Back-illuminated visible extended InGaAs detector with integrated mie-resonant silicon nitride nanorod super surface and preparation method thereof
By integrating a Mie resonant silicon nitride nanopillar metasurface structure onto a PIN photosensitive chip, the problems of high visible light absorption loss and high-temperature processing damage in back-illuminated InGaAs detectors were solved, achieving improved optical performance with low reflectivity and high transmittance.
Patent Information
- Application Number
- CN202611258775.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-19
- Publication Date
- 2026-11-10
AI Technical Summary
Existing back-illuminated extended-visibility InGaAs detectors have low quantum efficiency in the visible light band, high-temperature processing leads to indium pillar interconnect failure, poor uniformity of microstructure array wafer patterns, and conventional microstructures are difficult to achieve wide-angle low reflectivity and high transmittance.
By employing an integrated Mie resonant silicon nitride nanopillar metasurface structure, silicon nitride nanopillars are constructed on a PIN photosensitive chip using a low-temperature fabrication process. Combined with indium pillar interconnects, this achieves low-temperature processing and enhanced high-efficiency optical performance.
Within the incident angle range of 0~75°, the average reflectivity in the 400~1700nm band is ≤15%, and the visible light quantum efficiency is improved by 10%~20%, avoiding high-temperature damage and uneven patterning.
Smart Images

Figure CN123076035A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of visible-shortwave infrared focal plane detector manufacturing technology, specifically to a back-illuminated extended visible InGaAs detector with an integrated Mie resonant silicon nitride nanopillar metasurface and its fabrication process. It is applicable to the fabrication of extended visible InGaAs detectors of various specifications such as 640×512, 1280×1024, and 2560×2048 with a photosensitive element center-to-center distance of 10μm~30μm. Background Technology
[0002] Room-temperature operating back-illuminated extended-visibility InGaAs detectors can simultaneously respond to the 400–1700 nm visible light and short-wave infrared spectra, making them valuable for applications in low-light night vision and multispectral remote sensing equipment. These devices require the removal of the InP substrate, retaining only a nanoscale N-InP contact layer as the light incident window. However, InP materials have a high absorption coefficient in the visible light band, making it difficult to achieve wide-angle, wide-band low-reflection effects using only a single-layer dielectric passivation film. Consequently, the quantum efficiency of these devices in the visible band is generally low, limiting the signal-to-noise ratio in low-light imaging.
[0003] Currently, the industry primarily employs surface microstructures to achieve anti-reflection functionality. Existing micro / nano molding processes mostly utilize nanoimprinting technology, with photoresist curing temperatures generally exceeding 180°C. However, back-illuminated InGaAs photosensitive chips require pre-connection to the readout circuit via indium pillars. High-temperature processing can cause the indium alloy to melt, leading to interconnect failure. Furthermore, the microstructure arrays fabricated by nanoimprinting exhibit poor uniformity on large-area wafer patterns, and the demolding process can easily scratch the ultrathin InP layer, introducing surface leakage channels and increasing the blind cell rate of the detector.
[0004] In addition, conventional microstructures rely solely on interface gradients to achieve refractive index matching, lacking design for controlling the resonant light field in the visible band. Their photon capture capability in the 400nm~600nm band is limited, and their reflection performance degrades significantly under oblique incidence conditions. Existing semiconductor microstructures mostly use InP materials, which have high visible light absorption loss, making it difficult to simultaneously meet the requirements of high visible light transmittance and wide-angle low reflection. Summary of the Invention
[0005] The purpose of this invention is to overcome the common problems of existing back-illuminated extended visible InGaAs detectors, such as large visible light absorption loss, high wide-angle reflection of conventional antireflection structures, and high temperature damage to indium pillar interconnects during micro-nano fabrication. This invention provides a back-illuminated extended visible InGaAs detector with an integrated Mie resonant silicon nitride nanopillar metasurface, and also provides a matching fabrication method that is compatible with low temperature throughout the process.
