Device and method for producing iron oxide powder through spray roasting
Through spray roasting method and crushing and grading treatment technology, the problem of insufficient particle size distribution and specific surface area of iron oxide powder is solved, and efficient recovery of iron oxide powder is achieved, product quality and production efficiency are improved, and there are significant economic and environmental benefits.
Patent Information
- Application Number
- CN202411296648.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-14
- Publication Date
- 2024-12-06
AI Technical Summary
The iron oxide powder produced by spray roasting has problems such as wide distribution of particle size and insufficient specific surface area, which leads to limited product quality. The traditional method increases the specific surface area by reducing production concentration but at the expense of production efficiency and increasing energy consumption, and is not economical. .
A device including a production furnace, crushing mechanism and grading mechanism was designed to generate iron oxide powder by spray roasting, and use high-speed airflow crushing and grading to improve the specific surface area and particle size distribution of iron oxide powder, so as to achieve the improvement of product quality. .
It realizes efficient recycling of iron oxide powder from waste acid liquid, maintains low energy consumption, improves the specific surface area and activity of the product, has significant economic and environmental benefits, and the device is reasonable in design, simple in operation, and is suitable for industrial production.
Smart Images

Figure CN119084962A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of iron oxide powder production, and in particular to a device and method for producing iron oxide powder by spray roasting. Background Art
[0002] In key industries such as metallurgy, chlor-alkali and new energy material manufacturing, acidic substances such as hydrochloric acid are widely used in the leaching treatment of minerals and the pickling process of steel. These processes not only improve the processing performance of materials, but are also accompanied by the generation of a large amount of acid or waste acid containing ferrous ions. If these ferrous acids are not properly treated, they will not only cause waste of resources, but also pose a serious threat to the environment. Through the spray roasting process, acid or waste acid containing ferrous ions can be converted into oxide powder with high added value. Due to its excellent physical and chemical properties, this oxide powder has shown broad application prospects in the new energy materials, magnetic materials and alkaline materials manufacturing industries.
[0003] In the prior art, the iron oxide powder produced by the spray roasting method has the problems of wide particle size distribution and insufficient specific surface area, which limits the product quality. The traditional method of increasing the specific surface area by reducing the production concentration can improve the specific surface area of the product, but it sacrifices production efficiency and increases energy consumption, which is not economical in industrial applications. Therefore, a method and device for improving the quality of iron oxide powder continuously produced by the spray roasting method is urgently needed to solve the above problems. Summary of the invention
[0004] Therefore, in order to solve the above-mentioned problems, the present invention provides a device and method for producing iron oxide powder by spray roasting.
[0005] To achieve the above purpose, the technical solution provided by the present invention is as follows:
[0006] A device for producing iron oxide powder by spray roasting, comprising a production furnace, a first silo, a crushing mechanism, a grading mechanism and a second silo; the production furnace is used to receive waste acid liquid and spray roast it to convert it into iron oxide powder; the first silo is used to receive and buffer the iron oxide powder output by the production furnace; the crushing mechanism can generate a high-speed airflow to crush the iron oxide powder from the first silo; the grading mechanism is used to grade the crushed iron oxide powder according to the particle size, so that the iron oxide powder that meets the set grading standard enters the second silo, and the iron oxide powder that does not meet the set grading standard is returned to the crushing mechanism; the second silo is used to store the classified iron oxide powder.
[0007] Optionally, the crushing mechanism includes a crushing bin and a high-pressure airflow device, and the high-pressure airflow device includes a compressor, an air storage tank, a deoiler, a freeze dryer, a deoiler, a filter and an airflow nozzle connected in sequence; the airflow nozzle is connected to the crushing bin.
[0008] Optionally, the production furnace is equipped with a spray mechanism and a burner mechanism, the spray mechanism can evenly spray the waste acid liquid into the production furnace; the burner mechanism is used to provide heat energy to the production furnace.
[0009] Optionally, an impact gun is provided at the bottom of the first silo and / or the second silo.
