Method and device for adjusting the cut height of a double-sided vertical grinding machine

By measuring the silicon wafer thickness in real time and adjusting the cut height in a double-sided vertical grinding machine, the problems of low grinding efficiency and abnormal contact caused by silicon wafer thickness fluctuations are solved, achieving more efficient and safer silicon wafer processing.

CN123103513APending Publication Date: 2026-11-17XIAN ESWIN MATERIAL TECHNOLOGY CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611474341.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-21
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing double-sided vertical grinding equipment has difficulty effectively matching the cut height when dealing with fluctuations in silicon wafer thickness, resulting in low grinding efficiency or abnormal contact between the grinding wheel and the silicon wafer.

Method used

By measuring the silicon wafer thickness in real time during the V-groove inspection process and dynamically adjusting the cut height based on the measurement results, the silicon wafer thickness measuring device and control system can achieve the corresponding cut height correction, ensuring that each silicon wafer is ground at an appropriate cut height.

Benefits of technology

It improves silicon wafer grinding efficiency, reduces ineffective feed strokes, lowers the risk of abnormal contact between the grinding wheel and the silicon wafer, and enhances overall processing efficiency and equipment safety.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123103513A_ABST
    Figure CN123103513A_ABST
Patent Text Reader

Abstract

This disclosure relates to a method and apparatus for adjusting the cut height of a double-sided vertical polishing machine. The cut height adjustment method includes: during V-groove detection of the silicon wafer to be polished, measuring the thickness of the silicon wafer before polishing and generating a pre-polishing thickness measurement value; obtaining the pre-polishing thickness measurement value and determining a corresponding cut height correction value for the silicon wafer based on the pre-polishing thickness measurement value; and before polishing the silicon wafer, correcting the cut height of the silicon wafer during polishing based on the cut height correction value, so that the double-sided vertical polishing machine polishes the silicon wafer according to the corrected cut height. Therefore, a corresponding cut height can be set for each silicon wafer, improving polishing efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to the field of semiconductor manufacturing technology, and in particular to a method and apparatus for adjusting the cut height of a double-sided vertical grinding machine. Background Technology

[0002] In silicon wafer processing, double-sided vertical grinding equipment typically requires setting a cut height before grinding begins. The cut height is related to the initial control position of the grinding wheel before it enters the grinding feed. If the thickness of the incoming silicon wafer fluctuates, the equipment usually adopts a higher fixed cut height to reduce the risk of abnormal contact between the grinding components and the silicon wafer when the incoming wafer is too thick.

[0003] Silicon wafers typically undergo wire cutting before entering a double-sided vertical polishing machine. Due to factors such as differences in wire cutting equipment, wire breakage, wire skipping, and variations in wire tension, the thickness of the cut silicon wafers may vary between wafers. To accommodate thicker wafers, double-sided vertical polishing machines usually employ a higher fixed idle cutting height. This results in a longer ineffective feed stroke for thinner wafers, increasing the idle time before polishing and leading to low polishing efficiency. Summary of the Invention

[0004] This section provides a general overview of this disclosure, rather than a full disclosure of the entire scope or all features of this disclosure.

[0005] According to a first aspect of this disclosure, a method for adjusting the cut height of a double-sided vertical polishing apparatus is provided. The method includes: during V-groove detection of a silicon wafer to be polished, measuring the thickness of the silicon wafer before polishing and generating a pre-polishing thickness measurement value; obtaining the pre-polishing thickness measurement value and determining a corresponding cut height correction value for the silicon wafer to be polished based on the pre-polishing thickness measurement value; and before polishing the silicon wafer, correcting the cut height of the silicon wafer during polishing based on the cut height correction value, so that the double-sided vertical polishing apparatus polishes the silicon wafer to be polished according to the corrected cut height.

[0006] According to a second aspect of this disclosure, a device for adjusting the cut height of a double-sided vertical polishing apparatus is also provided. The device includes a silicon wafer thickness measuring device and a control system. During V-groove detection of the silicon wafer to be polished, the silicon wafer thickness measuring device measures the thickness of the silicon wafer before polishing and generates a pre-polishing thickness measurement value. The control system is communicatively connected to the silicon wafer thickness measuring device and is configured to acquire the pre-polishing thickness measurement value and determine a corresponding cut height correction value for the silicon wafer to be polished based on the pre-polishing thickness measurement value. The control system is further configured to correct the cut height of the silicon wafer to be polished during polishing based on the cut height correction value before polishing, so that the double-sided vertical polishing apparatus polishes the silicon wafer to be polished according to the corrected cut height. Attached Figure Description

[0007] Figure 1 This is a schematic diagram of an air-cutting height adjustment device for a double-sided vertical grinding apparatus according to an embodiment of the present disclosure.

