are relatively arranged on both sides of the upper lifting platform, and the output ends are respectively connected to the upper mold I and the upper mold II, and the corresponding sides of the upper mold I and the upper mold II are provided with upper forging dies; the two groups of upper horizontal drive modules are used to drive the upper mold I and the upper mold II to close or separate.
[0008] In one possible implementation, the lower mold assembly includes a lower mold I, a lower mold II and two groups of lower horizontal drive modules, wherein the lower mold I and the lower mold II are both horizontally slidably connected to the lower lifting platform, the two groups of lower horizontal drive modules are relatively arranged on both sides of the lower lifting platform, and the output ends are respectively connected to the lower mold I and the lower mold II, and the corresponding sides of the lower mold I and the lower mold II are provided with lower forging dies; the two groups of lower horizontal drive modules are used to drive the lower mold I and the lower mold II to close or separate.
[0009] In a possible implementation, the upper forging die and the lower forging die are trumpet-shaped structures that are mirror-imaged along the axial direction of the forging blank.
[0010] In one possible implementation, temperature control modules are provided in the upper mold I, the upper mold II, the lower mold I and the lower mold II.
[0011] In one possible implementation, the middle fixing assembly includes a fixing beam, a pressure cover and a profiling core, wherein the fixing beam is horizontally arranged and one end is connected to the press, a groove is arranged at the other end of the fixing beam, the forging blank is positioned in the groove and fixed by the pressure cover, and the profiling core is arranged on the inner side of the forging blank.
[0012] In a possible implementation, lifting guide pillars are provided on both sides of the press, and both sides of the upper lifting platform and the lower lifting platform are slidably matched with the corresponding lifting guide pillars;
[0013] In a possible implementation, two groups of upper lifting servo electric cylinders are provided on both sides of the upper part of the press, and the output ends of the two groups of upper lifting servo electric cylinders are respectively connected to both sides of the upper lifting platform;
[0014] In a possible implementation, two groups of lower lifting servo electric cylinders are respectively provided on both sides of the lower part of the press, and the output ends of the two groups of lower lifting servo electric cylinders are respectively connected to both sides of the lower lifting platform.
[0015] In a possible implementation, the forging includes a cylinder and bell mouths located at both ends of the cylinder, and the outer edge of the bell mouth is provided with a flat flange.
[0016] Another aspect of the present invention provides a forging method using the aluminum-based composite material thin-walled pipe forging die as described above, the forging method comprising the following steps:
[0017] Step S1: The middle part of the forged blank is fixed by a middle fixing assembly;
[0018] Step S2: After the two groups of upper horizontal driving modules drive the upper mold I and the upper mold II to close the mold, the upper mold I and the upper mold II are driven by the upper lifting platform to descend from the upper end of the forging blank to the first upper set process position;
[0019] After the two sets of lower horizontal driving modules drive the lower mold I and the lower mold II to close the mold, the lower mold I and the lower mold II are driven to rise from the lower end of the forging blank to the first lower set process position through the lower lifting platform;
[0020] Step S3: the upper forging head and the lower forging head move towards each other at the same speed, respectively performing a local forging and expanding forming on the upper port and the lower port of the forging blank;
[0021] Step S4: the upper die I and the upper die II perform temperature-controlled recrystallization on the local forging expansion forming portion of the upper port of the forging blank; the lower die I and the lower die II perform temperature-controlled recrystallization on the local forging expansion forming portion of the lower port of the forging blank;
[0022] Step S5: the upper forging head and the lower forging head move upward and downward respectively, separate from the upper die assembly and the lower die assembly, and obtain a partially forged forging;
[0023] Step S6: Repeat steps S2 to S5 cyclically, and perform segmented step-by-step forging cycle motion at different upper and lower process positions, respectively, until the entire expansion forming process of the upper and lower ports of the forging is completed.
