Compositions for water-based asphalt waterproof coatings, water-based asphalt waterproof coatings, their preparation methods and applications

By optimizing the composition and preparation method of water-based asphalt waterproof coatings, the problems of poor dispersibility and uneven performance after increasing the solid content in existing technologies have been solved. This has resulted in high-solid-content coatings with excellent mechanical properties and weather resistance, improved construction efficiency and performance adaptability, and made them suitable for the field of building waterproofing.

CN123107543APending Publication Date: 2026-11-17KESHUN WATERPROOF TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611277617.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-21
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing water-based asphalt waterproof coatings have defects such as poor dispersibility after increasing solid content, difficulty in balancing weather resistance and mechanical properties, insufficient anti-slip, wear resistance, and puncture resistance, weak acid and alkali resistance, weak hiding power, and insufficient crack resistance.

Method used

A composition of anionic emulsified asphalt, SBR emulsion, and composite fillers is used. Through melt blending and emulsification of multifunctional modified materials such as star-shaped SBS, disulfide-bonded phenylboronic acid and its derivatives, nano zinc oxide, and microcapsule phase change materials, combined with composite fillers with optimized particle size distribution, the solid content is improved and the mechanical properties and weather resistance of the coating are enhanced.

Benefits of technology

It achieves excellent mechanical properties, weather resistance, UV resistance and waterproof performance of high solids content (greater than 75wt%) coatings, improves construction efficiency, enhances wear resistance and acid and alkali resistance, has good storage stability, wide application compatibility, is environmentally friendly and recyclable, and has controllable costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
Patent Text Reader

Abstract

This invention relates to the field of building waterproofing, and discloses a composition for water-based asphalt waterproof coatings, the water-based asphalt waterproof coating itself, its preparation method, and its application. The composition consists of a main agent and additives. The main agent includes anionic emulsified asphalt, SBR emulsion, and composite filler. Based on the total mass of the composition, the content of the anionic emulsified asphalt is 12-18 wt%, the content of the SBR emulsion is 30-40 wt%, and the content of the composite filler is 38-50 wt%. The anionic emulsified asphalt is obtained by melt blending a base asphalt and a multifunctional modifying material followed by emulsification. The multifunctional modifying material includes star-shaped SBS, disulfide-bonded phenylboronic acid and its derivatives, nano-zinc oxide, and microcapsule phase change materials. The water-based asphalt waterproof coating provided by this invention exhibits excellent mechanical properties, weather resistance, wear resistance, and acid and alkali resistance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of building waterproofing, specifically to a composition for water-based asphalt waterproof coatings, water-based asphalt waterproof coatings, their preparation methods, and applications. Background Technology

[0002] Currently, water-based asphalt waterproof coatings are widely used in the building waterproofing field due to their environmental friendliness and ease of application. Existing exposed water-based asphalt waterproof coatings are mainly prepared using anionic emulsified asphalt as the base material, compounded with styrene-butadiene rubber latex, traditional inorganic fillers (such as heavy calcium carbonate and fumed silica), anti-aging additives (such as UV stabilizers and antioxidants), and functional additives (such as emulsifiers, defoamers, and thickeners). Some technical solutions improve the weather resistance of the coating by adding modified graphene, water-based epoxy resin, or by adding modified carbonyl iron powder to improve its anti-slip properties.

[0003] In existing technologies, the solid content of emulsified asphalt is typically controlled at 40-50%, the solid content of SBR rubber latex is 50-55%, and the overall solid content of coatings is mostly between 50-60%. The preparation process mainly involves room temperature stirring, high-speed dispersion, and ball mill grinding and mixing, achieving the dispersion and bonding of each component through physical blending. Furthermore, traditional exposed water-based asphalt waterproof coatings often use 600-1000 mesh heavy calcium carbonate and 1000-1500 mesh fumed silica as inorganic fillers, which only serve as basic fillers and compatibilizers, offering limited improvement to the wear resistance, acid and alkali resistance, and hiding power of the exposed core of the coating.

