Crack guide strips and construction methods for building structural surface layers
By using crack guide strips designed with guiding ramps and curved energy dissipation surfaces in plain concrete structures, the problem of disordered cracks in plain concrete structures was solved, achieving directional guidance and reducing secondary cracks, thus improving durability and waterproofing.
Patent Information
- Application Number
- CN202611556489.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-09
- Publication Date
- 2026-11-17
AI Technical Summary
In existing technologies, plain concrete structures are prone to generating disordered cracks under the effects of temperature shrinkage, drying shrinkage, and uneven deformation of the foundation, leading to leakage and surface spalling. Existing methods are difficult to effectively guide and control the location of cracks.
A crack guide strip is used, which includes a guide element, a flexible energy dissipation element, and a seal. The guide element is provided with a guide slope, the flexible energy dissipation element has an arc-shaped curved energy dissipation surface, and the seal is sealed to the plain concrete layer. The crack generation location is guided by pre-divided grid installation, and the deformation energy is absorbed at the flexible energy dissipation element. The seal prevents water vapor from rising.
It effectively limits the location of crack formation, reduces disordered secondary cracks, improves the durability and waterproof performance of plain concrete layers, and avoids additional cracks caused by stress concentration.
Smart Images

Figure CN123109397A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of building construction technology, and in particular to a crack guide strip and a method for constructing building structural surface layers. Background Technology
[0002] Non-load-bearing components such as foundation layers and slope-finding layers in building structures are usually cast using plain concrete to reduce construction costs. Plain concrete has excellent compressive strength, but its tensile strength is low and its brittleness is prominent. Under the combined effects of temperature shrinkage, drying shrinkage, and uneven deformation of the foundation, it is very prone to generating random and disordered cracks, causing defects such as leakage and surface peeling, which seriously affect the durability and normal use function of the components.
[0003] In existing technologies, the common methods to control the shrinkage deformation and alleviate cracking of plain concrete include adding functional admixtures, installing additional wire mesh, and cutting expansion joints later. However, admixtures can only reduce the overall shrinkage of concrete, but cannot eliminate cracking at its source, nor can they guide the location of cracks; cracks still form randomly. Additional wire mesh can only constrain the width of cracks after they have started to spread, but cannot prevent crack initiation. Furthermore, the wire mesh is prone to fatigue fracture due to repeated tension and compression, making it difficult to maintain its effectiveness in the long term. Cutting expansion joints later requires strict adherence to construction time, and this method only releases static shrinkage stress, which can still easily lead to secondary cracks.
[0004] Therefore, there is an urgent need for a crack guide strip and a construction method for building structural surface layers to solve the above problems. Summary of the Invention
[0005] The purpose of this invention is to provide a crack guide strip and a construction method for building structural surface layers, which can effectively limit the location of crack generation, significantly reduce the generation of disordered secondary cracks, and improve the durability of plain concrete layers.
[0006] To achieve this objective, the present invention adopts the following technical solution: Firstly, a crack guide strip is provided, comprising: The guide can be anchored in the plain concrete layer. The guide is provided with a guide slope that is set at an angle to the thickness direction of the plain concrete layer, so that the cross-sectional width of the upper end of the guide is greater than the cross-sectional width of the lower end of the guide, and the crack starts from the lower end of the guide. A flexible energy dissipation component is installed on the top of the guide component, and the flexible energy dissipation component is provided with an arc-shaped curved energy dissipation surface; The sealing element is located on top of the flexible energy dissipation element and can be sealed to the plain concrete layer. The guide element, the flexible energy dissipation element and the sealing element are arranged coaxially along the thickness direction of the plain concrete layer.
[0007] Optionally, the flexible energy dissipation component includes several arc-shaped protrusions and several arc-shaped recesses. Both the arc-shaped protrusions and the arc-shaped recesses extend circumferentially along the flexible energy dissipation component. The arc-shaped protrusions and the arc-shaped recesses are alternately arranged, and the energy dissipation surface is formed on the surface of the arc-shaped protrusions and the arc-shaped recesses.
