Laser light path adjusting device and forming method for melting additive manufacturing of laser powder bed
By using a laser optical path adjustment device in laser powder bed melting technology, using a piezoelectric ceramic ultrasonic motor to adjust the laser beam angle, combined with large spot filling and preheating mode, the problems of low printing efficiency and quality in the existing technology are solved, and the problem of low printing efficiency and quality is realized Efficient and stable additive manufacturing process.
Patent Information
- Application Number
- CN202411211356.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-08-30
AI Technical Summary
When improving printing efficiency, existing laser powder bed melting technology has problems such as optical path stability, high device complexity, high failure rate, low printing quality, and prone to cracks on the surface of difficult-to-form materials.
A laser optical path adjustment device is adopted, including a selection valve box, a plane mirror, an optical fiber head, a beam expanding mirror and a piezoelectric ceramic ultrasonic motor. The angle of the third reflector is adjusted through a single piezoelectric ceramic ultrasonic motor to achieve high power and low power The parallel arrangement and angle changes of the laser beam are combined with the large spot filling printing mode and the large spot preheating mode to improve printing efficiency and accuracy.
It reduces the difficulty and failure rate of the device, improves the printing efficiency of the internal filling area, ensures the performance of parts, expands the types of printable materials, simplifies the optical path structure, and improves the reliability and printing accuracy of equipment.
Smart Images

Figure CN119078192A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of additive manufacturing, and in particular relates to a laser optical path adjustment device and a forming method for laser powder bed melting additive manufacturing. Background Art
[0002] As an advanced additive manufacturing technology, laser powder bed fusion (LPBF) uses laser as the energy source and metal powder as the printing material. Under the heat of the laser beam, the metal powder is completely melted, quickly solidified, and added layer by layer. LPBF has attracted widespread attention due to the advantages of high precision, good surface quality, and excellent performance of the formed parts. The general process of LPBF printing is as follows: first, the three-dimensional model of the processed part is converted into a slice file to obtain the forming information of each section; then the powder laying system lays a layer of powder on the substrate according to the set powder layer thickness; then the high-energy laser beam selects and melts the metal powder according to the slice forming information to complete the processing of the current layer; then the substrate moves down one layer, and a new round of powder laying and scanning begins, and the entire part is processed layer by layer; during the LPBF forming process, the forming chamber is always filled with inert gas to prevent high-temperature oxidation of the metal. For laser powder bed fusion technology, improving printing efficiency is an important concern under the premise of ensuring the performance of the printed parts.
[0003] To improve the printing efficiency, the existing solutions mainly adopt variable spot printing. The printing area of each cross section of the part can be divided into two parts: one is the shape line area, and the other is the internal filling area, such as Figure 1 As shown, these two parts of the printing area correspond to the contour line and the filling line respectively. It can be seen intuitively that the area proportion of the internal filling area is much larger than the area proportion of the shape line area, and the number of filling lines is also much larger than the number of contour lines; therefore, in order to improve the printing efficiency under the premise of ensuring the performance of the parts, the shape line area and the internal filling area require different printing strategies. The purpose of variable spot printing is to use a small spot of a low-power laser to print the shape line area, and to use a large spot of a high-power laser to fill the internal filling area as much as possible, so as to increase the spacing between adjacent filling lines, thereby reducing the number of filling lines and improving the printing efficiency. For example, the patent application named "A dual-laser single galvanometer printing system and method" (publication number CN218799127U) adds two collimating lenses and a new galvanometer unit. The two collimating lenses change the spot size of the incident laser emitted by the low-power high-beam quality laser and the high-power laser respectively, and make the two laser beams have an intersection. The newly added x-axis and y-axis galvanometer units are driven by motors to change the angle, so that the optical paths of the low-power laser beam and the high-power laser beam coincide, thereby realizing variable spot printing to improve printing efficiency.