[0010] Optionally, a dust removal mechanism is provided on the top of the second silo.
[0011] Optionally, a baler for baling iron oxide powder is provided below the discharge port of the second silo.
[0012] A method for producing iron oxide powder by spray roasting, using the above-mentioned device, comprises the following steps:
[0013] S1, spraying the waste acid liquid into a production furnace for roasting to generate iron oxide powder;
[0014] S2, the iron oxide powder is transported to the pulverizing mechanism after being buffered in the first silo and pulverized by high-speed airflow;
[0015] S3, the crushed iron oxide powder is classified in the grading mechanism, and the iron oxide powder that meets the classification requirement set value enters the second silo; the iron oxide powder that does not meet the classification requirement set value is returned to the crushing mechanism for crushing;
[0016] S4, packaging and storing the iron oxide powder at the outlet of the second silo.
[0017] Optionally, in S2, the particle size (D50) of the iron powder entering the pulverizing mechanism is in the range of 25 to 50 μm.
[0018] Optionally, in S3, the particle size (D50) of the iron oxide powder entering the second silo is in the range of 1 to 10 μm.
[0019] Optionally, in S3, the specific surface area of the iron oxide powder entering the second silo is not less than 3.0m 2 / g.
[0020] The technical solution provided by the present invention has the following beneficial effects: waste acid liquid is used for high-temperature roasting to produce iron oxide powder, thereby maintaining low energy consumption and realizing efficient recovery of valuable substances from waste acid liquid, which has significant economic and environmental benefits; after being processed by a crushing mechanism and a grading mechanism, the specific surface area and activity of the product are increased, and the product quality is improved; and the whole set of equipment is reasonably designed, easy to operate, easy to realize industrial production, and has good prospects for promotion and application. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a schematic diagram of the overall structure of this embodiment.
[0022] Explanation of the accompanying drawings: 1. production furnace; 2. burner mechanism; 3. spray mechanism; 4. crusher; 5. rotary valve; 6. shut-off valve; 7. first silo; 8. impact gun; 9. compressor; 10. gas storage tank; 11. degreaser; 12. freeze dryer; 13. filter; 14. air flow nozzle; 15. crushing mechanism; 16. grading mechanism; 17. crushing bin; 18. second silo; 19. dust removal mechanism; 20. conveying fan; 21. baler. DETAILED DESCRIPTION
[0023] To further illustrate the various embodiments, the present invention provides drawings. These drawings are part of the disclosure of the present invention, which are mainly used to illustrate the embodiments and can be used in conjunction with the relevant descriptions in the specification to explain the operating principles of the embodiments. With reference to these contents, a person of ordinary skill in the art should be able to understand other possible implementations and advantages of the present invention. The components in the figures are not drawn to scale, and similar component symbols are generally used to represent similar components.
[0024] In the description of the present invention, unless otherwise clearly stipulated and limited, the terms "connection" and "connected" should be interpreted in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0025] In the description of the present invention, terms such as "up", "down", "left", "right", "front", "back", etc., and the orientation or position relationship are based on the orientation or position relationship shown in the drawings, and are only for the convenience of description and simplification of operation, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention.
[0026] In addition, in the description of the present invention, the terms "first" and "second" are only used to distinguish in the description, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. In addition, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features.
[0027] The present invention will now be further described with reference to the accompanying drawings and specific implementation methods.
[0028] Reference Figure 1The present embodiment provides a device for producing iron oxide powder by spray roasting, the device comprising a production furnace 1, a first silo 7, a crushing mechanism 15, a grading mechanism 16 and a second silo 18; the production furnace 1 is used to receive waste acid liquid and spray roast it to convert it into iron oxide powder; the first silo 7 is used to receive and buffer the iron oxide powder produced by the production furnace 1; the crushing mechanism 15 can generate a high-speed airflow to crush the iron oxide powder from the first silo 7; the grading mechanism 16 is connected to the end of the crushing mechanism 15, and is used to grade the crushed iron oxide powder according to the particle size, so that the iron oxide powder that meets the classification setting standard enters the second silo 18, and the iron oxide powder that does not meet the classification setting standard returns to the crushing mechanism 15; the second silo 18 is used to store the classified iron oxide powder.