[0004] Therefore, existing water-based asphalt waterproof coatings generally suffer from defects such as poor dispersibility after increasing solid content, difficulty in balancing weather resistance and mechanical properties, insufficient anti-slip, wear resistance, puncture resistance, weak acid and alkali resistance, weak hiding power, and insufficient crack resistance.

[0005] CN118359994A discloses an exposed water-based asphalt-based waterproof coating, its preparation method, and a waterproof laminate. The exposed water-based asphalt-based waterproof coating comprises anionic emulsified asphalt, a polymer emulsion, fillers, and additives. The anionic emulsified asphalt is prepared by melt-blending a base asphalt with a composite weather-resistant additive and then emulsifying the mixture. The composite weather-resistant additive is a combination of an antioxidant and an ultraviolet absorber at a mass ratio of 0.5-2:1. The polymer emulsion is one or more of weather-resistant styrene-acrylic emulsion, weather-resistant pure acrylic emulsion, and weather-resistant silicone-acrylic emulsion. The mass ratio of the anionic emulsified asphalt, polymer emulsion, fillers, and additives is 20-50:20-50:5-25:0.1-5. The waterproof coating system prepared by this method exhibits significantly improved stability and weather resistance. However, the waterproof coating obtained by this method has a solid content of about 55-60 wt%. The low solid content makes the coating dry slowly during construction and prone to sagging when applied thickly. In addition, the weather resistance of the coating relies solely on antioxidants and ultraviolet absorbers, and its weather resistance and service life need to be further improved. Summary of the Invention

[0006] The purpose of this invention is to provide a water-based asphalt waterproof coating with high solids content and good mechanical properties, weather resistance, and stability during long-term exposure.

[0007] To achieve the above objectives, a first aspect of the present invention provides a composition for a water-based asphalt waterproof coating, the composition comprising a main agent and an additive, wherein the main agent includes anionic emulsified asphalt, SBR emulsion and composite filler; Based on the total mass of the composition, the content of the anionic emulsified bitumen is 12-18 wt%, the content of the SBR emulsion is 30-40 wt%, and the content of the composite filler is 38-50 wt%. The anionic emulsified asphalt is prepared by melt blending of base asphalt and multifunctional modifying materials and then emulsifying them; the multifunctional modifying materials include star-shaped SBS, disulfide-bonded phenylboronic acid and its derivatives, nano zinc oxide and microcapsule phase change materials; The solid content of the anionic emulsified asphalt is 60-65 wt%. The solid content of the SBR emulsion is 65-70 wt%; The composite filler is a combination of sand, rubber powder, barium sulfate and ultraviolet shielding agent in a mass ratio of 1:1.5-2.5:3.5-4.5:0.15-0.2.

[0008] A second aspect of the present invention provides a method for preparing a water-based asphalt waterproof coating, the method being carried out using the components of the composition described in the first aspect above, the method comprising: stirring and mixing the components of the composition to obtain the water-based asphalt waterproof coating.

[0009] A third aspect of the present invention provides an aqueous bitumen waterproof coating prepared by the method described in the second aspect above.

[0010] The fourth aspect of the present invention provides the application of the water-based asphalt waterproof coating described in the third aspect above in the field of building waterproofing.

[0011] Through the above technical solution, the present invention has at least the following beneficial technical effects: (1) The water-based asphalt waterproof coating provided by the present invention has a solid content of more than 75wt%, and the amount of water evaporated during film formation is reduced by more than 30wt%. The drying time after construction is greatly shortened, and there are no problems of dampness or sagging during thick coating construction. The construction efficiency is significantly improved, and the coating is smooth without brush marks.

[0012] (2) The water-based asphalt waterproof coating provided by the present invention has excellent mechanical properties, weather resistance, UV resistance and waterproof performance, and its wear resistance and acid and alkali resistance are also significantly improved, and its construction adaptability is wider.

[0013] (3) The water-based asphalt waterproof coating provided by the present invention has good storage stability, convenient transportation and construction, and is environmentally friendly and recyclable with controllable cost. Detailed Implementation

[0014] The endpoints and any values ​​of the ranges disclosed herein are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of the various ranges, the endpoint values ​​of the various ranges and individual point values, and individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed herein.