[0004] Taking all factors into consideration, the above scheme has the following disadvantages: 1) The installation and layout of two or more collimating lenses has not been considered. The newly added unit is difficult to integrate with the original galvanometer system of the equipment, and it is difficult to be applied in printing equipment with space layout requirements; 2) The optical path stability of the laser powder bed melting equipment is a prerequisite for ensuring the stability of the quality of the formed parts. The newly added x-axis and y-axis galvanometer units are driven by ordinary motors to achieve angle changes. There are many problems such as difficulty in coordinated control of dual motors, slow motor response speed, low position resolution, and magnetic disturbance, which leads to the optical path of the low-power laser beam and the high-power laser beam not overlapping, which directly affects the formation. The quality stability of the shaped parts; 3) Although a single galvanometer system is adopted, the new x-axis and y-axis galvanometer units are added, which further increases the overall complexity of the galvanometer system. The additive manufacturing technology requires extremely high equipment reliability, which greatly increases the failure rate and maintenance difficulty; 4) The splicing problem of variable spot printing is an important reason affecting the performance of printed parts. Due to the obvious uneven distribution of large spot energy, the joints of the internal filling area and the shape line area inevitably have problems of low splicing accuracy and poor stability, and the performance of the parts cannot be guaranteed; 5) There is no preheating for difficult-to-form materials during the printing process, and cracks are prone to appear on the surface of the forming layer. Summary of the invention
[0005] In order to overcome the shortcomings of the above-mentioned prior art, the purpose of the present invention is to provide a laser optical path adjustment device and a forming method for laser powder bed fusion additive manufacturing. Under the premise of ensuring the performance of printed parts, the difficulty of device maintenance and the failure rate are reduced, the printing efficiency of the internal filling area in the additive manufacturing process is improved, and it can be applied to printing equipment with spatial layout requirements.
[0006] In order to achieve the above object, the technical solution adopted by the present invention is:
[0007] A laser optical path adjustment device for laser powder bed fusion additive manufacturing comprises a selector valve housing 1, a plane mirror 2 is provided at a laser beam outlet at the front end of the selector valve housing 1, two optical fiber head connection ports at the rear end of the selector valve housing 1 are respectively connected to a low-power laser optical fiber head 14 and a high-power laser optical fiber head 15, a high-power laser beam 23 input by the high-power laser optical fiber head 15 is emitted from the laser beam outlet via a beam expander 12, a second reflector 8, a third reflector 10, and a plane mirror 2, a low-power laser beam 24 input by the low-power laser optical fiber head 14 is emitted from the laser beam outlet via a first reflector 6, a third reflector 10, and a plane mirror 2, and the third reflector 10 can be rotated to change its angle.
[0008] The low-power laser optical fiber head 14 and the high-power laser optical fiber head 15 are connected to the selector valve housing 1 via the optical fiber support plate 3 by laser welding.
[0009] The third reflector 10 is connected to the piezoelectric ceramic ultrasonic motor 4 , the piezoelectric ceramic ultrasonic motor 4 is connected to the motor fixing plate 5 , and the motor fixing plate 5 is connected to the selection valve housing 1 by laser welding.
[0010] The first reflector 6 is connected to the first rectangular rod 7, and both ends of the first rectangular rod 7 are connected to the selection valve box 1; the second reflector 8 is connected to the second rectangular rod 9, and both ends of the second rectangular rod 9 are connected to the selection valve box 1; the third reflector 10 is connected to the rotating rod 11, and the rotating rod 11 is connected to the piezoelectric ceramic ultrasonic motor 4.
[0011] The rotating rod 11 is designed with an internal structure by using a lattice optimization method and is manufactured by using an additive manufacturing method.
[0012] The beam expander 12 is fixed on a beam expander bracket 13 , and the beam expander bracket 13 is connected to the selection valve box 1 .
