An electromagnetic shielding film and a printed circuit board
By designing inverted conical openings in the electromagnetic shielding film and optimizing the viscosity of the adhesive layer and the sandwich structure, the problem of residue removal during the multi-layer lamination process of the electromagnetic shielding film was solved, improving the heat-resistant lamination reliability and electrical performance of the film layers.
Patent Information
- Application Number
- CN202611524667.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-29
- Publication Date
- 2026-11-10
AI Technical Summary
Existing electromagnetic shielding films have difficulty in timely removal of residual moisture, solvents, and small volatile molecules during the multi-layer lamination process, leading to defects such as blistering of the insulation layer and interlayer delamination, which affect the electrical performance and service life of the product. At the same time, the perforation scheme leads to a decrease in the rigidity of the shielding layer, making it prone to deformation and cracking.
The openings in the metal shielding layer are designed to gradually decrease from the adhesive film side to the insulation layer side, forming an inverted conical structure. Combined with the optimization of the melt viscosity of the adhesive film layer and the use of connecting interlayers, exhaust channels and support are provided to reduce the risk of insulation layer damage.
Without altering the membrane structure, exhaust efficiency was improved, insulation layer damage and interface blistering issues were reduced, and the heat-resistant pressing reliability and electrical performance of the electromagnetic shielding membrane were enhanced.
Smart Images

Figure CN123075799A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of printed circuit board technology, specifically to an electromagnetic shielding film and a printed circuit board. Background Technology
[0002] As the electronics and information industry develops towards high-frequency, high-speed, and high-density integration, flexible printed circuit boards (FPCs) and high-frequency printed circuit boards (PCBs) place higher demands on the heat resistance, reliability, thinness, and shielding performance of electromagnetic shielding films. Conventional electromagnetic shielding films typically employ a three-layer stacked structure consisting of an insulating layer, a metal shielding layer, and an adhesive film layer. During the lamination process, residual moisture, solvents, and small volatile molecules within the film layers cannot be expelled in time, easily leading to vaporization and expansion under high temperature and pressure. This results in defects such as blistering of the insulating layer and interlayer delamination, severely affecting the electrical performance and lifespan of the product.
[0003] To address the venting issue during heat-resistant lamination, some industry solutions employ a perforated array in the metal shielding layer. These perforations create vertical venting channels, allowing gas generated during lamination to escape upwards through the shielding layer, thus suppressing interface bubbling defects. However, this approach presents several new drawbacks in practical applications: Firstly, the residual copper content decreases after perforation, and the insulation layer at the perforation location loses the rigid support of the metal shielding layer. Under the combined effects of lamination pressure and internal airflow impact, it is highly susceptible to indentation deformation and tensile cracking. Secondly, stress concentration in the copper layer around the perforations can easily cause puncture damage to the insulation layer, introducing a new yield bottleneck.
[0004] In summary, a solution is needed to address the problem of residual moisture, solvents, and small volatile molecules being difficult to remove in a timely manner during the multi-layer lamination process of electromagnetic shielding films, while minimizing the impact on the film structure. Summary of the Invention
[0005] This application provides an electromagnetic shielding film and a printed circuit board to solve the problem that residual moisture, solvents and small molecule volatiles are difficult to remove in time during the multi-layer lamination process of electromagnetic shielding film, while minimizing the impact on the film structure.
[0006] In one aspect of this application, an electromagnetic shielding film is provided, comprising: an insulating layer, a metal shielding layer, and an adhesive film layer, wherein the metal shielding layer is located between the insulating layer and the adhesive film layer; the metal shielding layer is provided with a plurality of openings penetrating the metal shielding layer in the thickness direction; the aperture of the openings gradually decreases from the adhesive film layer side to the insulating layer side.
[0007] The electromagnetic shielding film provided in this application features an opening in the metal shielding layer with the pore diameter gradually decreasing from the adhesive film side to the insulating layer side. This design serves two purposes: firstly, the openings provide an outlet for residual air bubbles, solvents, and small volatile molecules during lamination, allowing these substances to be more easily extruded; secondly, the large pore diameter on the adhesive film side of the inverted conical structure ensures sufficient air intake area and exhaust efficiency, while the small pore diameter on the insulating layer side reduces the suspended area and lowers the risk of insulation layer damage. Furthermore, the varying pore diameters form a slope, which serves the dual purpose of guiding exhaust and preventing adhesive overflow. Combined with optimized process conditions for other layers, this design reduces adhesive overflow tendency and offsets the rigidity loss caused by the openings. It simultaneously addresses insulation layer damage and interface bubbling issues during lamination without altering the overall product stack structure or compatibility with existing processes, thereby improving the heat-resistant lamination reliability of the electromagnetic shielding film.