[0006] Based on the above objectives, the specific technical solution of the present invention is as follows: a back-illuminated extended visible InGaAs detector with integrated Mie resonant silicon nitride nanopillar metasurface, characterized in that it includes a readout circuit and a PIN photosensitive chip, which are connected by an indium pillar interconnect structure; the PIN photosensitive chip is composed of an N-type InP cap layer, an intrinsic InGaAs absorption layer, and an ultrathin N-InP contact layer stacked sequentially; the thickness of the ultrathin N-InP contact layer is 8~12nm; a silicon nitride underlayer film and a periodic silicon nitride cylindrical nanopillar metasurface that generates Mie resonance at a wavelength of 450nm are sequentially disposed on the back side of the ultrathin N-InP contact layer.
[0007] Furthermore, the silicon nitride underlayer film has a thickness of 85~95nm; the nanopillars containing the micropillar metasurface are vertical cylindrical structures with a diameter of 210nm~230nm, an array period of 440~450nm, and a pillar height of 190~210nm; the nanopillars are made of silicon nitride, and the maximum temperature of the entire fabrication process of the silicon nitride nanopillar metasurface does not exceed 120℃, and the electron beam photoresist baking temperature is controlled at 95℃.
[0008] Furthermore, the ultrathin N-InP contact layer is preferably 10 nm thick; the silicon nitride bottom film is preferably 90 nm thick; the nanopillars are preferably 220 nm in diameter, 440 nm in period, and 200 nm in height, with no gradual tilt on the sidewalls of the nanopillars.
[0009] Furthermore, the photosensitive element center-to-center distance of the PIN photosensitive chip is 10μm~30μm, and it is compatible with array sizes of 640×512, 1280×1024, 2560×2048, etc.; within the incident angle range of 0°~75°, the device has an average reflectivity of ≤15% in the 400nm~1700nm wavelength band.
[0010] A method for fabricating a back-illuminated extended-visibility InGaAs detector with an integrated Mie resonant silicon nitride nanopillar metasurface, characterized by comprising the following steps:
[0011] Step S1, epitaxial growth of InGaAs epitaxial material with corrosion barrier layer: N-type InP buffer layer, N-type InGaAs barrier layer, ultrathin N-InP contact layer, intrinsic InGaAs absorber layer and N-type InP cap layer are sequentially grown on N-type InP substrate.
[0012] Step S2, prepare PIN photosensitive chip and complete flip-chip interconnection: the epitaxial wafer completes P-region selective diffusion, N-electrode trench etching, thickening electrode preparation, and indium pillar evaporation, and the PIN photosensitive chip and readout circuit are interconnected by indium pillar flip-chip to form a focal plane;
[0013] Step S3, selective substrate thinning: mechanical polishing combined with selective wet etching removes the InP substrate, N-type InP buffer layer and N-type InGaAs barrier layer, while retaining an 8~12nm ultrathin N-InP contact layer;
[0014] Step S4, Low-temperature deposition of silicon nitride underlayer film: On the surface of the ultrathin N-InP contact layer, silicon nitride underlayer film is deposited by inductively coupled plasma chemical vapor deposition at a temperature of 75℃ and a thickness of 285~295nm.
[0015] Step S5, Low-temperature electron beam lithography: Electron beam photoresist is spin-coated onto the surface of the silicon nitride underlayer film and cured at a low temperature of 95°C, using 80~140μC / cm. 2 Interval electron beam exposure and development to form photolithography masks;
[0016] Step S6, anisotropic etching to prepare nanopillars: The silicon nitride bottom film is anisotropically etched using reactive ions. After removing the photoresist, a silicon nitride nanopillar metasurface with a height of 190~210nm is formed, and the remaining silicon nitride bottom film has a thickness of 85~95nm.
[0017] Furthermore, in step S5, the preferred exposure dose is 100 μC / cm. 2 After etching, the diameter of the nanopillars stabilized at 220 nm.