[0013] The first reflector 6, the second reflector 8 and the third reflector 10 are all square in shape, with their centroids located on the same vertical line, and the area of the reflective surface is more than 100 times the area of the laser spot.
[0014] The first reflector 6, the second reflector 8 and the third reflector 10 are all made of high-purity ultraviolet fused quartz substrate and coated with ultra-high laser-induced damage threshold dielectric film, which can withstand high-energy pulses, with an incident angle of 0-45° and a reflectivity of more than 99%.
[0015] The low power laser uses a beam quality M 2 The single-mode fiber laser with a power of 400-800W and a power of less than 1.2 is used. The high-power laser uses a fiber laser with a power of more than 4000W.
[0016] A forming method using the laser optical path adjustment device for laser powder bed fusion additive manufacturing includes a large spot filling printing mode forming method and a large spot preheating mode forming method;
[0017] The method for forming a large light spot filling printing pattern comprises the following steps:
[0018] S1. Connect the low-power laser fiber head 14 and the high-power laser fiber head 15 to the selector valve housing 1, and arrange the two laser fiber heads in parallel so that the low-power laser beam 24 and the high-power laser beam 23 remain parallel; the spot diameter formed by the high-power laser beam 23 after passing through the beam expander 12 and the galvanometer system is larger than the spot diameter formed by the low-power laser beam 24 after passing through the galvanometer system;
[0019] S2. When printing the internal filling area, the high-power laser is turned on, the low-power laser is turned off, the piezoelectric ceramic ultrasonic motor 4 is started and the angle of the third reflector 10 is adjusted so that the expanded high-power laser beam 23 is reflected out of the dual laser selection valve and enters the galvanometer system, and then scans the filling line;
[0020] S3. When printing the shape line area, the low-power laser is turned on, the high-power laser is turned off, the piezoelectric ceramic ultrasonic motor 4 is started and the angle of the third reflector 10 is adjusted so that the low-power laser beam 24 is reflected out of the dual laser selection valve and enters the galvanometer system, and then scans the contour line;
[0021] S4. After the shape line area is printed, continue to use the low-power laser beam 24 to scan the joint between the internal filling area and the shape line area.
[0022] The large spot preheating mode forming method comprises the following steps:
[0023] S1. Connect the low-power laser fiber head 14 and the high-power laser fiber head 15 to the selector valve housing 1, and arrange the two laser fiber heads in parallel so that the low-power laser beam 24 and the high-power laser beam 23 remain parallel; the spot diameter formed by the high-power laser beam 23 after passing through the beam expander 12 and the galvanometer system is larger than the spot diameter formed by the low-power laser beam 24 after passing through the galvanometer system;
[0024] S2. When printing hard-to-melt materials, the high-power laser is turned on, the low-power laser is turned off, the piezoelectric ceramic ultrasonic motor 4 is started and the angle of the third reflector 10 is adjusted so that the expanded high-power laser beam 23 is reflected out of the dual laser selection valve and enters the galvanometer system, and then the printing surface is preheated;
[0025] S3. After the printing surface is preheated, the low-power laser is turned on, the high-power laser is turned off, the piezoelectric ceramic ultrasonic motor 4 is started and the angle of the third reflector 10 is adjusted so that the low-power laser beam 24 is reflected out of the dual laser selection valve and enters the galvanometer system, and then the part is printed;
[0026] S4. Repeat steps S2 and S3 for each cross section of the printed part until the part is printed.
[0027] In the steps S2 and S3, the angle at which the piezoelectric ceramic ultrasonic motor 4 rotates the third reflector 10 is 90°.
[0028] Compared with the prior art, the present invention has the following beneficial effects:
[0029] 1. The laser optical path adjustment device for laser powder bed fusion additive manufacturing of the present invention can be installed outside the galvanometer system, so that the overall printing equipment adopts a single galvanometer system without changing the structure and composition of the original galvanometer system. On the one hand, the cost of a set of galvanometer systems is saved, and on the other hand, the overall reliability of the equipment and the difficulty of daily maintenance are improved.