[0008] Figure 2 for Figure 1 A schematic diagram showing the coordination between the silicon wafer thickness measuring device and the positioning unit.

[0009] Figure 3 This is a flowchart illustrating a method for adjusting the air cutting height of a double-sided vertical grinding apparatus according to an embodiment of this disclosure.

[0010] Figure 4 For calibration Figure 1 The flowchart of the device method. Detailed Implementation

[0011] The technical solutions in this disclosure will now be clearly and completely described with reference to the accompanying drawings.

[0012] It should be noted that, for clarity, not all features of a particular embodiment are described or shown in the specification and drawings. Furthermore, to avoid unnecessary details obscuring the technical solutions of interest in this disclosure, only the device structure closely related to the technical solutions of this disclosure is described and shown in the specification and drawings, while other details that are not closely related to the technical content of this disclosure and are known to those skilled in the art are omitted.

[0013] In the process of processing silicon wafers using a double-sided vertical grinding machine, the grinding wheel does not start grinding the wafer directly from an arbitrary position. The grinding wheel typically starts at a certain initial control position, a certain distance from the wafer surface, and then feeds towards the wafer. The stroke from the initial control position to the point where the grinding wheel contacts the wafer surface for grinding is called the empty cutting stroke (also known as the ineffective feed stroke), and the height corresponding to this initial control position is called the empty cutting height. A higher empty cutting height provides a larger distance between the grinding wheel and the wafer, which is beneficial for accommodating thicker incoming wafers, but increases the ineffective feed stroke for thinner wafers. A lower empty cutting height shortens the ineffective feed stroke, but if the incoming wafer thickness is greater than expected, it may cause abnormal contact between the grinding wheel and the wafer surface, damaging both the wheel and the wafer. Therefore, matching the empty cutting height to the actual thickness of the wafer to be ground helps to simultaneously control the ineffective feed stroke and the risk of abnormal contact.

[0014] In related technologies, a fixed cut height can be set for a batch of silicon wafers. For example, when the nominal incoming material thickness is 900 micrometers, the grinding wheel's starting feed position can be set to 910 micrometers. It is understandable that incoming silicon wafers can be obtained by wire cutting silicon ingots. Wire-cut silicon wafers may exhibit thickness differences between wafers due to variations in wire cutting equipment, wire breakage, wire skipping, or changes in wire tension. When the thickness of a particular silicon wafer is less than the nominal thickness, the grinding wheel will experience a longer cut stroke as it moves from the 910-micrometer position towards the thinner wafer, thus increasing the cut time and reducing grinding efficiency.

[0015] Reference Figure 1 The air-cutting height adjustment device for implementing the air-cutting height adjustment method can be combined with a double-sided vertical grinding machine. The double-sided vertical grinding machine may include a gripping unit 220, a positioning unit 240, a grinding unit 260, a cleaning and drying unit 280, and a storage unit 210. The processing route of the silicon wafer W to be ground can be... Figure 1 Starting from point A as shown, and in Figure 1 Point B indicates the end. The gripping unit 220 retrieves the silicon wafer W to be ground from the pre-grinding silicon wafer storage box 250. The conveying mechanism transports the silicon wafer W to be ground to the positioning unit 240 via the conveyor belt 230. The positioning unit 240 positions the silicon wafer W to be ground. After positioning, the conveying mechanism transports the silicon wafer W to be ground to the grinding unit 260. The grinding unit 260 uses grinding wheels 262 located on both sides of the silicon wafer W to perform double-sided grinding. The ground silicon wafer is transported to the cleaning and drying unit 280 for cleaning and drying, and then stored in the post-grinding silicon wafer storage box 270 via the storage unit 210. The gripping, conveying, positioning, grinding, cleaning, drying, and storage processes can be automatically controlled by the equipment software.

[0016] The cut height adjustment device includes a silicon wafer thickness measuring device 120 and a control system 140. The silicon wafer thickness measuring device 120 cooperates with the positioning unit 240 to complete the pre-grinding thickness measurement during the V-groove detection process of the V-groove positioning device 246 on the silicon wafer W to be ground. The control system 140 is communicatively connected to the silicon wafer thickness measuring device 120 to receive the pre-grinding thickness measurement value generated by the silicon wafer thickness measuring device 120. The control system 140 can also be communicatively connected to the feed control unit of the grinding unit 260 to determine the cut height correction value corresponding to the current silicon wafer W to be ground based on the pre-grinding thickness measurement value, and correct the cut height adopted by the grinding unit 260 for the current silicon wafer W to be ground using this cut height correction value before grinding. The grinding unit 260 then grinds the current silicon wafer W according to the corrected cut height.

