Additive manufacturing magnetic sheet, laminated core and motor
By designing discrete structures of multiple material components and transition areas in magnetic sheets and adapting to different thermal expansion coefficients, the problem of warping or cracking of magnetic sheets at high speeds is solved, achieving higher strength and less stress Magnetic sheets are suitable for laminated cores and motors of high-efficiency motors.
Patent Information
- Application Number
- CN202380036345.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-05-31
- Filing Date
- 2023-04-19
- Publication Date
- 2024-12-06
AI Technical Summary
Existing magnetic sheets are prone to warping or cracking at high speeds, resulting in deterioration of mechanical or magnetic properties, mainly due to the inherent stress problems caused by the differences in thermal expansion coefficients of different material components.
At least two material components are designed in a magnetic sheet, the first material group is distributed in the radial inner region, the second material group is distributed in the radial outer region, and a transition region is provided between the two, in which the transition region exists. Discrete partial areas are arranged in a row along the radial direction to adapt to different coefficients of thermal expansion and optimized structures by finite element calculations to minimize stress.
Higher strength and less intrinsic stress of the magnetic sheet are achieved, mechanical stress caused by differences in thermal expansion coefficients are reduced, and stability and magnetic properties of the magnetic sheet are improved.
Smart Images

Figure CN119095684A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an additively produced magnetic sheet material according to claim 1 , a laminated core according to claim 14 and an electric machine according to claim 15 . Background Art
[0002] Screen printing or stencil printing is a new process for producing magnetic sheets for electric machines. Here, a printing paste is printed onto a substrate with the aid of a stencil, in which the opening areas can also be provided with a screen. This is called stencil printing or screen printing, stencil printing being a general term for screen printing. In addition to solvents and / or binders, the printing paste also contains metal powder, which has a functional effect in the subsequent component. Production of green blanks by screen printing technology After further heat treatment, the green compact is usually first debound and then subjected to a sintering process at a higher temperature, wherein the metal powder particles are sintered to one another, so that a structured sheet, ie a magnetic sheet, is formed.
[0003] In order to achieve a higher mechanical strength of such sheets, in particular at high rotational speeds of motor rotors, the manufacturability of two-component magnetic sheets is now becoming increasingly important. An example of this is described in EP 3723249 A1. In addition, EP 3 629 453 A1, EP 3 932 591 A1 and EP 3 725 435 A1 should also be mentioned here. The basic problem in such two-component magnetic sheets produced in a template printing process is that different materials, if they have good magnetic properties on the one hand and high strength on the other hand, usually have different coefficients of thermal expansion. For example, for the mechanical strength of the magnetic sheet, high-strength steel is a partial component, whose coefficient of expansion is 16×10 -6 K -1 Another soft magnetic material has a 10×10 -6 K -1 Up to 12×10 -6 K -1 When such different material components or material pairs are co-sintered in a green billet into a magnetic sheet, high mechanical stresses will form in the connection area or seam area between these material components due to these different thermal expansion coefficients, especially during the cooling process from the sintering temperature to room temperature. This may lead to warping or cracking of the magnetic sheet or overall mechanical stresses, which can significantly deteriorate the mechanical or magnetic properties. Summary of the invention
[0004] The technical problem to be solved by the present invention is to provide a magnetic sheet and to produce a laminated core and an electric machine therefrom, wherein the magnetic sheet has higher strength and less inherent stress than in the prior art by using at least two material components in the magnetic sheet.
[0005] The solution to the above-mentioned technical problem consists in a magnetic sheet having the features of claim 1 , a laminated core having the features of claim 14 and an electric machine having the features of claim 15 .
[0006] Claim 1 describes an additively manufactured magnetic sheet for a laminated core of an electric machine, wherein at least two material components are present which are separated from one another in a two-dimensional extension, characterized in that
[0007] - the first material component is arranged in a radially inner region of the magnetic sheet and the second material component is arranged in a radially outer region, and
[0008] a transition region is provided between the radially inner region and the radially outer region, in which transition region both the first material component and the second material component are present in discrete partial regions, wherein
[0009] The discrete partial regions are arranged in a row in the radial direction, so that a line following the radius intersects at least two discrete partial regions.