[0018] Furthermore, step S6 employs a reactive ion anisotropic etching process, resulting in high verticality of the nanopillar sidewalls after etching, thus avoiding resonant wavelength shift.
[0019] The core improvements of this invention are divided into two main parts: device structure design and supporting fabrication process.
[0020] 1. Innovative device structure design
[0021] 1) The thickness range of the ultra-thin N-InP contact layer is precisely limited to 8~12nm. If it is too thick, it will absorb visible light significantly, and if it is too thin, the mechanical support strength of the photosensitive chip will be insufficient.
[0022] 2) A composite antireflection system was constructed on the back side of an ultrathin N-InP contact layer. The bottom layer was paired with an 85~95nm silicon nitride film, and the top layer was prepared with periodic vertical silicon nitride cylindrical nanopillars. The target wavelength was 450nm visible light, and the column diameter, array period, and column height were matched based on the optimal value of Mie scattering efficiency.
[0023] 3) By utilizing the synergistic Mie resonance effect of dielectric nanopillar electric and magnetic dipoles to locally confine visible light, unlike the simple refractive index gradient matching approach, a low reflection level can be maintained continuously over a wide incident angle range of 0–75°; low-loss SiN is selected. x Dielectric materials that avoid the absorption of visible light by InP microstructures.
[0024] 2. Innovation in supporting low-temperature preparation processes
[0025] 1) Electron beam photoresist is used, and the curing and baking temperature is 95℃. The maximum temperature of the entire micro-nano processing is controlled within 120℃. After the photosensitive chip completes the indium pillar flip soldering and substrate removal process, the back microstructure processing can be carried out directly without damaging the indium pillar interconnect solder joints.
[0026] 2) Set to 80~140μC / cm 2 Gradient exposure range, quantitative compensation for electron beam pattern shrinkage error, and the size of the prepared nanopillars is highly matched with the theoretical resonance design value;
[0027] 3) Anisotropic RIE etching is used to form vertical sidewall nanopillars, avoiding the resonant wavelength shift caused by morphological changes; there is no nanoimprinting demolding step, eliminating scratches and leakage defects in the ultrathin InP contact layer, and the uniformity of the entire array pattern is significantly improved.
[0028] The beneficial effects of adopting the technical solution of this invention are as follows:
[0029] 1) Significant improvement in optical performance: The transmittance in the 450nm visible light band increased from 0.5 to over 0.8. Under any incident angle of 0~75°, the average reflectance across the entire 400~1700nm band is less than 15%, and the visible light quantum efficiency of the device is improved by 10%~20%.
[0030] 2) Significantly reduced process defects: The low-temperature preparation process eliminates the risk of indium pillar melting failure;
[0031] 3) It has good process versatility and can be seamlessly compatible with conventional planar InGaAs photosensitive chip front-end processes. It can be fabricated using existing 2-4 inch III-V process lines without the need for additional special equipment.
[0032] 4) The structure and process form an integrated complete solution, and a dedicated resonant microstructure design is formed to address the visible light loss problem of ultra-thin InP contact layer. Attached Figure Description
[0033] Figure 1 This is a schematic diagram of the cross-sectional structure of the InGaAs focal plane detector before substrate removal in specific embodiment 1;
[0034] Figure 2 This is a schematic diagram of the overall cross-sectional structure of the back-illuminated extended InGaAs detector with integrated Mie resonant silicon nitride nanopillar metasurface in specific embodiment 1.
[0035] Figure 3 This is a partial top view (i.e., from the perspective of) the Mie resonant silicon nitride nanopillar metasurface in Specific Embodiment 1. Figure 2The arrow indicates the "plane of incidence" as seen from the angle of photon incidence.