[0017] Pre-grinding thickness measurement refers to the thickness measurement performed before the silicon wafer W to be ground enters the grinding unit 260 and undergoes double-sided grinding. V-groove detection refers to the detection of the positioning groove at the edge of the silicon wafer to determine the reference position of the silicon wafer in the circumferential direction. The V-groove can also be called a notch. V-groove detection does not mean that the actual contour of the positioning groove is strictly limited to the letter V, but rather it is used to characterize the edge positioning structure that can provide a circumferential positioning reference for the silicon wafer. The positioning unit 240 can detect this positioning structure using the V-groove positioning device 246 during the rotation of the silicon wafer W to be ground. When the V-groove positioning device 246 identifies the position of the V-groove, the control system 140 can control the silicon wafer W to be ground to stop at a predetermined circumferential position, or record the angle of the V-groove relative to the equipment coordinate system so that a unified positioning reference can be used in subsequent handling and grinding processes.

[0018] The silicon wafer thickness measuring device 120 performs measurements during the V-groove detection process, meaning that at least a portion of the time spent on thickness measurement overlaps with the time spent on V-groove detection. For example, while the positioning unit 240 drives the silicon wafer W to be polished to rotate in search of the V-groove, the silicon wafer thickness measuring device 120 can simultaneously acquire thickness measurement data. The silicon wafer thickness measuring device 120 does not need to wait for the V-groove detection to complete before initiating a measurement process independent of the positioning process, nor does it need to transport the silicon wafer W to be polished to an additional independent thickness measurement station. This saves overall polishing time and improves polishing efficiency.

[0019] The thickness measurement value before polishing can be a value obtained from data collected by the silicon wafer thickness measuring device 120, representing the thickness of the silicon wafer W to be polished before polishing. The thickness measurement value before polishing can be directly generated by the silicon wafer thickness measuring device 120, or it can be generated by the control system 140 after processing the raw measurement data output by the silicon wafer thickness measuring device 120. In some embodiments, the thickness measurement value before polishing uses the maximum value among multiple thickness measurement data. It is conceivable that when the measurement method or control strategy is adjusted, the thickness measurement value before polishing can also use the calibrated maximum value, or a measurement result that can characterize the thicker portion of the silicon wafer W to be polished. This disclosure does not limit the specific data format of the raw signal.

[0020] The communication connection between the control system 140 and the silicon wafer thickness measuring device 120 refers to the ability for the two to transmit data related to thickness measurement. This communication connection can be achieved through internal data lines, fieldbuses, or other wired communication structures, or through wireless communication structures suitable for the equipment environment. The control system 140 can be the existing equipment control system of the double-sided vertical grinding machine, or it can include an independent controller that works in conjunction with the existing equipment control system. The control system 140 may include, for example, a processor, a memory, and input / output interfaces. The memory can store computer-executable instructions for receiving thickness measurement data, performing thickness calculations, determining the cut height correction value, and sending control parameters to the grinding unit 260. When the processor executes the above instructions, it can implement the measurement value acquisition and cut height correction functions of this disclosure.

[0021] In this disclosure, the cut height correction value refers to the corrected target cut height determined based on the pre-grinding thickness measurement of the silicon wafer W to be ground, and used for this grinding of the silicon wafer W. The cut height correction value represents the corrected cut height itself, rather than an increment or difference relative to the original fixed cut height. Correcting the cut height of the silicon wafer W during grinding based on the cut height correction value means setting the cut height used for this grinding of the silicon wafer W to be ground as the cut height correction value. For example, when the control system 140 determines a cut height correction value of 805 micrometers for a silicon wafer W with a thickness measurement of 800 micrometers, 805 micrometers is the cut height used for this grinding of the silicon wafer W.

[0022] In some implementations, the control system 140 can also establish a correspondence between the measurement results of the current silicon wafer W to be polished and the polishing parameters. This correspondence can reduce the possibility that the thickness measurement value is mistakenly used for other silicon wafers. For example, the control system 140 can assign identification information to the silicon wafer when the gripping unit 220 acquires it, and associate the pre-polishing thickness measurement value generated by the positioning unit 240, the empty cut height correction value used by the polishing unit 260, and the status of subsequent processes with this identification information. The double-sided vertical polishing equipment operates according to a determined single-wafer conveying sequence, and the control system 140 maintains the correspondence between the measurement results and the current silicon wafer based on the workstation status and conveying sequence.