[0008] Optionally, the crack guide strip also includes crack-resistant mesh fabric, which includes a relaxation section, two fastening sections, and two extension sections. The relaxation section is laid in a relaxed state on the upper surface of the sealant. The two fastening sections are located on both sides of the relaxation section. The two extension sections correspond one-to-one with the two fastening sections. One end of the fastening section is connected to the relaxation section, and the other end is connected to the corresponding extension section. The fastening section is fixedly connected to the sealant, and the extension section is fixedly laid on the upper surface of the plain concrete layer.
[0009] Optionally, the upper surface of the seal is provided with a first mounting groove corresponding to each of the two fastening sections, and the fastening sections are embedded in the corresponding first mounting grooves.
[0010] Optionally, the sealing element includes a connecting plate and a sealing part disposed on the connecting plate. The connecting plate is connected to the flexible energy dissipation element and is flush with the upper surface of the plain concrete layer. The sealing part is provided with a protective layer that can be detachably connected to it. When the protective layer is separated from the sealing part, the sealing part can adhere to and seal the plain concrete layer.
[0011] Optionally, the guide is provided with an anchoring part, the extension direction of which is set at an angle to the thickness direction of the plain concrete layer, so that the anchoring part can be anchored in the plain concrete layer.
[0012] Secondly, a construction method for a building structural surface layer is provided. The building structural surface layer includes a plain concrete layer and a leveling layer stacked on top of the plain concrete layer. The construction method for the building structural surface layer is applicable to the crack guide strip of the first aspect and includes the following steps: S1. Divide the surface to be constructed into a grid to form multiple grid edges; S2. Pour concrete onto the surface to be constructed to form a plain concrete layer; S3. Before the concrete initially sets, multiple crack guide strips are embedded into the concrete to a predetermined depth along multiple grid edges using an indentation structure, and adjacent crack guide strips are connected using a connecting joint. S4. After the concrete has cured, pour material onto the surface of the plain concrete layer to form a leveling layer; while pouring the material, ensure that the material is applied symmetrically and synchronously on both sides of the crack guide strip.
[0013] Optionally, the press-in structure includes a mounting base and a press-in component, wherein the press-in component is movably disposed on the mounting base along the thickness direction of the plain concrete layer and can engage with the sealing component of the crack guide strip. Step S3, when installing the crack guide strip into the concrete, includes the following steps: Engage the press-in component with the crack guide strip and move it along the thickness direction of the plain concrete layer until the mounting base is in contact with the upper surface of the plain concrete layer. Then, drive the press-in component to move relative to the mounting base along the thickness direction of the plain concrete layer. The press-in component drives the connected crack guide strip to move into the concrete until the upper surface of the seal of the crack guide strip is flush with the upper surface of the plain concrete layer.
[0014] Optionally, the connector includes a connecting body and a plurality of connecting grooves disposed in the connecting body; In step S3, the multiple crack guide strips to be connected are first inserted into the multiple connecting grooves of the connecting body one by one, and the crack guide strips are bonded to the groove walls; then, the multiple crack guide strips and multiple connecting joints are embedded in the concrete together using the pressing structure.
[0015] Optionally, the seal includes a sealing portion, on which a protective layer is detachably connected; In step S3, the protective layer is separated from the sealing part before the crack guide strip is embedded in the concrete; during the concrete setting process, the sealing part adheres to the concrete.
[0016] Compared with the prior art, the beneficial effects of the present invention are as follows: This invention provides a crack guide strip, where the cross-sectional width at the upper end of the guide is greater than that at the lower end, making the lower end the sharpest part of the entire guide. When the plain concrete hardens and shrinks, generating tensile stress, the stress will significantly concentrate at the lower end of the guide, causing the tensile stress in the plain concrete at the lower end of the guide to preferentially reach its tensile limit. Consequently, the crack can initiate from the lower end of the guide and extend upward along the guide slope to the flexible energy dissipator, and then extend upward from the flexible energy dissipator to the sealing element, effectively locking the location of crack formation. Compared to a flat surface, the curved energy dissipation surface allows the flexible energy dissipator to have pre-stored deformation margin. Therefore, when the plain concrete around the flexible energy dissipator shrinks and displaces, the flexible energy dissipator deforms accordingly, converting the relative displacement and opening / closing displacement of the crack into the bending deformation of the energy dissipation surface. This not only fully ensures the reliability of the connection between the flexible energy dissipator and the plain concrete but also effectively avoids the direct transfer of stress to the plain concrete, preventing secondary cracks caused by additional stress concentration in the plain concrete. The seal installed on top of the flexible energy dissipator can block moisture and guide the rise of cracks on the slope, effectively suppressing the formation of surface cracks in the plain concrete layer and reducing the occurrence of through cracks.
