A method for producing a polymer leading edge protector with chamfered side edges and a wind turbine blade having the polymer leading edge protector.

By using roller processing technology to form a polymer leading edge protection sheet with chamfered side edges, the problem of unevenness on the outer surface of wind turbine blades is solved, achieving higher smoothness and corrosion resistance.

CN120476253BActive Publication Date: 2026-11-17POLITECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202480006797.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2023-02-08
Filing Date
2024-01-05
Publication Date
2026-11-17
Estimated Expiration
2044-01-05

AI Technical Summary

Technical Problem

In the production of polymer leading edge protection sheets for wind turbine blades, the existing technology results in uneven outer surfaces, leading to insufficient smoothness of the film and an inability to effectively prevent erosion.

Method used

The polymer material sheet is processed using at least one pair of rollers. The thickness of the sheet is changed by the forming surface of the rollers to form a polymer leading edge protection sheet with chamfered side edges, ensuring the smoothness and precise shape of the surface profile.

Benefits of technology

A smoother surface profile was achieved, improving the corrosion resistance of the polymer leading edge protector, making it suitable for the protection of wind turbine blades.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120476253B_ABST
    Figure CN120476253B_ABST
Patent Text Reader

Abstract

This article discloses a method for producing a polymer leading edge protector with chamfered side edges, the polymer leading edge protector obtained by the method, and a wind turbine blade having the polymer leading edge protector.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a method for producing polymer leading edge protectors with chamfered side edges for use in wind turbine blades. Background Technology

[0002] For example, rotor blades in wind turbines, helicopters, and other similar applications are subjected to varying environmental conditions, including erosion caused by impacts from airborne materials such as rain, sand, dust, and other debris. The leading edge of wind turbine blades is particularly vulnerable to erosion. As rotor blades become longer, their tip velocities increase, and as wind turbines are erected in increasingly harsh and remote locations—including offshore sites—leading edge erosion becomes an even greater problem.

[0003] Industrially, methods such as membranes and coatings have been sought to prevent this erosion. In some examples, prefabricated sections made of a robust yet flexible polymer shell have been applied to the leading edge of wind turbine blades. The shell is designed and sized to absorb the kinetic energy from rain, hail, and airborne particles. Thus, the shell provides optimal protection for the rigid fiberglass surface of the blade.

[0004] In some examples, the membrane is applied to the leading edge of a wind turbine blade, wherein the membrane is applied around the leading edge of the wind turbine blade and adhered to the blade by an adhesive. The outermost surface of the commercial membrane is typically planar, and in its most basic configuration, the outermost surface of the commercial membrane comprises a polymer membrane as a protective layer and an adhesive layer for attachment to the wind turbine blade. Some membranes have an overall profile of the outer top surface of the membrane that is convexly curved or convexly trapezoidal.

[0005] Forming the outer top surface typically involves using a cutter to shape the surface after production. However, this results in an uneven outer surface on the membrane.

[0006] Therefore, there is a need for an improved method for producing polymer leading edge protectors for wind turbine blades, which provide improved smoothness to the film on the outer surface. Summary of the Invention

[0007] This article discloses, in its first aspect, a method for producing polymer leading-edge protectors with chamfered side edges for use in wind turbine blades. The term "wind turbine" refers to a wide range of wind turbine sizes.

[0008] The method includes the following steps:

[0009] - Provides a polymer material sheet including a first main surface and a second main surface, each main surface having a width extending in a width direction between the side edges of the polymer material sheet, wherein the first main surface and the second main surface are oriented oppositely, wherein the polymer material sheet has a thickness, and - the polymer material sheet is formed into a polymer leading edge protection sheet by disposing the polymer material sheet between at least a pair of rollers.

[0010] At least one pair of rollers includes a first roller and a second roller, wherein:

[0011] The first roller includes a first forming surface extending between opposite ends of the first roller, wherein the first forming surface extends recessively between the opposite ends;

[0012] The second roller includes a second forming surface extending between opposite ends of the second roller;

[0013] The first forming surface and the second forming surface are arranged opposite to each other; and

[0014] During the rotation of the first and second rollers, the thickness of the polymer material sheet is changed by means of the forming surface of the rollers to obtain a polymer leading edge protection sheet with chamfered side edges. The polymer leading edge protection sheet has a reduced thickness at the side edges compared to the sheet thickness in the central region.

[0015] The term "recessed extension of the first forming surface" means that at least a portion of the middle section of the first roll has a smaller diameter than the end section of the first roll. The roll may have a continuously decreasing diameter when measured from the side edge toward the center of the roll. Alternatively, the roll may have a continuously decreasing diameter when measured from the side edge toward a middle section spanning a certain width of the roll, for example, a middle section spanning 10% of the roll width.

[0016] By using at least one pair of rollers to modify and shape the polymer leading edge protector sheet, a polymer leading edge protector sheet with a specific surface profile can be obtained by selecting the roller forming surfaces to match requirements. This provides a smoother surface profile on the polymer leading edge protector sheet compared to methods that form a polymer leading edge protector sheet with chamfered edges by removing a portion of the polymer leading edge protector sheet after production. The use of rollers ensures that the polymer leading edge protector sheet accurately obtains the desired surface profile shape because cooling of the polymer leading edge protector sheet is allowed during the process of providing the polymer material sheet between at least one pair of rollers. Furthermore, the above method provides an improved method for producing polymer leading edge protector sheets with improved smoothness on the outer surface due to the use of at least one pair of rollers.

[0017] The recessed first forming surface can be curved. Therefore, in one or more examples, the first forming surface of the first roller is curved. Curved means that the surface deviates from a straight or planar surface without sharp breaks or angles.

[0018] In the second aspect, this article discloses a polymer leading edge protection sheet obtained according to the above method.

[0019] In a third aspect, this article discloses a wind turbine blade having a polymer leading edge protection sheet according to the above description.

[0020] The polymer material sheet can be obtained in several ways. One way is to melt the granular material and form it into a material sheet. Therefore, in one or more examples, the method further includes:

[0021] - By melting granular polymer materials through an extrusion process, a molten polymer material with a predetermined hardness is obtained, thereby obtaining a plasticized polymer material; and

[0022] - Plasticized polymer material is pressed using a flat die to form a polymer sheet.

[0023] After the plasticized polymer material is pressed by a flat die, it can be pulled through rollers to form a polymer sheet.