[0008] In some embodiments of this application, the difference between the diameter of the opening on the insulating layer side and the diameter of the opening on the adhesive film side is defined as the aperture difference; the arithmetic mean of the diameters of the opening on the insulating layer side and the opening on the adhesive film side is defined as the aperture mean; the ratio of the aperture difference to the aperture mean is less than 0.3.
[0009] In some embodiments of this application, the ratio of the aperture difference to the average aperture is 0.1 to 0.25.
[0010] In some embodiments of this application, the arithmetic mean thickness of the metal shielding layer is defined as H; the diameter of the opening on one side of the adhesive film layer with the aperture is defined as B; the relationship between the arithmetic mean thickness H of the metal shielding layer and the diameter B of the opening on one side of the adhesive film layer with the aperture satisfies B > 5H.
[0011] In some embodiments of this application, the aperture of the opening facing the insulating layer is 10μm~100μm.
[0012] In some preferred embodiments, the aperture of the opening facing the insulating layer is 25μm~75μm.
[0013] In some embodiments of this application, the openings are arranged in an array; the residual copper content of the metal shielding layer is 65%~95%.
[0014] In some embodiments of this application, the melt viscosity of the adhesive film layer is 5000 Pa within a temperature range of 80°C to 120°C. s ~20000 Pa s.
[0015] In some preferred embodiments, the melt viscosity of the adhesive film layer is 8000 Pa within a temperature range of 80°C to 120°C. s ~15000 Pa s.
[0016] In some embodiments of this application, the arithmetic mean thickness H of the metal shielding layer is 0.5 μm to 5 μm.
[0017] In some embodiments of this application, the electromagnetic shielding film further includes: a carrier film covering the surface of the insulating layer facing away from the metal shielding layer; and a protective film covering the surface of the adhesive film layer facing away from the metal shielding layer; both the carrier film and the protective film are release films.
[0018] In another aspect of this application, a printed circuit board is also provided, comprising: a circuit board body; an electromagnetic shielding film provided in this application, wherein the electromagnetic shielding film is attached to at least one side surface of the circuit board body; an adhesive film layer is located in the electromagnetic shielding film on the side closer to the circuit board body, and an insulating layer is located in the electromagnetic shielding film on the side farther away from the circuit board body; the circuit board body is a flexible circuit board or a rigid circuit board. Attached Figure Description
[0019] To more clearly illustrate the technical solutions in the specific embodiments of this application or the prior art, the drawings used in the description of the specific embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of this application. For those skilled in the art, other drawings can be obtained from these drawings without creative effort.
[0020] Figure 1 A schematic diagram of the structure of an electromagnetic shielding film; Figure 2 This is a morphological image of the metal shielding layer in an electromagnetic shielding film under an electron microscope. Figure 3 This is a morphological image of the metal shielding layer in an electromagnetic shielding film under an optical microscope. Figure 4 An electron microscope image of a cross-section of a portion of the electromagnetic shielding film; Figure 5 This is a schematic diagram of the structure of an electromagnetic shielding film according to an embodiment of this application; Figure 6 This is a schematic diagram of the structure of an electromagnetic shielding film according to another embodiment of this application; Figure 7 This is a schematic diagram of the structure of a printed circuit board according to an embodiment of this application. Detailed Implementation
[0021] The structure of various electromagnetic shielding films, such as Figure 1As shown, it includes a carrier film 110, an insulating layer 120, a metal shielding layer 130, an adhesive film layer 140, and a protective film 150 stacked in sequence. The core function of electromagnetic shielding is provided by the metal shielding layer 130.
[0022] As mentioned earlier, during the lamination process of the electromagnetic shielding film, residual moisture, solvents, and small volatile molecules inside the film cannot be discharged in time, which will seriously affect the electrical performance and service life of the product. Existing technologies typically improve this by providing openings 131 in the metal shielding layer 130. (Electron microscope morphology reference for a metal shielding layer with openings 131 is shown.) Figure 2 Morphological reference under an optical microscope Figure 3 The metal shielding layer 130 is disposed on the surface of the insulating layer 120, and an opening 131 is provided therein. The cross-sectional electron microscope morphology of this is for reference. Figure 4 The opening 131 provides an outlet for residual bubbles, solvents, and small volatile molecules, allowing them to be quickly discharged. However, this often introduces new defects, resulting in suboptimal performance of the electromagnetic shielding film.