[0030] 2. The laser optical path adjustment device for laser powder bed melting additive manufacturing of the present invention adjusts the angle of the third reflector through a single piezoelectric ceramic ultrasonic motor to ensure that the optical paths of the high-power laser beam and the low-power laser beam entering the galvanometer system are the same. On the basis of ensuring the simplicity of the optical path, it further realizes the characteristics of fast response speed, simple control, high optical path accuracy, compact overall structure and high practicality.
[0031] 3. The present invention provides a forming method for a laser optical path adjustment device for laser powder bed melting additive manufacturing, which uses a high-power laser beam to print an internal filling area, and uses a low-power laser beam to print a shape line area, and then uses a low-power laser beam to further scan the joints of the internal filling area and the shape line area, thereby improving the printing efficiency and ensuring the performance of the printed parts, overcoming the problem of low printing quality in existing variable spot printing and improving the practicability of variable spot printing.
[0032] 4. The forming method of the laser optical path adjustment device for laser powder bed melting additive manufacturing of the present invention has two working modes: a large spot filling printing mode and a large spot preheating mode; large spot preheating is performed on difficult-to-melt materials, which improves the printing and forming accuracy and performance of difficult-to-melt material parts, expands the types of printable materials of the printing equipment, and effectively reduces the equipment cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 It is a schematic diagram of the cross-section printing area of a variable spot printing part.
[0034] Figure 2 It is a structural diagram of a dual laser selection valve device according to an embodiment of the present invention.
[0035] Figure 3 1 is a structural diagram of a valve box body 1 selected in an embodiment of the present invention.
[0036] Figure 4 It is a structural diagram of the first rectangular parallelepiped rod 7 and the second rectangular parallelepiped rod 9 according to an embodiment of the present invention.
[0037] Figure 5 1 is a structural diagram of the rotating rod 11 according to an embodiment of the present invention.
[0038] Figure 6 It is a structural diagram of the first reflecting mirror 6, the second reflecting mirror 8 and the third emitting mirror 10 according to an embodiment of the present invention.
[0039] Figure 7 It is a schematic diagram of the path of a high-power laser beam in a dual laser selection valve according to an embodiment of the present invention.
[0040] Figure 8 It is a schematic diagram of the path of the low-power laser beam in the dual laser selection valve according to an embodiment of the present invention.
[0041] Fig. 9 It is a schematic diagram of a large-diameter light spot (right) formed on the printing surface by a high-power laser beam 23 and a small-diameter light spot (left) formed on the printing surface by a low-power laser beam 24 according to an embodiment of the present invention. DETAILED DESCRIPTION
[0042] The present invention will be described in detail below in conjunction with the accompanying drawings and embodiments. The following embodiments are used to illustrate the present invention but are not used to limit the scope of the present invention.
[0043] Reference Figure 2 and Figure 3 A laser optical path adjustment device for laser powder bed fusion additive manufacturing comprises a selector valve housing 1, a plane mirror 2 is arranged at the laser beam outlet at the front end of the selector valve housing 1, two optical fiber head connection ports at the rear end of the selector valve housing 1 are respectively connected to a low-power laser optical fiber head 14 and a high-power laser optical fiber head 15, a high-power laser beam 23 input by the high-power laser optical fiber head 15 is emitted from the laser beam outlet via a beam expander 12, a second reflector 8, a third reflector 10, and a plane mirror 2, a low-power laser beam 24 input by the low-power laser optical fiber head 14 is emitted from the laser beam outlet via a first reflector 6, a third reflector 10, and a plane mirror 2, and the third reflector 10 can be rotated to change its angle.
[0044] The low-power laser fiber head 14 and the high-power laser fiber head 15 are connected to the selector valve housing 1 by laser welding via the optical fiber support plate 3, in order to reduce the number of device parts and reduce the deformation of the selector valve housing 1 by utilizing the advantages of small heat-affected zone and small welding stress of laser welding.