[0024] During extrusion, granular polymer materials (such as thermoplastic polyurethane) are softened and melted by the frictional heat generated from compression of the material using a screw or screw shaft rotating within the extruder barrel. During the extrusion process, the granular polymer material is heated and obtained at elevated temperatures to produce a plasticized polymer material. The plasticized polymer material can be maintained at elevated temperatures within a die using one or more electrically heated zones, ensuring that the plasticized polymer material remains in a moldable / plasticized state.

[0025] Before melting the granular polymer material, the granular polymer material can be dried to reduce or remove any moisture. Therefore, in one or more examples, the method further includes providing the granular polymer material and drying it to a moisture level of 0.02 wt% or less before melting it. Drying can be performed, for example, by air drying in a desiccant air dryer.

[0026] In one or more examples, the polymer material is a polyurethane material. The polyurethane material can be a thermoplastic polyurethane material. Therefore, in one or more examples, the polymer front-edge protector is a polyurethane front-edge protector. The thermoplastic polyurethane material can contain polyols, chain extenders, and aliphatic isocyanates. The polyurethane front-edge protector can be a thermoplastic polyurethane front-edge protector. The polyurethane can be a commonly used polymer material as the main material in the polymer front-edge protector. However, alternative polymer materials can also be used, including thermoplastic olefins, styrene block copolymers, thermoplastic copolyesters, silicone thermoplastics, silicone polyethylene glycol amide, aliphatic polyether-based thermoplastic polyurethanes, copolyester ethers, crosslinked polyurethanes, polyurea, low-density polyethylene (LDPE), linear low-density polyethylene (LLDPE), styrene-butadiene-styrene block copolymers (SBS), styrene-ethylene-butene-styrene block copolymers (SEBS), and styrene-ethylene / propylene-styrene (SEPS) block copolymers. Combinations of any polymer material are also contemplated.

[0027] In one or more examples, the polymer material is a polyurethane material, and the granular polyurethane material is an aliphatic thermoplastic polyurethane (TPU) made of a polyol such as a difunctional polyol, a butanediol chain extender, and an aliphatic isocyanate. The term "difunctional polyol" means that each molecule of the thermoplastic polyurethane polymer has two reactive groups. Typically, thermoplastic polyurethanes are linear. The aliphatic thermoplastic polyurethane (TPU) can be the commonly used granular polyurethane material. However, alternative granular polymer materials can also be used, including particles of the following: thermoplastic olefins, styrene block copolymers, thermoplastic copolyesters, silicone thermoplastics, silicone polyethylene glycol amide, aliphatic polyether-based thermoplastic polyurethanes, copolyester ethers, crosslinked polyurethanes, polyurea, low-density polyethylene (LDPE), linear low-density polyethylene (LLDPE), styrene-butadiene-styrene block copolymers (SBS), styrene-ethylene-butene-styrene block copolymers (SEBS), and styrene-ethylene / propylene-styrene (SEPS) block copolymers. Any combination of polymer granular materials is also conceivable.

[0028] In one or more examples, the polymeric material is a polyurethane material, and the granular polyurethane material also contains one or more additives, such as UV absorbers, antioxidants, and / or pigments. The amount of additives can vary between 0.1 wt% and 50 wt%. Additives may also include dyes, fillers, stabilizers, or combinations thereof.

[0029] In one or more examples, the polymer material is a polyurethane material, and the granular polyurethane material does not contain a release agent. The release agent can be omitted to ensure a strong bond with the subsequent pressure-sensitive adhesive.

[0030] In one or more examples, the polymer leading edge protector is characterized by the following physical properties:

[0031] - Maximum thickness is between 0.8 mm and 2.0 mm;

[0032] - The Shore A hardness is between 65 and 75, and this Shore A hardness is measured by ISO 868;

[0033] - When measured using ISO 37 / 1A at 23°C, the elongation is greater than 400 mm;

[0034] - The speed of sound is below 1700 m / s, as measured by ISO 16810 and ISO 16811; and

[0035] - Corrosion resistance at 150 m / s for more than 8 hours, measured by DNV-RP-0171.

[0036] In one or more examples, the polymer leading edge protector is characterized by the following physical properties:

[0037] - Maximum thickness is between 0.7 mm and 2.0 mm;

[0038] - The Shore A hardness is between 68 and 78, and this Shore A hardness is measured by ISO 868;

[0039] - When measured using ISO 37 / 1A at 23°C, the elongation is greater than 400 mm;

[0040] - The speed of sound is below 1700 m / s, as measured by ISO 16810 and ISO 16811; and

[0041] - Corrosion resistance at 140 m / s for more than 10 hours, measured by DNV-RP-0171.

[0042] The term "maximum thickness" refers to the maximum thickness on the leading edge protector. The maximum thickness is typically found at the center of the polymer leading edge protector in the width direction. The thickness at the chamfered edge will always be less than the maximum thickness of the polymer leading edge protector. The maximum thickness will generally depend on the material's hardness. Typically, when the material hardness is between 65 and 78, the maximum thickness should be less than 2 mm, most likely less than 1.5 mm, or even less than 1.2 mm.

[0043] In one or more examples, the polymer leading edge protector has a minimum thickness greater than 0.01 mm, such as greater than 0.05 mm, or greater than 0.10 mm. The minimum thickness refers to the smallest thickness on the leading edge protector. This minimum thickness is typically found at the chamfered edge of the polymer leading edge protector. The maximum thickness of the polymer leading edge protector will always be greater than the minimum thickness at the chamfered edge. The minimum thickness will generally depend on the hardness of the material.

[0044] In one or more examples, the polymer leading edge protector has a width in the width direction between the side edges of the polymer leading edge protector, the width comprising a first third and a second third, wherein the first and second thirds are each located near the corresponding side edges of the polymer leading edge protector, wherein a remaining third is arranged between the first and second thirds, and wherein the thickness variation of the polymer leading edge protector in the width direction is greater at the first and second thirds than at the remaining thirds. The thickness variation of the polymer leading edge protector in the remaining thirds corresponds to the thickness variation in the middle segment of the polymer leading edge protector. If the polymer leading edge protector is substantially flat over a larger area surrounding the middle portion of the polymer leading edge protector, the thickness variation in the thirds can be close to zero. If the polymer leading edge protector has a continuously varying thickness profile, where the thickness profile has a maximum value in the middle region of the polymer leading edge protector, then the thickness variation in the remaining three equal divisions will be greater than zero. However, the thickness variation in the remaining three equal divisions will generally be less than the thickness variation in the first and second equal divisions of the polymer leading edge protector.

