POP packaging method and structure based on embedded fan-out packaging

By simplifying the multi-layer stacking structure using adapter plates in the POP packaging process, combining chemical vapor deposition and wiring dielectric layer design, the problems of high packaging complexity and cost in the prior art are solved, and more efficient heat dissipation and lower heat dissipation are achieved Cost packaging effect.

CN119092416AInactive Publication Date: 2024-12-06PEKING UNIV

Patent Information

Application Number
CN202411183807.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-12-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing POP packaging process based on embedded silicon-based fanout packaging has problems such as high manufacturing complexity, high cost, difficulty in heat dissipation, design complexity and application limitations, making it difficult to achieve ideal packaging effects.

Method used

By preparing the bottom and top packages based on the first and second adapter plates, bonding under heating and pressurization conditions, combining chemical vapor deposition and wiring dielectric layer design, the multi-layer stacking structure is simplified and the packaging design is reduced. Complexity and production cost to improve heat dissipation efficiency.

Benefits of technology

It has achieved simplified packaging design, reduced production costs and process difficulty, improved heat dissipation efficiency, overcome the problems of packaging complexity and high cost in the prior art, and is suitable for applications such as mobile devices and consumer electronics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119092416A_ABST
    Figure CN119092416A_ABST
Patent Text Reader

Abstract

The invention provides a POP packaging method and structure based on embedded fan-out packaging, and relates to the technical field of semiconductors, and the method comprises the steps: preparing a bottom packaging body based on a first adapter plate, and enabling the bottom packaging body to be an embedded fan-out packaging body; preparing a top packaging body based on the second adapter plate; and aligning the first micro convex points on the bottom packaging body with the second micro convex points on the top packaging body one by one, and carrying out bonding under heating and pressurizing conditions to obtain the pop packaging structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a POP packaging method and structure based on buried fan-out packaging. Background Art

[0002] Embedded Silicon Fan-Out (eSiFO) is an advanced packaging technology that combines the advantages of silicon-based packaging and fan-out packaging by embedding silicon-based chips into fan-out packages. This technology not only improves the performance and reliability of the chip, but also provides better electrical performance, thermal management and packaging density.

[0003] However, the existing packaging process for embedded silicon-based fan-out packaging POP is difficult to achieve the ideal packaging effect, and there are still a series of problems (such as complex process, high cost, heat dissipation difficulty, etc.). Summary of the invention

[0004] In view of the above problems, an embodiment of the present application provides a POP packaging method and structure based on buried fan-out packaging to overcome the above problems or at least partially solve the above problems.

[0005] According to a first aspect of an embodiment of the present application, a POP packaging method based on buried fan-out packaging is provided, the method comprising:

[0006] Based on the first adapter board, preparing a bottom package, wherein the bottom package is a buried fan-out package;

[0007] Based on the second transfer board, preparing a top package body;

[0008] The first micro-bumps on the bottom package body are aligned one by one with the second micro-bumps on the top package body, and bonding is performed under heating and pressure conditions to obtain a POP package structure.

[0009] In a possible implementation manner, the step of preparing a bottom package based on the first adapter plate includes:

[0010] Based on the size of the first chip to be embedded, etching a buried groove on the first surface of the first transfer board;

[0011] Under heating and pressurizing conditions, using a submicron chip mounter or a flip-chip bonding machine to embed the first chip into the center of the buried groove;

[0012] Depositing a layer of polyparaxylene film on the first surface by chemical vapor deposition, so that the polyparaxylene film completely fills the gap between the first chip and the buried groove;

[0013] Removing excess polyparaxylene film on the first surface by oxygen plasma etching;

[0014] Prepare a first wiring dielectric layer on the first surface, and realize metal interconnection between the first chips through the first wiring dielectric layer;

[0015] A plurality of first micro-bumps are prepared on a surface of the first wiring dielectric layer that is away from the first surface to obtain the bottom package.

[0016] In a possible implementation manner, preparing a first wiring dielectric layer on the first surface includes:

[0017] Spin coating a first height of a polyimide PI layer on the first surface;

[0018] A dual Damascene wiring process is used to prepare one or more first interconnect structures embedded in the PI layer, and metal interconnection between the first chips is achieved through the first interconnect structures to obtain the first wiring dielectric layer.