[0024] The advantages and beneficial effects of the present invention are:
[0025] 1. The present invention provides a forging die for aluminum-based composite thin-walled pipe fittings, which adopts a combination of upper and lower forging die settings and servo forging technology. The upper and lower forging heads move toward each other at the same speed. At the same time, through the step forging method, two bell-mouth shapes with consistent deformation laws are obtained, thereby improving product performance and production efficiency. The upper and lower die assemblies adopt a split structure to facilitate the discharge and removal of forging blanks; the lifting and floating structure of the upper and lower die assemblies enables the suspended sections at both ends of the forging blank to maintain an appropriate length during each step forging, reducing the convection heat dissipation area, and the end of the suspended section is close to the heating contact isothermal hot forging (higher than the recrystallization temperature) area of the upper and lower die assemblies, so that the lattice size of the forging is stable; at the same time, it avoids the crushing instability caused by the suspended section of the thin-walled aluminum-based composite material of the forging blank due to being too high; the suspended section of the thin-walled aluminum-based composite material of the forging blank maintains an appropriate length to ensure that the forging ratio of the bell mouth of the formed forging is consistent from the edge to the inside, avoiding the generation of quality and lattice defects such as microcracks, so that the special-shaped pipe fittings of the double-bell mouth silicon carbide reinforced aluminum-based composite material can be forged and formed, improving the performance and production efficiency of the product.
[0026] 2. The middle fixing assembly of the present invention has inner and outer supporting parts whose shapes match the inner hole and outer shaft curved surface of the forged tube blank, and is used to support the inner and outer tube surfaces of the forged tube blank before forging, effectively solving the problem of instability and deformation of the forged tube blank during forging.
[0027] Other features and advantages of the present invention will be described in the following description, and partly become apparent from the description, or understood by practicing the present invention. The purpose and other advantages of the present invention can be realized and obtained by the structures particularly pointed out in the written description and the accompanying drawings.
[0028] The technical solution of the present invention is further described in detail below through the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:
[0030] Figure 1 It is a schematic diagram of the existing hole expansion forging;
[0031] Figure 2This is a schematic structural diagram of a forging die for an aluminum-based composite material thin-walled pipe fitting according to the present invention;
[0032] Figure 3 This is an axonometric view of a forging die for an aluminum-based composite material thin-walled pipe fitting according to the present invention;
[0033] Figure 4 for Figure 3 Middle A is a partial enlarged view;
[0034] Figure 5 It is a schematic structural diagram of the middle fixing assembly in the present invention;
[0035] Figure 6 It is a structural schematic diagram of the upper mold I in the present invention;
[0036] Figure 7 It is a schematic diagram of the forging process of a forging die for an aluminum-based composite material thin-walled pipe fitting of the present invention;
[0037] Figure 8 It is a schematic diagram of the structure of the present invention after forging into place;
[0038] Fig. 9 for Figure 8 Schematic diagram of the local structure at B in the middle;
[0039] Fig.10 This is a schematic diagram of the structure of the forging prepared by the present invention.
[0040] In the figure: 1-forging blank, 101-blank fixed section, 102-blank suspended section, 2-forging, 201-cylinder, 202-bell mouth, 203-flat flange, 3-press, 301-lifting guide column, 302-upper lifting servo electric cylinder, 303-lower lifting servo electric cylinder, 4-fixed mold, 401-mold fixed section, 5-movable mold, 6-middle fixed component, 601-fixed beam, 602-pressure cover, 603-screw hole, 604-profile core, 605-inter Gap, 7-upper lifting platform, 8-upper die Ⅰ, 801-forging concave surface, 802-horizontal guide hole, 803-horizontal rod, 804-forging plane, 805-forging blank contact surface segment, 9-upper die Ⅱ, 10-upper forging head, 7B-lower lifting platform, 8B-lower die Ⅰ, 9B-lower die Ⅱ, 10B-lower forging head, 11-upper horizontal guide column, 12-upper horizontal servo electric cylinder, 11B-lower horizontal guide column, 12B-lower horizontal servo electric cylinder. DETAILED DESCRIPTION
[0041] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0042] The preferred embodiments of the present invention are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.