[0045] In one or more examples, the remaining three equal divisions have a maximum thickness of less than 1.5 mm. Therefore, the polymer leading edge protection sheet may be characterized by a maximum thickness between 0.7 mm and 1.5 mm, for example, between 0.8 mm and 1.5 mm.

[0046] In one or more examples, the remaining three equal divisions have a maximum thickness of less than 1.2 mm. Therefore, the polymer leading edge protection sheet may be characterized by a maximum thickness between 0.7 mm and 1.5 mm, for example, between 0.8 mm and 1.2 mm.

[0047] In one or more examples, the remaining three equal divisions have a maximum thickness of less than 1 mm. Therefore, the polymer leading edge protection sheet may be characterized by a maximum thickness between 0.7 mm and 1.5 mm, for example, between 0.8 mm and 1.0 mm.

[0048] In one or more examples, the first and second ternary sections have a minimum thickness of less than 0.5 mm. Therefore, if the maximum thickness is between 0.7 mm and 1.5 mm, for example between 0.8 mm and 2.0 mm, the difference between the thicknesses of the polymer leading edge protector over the entire width of the sheet can be at least 1.5 mm.

[0049] In one or more examples, the first and second tertiary divisions have a minimum thickness greater than 0.01 mm, such as greater than 0.05 mm, such as greater than 0.10 mm.

[0050] In one or more examples, the polymer leading edge protector has a width in the width direction between the side edges of the polymer leading edge protector, the width comprising a first quarter and a second quarter, wherein the first and second quarters are each located near the corresponding side edges of the polymer leading edge protector, wherein the remaining half is arranged between the first and second quarters, and wherein the thickness variation of the polymer leading edge protector in the width direction is greater at the first and second quarters than at the remaining half. The thickness variation of the polymer leading edge protector in the remaining half corresponds to the thickness variation in the middle segment of the polymer leading edge protector. If the polymer leading edge protector is substantially flat over a larger area surrounding the middle portion of the polymer leading edge protector, the thickness variation in the remaining half can be close to zero. If the polymer leading edge protector has a continuously varying thickness profile, wherein the thickness profile has a maximum value in the middle region of the polymer leading edge protector, the thickness variation in the remaining half will be greater than zero. However, the thickness variation in the remaining half will generally be less than the thickness variation in the first and second quarters of the polymer leading edge protector.

[0051] In one or more examples, the polymer leading edge protector has a Shore A hardness of 78 or less. Shore A hardness is measured according to ISO 868.

[0052] In one or more examples, the polymer leading edge protector has a Shore A hardness of 75 or less. Shore A hardness is measured according to ISO 868.

[0053] In one or more examples, the second forming surface of the second roller extends cylindrically between the opposite ends. "Cylindrical" means that the second roller has a diameter that does not change or only slightly changes along its length. Alternatively, the second forming surface may be slightly convex.

[0054] In one or more examples, the first roller and the second roller each have longitudinal axes (LA1, LA2) extending between their opposite ends, wherein the longitudinal axes (LA1, LA2) are substantially parallel. Therefore, the two rollers can be positioned relative to each other, with equal distances between their two ends. If a polymer leading edge protector with one side edge thinner than the other is associated, the distance between the first and second rollers at one end of the rollers can be slightly greater than the distance between the first and second rollers at the other end of the rollers.

[0055] In one or more examples, the second forming surface of the second roller is smooth. The polymer leading edge protector typically has a flat surface and a curved surface. When the polymer leading edge protector is positioned between the first pair of rollers, the first forming surface of the first roller will typically contact the curved surface of the polymer leading edge protector, and the second forming surface of the second roller will typically contact the flat surface of the polymer leading edge protector. After the polymer leading edge protector as described above is produced, an additional layer, such as an adhesive layer, can be added to the flat surface of the polymer leading edge protector. The smooth second forming surface of the second roller provides a smooth, flat surface on the polymer leading edge protector. If a pressure-sensitive adhesive is applied to the leading edge protector located on its flat surface side after production, it is crucial to maximize the contact area, which is optimally achieved by having a smooth surface with low roughness on the flat surface of the polymer leading edge protector. If high roughness exists on the second roller, the pressure-sensitive adhesive (PSA) applied to the polymer leading edge protector after leaving the roller may only attach itself to the peaks and will not contact the valleys on the surface of the polymer leading edge protector. This means that the total contact area between the polymer leading edge protector and the PSA is less than 100%.

[0056] The extruded leading edge protector sheet can be shaped by pushing thermoplastic material through a flat die tool. The thermoplastic preform can be pulled away from the hot die, onto and through a pair of rollers, cooled, and defined into its final shape. The pulling can be performed by rotating the rollers.

[0057] Guiding the polymer material sheet between the first pair of rollers, i.e., between the first roller and the second roller, can be achieved by pushing or pulling the polymer material sheet. A combination of both pushing and pulling the sheet between the rollers in the first pair of rollers can also be used. Therefore, in one or more examples, forming the polymer material sheet into a polymer leading edge protection sheet is achieved by pulling and / or pushing the polymer material sheet through at least one pair of rollers. The first roller can pull the polymer material sheet through at least one pair of rollers.

[0058] Alternatively, the second roller may be a roller that pulls the polymer material sheet through at least one pair of rollers. Again, alternatively, two of the at least one pair of rollers may pull the polymer material sheet through at least one pair of rollers. Thus, in one or more examples, forming the polymer material sheet into a polymer leading edge protection sheet is achieved by pulling the polymer material sheet through at least one pair of rollers, wherein at least the first roller and / or the second roller pulls the polymer material sheet through at least one pair of rollers.

[0059] In one or more examples, forming a polymer material sheet into a polymer leading edge protection sheet is achieved by pushing the polymer material sheet through at least one pair of rollers, wherein at least a flat die / extruder pushes the polymer material sheet through at least one pair of rollers. The polymer material sheet can be ejected from the flat die by one or more rotating screws. As the polymer material sheet enters the space between the first pair of rollers, the polymer material sheet can be pulled through the rollers at the same speed as additional polymer material sheets delivered by the rotating screws.

[0060] In one or more examples, the polymer material sheet is shaped into a polymer leading edge protector by allowing the polymer material sheet to fall into a cavity between at least one pair of rollers. This process is also known as using a hanger to obtain the shape of the polymer leading edge protector.

