A method for preventing plate skipping in a fast lamp annealing machine

By preheating the protective gas in the transfer chamber and controlling the pressure and gas channel parameters, the problems of wafer skipping and slit door opening difficulties in the rapid lamp annealing machine were solved, achieving efficient wafer heat treatment and stable equipment operation.

CN123076189APending Publication Date: 2026-11-10SHANGHAI IND U TECH RES INST
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510583219.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-07
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

When the rapid lamp annealing machine heats wafers with a thickness of 450μm or less, the thin wafers are prone to being thrown out due to rapid heating, resulting in low working efficiency of the annealing machine and difficulty in opening the slit door.

Method used

The protective gas in the transfer chamber is preheated to 150℃-200℃. After the wafer is preheated at a low temperature for 15s-25s, it is transferred to the processing chamber. By controlling the pressure difference between the transfer chamber and the processing chamber, as well as the temperature and flow rate of the gas channel, the wafer is prevented from deforming or jumping during the transfer process, while ensuring that the slit door opens smoothly.

Benefits of technology

It effectively prevents wafer skipping, improves work efficiency, saves costs, and ensures the smooth opening of the slit door, thereby improving heating efficiency and equipment operation stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123076189A_ABST
    Figure CN123076189A_ABST
Patent Text Reader

Abstract

This invention provides an anti-wafer skipping control method for a rapid lamp annealing machine, belonging to the field of semiconductor heat treatment technology. The anti-wafer skipping control method includes: heating a protective gas in the gas channel of the transfer cavity to any value between 150°C and 200°C before the wafer is transferred to the transfer cavity; introducing the heated protective gas after the wafer enters the transfer cavity and maintaining it for 15s-25s; transferring the wafer to the processing cavity and heat-treating the wafer at a heating rate greater than a first threshold, wherein the initial temperature of the processing cavity is any value between 90°C and 110°C. The anti-wafer skipping control method of this invention can improve work efficiency while preventing wafer skipping.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of semiconductor heat treatment technology, and in particular to a method for preventing chip skipping in a fast lamp annealing machine. Background Technology

[0002] A rapid lamp annealing machine (or rapid lamp annealing furnace, abbreviated as RTA) is a commonly used heat treatment equipment in semiconductor manufacturing, mainly used for rapid heating and cooling of wafers.

[0003] Rapid lamp annealing machines utilize high-intensity halogen lamps or infrared lamps as radiant heat sources, with their core processing chamber capable of instantaneously heating the wafer surface. This heating method is characterized by an extremely rapid temperature rise rate, reaching tens to hundreds of degrees Celsius per second, with maximum temperatures typically reaching 1000-1100 degrees Celsius. Furthermore, the processing chamber is equipped with a rotating stage capable of rotating at 240 RPM. Due to this rapid heating characteristic, wafers with a thickness of 450 μm or less are prone to deformation during rotational heat treatment, easily becoming ejected and triggering an alarm. In such cases, the wafer's position must be observed; if the fragment is far away, the processing chamber must be opened to manually remove the wafer, and the process restarted. This requires repeated adjustments to the heating rate between 25°C / s and 50°C / s, increasing setup time, reducing machine uptime, and severely impacting the annealing machine's efficiency. Summary of the Invention

[0004] One object of the present invention is to provide an anti-wafer skipping control method for a fast lamp annealing machine, which can improve work efficiency while preventing wafer skipping.

[0005] A further objective of this invention is to save costs.

[0006] Another objective of this invention is to ensure the smooth opening of the slit door.

[0007] Embodiments of the present invention provide a method for preventing wafer skipping in a rapid lamp annealing machine. The rapid lamp annealing machine includes a transfer chamber and a processing chamber. The transfer chamber is provided with a gas channel for introducing protective gas, and a heater is provided at the gas channel. An openable and closable slit door is provided between the transfer chamber and the processing chamber, and a conveying device for conveying wafers is provided. The method includes:

[0008] Before the wafer is transferred to the transfer cavity, the protective gas in the gas channel of the transfer cavity is heated to any value between 150°C and 200°C.

[0009] After the wafer enters the transfer cavity, the heated protective gas is introduced and maintained for 15-25 seconds.

[0010] The wafer is transferred to the processing cavity and heat-treated at a heating rate greater than a first threshold, wherein the initial temperature of the processing cavity is any value between 90°C and 110°C.

[0011] Furthermore, the process includes the following steps prior to transferring the wafer to the processing cavity:

[0012] The pressure in the transfer chamber is controlled to be between a value lower than the pressure in the processing chamber and higher than the minimum allowable pressure.