[0036] Figure 4 This is a schematic diagram of the complete metasurface preparation process in Specific Embodiment 1;
[0037] In the figure: 1-N-type InP substrate; 2-N-type InP buffer layer; 3-N-type InGaAs barrier layer; 4-Ultra-thin N-InP contact layer; 5-Intrinsic InGaAs absorber layer; 6-N-type InP cap layer; 7-SiN x Diffusion mask layer; 8-Photosensitive element diffusion hole; 9-Photosensitive element P-region; 10-Photosensitive element P-electrode; 11-N-electrode groove; 12-SiN x Passivation layer; 13-P thickened electrode; 14-N electrode; 15-P region interconnect In pillar; 16-N region interconnect In pillar; 17-Readout circuit; 18-Readout circuit interconnect In pillar; 19-SiN x Underlying thin film (i.e., silicon nitride underlying thin film); 20-nanopillar metasurface; d-nanopillar diameter; a-nanopillar period. Detailed Implementation
[0038] The following is in conjunction with the appendix Figures 1-4 In specific embodiment 1, taking a 10μm center-pitch 2560×2048 element back-illuminated extended InGaAs detector as an example, a detailed description of the integrated Mie resonant silicon nitride nanopillar metasurface is given.
[0039] This embodiment 1 provides a back-illuminated extended visible InGaAs detector with an integrated Mie resonant silicon nitride nanopillar metasurface, comprising a readout circuit and a PIN photosensitive chip, which are connected by an indium pillar interconnect structure; the PIN photosensitive chip consists of an N-type InP cap layer 6, an intrinsic InGaAs absorption layer 5, and an ultrathin N-InP contact layer 4 stacked sequentially; the thickness of the ultrathin N-InP contact layer 4 is 8~12nm; on the back side of the ultrathin N-InP contact layer 4, a silicon nitride underlayer film 19 and a periodic silicon nitride cylindrical nanopillar metasurface 20 that generates Mie resonance at a wavelength of 450nm are sequentially disposed.
[0040] The silicon nitride bottom film 19 has a thickness of 85~95nm; the nanopillars on which the micropillar metasurface 20 is located are vertical cylindrical structures with a diameter of 210nm~230nm, an array period of 440~450nm, and a pillar height of 190~210nm; the nanopillars are made of silicon nitride, and the highest temperature of the entire fabrication process of the silicon nitride nanopillar metasurface 20 does not exceed 120℃, and the electron beam photoresist baking temperature is controlled at 95℃.
[0041] The ultrathin N-InP contact layer 4 is preferably 10 nm thick; the silicon nitride bottom film 19 is preferably 90 nm thick; the nanopillars are preferably 220 nm in diameter, 440 nm in period, and 200 nm in height, with no gradual tilt on the sidewalls. Here, "no gradual tilt" means that the nanopillars are perpendicular to the chip surface (close to 90° perpendicular) and have no tilt angle; for example, along the height direction of the nanopillars, the angle between the sidewalls and the substrate surface does not change continuously, and the sidewall profile is approximately a straight line; the change in the sidewall angle along the height direction is no more than 5°.
[0042] A method for fabricating a back-illuminated extended InGaAs detector with an integrated Mie resonant silicon nitride nanopillar metasurface includes step S1, epitaxially growing InGaAs epitaxial material with an etching barrier layer. Figure 1 As shown, epitaxial materials were grown using molecular beam epitaxy (MBE) at a thickness of 625 μm, a diameter of 3 inches, and a carrier concentration of 3 × 10⁻⁶. 18 cm -3 On an N-type InP substrate 1, a 1 μm N-type InP buffer layer 2 is sequentially grown, with a carrier concentration of 2~4×10⁻⁶. 18 cm -3 ; 0.5 μm N-type InGaAs barrier layer 3, carrier concentration 2~4×10 18 cm -3 ; Ultrathin N-InP contact layer 4, thickness 8~12nm, carrier concentration 2~4×10 18 cm -3 ; an intrinsic InGaAs absorber layer with a thickness of 2.5 μm and a carrier concentration of 5 × 10⁵. 15 cm -3 A 1 μm thick N-type InP cap layer 6 with a carrier concentration of 5 × 10⁶. 16 cm -3 .