[0023] In view of this, this application provides an electromagnetic shielding film and a printed circuit board to solve the problem that residual moisture, solvents and small molecule volatiles are difficult to remove in time during the multi-layer lamination process of the electromagnetic shielding film, while minimizing the impact on the film structure.
[0024] This application provides an electromagnetic shielding film, comprising: an insulating layer, a metal shielding layer, and an adhesive film layer, wherein the metal shielding layer is located between the insulating layer and the adhesive film layer; the metal shielding layer is provided with a plurality of openings penetrating the metal shielding layer in the thickness direction; the aperture of the openings gradually decreases from the adhesive film layer side to the insulating layer side.
[0025] This application also provides a printed circuit board, comprising: a circuit board body; an electromagnetic shielding film provided in this application, wherein the electromagnetic shielding film is attached to at least one surface of the circuit board body; the circuit board body is a flexible circuit board or a rigid circuit board.
[0026] The present application will now be described in further detail with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the application and not intended to limit its scope. Furthermore, it should be noted that, for ease of description, only the parts relevant to the present application are shown in the drawings, not the entire structure. All other embodiments obtained by those skilled in the art based on the embodiments of the present application without inventive effort are within the scope of protection of the present application.
[0027] In the following description, descriptions of well-known structures and technologies are omitted to avoid unnecessarily obscuring the concepts of this application. Various structural schematic diagrams according to embodiments of this application are shown in the accompanying drawings. These drawings are not to scale, and some details are enlarged for clarity, and some details may be omitted. The shapes of the various regions and layers shown in the drawings, as well as their relative sizes and positional relationships, are merely exemplary and may deviate from reality due to manufacturing tolerances or technical limitations. Furthermore, those skilled in the art can design regions / layers with different shapes, sizes, and relative positions as needed. In the context of this application, when a layer / element is referred to as being "on" another layer / element, the layer / element may be directly on the other layer / element, or there may be an intermediate layer / element between them. Additionally, if a layer / element is "on" another layer / element in one orientation, then when the orientation is reversed, the layer / element may be "below" the other layer / element.
[0028] Example 1 This application provides an electromagnetic shielding film 100, for reference... Figure 5 ,include: An insulating layer 120, a metal shielding layer 130, and an adhesive film layer 140 are provided, with the metal shielding layer 130 located between the insulating layer 120 and the adhesive film layer 140. The metal shielding layer 130 is provided with a plurality of openings 131 that penetrate the metal shielding layer 130 in the thickness direction; The aperture of the opening 131 gradually decreases from the adhesive film layer 140 side to the insulating layer 120 side.
[0029] The electromagnetic shielding film provided in this application has an opening in the metal shielding layer 130 with the aperture gradually decreasing from the adhesive film layer 140 side to the insulating layer 120 side. This design serves two purposes: firstly, the opening provides an outlet for residual air bubbles, solvents, and small volatile molecules during lamination, allowing these substances to be more easily expelled; secondly, since the adhesive film layer 140 faces the circuit board during mounting, this side provides support. The large aperture on the adhesive film layer 140 side ensures sufficient air intake area and exhaust efficiency, while the small aperture on the insulating layer 120 side reduces the suspended area and lowers the risk of insulation layer damage. Furthermore, the varying aperture forms a slope, which serves the dual purpose of guiding airflow and preventing adhesive overflow. Based on this, by optimizing the process conditions of other layers, the tendency of adhesive overflow can be reduced and the rigidity loss caused by openings can be offset. Without changing the overall stacked structure of the product and being compatible with existing processes, the problems of insulation layer damage and interface blistering during the lamination process can be solved simultaneously, thereby improving the heat-resistant lamination reliability of the electromagnetic shielding film.
[0030] In some embodiments of this application, The difference between the diameter of the opening on one side of the insulating layer 120 of the aperture 131 and the diameter of the opening on one side of the adhesive film layer 140 of the aperture 131 is defined as the aperture difference. The arithmetic mean of the diameter of the opening on one side of the insulating layer 120 of the aperture 131 and the diameter of the opening on one side of the adhesive film layer 140 of the aperture 131 is defined as the aperture mean. The ratio of the aperture difference to the average aperture is less than 0.3.
