Preparation method of self-aligned trench isolation structure and semiconductor structure

By adopting the self-aligned trench isolation structure preparation method in semiconductor manufacturing, better smoothing effect is achieved, solving the problems of difficult and unsatisfactory top corner smoothing treatment, and improving the electrical performance and reliable production of semiconductor devices sex.

CN119092459APending Publication Date: 2024-12-06GTA SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411178280.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The traditional top corner smoothing process is difficult to perform, and the smoothing effect is not ideal, especially when the gate oxide layer is thicker, which increases, affects the electrical performance and reliability of semiconductor devices.

Method used

By using the preparation method of a self-aligning trench isolation structure, the mask material layer is formed on the substrate, the initial opening is etched and the target opening is back-etched, the steps are etched, and the corners are rounded on the steps. Processing to form an isolation medium layer to achieve a better and more precise smooth effect.

Benefits of technology

It improves the production yield of semiconductor processes and the reliability of devices, avoids the problems of process incompatibility or increased processing difficulty due to the failure of the side wall top corner morphology, reduces process costs and improves process efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119092459A_ABST
    Figure CN119092459A_ABST
Patent Text Reader

Abstract

The invention provides a preparation method of a self-aligned trench isolation structure and a semiconductor structure. The preparation method comprises the following steps: providing a substrate, and forming a mask material layer on one side of the substrate; an initial opening is etched in the mask material layer, an isolation groove is etched in the substrate based on the initial opening, and the reserved mask material layer serves as a graphical mask layer; performing back etching on the graphical mask layer to enable the initial opening to retreat along the direction of the expanded opening so as to form a target opening; etching a step at the vertex angle of the side wall of the isolation groove based on the target opening; and performing rounded corner processing on the step, and forming an isolation dielectric layer in the isolation groove after the rounded corner processing. According to the preparation method, a better and more accurate smooth effect can be realized, and the production yield of a semiconductor manufacturing process and the use reliability of a semiconductor device can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor manufacturing technology, and in particular to a method for preparing a self-aligned trench isolation structure and a semiconductor structure. Background Art

[0002] In the semiconductor manufacturing process, in order to avoid the electric field concentration effect caused by sharp corners, the corners of the active area can be rounded. The rounding process can not only reduce the electric field concentration, but also improve the increase of parasitic capacitance and parasitic resistance, avoid affecting the switching speed and energy consumption performance of semiconductor devices, and thus improve the electrical performance of semiconductor devices.

[0003] However, the traditional top corner rounding process is difficult to perform, the rounding effect is not ideal and has limitations. For example, when the gate oxide layer (Gate Oxide) is relatively thick, the difficulty of top corner rounding is further increased, thereby affecting the electrical performance and reliability of semiconductor devices.

[0004] It should be noted that the information disclosed in the above background technology section is only used to enhance the understanding of the background of the present application, and therefore may include information that does not constitute prior art known to ordinary technicians in the field. Summary of the invention

[0005] Based on this, the embodiments of the present application provide a method for preparing a self-aligned trench isolation structure and a semiconductor structure, which can achieve a better and more precise rounding effect, and help improve the production yield of the semiconductor process and the reliability of semiconductor devices.

[0006] According to some embodiments, the present application provides, on one hand, a method for preparing a self-aligned trench isolation structure, comprising the following steps:

[0007] Providing a substrate, and forming a mask material layer on one side of the substrate;

[0008] Etching an initial opening in the mask material layer, and etching an isolation trench in the substrate based on the initial opening, and retaining the mask material layer as a patterned mask layer;

[0009] Etching back the patterned mask layer so that the initial opening retreats in a direction of expanding the opening to form a target opening;

[0010] Based on the target opening, etching a step at a top corner of a sidewall of the isolation trench;

[0011] The step is rounded, and an isolation dielectric layer is formed in the isolation trench after the rounding.

[0012] In some embodiments, the patterned mask layer is etched back using a wet etching process.

[0013] In some embodiments, the mask material layer includes a nitride material layer.

[0014] In some embodiments, etching back the patterned mask layer comprises the following steps:

[0015] forming a filling dielectric layer in the isolation trench, wherein the top surface of the filling dielectric layer is not lower than the surface of the substrate;

[0016] Etching back the patterned mask layer so that the initial opening retreats in the direction of expanding the opening to form the target opening;

[0017] The filling medium layer is removed.