[0023] The air-cutting height adjustment device for a double-sided vertical grinding machine disclosed herein first obtains the actual thickness information of the silicon wafer W to be ground by the silicon wafer thickness measuring device 120. The control system 140 then converts the actual thickness information into an air-cutting height correction value corresponding to the current silicon wafer. The grinding unit 260 then starts the feeding process of the silicon wafer with the corrected air-cutting height. For silicon wafers with a thickness less than the thicker incoming material in the batch, the corrected air-cutting height can be lower than the fixed height originally set to accommodate thicker incoming materials, thereby shortening the air-cutting stroke from the starting control position to near the surface of the silicon wafer. For thicker silicon wafers, the corrected air-cutting height can be increased with the measured thickness, thereby reserving corresponding space before the grinding wheel enters the grinding feed. It is possible to set a corresponding air-cutting height for each silicon wafer, improving grinding efficiency while reducing the risk of abnormal contact.

[0024] Reference Figure 2 The positioning unit 240 may include a silicon wafer support stage 242, a drive motor 244, and a V-groove positioning device 246. The silicon wafer support stage 242 is used to support and hold the silicon wafer W to be ground. The drive motor 244 is connected to the silicon wafer support stage 242 and can drive the silicon wafer support stage 242 to rotate. When the silicon wafer W is held on the silicon wafer support stage 242, it rotates together with the silicon wafer support stage 242. The V-groove positioning device 246 is positioned towards the edge of the silicon wafer W to be ground, so as to detect the V-groove of the silicon wafer W during rotation.

[0025] A silicon wafer thickness measuring device 120 is positioned around the periphery of the silicon wafer W to be ground. (Refer to...) Figure 2 The silicon wafer thickness measuring device 120 is positioned opposite the V-groove positioning device 246 used for V-groove detection. In other arrangements that do not affect the operation of the double-sided vertical grinding equipment and the air-cutting height adjustment device, the silicon wafer thickness measuring device 120 may also be positioned adjacent to the V-groove positioning device 246.

[0026] The V-groove positioning device 246 and the silicon wafer thickness measuring device 120 can each complete the detection using the circumferential motion generated by the rotation of the silicon wafer W to be ground. The forward and backward movement area of ​​the silicon wafer thickness measuring device 120 and the detection area of ​​the V-groove positioning device 246 can be staggered, thereby reducing the possibility of mechanical interference when the two devices approach the silicon wafer simultaneously. The silicon wafer thickness measuring device 120 is set within the existing positioning unit 240, and the bearing, adsorption, and rotation functions of the positioning unit 240 can also be utilized, eliminating the need for a separate silicon wafer rotation mechanism for thickness measurement.

[0027] Reference Figure 2 The silicon wafer thickness measuring device 120 may include an upper probe 122 and a lower probe 124. The upper probe 122 is located on one side of the first surface of the silicon wafer W to be ground, and the lower probe 124 is located on the second surface of the silicon wafer W opposite to the first surface, and the upper probe 122 and the lower probe 124 correspond to each other in the thickness direction of the silicon wafer. When performing measurement, the silicon wafer thickness measuring device 120 can move relative to the silicon wafer W to be ground, so that the upper probe 122 and the lower probe 124 respectively reach a suitable position for measurement. After completing the measurement, the silicon wafer thickness measuring device 120 can move away from the silicon wafer W to provide space for the conveying mechanism to move the silicon wafer W into or out of the positioning unit 240.

[0028] The silicon wafer thickness measuring device 120 can employ a capacitive thickness measuring structure, a laser thickness measuring structure, or a contact thickness measuring structure. When using a capacitive thickness measuring structure, the upper probe 122 and lower probe 124 can obtain surface position information through changes in capacitance with the silicon wafer surface. When using a laser thickness measuring structure, the upper probe 122 and lower probe 124 can obtain the positions of the two surfaces through optical displacement measurement, and calculate the thickness based on the positional relationship between the two surfaces. When using a contact thickness measuring structure, the upper probe 122 and lower probe 124 can form controlled contact with the two surfaces of the silicon wafer, and obtain the thickness based on probe displacement. These are merely some possible implementations, and this disclosure does not limit the specific implementation of the silicon wafer thickness measuring device 120.

[0029] During the rotation of the silicon wafer W to be ground, the silicon wafer thickness measuring device 120 can measure multiple thickness measurement data of the silicon wafer W along a predetermined thickness measurement trajectory. The predetermined thickness measurement trajectory can be one or more circumferential trajectories extending around the center of the silicon wafer W. When the drive motor 244 drives the silicon wafer W to be ground to rotate, the upper probe 122 and lower probe 124, located at relatively fixed measurement positions, can sequentially sample at multiple circumferential positions. The multiple thickness measurement data can correspond to multiple measurement points spaced apart from each other in the circumferential direction, or to a set of measurement data formed by approximately continuous sampling. The number of samples and the sampling interval can be set according to the rotation speed of the silicon wafer W to be ground, the sampling frequency of the silicon wafer thickness measuring device 120, and the data processing capability of the control system 140.