[0013] Furthermore, the step of controlling the pressure in the transfer chamber to a value between lower than the pressure in the processing chamber and higher than the minimum permissible pressure also includes:

[0014] The actual temperature of the transfer chamber is collected so that the pressure in the transfer chamber can be controlled to a value that is inversely proportional to the actual temperature of the transfer chamber.

[0015] Furthermore, the process includes the following steps prior to transferring the wafer to the processing cavity:

[0016] After the slit door has been open for a preset period of time, the pressure in the transfer chamber is increased.

[0017] Furthermore, after the slit door has been open for a preset period of time, the flow rate of the gas channel is increased.

[0018] Furthermore, there are multiple gas channels, all of which are arranged within a preset fan-shaped area on the bottom surface of the transfer chamber. The gas channel that is farther away from the center of the preset fan-shaped area has a higher heating temperature.

[0019] Furthermore, the flow rate of the gas channel is smaller the further away from the center of the preset fan-shaped area.

[0020] Furthermore, anti-skid control methods also include:

[0021] When the rapid lamp annealing machine is in standby mode, the heating temperature in the gas channel of the transfer chamber is controlled to any value between 90°C and 110°C.

[0022] Furthermore, the first threshold is any value between 75℃ / s and 90℃ / s.

[0023] According to a first aspect of the invention, by preheating the protective gas to 150°C-200°C and introducing the preheated protective gas into the transfer cavity before it enters the processing cavity, the wafer arriving at room temperature can be preheated at a low temperature and held for 15-25 seconds before being transferred to the processing cavity, where it is directly and rapidly heated. This method of preheating the wafer in the transfer cavity effectively avoids deformation and wafer skipping caused by rapid heating of the wafer directly from room temperature. Furthermore, by utilizing the preheating method with the protective gas in the transfer cavity, preheating can be performed directly when the wafer enters the transfer cavity, thereby improving heating efficiency.

[0024] Furthermore, heating the transfer chamber directly using protective gas eliminates the need for a separate preheating chamber, which helps save costs.

[0025] Furthermore, the transfer chamber and the processing chamber are located close to each other, which helps to maintain the heat of the wafer and prevents it from cooling down and consuming heat due to long transmission distances.

[0026] According to a second aspect of the invention, since the transfer chamber is preheated, a temperature difference exists between the transfer chamber and the processing chamber. The transfer chamber is a high-temperature chamber relative to the processing chamber, therefore the hot gas in the transfer chamber expands more easily and flows to the low-temperature chamber, causing a sudden pressure surge at the moment the slit door opens. This embodiment, by controlling the pressure in the transfer chamber to be lower than the pressure in the processing chamber but higher than the minimum permissible pressure, can mitigate the pressure surge caused by the temperature difference between the transfer chamber and the processing chamber, ensuring the smooth opening of the slit door.

[0027] Furthermore, while ensuring the smooth opening of the slit door, the influence of the actual temperature of the transfer chamber was also considered. Different pressures were set at different actual temperatures to make the pressure of the transfer chamber more compatible with its actual temperature, thereby further ensuring the smooth opening of the slit door.

[0028] According to a third aspect of the present invention, a corresponding temperature and flow control strategy is provided for the gas channels that are not uniformly arranged at the bottom. By setting the temperature of the gas channels on both sides higher, it is beneficial to balance the temperature of the area without gas channels with the temperature of the area with gas channels.

[0029] Furthermore, setting a larger flow rate in the intermediate gas channel can promote the flow of air towards the area where no gas channel is arranged. The synergy of temperature and flow rate can enable the transfer chamber to be heated quickly and evenly. Attached Figure Description

[0030] Figure 1 A flowchart of an anti-skid control method according to an embodiment of the present invention;

[0031] Figure 2 A flowchart of an anti-skid control method according to another embodiment of the present invention;

[0032] Figure 3 This is a top view schematic diagram of the transfer chamber of a rapid lamp annealing machine according to an embodiment of the present invention;

[0033] Figure label:

[0034] 10-Transfer chamber, 20-Gas passage, 30-Temperature sensor, 40-Pressure control valve, 101-Preset sector area. Detailed Implementation

[0035] To make the above-mentioned objectives, features, and advantages of this application more apparent and understandable, the specific embodiments of this application are described in detail below with reference to the accompanying drawings. Many specific details are set forth in the following description to provide a thorough understanding of this application. However, this application can be implemented in many other ways different from those described herein, and those skilled in the art can make similar modifications without departing from the spirit of this application. Therefore, this application is not limited to the specific embodiments disclosed below.