[0061] In one or more examples, the method further includes disposing a polymer leading edge protector between a second pair of rollers, the second pair of rollers including a third roller and one of the first and second rollers. The polymer leading edge protector is thus guided first through the first pair of rollers and then through the second pair of rollers. By passing through the second pair of rollers sharing one of the rollers with the first pair of rollers, the polymer leading edge protector will generally follow the roller as it rotates, and is thus guided through the second pair of rollers after leaving the space between the first pair of rollers. The third roller can be similar to either the first or second roller in the sense that it has a similar forming surface. Thus, in the example, the third roller includes a third forming surface extending between opposite ends of the third roller, wherein the third forming surface extends recessedly between the opposite ends. Alternatively, in the example, the third roller includes a third forming surface extending between opposite ends of the third roller, wherein the third forming surface extends cylindrically between the opposite ends.

[0062] Alternatively, the second pair of rollers may include a third roller and a fourth roller, wherein neither the third roller nor the fourth roller is the first roller or the second roller.

[0063] In one or more examples, the first, second, and / or third rollers are cooled. By cooling one or more of the rollers, the polymer leading edge protector entering the first pair of rollers—and possibly subsequently the second pair—cools more rapidly as it passes through the rollers, resulting in an elevated temperature that allows it to form a polymer leading edge protector with chamfered side edges. This improves control over obtaining the desired surface profile shape. Cooling can be achieved by using cooling water circulating inside one or more of the rollers. Alternatively, instead of cooling water, different cooling liquids can be used, such as ethylene glycol.

[0064] The method may also include providing a polymer leading-edge protector through a quality control section that ensures the polymer leading-edge protector meets performance specifications / requirement specifications. This is typically performed after the protector has exited one or more pairs of rollers.

[0065] The method may also include winding the polymer leading edge protector onto one or more rollers before adding the adhesive and / or shortening the polymer leading edge protector. Attached Figure Description

[0066] Various examples are described below with reference to the accompanying drawings. The same reference numerals always refer to the same elements. Therefore, the same elements will not be described in detail for each drawing. It should also be noted that the drawings are intended only to facilitate the description of examples. The drawings are not intended as an exhaustive description of the claimed invention or as a limitation on the scope of the claimed invention. Furthermore, the illustrated examples do not need to possess all the aspects or advantages shown. Aspects or advantages described in connection with a particular example are not necessarily limited to that example and can be practiced in any other example, even if not so illustrated or so explicitly described.

[0067] Figure 1 A system for producing polymer leading edge protection sheets with chamfered side edges is shown.

[0068] Figure 2 A method for producing polymer leading edge protection sheets with chamfered side edges is schematically illustrated.

[0069] Figure 3 The flat mold is shown in a three-dimensional view.

[0070] Figures 4A to 4C The different systems, including the flat die and roller system, are shown in a side view.

[0071] Figures 5A to 5B The diagram shows a first pair of rollers with and without leading edge guards between the rollers.

[0072] Figures 6A to 6C Three different sets of first and second roller pairs are shown.

[0073] Figures 7A to 7D Different examples of leading edge protective sheets with chamfered side edges are shown.

[0074] Figure 8 A system for producing polymer leading edge protection sheets with chamfered side edges is shown. Detailed Implementation

[0075] Exemplary examples will now be described more fully below with reference to the accompanying drawings. In this regard, the examples may take different forms and should not be construed as limited to the description set forth herein. Therefore, the examples are described below only with reference to the accompanying drawings to explain various aspects. As used herein, the term “and / or” includes any and all combinations of one or more of the associated listed items. Expressions such as “at least one of…” when following a list of elements modify the entire list of elements, not the individual elements of the list.

[0076] In the accompanying drawings, the thickness of the multiple layers and regions is illustrated in an enlarged manner for clarity and ease of description. When a layer, region, element, or plate is referred to as being "on top of" another layer, region, element, or plate, the layer, region, element, or plate may be directly situated on the other layer, region, element, or plate, or an intermediate layer, region, element, or plate may exist between the layer, region, element, or plate and the other layer, region, element, or plate. Conversely, when a layer, region, element, or plate is referred to as being "directly situated on" another layer, region, element, or plate, there is no intermediate layer, region, element, or plate between the layer, region, element, or plate and the other layer, region, element, or plate. Furthermore, when a layer, region, element, or plate is referred to as being "below" another layer, region, element, or plate, the layer, region, element, or plate may be directly situated below the other layer, region, element, or plate, or an intermediate layer, region, element, or plate may exist between the layer, region, element, or plate and the other layer, region, element, or plate. Conversely, when a layer, region, element, or board is referred to as "directly below another layer, region, element, or board," there is no intermediate layer, region, element, or board between the layer, region, element, or board and the other layer, region, element, or board.

[0077] For ease of description, spatial relative terms such as “lower” or “bottom” and “upper” or “top”, “below”, “under”, “less”, “above”, etc., may be used herein to describe the relationship between one element or component and another element or component as illustrated in the accompanying drawings. It will be understood that spatial relative terms are intended to cover different orientations of the device in use or operation other than those depicted in the drawings. For example, if the device illustrated in the drawings is flipped, an element described as being “below” or “under” another element will be oriented to be “above” or “below” another element. Thus, the illustrative term “below” or “under” can include both a “lower” orientation and an “upper” orientation, depending on the specific orientation of the figure. Similarly, if the device in one of the figures is flipped, an element described as being “below” or “under” another element will be oriented to be “above” another element. Thus, the exemplary term “below” or “under” can include both upper and lower orientations, and therefore, spatial relative terms can be interpreted differently depending on the described orientation.

[0078] Throughout the specification, when an element is referred to as being “connected” to another element, the element is “directly connected” to another element, or “electrically connected” to another element if one or more intermediate elements are inserted between the element and the other element.

[0079] The terminology used herein is for the purpose of describing particular examples only and is not intended to be limiting. Unless the context clearly indicates otherwise, the singular forms “a,” “an,” and “the” as used herein are intended to include the plural forms, i.e., “at least one.” “At least one” should not be construed as limiting “a” or “an.” It will also be understood that, when used in this specification, the terms “comprising,” “including,” “containing,” and / or “comprising” indicate the presence of the stated feature, integer, step, operation, element, and / or component, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups thereof.