[0043] An embodiment of the present invention provides a forging die for thin-walled aluminum-based composite pipe fittings, which uses a forging blank placed vertically and is forged simultaneously up and down by a press to form two bidirectional bell mouths. Figure 2 To Figure Fig.10 As shown, the aluminum-based composite thin-walled pipe forging die is arranged on a press 3, and the press 3 has an upper forging head 10 and a lower forging head 10B arranged relatively. The aluminum-based composite thin-walled pipe forging die comprises an upper die assembly, a middle fixed assembly 6, an upper lifting platform 7, a lower die assembly and a lower lifting platform 7B, wherein the upper lifting platform 7, the middle fixed assembly 6 and the lower lifting platform 7B are arranged on the press 3 from top to bottom in sequence, the middle fixed assembly 6 is used to fix the cylindrical forging blank, the upper die assembly and the lower die assembly are respectively arranged on the upper lifting platform 7 and the lower lifting platform 7B, the upper lifting platform 7 and the lower lifting platform 7B are respectively used to drive the upper die assembly and the lower die assembly to rise and fall, the upper die assembly and the upper forging head 10 cooperate to realize the expansion forging of the upper port of the forging blank, and the lower die assembly and the lower forging head 10B cooperate to realize the expansion forging of the lower port of the forging blank, so as to obtain a forging 2 with two trumpet-shaped ports.
[0044] See also Figures 2 to 4 As shown, in the embodiment of the present invention, the press 3 is a servo press, and lifting guide columns 301 are provided on both sides of the press 3, and both sides of the upper lifting platform 7 and the lower lifting platform 7B are slidably matched with the corresponding lifting guide columns 301; two groups of upper lifting servo electric cylinders 302 are provided on both sides of the upper part of the press 3, and the output ends of the two groups of upper lifting servo electric cylinders 302 are respectively connected to the two sides of the upper lifting platform 7; the two groups of upper lifting servo electric cylinders 302 synchronously drive the upper lifting platform 7 to move up and down along the lifting guide columns 301. Two groups of lower lifting servo electric cylinders 303 are provided on both sides of the lower part of the press 3, and the output ends of the two groups of lower lifting servo electric cylinders 303 are respectively connected to the two sides of the lower lifting platform 7B, and the two groups of lower lifting servo electric cylinders 303 synchronously drive the lower lifting platform 7B to move up and down along the lifting guide columns 301.
[0045] In the embodiment of the present invention, the upper lifting platform 7 includes two upper sliding blocks and two upper horizontal guide pillars 11, wherein the two upper sliding blocks are respectively slidably connected to the lifting guide pillars 301 on both sides of the press 3. Preferably, two lifting guide pillars 301 are provided on both sides of the press 3. The two upper horizontal guide pillars 11 are arranged in parallel between the two upper sliding blocks, and the two ends of each upper horizontal guide pillar 11 are fixed as a whole with the two sliders. The upper mold I8 is slidably matched with one end of the two upper horizontal guide pillars 11, and the upper mold II9 is slidably matched with the other end of the two upper horizontal guide pillars 11.
[0046] In the embodiment of the present invention, the lower lifting platform 7B includes two lower sliding blocks and two lower horizontal guide pillars 11B, wherein the two lower sliding blocks are respectively slidably connected to the lifting guide pillars 301 on both sides of the press 3, and the two lower horizontal guide pillars 11B are arranged in parallel between the two lower sliding blocks, and the two ends of each lower horizontal guide pillar 11B are respectively fixedly connected to the two lower sliding blocks. The lower mold I8B is slidably matched with one end of the two lower horizontal guide pillars 11B, and the lower mold II9B is slidably matched with the other end of the two lower horizontal guide pillars 11B.
