Method for repairing ganged brick outer wall of historical building

By evaluating and targeted repairing the damage degree of the exterior walls of clean water bricks in historical buildings, the problem of single traditional repair methods has been solved and better repair results have been achieved.

CN119083771APending Publication Date: 2024-12-06SHANGHAI BUILDING DECORATION ENG GRP CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411372311.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-29
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The clean water brick exterior walls of historical buildings are single, and they cannot effectively deal with damage of varying degrees, resulting in poor repair results.

Method used

By judging the damage degree of the clean water brick exterior wall, a corresponding repair plan is formulated, including pretreatment, damage degree assessment, and the selection of appropriate repair methods, such as opening treatment, cleaning treatment, enhancement treatment, repair and grout treatment, for Different repair steps are taken at different damage depths.

Benefits of technology

The repair effect is improved, and corresponding repair measures are taken for damage of varying degrees are ensured, the singleness of traditional repair methods is improved, and the repair effect is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119083771A_ABST
    Figure CN119083771A_ABST
Patent Text Reader

Abstract

The invention discloses a method for repairing a ganged brick outer wall of a historical building. The method for repairing the ganged brick outer wall of the historical building comprises the following steps that the ganged brick outer wall is pretreated; determining the damage degree of the ganged brick outer wall; selecting a corresponding repairing method according to the damage degree; and repairing the ganged brick outer wall based on the corresponding repairing method. According to the method for repairing the ganged brick outer wall of the historical building, the surface damage degree of the ganged brick outer wall is judged, the corresponding repairing method is selected according to the judgment result, the problem that a traditional repairing method is single is solved, and the repairing effect is good.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of historical building repair, and in particular to a method for repairing the exposed brick exterior wall of a historical building. Background Art

[0002] Historical buildings often have varying degrees of damage to their exterior walls due to their age. However, the development history of historical buildings is closely linked to the history and cultural value of the city. Therefore, historical buildings need to be repaired to allow these ancient buildings to glow with new vitality in the new era. The current repair methods are relatively single, and there are no corresponding repair methods for different types of damage, so the repair effect is poor. Summary of the invention

[0003] In view of this, the purpose of the present invention is to provide a method for repairing the exposed brick exterior wall of a historical building, to judge the degree of surface damage of the exposed brick exterior wall, and to select a corresponding repair method according to the judgment result, thereby changing the problem of the single traditional repair method and achieving a good repair effect.

[0004] The present invention provides a method for repairing the exterior wall of a historical building using exposed bricks, comprising the following steps:

[0005] Pre-treat the exposed brick exterior wall;

[0006] Determine the extent of damage to the exposed brick exterior wall;

[0007] Select the corresponding repair method according to the degree of damage;

[0008] The exposed brick exterior wall is repaired based on the corresponding repair method.

[0009] In one embodiment, the damage degree includes:

[0010] The damage depth is no more than 5 mm, the damage depth is greater than 5 mm and no more than 20 mm, the damage depth is greater than 20 mm and no more than 50 mm, and the damage depth is greater than 50 mm.

[0011] In one embodiment, when the damage depth is no more than 5 mm, the repair method further comprises:

[0012] Performing seam opening treatment on the exposed brick exterior wall;

[0013] Cleaning the exposed brick exterior wall;

[0014] Carry out local repairs on the cleaned exposed brick exterior wall;

[0015] The exposed brick exterior wall is subjected to grouting treatment.

[0016] In one embodiment, when the damage depth is greater than 5 mm and not greater than 20 mm, the repair method further comprises:

[0017] Performing seam opening treatment on the exposed brick exterior wall;

[0018] Cleaning the exposed brick exterior wall after the seam opening treatment;

[0019] Performing a reinforcement treatment on the cleaned brick body of the exposed brick exterior wall;

[0020] Repairing the brick surface of the exposed brick exterior wall;

[0021] The exposed brick exterior wall is subjected to grouting treatment.

[0022] In one embodiment, when the damage depth is greater than 20 mm and not greater than 50 mm, the repair method further comprises:

[0023] Performing seam opening treatment on the exposed brick exterior wall;

[0024] Cleaning the exposed brick exterior wall after the seam opening treatment;

[0025] Performing a reinforcement treatment on the cleaned brick body of the exposed brick exterior wall;

[0026] Inlaying bricks on the surface of the exposed brick exterior wall;

[0027] The exposed brick exterior wall is subjected to grouting treatment.