[0015] As mentioned above, a first aspect of the present invention provides a composition for a water-based asphalt waterproof coating, the composition comprising a main agent and an additive, wherein the main agent includes anionic emulsified asphalt, SBR emulsion and composite filler; Based on the total mass of the composition, the content of the anionic emulsified bitumen is 12-18 wt%, the content of the SBR emulsion is 30-40 wt%, and the content of the composite filler is 38-50 wt%. The anionic emulsified asphalt is prepared by melt blending of base asphalt and multifunctional modifying materials and then emulsifying them; the multifunctional modifying materials include star-shaped SBS, disulfide-bonded phenylboronic acid and its derivatives, nano zinc oxide and microcapsule phase change materials; The solid content of the anionic emulsified asphalt is 60-65 wt%. The solid content of the SBR emulsion is 65-70 wt%; The composite filler is a combination of sand, rubber powder, barium sulfate and ultraviolet shielding agent in a mass ratio of 1:1.5-2.5:3.5-4.5:0.15-0.2.

[0016] According to a preferred embodiment, the mass ratio of the anionic emulsified bitumen to the SBR emulsion is 1:2-2.5. The inventors of this invention have discovered that, under this preferred embodiment, the water-based bitumen waterproof coating provided by this invention has better weather resistance and waterproofing performance.

[0017] According to a preferred embodiment, the SBR emulsion contains 35-40 wt% styrene structural units, and the viscosity of the SBR emulsion at 25°C is 600-1200 mPa·s. The inventors of this invention have found that, under this preferred embodiment, the water-based asphalt waterproof coating provided by this invention exhibits better adhesion to the base material.

[0018] According to one specific embodiment, in the anionic emulsified asphalt, relative to 100 parts by weight of the base asphalt, the content of the star-shaped SBS is 4-5 parts by weight, the content of the disulfide-bonded phenylboronic acid and its derivatives is 0.3-0.5 parts by weight, the content of the nano zinc oxide is 1-1.5 parts by weight, and the content of the microcapsule phase change material is 2-3 parts by weight.

[0019] In some embodiments, the multifunctional modified material in the anionic emulsified asphalt further includes an antioxidant and naphthenic oil, wherein the antioxidant content is 0.15-0.25 parts by weight and the naphthenic oil content is 2-3 parts by weight relative to 100 parts by weight of the base asphalt.

[0020] In some embodiments, the base asphalt is selected from at least one of Grade 70 A road petroleum asphalt, Grade 90 A road petroleum asphalt, and Grade 100 A road petroleum asphalt.

[0021] Preferably, the base asphalt is selected from Grade 70 A road petroleum asphalt.

[0022] In some embodiments, the disulfide-containing phenylboronic acid and its derivatives are selected from at least one of 2,2'-dithiodiphenylboronic acid, 4,4'-dithiodiphenylboronic acid, and dithiodiethyl phenylboronic acid.

[0023] In some embodiments, the microcapsule phase change material is selected from at least one of paraffin-based microcapsule phase change materials, fatty acid-based microcapsule phase change materials, and polyethylene glycol-based microcapsule phase change materials.

[0024] In some embodiments, the antioxidant is selected from at least one of antioxidant 1010, antioxidant 168, and antioxidant 1076.

[0025] According to a preferred embodiment, in the composite filler, the sand is river sand and / or manufactured sand, with an average particle diameter of 0.18-0.45 mm.

[0026] According to a preferred embodiment, the average particle diameter of the rubber powder is 0.4-0.8 mm.

[0027] According to a preferred embodiment, the average particle diameter of the barium sulfate is 10-15 μm.

[0028] According to a preferred embodiment, the average particle diameter of the ultraviolet shielding agent is 20-30 nm.

[0029] According to one specific embodiment, the ultraviolet shielding agent is selected from at least one of nano-titanium dioxide, nano-zinc oxide, and nano-cerium oxide.

[0030] The inventors of this invention have discovered that by controlling the particle size distribution and gradation of the composite filler, a composite system consisting of large-particle-size components and small-particle-size components can be constructed, which better solves the problems of easy sedimentation, agglomeration and abnormal viscosity of composite fillers in high-solids-content systems. This results in water-based asphalt waterproof coatings with better interfacial bonding strength and superior weather resistance, wear resistance and UV resistance.