[0019] In a possible implementation manner, the step of preparing a top package based on the second transfer board includes:

[0020] preparing a copper-filled first through hole on the second surface of the second adapter plate;

[0021] Prepare one or more metal pads on the second surface, and realize metal interconnection between the first through holes through the metal pads;

[0022] Thinning a side of the second adapter plate away from the second surface until the first through hole is exposed on the surface;

[0023] Bonding one or more second chips to the second surface of the second adapter board using a DAF film or bonding glue;

[0024] By means of a wire bonding process, an electrical connection is achieved between the PAD of the second chip and the metal pad on the second adapter board;

[0025] A plurality of the second micro-bumps are prepared on the surface of the second transfer plate facing away from the second surface to obtain the top package.

[0026] In a possible implementation manner, the first adapter plate and the second adapter plate are any one of the following:

[0027] Silicon adapter board;

[0028] Ceramic adapter plate;

[0029] Glass adapter plate.

[0030] In a possible implementation manner, the height of the buried trench is the same as the height of the first chip, and the width of the buried trench is 6-30 microns longer than the width of the first chip.

[0031] In a possible implementation manner, the first height is 3-10 micrometers.

[0032] In a possible implementation manner, the metal material used to prepare the first interconnect structure and the metal pad is copper.

[0033] In a possible implementation manner, the material of the first micro-bump and the second micro-bump is copper or tin.

[0034] The second aspect of the embodiment of the present application further provides a POP packaging structure, which is prepared by the POP packaging method based on buried fan-out packaging described in the first aspect.

[0035] A third aspect of an embodiment of the present application provides a POP encapsulation device based on buried fan-out encapsulation, which is used to execute the steps of the POP encapsulation method based on buried fan-out encapsulation provided in the first aspect, and the device includes:

[0036] A first preparation module is used to prepare a bottom package based on a first adapter board, wherein the bottom package is a buried fan-out package;

[0037] A second preparation module, used for preparing a top package body based on a second adapter plate;

[0038] The packaging module is used to align the first micro-bumps on the bottom packaging body with the second micro-bumps on the top packaging body one by one, and bond them under heating and pressure conditions to obtain a POP packaging structure.

[0039] An embodiment of the present application provides a POP packaging method based on a buried fan-out package, the method comprising: preparing a bottom package body based on a first adapter board, wherein the bottom package body is a buried fan-out package body; preparing a top package body based on a second adapter board; aligning the first micro-bumps on the bottom package body with the second micro-bumps on the top package body one by one, and bonding them under heating and pressurization conditions to obtain a POP packaging structure.

[0040] The POP packaging method based on embedded fan-out packaging provided in the present application prepares a bottom package body based on a first adapter board, and prepares a top package body based on a second adapter board, and uses an adapter board to replace a multi-layer wafer structure, thereby simplifying the multi-layer stacking structure, reducing the complexity of the packaging design, improving the heat dissipation efficiency, and reducing the process difficulty and production cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the description of the embodiments of the present application will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.

[0042] Figure 1 It is a flowchart of the steps of a POP packaging method based on buried fan-out packaging provided by an embodiment of the present application;

[0043] Figure 2 It is a schematic structural diagram of a bottom packaging body formed in a POP packaging method provided in an embodiment of the present application;

[0044] Figure 3 It is a structural schematic diagram of a buried groove of a first adapter plate formed in a POP packaging method provided in an embodiment of the present application;

[0045] Figure 4 It is a schematic diagram of an intermediate structure formed in a POP packaging method provided in an embodiment of the present application;

[0046] Figure 5 It is a schematic structural diagram of a polyimide PI layer formed in a POP packaging method provided in an embodiment of the present application;

[0047] Figure 6 It is a structural schematic diagram of a first wiring dielectric layer formed in a POP packaging method provided in an embodiment of the present application.

[0048] Figure 7 It is a schematic structural diagram of a top package body formed in a POP packaging method provided in an embodiment of the present application;

[0049] Figure 8 is a schematic structural diagram of a first through hole formed in a POP packaging method provided in an embodiment of the present application;

[0050] Fig. 9 It is a schematic diagram of a thinned structure formed in a POP packaging method provided in an embodiment of the present application;

[0051] Fig.10 It is a schematic diagram of the chip structure after bonding formed in a POP packaging method provided in an embodiment of the present application;

[0052] Fig.11 It is a schematic diagram of the chip structure after bonding formed in a POP packaging method provided in an embodiment of the present application;

[0053] Fig.12 It is a structural schematic diagram of a POP packaging structure provided in an embodiment of the present application;

[0054] Fig.13 It is a structural schematic diagram of a POP packaging device provided in an embodiment of the present application;

[0055] Description of the drawings: first adapter plate 100, buried trench 101, first chip 102, polyparaxylene film 103, PI layer 104, first interconnect structure 105, first micro bump 106;

[0056] The second transfer board 200 , the first through hole 201 , the metal pad 202 , the second chip 203 , the metal wire 204 , and the second micro bump 205 . DETAILED DESCRIPTION

[0057] The exemplary embodiments of the present application will be described in more detail below in conjunction with the accompanying drawings in the embodiments of the present application. Although the exemplary embodiments of the present application are shown in the accompanying drawings, it should be understood that the present application can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present application and to enable the scope of the present application to be fully communicated to those skilled in the art.