[0031] The ratio of the aperture difference to the average aperture reflects the inclination of the opening sidewall. When this ratio is less than 0.3, the inclination allows both openings to function appropriately. If the ratio is too small, it resembles a straight hole structure, failing to demonstrate the differentiated advantages of the tapered hole. If the ratio is too large, the taper is too steep, resulting in significant stress concentration on the inclined surface of the hole wall, greatly increasing the difficulty of etching and making the hole wall collapse defect more likely. By controlling this ratio within a reasonable range, it is possible to ensure a significant reduction in the aperture on the insulating side to reduce the suspended area, while maintaining a smooth hole wall transition and dispersing the stress at the hole edge. When the ratio is less than 0.3, on the one hand, a certain residual copper ratio is ensured to provide sufficient rigid support near the opening, preventing concave deformation and tensile cracking; on the other hand, excessive stress concentration is avoided, preventing puncture damage at the edge. Therefore, this ratio range achieves a good balance between minimizing deformation and cracking and minimizing puncture damage.
[0032] In some preferred embodiments, the ratio of the aperture difference to the average aperture is 0.1 to 0.25.
[0033] A ratio of the aperture difference to the average aperture in the range of 0.1 to 0.25 can further ensure sufficient rigid support, while also minimizing stress concentration and preventing puncture damage at the edges.
[0034] In some embodiments of this application, Define the arithmetic mean thickness of the metal shielding layer 130 as H; Define the diameter of the opening on one side of the adhesive film layer 140 of the aperture 131 as B; The arithmetic mean thickness H of the metal shielding layer 130 and the diameter B of the opening on one side of the adhesive film layer 140 of the aperture 131 satisfy the relationship that B > 5H.
[0035] The relationship between the arithmetic mean thickness H of the metal shielding layer 130 and the diameter B of the opening on one side of the adhesive film layer 140 of the aperture 131 is another manifestation of the inclination of the aperture wall and the degree of opening of the aperture 131. This proportional relationship ensures that the perforation has a sufficient flow cross-sectional area, so that the exhaust efficiency is not limited by the copper thickness. At the same time, a reasonable aspect ratio allows the tapered slope to play a good airflow guiding role, accelerating the upward exhaust of gas. In addition, a sufficiently large aperture to copper thickness ratio can keep the inclination angle of the aperture wall in a gentle range, avoiding stress concentration caused by steep slopes, while providing sufficient obstruction stroke for the flow of adhesive, improving the anti-overflow effect. When the relationship between the two satisfies B > 5H, on the one hand, a certain residual copper ratio is ensured to provide sufficient rigid support near the opening, avoiding concave deformation and tensile cracking; on the other hand, excessive stress concentration is avoided, and puncture damage at the edge is avoided. Therefore, this relationship range can achieve a good balance between avoiding deformation and cracking as much as possible and avoiding puncture damage as much as possible.
[0036] In some preferred embodiments, the arithmetic mean thickness H of the metal shielding layer 130 and the diameter B of the opening on one side of the adhesive film layer 140 of the aperture 131 satisfy the relationship B=6H~20H.
[0037] The arithmetic mean thickness H of the metal shielding layer 130 and the diameter B of the opening on one side of the adhesive film layer 140 of the aperture 131 satisfy the relationship range of B=6H~20H, which can further ensure a certain residual copper rate, provide sufficient rigid support near the opening, avoid dent deformation and tensile cracking, and further avoid excessive stress concentration and avoid puncture damage at the edge.
[0038] In some embodiments of this application, the aperture of the opening 131 facing the insulating layer 120 is 10μm to 100μm.
[0039] The aperture of the opening 131 facing the insulating layer 120 has a lower limit that can provide sufficient escape channels for residual bubbles and other substances, ensuring their rapid escape and preventing accumulation or buildup in the film layer that could cause deformation or damage. The upper limit can prevent the opening from being too large, which would prevent sufficient rigid support from being provided near the opening.
[0040] In some preferred embodiments, the aperture of the opening 131 facing the insulating layer 120 is 25μm to 75μm.
[0041] The aperture of the opening 131 facing the insulating layer 120 is 25μm~75μm, which can further satisfy the requirement to provide sufficient escape channels for residual bubbles and other substances, ensuring their rapid escape and avoiding accumulation or aggregation in the film layer, which would cause film layer deformation or damage. At the same time, it can further avoid the opening being too large, which would prevent sufficient rigid support from being provided near the opening.
[0042] In some embodiments of this application, the openings 131 are arranged in an array; the residual copper content of the metal shielding layer 130 is 65%~95%.