[0047] See also Figure 5 As shown, in the embodiment of the present invention, the middle fixed assembly 6 includes a fixed beam 601, a gland 602 and a profiling core 604, wherein the fixed beam 601 is horizontally arranged, and one end is connected to the press 3, the other end of the fixed beam 601 is provided with a semicircular groove, one side of the forging blank is positioned by the semicircular groove, and the other side of the forging blank is positioned by the concave surface of the gland 602, the two sides of the gland 602 are respectively connected to the screw holes 603 on the two sides of the fixed beam 601 by bolts, and a gap 605 is left between the two sides of the gland 602 and the fixed beam 601, so that the contact surfaces between the fixed beam 601, the forging blank, the profiling core 604 and the gland 602 are compacted and close. The profiling core 604 is arranged in the forging blank, and during forging, the profiling core 604 prevents the middle cylinder of the forging blank from deformation and instability. When the screws lock the fixed beam 601 and the gland 602, the middle fixed assembly 6 is locked with the middle of the forging blank. The end groove of the fixed beam 601 and the concave curved surface of the pressure cover 602 match the outer surface shape of the forging blank, and the outer circumferential shape of the profiling core 604 matches the inner surface shape of the forging blank, providing stable support for the inner and outer sides of the forging blank, effectively solving the problem of instability and deformation of the forging blank during forging.
[0048] See also Figures 2 to 4As shown, in an embodiment of the present invention, the upper mold assembly includes an upper mold Ⅰ8, an upper mold Ⅱ9 and two groups of upper horizontal drive modules, wherein the upper mold Ⅰ8 and the upper mold Ⅱ9 are both horizontally slidably connected to the upper lifting platform 7, the two groups of upper horizontal drive modules are relatively arranged on both sides of the upper lifting platform 7, and the output ends are respectively connected to the upper mold Ⅰ8 and the upper mold Ⅱ9, and the corresponding sides of the upper mold Ⅰ8 and the upper mold Ⅱ9 are provided with upper forging dies; the two groups of upper horizontal drive modules are used to drive the upper mold Ⅰ8 and the upper mold Ⅱ9 to close or separate.
[0049] In an embodiment of the present invention, the lower mold assembly includes a lower mold Ⅰ8B, a lower mold Ⅱ9B and two groups of lower horizontal drive modules, wherein the lower mold Ⅰ8B and the lower mold Ⅱ9B are both horizontally slidably connected to the lower lifting platform 7B, the two groups of lower horizontal drive modules are relatively arranged on both sides of the lower lifting platform 7B, and the output ends are respectively connected to the lower mold Ⅰ8B and the lower mold Ⅱ9B, and the corresponding sides of the lower mold Ⅰ8B and the lower mold Ⅱ9B are provided with lower forging dies; the two groups of lower horizontal drive modules are used to drive the lower mold Ⅰ8B and the lower mold Ⅱ9B to close or separate.
[0050] In this embodiment, the upper horizontal driving module is an upper horizontal servo electric cylinder 12. The two upper horizontal servo electric cylinders 12 are arranged horizontally opposite to each other and are both located between the two upper horizontal guide columns 11. The tails of the two upper horizontal servo electric cylinders 12 are respectively fixedly connected to the two upper sliding blocks of the upper lifting platform 7, and the cylinder rods of the two upper horizontal servo electric cylinders 12 are respectively connected to the upper mold Ⅰ8 and the upper mold Ⅱ9. The lower horizontal driving module is a lower horizontal servo electric cylinder 12B. The two lower horizontal servo electric cylinders 12B are arranged horizontally opposite to each other and are both located between the two lower horizontal guide columns 11B. The tails of the two lower horizontal servo electric cylinders 12B are respectively fixedly connected to the two lower sliding blocks of the lower lifting platform 7B, and the cylinder rods of the two lower horizontal servo electric cylinders 12B are respectively connected to the lower mold Ⅰ8B and the lower mold Ⅱ9B.
[0051] Furthermore, the upper mold I8, the upper mold II9, the lower mold I8B and the lower mold II9B are all provided with a temperature control module, which is used to heat and recrystallize the forging blank. Specifically, the temperature control module includes common near-isothermal forging devices such as a heating coil, a temperature measurement sensor, and a water cooling pipeline system.
[0052] See also Fig.10 As shown, the forging 2 includes a cylinder 201 and bell mouths 202 located at both ends of the cylinder 201 . The bell mouth 202 is an open structure with a gradually variable thickness, and the outer edge of the bell mouth 202 is provided with a flat flange 203 .