[0080] It will be understood that although the terms “first,” “second,” “third,” etc., may be used in this text to describe various elements, these elements should not be limited by these terms. These terms are only used to distinguish one element from another. Therefore, the “first element” discussed below may be referred to as the “second element” or the “third element,” and without departing from the teachings of this text, the “second element” and the “third element” may also be referred to as the “first element.”

[0081] As used herein, “about” or “approximately” includes the stated value and means within an acceptable range of deviation from the given value, as determined by a person of ordinary skill in the art, taking into account the measurement in question and the errors associated with the measurement of the given quantity (i.e., limitations of the measurement system). For example, “about” may mean within one or more standard deviations, or within ±30%, ±20%, ±10%, ±5% of the stated value.

[0082] Unless otherwise defined, all terms used herein (including technical and scientific terms) shall have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains. It will also be further understood that terms, such as those defined in common dictionaries, shall be interpreted as having meanings consistent with their meanings in the context of the relevant field, and shall not be construed as having idealized or overly formal meanings unless expressly defined herein.

[0083] This document describes exemplary examples with reference to cross-sectional views as idealized examples, wherein the same reference numerals refer to the same elements throughout the specification. Therefore, variations in the illustrated shapes are expected due to, for example, manufacturing techniques and / or tolerances. Consequently, the examples described herein should not be construed as limited to a specific shape of the areas illustrated herein, but rather include, for example, shape deviations due to manufacturing processes. For example, an illustrated or described flat area may have rough and / or non-linear characteristics. Furthermore, acute angles in the illustrations may be rounded. Therefore, the areas illustrated in the figures are schematic in nature, and their shapes are not intended to represent the precise shapes of the illustrated areas, nor are they intended to limit the scope of the claims. For the sake of specifically describing exemplary examples of this disclosure, some parts unrelated to the description may be omitted.

[0084] Figure 1 A system for producing a polymer leading edge protector 120 with chamfered side edges 122 is shown, and Figure 2 The illustration shows the method of use. Figure 1 A method for producing polymer leading edge protection sheets using a systematic approach. Figure 1 The system shown includes an extrusion system 10, a screen system 20, a flat die 50, a roller system 60, a conveyor 70, a quality control section 80, and a pull roller unit 90.

[0085] When producing the polymer leading edge protection sheet 120, the polymer material sheet 106 is provided by placing the polymer material sheet 106 between at least a pair of rollers in the roller system 60 and forming the polymer material sheet 106 into the polymer leading edge protection sheet 120.

[0086] The polymer material sheet 106 can be obtained in a variety of different ways, for example, Figure 1 and Figure 2As shown, the granular polymer material 100 is obtained by melting 202 during the extrusion process in the extrusion system 10 to obtain a molten polymer material 102 with a predetermined hardness, thereby obtaining a plasticized polymer material 104, and then pressing 204 of the plasticized polymer material 104 through a flat die 50 to form a polymer material sheet 106. During the extrusion process, the granular polymer material 100 can be softened and melted by the frictional heat generated by compression and rotation using a screw or screw shaft in the extruder barrel. Before melting 202, the granular polymer material 100 can be air-dried to a moisture level of 0.02 wt% or less in an air dryer.

[0087] like Figure 3 As shown, the polymer material sheet 106 is formed into a polymer leading edge protection sheet 120 by pulling and / or pushing the polymer material sheet 106 through at least one pair of rollers. When the polymer material sheet 106 is pulled through at least one pair of rollers, at least the first roller 610 and / or the second roller 620 pull the polymer material sheet 106 through at least one pair of rollers.

[0088] After obtaining the polymer leading edge protector 120, it can be guided via conveyor 70 through quality control section 80 208, which ensures the performance specifications / requirements of the polymer leading edge protector 120. Then, before adding adhesive and / or shortening the polymer leading edge protector 120, it can be wound 210 onto pull roller unit 90. The polymer leading edge protector 120 can be cut into smaller pieces.

[0089] Figure 3 A portion of the flat mold 50 is shown in a three-dimensional view. Figures 4A to 4C In the diagram, a flat die 50 is shown in a side view along with three different roller systems 60. The flat die 50 includes an inlet channel 502 through which the plasticized polymer material 104 is guided via a side surface 504 onto a flat outlet channel 506. The polymer material sheet 106 exits the flat die 50 at a departure edge 508 of the flat outlet channel. The plasticized polymer material 104 is maintained at an elevated temperature within the flat die 50 by an electrically heated zone 510, ensuring that the plasticized material remains in a moldable / plasticized state.

[0090] Figure 4AThe illustrated roller system 60 includes a plurality of rollers arranged in pairs. The pairs of rollers include a first pair of rollers 61, which includes a first roller 610 and a second roller 620. The first rollers 610 and 620 are arranged such that a polymer material sheet 106 exiting the die 50 passes between the first roller 610 and the second roller 620 before passing between the second pair of rollers 62. Typically, if these rollers are cooled, the warm polymer material sheet 106 exiting the die 50 is cooled upon contact with the rollers. The second pair of rollers 62 includes a second roller 620 and a third roller 630. The first roller 610 and the third roller 630 rotate in the same direction, while the second roller 620 rotates in the opposite direction to the first roller 610 and the third roller 630. A first primary surface 108 of the polymer material sheet 106 will contact the first roller 610, and a second primary surface 110 will contact the second roller 620. The surfaces of the first roller 610 and the second roller 620 typically define the shape of the polymer leading edge protection sheet 120 that separates the space between the two rollers.

[0091] and Figure 4A Compared to the roller system 60 shown, Figure 4B The roller system 60 shown includes at least one roller, consisting only of a roller pair 61 comprising a first roller 610 and a second roller 620. Figure 4B Compared to the roller system 60, Figure 4C The roller system 60 includes two roller pairs 61 and 62. The first roller pair 61, including a first roller 610 and a second roller 620, is arranged such that the polymer material sheet 106 leaving the flat die 50 first passes between the first roller 610 and the second roller 620 before passing between the second roller pair 62. The second roller pair 62 includes a third roller 630 and a fourth roller 640. The first roller 610 and the third roller 630 rotate in the same direction, while the second roller 620 and the fourth roller 640 rotate in the opposite direction to the first roller 610 and the third roller 630. The two roller pairs 61 and 62 are arranged in parallel. Therefore, with... Figure 4A Compared to the roller system 60, the same rollers are not shared between the two pairs of rollers 61 and 62.

[0092] Figures 4A to 4C The rollers shown are depicted as seen from one of the ends of each roller extending therebetween.