[0036] It should be noted that when a component is referred to as being "fixed to" or "set on" another component, it can be directly on the other component or there may be an intermediate component. When a component is considered to be "connected to" another component, it can be directly connected to the other component or there may be an intermediate component present. The terms "vertical," "horizontal," "upper," "lower," "left," "right," and similar expressions used in this application's specification are for illustrative purposes only and do not represent the only possible implementation.

[0037] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of this application, "multiple" means at least two, such as two, three, etc., unless otherwise explicitly specified.

[0038] In this application, unless otherwise expressly specified and limited, "above" or "below" the second feature can mean that the first feature is in direct contact with the second feature, or that the first feature and the second feature are in indirect contact through an intermediate medium. Furthermore, "above," "over," and "on top" the second feature can mean that the first feature is directly above or diagonally above the second feature, or simply indicates that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature can mean that the first feature is directly below or diagonally below the second feature, or simply indicates that the first feature is at a lower horizontal level than the second feature.

[0039] Unless otherwise defined, all technical and scientific terms used in this application have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used in this application is for the purpose of describing particular embodiments only and is not intended to be limiting of the application. The term "and / or" as used in this application includes any and all combinations of one or more of the associated listed items.

[0040] Figure 1 This is a flowchart of an anti-wafer skipping control method according to an embodiment of the present invention. The anti-wafer skipping control method of the present invention is used in a rapid lamp annealing machine (e.g., an AMAT Centura rapid lamp annealing machine). The rapid lamp annealing machine includes a transfer chamber and a processing chamber. The transfer chamber has a gas channel for introducing a protective gas, which can be an inert gas such as nitrogen and / or argon, to form a protective atmosphere and prevent oxidation or other adverse reactions. A heater, such as a heating strip attached to the gas channel, is provided at the gas channel, and a temperature controller is also installed for temperature control. An openable and closable slit door and a conveying device for transferring wafers are provided between the transfer chamber and the processing chamber. The slit door is generally located on the side wall of the chamber. The normal heating rate of this rapid lamp annealing machine is about 75°C / s, and the maximum heating rate can reach 100°C / s. In standby mode, the temperature in each chamber is maintained at about 100°C. However, at the moment the heating lamp is turned on, the temperature in the processing chamber instantly reaches a high temperature of about 390°C. Figure 1 As shown, in one embodiment, the anti-skid control method includes the following steps:

[0041] Step S100: Before the wafer is transferred to the transfer cavity, the protective gas in the gas channel of the transfer cavity is heated to any value between 150°C and 200°C.

[0042] Step S200: After the wafer enters the transfer cavity, a heated protective gas is introduced and maintained for 15s-25s;

[0043] In step S300, the wafer is transferred to the processing cavity and heat-treated at a heating rate greater than a first threshold. The initial temperature of the processing cavity is any value between 90°C and 110°C.

[0044] In step S100, the heating temperature of the protective gas can be 150℃, 160℃, 170℃, 175℃, 180℃, 190℃, 195℃ or 200℃, or any other value between 150℃ and 200℃, and there is no limitation here.

[0045] Step S200 is used to preheat the wafer. The preheating holding time can be 15s, 17s, 18s, 20s, 22s or 25s, or any other value between 15s and 25s. No restrictions are imposed here.

[0046] In step S300, the initial temperature of the processing chamber can be 90°C, 95°C, 100°C, 105°C, or 110°C, or any other value between 90°C and 110°C, without limitation. The first threshold is the normal, higher, or highest rate of rapid heating of the processing chamber. In one embodiment, the first threshold is any value between 75°C / s and 90°C / s. For example, the first threshold can be 75°C / s, 80°C / s, 85°C / s, or 90°C / s, or any other value between 75°C / s and 90°C / s, without limitation.

[0047] This embodiment preheats the protective gas to 150℃-200℃ and introduces this preheated protective gas into the transfer cavity before it enters the processing cavity. This allows for low-temperature preheating of the wafer from room temperature for 15-25 seconds before it is transferred to the processing cavity, where it undergoes rapid heating. This preheating of the wafer in the transfer cavity effectively avoids deformation and wafer skipping that occur when the wafer is rapidly heated directly from room temperature. Furthermore, the preheating with the protective gas in the transfer cavity improves heating efficiency as the wafer enters the cavity. Additionally, direct heating with the protective gas in the transfer cavity eliminates the need for a separate preheating chamber, saving costs. The adjacent placement of the transfer and processing cavities also helps maintain the wafer's heat, preventing cooling and heat loss due to long transfer distances.