[0029] Specifically, the production furnace 1 is equipped with a spray mechanism 3 and a burner mechanism 2. The spray mechanism 3 can spray the waste acid liquid evenly into the production furnace 1; the burner mechanism 2 is used to provide heat energy to the production furnace 1, and gas and combustion-supporting air are introduced into the production furnace 1 through the burner mechanism 2. After ignition, a large amount of heat energy is generated to roast the waste acid liquid spray. A flow guide device can be set in the production furnace 1 so that the iron oxide powder can be output from the outlet of the production furnace 1. A crusher 4 is also arranged at the bottom of the production furnace 1, which is used to preliminarily crush the large pieces of powder generated in the furnace to ensure that the powder is not blocked at the discharge port and is smoothly transported to the first silo 7. A rotary valve 5 and a cut-off valve 6 are installed in sequence between the discharge port of the production furnace 1 and the feed port of the first silo 7 to facilitate the control of the transportation of the powder.
[0030] The first silo 7 receives and buffers the iron oxide powder produced by the production furnace 1. The bottom of the first silo 7 is an inverted cone structure, and impact guns 8 are arranged at intervals at the bottom to ensure that the iron oxide powder can be smoothly transported out from the discharge port at the bottom of the first silo 7. A rotary valve 5 and a cut-off valve 6 are installed in sequence between the discharge port of the first silo 7 and the feed port of the crushing mechanism 15 to facilitate the control of the transportation of the powder and ensure that the material enters the next link smoothly.
[0031] The pulverizing mechanism 15 includes a pulverizing bin 17 and a high-pressure airflow device, wherein the high-pressure airflow device includes a compressor 9, an air tank 10, a deoiler 11, a freeze dryer 12, a deoiler 11, a filter 13 and an airflow nozzle 14 connected in sequence; the airflow nozzle 14 is connected to the pulverizing bin 17. The bottom of the pulverizing bin 17 is an inverted cone structure, and the airflow nozzle 14 is arranged inside the pulverizing bin 17 along the interval. The iron oxide powder is fully and efficiently pulverized by high-pressure airflow to increase the specific surface area of the iron oxide powder. The pressure range of the high-pressure airflow is 0.6 to 1.0 MPa. Among them, the particle size (D50) of the iron oxide powder entering from the feed port of the pulverizing bin 17 ranges from 25 to 50 μm.
[0032] The grading mechanism 16 is connected to the end of the crushing bin 17 to classify the crushed iron oxide powder according to the particle size to ensure that the powder particles meet the subsequent process requirements. The iron oxide powder that meets the grading setting standard enters the second silo 18, and the iron oxide powder that does not meet the grading setting standard returns to the crushing mechanism 15 for further crushing. In this embodiment, the grading particle size of the grading mechanism 16 is 5 to 15 μm to ensure the uniformity and accuracy of the particle size distribution. After being processed by the grading mechanism 16, the particle size (D50) of the iron oxide powder entering the second silo 18 is in the range of 1 to 10 μm, and the powder specific surface area BET ≥ 3.0m 2 That is, the smaller particles enter the second silo 18, and the larger particles stay in the pulverizing mechanism 15 and continue to be pulverized.
[0033] The bottom of the second silo 18 is an inverted cone structure, and impact guns 8 are arranged at intervals at its bottom to ensure that the iron oxide powder can be smoothly transported out from the discharge port at the bottom of the second silo 18. In addition, the discharge port of the second silo 18 is connected and installed with a shut-off valve 6, a rotary valve 5 and a baler 21 in sequence, and the iron oxide powder is packaged and stored in time through the baler 21. In addition, a dust removal mechanism 19 is arranged on the top of the second silo 18. The dust removal mechanism 19 can be a pulse dust collector, an electrostatic dust collector or a plastic sintered plate dust collector, which is used to efficiently remove dust from the exhaust gas, reduce environmental pollution and improve product purity. The dust removal mechanism 19 is also connected to a conveying fan 20 to ensure the dust removal effect. In this embodiment, the dust removal mechanism 19 adopts a pulse dust collector.