[0028] In one embodiment, when the damage depth is greater than 20 mm and not greater than 50 mm, the repair method further comprises:

[0029] Removing damaged bricks from the exposed brick exterior wall;

[0030] Inlaying the removed positions of the exposed brick exterior wall;

[0031] Partially repairing the exposed brick exterior wall;

[0032] The exposed brick exterior wall is subjected to grouting treatment.

[0033] In one embodiment, the repair method further comprises:

[0034] Determining whether the exposed brick exterior wall is alkali-prone;

[0035] In the case that efflorescence exists on the exposed brick exterior wall, the exposed brick exterior wall is subjected to a salt removal treatment.

[0036] In one embodiment, the pretreatment of the exposed brick exterior wall further comprises:

[0037] Removing the additional parts on the exposed brick exterior wall;

[0038] Removing the plaster surface of the surface of the exposed brick exterior wall;

[0039] The derivatives on the exterior wall of the clear brick are removed.

[0040] The method for repairing the exposed brick exterior wall of a historical building provided by the present invention determines the degree of surface damage of the exposed brick exterior wall and selects a corresponding repair method according to the judgment result, thereby changing the problem of the single traditional repair method and achieving a good repair effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.

[0042] Figure 1 A schematic diagram of the process of the method for repairing the exposed brick exterior wall of a historical building provided by the present invention. DETAILED DESCRIPTION

[0043] The specific embodiments of the present invention will be described in detail below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the description of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0044] In the description of the present invention, unless otherwise clearly specified and limited, the terms "set", "install", "connection" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms can be understood according to specific circumstances.

[0045] The directions or positional relationships indicated by terms such as “upper”, “lower”, “left”, “right”, “front”, “back”, “top”, “bottom”, “inside” and “outside” are based on the directions or positional relationships shown in the accompanying drawings, or are the directions or positional relationships in which the inventive product is usually placed when used. They are only for the convenience of description and simplified description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present invention.

[0046] The terms "first", "second", "third" and the like are merely used to distinguish elements of similar nature, and do not indicate or imply relative importance or a particular order.

[0047] The terms "comprises," "comprising," or any other variations thereof, are intended to cover a non-exclusive inclusion of the elements listed and may also include additional elements not expressly listed.

[0048] See also Figure 1 The method for repairing the exterior wall of a historical building with exposed bricks provided by the present invention comprises the following steps:

[0049] S1, pre-treat the exposed brick exterior wall.

[0050] It is understood that the pre-processing may further include:

[0051] Remove the additional parts on the exposed brick exterior wall.

[0052] It can be known that the exposed part of the additional parts can be removed by "cutting"; the wooden wedges, bolts and other debris left in the wall can be pulled out with the help of tools such as "pliers or drill bits"

[0053] Remove the plaster surface on the surface of the exposed brick exterior wall.

[0054] It is understandable that when removing various types of plaster layers added to the surface of the exposed brick exterior wall, they should be removed "manually" and carefully chiseled off one by one. When manually chiseling, first use a flat chisel to slowly peel off the junction of the "plaster layer" and the "exposed brick exterior wall"; after chiseling out the working surface, use a flat chisel to manually chisel vertically downward along the junction of the "plaster layer" and the "exposed brick exterior wall" to minimize damage to the original brick surface and ensure the integrity of the "exposed wall" brick surface to the greatest extent.

[0055] Remove derivatives on the exterior wall of exposed bricks.

[0056] It is understandable that 1) for large-scale overall removal of creeper plants, first cut off the parts connected to the wall, and after all connections are cleared, gently remove the creepers clinging to the wall from top to bottom. After a large area of ​​plants on the wall is cleared, local plants are cleaned separately. When the roots of plants grow into the inside of the brick wall, they are chiseled out and removed. The chiseled area is controlled and removed, and the surrounding walls are covered and protected. The wall is slowly chiseled open to remove the roots of plants growing inside the wall. Minimize damage to the wall during chiseling, and spray the cleaned wall with plant decay agents to inhibit its growth inside the wall.

[0057] 2) To remove moss from the wall, use a spatula to gently scrape away the moss on the surface of the brick wall. Stop construction when the original brick wall is scraped away. Use a special remover to treat the traces of moss left on the wall. When general cleaning cannot meet the expected requirements, use biological and physical methods (active decontamination enzymes, carbon silicon brushes) combined with water flushing to clean.