[0010] The advantage of the magnetic sheet described above is that, on the one hand, a material region with very good magnetic properties can be locally expressed by local material design, and on the other hand, a material region with very high mechanical strength can be expressed. In one or more transition regions, both material components exist in the form of discrete partial regions. The discrete partial regions are arranged along the line following the radius so that the line intersects with at least two partial regions. This means that the partial regions repeat in the radial direction and strengthen their effect and improve the connection between the two material components. The transition region with the discrete partial regions described respectively of each material component is particularly suitable for adapting different thermal expansion coefficients to each other. In the case of the discrete partial regions described in its planar extension, the absolute expansion itself during heating during operation or during sintering shrinkage is smaller than in the larger region (i.e., the radial inner region and the radial outer region). By, for example, using finite element calculations, the appropriate structure of the discrete partial regions in the transition region can be determined, and therefore the stress in the magnetic sheet can also be minimized by applying the described finite element method. In addition, the longer boundary lines alternating in different directions caused by the discrete partial regions offset the mechanical stress caused by different thermal expansion coefficients.
[0011] Discrete partial regions are understood here to mean that there is no mixture of the individual material components in the transition region, but that there are segmented regions in the transition region, in which the first material component and the second material component are separated from each other, i.e., discrete. Therefore, discrete regions can be formed by the first material component and the second material component. These discrete regions can exist adjacent to each other in the transition region. Here, the discrete regions can be directly connected discretely to the corresponding material regions corresponding thereto, i.e., the inner or outer regions. That is, the discrete regions with the material components grow from their corresponding regions into another material component, but the discrete regions exist in a discrete manner relative to the other material component.
[0012] Here, the individual material components in the transition region can be arranged continuously in the inner or outer region, or can be present as islands within the respective other material component. The transition region with the respectively described discrete partial regions of the individual material components is particularly suitable for adapting different thermal expansion coefficients to one another. In the case of the described smaller discrete partial regions, the absolute expansion during heating during operation or during sintering shrinkage is itself smaller than in larger regions. By calculations, for example using finite elements, a suitable structure of the discrete partial regions in the transition region can be determined, so that stresses in the magnetic sheet can also be minimized by applying the described finite element method.
[0013] In particular, when island-shaped discrete partial regions are formed in the transitional printing region, it is costly in terms of process technology to press a material component into the already printed material component. In this case, it may be appropriate to use a non-printing additive manufacturing process, in particular a spraying process, to form the second printing material front component, in particular in the island region.
[0014] In a preferred design, the magnetic sheet is designed so that, in the boundary region between the first material component and the second material component, there is a diffusion zone in the transition region, which extends at least 50 μm into the corresponding other material component. This specifically introduced diffusion zone is wider than the diffusion zone that usually exists in the co-sintering process of two different material components. The wider diffusion zone causes further adjustment of different expansion coefficients.
[0015] It has proven to be suitable if the surface proportion of the first material component in the transition region is between 5% and 40%. The ratio between the first material component and the second material component in the transition region is such that thermally induced stresses are well reduced.
[0016] Depending on the expansion of the magnetic sheet and therefore on the diameter of the laminated core and the motor rotor, it is appropriate that the transition region has a radial extension of between 1 mm and 30 mm. Preferably, the transition region has a radial extension that is between 3 mm and 10 mm along the radius of the magnetic sheet. The discrete region has a maximum extension of between 0.5 mm and 10 mm. "Maximum extension" is understood here to be the maximum straight line that can be stretched within the discrete region without leaving the region.
[0017] It is also advantageous if a plurality of discrete partial regions of at least one material component intersect in such a way that at least one discrete partial region of the respective other material component is enclosed thereby. Such a fence-like structure is particularly suitable for establishing a mesh between the individual material components and thereby minimizing the influence of different expansion coefficients.
[0018] In another embodiment of the invention, the second material component is an iron alloy having at least 95% by weight, in particular at least 97% by weight, and very particularly preferably at least 99% by weight of iron. Ideally, this is pure iron, since pure iron has an optimal ferrite structure or martensite structure and has very good soft magnetic properties, which facilitates corresponding repeated magnetization in the electric machine.
[0019] The first material component in the radially inner region of the magnetic sheet is preferably designed to have the highest possible strength and to withstand the mechanical loads acting on the magnetic sheet. For this purpose, a chromium-nickel alloy is suitable as the starting material for the first material component. The chromium-nickel alloy preferably has a chromium content of between 22% by weight and 28% by weight, in particular between 24% by weight and 26% by weight.
[0020] In a suitable embodiment of the invention, the nickel content is between 4% by weight and 10% by weight, in particular between 6% by weight and 8% by weight, wherein the critical values are respectively contained in the stated ranges. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Further embodiments of the invention and further features of the invention are apparent from the following drawings, which are purely schematic representations and do not represent a limitation of the scope of protection.