[0018] In some embodiments, the material forming the filling dielectric layer includes at least one of an oxide filling material and an organic filling material.

[0019] In some embodiments, a gate dielectric layer is further formed between the patterned mask layer and the substrate.

[0020] In some embodiments, the rounding of the step comprises the following steps:

[0021] A passivation layer is formed on the inner wall of the isolation trench, and the passivation layer also covers the step.

[0022] In some embodiments, the passivation layer and the isolation dielectric layer have the same constituent material.

[0023] In some embodiments, the step of forming a passivation layer on the inner wall of the isolation trench comprises the following steps:

[0024] A furnace tube process is adopted to form a liner oxide layer on the inner wall of the isolation trench, and the liner oxide layer is used as the passivation layer.

[0025] According to some embodiments, the present application further provides a semiconductor structure on the other hand, wherein the semiconductor structure has a trench isolation structure, and the trench isolation structure is prepared by the preparation method of the self-aligned trench isolation structure provided in the aforementioned embodiments.

[0026] It should be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the present application.

[0027] The embodiments of the present application may or at least have the following advantages:

[0028] In an embodiment of the present application, an isolation trench is first etched in a substrate based on a patterned mask layer having an initial opening, and then the patterned mask layer is back-etched so that the initial opening is self-aligned by retreating in the direction of the expanded opening, thereby forming a target opening, and a step is etched at the sidewall top corner of the isolation trench based on the target opening. In the embodiment of the present application, the sidewall top corner of the isolation trench is rounded based on the step. Compared with the traditional rounding process, the rounding based on the step makes the roundness of the sidewall top corner of the isolation trench controllable, which is conducive to making the sidewall top corner have a better and more precise morphology, thereby improving the production yield of the semiconductor process and the reliability of the use of the semiconductor device. For example, by controlling the roundness of the sidewall top corner of the isolation trench, it is possible to avoid problems such as process incompatibility or increased processing difficulty due to the sidewall top corner morphology not meeting the requirements in the subsequent process. Therefore, the embodiment of the present application can help optimize the semiconductor process while ensuring the performance and reliability of the semiconductor device. At the same time, the embodiment of the present application completes self-alignment by allowing the initial opening to retreat in the direction of the expanded opening. Compared with the traditional photolithography alignment method, the embodiment of the present application does not require the use of an additional mask, and is therefore beneficial for improving process efficiency and reducing process costs.

[0029] Other advantages, objectives and features of the present application will be described in the following description to some extent, and will be apparent to those skilled in the art based on the following examination and study, or can be taught from the practice of the present application to some extent. The objectives and other advantages of the present application can be achieved and obtained through the following description. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Other features, objects and advantages of the present application will become more apparent by reading the detailed description of non-limiting embodiments made with reference to the following drawings.

[0031] Figure 1 A schematic diagram of a process for preparing a self-aligned trench isolation structure provided in some embodiments of the present application;

[0032] Figure 2 A schematic diagram of a process of etching back a patterned mask layer in a method for preparing a self-aligned trench isolation structure provided in some embodiments of the present application;

[0033] Figure 3 A schematic cross-sectional view of a structure obtained after a mask material layer is formed in a method for preparing a self-aligned trench isolation structure provided in some embodiments of the present application;

[0034] Figure 4 A schematic diagram of a cross-sectional structure of a structure obtained after etching an initial opening in a method for preparing a self-aligned trench isolation structure provided in some embodiments of the present application;

[0035] Figure 5 A schematic diagram of a cross-sectional structure of a structure obtained after a filling dielectric material layer is formed in a method for preparing a self-aligned trench isolation structure provided in some embodiments of the present application;

[0036] Figure 6 A schematic diagram of a cross-sectional structure of a structure obtained after a filling dielectric layer is formed in a method for preparing a self-aligned trench isolation structure provided in some embodiments of the present application;

[0037] Figure 7 A schematic diagram of a cross-sectional structure of a structure obtained after a target opening is formed in a method for preparing a self-aligned trench isolation structure provided in some embodiments of the present application;

[0038] Figure 8 A schematic diagram of a cross-sectional structure of a structure obtained after removing a filling dielectric layer in a method for preparing a self-aligned trench isolation structure provided in some embodiments of the present application;

[0039] Fig. 9 A schematic diagram of a cross-sectional structure of a structure obtained after rounding a step in a method for preparing a self-aligned trench isolation structure provided in some embodiments of the present application;

[0040] Fig.10 A schematic cross-sectional view of a structure obtained after forming an isolation dielectric layer in a method for preparing a self-aligned trench isolation structure provided in some embodiments of the present application.