[0048] Figure 2 This is a flowchart of an anti-skid control method according to another embodiment of the present invention. In one embodiment, the method further includes the following steps before step S300:

[0049] Step S240: Control the pressure in the transfer chamber to a value between lower than the pressure in the processing chamber and higher than the minimum allowable pressure.

[0050] To ensure the smooth opening of the slit between the two chambers, the pressure difference between them needs to be controlled within a target pressure difference, such as 5 Torr. Therefore, it's generally necessary to keep the pressures in the two chambers as consistent as possible; for example, maintaining the pressures in both the transfer chamber and the processing chamber at 780 Torr. In this embodiment, the minimum permissible pressure, i.e., the minimum pressure value in the transfer chamber that can maintain the aforementioned target pressure difference, is 775 Torr when the target pressure difference is 5 Torr and the pressure in the processing chamber is 780 Torr.

[0051] In this embodiment, because the transfer chamber is preheated, a temperature difference exists between the transfer chamber and the processing chamber. The transfer chamber is the higher-temperature chamber compared to the processing chamber. Therefore, the hot gas in the transfer chamber expands more easily and flows to the lower-temperature chamber, causing a sudden pressure surge when the slit door opens. This embodiment mitigates the pressure surge caused by the temperature difference between the transfer chamber and the processing chamber by controlling the pressure in the transfer chamber to be lower than the pressure in the processing chamber but higher than the minimum allowable pressure, thus ensuring the smooth opening of the slit door.

[0052] Figure 3 This is a top view schematic diagram of the transfer chamber 10 of a rapid lamp annealing machine according to an embodiment of the present invention. In a further embodiment, such as... Figure 3 As shown, a temperature sensor 30 for collecting the actual temperature of the transfer chamber 10 is also provided inside the transfer chamber 10. Before step S240, the following is also included:

[0053] Step S220: Collect the actual temperature of the transfer chamber 10.

[0054] In step S240, the pressure in the transfer chamber 10 is inversely proportional to the actual temperature of the transfer chamber 10. That is to say, in addition to meeting the conditions of being lower than the pressure of the processing chamber and higher than the minimum allowable pressure, the pressure in the transfer chamber 10 will also be adjusted according to the actual temperature of the transfer chamber 10. That is, when the actual temperature of the transfer chamber 10 is higher, the pressure in the transfer chamber 10 is set lower.

[0055] This embodiment ensures the smooth opening of the slit door while also taking into account the influence of the actual temperature of the transfer chamber 10. Different pressures are set at different actual temperatures so that the pressure of the transfer chamber 10 is more matched with its actual temperature, further ensuring the smooth opening of the slit door.

[0056] In a further embodiment, such as Figure 2 As shown, after step S240, the following is also included:

[0057] Step S260: After the slit door has been open for a preset time, increase the pressure in the transfer chamber 10 and / or the flow rate in the gas channel 20.

[0058] like Figure 3 As shown, a pressure control valve 40 is also provided at the bottom surface of the transfer chamber 10. By increasing its opening degree, the amount of air supplied can be increased, thereby increasing the pressure inside the transfer chamber 10. The preset duration in step S260 is used to ensure that the slit door has been opened to a certain degree, such as fully open or 3 / 4 open. Of course, in addition to predicting the opening degree of the slit door based on the opening time, the opening degree of the slit door can also be directly collected, or the opening degree of the slit door can be indirectly predicted using other methods. There are no restrictions here.

[0059] In this embodiment, after the slit door has reached a certain opening, by increasing the pressure of the pressure transfer chamber 10 and / or increasing the flow rate of the gas channel 20, the relatively low temperature air in the processing chamber can be effectively impacted. The impact area forms a temperature transition zone between the transfer chamber 10 and the processing chamber, so that the wafer has a good temperature buffer during transfer, further reducing the possibility of wafer deformation.

[0060] In one embodiment, such as Figure 3 As shown, there are multiple gas channels 20, all of which are arranged in a pre-defined fan-shaped area 101 on the bottom surface of the transfer chamber 10 (see [reference]). Figure 3 Within the dotted area (as shown in the diagram). This is the original gas channel 20 arrangement of a rapid lamp annealing machine, with three gas channels 20. The central angle of the preset fan-shaped area 101 is less than 180°, meaning the coverage area of ​​the gas channels 20 does not exceed a semi-circular area. Therefore, uneven temperature distribution occurs when the heated protective gas enters. In this embodiment, the heating temperature of the gas channels 20 farther from the center of the preset fan-shaped area 101 is higher, and the flow rate of the gas channels 20 farther from the center of the preset fan-shaped area 101 is lower. For example... Figure 3 The heating temperature of the gas channels 20 on the left and right sides is higher than that of the gas channel 20 in the middle, and the flow rate of the gas channels 20 on the left and right sides is lower than that of the gas channel 20 in the middle.