[0045] The third reflector 10 is connected to the piezoelectric ceramic ultrasonic motor 4, the piezoelectric ceramic ultrasonic motor 4 is connected to the motor fixing plate 5, and the motor fixing plate 5 is connected to the selection valve box 1 by laser welding, so as to reduce the number of parts of the device and utilize the advantages of small heat affected zone and small welding stress of laser welding to reduce the deformation of the selection valve box 1.
[0046] The first reflector 6 is used to change the direction of a low-power, high-beam-quality laser beam. The first reflector 6 is connected to a first rectangular rod 7, and both ends of the first rectangular rod 7 are connected to the selection valve box 1; the second reflector 8 is used to change the direction of a high-power laser beam. The second reflector 8 is connected to a second rectangular rod 9, and both ends of the second rectangular rod 9 are connected to the selection valve box 1; the third reflector 10 is used to change the direction of a high-power laser beam or change the direction of a low-power, high-beam-quality laser beam. The third reflector 10 is connected to a rotating rod 11, and the rotating rod 11 is connected to a piezoelectric ceramic ultrasonic motor 4.
[0047] The beam expander 12 is fixed on a beam expander bracket 13 , and the beam expander bracket 13 is connected to the selection valve box 1 .
[0048] Reference Figure 3 The selection valve box body 1 has first square fixing holes 101 on the upper left and right sides for positioning the first rectangular rod 7; the selection valve box body 1 has first circular fixing holes 102 in the middle left and right sides for positioning the rotating rod 11; the selection valve box body 1 has second square fixing holes 103 on the lower left and right sides for positioning the second rectangular rod 9; the selection valve box body 1 has a second circular fixing hole 104 at the front end for fixing the plane mirror 2; the selection valve box body 1 has a first optical fiber head connection port 105 and a second optical fiber head connection port 106 at the rear end for fixing the low-power laser optical fiber head 14 and the high-power laser optical fiber head 15 respectively; the selection valve box body 1 has a first screw hole 107 on the inner bottom plate, and the beam expander bracket 13 is connected to the selection valve box body 1 through the first screw 16 through the first screw hole 107.
[0049] Reference Figure 3 The motor fixing plate 5 is provided with a threaded through hole 501 , and the piezoelectric ceramic ultrasonic motor 4 is connected to the motor fixing plate 5 via a bolt 17 through the threaded through hole 501 .
[0050] Reference Figure 4 The first rectangular parallelepiped rod 7 has second screw holes 701 at both ends and is fixed to the selection valve box 1 by second screws 18; a fifth screw hole 702 is opened in the middle of the first rectangular parallelepiped rod 7 for fixing the first reflector 6.
[0051] Reference Figure 4 The second rectangular rod 9 has third screw holes 901 at both ends and is fixed to the selection valve box 1 by third screws 19; a sixth screw hole 902 is opened in the middle of the second rectangular rod 9 for fixing the second reflector 8.
[0052] Reference Figure 5A fourth screw hole 1101 is formed at one end of the rotating rod 11 and is fixed to the selection valve housing 1 by a fourth screw 20; a square hole 1102 is formed at the other end of the rotating rod 11 and is connected to the transmission shaft of the piezoelectric ceramic ultrasonic motor 4; a seventh screw hole 1103 is formed in the middle of the rotating rod 11 and is used to fix the third reflector 10.
[0053] The rotating rod 11 is designed with an internal structure by a dot matrix optimization method and is manufactured by an additive manufacturing method, so as to reduce the weight and the moment of inertia, thereby improving the response speed of the third reflector 10 .
[0054] The lengths of the first rectangular parallelepiped rod 7 , the second rectangular parallelepiped rod 9 and the rotating rod 11 are all the same as the width of the selector valve housing 1 .