[0093] Figure 5AA first pair of rollers 61, including a first roller 610 and a second roller 620, is shown. The first roller 610 includes a first forming surface 612 extending concavely between first opposite ends 614 of the first roller 610. The term "concave" for the first roller 610 means that the middle section 616 of the first roller 610 has a smaller diameter than the end sections 618 of the first roller 610. This can also be seen in the figures, where the concave shape is clearly observed. The first forming surface 612 may be curved, as shown in the figures, where "curved" means that the surface deviates from a straight or planar surface without sharp breaks or angles. The length of the first roller 610 is shown as a first length LA1 extending through the middle of the first roller 610.

[0094] The second roller 620 includes a second forming surface 622 extending between second opposite ends 624 of the second roller 620. The second forming surface 622 typically extends cylindrically between the second opposite ends 624. "Cylindrical" means that the second roller 620 has a diameter that is either constant or only slightly varied along a second length LA2 of the second roller 620. Alternatively, the second forming surface 622 may be slightly convex.

[0095] like Figure 5A As shown, the first forming surface 612 and the second forming surface 622 are arranged opposite to each other. Figure 5B As shown, a polymer material sheet 106 passes through the space between a first forming surface 612 and a second forming surface 622 to obtain a polymer leading edge protection sheet 120 with chamfered side edges 122, which are defined by the first forming surfaces 612 extending recessedly between the first opposite ends 614 of the first roller 610. This results in a reduced thickness of the polymer leading edge protection sheet 120 at the chamfered side edges 122 compared to the sheet thickness at the central region 124.

[0096] Figures 6A to 6C Three rollers are shown arranged as a first group of rollers 61 and a second group of rollers 62. The first group of rollers 61 includes, as shown... Figure 5A The first roller 610 and the second roller 620 are shown. Figures 6A to 6B The second set of rollers 62 shown includes a third roller 630 and, as... Figure 5A The second roller 620 is shown. The third roller 630 includes a third forming surface 632 extending between the third opposite ends 634 of the third roller 630. The second forming surface 622 and the third forming surface 632 are arranged opposite to each other.

[0097] Figure 6A The third forming surface 632, located on the third roller 630, extends cylindrically between the third opposite ends 634. Alternatively, the third forming surface 632 may be slightly convex. Figure 6BThe third forming surface 632 shown on the third roller 630 extends recessedly between the third opposite ends 634 of the third roller 630.

[0098] Figure 6C The second set of rollers 62 shown includes a third roller 630 and, as... Figure 5A The first roller 610 is shown. The third roller 630 includes a third forming surface 632 extending between the third opposite ends 634 of the third roller 630. The first forming surface 612 and the third forming surface 632 are arranged opposite to each other. Figure 6C The third forming surface 632, located on the third roller 630, extends cylindrically between the third opposite ends 634. Alternatively, the third forming surface 632 may be slightly convex.

[0099] like Figures 6A to 6C As shown, a polymer material sheet 106 passes through the space between the first molding surface 612 and the second molding surface 622 to obtain a polymer leading edge protection sheet 120 with chamfered side edges 122. The polymer leading edge protection sheet 120 also passes through the space between the second molding surface 622 and the third molding surface 632, as shown... Figures 6A to 6C As shown.

[0100] Typically, the forming surface is a smooth surface. When pressure-sensitive adhesive is applied to the polymer leading edge protector 120 after its production, it is crucial to maximize the contact area. This can be achieved by having a flat surface with low roughness on the forming surface of the roller.

[0101] Similar to other rollers, Figure 4C The fourth roller 640 shown includes a fourth forming surface (not shown) extending between fourth opposite ends 644 of the fourth roller 640. Figure 4C In the example shown, the fourth forming surface is arranged opposite to the third forming surface 632 located on the third roller 630. The fourth forming surface may extend cylindrically between the fourth opposite ends 644. Alternatively, the fourth forming surface may be slightly convex. Still alternatively, the fourth forming surface may be concave. The shape of the forming surface depends on the shape of the third forming surface 632 positioned opposite to it.

[0102] Figures 7A to 7D Different examples of polymer leading edge protectors 120 with chamfered side edges 122 are shown. The polymer leading edge protector 120 has a width in the width direction W between the chamfered side edges 122 of the polymer leading edge protector 120. Figures 7A to 7D The difference between the polymer leading edge protectors 120 shown is the thickness T of the polymer leading edge protector 120 at the chamfered side edge 122 compared to the thickness at the central region 124, and the variation along the contour of the width W.

[0103] like Figure 7A , Figure 7C and Figure 7D As shown, the width of the polymer leading edge protection sheet 120 includes a first third portion 131 and a second third portion 132, wherein the first third portion 131 and the second third portion 132 are each located near the chamfered side edge 122 corresponding to the first third portion 131 and the second third portion 132. A remaining third portion 133 is arranged between the first third portion 131 and the second third portion 132. The thickness variation of the polymer leading edge protection sheet 120 in the width direction is greater at the first third portion 131 and the second third portion 132, i.e., at the chamfered side edge 122, than at the remaining third portion 133. This is... Figure 7D The most clearly visible part is the third tertiary division at point 133, where the thickness variation is almost zero.

[0104] The first three equal parts 131 and the second three equal parts 132 may have a minimum thickness of less than 0.5 mm, while the remaining three equal parts 133 may have a maximum thickness of less than 1 mm. The first three equal parts 131 and the second three equal parts 132 may have a minimum thickness of greater than 0.01 mm, for example greater than 0.05 mm, for example greater than 0.10 mm.

[0105] like Figure 7B As shown, the width of the polymer leading edge protection sheet 120 includes a first quarter portion 141 and a second quarter portion 142, wherein the first quarter portion 141 and the second quarter portion 142 are each located near the chamfered side edge 122 corresponding to the first quarter portion 141 and the second quarter portion 142. A remaining half portion 143 is arranged between the first quarter portion 141 and the second quarter portion 142. The thickness variation of the polymer leading edge protection sheet 120 in the width direction is greater at the first quarter portion 141 and the second quarter portion 142, i.e., at the chamfered side edge 122, than at the remaining half portion 143.