[0017] This invention provides a construction method for building structural surface layers. A pre-divided grid can locate the installation position of crack guide strips, improving the installation accuracy. By pressing the crack guide strips into the concrete while pouring the plain concrete layer, the location of crack formation can be effectively limited, significantly reducing the generation of disordered secondary cracks and improving the durability of the plain concrete layer. During the pouring of the leveling layer, symmetrical and synchronous construction on both sides of the flexible connector allows for synchronized shrinkage and hardening of the material on both sides of the flexible connector, resulting in balanced stress. This effectively prevents unilateral shrinkage from causing the crack guide strips to shift, ensuring that cracks only occur at the designated locations. Attached Figure Description
[0018] Figure 1 A cross-sectional schematic diagram of a crack guide strip provided in an embodiment of the present invention; Figure 2 A cross-sectional schematic diagram of a crack guide strip in a plain concrete layer according to an embodiment of the present invention; Figure 3 A flowchart of a construction method for building structure surface layer provided in an embodiment of the present invention; Figure 4 A plan view illustrating the arrangement of crack guide strips in concrete in a construction method for building structural surface layers provided in an embodiment of the present invention; Figure 5 A schematic diagram of the press-fit structure used in the construction method of building structure surface layer provided in the embodiments of the present invention; Figure 6 This is a cross-sectional schematic diagram of the building structure surface layer during the construction of the roof slope-finding layer according to the building structure surface layer construction method provided in the embodiment of the present invention.
[0019] In the picture: 10. Plain concrete layer; 20. Leveling layer; 30. Floor slab; 40. Bonding layer; 50. Floor tile layer; 60. Roof slab; 70. Insulation layer; 80. Protective layer; 100. Crack guide strip; 110. Guide element; 111. Guide slope; 112. Anchoring part; 120. Flexible energy dissipation element; 121. Energy dissipation surface; 122. Arc-shaped protrusion; 123. Arc-shaped recess; 130. Sealing element; 131. Connecting plate; 132. Sealing part; 133. First mounting groove; 200. Press-in structure; 210. Mounting base; 211. U-shaped base; 212. Operating handle; 213. Connecting rod; 214. Spring; 215. Leveling component; 216. Adhesive plate; 220. Press-in component; 221. Slot; 300. Connecting connector. Detailed Implementation
[0020] The present invention will now be described in further detail with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the invention and not intended to limit it. Furthermore, it should be noted that, for ease of description, the accompanying drawings show only the parts relevant to the present invention, and not all of the structures.
[0021] In the description of this invention, unless otherwise explicitly specified and limited, the terms "connected," "linked," and "fixed" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.
[0022] In this invention, unless otherwise explicitly specified and limited, "above" or "below" the second feature can include direct contact between the first and second features, or contact between the first and second features through another feature between them. Furthermore, "above," "over," and "on top" of the second feature includes the first feature directly above or diagonally above the second feature, or simply indicates that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature includes the first feature directly below or diagonally below the second feature, or simply indicates that the first feature is at a lower horizontal level than the second feature.
[0023] In the description of this embodiment, the terms "upper," "lower," "right," etc., refer to the orientation or positional relationship shown in the accompanying drawings. They are used only for ease of description and simplification of operation, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the present invention. In addition, the terms "first" and "second" are used only for distinction in description and have no special meaning.
[0024] Example 1 like Figure 1 and Figure 2 As shown, this embodiment provides a crack guide strip 100, which can effectively limit the location of crack generation, significantly reduce the generation of disordered secondary cracks, and improve the durability of plain concrete layer 10.