[0043] Step S2 involves fabricating a PIN photosensitive chip and completing flip-chip interconnection. The diffusion, electrode, and indium pillar processes for the 2560×2048 element PIN photosensitive chip are essentially consistent with existing mature InGaAs photosensitive chip fabrication processes. A 300nm thick SiN layer is grown on the epitaxial material surface using plasma-enhanced chemical vapor deposition (PECVD). xDiffusion mask layer 7. Diffusion holes 8, with a diameter of Φ5μm, are obtained for the photosensitive element through photolithography and reactive ion etching. Closed-tube diffusion is performed using a Zn3P2 doped source at a diffusion temperature of 530℃ and a diffusion time of 10-13 minutes to form the P-region of the photosensitive element 9. P-electrode holes, with a size of Φ4μm, are obtained for the photosensitive element through photolithography and reactive ion etching. A single layer of Au with a thickness of 50nm is obtained by electron beam evaporation to form the P-electrode 10. N-electrode trenches 11, with a width of 40μm and a length of 12800μm, are obtained through photolithography and etching, with one trench on each side of the array. Selected areas of SiN are etched away. x A diffusion mask layer 7, an N-type InP cap layer 6, and an intrinsic InGaAs absorber layer 5 are formed, leading to the interface between the intrinsic InGaAs absorber layer 5 and the ultrathin N-InP contact layer 4. The N-electrode trench 11 has a depth of 3.5 μm. A 300 nm thick SiN layer is grown on the chip surface using plasma-enhanced chemical vapor deposition. x Passivation layer 12.
[0044] SiN was obtained through photolithography and reactive ion etching. x A passivation layer 12 exposes 2560×2048 photosensitive P-electrodes 10 and two N-electrode trenches 11. The diameter of the photosensitive P-electrodes 10 is Φ4μm, and the size of the N-electrode trenches 11 is 40μm×12800μm. A Ti / Au composite metal layer is obtained through photolithography and electron beam evaporation. The Ti metal layer is 50nm thick, and the Au metal layer is 300nm thick, resulting in photosensitive P-thickened electrodes 13 and N-electrodes 14. The size of the P-thickened electrodes 13 is Φ6.5μm, and the size of the N-electrodes 14 is 100μm×12800μm. A single layer of In is obtained through photolithography and thermal evaporation. The photosensitive elements P-region interconnect In pillar 15 and N-region interconnect In pillar 16 used for flip-soldering interconnection have a ball diameter of Φ5.5μm and a height of 5~7μm. A 3-inch wafer is diced to obtain four 2560×2048 element photosensitive chips. Each photosensitive chip and a matching 2560×2048 element readout circuit 17 are interconnected by flip-soldering through In pillars to form a focal plane detector. The readout circuit is fabricated with readout circuit interconnect In pillar 18 that is completely mirror-matched to the In pillars of the photosensitive chip. The flip-soldering pressure is 180kg~200kg to form a 2560×2048 element InGaAs focal plane detector.
[0045] Step S3: Selectively thin the substrate, and remove the N-type InP substrate 1, N-type InP buffer layer 2 and N-type InGaAs barrier layer 3 by mechanical polishing combined with selective wet etching, while retaining an 8~12nm ultrathin N-InP contact layer 4. The specific process flow is as follows: First, the interconnect In pillar regions of the InGaAs focal plane detector are reinforced with epoxy resin, which is then cured at room temperature for more than 24 hours. Photolithographic protective adhesive is spin-coated onto the surface of the focal plane detector, and most of the N-type InP substrate 1 is removed by mechanical rough polishing, reducing the substrate thickness from 625μm to about 100μm. Then, InP etching solution (hydrochloric acid: phosphoric acid = 3:1) is used for wet thinning at room temperature. This etching solution has good selectivity, with an etching rate of about 120nm / s for InP material and almost no etching for InGaAs material. This selective etching solution is used to completely remove the N-type InP substrate 1 and the N-type InP buffer layer 2. The N-type InGaAs barrier layer 3 is removed by wet etching with InGaAs etching solution (tartaric acid: hydrogen peroxide = 5:1). This etching solution has an etching rate of about 10nm / s for InGaAs material and almost no etching for InP material.