[0030] The control system 140 can determine the maximum value among multiple thickness measurement data as the thickness measurement value before grinding. The maximum value represents the relatively thicker position on the measured circumferential trajectory. When using this maximum value as the thickness basis for calculating the cut height correction value, even if there is a certain thickness variation in the circumferential direction of the silicon wafer W to be ground, the control system 140 can still reserve corresponding feed space for the thicker part in the measured trajectory, reducing the risk of abnormal contact during the grinding process.

[0031] In some implementations, the control system 140 can determine the cut height correction value as the sum of the pre-grinding thickness measurement and a preset compensation amount. If H represents the cut height correction value (i.e., the corrected target cut height used in this grinding of the current silicon wafer W), T represents the pre-grinding thickness measurement of the current silicon wafer W, and Δ represents the preset compensation amount, then this relationship can be expressed as H = T + Δ. The preset compensation amount is used to create an additional interval based on the measured thickness of the current silicon wafer to accommodate measurement errors, equipment mechanical errors, and fluctuations during the feed control process.

[0032] The preset compensation amount can be pre-stored in the control system 140 and used in the calculation after the control system 140 obtains the pre-grinding thickness measurement value of the current silicon wafer W to be ground. In one embodiment, the preset compensation amount can be 5 micrometers, that is, the cut height correction value can be equal to the pre-grinding thickness measurement value plus 5 micrometers. For example, when the silicon wafer thickness measuring device 120 detects that the pre-grinding thickness measurement value of the current silicon wafer W to be ground is 800 micrometers, the control system 140 can determine the corresponding cut height correction value of the silicon wafer as 805 micrometers. As another example, when the pre-grinding thickness measurement value of another silicon wafer W to be ground is detected as 803 micrometers, the control system 140 can determine the corresponding cut height correction value of the silicon wafer as 808 micrometers. The two cut height correction values ​​follow the actual measured thickness changes of the two silicon wafers respectively, so that the starting control position of the grinding wheel of each silicon wafer is maintained at an interval of approximately 5 micrometers from its own thickness.

[0033] A 5-micron preset compensation value can be used to balance equipment safety and grinding efficiency. If the preset compensation value is set to greater than 5 microns, such as 10 microns, the cut height correction value for a silicon wafer with a thickness measurement of 800 microns will be 810 microns. Compared to a 5-micron compensation value, the grinding wheel will increase its ineffective feed distance by approximately 5 microns, and correspondingly increase the feed time. If the preset compensation value is set to less than 5 microns, such as 2 microns, the cut height correction value for a silicon wafer with a thickness measurement of 800 microns will be 802 microns. Measurement errors or equipment mechanical errors may increase the risk of damage to the grinding wheel teeth or breakage of the silicon wafer. Understandably, the preset compensation value can be appropriately increased or decreased for different equipment precision or process conditions.

[0034] The silicon wafer thickness measuring device 120 may develop measurement deviations after long-term operation or changes in environmental conditions, which may lead to errors in the final calculated actual cut height. For example, if the measured thickness is greater than the actual thickness, the calculated cut height will be correspondingly higher, increasing ineffective feed; if the measured thickness is smaller than the actual thickness, the calculated cut height will be correspondingly lower, reducing the actual gap between the grinding wheel and the silicon wafer and decreasing the safety of grinding. Therefore, it is conceivable that the control system 140 can also periodically calibrate the silicon wafer thickness measuring device 120.

[0035] The control system 140 can acquire the standard thickness value of a standard silicon wafer and the thickness measurement value obtained by the silicon wafer thickness measuring device 120 from the standard silicon wafer. The standard silicon wafer is a silicon wafer with a known thickness that can provide a comparison reference for the silicon wafer thickness measuring device 120; the standard thickness value can be the known maximum thickness of the standard silicon wafer. The control system 140 can pre-store the standard thickness value in its memory or receive the standard thickness value input by the operator in response to a calibration operation.

[0036] The control system 140 compensates for subsequent thickness measurements based on the difference between the measured thickness of the standard silicon wafer and the standard thickness value. If Tm represents the thickness measurement of the standard silicon wafer by the silicon wafer thickness measuring device 120, and Ts represents the standard thickness value, then the measurement difference can be expressed as e = Tm - Ts. The control system 140 determines a measurement compensation value C based on the measurement difference e and applies the compensation value C to subsequent thickness measurements. For example, when using linear translation compensation, the compensated thickness measurement can be expressed as Tc = Tr + C, where Tr is the subsequent original thickness measurement value, and Tc is the compensated thickness measurement value. The measurement compensation value C can have the opposite sign to the measurement difference e, making the compensated result closer to the standard thickness value.