[0043] The array-arranged openings ensure a uniform distribution of the opening positions 131, meaning a uniform distribution of areas without metal layer support. This avoids film damage caused by insufficient local support or excessive stress. The residual copper ratio is crucial; if it falls below the lower limit, insufficient local support can easily lead to film damage, while if it exceeds the upper limit, it will insufficiently guide residual bubbles and other substances, allowing them to accumulate within the film and easily cause damage during lamination. Therefore, a residual copper ratio of 65% to 95% in the metal shielding layer strikes a balance between providing sufficient support and maximizing escape guidance.
[0044] In some embodiments of this application, the melt viscosity of the adhesive film layer 140 is 5000 Pa within a temperature range of 80°C to 120°C. s ~20000 Pa s.
[0045] The melt viscosity of the adhesive film layer 140 within the temperature range of 80℃ to 120℃ can reduce the tendency for adhesive overflow at the material level. 80~120℃ is the early venting stage of the lamination process. At this time, the adhesive layer begins to melt but has not yet entered the cross-linking and curing stage. Increasing the viscosity in this range can significantly reduce the flow properties of the adhesive, reducing the amount of adhesive flowing into the perforations under lamination pressure. This, combined with the narrowing structure of the tapered orifice, forms a double anti-clogging barrier, preventing the adhesive from filling the perforations and causing the venting channels to fail. Simultaneously, it ensures that the adhesive still has sufficient flowability during the high-temperature curing stage to meet the requirements of interface wetting and circuit filling. If the viscosity is too low, the adhesive film layer will be too fluid and easily overflow from the opening 131, damaging the film structure; if the viscosity is too high, it will easily clog the opening 131. Therefore, the melt viscosity of the adhesive film layer 140 within the temperature range of 80℃ to 120℃ is 5000 Pa. s ~20000 Pa A balance can be struck between minimizing adhesive overflow and minimizing clogging of openings.
[0046] In some preferred embodiments, the melt viscosity of the adhesive film layer 140 is 8000 Pa within a temperature range of 80°C to 120°C. s~15000 Pa s.
[0047] In some embodiments of this application, the arithmetic mean thickness H of the metal shielding layer 130 is 0.5 μm to 5 μm.
[0048] In materials mechanics, the in-plane bending stiffness of sheet materials is proportional to the cube of their thickness. Appropriately increasing the copper thickness can maintain or even improve the overall rigidity and anti-warping ability of the shielding layer even with a decrease in residual copper content. This reduces local deformation, wrinkles, and warping during lamination, thereby lowering the risk of stretching and tearing of the insulation layer due to shielding layer deformation. Simultaneously, it ensures uniform in-plane heat conduction and reduces the problem of premature curing and sealing of the adhesive layer caused by localized hot spots. The arithmetic mean thickness of the 130mm metal shielding layer serves two purposes: firstly, it ensures the required electromagnetic shielding effect; secondly, it avoids excessive thickness that could affect the film's dimensions. If the arithmetic mean thickness of the metal shielding layer is less than 0.5μm, it may be insufficient to provide adequate electromagnetic shielding, and secondly, it may result in insufficient support or excessively sharp openings causing film damage. If the average thickness is greater than 5μm, the film is too thick, affecting the overall dimensions of the shielding film and its application.
[0049] In some preferred embodiments, the arithmetic mean thickness H of the metal shielding layer 130 is 1 μm to 2 μm.
[0050] In some embodiments of this application, the metal shielding layer 130 is a planar layer (e.g., Figure 4 (as shown in the example); or, the metal shielding layer 130 is an irregularly shaped layer with a longitudinal section of irregular wavy shape (such as...). Figure 5 (As shown in the diagram). The irregularly wavy, irregularly shaped layer includes several non-uniformly distributed protrusions and depressions. The horizontal dimensions of each protrusion and depression are not exactly the same as the dimensions in the thickness direction of the metal shielding layer, and their shapes are also not exactly the same. That is, the shapes and dimensions may be partially the same, or they may all be different, but not all of them are the same.