[0058] 3) Finally, anti-algae agent is used for anti-algae protection treatment. Especially in the parts where water is easily retained and in the damp parts all year round, anti-algae treatment is needed. This kind of material has the dual functions of weathering prevention and inhibiting the growth of moss. After use, it can avoid the appearance damage and corrosion caused by the growth of microorganisms such as moss.

[0059] S2, determine the extent of damage to the exposed brick exterior wall.

[0060] It is understandable that the degree of damage can be obtained through some image processing algorithms;

[0061] The damage degree judgment includes damage depth no more than 5 mm, damage depth greater than 5 mm and no more than 20 mm, damage depth greater than 20 mm and no more than 50 mm, and damage depth greater than 50 mm.

[0062] S3, select the corresponding repair method according to the degree of damage;

[0063] S4, repair the exposed brick exterior wall based on the corresponding repair method.

[0064] (i) For damage depth not exceeding 5 mm, the repair method further includes:

[0065] Make seams on the exposed brick exterior wall.

[0066] It is understandable that some intact brick joints can be retained, while some damaged ones should be removed. When removing, a special flat steel chisel should be used to lightly chisel on both sides of the brick joint. After it is loosened, use a removal tool to chisel along the brick joint direction. The depth should not be less than 8mm or chisel to the original masonry mortar layer. When removing damaged brick joints, the bricks must not be damaged.

[0067] Clean the exposed brick exterior wall after the seam treatment.

[0068] It is understandable that the cleaning of the exterior wall should not have an adverse effect on the building, and should not damage the surface of the protected part and the adjacent area. The wall surface after cleaning should not be yellowed, discolored, or loose, and ensure that the wall surface does not leak. According to the different characteristics of the exterior wall finish, the cause of the dirt, the degree of contamination, and the protection requirements of the historical building, the following methods are generally adopted for cleaning.

[0069] Cleaning methods may include:

[0070] 1) Physical cleaning method: Use physical methods such as medium and low pressure water washing to remove surface dirt.

[0071] Low-pressure water spraying, gentle water flow, easy to control, suitable for removing non-sticky dirt on the surface;

[0072] Medium-pressure water spraying is highly efficient and inexpensive, and is suitable for removing sticky dirt such as glue and hard scale on the surface; however, the strong pressure can easily damage the edges and corners of bricks and stones, and is not suitable for fancy components.

[0073] 2) Chemical cleaning method: that is, chemical reactions occur between chemical drugs and surface diseases to eliminate the diseases.

[0074] Chemical cleaning is the most effective and easy-to-use method for cleaning exterior walls. It is also the most commonly used method, but it is also the most difficult method to control and master. If you are not careful, it will cause permanent damage to the finish. The specific method of chemical cleaning must be determined through on-site tests. It is recommended to use neutral detergents for cleaning; check whether it has no corrosive or polluting effects on the wall; after cleaning, the wall surface should be tested for the residual amount of detergent, which meets the relevant standards.

[0075] Clean with slightly acidic detergent, suitable for local alkaline pollution;

[0076] Clean with slightly alkaline detergent, suitable for local acidic pollution;

[0077] Clean with neutral detergent, suitable for general pollution;

[0078] Solvent-based chemical cleaning, using chemicals such as alcohol, toluene, xylene, acetone, nitro solvents, paint removers, etc., is suitable for grease and oil stain pollution. Oil removal agents are more effective than general detergents, but they are harmful and toxic gases evaporate, so you should pay attention to protection. It is not suitable for large-scale use in engineering, but can be used in small areas in small quantities.

[0079] 3) Cleaning of light pollution.

[0080] For light pollution such as floating dust, use the "carbon silicon nylon brush + clean water flushing" method to clean.

[0081] 4) Cleaning of stubborn stains.

[0082] For rainwater dripping and stubborn dirt on the wall such as the top brick, brick arch, brick line, and the lower end of the eaves, special reagents are used to dissolve. The duration of the application of the dressing agent on the dirt can be determined according to the stubbornness of the dirt. Generally, 6 hours is the standard, and the time can be increased or decreased, or the content of the cleaning agent can be increased or decreased, and 5% of the surfactant can be added. After cleaning, rinse with clean water.

[0083] The above-mentioned pasting method is to use adsorbent materials such as fibers, powders or colloids to wet the cleaning agent and apply it on the surface. In order to retain moisture and prolong the action time, it is usually necessary to cover it with a plastic film.

[0084] 5) Cleaning method of steam cleaning machine.