[0041] Description of reference numerals:

[0042] 11. substrate; 12. mask material layer; 13. gate dielectric material layer; 14. advanced graphic film; 15. dielectric anti-reflection layer; 16. patterned photoresist layer; 21. patterned mask layer; 22. gate dielectric layer; 31. filling dielectric layer; 31', filling dielectric material layer; 51. isolation dielectric layer; 52. passivation layer;

[0043] t1, initial opening; T, isolation trench; t2, target opening; S, step. DETAILED DESCRIPTION

[0044] In order to facilitate understanding of the present application, the present application will be described more fully below with reference to the relevant drawings. Embodiments of the present application are provided in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present application more thorough and comprehensive.

[0045] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application.

[0046] It should be understood that when an element or layer is referred to as being "on," "adjacent to," "connected to," or "coupled to" another element or layer, it can be directly on, adjacent to, connected to, or coupled to the other element or layer, or there may be intervening elements or layers. In contrast, when an element is referred to as being "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" another element or layer, there are no intervening elements or layers.

[0047] Spatially relative terms such as "under," "beneath," "below," "under," "above," "above," and the like may be used herein to describe the relationship of an element or feature shown in the figures to other elements or features. It should be understood that, in addition to the orientations shown in the figures, spatially relative terms also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is flipped, an element or feature described as "under other elements" or "under it" or "under it" will be oriented as "over" the other elements or features. Thus, the exemplary terms "under" and "under" may include both upper and lower orientations. In addition, the device may also include additional orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptors used herein are interpreted accordingly.

[0048] When used herein, the singular forms "a", "an", and "said / the" may also include plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "include / comprise" or "have" and the like specify the presence of stated features, wholes, steps, operations, components, parts, or combinations thereof, but do not exclude the possibility of the presence or addition of one or more other features, wholes, steps, operations, components, parts, or combinations thereof. At the same time, in this specification, the term "and / or" includes any and all combinations of the relevant listed items.

[0049] Embodiments of the invention are described herein with reference to cross-sectional views that are schematic representations of ideal embodiments (and intermediate structures) of the present application, such that variations in the shapes shown due to, for example, manufacturing techniques and / or tolerances are anticipated. Thus, embodiments of the present application should not be limited to the specific shapes of the regions shown herein, but include deviations in shapes due to, for example, manufacturing techniques. The regions shown in the figures are schematic in nature, and their shapes do not represent the actual shapes of the regions of the device, and do not limit the scope of the present application.

[0050] In the semiconductor manufacturing process, in order to avoid the electric field concentration effect caused by sharp corners, the corners of the active area can be rounded. The rounding process can not only reduce the electric field concentration, but also improve the increase of parasitic capacitance and parasitic resistance, avoid affecting the switching speed and energy consumption performance of semiconductor devices, and thus improve the electrical performance of semiconductor devices.

[0051] However, the traditional top corner rounding process is difficult to perform, the rounding effect is not ideal and has limitations. For example, when the gate oxide layer (Gate Oxide) is relatively thick, the difficulty of top corner rounding is further increased, thereby affecting the electrical performance and reliability of semiconductor devices.

[0052] In view of the shortcomings of the related art, the present application provides a method for preparing a self-aligned trench isolation structure and a semiconductor structure, which can achieve a better and more precise rounding effect, and help improve the production yield of semiconductor processes and the reliability of semiconductor devices. The details will be described in the subsequent embodiments.

[0053] See also Figure 1 The present application provides a method for preparing a self-aligned trench isolation structure. The preparation method may specifically include the following steps S100 to S500:

[0054] S100: providing a substrate, and forming a mask material layer on one side of the substrate.

[0055] S200: etching an initial opening in the mask material layer, and etching an isolation trench in the substrate based on the initial opening, and the remaining mask material layer is used as a patterned mask layer.

[0056] S300: etching back the patterned mask layer so that the initial opening retreats in the direction of expanding the opening to form a target opening.