[0025] See Figure 1 and Figure 2 The crack guide strip 100 includes a guide element 110, a flexible energy dissipation element 120, and a sealing element 130. The guide element 110 can be anchored in the plain concrete layer 10, and the guide element 110 is provided with a direction parallel to the thickness direction of the plain concrete layer 10. Figure 1The guide slope 111 is set at an angle (in the X direction) so that the cross-sectional width of the upper end of the guide 110 is greater than the cross-sectional width of the lower end of the guide 110, and the crack starts from the lower end of the guide 110; the flexible energy dissipation element 120 is set on the top of the guide 110, and the flexible energy dissipation element 120 is provided with an arc-shaped curved energy dissipation surface 121; the sealing element 130 is set on the top of the flexible energy dissipation element 120 and can be sealed to the plain concrete layer 10. The guide 110, the flexible energy dissipation element 120 and the sealing element 130 are arranged coaxially along the thickness direction of the plain concrete layer 10.
[0026] The crack guide strip 100 provided in this embodiment has a cross-sectional width at the upper end of the guide member 110 that is greater than that at the lower end, making the lower end of the guide member 110 the sharpest part of its entire structure. When the plain concrete hardens and shrinks, generating tensile stress, the stress will be significantly concentrated at the lower end of the guide member 110, causing the tensile stress of the plain concrete at the lower end of the guide member 110 to preferentially reach the tensile limit. Consequently, the crack can initiate from the lower end of the guide member 110 and extend upward along the guide slope 111 to the flexible energy dissipation member 120, and then extend upward from the flexible energy dissipation member 120 to the sealing member 130, effectively locking the location where the crack will form. Compared to a flat surface, the curved energy-dissipating surface 121 allows the flexible energy-dissipating element 120 to have pre-existing deformation margin. Therefore, when the plain concrete surrounding the flexible energy-dissipating element 120 shrinks and displaces, the flexible energy-dissipating element 120 deforms accordingly, converting the relative displacement and opening / closing displacement of the cracks into the bending deformation of the energy-dissipating surface 121. This not only ensures the reliability of the connection between the flexible energy-dissipating element 120 and the plain concrete but also effectively prevents stress from being directly transferred to the plain concrete, preventing secondary cracks caused by additional stress concentration. The sealing element 130 located at the top of the flexible energy-dissipating element 120 blocks moisture and guides the rise of cracks at the inclined surface 111, effectively suppressing the formation of surface cracks in the plain concrete layer 10 and reducing the occurrence of through cracks.
[0027] In other words, the guide 110 can guide the location where the crack occurs, the flexible energy dissipation component 120 can absorb the concrete deformation at the crack, and the seal 130 can block water vapor and the crack. In this embodiment, the guide 110, the flexible energy dissipation component 120 and the seal 130 of the crack guide strip 100 have the functions of sequentially undertaking and are indispensable.
[0028] In this embodiment, the crack guide strip 100 has a strip-shaped structure, and the applicable plain concrete includes, but is not limited to, plain lightweight aggregate concrete and plain ordinary concrete.
[0029] For example, see Figure 1 The cross-sectional shape of the guide 110 is an inverted cone or an inverted trapezoid.
[0030] For example, both the guide 110 and the seal 130 are made of rigid polyvinyl chloride, with the guide 110 having a Shore hardness of 75-85 and the seal 130 having a Shore hardness of 70-80; the flexible energy dissipation element 120 is made of flexible polyvinyl chloride, with a Shore hardness of 16-33, and the flexible energy dissipation element 120 is connected to the guide 110 and to the seal 130 by a fusion method.
[0031] Optionally, see Figure 1 and Figure 2 The flexible energy dissipator 120 includes several arc-shaped protrusions 122 and several arc-shaped recesses 123. Both the arc-shaped protrusions 122 and the arc-shaped recesses 123 extend circumferentially along the flexible energy dissipator 120. The arc-shaped protrusions 122 and arc-shaped recesses 123 are alternately arranged vertically. An energy dissipation surface 121 is formed on the surfaces of the arc-shaped protrusions 122 and arc-shaped recesses 123. This arrangement makes the energy dissipation surface 121 wavy, with several nodes and several antinodes, which not only adapts to the reciprocating deformation of the crack opening and closing simultaneously, but also achieves the gradual dissipation of energy through the deformation of the flexible energy dissipator 120.