[0046] Step S4: Low-temperature deposition of silicon nitride underlayer film. On the surface of the ultrathin N-InP contact layer 4, SiNx underlayer film 19 is deposited by inductively coupled plasma chemical vapor deposition (ICPCVD) at a temperature of 75℃, with a thickness of 285~295nm.
[0047] Step S5: Low-temperature electron beam lithography. On SiN... x ZEP520A electron beam photoresist was spin-coated onto the surface of the bottom film 19 at a spin speed of 6000 oz / s and a spin time of 60 oz. The film was then cured at 95°C for 200 s. Electron beam exposure was performed in the range of 80~140 μC / cm². The nanopillar diameter d of the lithographic pattern was 210 nm~230 nm, and the nanopillar period a was 440~450 nm. o-xylene was used as the developer, and the development time was 90 s~120 s.
[0048] Step S6: Anisotropic etching to prepare nanopillars. RIE anisotropic etching (i.e., reactive ion anisotropic etching process) is used to fabricate SiN. x The bottom thin film 19 has an etching depth of approximately 200 μm and is made of SiN. xThe remaining thickness of the bottom thin film 19 is 85nm~95nm. After removing the electron beam photoresist, the nanopillar metasurface 20 is obtained. The height of the nanopillars is about 200nm, and the diameter d of the nanopillars is 210nm~230nm. SEM morphology observation shows that after etching, the sidewalls of the nanopillars are steep (i.e., high verticality, the standard for high verticality is the same as the standard for "no gradual tilt"), with no obvious tilt. In the incident range of 0°~75°, the detector has an average reflectivity of ≤15% in the 400nm~1700nm band, and the visible light quantum efficiency of the device is improved by 10%~20%.
[0049] This invention provides a complete processing flow adaptable to various visible extended InGaAs focal plane array detectors with photosensitive element center-to-center distances ranging from 10μm to 30μm, including sizes such as 640×512, 1280×1024, and 2560×2048. This invention addresses common challenges in back-illuminated InGaAs detectors, such as high visible light absorption loss, high-temperature process damage to indium pillar interconnects, and uneven large-area patterning in the microstructure array, by coupling a Mie resonant silicon nitride vertical nanopillar structure with an ultrathin N-InP contact layer and employing a 95℃ low-temperature electron beam lithography process.
Claims
1. A back-illuminated extended-visibility InGaAs detector with an integrated Mie resonant silicon nitride nanopillar metasurface, characterized in that, It includes a readout circuit and a PIN photosensitive chip, which are connected by an indium pillar interconnect structure. The PIN photosensitive chip consists of an N-type InP cap layer (6), an intrinsic InGaAs absorption layer (5), and an ultrathin N-InP contact layer (4) stacked in sequence. The thickness of the ultrathin N-InP contact layer (4) is 8~12nm. A silicon nitride bottom film (19) and a periodic silicon nitride cylindrical nanopillar metasurface (20) that generates Mie resonance at a wavelength of 450nm are sequentially disposed on the back side of the ultrathin N-InP contact layer (4).
2. The back-illuminated extended visible InGaAs detector with integrated Mie resonant silicon nitride nanopillar metasurface according to claim 1, characterized in that, The silicon nitride bottom film (19) has a thickness of 85~95nm; the nanopillars on which the nanopillar metasurface (20) is located are vertical cylindrical structures with a diameter of 210nm~230nm, an array period of 440~450nm, and a pillar height of 190~210nm; the nanopillars are made of silicon nitride, and the highest temperature of the complete fabrication process of the silicon nitride nanopillar metasurface (20) does not exceed 120℃, and the electron beam photoresist baking temperature is controlled at 95℃.