[0057] S400: Based on the target opening, a step is etched at a top corner of a sidewall of the isolation trench.

[0058] S500: performing a rounding process on the step, and forming an isolation dielectric layer in the rounded isolation trench.

[0059] In the above preparation method, an isolation groove is first etched in the substrate based on a patterned mask layer having an initial opening, and then the patterned mask layer is back-etched to make the initial opening retreat in the direction of expanding the opening to form a target opening, and a step is etched at the top corner of the side wall of the isolation groove based on the target opening.

[0060] The above-mentioned preparation method rounds the top corners of the side walls of the isolation trench based on steps. Compared with the traditional rounding treatment process, this step-based rounding treatment makes the roundness of the top corners of the side walls of the isolation trench controllable, which is conducive to making the top corners of the side walls have better and more precise morphology, thereby improving the production yield of the semiconductor process and the reliability of the use of semiconductor devices.

[0061] Furthermore, the above-mentioned preparation method can control the smoothness of the top angle of the isolation trench sidewall, thereby avoiding problems such as process incompatibility or increased processing difficulty caused by the sidewall top angle morphology not meeting the requirements in subsequent processes. Therefore, the above-mentioned preparation method can help optimize the semiconductor process while ensuring the performance and reliability of the semiconductor device.

[0062] At the same time, the above preparation method etches back the patterned mask layer so that the initial opening is self-aligned by retreating in the direction of the expanded opening, thereby forming a target opening. Compared with the traditional photolithography alignment method, the above preparation method does not require the use of an additional mask, so it is also beneficial to improve process efficiency and reduce process costs.

[0063] See also Figure 2 In some embodiments, the process of etching back the patterned mask layer in step S300 may be specifically performed as follows: steps S310 to S330:

[0064] S310: forming a filling dielectric layer in the isolation trench, wherein a top surface of the filling dielectric layer is not lower than a surface of the substrate.

[0065] S320: etching back the patterned mask layer so that the initial opening retreats in the direction of expanding the opening to form a target opening.

[0066] S330: removing the filling dielectric layer.

[0067] In order to more clearly illustrate the preparation methods in some of the above embodiments, Figures 3 to 10 Understand some embodiments of the present application.

[0068] In step S100, refer to Figure 3 , provide a substrate 11, and form a mask material layer 12 on one side of the substrate 11.

[0069] For example, the substrate 11 can be made of semiconductor material, insulating material, conductor material or any combination of their material types. The substrate 11 can be a single-layer structure or a multi-layer structure. For example, the substrate 11 can be a silicon (Si) substrate, a silicon germanium (SiGe) substrate, a silicon germanium carbon (SiGeC) substrate, a silicon carbide (SiC) substrate, a gallium arsenide (GaAs) substrate, an indium arsenide (InAs) substrate, an indium phosphide (InP) substrate or other III / V semiconductor substrates or II / VI semiconductor substrates. Or, for example, the substrate 11 can be a layered substrate including a stack of Si and SiGe, a stack of Si and SiC, a silicon on insulator (SOI) or a silicon germanium on insulator, etc.

[0070] The present embodiment of the application does not specifically limit the constituent material of the mask material layer 12 formed in step S100. In some embodiments, the mask material layer 12 may include but is not limited to a nitride material layer. Nitride materials have high corrosion resistance and stability, and can provide a good masking effect in the subsequent etching process, ensuring high processing accuracy in the formation process of the initial opening and the target opening, thereby ensuring the accuracy and production yield of the trench isolation structure.

[0071] Exemplarily, the nitride material layer may include but is not limited to a silicon nitride (SiN) layer.

[0072] In step S200, refer to Figure 4 , an initial opening t1 is etched in the mask material layer 12 , and an isolation trench T is etched in the substrate 11 based on the initial opening t1 , and the remaining mask material layer 12 is used as a patterned mask layer 21 .

[0073] In some embodiments, in step S200, an initial opening t1 is etched in the mask material layer 12, which can be specifically performed as follows:

[0074] First, if Figure 3 As shown, an advanced pattern film 14 (APF) and a dielectric anti-reflective layer 15 are sequentially formed on the side of the mask material layer 12 away from the substrate 11 as a hard mask, and a patterned photoresist (PR) layer 16 is formed on the side of the dielectric anti-reflective layer 15 away from the advanced pattern film 14.