[0031] In some embodiments, the rubber powder in the composite filler is obtained by modifying raw rubber powder with a silane coupling agent, wherein the silane coupling agent is selected from at least one of γ-aminopropyltriethoxysilane, γ-glycidoxypropyltrimethoxysilane, and γ-methacryloyloxypropyltrimethoxysilane.

[0032] Preferably, the mass ratio of the raw rubber powder to the silane coupling agent is 1:0.02-0.04.

[0033] In some embodiments, the additives contain an anti-aging agent, an anti-slip agent, an antifoaming agent, a preservative, and a thickener; based on the total mass of the composition, the content of the anti-aging agent is 0.6-0.8 wt%, the content of the anti-slip agent is 0.3-0.5 wt%, the content of the antifoaming agent is 0.2-0.3 wt%, the content of the preservative is 0.1-0.2 wt%, and the content of the thickener is 0.2-0.3 wt%.

[0034] This invention does not impose any particular requirements on the specific types of the anti-aging agent, anti-slip agent, defoamer, preservative, and thickener. Those skilled in the art can select known anti-aging agents, anti-slip agents, defoamers, preservatives, and thickeners according to actual circumstances. For example, the anti-aging agent may be selected from at least one of ultraviolet absorbers, light stabilizers, and hindered amine light stabilizers; the anti-slip agent may be selected from at least one of corundum, quartz sand, and silicon carbide; the defoamer may be selected from at least one of organosilicon defoamers, polyether defoamers, and mineral oil defoamers; the preservative may be an isothiazolinone preservative; and the thickener may be selected from at least one of hydroxyethyl cellulose, sodium polyacrylate, and xanthan gum.

[0035] This invention does not impose any particular requirements on the specific types of the ultraviolet absorber, the light stabilizer, and the hindered amine light stabilizer. Those skilled in the art can select known ultraviolet absorbers, light stabilizers, and hindered amine light stabilizers for application in this invention according to actual circumstances. For example, the ultraviolet absorber is selected from at least one of UV-326, UV-327, and UV-531; the light stabilizer is selected from at least one of UV-770, UV-944, and UV-622.

[0036] According to one specific embodiment, the adjuvant also contains 1-10 wt% water based on the total mass of the composition.

[0037] As previously stated, a second aspect of the present invention provides a method for preparing a water-based asphalt waterproof coating, the method comprising using the components of the composition described in the first aspect above, the method comprising: stirring and mixing the components of the composition to obtain the water-based asphalt waterproof coating.

[0038] According to one specific embodiment, the method for preparing the water-based asphalt waterproof coating includes: S1. Mix the raw rubber powder with a mass ratio of 1:0.02-0.04 and the silane coupling agent to obtain the modified rubber powder. S2. Mix the anionic emulsified asphalt with the SBR emulsion for 15-20 minutes to obtain the base mixture. S3. The sand and the rubber powder obtained in step S1 are stirred and mixed with the base material mixture at a speed of 1200-1500 rpm for 30-40 min. Then, barium sulfate and ultraviolet shielding agent are added to the resulting mixture and stirred at a speed of 300-600 rpm for 20-25 min to obtain a composite filler-base material system. S4. At a speed of 800-1000 rpm, the additives and the composite filler-base system are mixed for 20-25 minutes. The resulting mixture is then ground and homogenized to obtain the water-based asphalt waterproof coating.

[0039] As previously stated, a third aspect of the present invention provides an aqueous bitumen waterproof coating prepared by the method described in the second aspect above.

[0040] As previously stated, the fourth aspect of the present invention provides the application of the water-based asphalt waterproofing coating described in the third aspect in the field of building waterproofing.

[0041] To provide a clearer understanding of the technical features, objectives, and beneficial effects of this invention, the invention is now described in detail through embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the invention, and the scope of protection of this invention is not limited to the following description. In the following examples, unless otherwise specified, all raw materials and reagents used are common commercially available products.