[0058] Package on Package (POP) packaging is a packaging technology that stacks two or more chip packages vertically together. This technology allows chips with different functions (such as processors and memory) to be integrated in one package to save space and improve performance. POP packaging is made up of multiple independently packaged chips stacked vertically, and mainly includes the following structural features: 1. Bottom Package: Usually contains the main processor (such as application processor, baseband processor, etc.). 2. Top Package: Usually contains memory chips (such as DRAM or flash memory), or sensors / actuators. The top package is electrically connected to the bottom package through solder balls (ball grid array, BGA). 3. Electrical connection: The bottom and top packages are electrically connected through solder balls or bumps to ensure fast signal transmission. This connection method shortens the data transmission path, reduces latency and power consumption. 4. Mechanical support: The two layers of packaging are held together by mechanical support and adhesives to ensure structural stability and reliability.

[0059] POP packaging has the following advantages: 1. Space saving: By stacking chips vertically, the space occupied on the PCB is greatly reduced. 2. Performance improvement: The signal transmission path is shorter, which reduces delay and power consumption and improves system performance. 3. Flexibility and scalability: Different functional chips can be flexibly combined to facilitate system design and upgrade. 4. Manufacturing simplification: Separate packaging and stacking simplifies the manufacturing process and reduces manufacturing risks. 5. Cost-effectiveness: Although the packaging itself adds some costs, the overall design and manufacturing costs are reduced.

[0060] Embedded silicon fan-out packaging (eSiFO) is an advanced packaging technology that combines the advantages of silicon-based packaging and fan-out packaging by embedding silicon-based chips into fan-out packaging. This technology not only improves the performance and reliability of the chip, but also provides better electrical performance, thermal management and packaging density. However, there is currently a lack of POP packaging processes and methods based on embedded silicon fan-out packaging. Therefore, this briefing document proposes the eSiFO-POP process to provide a technical basis for applications such as mobile devices, consumer electronics, and embedded systems.

[0061] At present, the related InFO-POP (Integrated Fan-Out Package on Package) packaging is an advanced packaging technology that combines the advantages of fan-out packaging and POP packaging. However, despite its significant advantages, InFO-POP packaging also has some disadvantages: 1. High manufacturing complexity and complex process: InFO-POP packaging requires complex manufacturing processes, including the formation of multi-layer redistribution layers (RDL) and precise alignment technology. This increases the difficulty and complexity of the production process. High equipment requirements: The manufacture of InFO-POP packaging requires advanced manufacturing equipment and precise process control, resulting in a high initial investment. 2. High cost. Material cost: The use of high-performance packaging materials and multi-layer redistribution layers increases material costs. Production cost: The complex manufacturing process and strict process control requirements make the production cost high. 3. Heat dissipation problems. Thermal management challenges: Although the InFO-POP package has improved certain thermal management capabilities through the fan-out structure, the multi-layer stacked structure may still bring heat dissipation difficulties, especially in high-power applications, requiring additional heat dissipation design. 4. Yield control is difficult. High defect rate: Complex manufacturing processes and multi-layer structures may lead to more defects in the production process, affecting the yield of the package. Difficult detection: The multi-layer structure makes it more difficult to detect and repair defects, requiring more advanced detection equipment and technology. 5. Design limitations. Design complexity: The design of the InFO-POP package needs to consider multiple redistribution layers and precise electrical connections, which increases the complexity of the design. Limited flexibility: During the design and manufacturing process, the alignment and connection between layers need to be strictly controlled, which limits the flexibility of the design. 6. Application limitations. Limited application areas: Due to cost and process complexity, InFO-POP packaging is mainly used in high-performance and high-density electronic products, and does not have a competitive advantage for low-cost and low-performance applications.

[0062] In view of the above problems, the embodiment of the present application proposes a POP packaging method and structure based on buried fan-out packaging to realize the POP packaging process design based on buried fan-out packaging. In combination with the accompanying drawings, the POP packaging method based on buried fan-out packaging provided by the embodiment of the present application is described in detail through some embodiments and their application scenarios.