[0075] The pattern in the patterned photoresist layer 16 can be used to define the shape, size and distribution of the isolation trench T. The advanced pattern film 14 can be used to improve the accuracy of transferring the pattern in the patterned photoresist layer 16 to the mask material layer 12. The dielectric anti-reflection layer 15 can be used to absorb the light irradiated thereon, thereby improving the pattern transferred to the advanced pattern film 14 and the advanced pattern film 14 can be used to improve the accuracy of transferring the pattern in the patterned photoresist layer 16 to the mask material layer 12. The constituent material of the dielectric anti-reflection layer 15 can include but is not limited to silicon oxynitride (SiON).

[0076] After forming the patterned photoresist layer 16, the dielectric anti-reflection layer 15 and the advanced patterned film 14 are sequentially etched using the patterned photoresist layer 16 as a mask, so as to transfer the pattern in the patterned photoresist layer 16 to the mask material layer 12. Figure 4 As shown, an initial opening t1 is etched.

[0077] In some embodiments, please refer to Figure 4 A gate dielectric layer 22 may be formed between the patterned mask layer 21 and the substrate 11. The gate dielectric layer 22 may include, for example, a gate oxide layer (Gate Oxide, GOX for short).

[0078] In the above embodiment, a gate dielectric material layer 13, a mask material layer 12, an advanced graphic film 14 and a dielectric anti-reflection layer 15 may be sequentially formed on one side of the substrate 11 as a hard mask. Figure 4 As shown, the patterned photoresist layer 16 is used as a mask to sequentially etch the dielectric anti-reflection layer 15 and the advanced patterned film 14, so as to transfer the pattern in the patterned photoresist layer 16 to the mask material layer 12 and the gate dielectric material layer 13, and etch out an initial opening t1. At this point, the gate dielectric material layer 13 is retained as the gate dielectric layer 22.

[0079] In step S300, refer to Figures 5 to 8 , the patterned mask layer 21 is etched back, so that the initial opening t1 retreats in the direction of the expanded opening, so that the opening of the initial opening t1 is aligned and matched with the shape and position of the predefined target opening t2, and self-alignment is completed to form the target opening t2. Since step S300 adopts the back etching method, self-alignment can be achieved without the assistance of a mask, so the use of a mask can be saved and the process cost can be reduced.

[0080] It should be noted that, in some embodiments, the patterned mask layer 21 and the gate dielectric layer 22 may be etched back simultaneously, so that the sidewalls of the patterned mask layer 21 and the gate dielectric layer 22 simultaneously retreat in the direction of expanding the initial opening t1, thereby forming a target opening t2.

[0081] In some embodiments, the patterned mask layer 21 may be etched back using the following steps S310 to S330:

[0082] In step S310, Figures 5 and 6 As shown, a filling dielectric layer 31 is formed in the isolation trench T, and the top surface of the filling dielectric layer 31 is not lower than the surface of the substrate 11 .

[0083] In step S320, Figure 7 As shown, the patterned mask layer 21 is etched back so that the initial opening t1 retreats in the direction of expanding the opening to form a target opening t2.

[0084] In step S330, Figure 8 As shown, the filling dielectric layer 31 is removed.

[0085] In the above preparation method, a filling dielectric layer 31 is first formed in the isolation trench T, and then the patterned mask layer 21 is etched back. The filling dielectric layer 31 can protect the isolation trench T in the subsequent back-etching process, so that the morphology of the isolation trench T will not be damaged in the back-etching process, and at the same time ensure that the patterned mask layer 21 obtains the required target opening t2 size in the back-etching process, which is helpful for the formation of steps in the subsequent process steps.

[0086] The present embodiment of the application does not specifically limit the constituent material of the filling dielectric layer 31 formed in the above step S310. In some embodiments, the constituent material of the filling dielectric layer 31 may include at least one of an oxide filling material and an organic filling material.

[0087] The oxide filling material may be, for example, an oxide (SiO x ) material or doped oxide material, etc., but not limited thereto; a thin film deposition process can be used to deposit an oxide filling material in the isolation trench T as the filling dielectric layer 31. The organic filling material can be, for example, a bottom anti-reflective coating (Bottom Anti-Reflective Coating, referred to as BARC) material or a spin-on carbon (Spin-On Carbon, referred to as SOC) material, but not limited thereto; a spin coating process can be used to spin-coat an organic filling material in the isolation trench T as the filling dielectric layer 31.