[0085] Graffiti is mainly advertisements and phone numbers. Usually, the main material of graffiti is acrylic paint, which has strong permeability and adhesion. When cleaning, apply the detergent on the graffiti, spread it evenly and let it work with the graffiti for about 20 minutes. The detergent must be applied evenly and repeatedly, and finally use a small steam machine to rinse away the dissolved graffiti dirt and detergent. Since the viscosity of the detergent is very low, it can prevent the detergent and the dissolved graffiti dirt from being reabsorbed by the material itself. For graffiti with permeability, first remove the graffiti on the surface, then use a high-temperature steam cleaner to clean it, then apply the detergent on the graffiti surface using the application method, and finally use a high-temperature steam machine to clean it until the surface graffiti is cleaned.

[0086] 6) Coating cleaning.

[0087] Generally, a jet cleaning machine is used. The specific pressure value is adjusted according to the actual situation on site, and the swirl washing and peeling is carried out from top to bottom. The coating is softened and powdered by external force, and finally separated from the outer wall of the building. The unpowdered coating can be cleaned by a hard bristle brush and a combination of water flushing.

[0088] First test a small area, then construct a large area;

[0089] If there are areas that cannot be cleaned, use a paint stripper to remove the paint from the exterior wall coating;

[0090] Clean heavily contaminated areas multiple times.

[0091] 7) Cleaning of paint pollution.

[0092] Because paint has strong adhesion, toughness after film formation, strong weather resistance, acid and alkali resistance, it is very difficult to clean, especially after penetrating into the interior of the dry wall. Use a high-efficiency paint remover mixed with a dressing and apply it on the surface of the dry wall to promote the emulsification of the active ingredients in the paint remover with the paint film. Use a high-temperature steam cleaner with cleaning tools for cleaning, and finally clean with clean water.

[0093] 8) Cleaning of rust stains.

[0094] The treatment method for rust stains is mainly to use rust removers, which mainly rely on reducing and stabilizing iron ions. The basic steps are:

[0095] Reduce ferric iron ions to ferrous iron ions: Since rust mostly exists in the solid state of ferric iron ions, it is reduced to soluble ferrous iron ions, which are basically colorless.

[0096] Stabilize divalent iron ions: Use stabilizers to prevent the reverse reaction and reduce the possibility of rusting out of residues in the micropores of the surface in the future;

[0097] Absorb divalent iron ions: Use covering method or other cleaning measures to remove the reduced iron ions and residual liquid of the medicine from the surface of the finish.

[0098] Use a brush to evenly apply the rust remover to the rust-contaminated area to allow it to fully react. For areas with severe rust, cover them with clean dressings and rust remover to extend the reaction time. If necessary, perform two or more treatments. After the surface is treated, wash it with clean water and apply rust inhibitor to prevent the recurrence of rust spots and provide long-term protection.

[0099] Carry out local repairs on the cleaned exposed brick exterior wall.

[0100] It is understood that local repair may further include:

[0101] Lime-based cementitious material or brick powder repair: Mix the lime-based cementitious material or brick powder into a semi-dry paste and apply it to the damaged brick surface. After "repairing the brick edges and corners with lime-based cementitious material or brick powder", use a silicon brush to evenly polish and improve the repair marks to make it consistent with the surrounding plain brick exterior wall surface.

[0102] Brick repair: Bricks are cut from old bricks removed from the interior, and the surface layer is used. Brick bonding materials are lime-based bonding materials, which are bonded to the local damaged areas.

[0103] The exposed brick exterior wall is grouted.

[0104] It is understandable that when grouting the concave flat joints or ingot joints, after the wall surface is dry, the finished lime-based grouting agent is used for grouting. The color of the grouting agent should be consistent with the original wall brick joints, and the brick joints should be filled evenly, fully and densely. Grouting is done from top to bottom, first horizontal joints, then vertical joints. The wall joints should be horizontal and vertical, the cross joints should be overlapped and flat, compacted and polished, and no omissions should be allowed. The depth of the concave flat joints is 3 to 4 mm from the brick mouth, and the depth rises and falls along the weathered old bricks, highlighting the three-dimensional effect of the bricks. The ingot joints protrude 3 to 4 mm, and the arch surface is flush with the brick surface. The surface joints must be grouted with a customized grouting mold. Ensure that the grouting is smooth, the grouting width, and the concave and convex are consistent.

[0105] (ii) Where the damage depth is greater than 5 mm and not greater than 20 mm, the repair method further includes:

[0106] Open the seams on the exposed brick exterior wall;

[0107] Clean the exposed brick exterior wall after the seam treatment.