[0042] The following examples include some of the raw materials used and their sources: SBR emulsion-I: solid content is 70wt%, styrene structural unit content is 38wt%, viscosity at 25°C is 1100mPa·s, grade is LIPATON™ SB 4070, purchased from Synthomer. SBR Emulsion-II: Solid content is 67wt%, styrene structural unit content is 33wt%, viscosity at 25°C is 1100mPa·s, grade is LIPATON™ SB 2540, purchased from Synthomer. SBR Emulsion-III: Solid content is 55wt%, styrene structural unit content is 29wt%, viscosity at 25°C is 450mPa·s, grade is LIPATON™ SB 20W20, purchased from Synthomer. Sand: Manufactured sand, with an average particle diameter of 0.3 mm; Rubber Powder-I: 5g of γ-aminopropyltriethoxysilane (KH-550) was diluted with anhydrous ethanol to prepare a 5wt% solution; 125g of raw rubber powder (average particle diameter of 0.6mm) was added, and the mixture was stirred at 60℃ and 500rpm for 30min; then dried at 80℃ for 2h to obtain modified rubber powder-I with an average particle diameter of 0.6mm. Rubber Powder-II: The modification treatment is similar to that used in the preparation of Rubber Powder-I, except that the average particle diameter of the raw rubber powder is 0.2 mm, resulting in Rubber Powder-II with an average particle diameter of 0.2 mm after modification. Barium sulfate-I: Natural barium sulfate, with an average particle diameter of 12μm, purchased from Guangdong Yuanlei Powder Co., Ltd. Barium sulfate-II: Natural barium sulfate, with an average particle diameter of 23 μm, purchased from Guangdong Yuanlei Powder Co., Ltd. UV shielding agent: Nano titanium dioxide: Particles with an average diameter of 25nm, purchased from Nanjing Titanium Dioxide Chemical Co., Ltd. Anti-aging agents: UV-327 (ultraviolet absorber) and UV-770 (light stabilizer) are compounded in a mass ratio of 2:1; Anti-slip agent: corundum, purchased from Henan Ruishi New Materials Co., Ltd.; Defoamer: Silicone defoamer, brand name BYK-024, purchased from BYK, Germany. Preservative: 1,2-benzisothiazolin-3-one, purchased from Shanghai Qihe Chemical Co., Ltd.; Thickener: Associative polyurethane thickener, brand name RM-8W, purchased from Dow Chemical; Preparation of anionic emulsified bitumen-I: 100 parts by weight of Grade 70 A road petroleum asphalt were heated to 170℃ and melted. Then, 4.5 parts by weight of star-shaped SBS (purchased from Sinopec Baling Petrochemical Company, grade 4303-1), 0.4 parts by weight of 2,2'-dithiodiphenylboronic acid, 1.2 parts by weight of nano-zinc oxide, 2.5 parts by weight of microencapsulated phase change material (purchased from Suzhou Zhongjieneng New Material Technology Co., Ltd., grade PCM28), 0.2 parts by weight of antioxidant 1010, and 0.2 parts by weight of anti-... Oxygen agent 168 and 2.5 parts by weight of naphthenic oil (purchased from Karamay Petrochemical Company, brand name KN4010) were stirred at 400 rpm for 50 min until completely melted and blended. The above melt was slowly added to an aqueous solution of composite emulsifier (containing 2.5 parts by weight of sodium dodecylbenzene sulfonate and 0.5 parts by weight of sodium lignosulfonate) at 85°C, and emulsified at 4500 rpm for 18 min. After cooling to room temperature, an anionic emulsified asphalt-I with a solid content of 63 wt% was obtained. Preparation of anionic emulsified asphalt-II: 100 parts by weight of Grade 70 A road petroleum asphalt were heated to 170°C to melt, and 4.5 parts by weight of star-shaped SBS (purchased from Sinopec Baling Petrochemical Company, grade 4303-1), 0.2 parts by weight of antioxidant 1010, 0.2 parts by weight of antioxidant 168, and 2.5 parts by weight of naphthenic oil (purchased from Karamay Petrochemical Company, grade KN4010) were added. The mixture was stirred at 400 rpm for 50 minutes until completely melted and blended. The subsequent emulsification process was the same as that of anionic emulsified asphalt-I to obtain anionic emulsified asphalt-II with a solid content of 55 wt%.