[0106] Figure 8 An alternative system for producing a polymer leading edge protection sheet 120 with chamfered side edges is shown. Figure 8The system shown includes an extrusion system 10, a flat die 50, a roller system 60, a conveyor 70, a quality control section 80, and a pull roller unit 90. The roller system 60 includes a first pair of rollers 61, which includes a first roller and a second roller 620. The roller system 60 also includes a second pair of rollers 62, which includes a second roller 620 and a third roller 630. The second pair of rollers 62 serves as a cooling roller. The second pair of rollers 62 is controlled by a control unit 64 and a cooling control unit 66, which controls the cooling of the second pair of rollers 62. The quality control section 80 includes a thickness measuring unit 82 for measuring the thickness of the polymer leading edge protection sheet 120. The system also includes a traction station 84 for pulling the polymer leading edge protection sheet 120 toward the pull roller unit 90. The pull roller unit 90 includes a traction roller 94 and a tension control unit 92 for controlling the tension of the pull roller unit 90. Figure 8 The alternative system shown for producing polymer leading edge protection sheet 120 with chamfered side edges functions similarly to... Figure 1 The functions of the system have already been described.

[0107] List of reference numerals

[0108] 10 Extrusion System

[0109] 20-sieve system

[0110] 50 flat mold

[0111] 60-roll system

[0112] 61 First pair of rollers

[0113] 62 Second pair of rollers

[0114] 64 Control unit for the second pair of rollers

[0115] 66 Cooling control unit for controlling the cooling of the second pair of rollers

[0116] 70 Conveyor

[0117] 80 Quality Control Section

[0118] 82 Thickness Measurement Unit

[0119] 84 Traction Station

[0120] 90 roller unit

[0121] 92 Tension control unit for controlling the tension of the pull roller unit

[0122] 94 tension rollers

[0123] 100 granular polymer materials

[0124] 102 Molten Polymer Materials

[0125] 104 Plasticized polymer materials

[0126] 106 Polymer Material Sheets

[0127] 108 First Primary Surface

[0128] 110 Second Main Surface

[0129] 120 Polymer Leading Edge Protective Sheet

[0130] 122 Chamfered side edge

[0131] 124 Central Region

[0132] 131 First and Third Divisions

[0133] 132 Second and Third Divisions

[0134] 133 The remaining three divisions

[0135] 141 First and Fourth Divisions

[0136] 142 Second and Fourth Divisions

[0137] 143 The Remaining Half

[0138] 202 During the extrusion process, the granular polymer material is melted at 100%.

[0139] 204 The plasticized polymer material 104 is pressed by the flat mold 50 to form a polymer material sheet 106.

[0140] 206 Step of providing a polymer material sheet 106 and forming the polymer material sheet 106 into a polymer leading edge protection sheet 120

[0141] 208 Guides the polymer leading edge protection sheet 120 through the quality control section.

[0142] 210 The polymer leading edge protection sheet 120 is wound onto one or more rollers.

[0143] 502 Entrance Passage

[0144] 504 side surface

[0145] 506 Flat Exit Passage

[0146] 508 Flat exit channel departure edge

[0147] 510 Electric heater

[0148] 610 First Roller

[0149] 612 First Forming Surface

[0150] 614 First opposite end

[0151] 616 The middle section of the first roller

[0152] 618 End section of the first roller

[0153] 620 Second Roller

[0154] 622 Second Forming Surface

[0155] 624 Second opposite end

[0156] 630 Third Roller

[0157] 632 Third Forming Surface

[0158] 634 Third opposite end

[0159] 640 Fourth Roller

[0160] 644 Fourth opposite end

[0161] LA1 First longitudinal axis length

[0162] LA2 Second longitudinal axis length

[0163] LA3 Third longitudinal axis length

[0164] W1 First Width

[0165] W2 Second Width

[0166] RC curve radius

Claims

1. A method for producing a polymer leading edge protector (120) with chamfered side edges (122) for use in wind turbine blades, the method comprising the steps of: - A polymer material sheet (106) is provided, comprising a first main surface (108) and a second main surface (110), each main surface having a width extending in a width direction between the side edges of the polymer material sheet (106), wherein the first main surface (108) and the second main surface (110) are oriented oppositely, and wherein the polymer material sheet (106) has a thickness. - The polymer material sheet (106) is formed (206) into a polymer leading edge protection sheet (120) by disposing the polymer material sheet (106) between at least a pair of rollers including a first roller (610) and a second roller (620), wherein: The first roller (610) includes a first forming surface (612) extending between first opposite ends (614) of the first roller (610), wherein the first forming surface (612) extends recessedly between the first opposite ends (614); The second roller (620) includes a second forming surface (622) extending between the second opposite ends (624) of the second roller (620); The first forming surface (612) and the second forming surface (622) are arranged opposite to each other; During the rotation of the first roller (610) and the second roller (620), the thickness of the polymer material sheet (106) is changed by means of the first forming surface (612) of the first roller (610) and the second forming surface (622) of the second roller (620) to obtain the polymer leading edge protection sheet (120) with a chamfered side edge (122), which has a reduced thickness at the chamfered side edge (122) compared to the sheet thickness at the central region (124).

2. The method according to claim 1, wherein, The method further includes: - The granular polymer material (100) is melted (202) by an extrusion process to obtain a molten polymer material (102) with a predetermined hardness, thereby obtaining a plasticized polymer material (104); and - The plasticized polymer material (104) is pressed (204) by a flat die (50) to form the plasticized polymer material (104) into a polymer material sheet (106).

3. The method of claim 2 further comprises providing a granular polymer material (100) and drying the granular polymer material (100) to a moisture level of 0.02 wt% or less before melting the granular polymer material (100).

4. The method according to any one of claims 1 to 3, wherein, The polymer material is a polyurethane thermoplastic material containing polyols, chain extenders, and aliphatic isocyanates.

5. The method according to any one of claims 1 to 3, wherein, The polymer material is polyurethane, and the polymer leading edge protection sheet (120) is a polyurethane leading edge protection sheet.

6. The method according to claim 2 or 3, wherein, The polymer material is a polyurethane material, and wherein the granular polyurethane material is an aliphatic thermoplastic polyurethane (TPU) made of a polyol such as a difunctional polyol, a butanediol chain extender, and an aliphatic isocyanate.

7. The method according to claim 2 or 3, wherein, The polymer material is a polyurethane material, and the granular polyurethane material further comprises one or more additives.

8. The method according to claim 7, wherein, The additives are UV absorbers, antioxidants, and / or pigments.

9. The method according to any one of claims 2 to 3, 8, wherein, The polymer material is a polyurethane material, and the granular polyurethane material does not contain a release agent.