[0032] Specifically, when the plain concrete on both sides of the crack separates from each other, the energy dissipation surface 121 is gradually straightened, and the expansion of the nodes and antinodes adapts to the opening amount of the plain concrete; when the concrete on both sides of the crack approaches each other, the energy dissipation surface 121 undergoes compression buckling and bending concave, accommodating the compression displacement, and can simultaneously adapt to the opening and closing reciprocating deformation of the crack.
[0033] For example, the flexible energy dissipation component 120 can accommodate the opening and closing displacement of the plain concrete on both sides of the crack from 0.5 mm to 3.0 mm; the traditional rigid separation joint can only accommodate the opening and closing displacement of no more than 0.5 mm. In comparison, the flexible energy dissipation component 120 has a wider applicable displacement range and can fully adapt to three types of deformation conditions: temperature deformation, shrinkage deformation, and slight uneven settlement of the foundation.
[0034] Specifically, the displacement load of plain concrete acting on the flexible energy dissipator 120 is segmented along the wave length of the energy dissipation surface 121. The wave nodes bend, the antinodes are subjected to tension and compression, and the deformation is distributed gradually on multiple wave bodies, without forming a stress mutation in a single section.
[0035] In this embodiment, see Figure 1 The flexible energy dissipation component 120 includes two arc-shaped protrusions 122 and one arc-shaped recess 123. The two arc-shaped protrusions 122 are respectively disposed on the upper and lower sides of the arc-shaped recess 123. In other embodiments, there are 2 to 4 arc-shaped recesses 123, and the number of arc-shaped protrusions 122 is one more or one less than the number of arc-shaped recesses 123.
[0036] Optionally, seeFigure 1 and Figure 2 The sealing element 130 includes a connecting plate 131 and a sealing portion 132 disposed on the connecting plate 131. The connecting plate 131 is connected to the flexible energy dissipation element 120 and is flush with the upper surface of the plain concrete layer 10. The sealing portion 132 is provided with a protective layer that can be detachably connected to it. When the protective layer is separated from the sealing portion 132, the sealing portion 132 can adhere to and seal the plain concrete layer 10. The connecting plate 131 is a plate with a large cross-sectional area. Therefore, when the sealing portion 132 is sealed to the plain concrete, the connecting plate 131 can block water vapor and cracks from rising over a large area, improving the inhibition effect on the formation of cracks on the surface of the concrete layer. When the protective layer is connected to the sealing portion 132, it can fully protect the sealing portion 132 and prevent the sealing portion 132 from adhering to other structures. After the protective layer is separated from the sealing portion 132, the sealing portion 132 can fully contact and adhere to the surrounding plain concrete to form a sealed structure, effectively blocking the rise of water vapor and cracks.
[0037] Specifically, see Figure 1 There are two sealing parts 132, which are arranged symmetrically about the center of the connecting plate 131 and are located on the lower surface of the connecting plate 131.
[0038] For example, the connecting plate 131 is made of polyvinyl chloride, the sealing part 132 is made of butyl rubber sealing tape, and the protective layer is made of tearable polyethylene release film. Both butyl rubber sealing tape and polyethylene release film are existing technologies in the art and will not be described in detail here.
[0039] Optionally, the crack guide strip 100 also includes a crack-resistant mesh fabric, which includes a relaxation section, two fastening sections, and two extension sections. The relaxation section is laid in a relaxed state on the upper surface of the sealant 130. The two fastening sections are located on both sides of the relaxation section. The two extension sections correspond one-to-one with the two fastening sections. One end of the fastening section is connected to the relaxation section, and the other end is connected to the corresponding extension section. The fastening section is fixedly connected to the sealant 130, and the extension sections are fixedly laid on the upper surface of the plain concrete layer 10. This arrangement makes the crack-resistant mesh fabric on the sealant 130 appear as a pile segment with a relaxed middle and tensioned sides. Therefore, when cracks occur inside the concrete, the relaxed section can adapt to the deformation of the concrete, and the fixed extension sections can play a bridging role through the fastening sections. The crack-resistant mesh fabric as a whole can effectively disperse the shrinkage and temperature stress of the concrete surface, limit the crack width, and prevent the crack from expanding rapidly.