[0055] Reference Figure 6 The first reflector 6 has first through holes 601 on both sides and is fixed to the middle of the first rectangular rod 7 by a fifth screw 21. The angle between its reflective surface and the bottom surface of the selection valve box 1 is 45°.
[0056] Reference Figure 6 The second reflector 8 has second through holes 801 on both sides and is fixed in the middle of the second rectangular rod 9 by the sixth screw 22. The angle between its reflective surface and the bottom surface of the selection valve box 1 is 135°.
[0057] Reference Figure 6 The third reflector 10 has third through holes 1001 on both sides and is fixed to the middle of the rotating rod 11 by a seventh screw 23.
[0058] The first reflector 6, the second reflector 8 and the third reflector 10 are all square in shape, with their centroids located on the same vertical line, and the area of the reflective surface is more than 100 times the area of the laser spot.
[0059] The first reflector 6, the second reflector 8 and the third reflector 10 are all made of high-purity ultraviolet fused quartz substrate and coated with ultra-high laser-induced damage threshold dielectric film, which can withstand high-energy pulses, with an incident angle of 0-45° and a reflectivity of more than 99%.
[0060] The low power laser uses a beam quality M 2 The single-mode fiber laser with a power of 400-800W and a power of less than 1.2 is used. The high-power laser uses a fiber laser with a power of more than 4000W.
[0061] A forming method using the laser optical path adjustment device for laser powder bed fusion additive manufacturing includes a large spot filling printing mode forming method and a large spot preheating mode forming method;
[0062] The method for forming a large light spot filling printing pattern comprises the following steps:
[0063] S1. Reference Figure 7 and Figure 8 , connect the low-power laser fiber head 14 and the high-power laser fiber head 15 to the selector valve housing 1, and arrange the two laser fiber heads in parallel so that the low-power laser beam 24 and the high-power laser beam 23 remain parallel; the spot diameter formed by the high-power laser beam 23 after passing through the beam expander 12 and the galvanometer system is 10 times the spot diameter formed by the low-power laser beam 24 after passing through the galvanometer system;
[0064] S2. Reference Figure 7 and Fig. 9 When printing the internal filling area, the high-power laser is turned on, the low-power laser is turned off, the piezoelectric ceramic ultrasonic motor 4 is started and the angle of the third reflector 10 is adjusted. The high-power laser beam 23 emitted by the high-power laser passes through the second reflector 8 and the third emission mirror 10 successively, so that the expanded high-power laser beam 23 is reflected out of the dual laser selection valve and enters the galvanometer system, and then scans the filling line. The spot diameter formed on the printing surface is 800μm;
[0065] S3. Reference Figure 8 and Fig. 9 When printing the shape line area, the low-power laser is turned on, the high-power laser is turned off, the piezoelectric ceramic ultrasonic motor 4 is started and the angle of the third reflector 10 is adjusted. The low-power laser beam 24 emitted by the low-power laser passes through the first reflector 6 and the third emission mirror 10 successively, so that the low-power laser beam 24 is reflected out of the dual laser selection valve and enters the galvanometer system, and then scans the contour line. The spot diameter formed on the printing surface is 80μm;
[0066] S4. Considering the uneven energy distribution of the laser spot, which leads to low stitching accuracy and poor stability at the joints of the internal filling area and the shape line area, after the shape line area is printed, continue to use a low-power laser beam 24 to scan the joints of the internal filling area and the shape line area.