[0063] The first aspect of the embodiment of the present application provides a POP packaging method based on embedded fan-out packaging, referring to Figure 1 , Figure 1 A flowchart of a POP packaging method based on embedded fan-out packaging is provided in an embodiment of the present application, such as Figure 1 As shown, the method includes:

[0064] Step S101 : preparing a bottom package based on a first adapter board, wherein the bottom package is a buried fan-out package.

[0065] The POP package structure mainly includes a bottom package and a top package. In this embodiment, the bottom package is a buried fan-out package, which refers to a package structure in which one or more chips are embedded in a fan-out package. First, based on the first adapter board, a bottom package is prepared. In this step, the first adapter board used is the substrate of the adapter board. Figure 2 , Figure 2 A schematic diagram of the structure of a bottom package body formed in a POP packaging method is shown. Figure 2 As shown, a plurality of first chips 102 are embedded in the first adapter board 100, and the plurality of first chips 102 are interconnected via a first interconnect structure 105 in the first wiring medium layer. A plurality of first micro bumps 106 are also provided on the first interconnect structure 105 as bonding points for subsequent bonding with the top package body.

[0066] In a possible implementation manner, the step S101, preparing a bottom package based on the first adapter board, includes:

[0067] Step S201 , etching a buried groove on the first surface of the first transfer board based on the size of the first chip to be buried.

[0068] The first surface of the first adapter plate is the surface to be bonded. Figure 3 , Figure 3 A schematic structural diagram of a buried groove of a first adapter plate formed in a POP packaging method is shown, Figure 3As shown, according to the size of the first chip to be embedded, a buried groove 101 is prepared by etching on the first surface of the first adapter plate 100. The position of the buried groove (i.e., the position of the first chip) can be determined according to actual application requirements and is not limited in this embodiment.

[0069] In a possible implementation, the height of the buried groove is the same as the height of the first chip, and the width of the buried groove is 6-30 microns longer than the width of the first chip. In order to ensure that the first chip can be accurately placed in the buried groove, a certain width can be reserved when etching the buried groove, that is, the buried groove is designed to be 6-30 microns wider than the first chip.

[0070] Step S202: Under heating and pressurizing conditions, using a sub-micron chip mounter or a flip-chip bonding machine to embed the first chip into the center of the embedding groove.

[0071] Specifically, the first chip may be bonded to the bottom of the buried trench by using a DAF film or other bonding adhesive.

[0072] Step S203 , depositing a layer of polyparaxylene film on the first surface by chemical vapor deposition, so that the polyparaxylene film completely fills the gap between the first chip and the buried groove.

[0073] Specifically, since the etched buried groove is wider than the first chip, there will be a gap between the first chip and the buried groove. In this embodiment, room temperature chemical vapor deposition can be used to make the polyparaxylene film completely fill the gap between the first chip and the inner wall of the buried groove (that is, the thickness of the polyparaxylene film should be greater than the maximum value of the gap between the embedded chip and the adapter board).

[0074] Step S204 , removing the excess polyparaxylene film on the first surface by oxygen plasma etching.

[0075] Reference Figure 4 , Figure 4 A schematic diagram of an intermediate structure formed in a POP packaging method is shown, Figure 4 As shown, a first chip 102 is placed in the buried groove 101, and a polyparaxylene film 103 is filled in the gap between the first chip 102 and the buried groove 101. The excess polyparaxylene film on the first surface is removed by oxygen plasma etching, so that the first surface remains a smooth plane.

[0076] Step S205 , preparing a first wiring dielectric layer on the first surface, and realizing metal interconnection between the first chips through the first wiring dielectric layer.

[0077] In a possible implementation manner, the step S205 of preparing a first wiring dielectric layer on the first surface includes:

[0078] Step S2051, spin-coating a first-height polyimide PI layer on the first surface. Figure 5 , Figure 5 A schematic diagram of the structure of a polyimide PI layer formed in a POP packaging method is shown, Figure 5 As shown, a PI layer 104 with a first height is spin-coated on the first surface. In a possible implementation, the first height is 3-10 microns.

[0079] Step S2052: using a dual damascene wiring process to prepare one or more first interconnect structures embedded in the PI layer, and realizing metal interconnection between the first chips through the first interconnect structures to obtain the first wiring dielectric layer.