[0108] It is to be understood that the slit opening process and cleaning process refer to the method described above.

[0109] The cleaned exposed brick exterior wall is reinforced.

[0110] It is understandable that the enhancement treatment can be achieved by applying additional paint on the brick surface of the exterior wall made of ethyl silicate bonded plain bricks.

[0111] Repair the brick surface of the exposed brick exterior wall.

[0112] It can be known that after the above cleaning, the interface agent is applied on the brick surface, and the alkali-resistant mortar is used for leveling, leaving a thickness of at least 3 to 5 mm of lime-based cementitious material or brick powder. After the surface is cured, it is repaired with special lime-based cementitious material or brick powder.

[0113] The exposed brick exterior wall is grouted.

[0114] It is understandable that the grouting method also adopts the above-mentioned record.

[0115] (III) Where the damage depth is greater than 20 mm and not greater than 50 mm, the repair method further includes:

[0116] Open the seams on the exposed brick exterior wall;

[0117] Clean the exposed brick exterior wall after the seam treatment;

[0118] The cleaned exposed brick exterior wall is reinforced.

[0119] It can be understood that the slit processing, cleaning processing and strengthening processing can all refer to the above description.

[0120] Bricks are inlaid on the surface of the exposed brick exterior wall.

[0121] It is understandable that old bricks of the same specifications are used for brick removal and inlay repair. Manual chiseling requires replacing the mortar joints around the bricks; then remove the bricks with serious damage on the brick surface; remove the dirt and debris in the brick holes and scrub them clean; choose lime-based masonry mortar and use a trowel to build the mortar belly into the wet bricks. The whole brick removed during the cleaning process must be inlaid with a whole brick, and the inlaid whole brick must match and coordinate with the surrounding bricks.

[0122] The exposed brick exterior wall is grouted.

[0123] It can be known that the method for grouting can also refer to the above method.

[0124] S5, judging whether the exposed brick exterior wall is alkali-eluting;

[0125] In case of efflorescence on the exposed brick exterior wall, the exposed brick exterior wall shall be treated for salt removal.

[0126] It is understandable that the exposed brick exterior walls are most susceptible to different degrees of water-soluble salt damage, resulting in alkali reversion in the wall, which not only affects the appearance, but also causes the material to disintegrate and pulverize during the crystallization-dissolution process. Therefore, in addition to blocking the water source from invading the wall, the salt in the wall should be removed as much as possible. The water-soluble salts in the clay bricks of the exposed brick exterior walls are mainly concentrated in the surface area less than 20mm. At the same time, since the temperature, humidity, etc. change most dramatically within the surface area, the surface salt is also the most dangerous to historical materials, and it is necessary to take measures to remove these salts.

[0127] Before the salt removal treatment, the moisture content of the wall should be reduced. The moisture content of the wall can be controlled by reducing the cover on the surface of the historical building, maintaining natural ventilation, taking rain shelter measures during the salt removal treatment, and promptly completing the repair of the "moisture-proof layer" of the historical building.

[0128] There are many ways to remove salt from exposed brick exterior walls, generally using replacement method, electrochemical method, application method and alkali removal agent cleaning method for salt removal.

[0129] The replacement method is to remove the bricks and seams that are seriously contaminated by salt and replace them with new materials with low salt content. The replacement method not only has the problem of excessive intervention in historical buildings and damage to the original walls, but also the problem of compatibility between the replacement materials and the original historical materials and the introduction of new salt, so this method is rarely used in the repair of historical buildings.

[0130] The electrochemical method uses the principle that the anions and cations of water-soluble salts migrate to the anode and cathode respectively under the action of electric current to remove salt. The advantage of this method is that it has little interference with the base layer, but the disadvantage is that the salt removal effect is limited, the construction period is long, and the construction must be organized by a very professional company. Therefore, this method is rarely chosen for the salt removal of the clear water walls of historical buildings.

[0131] The non-destructive salt removal by application method is a method that uses the capillary action of water-soluble salt ions to concentrate the salt in the base layer into the removable surface application material, thereby reducing the salt in the base layer. This method is more suitable for salt removal from the clear water walls of historical buildings. Suitable materials are:

[0132] Salt-removal mortar: a slurry material that can be used directly on site and is made of a variety of fibers, clay and other materials.