[0051] In some embodiments, to further enhance interlayer adhesion and suppress interfacial blistering, a connecting interlayer (not shown in the figure) can be added at the interface. This connecting interlayer can be disposed between the insulating layer 120 and the metal shielding layer 130, or simultaneously between the metal shielding layer 130 and the adhesive film layer 120. The thickness of the connecting interlayer is limited to 0.5 μm to 3 μm, preferably 1 μm to 2 μm. The connecting interlayer can be formed by a silane coupling agent coating or a modified epoxy resin primer, or a metal oxide layer formed by plasma treatment. Through the dual effects of chemical coupling and micromechanical interlocking, the connecting interlayer significantly improves interfacial adhesion, compensates for the decrease in effective bonding area caused by openings, enhances interlayer anti-peeling ability, and effectively resists the pushing effect of internal residual gas pressure, preventing interfacial peeling and blistering. Simultaneously, the connecting layer can fill microscopic gaps and uneven defects at the edge of the opening, optimize the interfacial stress distribution, and reduce interfacial cracking caused by stress concentration at the edge of the opening.
[0052] In some embodiments of this application, the electromagnetic shielding film further includes: A carrier film 110 covers the surface of the insulating layer 120 on the side opposite to the metal shielding layer 130; A protective film 150 covers the surface of the adhesive film layer 140 on the side facing away from the metal shielding layer 130; Both the carrier film 110 and the protective film 150 are release films.
[0053] The protective film 150 isolates and protects the adhesive film layer 140, preventing it from coming into contact with air and becoming contaminated, thus causing the film layer to fail, when the electromagnetic shielding film is not applied. The carrier film 110 plays a role in bearing the applied force during the application process.
[0054] In practical use, the electromagnetic shielding film 100 is first peeled off the protective film 150 to expose the adhesive film layer 140, and then attached to the surface of the printed circuit board through the adhesive film layer 140. After complete attachment, the carrier film 110 is removed.
[0055] The structural and material parameters mentioned above were obtained using standardized testing methods. The testing environment was normal temperature and humidity (23±2℃, 50±5%RH). All parameters were tested repeatedly more than 3 times, and the arithmetic mean was taken as the final result.
[0056] 1. Percentage of the difference between the upper and lower diameters and the overall diameter of the opening. Parameter definition: The upper side diameter refers to the equivalent circle diameter of the opening 131 on the side of the metal shielding layer 130 facing the insulating layer 120, and the lower side diameter refers to the equivalent circle diameter of the opening 131 on the side of the metal shielding layer 130 facing the adhesive film layer 140; the formula for calculating the diameter difference ratio is: (lower side diameter - upper side diameter) ÷ [(lower side diameter + upper side diameter) ÷ 2] × 100%, which is used to characterize the taper of the opening 131.
[0057] Test methods: The opening contours on the upper and lower surfaces of the shielding layer were scanned using a laser confocal microscope. The equivalent circle of each opening was fitted using image analysis software, and the equivalent diameters of the upper and lower surfaces were read. Alternatively, a cross-sectional sample of a single perforation was prepared by focused ion beam cutting, and the cross-sectional morphology was observed using a field emission scanning electron microscope to directly measure the upper and lower aperture dimensions. At least 20 openings were randomly selected for testing, and the average diameter difference percentage was calculated.
[0058] 2. Aspect ratio of the metal shielding layer thickness H to the lower aperture B Parameter definition: H is the arithmetic mean thickness of the metal shielding layer 130, and B is the maximum equivalent circle diameter of the lower side of the opening (i.e., the side of the opening 131 on the metal shielding layer 130 facing the adhesive film layer 140). The ratio of the two is used to characterize the aspect ratio of the perforation.
[0059] Test method: The thickness of the metal shielding layer was measured at 5 points in the non-porous area of the metal shielding layer using a step meter, and the arithmetic mean was taken to obtain H; the lower aperture B was obtained using the above aperture test method, and the ratio of B to H was calculated.
[0060] 3. Warm melt viscosity of the adhesive film material Parameter definition: The melt viscosity of the adhesive film material in the main temperature range of 80~120℃ during pressing and degassing. The lowest viscosity in this temperature range is taken as the evaluation index.
[0061] Test method: A rotational rheometer was used to heat the adhesive from room temperature to 180°C at a heating rate of 3°C / min. The viscosity-temperature curve of the adhesive was tested using a plate oscillation mode. The minimum viscosity value in the range of 80~120°C was read as the test result.
[0062] 4. Thickness of connecting interlayer Parameter definition: Vertical thickness of the interlayer connecting at the interface, taken as the arithmetic mean of multiple measurements.
[0063] Test method: The membrane cross-section sample was prepared by liquid nitrogen brittle fracture, the interface morphology was observed by field emission scanning electron microscopy, the vertical thickness of the bonding layer was measured, and five different locations were randomly selected for testing, and the arithmetic mean was taken.