[0080] In this embodiment, the first interconnection structure is used to realize metal interconnection between multiple first chips. Figure 6 , Figure 6 A schematic structural diagram of a first wiring dielectric layer formed in a POP packaging method is shown. Figure 6 As shown, the first interconnection structure 105 includes: interconnection wiring grooves and interconnection vias. In the PI layer 104, multiple first interconnection structures 105 are embedded, wherein the height of the interconnection vias in the first interconnection structure is the same as the thickness of the PI layer 104, the bottom of the interconnection vias is connected to the first chip 102, and the top of the interconnection vias is connected to the interconnection wiring grooves. For each interconnection wiring groove, one or more interconnection vias are connected, so that the metal interconnection between multiple first chips is realized through the interconnection wiring grooves and the interconnection vias (i.e., the first interconnection structure 105). In a possible embodiment, the metal material for preparing the first interconnection structure is copper, which has excellent conductive properties and is conducive to realizing metal interconnection between chips. Among them, the specific shape and position of the first interconnection structure 105 can be set according to actual needs, so as to determine the specific position according to the actual metal interconnection needs between the first chips.

[0081] Step S206, preparing a plurality of first micro bumps on a surface of the first wiring dielectric layer away from the first surface to obtain the bottom package.

[0082] like Figure 2As shown, a plurality of first micro-bumps 106 are prepared on the first wiring dielectric layer. In a possible implementation, the material of the first micro-bumps is copper or tin. The first micro-bumps serve as bonding points for subsequent bonding of the bottom package and the top package. The positions of the first micro-bumps can be set according to actual needs and are not specifically limited in this embodiment.

[0083] Step S102 : preparing a top package based on the second transfer board.

[0084] In this embodiment, the top package is the top package, which usually includes a memory chip (such as DRAM or flash memory), and can also be a sensor / actuator. First, based on the second adapter board, a top package is prepared. In this step, the second adapter board used is the substrate of the adapter board. In a possible implementation, the first adapter board and the second adapter board are any one of the following: a silicon adapter board; a ceramic adapter board; a glass adapter board. The POP packaging method based on embedded fan-out packaging provided in the present application prepares a bottom package based on the first adapter board, and prepares a top package based on the second adapter board, and uses an adapter board to replace a multi-level wafer structure, thereby simplifying the multi-layer stacked structure, reducing the complexity of the packaging design, improving the heat dissipation efficiency, and reducing the process difficulty and production cost.

[0085] It should be noted that there is no sequential execution relationship between step S101 and step S102, that is, the first adapter board can be processed first (execute step S101) to obtain the bottom package, and then the second adapter board can be processed (execute step S102) to obtain the top package; the second adapter board can be processed first (execute step S102) and then the first adapter board can be processed (execute step S101); the first adapter board and the second adapter board can also be processed at the same time (execute step S101 and step S102 at the same time).

[0086] Reference Figure 7 , Figure 7 A schematic diagram of the structure of a top package body formed in a POP packaging method is shown. Figure 7 As shown, a plurality of first through holes 201 are embedded in the second adapter board 200, a plurality of metal pads 202 and a second chip 203 are prepared on the surface away from the bonding surface, the first through holes 201 are connected through the metal pads 202, and a wire bonding process (corresponding to Figure 7 The metal wire 204 in the bottom of the chip 203 realizes the electrical connection between the metal pad 202 and the second chip 203. A plurality of second micro bumps 205 are also provided on the surface to be bonded as bonding points for bonding with the bottom package body.

[0087] In a possible implementation manner, the step S102, preparing a top package based on the second adapter board, includes:

[0088] Step S1021, preparing a first through hole filled with copper on the second surface of the second adapter board.

[0089] The second surface of the second transfer plate is the surface of the top package body facing away from the surface to be bonded. Figure 8 , Figure 8 A schematic diagram of the structure of a first through hole formed in a POP packaging method is shown. Figure 8 As shown, a plurality of copper-filled first through holes 201 are prepared on the second surface of the second adapter board 200. Specifically, a pattern is defined on the surface of the second adapter board by photolithography, and the position of the pattern corresponds to the position of the first through hole. According to the pattern, the second adapter board 200 is etched until a preset through hole height is reached to obtain a plurality of through holes, and then a seed layer is deposited in the through hole, and the material of the seed layer is metallic copper. On the seed layer, metallic copper is filled into the through hole by electroplating, so that the metal material of the seed layer is combined with the metallic copper filled by electroplating until the metallic copper completely fills the through hole, and finally, by chemical mechanical polishing (CMP), the excess metallic copper on the second surface is removed to make the surface flat, and the copper-filled first through hole 201 is obtained. The height and other dimensional information of the first through hole 201 can be determined according to actual application requirements, and is not limited in this embodiment.