[0043] Preparation of anionic emulsified bitumen-III: 100 parts by weight of Grade 70 A road petroleum asphalt were heated to 170°C to melt, and 4.5 parts by weight of star-shaped SBS (purchased from Sinopec Baling Petrochemical Company, grade 4303-1), 0.4 parts by weight of 2,2'-dithiodiphenylboronic acid, 1.2 parts by weight of nano zinc oxide, 0.2 parts by weight of antioxidant 1010, 0.2 parts by weight of antioxidant 168, and 2.5 parts by weight of naphthenic oil (purchased from Karamay Petrochemical Company, grade KN4010) were added. The mixture was stirred at 400 rpm for 50 minutes until completely melted and blended. The subsequent emulsification process was the same as that of anionic emulsified asphalt-I to obtain anionic emulsified asphalt-III with a solid content of 55 wt%.

[0044] Preparation of anionic emulsified bitumen-IV: 100 parts by weight of Grade 70 A road petroleum asphalt were heated to 170°C to melt, and 4.5 parts by weight of star-shaped SBS (purchased from Sinopec Baling Petrochemical Company, grade 4303-1), 0.4 parts by weight of 2,2'-dithiodiphenylboronic acid, 2.5 parts by weight of microencapsulated phase change material (purchased from Suzhou Zhongjieneng New Material Technology Co., Ltd., grade PCM28), 0.2 parts by weight of antioxidant 1010, 0.2 parts by weight of antioxidant 168, and 2.5 parts by weight of naphthenic oil (purchased from Karamay Petrochemical Company, grade KN4010) were added. The mixture was stirred at 400 rpm for 50 min until completely melted and blended. The subsequent emulsification process was the same as that of anionic emulsified asphalt-I to obtain anionic emulsified asphalt-IV with a solid content of 55 wt%.

[0045] Preparation of anionic emulsified bitumen-V: 100 parts by weight of Grade 70 A road petroleum asphalt were heated to 170°C to melt, and 4.5 parts by weight of star-shaped SBS (purchased from Sinopec Baling Petrochemical Company, grade 4303-1), 1.2 parts by weight of nano zinc oxide, 2.5 parts by weight of microcapsule phase change material (purchased from Suzhou Zhongjieneng New Material Technology Co., Ltd., grade PCM28), 0.2 parts by weight of antioxidant 1010, 0.2 parts by weight of antioxidant 168, and 2.5 parts by weight of naphthenic oil (purchased from Karamay Petrochemical Company, grade KN4010) were added. The mixture was stirred at 400 rpm for 50 minutes until completely melted and blended. The subsequent emulsification process was the same as that of anionic emulsified asphalt-I to obtain anionic emulsified asphalt-V with a solid content of 55 wt%.

[0046] Example 1 (1) Anionic emulsified asphalt and SBR emulsion were stirred and mixed at 350 rpm for 20 min to obtain a base mixture; (2) The sand, rubber powder and the above base material mixture are stirred and mixed at a speed of 1200 rpm for 40 min; then barium sulfate and ultraviolet shielding agent are added and stirred at a speed of 500 rpm for 20 min to obtain the composite filler-base material system. (3) At a speed of 1000 rpm, the additives and the above composite filler-base system are mixed for 20 min. The resulting mixture is then ground and homogenized in a horizontal sand mill. The grinding media is zirconia beads (particle size of 1.0 mm). The grinding speed is 1500 rpm and the grinding time is 30 min. After discharge, the mixture is filtered through a 20-mesh filter and the sieve material is collected to prepare water-based asphalt waterproof coating.

[0047] The specific types and amounts of substances used in this embodiment are shown in Table 1.

[0048] Unless otherwise specified, Examples 2 and 3 are carried out with reference to the method of Example 1, except that the types and amounts of substances used are different, as detailed in Table 1.

[0049] Table 1

[0050] Example 4 This embodiment uses a method similar to that of Example 1, except that an equal weight portion of SBR emulsion-II is used to replace SBR emulsion-I in Example 1 to prepare a water-based asphalt waterproof coating.