[0067] The large spot preheating mode forming method comprises the following steps:
[0068] S1. Reference Figure 7 and Figure 8 , connect the low-power laser fiber head 14 and the high-power laser fiber head 15 to the selector valve housing 1, and arrange the two laser fiber heads in parallel so that the low-power laser beam 24 and the high-power laser beam 23 remain parallel; the spot diameter formed by the high-power laser beam 23 after passing through the beam expander 12 and the galvanometer system is 10 times the spot diameter formed by the low-power laser beam 24 after passing through the galvanometer system;
[0069] S2. Reference Figure 7 and Fig. 9 When printing hard-to-melt materials, the high-power laser is turned on, the low-power laser is turned off, the piezoelectric ceramic ultrasonic motor 4 is started and the angle of the third reflector 10 is adjusted. The high-power laser beam 23 emitted by the high-power laser passes through the second reflector 8 and the third emission mirror 10 successively, so that the expanded high-power laser beam 23 is reflected out of the dual laser selection valve and enters the galvanometer system. The spot diameter formed on the printing surface is 800μm, and then the printing surface is preheated;
[0070] S3. Reference Figure 8 and Fig. 9 After the preheating of the printing surface is completed, the low-power laser is turned on, the high-power laser is turned off, the piezoelectric ceramic ultrasonic motor 4 is started and the angle of the third reflector 10 is adjusted. The low-power laser beam 24 emitted by the low-power laser passes through the first reflector 6 and the third emission mirror 10 successively, so that the low-power laser beam 24 is reflected out of the dual laser selection valve and enters the galvanometer system. The spot diameter formed on the printing surface is 80μm, and then the part is printed;
[0071] S4. Repeat steps S2 and S3 for each cross section of the printed part until the part is printed.
[0072] In the steps S2 and S3, the angle at which the piezoelectric ceramic ultrasonic motor 4 rotates the third reflector 10 is 90°, thereby ensuring that the high-power laser beam 23 and the low-power laser beam 24 have the same optical path when entering the galvanometer system.
[0073] The present invention is described in detail above in conjunction with the embodiments, but the contents described are only preferred embodiments of the present invention and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made according to the scope of application of the present invention should still fall within the scope of the present invention.
Claims
1. A laser optical path adjustment device for laser powder bed fusion additive manufacturing, comprising a selector valve housing (1), Features: A plane mirror (2) is provided at the laser beam outlet at the front end of the selector valve housing (1), and two optical fiber head connection ports at the rear end of the selector valve housing (1) are respectively connected to a low-power laser optical fiber head (14) and a high-power laser optical fiber head (15). A high-power laser beam (23) input by the high-power laser optical fiber head (15) is emitted from the laser beam outlet via a beam expander (12), a second reflector (8), a third reflector (10), and a plane mirror (2). A low-power laser beam (24) input by the low-power laser optical fiber head (14) is emitted from the laser beam outlet via a first reflector (6), a third reflector (10), and a plane mirror (2), and the third reflector (10) rotates to change its angle.
2. The device according to claim 1, Features: The low-power laser optical fiber head (14) and the high-power laser optical fiber head (15) are connected to the selection valve box (1) through the optical fiber support plate (3) by laser welding.
3. The device according to claim 1, Features: The third reflector (10) is connected to a piezoelectric ceramic ultrasonic motor (4), the piezoelectric ceramic ultrasonic motor (4) is connected to a motor fixing plate (5), and the motor fixing plate (5) is connected to the selection valve housing (1) by laser welding.
4. The device according to claim 1, Features: The first reflector (6) is connected to a first rectangular parallelepiped rod (7), and both ends of the first rectangular parallelepiped rod (7) are connected to a selection valve housing (1); the second reflector (8) is connected to a second rectangular parallelepiped rod (9), and both ends of the second rectangular parallelepiped rod (9) are connected to the selection valve housing (1); the third reflector (10) is connected to a rotating rod (11), and the rotating rod (11) is connected to a piezoelectric ceramic ultrasonic motor (4).
5. The device according to claim 1, Features: The beam expander (12) is fixed on a beam expander bracket (13), and the beam expander bracket (13) is connected to the selection valve box (1).