[0090] Step S1022: prepare one or more metal pads on the second surface, and realize metal interconnection between the first through holes through the metal pads.

[0091] Specifically, each metal pad is connected to one or more first through holes, thereby realizing metal interconnection between the first through holes. In a possible implementation, the metal material for preparing the first interconnection structure and the metal pad is copper, which has excellent conductive properties and is conducive to realizing metal interconnection between chips. Exemplarily, in the actual preparation process, an insulating layer (such as a silicon dioxide layer) can be deposited on the second surface, and then (photolithography and etching can be used) a through hole corresponding to the shape of the metal pad is etched in the insulating layer, and then a seed layer is deposited on the surface of the through hole by magnetron sputtering, and a metal material (such as copper) is filled in the through hole. After removing the excess metal material on the surface of the insulating layer, the insulating layer is removed, and then one or more metal pads on the second surface can be obtained. The position of the metal pad should correspond to the position of the first through hole, so that the metal pad can be connected to one or more first through holes, so that the first through hole can be combined with the metal pad. The specific shape, size and position of the metal pad can be set according to actual needs, and are not limited in this embodiment.

[0092] Step S1023, thinning the side of the second adapter plate away from the second surface until the first through hole is exposed on the surface.

[0093] Reference Fig. 9 , Fig. 9 A schematic diagram of a thinned structure formed in a POP packaging method is shown, Fig. 9 As shown, the second adapter plate 200 is thinned (a multi-step thinning method may be used) until the first through hole 201 is exposed on the surface, thereby obtaining the surface to be bonded of the second adapter plate. The thinning process may generally use a multi-step thinning method (mechanical thinning-CMP-dry etching) to achieve the required adapter plate thickness. In this case, the height of the thinned second adapter plate 200 and the first through hole 201 embedded in the second adapter plate are the same.

[0094] Step S1024: using a DAF film or bonding glue to bond one or more second chips to the second surface of the second transfer board.

[0095] Reference Fig.10 , Fig.10 A schematic diagram of the chip bonding structure formed in a POP packaging method is shown. Fig.10 As shown, on the second surface of the second adapter board 200, one or more metal pads 202 are prepared through step S1022, and the second chip 203 is bonded on the metal pad 202. For bonding requirements, a DAF film or bonding glue can be pre-coated on the metal pad so that the second chip 203 can be fixed on the metal pad 202.

[0096] Step S1025 , achieving electrical connection between the PAD of the second chip and the metal pad on the second adapter board through a wire bonding process.

[0097] Specifically, refer to Fig.11 , Fig.11 A schematic diagram of the chip bonding structure formed in a POP packaging method is shown. Fig.11 As shown, the metal wire 204 made by wire bonding is used to achieve the connection between the PAD of the second chip 203 and the metal pad 202. Wire bonding, also known as wire bonding, refers to the use of metal wires (gold wires, aluminum wires, etc.) to complete the connection of the internal interconnection wiring of the solid-state circuit in the microelectronic device by using heat pressing or ultrasonic energy (that is, one end of the metal wire 204 is connected to the PAD of the second chip 203, and the other end is connected to the metal pad 202).

[0098] Step S1026, preparing a plurality of second micro bumps on the surface of the second transfer plate facing away from the second surface to obtain the top package body.

[0099] like Figure 7 As shown, a plurality of second micro-bumps 205 are prepared on the surface to be bonded (i.e., the surface away from the second surface) of the second adapter plate 200. In a possible implementation, the material of the first micro-bump and the second micro-bump is copper or tin. The second micro-bump serves as a bonding point for subsequent bonding of the bottom package and the top package. The position of the second micro-bump can be set according to actual needs and is not specifically limited in this embodiment.

[0100] Step S103, aligning the first micro-bumps on the bottom package body with the second micro-bumps on the top package body one by one, and bonding them under heating and pressure conditions to obtain a POP package structure.

[0101] In this embodiment, refer to Fig.12 , Fig.12 A schematic diagram of a POP packaging structure is shown. Fig.12 As shown, the first micro-bump on the bottom package body and the second micro-bump on the top package body are in a one-to-one correspondence, so that the bottom package body and the top package body can be bonded under heating and pressurization conditions by aligning the two to obtain a POP packaging structure. In this way, the embodiment of the present application provides a POP packaging method based on a buried fan-out package, prepares a bottom package body based on a first adapter plate, prepares a top package body based on a second adapter plate, and uses an adapter plate to replace a multi-level wafer structure, thereby simplifying the multi-layer stacked structure, reducing the complexity of the packaging design, improving the heat dissipation efficiency, and reducing the process difficulty and production cost.