[0133] Sacrificial mortar: low-strength mortar with lime as binder. When salt accumulates in this layer, it is removed to achieve the effect of removing salt. Compared with salt-removing mortar, it takes longer.

[0134] The principles of the two are basically the same, but the sacrificial mortar takes a longer time to react, generally 6 to 12 months. The salt-removing mortar has the advantages of short construction period and convenient construction.

[0135] Alkali-return cleaning method: Before construction, clean the dust and dirt on the wall. After the wall is dry, spray the alkali-return cleaning agent 2 to 3 times to ensure that the wall will not return to alkali within a certain period of time. The use of alkali-return cleaning agent can form a protective film on the wall surface to completely block the entry of moisture and carbon dioxide, so as to ensure that the wall will not return to alkali again within a certain period of time.

[0136] From the above description, it can be known that the method for repairing the exposed brick exterior wall of a historical building provided by the present invention judges the degree of surface damage of the exposed brick exterior wall and selects a corresponding repair method according to the judgment result, which changes the problem of the single traditional repair method and has a good repair effect.

[0137] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the attached claims.

Claims

1. A method for repairing the exterior wall of a historical building with exposed bricks. It is characterized in that The steps include: Pre-treat the exposed brick exterior wall; Determine the extent of damage to the exposed brick exterior wall; Select the corresponding repair method according to the degree of damage; The exposed brick exterior wall is repaired based on the corresponding repair method.

2. The method for repairing the exterior wall of a historical building using exposed bricks as claimed in claim 1, It is characterized in that The extent of the damage includes: The damage depth is no more than 5 mm, the damage depth is greater than 5 mm and no more than 20 mm, the damage depth is greater than 20 mm and no more than 50 mm, and the damage depth is greater than 50 mm.

3. The method for repairing the exterior wall of a historic building using exposed bricks as claimed in claim 2, It is characterized in that When the damage depth is no more than 5 mm, the repair method further comprises: Performing seam opening treatment on the exposed brick exterior wall; Cleaning the exposed brick exterior wall; Carry out local repairs on the cleaned exposed brick exterior wall; The exposed brick exterior wall is subjected to grouting treatment.

4. The method for repairing the exterior wall of a historic building using exposed bricks as claimed in claim 2, It is characterized in that When the damage depth is greater than 5 mm and not greater than 20 mm, the repair method further comprises: Performing seam opening treatment on the exposed brick exterior wall; Cleaning the exposed brick exterior wall after the seam opening treatment; Performing a reinforcement treatment on the cleaned brick body of the exposed brick exterior wall; Repairing the brick surface of the exposed brick exterior wall; The exposed brick exterior wall is subjected to grouting treatment.

5. The method for repairing the exterior wall of a historic building using exposed bricks as claimed in claim 2, It is characterized in that When the damage depth is greater than 20 mm and not greater than 50 mm, the repair method further comprises: Performing seam opening treatment on the exposed brick exterior wall; Cleaning the exposed brick exterior wall after the seam opening treatment; Performing a reinforcement treatment on the cleaned brick body of the exposed brick exterior wall; Inlaying bricks on the surface of the exposed brick exterior wall; The exposed brick exterior wall is subjected to grouting treatment.

6. The method for repairing the exterior wall of a historic building using exposed bricks as claimed in claim 2, It is characterized in that When the damage depth is greater than 20 mm and not greater than 50 mm, the repair method further comprises: Removing damaged bricks from the exposed brick exterior wall; Inlaying the removed positions of the exposed brick exterior wall; Partially repairing the exposed brick exterior wall; The exposed brick exterior wall is subjected to grouting treatment.

7. The method for repairing the exterior wall of a historic building made of exposed bricks according to any one of claims 3 to 6, It is characterized in that The repair method also includes: Determining whether the exposed brick exterior wall is alkali-prone; In the case that efflorescence exists on the exposed brick exterior wall, the exposed brick exterior wall is subjected to a salt removal treatment.

8. The method for repairing the exterior wall of a historic building using exposed bricks as claimed in claim 1, It is characterized in that The pretreatment of the exposed brick exterior wall further comprises: Removing the additional parts on the exposed brick exterior wall; Removing the plaster surface of the surface of the exposed brick exterior wall; The derivatives on the exterior wall of the clear brick are removed.

Citation Information

Patent Citations

  • Historical building clean water red brick wall renovation technique

    CN101429816A

  • Historical building plain brick wall repair construction method

    CN109653529A

  • Concrete brick repairing process

    CN117822926A