[0040] For example, the crack-resistant mesh is made of alkali-resistant coated fiberglass mesh, with the relaxation section, fastening section and extension section integrally formed. The alkali-resistant coated fiberglass mesh has the characteristics of being lightweight, high-strength, temperature-resistant, alkali-resistant, waterproof, corrosion-resistant, crack-resistant, and dimensionally stable, which can effectively avoid cracking caused by surface tension shrinkage and external forces in the plain concrete layer 10.
[0041] For example, the relaxation amount of the relaxation section is 2% to 5%, and the length of the extension section is 120mm to 150mm.
[0042] In this embodiment, see Figure 1 The upper surface of the seal 130 is provided with a first mounting groove 133 corresponding to the two fastening sections. The fastening sections are embedded in the corresponding first mounting groove 133 to fix the fastening sections on the seal 130 and to keep the loosening sections in a loose state on the upper surface of the seal 130.
[0043] Specifically, the first mounting groove 133 is disposed on the upper surface of the connecting plate 131 of the sealing member 130, and the cross-sectional shape of the first mounting groove 133 includes, but is not limited to, trapezoidal, rectangular, and dovetail shapes.
[0044] For example, when the cross-sectional shape of the first mounting groove 133 is dovetail-shaped, the width of the opening of the first mounting groove 133 is 3mm, the bottom width of the first mounting groove 133 is 400mm, and the depth of the first mounting groove 133 is 1.5mm.
[0045] For example, the distance between the two first mounting slots 133 is 20mm to 30mm.
[0046] For example, the first mounting groove 133 can be formed by either recessing the upper surface of the seal 130 or by bending a structure that protrudes from the upper surface of the seal 130.
[0047] Optionally, see Figure 1 and Figure 2 An anchoring part 112 is provided on the guide 110. The extension direction of the anchoring part 112 is set at an angle to the thickness direction of the plain concrete layer 10, so that the anchoring part 112 can be anchored in the plain concrete layer 10, thereby improving the reliability of the guide 110 anchoring in the plain concrete.
[0048] In this embodiment, the anchoring part 112 is inclined upward or perpendicular to the thickness direction of the plain concrete layer 10, so that when the guide 110 has the tendency to move upward and detach from the plain concrete layer 10, the anchoring part 112 can engage with the plain concrete, thereby improving the reliability of the anchoring.
[0049] For example, the anchoring part 112 has a triangular cross-sectional shape, and the root of the anchoring part 112 transitions to the surface of the guide 110 in an arc shape.
[0050] In this embodiment, see Figure 1 and Figure 2The guide 110 is provided with multiple anchoring layers spaced apart along the thickness direction of the plain concrete layer 10. Each anchoring layer includes multiple anchoring parts 112, which are spaced apart circumferentially along the guide 110. This arrangement allows multiple anchoring positions to be formed between the guide 110 and the plain concrete, significantly improving the reliability of the guide 110's anchorage in the plain concrete.
[0051] For example, the anchoring layer is provided with four layers, and each layer is provided with two anchoring parts 112.
[0052] Optionally, the crack guide strip 100 in this embodiment has various specifications. The length of the crack guide strip 100 along the thickness direction of the plain concrete layer 10 is 40mm to 180mm, the width of the upper end of the guide member 110 is in the range of 12mm to 18mm, the width of the lower end of the guide member 110 is in the range of 2mm to 5mm, the anchoring layer is provided with 3 to 6 layers, the extension length of the anchoring part 112 is in the range of 4mm to 8mm, and the upward tilt angle of the anchoring part 112 is in the range of 10° to 20°; the maximum width of the flexible energy dissipation member 120 is 8mm to 12mm. Within the specified range, the minimum width of the flexible energy dissipator 120 is in the range of 3mm to 6mm, the ratio of the radius of curvature of the arc-shaped protrusion 122 to the radius of curvature of the arc-shaped recess 123 is in the range of 1:1.2 to 1:1.8; the width of the connecting plate 131 is in the range of 40mm to 60mm, the thickness of the connecting plate 131 is in the range of 4mm to 6mm, the width of the sealing part 132 is in the range of 10mm to 15mm, and the thickness of the sealing part 132 is in the range of 1.5mm to 2.5mm.