[0053] In the embodiment of the present invention, the upper forging die and the lower forging die are horn-shaped structures mirror-set along the axis direction of the forging blank. Figure 6 As shown, the upper forging die and the lower forging die both include a forging plane 804, a forging concave curved surface 801 and a forging blank contact curved surface section 805 which are arranged in sequence from the outside to the inside, wherein the forging blank contact curved surface section 805 is used to fix and limit the forging 2 during forging, the forging concave curved surface 801 is used to form the bell mouth 202 of the forging 2, and the forging plane 804 is used to form the plane flange 203 of the forging 2.
[0054] Furthermore, the rear ends of the upper mold I8, the upper mold II9, the lower mold I8B and the lower mold II9B are all provided with horizontal rods 803 for connecting with the horizontal driving module. The upper mold I8, the upper mold II9, the lower mold I8B and the lower mold II9B are all provided with horizontal guide holes 802 on both sides.
[0055] In this embodiment, the forging blank is a thin-walled tube, and the cross-section of the forging blank is a regular shape, such as the ellipse in this embodiment, or any regular geometric shape such as a quadrilateral, five-deformation, six-deformation, etc. The material of the forging blank is silicon carbide fiber reinforced aluminum-based composite material.
[0056] In the embodiment of the present invention, the outer edges of the punch ends of the upper forging head 10 and the lower forging head 10B are rounded to facilitate smooth insertion into the forged tube blank. Accordingly, the inner edges of the ends of the forged tube blank are rounded to inhibit the inflow of metal at the inner edge of the original blank and prevent local folding.
[0057] An embodiment of the present invention provides a forging die for thin-walled pipe fittings of aluminum-based composite materials. The forged pipe blank is placed vertically and fixed by a middle fixing component 6. The upper forging head 10 and the lower forging head 10B move toward each other at the same speed to perform synchronous forging and expanding at both ends of the forged blank. Through servo step forging, the upper forging die and the lower forging die are controlled to synchronously retreat by one process step, thereby obtaining two bell-mouth shapes with consistent deformation laws, so that double-bell-mouth silicon carbide reinforced aluminum-based composite material special-shaped pipe fittings can be forged and formed, thereby improving product performance and production efficiency.
[0058] See also Figures 2 to 10 As shown, another embodiment of the present invention provides a forging method using the aluminum-based composite material thin-walled pipe forging die in the above embodiment, and the forging method includes the following steps:
[0059] Step S1: The middle part of the forged blank is fixed by a middle fixing assembly 6;
[0060] Step S2: After the two upper horizontal drive modules drive the upper mold I8 and the upper mold II9 to close the mold, the upper mold I8 and the upper mold II9 are driven by the upper lifting platform 7 to descend from the upper end of the forging blank to the first upper setting process position, see Figure 7 (a)
[0061] After the two sets of lower horizontal driving modules drive the lower mold Ⅰ8B and the lower mold Ⅱ9B to close the mold, the lower mold Ⅰ8B and the lower mold Ⅱ9B are driven by the lower lifting platform 7B to rise from the lower end of the forging blank to the first lower setting process position;
[0062] Step S3: The upper forging head 10 and the lower forging head 10B move towards each other at the same speed, and the upper forging head 10 and the lower forging head 10B respectively perform a local forging and expanding forming on the upper port and the lower port of the forging blank, see Figure 7 (b)
[0063] Step S4: the upper die I8 and the upper die II9 perform temperature-controlled recrystallization on the local forging expansion forming portion of the upper port of the forging blank; the lower die I8B and the lower die II9B perform temperature-controlled recrystallization on the local forging expansion forming portion of the lower port of the forging blank;
[0064] Step S5: the upper forging head 10 and the lower forging head 10B move upward and downward respectively, separate from the upper die assembly and the lower die assembly, and obtain a partially forged forging 2;
[0065] Step S6: Repeat steps S2 to S5 in a loop;
[0066] Specifically, the upper mold I8 and the upper mold II9 are driven down to the second upper setting process position by the upper lifting platform 7, see Figure 7 (c) As shown; the lower die Ⅰ8B and the lower die Ⅱ9B are driven to rise to the second lower setting process position by the lower lifting platform 7B; the upper forging head 10 and the lower forging head 10B respectively perform secondary local forging and expanding forming on the upper and lower ports of the forging blank, see Figure 7 (d) As shown; the upper die Ⅰ8 and the upper die Ⅱ9 perform temperature-controlled recrystallization on the secondary local forging expansion forming part of the upper port of the forging blank; the lower die Ⅰ8B and the lower die Ⅱ9B perform temperature-controlled recrystallization on the secondary local forging expansion forming part of the lower port of the forging blank; the upper forging head 10 and the lower forging head 10B move upward and downward respectively, and separate from the upper die assembly and the lower die assembly; the upper die Ⅰ8 and the upper die Ⅱ9 are driven by the upper lifting platform 7 to descend to the third upper setting process position, see Figure 7 (e) As shown; the lower die I8B and the lower die II9B are driven by the lower lifting platform 7B to rise to the third lower set process position, and three local forging expansion forming and temperature control recrystallization are performed; in this way, the segmented step-by-step forging cycle movement is performed at different upper and lower set process positions respectively until the entire expansion forming process of the upper and lower ports of the forging 2 is completed, and finally the forging 2 with bell mouths at both ends is obtained, see Fig.10shown.