[0034] The production workflow of the equipment is as follows:
[0035] Start the production furnace 1, and spray the waste acid liquid evenly into the furnace through the spray mechanism 3, and control the flow rate of the waste acid liquid at 50 liters / hour. Start the burner mechanism 2 to provide the necessary heat energy, adjust the temperature in the furnace to 800°C to adapt to the high-temperature hydrolysis reaction of the waste acid liquid, and maintain the temperature in the furnace stable to ensure that the waste acid liquid is fully roasted. The iron oxide powder generated during the roasting process is collected by the guide device in the furnace and transported to the first silo 7.
[0036] In the first silo 7, the impact gun 8 assists in feeding and controls the flow of iron oxide powder to ensure that the material enters the crushing mechanism 15 smoothly. The high-pressure airflow device is started, and the output pressure of the compressor 9 is set to 0.8Mpa to generate a high-speed jet. The iron oxide powder is impacted by the high-speed airflow in the crushing bin 17 to achieve crushing, and the pressure of the crushing bin 17 is maintained at 0.65Mpa. The crushed iron oxide powder is transported to the grading mechanism 16 by the fan, and the speed of the grading wheel of the grading mechanism 16 is set to 2000 rpm to ensure that the powder with a particle size (D50) ranging from 1 to 10μm is classified.
[0037] The classified iron oxide powder is sent to the second silo 18 through the conveying system, and the pulse dust collector above the silo is started to remove dust from the tail gas. The baler 21 below the silo is started to automatically pack the iron oxide powder.
[0038] The crushed iron oxide powder was sampled and the particle size distribution was tested by a laser particle size analyzer to ensure that the (D50) requirement of 1 to 10 μm was met. The specific surface area of the iron oxide powder was measured by a BET specific surface area analyzer to ensure that it was not less than 3.0 m 2 / g.
[0039] This embodiment also provides a method for producing iron oxide powder by spray roasting, using the above-mentioned device, comprising the following steps:
[0040] S1, spraying the waste acid liquid into the production furnace 1 for roasting to generate iron oxide powder;
[0041] S2, the iron oxide powder is transported to the pulverizing mechanism 15 after being buffered in the first silo 7 and pulverized by the air high-speed airflow;
[0042] S3, the crushed iron oxide powder is classified in the classification mechanism 16, and the iron oxide powder that meets the classification requirement set value enters the second silo 18; the iron oxide powder that does not meet the classification requirement set value returns to the crushing mechanism 15 for crushing;
[0043] S4, packaging and storing the iron oxide powder at the outlet of the second silo 18.
[0044] Specifically, in S2, the particle size (D50) of the iron powder entering the pulverizing mechanism 15 is in the range of 25 to 50 μm. It should be noted that the particle size (D50) refers to the particle size corresponding to when the cumulative particle size distribution percentage of a sample reaches 50%. Its physical meaning is that particles with a particle size larger than it account for 50%, and particles with a particle size smaller than it also account for 50%. D50 is also called the median diameter or median particle size.
[0045] Furthermore, in S3, after the classification process, the particle size (D50) of the iron oxide powder entering the second silo 18 is in the range of 1 to 10 μm, that is, the smaller particles enter the second silo 18, and the larger particles remain in the pulverizing mechanism 15 for further pulverization. The specific surface area of the iron oxide powder entering the second silo 18 is not less than 3.0 m 2 / g.