[0064] 5. Preparation process flow An insulating layer 120 is formed on the carrier film 110 through a coating process. Then, an adhesive mixed with filler particles is coated, followed by baking and recoating, creating a rough surface with raised and recessed areas on the insulating layer 120. A seed layer is formed on one side of the rough surface by sputtering, and then electroplating is used to thicken it into a metal shielding layer 130. The surface roughness Ra is controlled within a preset range to form... Figure 6 The structure shown. Alternatively, a metal shielding layer 130 can be formed by directly attaching copper foil, forming... Figure 5 The structure is shown. Roughness control can be achieved by adjusting the roughness of the insulating layer 120 so that the metal shielding layer 130, which is replicated on the insulating layer 120, has a corresponding roughness. Alternatively, the roughness Ra of the metal shielding layer 130 can be adjusted by modifying the electroplating process during the thickening process of the metal shielding layer 130.
[0065] Roughening treatment: The exposed surface of the metal shielding layer 130 is slightly roughened to form a rough protrusion for grounding.
[0066] Laser drilling: Using ultraviolet or infrared lasers, a perforated array is fabricated on the metal shielding layer 130, controlling the hole diameter and density within a set range. The roughened surface undulations naturally create rough edges at the hole openings. Drilling can be performed during seed layer sputtering or after electroplating thickening.
[0067] Coating the adhesive film: A thermosetting adhesive is applied to the roughened surface and pre-cured in an oven to form an adhesive film layer 140. A protective film 150 is then formed on the surface of the adhesive film layer 140.
[0068] Slitting: Slitting the finished product into specified specifications.
[0069] Effect comparison: One set of comparative examples and four sets of gradient test examples were selected for comparison testing. All samples had the same basic structure: the insulating layer 130 was a 12μm PI film, the metal shielding layer 130 had a base copper thickness of 12μm, the overall porosity was 30%, the perforations were circular holes in an equilateral triangular staggered array, and the adhesive layer 140 was a 15μm modified epoxy adhesive layer. The pressing test conditions were uniformly set as 180℃ temperature, 3MPa pressure, and 60min heat and pressure holding. The test indicators included the insulation layer breakage rate, interface blistering rate, interlayer peel strength, and saturated degassing time.
[0070] in: Comparative Example 1 shows that opening 131 is set as a conventional straight hole.
[0071] Test Example 1 is a test example where only the aperture 131 is set to be a tapered aperture that gradually decreases from the adhesive layer side to the insulating layer side; the other film layers are set the same as in Comparative Example 1.
[0072] Test Example 2 is based on Test Example 1, with the addition of viscosity optimization settings for the adhesive film layer 140. Specific optimization data can be found in the comparison table. Test Example 3 is based on Test Example 2 with an increased thickness of the metal shielding layer 130.
[0073] Test Example 4 is based on Test Example 3 with the addition of a connecting mezzanine.
[0074] The specific parameters and test results are shown in the table below:
[0075] As shown in the table above, Test Examples 1-4 are significantly better than Comparative Example 1 in terms of insulation layer breakage rate, interface bubble rate, and saturation venting time. Regarding 180° peel strength, although Test Examples 1-4 show no significant difference from Comparative Example 1, the results are still better. These test results demonstrate that the electromagnetic shielding film proposed in this application can reduce the suspended area and lower the risk of insulation layer breakage while ensuring air intake area and venting efficiency. Furthermore, combined with optimization schemes such as viscosity optimization, copper layer thickness adjustment, and the addition of connecting interlayers, it can further reduce adhesive overflow tendency and offset the rigidity loss caused by openings. This allows for the simultaneous resolution of insulation layer breakage and interface bubbling issues during the lamination process without altering the overall product stack-up architecture or compatibility with existing processes, thereby improving the heat-resistant lamination reliability of the electromagnetic shielding film.
[0076] Example 2 This embodiment provides a printed circuit board, referenced Figure 7 ,include: The circuit board body 200 includes a substrate 210, a substrate layer 220 on the surface of the substrate and a circuit layer (not shown in the figure) in the substrate layer, and a cover film 240 on the surface of the substrate layer. As provided in Embodiment 1 above, the electromagnetic shielding film 100 is attached to at least one side surface of the circuit board body 200; the adhesive film layer 140 is located in the electromagnetic shielding film on the side closer to the circuit board body 200, and the insulating layer 120 is located in the electromagnetic shielding film on the side away from the circuit board body 200.