10. The method according to any one of claims 1 to 3, 8, wherein, The polymer leading edge protection sheet (120) is characterized by the following physical properties: - Maximum thickness is between 0.8 mm and 2.0 mm; - The Shore A hardness is between 65 and 75, and the Shore A hardness is measured by ISO 868; - When measured using ISO 37 / 1A at 23°C, the elongation is greater than 400 mm; - The speed of sound is below 1700 m / s, measured by ISO 16810 and ISO 16811; and - Resistance to corrosion at 150 m / s for more than 8 hours, the corrosion resistance being measured by DNV-RP-0171.

11. The method according to any one of claims 1 to 3, 8, wherein, The polymer leading edge protection sheet (120) is characterized by the following physical properties: - Maximum thickness is between 0.7 mm and 2.0 mm; - The Shore A hardness is between 68 and 78, and the Shore A hardness is measured by ISO 868; - When measured using ISO 37 / 1A at 23°C, the elongation is greater than 400 mm; - The speed of sound is below 1700 m / s, as measured by ISO 16810 and ISO 16811; and - Corrosion resistance at 140 m / s for more than 10 hours, the corrosion resistance being measured by DNV-RP-0171.

12. The method according to any one of claims 1 to 3, 8, wherein, The polymer leading edge protection sheet (120) has a Shore A hardness of less than or equal to 78.

13. The method according to any one of claims 1 to 3, 8, wherein, The polymer leading edge protection sheet (120) has a Shore A hardness of less than or equal to 75.

14. The method according to any one of claims 1 to 3, 8, wherein, The polymer leading edge protection sheet (120) has a width in the width direction between the chamfered side edges (122) of the polymer leading edge protection sheet (120), the width including a first third portion (131) and a second third portion (132), wherein the first third portion (131) and the second third portion (132) are each located near the chamfered side edges (122) of the polymer leading edge protection sheet (120) corresponding to the first third portion (131) and the second third portion (132), wherein a remaining third portion (133) is arranged between the first third portion (131) and the second third portion (132), wherein the thickness variation of the polymer leading edge protection sheet (120) in the width direction is greater at the first third portion (131) and the second third portion (132) than at the remaining third portion (133).

15. The method according to claim 14, wherein, The remaining three equal parts (133) have a maximum thickness of less than 1 mm.

16. The method of claim 14, wherein, The first three equal parts (131) and the second three equal parts (132) have a minimum thickness of less than 0.5 mm.

17. The method according to any one of claims 1 to 3, 8, 15 to 16, wherein, The polymer leading edge protector (120) has a width in the width direction between the chamfered side edges (122) of the polymer leading edge protector (120), the width including a first quarter (141) and a second quarter (142), wherein the first quarter (141) and the second quarter (142) are each located near the chamfered side edges (122) of the polymer leading edge protector (120) corresponding to the first quarter (141) and the second quarter (142), wherein a remaining half (143) is arranged between the first quarter (141) and the second quarter (142), wherein the thickness variation of the polymer leading edge protector (120) in the width direction is greater at the first quarter (141) and the second quarter (142) than at the remaining half (143).

18. The method according to any one of claims 1 to 3, 8, 15 to 16, wherein, The second forming surface (622) of the second roller (620) extends cylindrically between the second opposite ends (624).

19. The method according to any one of claims 1 to 3, 8, 15 to 16, wherein, The first roller (610) has a first longitudinal axis (LA1) extending between the first opposite ends (614), and the second roller (620) has a second longitudinal axis (LA2) extending between the second opposite ends (624), wherein the first longitudinal axis (LA1) and the second longitudinal axis (LA2) are substantially parallel.

20. The method according to any one of claims 1 to 3, 8, 15 to 16, wherein, The first forming surface (612) of the first roller (610) is curved.

21. The method according to any one of claims 1 to 3, 8, 15 to 16, wherein, The second forming surface (622) of the second roller (620) is smooth.

22. The method according to any one of claims 1 to 3, 8, 15 to 16, wherein, The polymer material sheet (106) is formed into the polymer leading edge protection sheet (120) by pulling and / or pushing the polymer material sheet (106) through the at least one pair of rollers.

23. The method according to any one of claims 1 to 3, 8, 15 to 16, wherein, Forming the polymer material sheet (106) into the polymer leading edge protection sheet (120) is achieved by pulling the polymer material sheet (106) through the at least one pair of rollers, wherein at least the first roller (610) and / or the second roller (620) pull the polymer material sheet (106) through the at least one pair of rollers.

24. The method according to any one of claims 1 to 3, 8, 15 to 16, wherein, The polymer material sheet (106) is formed into the polymer leading edge protection sheet (120) by allowing the polymer material sheet (106) to fall into the cavity between the at least one pair of rollers.

25. The method according to any one of claims 1 to 3, 8, 15 to 16, wherein, The method further includes disposing the polymer leading edge protection sheet (120) between a second pair of rollers, the second pair of rollers including a third roller (630), and one of the first roller (610) and the second roller (620).

26. The method according to claim 25, wherein, The third roller (630) includes a third forming surface (632) extending between the third opposite ends (634) of the third roller (630), wherein the third forming surface (632) extends recessedly between the third opposite ends (634).

27. The method according to claim 25, wherein, The third roller (630) includes a third forming surface (632) extending between the third opposite ends (634) of the third roller (630), wherein the third forming surface (632) extends cylindrically between the third opposite ends (634).

28. The method according to any one of claims 1 to 3, 8, 15 to 16, 26 to 27, wherein, Cool the first roller (610), the second roller (620) and / or the third roller (630).

29. The method according to any one of claims 1 to 3, 8, 15 to 16, 26 to 27, further comprising providing the polymer leading edge protection sheet (120) through a quality control section (80) that ensures the performance specifications / requirement specifications of the polymer leading edge protection sheet (120).

30. The method according to any one of claims 1 to 3, 8, 15 to 16, 26 to 27, further comprising winding the polymer leading edge protector (120) onto the pull roller unit (90) before adding the adhesive and / or shortening the polymer leading edge protector (120).

31. A polymer leading edge protection sheet (120) obtained by the method according to claims 1 to 30.

32. A wind turbine blade having a polymer leading edge protection sheet (120) according to claim 31.

Citation Information

Patent Citations

  • Profiled films

    CN110603130A

  • Method for making a composite extruded profile formed with thermoplastic organic material reinforced with reinforcing fibres

    US20060087059A1