[0022] Here in the attached figure:
[0023] Figure 1 An exploded representation of an electrical machine in the form of an electric motor is shown;
[0024] Figure 2A laminated core for a rotor is shown;
[0025] Figure 3 A top view of a magnetic sheet having regions of different materials is shown;
[0026] Figure 4 Shows Figure 3 A magnified fragment in the region of the transition zone between two material components;
[0027] Figure 5 Shows Figure 4 A magnified representation of the transition region in ;
[0028] Figures 6 to 10 Different designs of discrete regions in the transition region are shown;
[0029] Fig.11 Shows Figure 6 , Figure 7 , Fig. 9 An enlarged representation of fragment XII in FIG. 1 , showing the boundary region with the diffusion zone. DETAILED DESCRIPTION
[0030] exist Figure 1 1 shows an exploded representation of an electric machine 6, for example for an electric vehicle, here in the form of an electric motor. The individual components of the electric machine 6 will not be discussed further at this point. However, a rotor 30 is shown which is mounted on a shaft 32. The rotor 30 here comprises a laminated core 4 which is arranged on a Figure 2 30 , wherein the laminated core 4 is composed of individual magnetic sheets 2 in a stacked manner. In the installed position of the rotor 30 , the laminated core 4 is surrounded by a winding which is not shown here.
[0031] exist Figure 3 , a top view of a magnetic sheet 2 is shown, which has two regions, namely a radially inner region 12 and a radially outer region 14. Here, the radially inner region 12 comprises a first material component 8 and the radially outer region 14 comprises a second material component 10.
[0032] Here, the first material component 8 is designed to exhibit a high bearing strength of the magnetic sheet 2. For example, a chromium-nickel-based high-alloy steel is provided for this purpose. The first material component 8 is preferably, but not necessarily, a chromium-nickel alloy having, for example, 25% by weight of chromium and here 7% by weight of nickel. This alloy is a stainless steel alloy with very high strength. The first material component 8, which forms the radial inner region 12 of the magnetic sheet 2, is responsible for the strength of the magnetic sheet 2, especially as a bearing structure, especially at high rotational speeds. In contrast, the second material component 10 is designed as a magnetic material component, especially a soft magnetic component. The second material component has a very high iron content, which preferably exceeds 95% by weight, and very particularly preferably exceeds 99% by weight. Such a high iron content (ideally pure iron) leads to a ferrite material structure, which has particularly good soft magnetic properties. This pure iron structure makes it very easy to re-magnetize, wherein the hysteresis losses are very low in the re-magnetization of the material.
[0033] The production of such a magnetic sheet 2 can be particularly well represented by a stencil printing process or a screen printing process. The screen printing process is a subtype of the stencil printing process, in which a stencil is placed on a substrate and a printing paste is printed onto the substrate through the opening area of the stencil with the aid of a doctor blade. In the screen printing process, the opening area of the stencil is constructed from a fine screen, thereby achieving more favorable rheological effects.
[0034] In screen printing, the described regions, i.e. the radially inner region 12 and the radially outer region 14, are printed one after another using different printing pastes. Here, the first printing paste, which comprises the inner region 12 or the first material component 8, has material particles which become the first material component 8 after the sintering process. That is, in addition to the organic binder, the first printing paste also has metal particles as functional components, which contain the material composition and alloying elements of the first material component. Conversely, the second printing paste (forming the subsequent second material component 10) has metal particles of alloying elements from the second material component 10 in addition to the organic binder.
[0035] For example, in order to produce a magnetic sheet 2, a first printing paste for the inner region 12 is first printed. The substrate with the printing paste is preferably dried briefly, and in a second printing step, the outer region 14 is printed using an additional template, which leaves the outer region 2 of the magnetic sheet 14. Thus, the preparatory stage of the outer region 14 is printed. This is followed by a further drying step to reach a green blank and, if necessary, integrated into a process step, i.e., a degreasing step. Here, organic binders and printing aids are thermally decomposed from the printed printing paste. After degreasing, the brown blank produced in this way essentially still has only functional material particles of the corresponding material components. This is followed by a sintering step, in which the brown blank is sintered into a magnetic sheet 2. Sintering involves a heat treatment process in which particles that are attached to each other form an integral connection through a diffusion process. Here, molten phases may occur locally, but these molten phases do not dominate.
[0036] During the sintering of metallic materials, such as the current magnetic sheets, the temperatures are usually between 900°C and 1400°C.