[0046] This method utilizes waste acid liquid for high-temperature roasting to produce iron oxide powder, maintains low energy consumption, realizes efficient recovery of valuable substances from waste acid liquid, and has significant economic and environmental benefits; and then undergoes processing by a crushing mechanism 15 and a grading mechanism 16 to increase the specific surface area and activity of the product, thereby improving product quality.
[0047] Although the present invention has been specifically shown and described in conjunction with the preferred embodiments, it should be understood by those skilled in the art that various changes may be made to the present invention in form and details without departing from the spirit and scope of the present invention as defined by the appended claims, all of which are within the scope of protection of the present invention.
Claims
1. A device for producing iron oxide powder by spray roasting, Features: It includes a production furnace, a first silo, a crushing mechanism, a grading mechanism and a second silo; the production furnace is used to receive waste acid liquid and spray-roast it to convert it into iron oxide powder; the first silo is used to receive and buffer the iron oxide powder produced by the production furnace; the crushing mechanism can generate a high-speed airflow to crush the iron oxide powder from the first silo; the grading mechanism is used to grade the crushed iron oxide powder according to the particle size, so that the iron oxide powder that meets the grading set standard enters the second silo, and the iron oxide powder that does not meet the grading set standard is returned to the crushing mechanism; the second silo is used to store the classified iron oxide powder.
2. The device for producing iron oxide powder by spray roasting according to claim 1, Features: The pulverizing mechanism includes a pulverizing bin and a high-pressure airflow device, wherein the high-pressure airflow device includes a compressor, an air storage tank, a deoiler, a freeze dryer, a deoiler, a filter and an airflow nozzle which are connected in sequence; the airflow nozzle is connected to the pulverizing bin.
3. The device for producing iron oxide powder by spray roasting according to claim 1, Features: The production furnace is equipped with a spray mechanism and a burner mechanism. The spray mechanism can evenly spray the waste acid liquid into the production furnace; the burner mechanism is used to provide heat energy to the production furnace.
4. The device for producing iron oxide powder by spray roasting according to claim 1, Features: An impact gun is arranged at the bottom of the first silo and / or the second silo.
5. The device for producing iron oxide powder by spray roasting according to claim 1, Features: A dust removal mechanism is provided on the top of the second silo.
6. The device for producing iron oxide powder by spray roasting according to claim 1, Features: A baler for baling iron oxide powder is provided below the discharge port of the second silo.
7. A method for producing iron oxide powder by spray roasting, Features: The device for producing iron oxide powder by spray roasting according to any one of claims 1 to 6 comprises the following steps: S1, spraying the waste acid liquid into a production furnace for roasting to generate iron oxide powder; S2, the iron oxide powder is transported to the pulverizing mechanism after being buffered in the first silo and pulverized by high-speed airflow; S3, the crushed iron oxide powder is classified in the grading mechanism, and the iron oxide powder that meets the classification requirement set value enters the second silo; the iron oxide powder that does not meet the classification requirement set value is returned to the crushing mechanism for crushing; S4, packaging and storing the iron oxide powder at the outlet of the second silo.
8. The method for producing iron oxide powder by spray roasting according to claim 7, Features: In S2, the particle size (D50) of the iron powder entering the pulverizing mechanism ranges from 25 to 50 μm.
9. The method for producing iron oxide powder by spray roasting according to claim 7, Features: In S3, the particle size (D50) of the iron oxide powder entering the second silo is in the range of 1 to 10 μm.
10. The method for producing iron oxide powder by spray roasting according to claim 7, Features: In S3, the specific surface area of the iron oxide powder entering the second silo is not less than 3.0m 2 / g.
Citation Information
Patent Citations
Preparation system and preparation method of low-oxygen ultrafine molybdenum disulfide
CN105536960A
Efficient and rapid crushing system
CN108816454A
Recovery process for preparing high-purity iron oxide from waste acid
CN114940514A
Method and device for continuously producing high-purity oxide powder on line
CN117861559A
Lithium iron phosphate multi-stage crushing and screening device and treatment method thereof
CN118268098A