[0088] As an example, on the basis of the above steps, a chemical mechanical planarization (CMP) process or other planarization processes can be used to planarize the top surface of the filling dielectric layer 31 to achieve precise flatness and uniformity, thereby ensuring that subsequent back-etching process steps can be performed on a flat surface, improving the processing accuracy of subsequent back-etching steps, and reducing the generation of defects, which is conducive to more accurately defining the morphology of the target opening t2.

[0089] For example, Figure 6 As shown, the top surface of the filling dielectric layer 31 can be flush or substantially flush with the interface between the gate dielectric layer 22 and the patterned mask layer 21. In this way, it can be ensured that the top surface of the filling dielectric layer 31 is higher than the surface of the substrate 11, thereby providing a better protection effect for the isolation trench T and preventing the morphology of the isolation trench T from being damaged during the back etching process.

[0090] In some embodiments, Figure 5 As shown, a filling dielectric material layer 31' is first formed to fill the isolation trench T and cover the patterned mask layer 21, and then Figure 6 As shown, the filling dielectric material layer 31 ′ is etched back to remove a portion of the filling dielectric material layer 31 ′, and ensure that the top surface of the remaining filling dielectric material layer 31 ′ is not lower than the surface of the substrate 11 , as the filling dielectric layer 31 .

[0091] The embodiment of the present application does not specifically limit the manner of etching back the patterned mask layer 21 in step S300. In some embodiments, a wet etching process may be used to etch back the patterned mask layer 21. Using a wet etching process to etch back the patterned mask layer 21 can more accurately control the rate and direction of the etching back process, thereby effectively expanding the size of the initial opening t1, so that the rounding of the top angle of the side wall of the isolation trench T in the subsequent process can be more uniform.

[0092] As an example, the etch-back process involved in step S300 may include a pull-back process. The pull-back process can achieve partial etching of the current layer material (i.e., the patterned mask layer 21), so that the sidewall of the current patterned mask layer 21 shrinks or retreats inward, thereby exposing a larger area of ​​the underlying material, so as to facilitate the control of the subsequent etching steps, such as the step of etching the step in step S400, so that it can more accurately define tiny structural features.

[0093] It should be noted that the embodiment of the present application does not specifically limit the time of performing the above step S330. For example, after performing step S400 and etching the step at the top corner of the sidewall of the isolation trench, the filling dielectric layer 31 can be removed.

[0094] In step S400, refer to Figure 8 Based on the target opening t2, a step S is etched at the top corner of the sidewall of the isolation trench T.

[0095] In step S500, refer to Fig. 9 , the step S is rounded, and an isolation dielectric layer 51 is formed in the isolation trench T after the rounding process. Fig.10 shown.

[0096] In some embodiments, Fig. 9 As shown, the process of rounding the step S may include the following steps:

[0097] A passivation layer 52 is formed on the inner wall of the isolation trench T, and the passivation layer 52 also covers the step S.

[0098] The present application embodiment does not specifically limit the constituent material of the passivation layer 52 formed in the above steps. In some embodiments, the passivation layer 52 and the isolation dielectric layer 51 may have the same constituent material. That is, the isolation dielectric layer 51 may be formed using the same constituent material as the passivation layer 52. Using the same constituent material as the passivation layer 52 as the isolation dielectric material can ensure that in the subsequent heat treatment and use process, there will be no inconsistency in stress or interface effects due to differences in constituent materials, thereby improving the production yield and use reliability of the trench isolation structure.

[0099] Similarly, the passivation layer 52 may be formed of the same material as the gate dielectric layer 22. For example, the gate dielectric layer 22, the passivation layer 52 and the isolation dielectric layer 51 may have the same material to further improve the production yield and reliability of the trench isolation structure.

[0100] The present embodiment of the application does not specifically limit the material of the isolation dielectric layer 51. As an example, the constituent material of the isolation dielectric layer 51 may include but is not limited to oxide materials (such as silicon dioxide).