[0037] The magnetic sheets 2 produced in this way are optionally further processed and stacked to form a laminated core, such as in Figure 2 As shown in. Figure 2 The magnetic sheets 2 in the laminated core 4 do not have Figure 3 Different material areas are shown. Therefore, Figure 2 It is only used to illustrate the laminated core 4 itself. In addition to the advantages of different material compositions, according to Figure 3 The magnetic sheet 2 has the advantage that it is designed to be thinner by about 80 μm to 200 μm compared to conventional magnetic sheets punched from larger sheets. A thinner magnetic sheet is more beneficial to the magnetic properties and thus to the power density of the motor.
[0038] Figure 4 An enlarged representation of the magnetic sheet 2 in its outer region is shown. Here, the transition region 16 is drawn with a dashed line. The transition region 16 represents the transition between the first material component 8 and the second material component 10. The transition region is Figure 5 Zoom in again, where Figure 5 In the example, discrete partial areas 18 and 18' are drawn. Figures 6 to 10 Its role is discussed in more detail in .
[0039] The transition region 16 is the region where both the first material component 8 and the second material component 10 are present. More precisely, the two material components 8, 10 are not present mixed here, but discrete partial regions 18 are provided, which in turn form a widely discrete material boundary 25 to the respective other material component (see Fig.11 ).
[0040] exist Figures 6 to 10 In the figure, an arrow with the reference numeral 20 is drawn, which points in the radial direction, i.e. follows an arbitrary radius of the magnetic sheet 2 and forms a line 22 there. If the arrow 20 is followed from the inner region 12 to the outer region 14, the line 22 intersects at least two discrete regions 18. This means that along the transition region 16 there are multiple changes between the first material component and the second material component in the form of discrete regions 18, 18'. In this way, the stresses caused by the different thermal expansion coefficients are reduced. In this way, the entire boundary line 34 between the first material component 8 and the second material component 10 is raised as a whole and directed in a plurality of different directions, so that the stresses that occur can offset each other.
[0041] It may also be suitable here for discrete regions 18 of a material component 8, 10 to surround discrete regions 18' of the respective other material component 8, 10, such as in Figure 6 and Figure 8 In these figures, this is depicted in the form of a fence-like structure of discrete areas 18, 18'. Figure 8 In the embodiment, the discrete regions 18 of the first material component 8 are configured in a rod-shaped, elongated manner, and the discrete regions 18' formed by the second material component 10 are configured in the form of rectangular surfaces with a low aspect ratio. Figure 6 Also shown is a discrete region 18 containing a discrete region 18', wherein Figure 8 Compared with the situation Figure 6 Involving fewer right-angle design options.
[0042] The discrete regions 18 and 18' described in the previous paragraph can also be designed to be complementary in terms of the first material component 8 and the second material component 10. In this case, the discrete region 18 can be directly connected to the corresponding material component 8, 10, which is present in the inner region 12 or the outer region 14, for example, Figure 6 and Figure 8 As shown in , or the discrete regions can be spaced apart from each other, as for example in Fig. 9 , Fig.10 and Figure 7 As shown in . Figure 7 A hybrid is depicted here, with some discrete regions 18 directly abutting and growing out of corresponding counterpart regions, and other discrete regions being completely separated from the regions.
[0043] It is suitable here to calculate the shape, area extension and size of the discrete regions 18, 18' by means of the finite element method so that the minimum stress is generated under the obtained thermal expansion coefficient. Here, depending on the diameter of the magnetic sheet 2, the transition region 16 is between 1 mm and 30 mm in width, preferably between 3 mm and 10 mm. It has been shown that in such a wide transition region, which extends beyond the microscopic fine structure, the difference in expansion coefficient can be compensated most effectively. In addition, it is suitable here that in the transition region 16, the area share of the first material component is <50%, preferably between 5% and 40%. It is also advantageous, especially in terms of the magnetic properties of the outer region 14, that the area share of the non-soft magnetic first material component is not too large as a whole. In terms of good soft magnetic properties, but also in terms of minimization of thermal stresses, this area share should be located within the described area.