[0037] In one embodiment, the known maximum thickness of a standard silicon wafer is 901 micrometers, and the maximum thickness measured by the silicon wafer thickness measuring device 120 is 902 micrometers. In this case, the measured thickness value is 1 micrometer larger than the standard thickness value. The measurement result can be uploaded to the control system 140, which can set a measurement compensation value in the range of approximately -1.5 micrometers to -0.5 micrometers, for example, -1 micrometer. After setting, the control system 140 applies the measurement compensation value to subsequent thickness measurements generated by the silicon wafer thickness measuring device 120, bringing the displayed value and the thickness value used in the cut height calculation closer to the standard thickness value.

[0038] After compensation, the control system 140 can reacquire the thickness measurement value of the standard silicon wafer measured by the silicon wafer thickness measuring device 120, and redetermine the difference between the reacquired thickness measurement value and the standard thickness value. If the absolute value of the difference between the reacquired thickness measurement value and the standard thickness value is less than 0.5 micrometers, the control system 140 ends the calibration of the silicon wafer thickness measuring device 120. Regardless of whether the difference is positive or negative, as long as its absolute value is less than 0.5 micrometers, it indicates that the deviation between the compensated measurement result and the standard value has entered the set calibration range.

[0039] If the absolute value of the difference between the remeasured thickness value and the standard thickness value is still greater than or equal to 0.5 micrometers, the control system 140 can readjust the measurement compensation value based on the new difference and continue to compensate using the adjusted measurement compensation value. Then, the standard silicon wafer is measured again, and the measurement results are compared. This process of measurement, difference calculation, compensation, and remeasurement is repeated multiple times until the absolute value of the difference is less than 0.5 micrometers. Compared to ending calibration directly based on a single measurement result, cyclic calibration can verify the compensation effect using the remeasurement results and reduce residual deviations caused by excessively large or small compensation settings.

[0040] The air-cutting height adjustment method disclosed herein can be executed by the aforementioned air-cutting height adjustment device, or by other double-sided vertical grinding equipment with corresponding measurement and control capabilities.

[0041] Reference Figure 3 The method includes: Step S320: During the V-groove detection process of the silicon wafer W to be polished, the thickness of the silicon wafer W to be polished before polishing is measured, and the thickness measurement value of the silicon wafer W to be polished before polishing is generated.

[0042] In step S320, the gripping unit 220 can retrieve the silicon wafer W to be ground from the pre-grinding silicon wafer storage box 250 and transport it to the positioning unit 240. The silicon wafer support platform 242 holds the silicon wafer W to be ground. The drive motor 244 drives the silicon wafer support platform 242 and the silicon wafer W to be ground to rotate, and the V-groove positioning device 246 searches for the V-groove of the silicon wafer W to be ground during the rotation. The silicon wafer thickness measuring device 120 measures the thickness of the silicon wafer W to be ground. Therefore, the thickness measurement does not need to occupy a complete silicon wafer rotation cycle after the V-groove detection is completed, improving the measurement efficiency.

[0043] Step S340: Obtain the thickness measurement value before grinding, and determine the empty cutting height correction value corresponding to the silicon wafer W to be ground based on the thickness measurement value before grinding.

[0044] In step S340, the silicon wafer thickness measuring device 120 can upload the measurement results to the control system 140. The control system 140 can first call the currently valid measurement compensation value to compensate the measurement results, and then calculate the cut height correction value based on the compensated pre-grinding thickness measurement value. If the device does not detect a state that requires updating the measurement compensation value after calibration, the control system 140 can continue to use the saved measurement compensation value.

[0045] Step S360: Before grinding the silicon wafer W, the cut height of the silicon wafer W to be ground is corrected based on the cut height correction value, so that the double-sided vertical grinding equipment grinds the silicon wafer W to be ground according to the corrected cut height.

[0046] In step S360, the control system 140 can write the empty cut height correction value into the grinding control parameters corresponding to the silicon wafer after the positioning unit 240 completes the V-groove positioning and before the silicon wafer W to be ground enters the grinding unit 260. The control system 140 completes the parameter writing after the silicon wafer W to be ground reaches the grinding unit 260 and before the grinding feed begins. The specific timing of parameter writing can be set according to the equipment control timing, as long as the grinding unit 260 uses the corrected empty cut height when it starts the grinding feed of the silicon wafer.