[0102] The second aspect of the embodiment of the present application further provides a POP packaging structure, which is prepared by the POP packaging method based on buried fan-out packaging described in the first aspect.

[0103] The third aspect of the embodiment of the present application provides a POP packaging device based on buried fan-out packaging, which is used to execute the steps of the POP packaging method based on buried fan-out packaging provided in the first aspect, referring to Fig.13 , Fig.13 A schematic diagram of the structure of a POP packaging device is shown. Fig.13 As shown, the device comprises:

[0104] A first preparation module is used to prepare a bottom package based on a first adapter board, wherein the bottom package is a buried fan-out package;

[0105] A second preparation module, used for preparing a top package body based on a second adapter plate;

[0106] The packaging module is used to align the first micro-bumps on the bottom packaging body with the second micro-bumps on the top packaging body one by one, and bond them under heating and pressure conditions to obtain a POP packaging structure.

[0107] In a possible implementation, the first preparation module is used to:

[0108] Based on the size of the first chip to be embedded, etching a buried groove on the first surface of the first transfer board;

[0109] Under heating and pressurizing conditions, using a submicron chip mounter or a flip-chip bonding machine to embed the first chip into the center of the buried groove;

[0110] Depositing a layer of polyparaxylene film on the first surface by chemical vapor deposition, so that the polyparaxylene film completely fills the gap between the first chip and the buried groove;

[0111] Removing excess polyparaxylene film on the first surface by oxygen plasma etching;

[0112] Prepare a first wiring dielectric layer on the first surface, and realize metal interconnection between the first chips through the first wiring dielectric layer;

[0113] A plurality of first micro-bumps are prepared on a surface of the first wiring dielectric layer that is away from the first surface to obtain the bottom package.

[0114] In a possible implementation manner, preparing a first wiring dielectric layer on the first surface includes:

[0115] Spin coating a first height of a polyimide PI layer on the first surface;

[0116] A dual Damascene wiring process is used to prepare one or more first interconnect structures embedded in the PI layer, and metal interconnection between the first chips is achieved through the first interconnect structures to obtain the first wiring dielectric layer.

[0117] In a possible implementation manner, the second preparation module is used to:

[0118] preparing a copper-filled first through hole on the second surface of the second adapter plate;

[0119] Prepare one or more metal pads on the second surface, and realize metal interconnection between the first through holes through the metal pads;

[0120] Thinning a side of the second adapter plate away from the second surface until the first through hole is exposed on the surface;

[0121] Bonding one or more second chips to the second surface of the second adapter board using a DAF film or bonding glue;

[0122] By means of a wire bonding process, an electrical connection is achieved between the PAD of the second chip and the metal pad on the second adapter board;

[0123] A plurality of the second micro-bumps are prepared on the surface of the second transfer plate facing away from the second surface to obtain the top package.

[0124] In a possible implementation manner, the first adapter plate and the second adapter plate are any one of the following:

[0125] Silicon adapter board;

[0126] Ceramic adapter plate;

[0127] Glass adapter plate.

[0128] In a possible implementation manner, the height of the buried trench is the same as the height of the first chip, and the width of the buried trench is 6-30 microns longer than the width of the first chip.

[0129] In a possible implementation manner, the first height is 3-10 micrometers.

[0130] In a possible implementation manner, the metal material used to prepare the first interconnect structure and the metal pad is copper.

[0131] In a possible implementation manner, the material of the first micro-bump and the second micro-bump is copper or tin.

[0132] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.

[0133] The embodiments of the present application are described with reference to the flowcharts and / or block diagrams of the methods, apparatuses, electronic devices, and computer program products according to the embodiments of the present application. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as the combination of the processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing terminal device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing terminal device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.

[0134] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing terminal device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce a manufactured product including an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.

[0135] These computer program instructions can also be loaded onto a computer or other programmable data processing terminal device so that a series of operating steps are executed on the computer or other programmable terminal device to produce a computer-implemented process, thereby providing instructions for executing on the computer or other programmable terminal device to implement the process. Figure 1 A process or multiple processes and / or boxes Figure 1 The steps for the functions specified in one or more boxes.