[0067] Specifically, the upper and lower setting process positions are simulated by forging simulation software, which helps to ensure forging streamlines, reduce forging defects, and improve forging quality.
[0068] See also Figure 8 As shown, when the last forging is completed, the edge of the upper port of the forging 2 is in contact with the forging plane 804 of the upper die Ⅰ8 and the upper die Ⅱ9, and the edge of the lower port of the forging 2 is in contact with the forging plane 804 of the lower die Ⅰ8B and the lower die Ⅱ9B, forming a flat flange 203 of the forging 2.
[0069] Another embodiment of the present invention provides a forging method for thin-walled aluminum-based composite material pipe fittings, which uses servo forging technology to achieve a step-by-step forging cycle with a high degree of hole expansion, so that double-flared silicon carbide reinforced aluminum-based composite material special-shaped pipe fittings can be forged and formed, thereby improving product performance and production efficiency. It is also easy to put the forged pipe blank into the mold and convenient to take out the formed part.
[0070] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A forging die for aluminum-based composite thin-walled pipe fittings, arranged on a press (3), the press (3) having an upper forging head (10) and a lower forging head (10B) arranged opposite to each other, characterized in that: The forging die comprises an upper die assembly, a middle fixed assembly (6), an upper lifting platform (7), a lower die assembly and a lower lifting platform (7B), wherein the upper lifting platform (7), the middle fixed assembly (6) and the lower lifting platform (7B) are arranged on the press (3) in sequence from top to bottom, the middle fixed assembly (6) is used to fix the cylindrical forging blank, the upper die assembly and the lower die assembly are respectively arranged on the upper lifting platform (7) and the lower lifting platform (7B), the upper lifting platform (7) and the lower lifting platform (7B) are respectively used to drive the upper die assembly and the lower die assembly to rise and fall, the upper die assembly and the upper forging head (10) cooperate to realize the expansion forging of the upper port of the forging blank, and the lower die assembly and the lower forging head (10B) cooperate to realize the expansion forging of the lower port of the forging blank, so as to obtain a forging (2) with two trumpet-shaped ports.
2. The aluminum-based composite material thin-wall pipe forging die according to claim 1, characterized in that: The upper mold assembly comprises an upper mold I (8), an upper mold II (9) and two groups of upper horizontal drive modules, wherein the upper mold I (8) and the upper mold II (9) are both horizontally slidably connected to the upper lifting platform (7), the two groups of upper horizontal drive modules are relatively arranged on both sides of the upper lifting platform (7), and the output ends are respectively connected to the upper mold I (8) and the upper mold II (9), and the corresponding sides of the upper mold I (8) and the upper mold II (9) are both provided with upper forging dies; the two groups of upper horizontal drive modules are used to drive the upper mold I (8) and the upper mold II (9) to close or separate the molds.