[0047] By using the air-cutting height adjustment method provided in this disclosure, the air-cutting height can be adjusted one by one according to the incoming thickness of different silicon wafers to be ground, thereby reducing the time waste caused by using a batch of uniform high values ​​for thinner silicon wafers and improving grinding efficiency.

[0048] In some embodiments, during step S320, when the silicon wafer W to be ground is subjected to V-groove detection, the silicon wafer W can be rotated, and multiple thickness measurement data of the silicon wafer W can be measured. Subsequently, the maximum value among the multiple thickness measurement data is determined as the thickness measurement value before grinding. The rotation of the silicon wafer W to be ground can be achieved by the drive motor 244 driving the silicon wafer support stage 242. Multiple thickness measurement data can be collected during one or more rotations and correspond to different positions on the same circumferential thickness measurement trajectory. The control system 140 or the silicon wafer thickness measurement device 120 compares multiple data and selects the maximum value, so that the subsequent empty cutting height calculation is based on the thicker position in the measured trajectory.

[0049] In some embodiments, in step S340, the control system 140 can determine the cut height correction value as the sum of the thickness measurement value before grinding and a preset compensation amount. The preset compensation amount can be stored as a process parameter of the equipment, and this calculation can be performed automatically after the control system 140 receives the thickness measurement value before grinding. Thus, the cut height correction value can change with the thickness measurement value, ensuring the safety of grinding and reducing ineffective feed strokes, thereby improving grinding efficiency.

[0050] In one embodiment, the preset compensation amount can be 5 micrometers. If the pre-grinding thickness measurement of the current silicon wafer W to be ground is 800 micrometers, the cut height correction value is 805 micrometers; if the pre-grinding thickness measurement of the next silicon wafer W to be ground is 803 micrometers, the cut height correction value is 808 micrometers. The control system 140 uses 805 micrometers and 808 micrometers respectively for the corresponding silicon wafers, instead of using one of the values ​​as a fixed setting for the entire batch of silicon wafers. This allows a pre-set distance of approximately 5 micrometers to be formed between the grinding wheel and the silicon wafer during grinding.

[0051] In some implementations, refer to Figure 4 The air-cutting height adjustment method also includes: Step S310: The thickness of a standard silicon wafer with a known thickness is measured to obtain the thickness measurement value of the standard silicon wafer. The standard silicon wafer can be placed on the silicon wafer support stage 242, and the drive motor 244 drives the standard silicon wafer to rotate. The silicon wafer thickness measuring device 120 measures the standard silicon wafer using the measurement position and sampling method used during normal production. The thickness measurement value can be the maximum value among multiple measurement data for comparison with the known maximum thickness of the standard silicon wafer.

[0052] Step S330: Determine the difference between the measured thickness value and the standard thickness value of the standard silicon wafer. The standard thickness value can be pre-entered into the control system 140. After receiving the measured thickness value uploaded by the silicon wafer thickness measuring device 120, the control system 140 subtracts the standard thickness value from the measured thickness value to obtain a signed difference. A positive difference indicates that the measured result is higher than the standard thickness value, and a negative difference indicates that the measured result is lower than the standard thickness value. The signed difference provides a basis for determining the compensation direction in the next step.

[0053] In step S350, compensation is applied to subsequent thickness measurements based on the difference. When the difference is positive, the control system 140 can set a negative measurement compensation value; when the difference is negative, the control system 140 can set a positive measurement compensation value. The compensation can be applied to the raw data output by the silicon wafer thickness measuring device 120, or it can be performed by the control system 140 after receiving the raw data. The thickness value used by the control system 140 for calculating the cut height can be the thickness value corrected by this measurement compensation value.

[0054] After compensating subsequent thickness measurements based on the difference, the thickness of the standard silicon wafer is measured again, and the measurement result is compensated. The control system 140 recalculates the difference between the compensated thickness measurement and the standard thickness value. If the absolute value of this difference is less than 0.5 micrometers, the calibration ends. If the absolute value of the difference is greater than or equal to 0.5 micrometers, the measurement compensation value is updated based on the new difference, and the process of re-measuring, compensating, and comparing continues until the absolute value of the difference between the re-measured and compensated thickness measurement and the standard thickness value is less than 0.5 micrometers. This reduces the impact of the measurement deviation of the silicon wafer thickness measurement device on the determination of the cut height.

[0055] It should be noted that the technical solutions described in this disclosure can be combined arbitrarily as long as they do not conflict.

[0056] In this disclosure, the terms "first," "second," etc., are used merely for descriptive purposes and should not be considered restrictive. Furthermore, although this disclosure has been described with reference to exemplary embodiments, it should be understood that this disclosure is not limited to the specific embodiments described and shown herein. Various changes to the exemplary embodiments can be made by those skilled in the art without departing from the scope defined by the claims of this disclosure.