[0053] Among them, the width direction of each component is Figure 1 in the Y direction.
[0054] Specifically, when the thickness of the plain concrete layer 10 is in the range of 50mm to 80mm, the length of the crack guide strip 100 along the thickness direction of the plain concrete layer 10 is 40mm, the length of the guide member 110 along the thickness direction of the plain concrete layer 10 is 20mm, and the length of the flexible energy dissipation member 120 along the thickness direction of the plain concrete layer 10 is 15mm; when the thickness of the plain concrete layer 10 is in the range of 80mm to 130mm, the length of the crack guide strip 100 along the thickness direction of the plain concrete layer 10 is 65mm, the length of the guide member 110 along the thickness direction of the plain concrete layer 10 is 35mm, and the length of the flexible energy dissipation member 120 along the thickness direction of the plain concrete layer 10 is 25mm; when When the thickness of the plain concrete layer 10 is in the range of 130mm to 200mm, the length of the crack guide strip 100 along the thickness direction of the plain concrete layer 10 is 100mm, the length of the guide element 110 along the thickness direction of the plain concrete layer 10 is 55mm, and the length of the flexible energy dissipation element 120 along the thickness direction of the plain concrete layer 10 is 40mm; when the thickness of the plain concrete layer 10 is in the range of 200mm to 300mm, the length of the crack guide strip 100 along the thickness direction of the plain concrete layer 10 is 180mm, the length of the guide element 110 along the thickness direction of the plain concrete layer 10 is 100mm, and the length of the flexible energy dissipation element 120 along the thickness direction of the plain concrete layer 10 is 75mm.
[0055] For example, along the thickness direction of the plain concrete layer 10, the guide member 110 has a length of 35 mm, and the flexible energy dissipator 120 has a length of 25 mm. The guide member 110 has a width of 15 mm at the upper end and a width of 3 mm at the lower end; the flexible energy dissipator 120 has a maximum width of 10 mm and a minimum width of 4 mm, the arc-shaped protrusion 122 has a radius of curvature of 3 mm, and the arc-shaped recess 123 has a radius of curvature of 4.5 mm; the connecting plate 131 has a width of 50 mm and a thickness of 5 mm, and the sealing part 132 has a width of 12 mm and a thickness of 2 mm.
[0056] Example 2 like Figures 1 to 6 As shown, this embodiment provides a construction method for a building structure surface layer. The building structure surface layer includes a plain concrete layer 10 and a leveling layer 20 stacked on top of the plain concrete layer 10. The construction method for the building structure surface layer is applicable to the crack guide strip 100 of Embodiment 1 and includes the following steps: S1. Divide the surface to be constructed into a grid to form multiple grid edges.
[0057] The building structure surface layer construction method provided in this embodiment can locate the installation position of the crack guide strip 100 by pre-dividing the grid, thereby improving the installation accuracy of the crack guide strip 100.
[0058] Specifically, see Figure 4After the surface to be worked on is cleaned, multiple 3m×3m grids are drawn on the surface according to the marked lines positioning method. Marked line positioning is existing technology in this field and will not be described in detail here.
[0059] The structural surface layer construction method of this embodiment is applicable not only to new buildings, but also to existing building renovation projects. When used for the renovation of existing floor slabs 30, the following steps are included before step S1: removing the original floor adhesive and loose leveling layer 20 on the structural floor slab 30 to expose the floor slab 30.
[0060] S2. Pour concrete onto the surface to be constructed to form a plain concrete layer 10.
[0061] Specifically, during the pouring process, the concrete is spread, vibrated, and leveled. Concrete pouring is an existing technology in this field and will not be described in detail here.