[0077] The electromagnetic shielding film 100, attached to the circuit board body 200, comprises only an insulating layer 120, a metal shielding layer 130, and an adhesive film layer 140; the specific attachment process can be found in the specific usage section of Embodiment 1 above. Since the attachment process removes the carrier film 110 and the protective film 150, only the adhesive film layer 140 for bonding and fixing, the metal shielding layer 130 providing the core function, and the insulating layer 140 for protection remain on the final printed circuit board. If the electromagnetic shielding film 100 also includes a connecting interlayer, then the connecting interlayer is also included.
[0078] The circuit board body 200 is a flexible circuit board or a rigid circuit board.
[0079] In the description of this specification, the references to terms such as "this embodiment," "an embodiment," "some embodiments," "example," "specific example," or "some examples," etc., refer to specific features, structures, materials, or characteristics described in connection with that embodiment or example, which are included in at least one embodiment or example of this application. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples. Furthermore, those skilled in the art can combine and integrate the different embodiments or examples described in this specification and the features of different embodiments or examples without contradiction. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of this application, "a plurality of" means at least two, such as two, three, etc., unless otherwise explicitly specified.
[0080] The above description does not provide detailed explanations of the technical aspects of each layer's patterning, etching, etc. However, those skilled in the art should understand that various technical means can be used to form layers and regions of the desired shape. Furthermore, to form the same structure, those skilled in the art can also design methods that are not entirely identical to those described above. Additionally, although various embodiments have been described above, this does not mean that the measures in the various embodiments cannot be used advantageously in combination.
[0081] The above description is merely a preferred embodiment and the technical principles employed in this application. Those skilled in the art will understand that this application is not limited to the specific embodiments described above, and various obvious changes, readjustments, combinations, and substitutions can be made without departing from the scope of protection of this application. Therefore, although this application has been described in detail through the above embodiments, this application is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of this application. The scope of protection of this application is determined by the scope of the appended claims.
Claims
1. An electromagnetic shielding film, characterized in that, include: An insulating layer, a metal shielding layer, and an adhesive film layer, wherein the metal shielding layer is located between the insulating layer and the adhesive film layer; The metal shielding layer is provided with a plurality of openings that penetrate the metal shielding layer in the thickness direction; The aperture of the opening gradually decreases from the adhesive film side to the insulating layer side.
2. The electromagnetic shielding film according to claim 1, characterized in that, The difference between the diameter of the opening on the insulating layer side of the aperture and the diameter of the opening on the adhesive film side of the aperture is defined as the aperture difference. The arithmetic mean of the diameter of the opening on the insulating layer side of the aperture and the diameter of the opening on the adhesive film side of the aperture is defined as the aperture mean. The ratio of the aperture difference to the average aperture is less than 0.
3.
3. The electromagnetic shielding film according to claim 2, characterized in that, The ratio of the aperture difference to the average aperture is 0.1 to 0.
25.
4. The electromagnetic shielding film according to claim 2, characterized in that, The arithmetic mean thickness of the metal shielding layer is defined as H; The diameter of the opening on one side of the adhesive film layer with the aperture is defined as B; The arithmetic mean thickness H of the metal shielding layer and the diameter B of the opening on one side of the perforated adhesive film layer satisfy the relationship that B > 5H.
5. The electromagnetic shielding film according to claim 3, characterized in that, The aperture of the opening facing the insulating layer is 10μm~100μm.
6. The electromagnetic shielding film according to claim 1, characterized in that, The openings are arranged in an array; The residual copper content of the metal shielding layer is 65%~95%.
7. The electromagnetic shielding film according to claim 1, characterized in that, The adhesive film layer has a melt viscosity of 5000 Pa within a temperature range of 80℃ to 120℃. s ~20000Pa s.
8. The electromagnetic shielding film according to claim 1, characterized in that, The arithmetic mean thickness H of the metal shielding layer is 0.5 μm to 5 μm.
9. The electromagnetic shielding film according to claim 1, characterized in that, Also includes: A carrier film covers the surface of the insulating layer facing away from the metal shielding layer; A protective film covers the surface of the adhesive film layer facing away from the metal shielding layer; Both the carrier film and the protective film are release films.
10. A printed circuit board, characterized in that, include: Circuit board body, The electromagnetic shielding film as described in any one of claims 1 to 9 is attached to at least one surface of the circuit board body; the adhesive film layer is located on the side of the electromagnetic shielding film closer to the circuit board body, and the insulating layer is located on the side of the electromagnetic shielding film away from the circuit board body; The circuit board body is a flexible circuit board or a rigid circuit board.