[0051] Example 5 This embodiment uses a method similar to that of Example 1, except that rubber powder-II is used in place of rubber powder-I in Example 1 in equal parts by weight to prepare a water-based asphalt waterproof coating.

[0052] Example 6 This embodiment uses a method similar to that of Example 1, except that barium sulfate-II is used in place of barium sulfate-I in Example 1 in equal parts by weight to prepare a water-based asphalt waterproof coating.

[0053] Comparative Example 1 This comparative example was conducted using a method similar to that of Example 1, except that an equal weight portion of SBR emulsion-III was used to replace SBR emulsion-I in Example 1 to prepare a water-based asphalt waterproof coating.

[0054] Comparative Example 2 This comparative example was conducted using a method similar to that of Example 1, except that an anionic emulsified bitumen-II was used in place of an anionic emulsified bitumen-I in Example 1 in equal parts by weight to prepare a water-based bitumen waterproof coating.

[0055] Comparative Example 3 This comparative example was prepared using a method similar to that of Example 1. The difference is that no rubber powder was added in this comparative example, and the amount of sand was adjusted to 18 parts by weight to prepare a water-based asphalt waterproof coating.

[0056] Comparative Example 4 This comparative example was prepared using a method similar to that of Example 1. The difference is that 43 parts by weight of rubber powder-I were used to replace the composite filler in the example to prepare a water-based asphalt waterproof coating.

[0057] Comparative Example 5 This comparative example was conducted using a method similar to that of Example 1. The difference is that the composite filler used in this comparative example is: 6 parts by weight of sand, 6 parts by weight of rubber powder-I, 27 parts by weight of barium sulfate-I, and 1 part by weight of ultraviolet shielding agent. The dosage and operation of the remaining components are the same as in Example 1, and a water-based asphalt waterproof coating is prepared.

[0058] Comparative Example 6 This comparative example was conducted using a method similar to that of Example 1, except that an anionic emulsified bitumen-III was used in place of anionic emulsified bitumen-I in Example 1 in equal parts by weight to prepare a water-based bitumen waterproof coating.

[0059] Comparative Example 7 This comparative example was conducted using a method similar to that of Example 1, except that an anionic emulsified bitumen-IV was used in place of an anionic emulsified bitumen-I in Example 1 in equal parts by weight to prepare a water-based bitumen waterproof coating.

[0060] Comparative Example 8 This comparative example was conducted using a method similar to that of Example 1, except that an anionic emulsified bitumen-V was used in place of an anionic emulsified bitumen-I in Example 1 in equal parts by weight to prepare a water-based bitumen waterproof coating.

[0061] Test case This test example illustrates the performance testing of the water-based asphalt waterproof coatings prepared in the above embodiments and comparative examples. Specifically: Solid content: Refer to Chapter 5 of GB / T 16777-2008 standard (105℃, constant temperature for 3h); Tensile strength and nerve length at break: Refer to Chapter 9 of GB / T 16777-2008 standard (tensile speed 200 mm / min); Weathering resistance test (artificial accelerated aging): Refer to Chapter 9 of GB / T 16777-2008 standard (Xenon arc lamp requirements, 1000h); Wear resistance test: Refer to GB / T 1768-2006 standard (Taber abrasion tester, CS-10 grinding wheel, 750g load, 500 revolutions). Acid and alkali resistance test: Refer to Chapter 9 of GB / T 16777-2008 standard (5% H2SO4 solution / 5% NaOH solution, immersion at 23℃ for 168h). Impermeability: Refer to Chapter 15 of GB / T 16777-2008 standard (0.3MPa, maintain for 30min).

[0062] The specific test results are shown in Table 2.

[0063] Table 2

[0064] As can be seen from the results in Table 2, the water-based asphalt waterproof coating provided by this invention breaks through the technical bottleneck of existing water-based asphalt waterproof coatings with single filler function and contradictory performance. While achieving a high solid content of more than 75wt%, it achieves a synergistic improvement in weather resistance, mechanical properties, construction performance, wear resistance and acid and alkali resistance. Moreover, it is environmentally friendly, recyclable, and cost-controllable, and is suitable for waterproof construction of various complex exposed projects. It has significant technical advantages, environmental benefits and market application value.