[0044] The term "extensive" is used above when introducing the term "discrete material boundary 25". This means that the material boundary 25 is quite discrete in the macroscopic sense relative to the width of the transition region 16, but in microscopic observation, the width has a diffuse region 26, as shown in FIG. Fig.11 is an enlarged representation of fragment XI. Figure 6 , Figure 7 and Fig. 9 XI is only a schematic diagram of the fragment. This fragment is an example for the entire boundary area 24 between the first material component 8 and the second material component 10 along the boundary line 34. Fig.11 , wherein the second material component 10 extends on the right and the first material component 8 is arranged on the left. A diffusion zone 26 is located between the two material components 8, 10, which diffusion zone usually has an expansion of >50 μm. In the conventional boundary region between two materials, although ion diffusion from one material region to the other and vice versa can basically occur during the sintering process, attempts are conventionally made to keep this influence as low as possible by process technology measures. However, according to Fig.11 The diffusion zone 26 is designed to be significantly wider than a conventional diffusion zone, which can be achieved by a correspondingly higher temperature or duration of the sintering process. To achieve this, it is suitable, for example, to increase the temperature by 50 K-100 K and / or to extend the holding time at the maximum sintering temperature by 30 minutes to 2 hours compared to the temperature or time actually required for the sealing sintering. The diffusion zone between the material components widened in this way also helps to reduce the stresses caused by different thermal expansion coefficients.
[0045] Reference numerals list
[0046] 2 Magnetic sheet
[0047] 4-Laminated Core
[0048] 6 Motor
[0049] 8. First Material Component
[0050] 10 Second Material Component
[0051] 12 Radial inner area
[0052] 14 Radial outer area
[0053] 16 Transition Zone
[0054] 18 Discrete Partial Areas
[0055] 20 Radial direction
[0056] 22 lines
[0057] 24 Border Area
[0058] 25 Material Boundary
[0059] 26 Diffusion Zone
[0060] 28 radial extension
[0061] 30 rotors
[0062] 32 Axis
[0063] 34 Boundary Line
Claims
1. An additively manufactured magnetic sheet (2), the magnetic sheet being used for a laminated core (4) of an electric motor (6), in, There are at least two material components (8, 10) separated from one another in two-dimensional extension, characterized in that - the first material component (8) is arranged in a radially inner region (12) of the magnetic sheet (2) and the second material component (10) is arranged in a radially outer region (14), and a transition region (16) is provided between the radially inner region (12) and the radially outer region (14), in which the first material component (8) and the second material component (10) are present in discrete partial regions (18), wherein The discrete partial regions (18) are arranged in a row in a radial direction (20) such that a line (22) following a radius intersects at least two discrete partial regions (18).
2. The magnetic sheet according to claim 1, It is characterized in that In a boundary region (24) between the first material component (8) and the second material component (10), a diffusion zone (26) is present in the transition region (16), which extends at least 50 μm into the respective other material component (8, 10).
3. The magnetic sheet according to claim 1 or 2, It is characterized in that In the transition region (16), the area fraction of the first material component (8) is between 5% and 40%.
4. The magnetic sheet according to any one of the preceding claims, It is characterized in that The transition region (16) has a radial extension (28) of between 1 mm and 30 mm.
5. The magnetic sheet according to any one of the preceding claims, It is characterized in that The discrete areas have a maximum extension between 0.5 mm and 10 mm.
6. The magnetic sheet according to claim 5, It is characterized in that The transition region (16) has a radial extension (28) of between 3 mm and 10 mm.
7. The magnetic sheet according to any one of the preceding claims, It is characterized in that A plurality of discrete partial regions (18) of at least one material component (8, 10) intersect in such a way that at least one discrete partial region (18') of the respective other material component (8, 10) is enclosed thereby.
8. The magnetic sheet according to any one of claims 1 to 7, It is characterized in that The first material component (8) comprises an iron alloy having an austenitic structure of at least 25% by volume.
9. The magnetic sheet according to any one of claims 1 to 8, It is characterized in that The second material component (10) comprises an iron alloy having at least 95% by weight, in particular at least 97% by weight, of iron.
10. The magnetic sheet according to claim 9, It is characterized in that The second material component (10) has a ferrite or martensite structure.
11. The magnetic sheet according to any one of claims 1 to 10, It is characterized in that The first material component (8) is a chromium-nickel alloy.
12. The magnetic sheet according to claim 11, It is characterized in that The first material component (8) is an iron-chromium alloy having a chromium content of between 22% by weight and 28% by weight, in particular between 24% by weight and 26% by weight.
13. The magnetic sheet according to claim 9 or 12, It is characterized in that The first material component (8) has a nickel content of between 4% by weight and 10% by weight, in particular between 6% by weight and 8% by weight.
14. A laminated core for a rotor (30) of an electric machine (6), the laminated core comprising a plurality of magnetic sheets (2) according to any one of claims 1 to 13.
15. An electric machine comprising the laminated core (4) according to claim 14.