3. The aluminum-based composite material thin-wall pipe forging die according to claim 2, characterized in that: The lower mold assembly comprises a lower mold I (8B), a lower mold II (9B) and two groups of lower horizontal drive modules, wherein the lower mold I (8B) and the lower mold II (9B) are both horizontally slidably connected to the lower lifting platform (7B), the two groups of lower horizontal drive modules are relatively arranged on both sides of the lower lifting platform (7B), and the output ends are respectively connected to the lower mold I (8B) and the lower mold II (9B), and the corresponding sides of the lower mold I (8B) and the lower mold II (9B) are both provided with lower forging dies; the two groups of lower horizontal drive modules are used to drive the lower mold I (8B) and the lower mold II (9B) to close or separate the molds.
4. The aluminum-based composite material thin-wall pipe forging die according to claim 3, characterized in that: The upper forging die and the lower forging die are trumpet-shaped structures mirror-set along the axial direction of the forging blank.
5. The aluminum-based composite material thin-wall pipe forging die according to claim 4, characterized in that: The upper mold I (8), the upper mold II (9), the lower mold I (8B) and the lower mold II (9B) are all provided with temperature control modules.
6. The aluminum-based composite material thin-wall pipe forging die according to claim 5, characterized in that: The middle fixing assembly (6) comprises a fixing beam (601), a pressure cover (602) and a profiling core (604), wherein the fixing beam (601) is arranged horizontally and one end is connected to the press (3), a groove is arranged at the other end of the fixing beam (601), the forging blank is positioned in the groove and fixed by the pressure cover (602), and the profiling core (604) is arranged on the inner side of the forging blank.
7. The aluminum-based composite material thin-wall pipe forging die according to claim 6, characterized in that: The press (3) is provided with lifting guide pillars (301) on both sides, and the upper lifting platform (7) and the lower lifting platform (7B) are slidably matched with the corresponding lifting guide pillars (301); Two groups of upper lifting servo electric cylinders (302) are provided on both sides of the upper part of the press (3), and the output ends of the two groups of upper lifting servo electric cylinders (302) are respectively connected to both sides of the upper lifting platform (7); Two groups of lower lifting servo electric cylinders (303) are respectively provided on both sides of the lower part of the press (3), and the output ends of the two groups of lower lifting servo electric cylinders (303) are respectively connected to both sides of the lower lifting platform (7B).
8. The aluminum-based composite material thin-wall pipe forging die according to claim 1, characterized in that: The forging (2) comprises a cylinder (201) and bell mouths (202) located at two ends of the cylinder (201), and the outer edge of the bell mouth (202) is provided with a plane flange (203).
9. A forging method using the aluminum-based composite material thin-walled pipe forging die according to claim 7, characterized in that: The forging method comprises the following steps: Step S1: The middle part of the forged blank is fixed by a middle fixing assembly (6); Step S2: After the two groups of upper horizontal driving modules drive the upper mold I (8) and the upper mold II (9) to close the mold, the upper mold I (8) and the upper mold II (9) are driven by the upper lifting platform (7) to descend from the upper end of the forging blank to the first upper set process position; After the two sets of lower horizontal driving modules drive the lower mold I (8B) and the lower mold II (9B) to close the mold, the lower mold I (8B) and the lower mold II (9B) are driven by the lower lifting platform (7B) to rise from the lower end of the forging blank to the first lower set process position; Step S3: the upper forging head (10) and the lower forging head (10B) move towards each other at the same speed, respectively performing a local forging and expanding forming on the upper port and the lower port of the forged blank; Step S4: the upper die I (8) and the upper die II (9) perform temperature-controlled recrystallization on the local forging expansion forming portion of the upper port of the forging blank; the lower die I (8B) and the lower die II (9B) perform temperature-controlled recrystallization on the local forging expansion forming portion of the lower port of the forging blank; Step S5: the upper forging head (10) and the lower forging head (10B) move upward and downward respectively, separate from the upper die assembly and the lower die assembly, and obtain a partially forged forging (2); Step S6: Repeating steps S2 to S5 cyclically, respectively performing segmented stepwise forging cycle motion at different upper and lower setting process positions, until the entire expansion forming process of the upper and lower ports of the forging (2) is completed.