[0101] In some embodiments, a furnace tube process may be used to form a liner oxide layer on the inner wall of the isolation trench T, and the liner oxide layer is used as the passivation layer 52. The difference in consumption of substrate materials by the furnace tube process makes the top angle of the side wall of the isolation trench T smoother under the action of the step and can extend downward to a certain extent, so that the top angle of the side wall of the isolation trench T has better smoothness, further reduces electric field concentration, and improves the increase of parasitic capacitance and parasitic resistance.

[0102] It can be understood that in the aforementioned step of back-etching the patterned mask layer 21, the side wall of the patterned mask layer 21 is retreated in the direction of expanding the initial opening t1. The specific expansion size of the initial opening t1 here can be determined by referring to the thickness of the substrate material consumed in the above-mentioned process of forming the passivation layer 52, and the present application does not make any specific limitation on this.

[0103] Based on the same inventive concept, the embodiment of the present application also provides a semiconductor structure on the other hand. The semiconductor structure has a trench isolation structure, and the trench isolation structure is prepared by the preparation method of the self-aligned trench isolation structure provided in the above embodiment. Therefore, the technical effects that can be achieved by the preparation method of the above self-aligned trench isolation structure can also be achieved by the semiconductor structure, which will not be repeated here.

[0104] It can be understood that the specific definition of the semiconductor structure can refer to the definition of the preparation method of the self-aligned trench isolation structure mentioned above, and the technical features between the method embodiment and the structural embodiment can also be replaced and supplemented with each other without conflict, so that those skilled in the art can understand the technical content of this application. No further details will be given here.

[0105] In addition, those skilled in the art will understand that Fig.10 The structure shown is merely a schematic diagram of some layers and / or parts related to the scheme of the present application, and does not constitute a limitation of the scheme of the present application. The specific semiconductor structure may include more layers and / or parts than those shown in the figure, or combine certain layers and / or parts, or have a different arrangement.

[0106] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features of the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0107] The above-described embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be construed as limiting the scope of the patent application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent application shall be subject to the attached claims.

Claims

1. A method for preparing a self-aligned trench isolation structure, characterized in that: The steps include: Providing a substrate, and forming a mask material layer on one side of the substrate; Etching an initial opening in the mask material layer, and etching an isolation trench in the substrate based on the initial opening, and retaining the mask material layer as a patterned mask layer; Etching back the patterned mask layer so that the initial opening retreats in a direction of expanding the opening to form a target opening; Based on the target opening, etching a step at a top corner of a sidewall of the isolation trench; The step is rounded, and an isolation dielectric layer is formed in the isolation trench after the rounding.

2. The method for preparing a self-aligned trench isolation structure according to claim 1, characterized in that: The patterned mask layer is etched back using a wet etching process.

3. The method for preparing a self-aligned trench isolation structure according to claim 1, characterized in that: The mask material layer includes a nitride material layer.

4. The method for preparing a self-aligned trench isolation structure according to claim 1, characterized in that: The etching back of the patterned mask layer comprises the following steps: forming a filling dielectric layer in the isolation trench, wherein the top surface of the filling dielectric layer is not lower than the surface of the substrate; Etching back the patterned mask layer so that the initial opening retreats in the direction of expanding the opening to form the target opening; The filling medium layer is removed.

5. The method for preparing a self-aligned trench isolation structure according to claim 4, characterized in that: The constituent material of the filling dielectric layer includes at least one of an oxide filling material and an organic filling material.

6. The method for preparing a self-aligned trench isolation structure according to claim 1, characterized in that: A gate dielectric layer is also formed between the patterned mask layer and the substrate.

7. The method for preparing a self-aligned trench isolation structure according to claim 1, characterized in that: The step of rounding the steps comprises the following steps: A passivation layer is formed on the inner wall of the isolation trench, and the passivation layer also covers the step.

8. The method for preparing a self-aligned trench isolation structure according to claim 7, characterized in that: The passivation layer and the isolation dielectric layer have the same constituent material.

9. The method for preparing a self-aligned trench isolation structure according to claim 7, characterized in that: The step of forming a passivation layer on the inner wall of the isolation trench comprises the following steps: A furnace tube process is adopted to form a liner oxide layer on the inner wall of the isolation trench, and the liner oxide layer is used as the passivation layer.

10. A semiconductor structure, characterized in that: The semiconductor structure has a trench isolation structure, and the trench isolation structure is prepared by the method for preparing a self-aligned trench isolation structure according to any one of claims 1 to 9.