[0065] The preferred embodiments of the present invention have been described in detail above; however, the present invention is not limited thereto. Within the scope of the inventive concept, various simple modifications can be made to the technical solutions of the present invention, including combinations of various technical features in any other suitable manner. These simple modifications and combinations should also be considered as the content disclosed in the present invention and are all within the protection scope of the present invention.

Claims

1. A composition for a water-based asphalt waterproof coating, characterized in that, The composition consists of a main agent and an auxiliary agent, wherein the main agent includes anionic emulsified asphalt, SBR emulsion and composite filler; Based on the total mass of the composition, the content of the anionic emulsified bitumen is 12-18 wt%, the content of the SBR emulsion is 30-40 wt%, and the content of the composite filler is 38-50 wt%. The anionic emulsified asphalt is prepared by melt blending of base asphalt and multifunctional modifying materials and then emulsifying them; the multifunctional modifying materials include star-shaped SBS, disulfide-bonded phenylboronic acid and its derivatives, nano zinc oxide and microcapsule phase change materials; The solid content of the anionic emulsified asphalt is 60-65 wt%. The solid content of the SBR emulsion is 65-70 wt%; The composite filler is a combination of sand, rubber powder, barium sulfate and ultraviolet shielding agent in a mass ratio of 1:1.5-2.5:3.5-4.5:0.15-0.

2.

2. The composition according to claim 1, wherein, The mass ratio of the anionic emulsified bitumen to the SBR emulsion is 1:2-2.5; And / or, the content of styrene structural units in the SBR emulsion is 35-40 wt%, and the viscosity of the SBR emulsion at 25°C is 600-1200 mPa·s.

3. The composition according to claim 1, wherein, In the anionic emulsified asphalt, relative to 100 parts by weight of the base asphalt, the content of the star-shaped SBS is 4-5 parts by weight, the content of the disulfide-bonded phenylboronic acid and its derivatives is 0.3-0.5 parts by weight, the content of the nano zinc oxide is 1-1.5 parts by weight, and the content of the microcapsule phase change material is 2-3 parts by weight.

4. The composition according to claim 1, wherein, In the composite filler, the sand is river sand and / or manufactured sand, with an average particle diameter of 0.18-0.45 mm; And / or, the average particle diameter of the rubber powder is 0.4-0.8 mm; And / or, the average particle diameter of the barium sulfate is 10-15 μm; And / or, the average particle diameter of the UV shielding agent is 20-30 nm; And / or, the ultraviolet shielding agent is selected from at least one of nano-titanium dioxide, nano-zinc oxide, and nano-cerium oxide.

5. The composition according to claim 1, wherein, In the composite filler, the rubber powder is obtained by modifying raw rubber powder with a silane coupling agent, wherein the silane coupling agent is selected from at least one of γ-aminopropyltriethoxysilane, γ-glycidoxypropyltrimethoxysilane and γ-methacryloyloxypropyltrimethoxysilane.

6. The composition according to any one of claims 1-5, wherein, The additives contain anti-aging agents, anti-slip agents, defoamers, preservatives, and thickeners; Based on the total mass of the composition, the content of the anti-aging agent is 0.6-0.8 wt%, the content of the anti-slip agent is 0.3-0.5 wt%, the content of the defoamer is 0.2-0.3 wt%, the content of the preservative is 0.1-0.2 wt%, and the content of the thickener is 0.2-0.3 wt%.

7. The composition according to any one of claims 1-5, wherein, Based on the total mass of the composition, the adjuvant also contains 1-10 wt% water.

8. A method for preparing water-based asphalt waterproof coating, characterized in that, The method is carried out using the components of the composition according to any one of claims 1-7, and the method includes: stirring and mixing the components of the composition to obtain the water-based asphalt waterproof coating.

9. The water-based asphalt waterproof coating prepared by the method of claim 8.

10. The application of the water-based asphalt waterproof coating according to claim 9 in the field of building waterproofing.