[0136] Although the preferred embodiments of the present application have been described, those skilled in the art may make additional changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the embodiments of the present application.

[0137] Finally, it should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or terminal device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or terminal device. In the absence of further restrictions, the elements defined by the sentence "including one..." do not exclude the existence of other identical elements in the process, method, article or terminal device including the elements.

[0138] The above is a detailed introduction to a POP packaging method and structure based on embedded fan-out packaging provided by the present application. This article uses specific examples to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method of the present application and its core idea; at the same time, for general technical personnel in this field, according to the idea of ​​the present application, there will be changes in the specific implementation method and application scope. In summary, the content of this specification should not be understood as a limitation on the present application.

Claims

1. A POP packaging method based on embedded fan-out packaging, It is characterized in that The method comprises: Based on the first adapter board, preparing a bottom package, wherein the bottom package is a buried fan-out package; Based on the second transfer board, preparing a top package body; The first micro-bumps on the bottom package body are aligned one by one with the second micro-bumps on the top package body, and bonding is performed under heating and pressure conditions to obtain a POP package structure.

2. The POP packaging method based on buried fan-out packaging according to claim 1, It is characterized in that The method of preparing a bottom package based on the first adapter plate includes: Based on the size of the first chip to be embedded, etching a buried groove on the first surface of the first transfer board; Under heating and pressurizing conditions, using a submicron chip mounter or a flip-chip bonding machine to embed the first chip into the center of the buried groove; Depositing a layer of polyparaxylene film on the first surface by chemical vapor deposition, so that the polyparaxylene film completely fills the gap between the first chip and the buried groove; Removing excess polyparaxylene film on the first surface by oxygen plasma etching; Prepare a first wiring dielectric layer on the first surface, and realize metal interconnection between the first chips through the first wiring dielectric layer; A plurality of the first micro-bumps are prepared on a surface of the first wiring dielectric layer that is away from the first surface to obtain the bottom package.

3. The POP packaging method based on buried fan-out packaging according to claim 2, It is characterized in that The step of preparing a first wiring dielectric layer on the first surface comprises: Spin coating a first height of a polyimide PI layer on the first surface; A dual Damascene wiring process is used to prepare one or more first interconnect structures embedded in the PI layer, and metal interconnection between the first chips is achieved through the first interconnect structures to obtain the first wiring dielectric layer.

4. The POP packaging method based on buried fan-out packaging according to claim 3, It is characterized in that The method of preparing a top package based on the second transfer board includes: preparing a copper-filled first through hole on the second surface of the second adapter plate; Prepare one or more metal pads on the second surface, and realize metal interconnection between the first through holes through the metal pads; Thinning a side of the second adapter plate away from the second surface until the first through hole is exposed on the surface; Bonding one or more second chips to the second surface of the second adapter board using a DAF film or bonding glue; By means of a wire bonding process, an electrical connection is achieved between the PAD of the second chip and the metal pad on the second adapter board; A plurality of the second micro-bumps are prepared on the surface of the second transfer plate facing away from the second surface to obtain the top package.

5. The POP packaging method based on buried fan-out packaging according to claim 1, It is characterized in that The first adapter plate and the second adapter plate are any one of the following: Silicon adapter board; Ceramic adapter plate; Glass adapter plate.

6. The POP packaging method based on buried fan-out packaging according to claim 2, It is characterized in that The height of the buried trench is the same as that of the first chip, and the width of the buried trench is 6-30 microns longer than that of the first chip.

7. The POP packaging method based on buried fan-out packaging according to claim 3, It is characterized in that The first height is 3-10 micrometers.

8. The POP packaging method based on buried fan-out packaging according to claim 4, It is characterized in that The metal material used to prepare the first interconnect structure and the metal pad is copper.

9. The POP packaging method based on buried fan-out packaging according to claim 1, It is characterized in that The materials of the first micro-bumps and the second micro-bumps are copper or tin.

10. A pop packaging structure, It is characterized in that The POP packaging structure is prepared by the POP packaging method based on buried fan-out packaging described in any one of claims 1-9.

Citation Information

Patent Citations

  • Embedded silicon substrate fan-out type packaging structure and manufacturing method thereof

    CN105023900A

  • Stacked semiconductor package and method of manufacturing thereof

    KR1020120040039A

  • Package method and package structure of fan-out chip

    US20190006307A1

Cited By

  • Light-heat isolation co-packaging structure preparation method and co-packaging structure

    CN119342932A

  • A method for preparing a light-heat-isolated co-packaging structure and a co-packaging structure

    CN119342932B