3. The back-illuminated extended visible InGaAs detector with integrated Mie resonant silicon nitride nanopillar metasurface according to claim 1, characterized in that, The ultrathin N-InP contact layer (4) is preferably 10 nm thick; the silicon nitride bottom film (19) is preferably 90 nm thick; the nanopillars are preferably 220 nm in diameter, 440 nm in period, and 200 nm in height; the sidewalls of the nanopillars are not gradually tilted.
4. A back-illuminated extended-visibility InGaAs detector with an integrated Mie resonant silicon nitride nanopillar metasurface according to claim 1 or 2, characterized in that, The photosensitive element center-to-center distance of the PIN photosensitive chip is 10μm~30μm, and it is compatible with array sizes of 640×512, 1280×1024, 2560×2048, etc.; within the incident angle range of 0°~75°, the device has an average reflectivity of ≤15% in the 400nm~1700nm wavelength band.
5. A method for fabricating a back-illuminated extended-visibility InGaAs detector with an integrated Mie resonant silicon nitride nanopillar metasurface, relating to the back-illuminated extended-visibility InGaAs detector with an integrated Mie resonant silicon nitride nanopillar metasurface as described in any one of claims 1 to 4, characterized in that, Includes the following steps: Step S1, epitaxial growth of InGaAs epitaxial material with corrosion barrier layer: N-type InP buffer layer (2), N-type InGaAs barrier layer (3), ultrathin N-InP contact layer (4), intrinsic InGaAs absorber layer (5) and N-type InP cap layer (6) are sequentially grown on N-type InP substrate (1). Step S2, prepare PIN photosensitive chip and complete flip-chip interconnection: the epitaxial wafer completes P-region selective diffusion, N-electrode trench etching, thickening electrode preparation, and indium pillar evaporation, and the PIN photosensitive chip and readout circuit are interconnected by indium pillar flip-chip to form a focal plane; Step S3, selectively thin the substrate: mechanical polishing combined with selective wet etching removes the InP substrate (1), N-type InP buffer layer (2) and N-type InGaAs barrier layer (3), while retaining an 8~12nm ultrathin N-InP contact layer (4). Step S4, Low-temperature deposition of silicon nitride underlayer film: On the surface of the ultrathin N-InP contact layer (4), silicon nitride underlayer film (19) is deposited by inductively coupled plasma chemical vapor deposition at a temperature of 75°C and a thickness of 285~295nm; Step S5, Low-temperature electron beam lithography: Electron beam photoresist is spin-coated onto the surface of the silicon nitride underlayer film (19), and cured at a low temperature of 95°C, using 80~140μC / cm 2 Interval electron beam exposure and development to form photolithography masks; Step S6, anisotropic etching to prepare nanopillars: The silicon nitride bottom film (19) is anisotropically etched by reactive ions. After removing the photoresist, a silicon nitride nanopillar metasurface (20) with a height of 190~210nm is formed. The remaining silicon nitride bottom film (19) has a thickness of 85~95nm.
6. The method for fabricating a back-illuminated extended visible InGaAs detector with an integrated Mie resonant silicon nitride nanopillar metasurface according to claim 5, characterized in that, In step S5, the preferred exposure dose is 100 μC / cm. 2 After etching, the diameter of the nanopillars stabilized at 220 nm.
7. The method for fabricating a back-illuminated extended visible InGaAs detector with an integrated Mie resonant silicon nitride nanopillar metasurface according to claim 5, characterized in that, Step S6 employs a reactive ion anisotropic etching process, resulting in high verticality of the nanopillar sidewalls after etching, thus avoiding resonant wavelength shift.