6. The device according to claim 1, Features: The first reflector (6), the second reflector (8) and the third reflector (10) are all square in shape, with their centroids located on the same vertical line, and the area of the reflective surface is more than 100 times the area of the laser spot; the first reflector (6), the second reflector (8) and the third reflector (10) are all made of high-purity ultraviolet fused quartz substrates and coated with ultra-high laser-induced damage threshold dielectric films, and can withstand high-energy pulses, with an incident angle of 0-45° and a reflectivity of more than 99%.
7. The device according to claim 1, Features: Low power lasers use beam quality M 2 The single-mode fiber laser with a power of 400-800W and a power of less than 1.2 is used. The high-power laser uses a fiber laser with a power of more than 4000W.
8. The device according to claim 4, Features: The rotating rod (11) is designed with an internal structure by using a lattice optimization method and is manufactured by using an additive manufacturing method.
9. A forming method of a laser optical path adjustment device for laser powder bed fusion additive manufacturing using any one of claims 1 to 8, comprising a large spot filling printing mode forming method and a large spot preheating mode forming method; The large spot filling printing mode forming method, The following steps are involved: S1. Connect a low-power laser fiber head (14) and a high-power laser fiber head (15) to the selector valve housing (1), and arrange the two laser fiber heads in parallel so that the low-power laser beam (24) and the high-power laser beam (23) remain parallel; the spot diameter formed by the high-power laser beam (23) after passing through the beam expander (12) and the galvanometer system is larger than the spot diameter formed by the low-power laser beam (24) after passing through the galvanometer system; S2. When printing the internal filling area, the high-power laser is turned on, the low-power laser is turned off, the piezoelectric ceramic ultrasonic motor (4) is started and the angle of the third reflector (10) is adjusted so that the expanded high-power laser beam (23) is reflected out of the dual laser selection valve and enters the galvanometer system, and then scans the filling line; S3. When printing the shape line area, the low-power laser is turned on, the high-power laser is turned off, the piezoelectric ceramic ultrasonic motor (4) is started and the angle of the third reflector (10) is adjusted so that the low-power laser beam (24) is reflected out of the dual laser selection valve and enters the galvanometer system, and then scans the contour line; S4. After the shape line area is printed, continue to use the low-power laser beam (24) to scan the joint between the internal filling area and the shape line area; The large spot preheating mode forming method comprises the following steps: S1. Connect a low-power laser fiber head (14) and a high-power laser fiber head (15) to the selector valve housing (1), and arrange the two laser fiber heads in parallel so that the low-power laser beam (24) and the high-power laser beam (23) remain parallel; the spot diameter formed by the high-power laser beam (23) after passing through the beam expander (12) and the galvanometer system is larger than the spot diameter formed by the low-power laser beam (24) after passing through the galvanometer system; S2. When printing hard-to-melt materials, the high-power laser is turned on, the low-power laser is turned off, the piezoelectric ceramic ultrasonic motor (4) is started and the angle of the third reflector (10) is adjusted so that the expanded high-power laser beam (23) is reflected out of the dual laser selection valve and enters the galvanometer system, and then the printing surface is preheated; S3. After the printing surface is preheated, the low-power laser is turned on, the high-power laser is turned off, the piezoelectric ceramic ultrasonic motor (4) is started and the angle of the third reflector (10) is adjusted so that the low-power laser beam (24) is reflected out of the dual laser selection valve and enters the galvanometer system, and then the part is printed; S4. Repeat steps S2 and S3 for each cross section of the printed part until the part is printed.
10. The printing method according to claim 9, Features: In the steps S2 and S3, the angle at which the piezoelectric ceramic ultrasonic motor (4) rotates the third reflector (10) is 90°.
Citation Information
Patent Citations
A dual-laser single-galvanometer printing system
CN218799127U
Double-beam selective laser melting additive manufacturing method
CN109622955A
Laser processing system
CN217122084U
Same-breadth multi-type laser additive and subtractive composite forming device
CN217122101U
Laser high-power converter using superposition of multiple lasers
KR1020180106654A