[0057] The features mentioned and / or shown in the foregoing description of exemplary embodiments of this disclosure may be combined in the same or similar manner with one or more other embodiments, combined with features in other embodiments, or substituted for corresponding features in other embodiments. Such combinations or substitutions should also be considered as including within the scope of protection of this disclosure.

[0058] The above description is merely a specific embodiment of this disclosure, but the scope of protection of this disclosure is not limited thereto. Any changes or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this disclosure should be included within the scope of protection of this disclosure.

Claims

1. A method for adjusting the air cutting height of a double-sided vertical grinding machine, characterized in that, The method includes: During the V-groove detection process of the silicon wafer to be polished, the thickness of the silicon wafer to be polished is measured before polishing, and the thickness measurement value of the silicon wafer to be polished before polishing is generated. Obtain the thickness measurement value before grinding, and determine the blanking height correction value corresponding to the silicon wafer to be ground based on the thickness measurement value before grinding; and Before the silicon wafer to be polished is polished, the cut height of the silicon wafer to be polished is corrected based on the cut height correction value, so that the double-sided vertical polishing equipment polishes the silicon wafer to be polished according to the corrected cut height.

2. The method for adjusting the air cutting height of a double-sided vertical grinding equipment according to claim 1, characterized in that, The process of V-groove detection on the silicon wafer to be polished, including measuring the thickness of the silicon wafer before polishing and generating the pre-polishing thickness measurement value, specifically includes: During the V-groove inspection of the silicon wafer to be polished, the silicon wafer is rotated, and multiple thickness measurements are taken. The maximum value among the plurality of thickness measurement data is determined as the thickness measurement value before grinding.

3. The method for adjusting the air cutting height of a double-sided vertical grinding equipment according to claim 1, characterized in that, The step of obtaining the thickness measurement value before grinding and determining the cut height correction value corresponding to the silicon wafer to be ground based on the thickness measurement value before grinding includes: The air-cutting height correction value is determined as the sum of the thickness measurement value before grinding and the preset compensation amount.

4. The method for adjusting the air cutting height of a double-sided vertical grinding equipment according to claim 3, characterized in that, The preset compensation amount is 5 micrometers.

5. The method for adjusting the air cutting height of a double-sided vertical grinding equipment according to claim 1, characterized in that, Before the silicon wafer to be ground enters the grinding unit, the empty cut height correction value is written into the grinding control parameters corresponding to the silicon wafer to be ground, so that the corrected empty cut height is used when the silicon wafer to be ground starts grinding feed.

6. The method for adjusting the air cutting height of a double-sided vertical grinding equipment according to claim 1, characterized in that, The method further includes: The thickness of a standard silicon wafer of known thickness is measured to obtain the thickness measurement value of the standard silicon wafer; Determine the difference between the thickness measurement value and the standard thickness value of the standard silicon wafer; and The difference is used to compensate for subsequent thickness measurements.

7. The method for adjusting the air cutting height of a double-sided vertical grinding equipment according to claim 6, characterized in that, After compensating subsequent thickness measurements based on the difference, the standard silicon wafer is re-measured for thickness, and the measurement results are compensated again until the absolute value of the difference between the re-measured and compensated thickness value and the standard thickness value is less than 0.5 micrometers.

8. A device for adjusting the air cutting height of a double-sided vertical grinding machine, characterized in that, include: A silicon wafer thickness measuring device is configured to measure the thickness of the silicon wafer before grinding during the V-groove detection process and generate a pre-grinding thickness measurement value of the silicon wafer. as well as The control system is communicatively connected to the silicon wafer thickness measuring device. The control system is configured to acquire the thickness measurement value before polishing and determine the empty cutting height correction value corresponding to the silicon wafer to be polished based on the thickness measurement value before polishing. The control system is further configured to correct the cut height of the silicon wafer to be ground during grinding based on the cut height correction value before grinding, so that the double-sided vertical grinding equipment grinds the silicon wafer to be ground according to the corrected cut height.

9. The air cutting height adjustment device for a double-sided vertical grinding equipment according to claim 8, characterized in that, The silicon wafer thickness measuring device is located on the periphery of the silicon wafer to be ground.

10. The air cutting height adjustment device for a double-sided vertical grinding equipment according to claim 8, characterized in that, The silicon wafer thickness measuring device is configured to measure multiple thickness measurement data of the silicon wafer to be ground during the rotation of the silicon wafer to be ground; The control system is configured to determine the maximum value among the plurality of thickness measurement data as the pre-grinding thickness measurement value.