[0061] This embodiment employs a corresponding temperature and flow control strategy for the non-uniformly arranged gas channels 20 at the bottom. By setting higher temperatures for the gas channels 20 on both sides, it helps to balance the temperature between the areas without gas channels 20 and the areas with gas channels 20. Furthermore, setting a higher flow rate for the middle gas channel 20 promotes airflow towards the areas without gas channels 20. The synergy of temperature and flow rate enables rapid and uniform heating within the transfer chamber 10.

[0062] Furthermore, this method of achieving uniform heating by controlling the temperature and flow rate of the gas channel 20 does not require changing the original design of the transfer chamber 10, thus making it simple and low-cost.

[0063] In a further embodiment, the anti-skid control method further includes the following steps:

[0064] When the rapid lamp annealing machine is in standby mode, the heating temperature in the gas channel 20 of the control transfer chamber 10 is controlled to be any value between 90℃ and 110℃, for example, the heating temperature is 90℃, 100℃ or 110℃, without any limitation.

[0065] In this embodiment, when the rapid annealing machine is in standby mode, the heating temperature in the gas channel 20 is controlled between 90°C and 110°C. When the transfer chamber 10 enters the working state, the protective gas can be rapidly heated to 150°C-200°C and maintained at the same standby temperature as the processing chamber and other chambers.

[0066] The embodiments described above are merely illustrative of several implementations of the present invention, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the invention patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these all fall within the protection scope of the present invention. Therefore, the protection scope of this invention patent should be determined by the appended claims.

Claims

1. A method for preventing wafer skipping in a rapid lamp annealing machine, the rapid lamp annealing machine comprising a transfer chamber and a processing chamber, the transfer chamber having a gas channel for introducing protective gas, a heater being provided at the gas channel, an openable and closable slit door being provided between the transfer chamber and the processing chamber, and a conveying device for conveying wafers, characterized in that, The method includes: Before the wafer is transferred to the transfer cavity, the protective gas in the gas channel of the transfer cavity is heated to any value between 150°C and 200°C. After the wafer enters the transfer cavity, the heated protective gas is introduced and maintained for 15-25 seconds. The wafer is transferred to the processing cavity and heat-treated at a heating rate greater than a first threshold, wherein the initial temperature of the processing cavity is any value between 90°C and 110°C.

2. The anti-skid control method for a rapid lamp annealing machine according to claim 1, characterized in that, The process includes, prior to the step of transferring the wafer to the processing cavity: The pressure in the transfer chamber is controlled to be between a value lower than the pressure in the processing chamber and higher than the minimum allowable pressure.

3. The anti-skid control method for a rapid lamp annealing machine according to claim 2, characterized in that, The step of controlling the pressure in the transfer chamber to a value between lower than the pressure in the processing chamber and higher than the minimum permissible pressure further includes: The actual temperature of the transfer chamber is collected so that the pressure in the transfer chamber can be controlled to a value that is inversely proportional to the actual temperature of the transfer chamber.

4. The anti-skid control method for a rapid lamp annealing machine according to claim 1, characterized in that, The process includes, prior to the step of transferring the wafer to the processing cavity: After the slit door has been open for a preset period of time, the pressure in the transfer chamber is increased.

5. The anti-skid control method for a rapid lamp annealing machine according to claim 1, characterized in that, After the slit door has been open for a preset period of time, the flow rate of the gas channel is increased.

6. The anti-skid control method for a rapid lamp annealing machine according to any one of claims 1-5, characterized in that, The number of gas channels is multiple, and they are all arranged in a preset fan-shaped area on the bottom surface of the transfer chamber. The gas channel that is farther away from the center of the preset fan-shaped area has a higher heating temperature.

7. The anti-skid control method for a rapid lamp annealing machine according to claim 6, characterized in that, The flow rate of the gas channel is smaller the further away from the center of the preset fan-shaped area.

8. The anti-skid control method for a rapid lamp annealing machine according to any one of claims 1-5, characterized in that, Also includes: When the rapid lamp annealing machine is in standby mode, the heating temperature in the gas channel of the transfer chamber is controlled to any value between 90°C and 110°C.

9. The anti-skid control method for a rapid lamp annealing machine according to claim 1, characterized in that, The first threshold is any value between 75℃ / s and 90℃ / s.