[0062] S3. Before the concrete initially sets, multiple crack guide strips 100 are embedded into the concrete to a predetermined depth using the press-in structure 200 along multiple grid edges, and adjacent crack guide strips 100 are connected using the connecting joint 300.
[0063] The preset depth is 1 / 3 to 2 / 3 of the thickness of the plain concrete layer 10, so that the distance between the lower end of the crack guide strip 100 and the lower surface of the plain concrete layer 10 along the thickness direction of the plain concrete layer 10 does not exceed 10mm to 20mm.
[0064] The construction method for the building structure surface layer provided in this embodiment can effectively limit the location of crack generation, significantly reduce the generation of disordered secondary cracks, and improve the durability of the plain concrete layer 10 while pouring the plain concrete layer 10.
[0065] In this embodiment, the number of crack guide strips 100 is determined according to the number of grid edges and the length of crack guide strips 100, as long as multiple crack guide strips 100 can be fully distributed along multiple grid edges.
[0066] In this embodiment, see Figure 2 and Figure 5 The press-in structure 200 includes a mounting base 210 and a press-in member 220. The press-in member 220 is movably disposed on the mounting base 210 along the thickness direction of the plain concrete layer 10 and can be engaged with the sealing member 130 of the crack guide strip 100.
[0067] When installing the crack guide strip 100 into the concrete in step S3, the following steps are included: engaging the press-in member 220 with the crack guide strip 100 and moving the press-in structure 200 along the thickness direction of the plain concrete layer 10 until the mounting base 210 is in contact with the upper surface of the plain concrete layer 10; then, driving the press-in member 220 to move relative to the mounting base 210 along the thickness direction of the plain concrete layer 10, the press-in member 220 drives the connected crack guide strip 100 to move into the concrete until the upper surface of the sealing member 130 of the crack guide strip 100 is flush with the upper surface of the plain concrete layer 10.
[0068] Specifically, see Figure 1 and Figure 5 The press-in part 220 is provided with a slot 221, and the seal 130 can be inserted into the slot 221.
[0069] Specifically, see Figure 2 and Figure 5 The mounting base 210 includes a U-shaped base 211, an operating handle 212, a connecting rod 213, a spring 214, a leveling element 215, and two bonding plates 216. One end of the connecting rod 213 is connected to the press-in element 220, and the other end is slidably inserted through the U-shaped base 211 along the thickness direction of the plain concrete layer 10 and connected to the operating handle 212. The spring 214 is sleeved on the connecting rod 213 and located in the U-shaped groove of the U-shaped base 211. The leveling element 215 is set on the U-shaped base 211 and is configured to detect the levelness of the U-shaped base 211. The two bonding plates 216 are respectively set at both ends of the U-shaped base 211.
[0070] In step S3, after the pressing structure 200 is moved to the point where the bonding plate 216 is bonded to the upper surface of the plain concrete layer 10, the level of the U-shaped seat 211 is adjusted by the leveling component 215. After the U-shaped seat 211 is level, the operating handle 212 is used to drive the connecting rod 213 to slide. The connecting rod 213 drives the pressing component 220 to move, and the pressing component 220 presses down on the crack guide strip 100. At the same time, the spring 214 deforms. Subsequently, after the crack guide strip 100 is pressed into place, the operating handle 212 is released. Under the elastic force of the spring 214, the connecting rod 213 drives the pressing component 220 to move away from the plain concrete layer 10. The pressing component 220 separates from the sealing component 130, completing the installation of the crack guide strip 100.
[0071] For example, the connecting rod 213 is a telescopic rod so that it can be adapted to different sizes of crack guide strips 100. The leveling component 215 is a level to ensure that the height difference between the two sides of the connecting plate 131 does not exceed 2mm.
[0072] The pressing structure 200 of this embodiment is simple and convenient to operate, which helps to improve construction efficiency. Moreover, by using the pressing structure 200 of this embodiment, the installation consistency of multiple crack guide strips 100 in concrete can be effectively improved, providing qualified construction conditions for subsequent construction.
[0073] In this embodiment, the connecting joint 300 includes a connecting body and multiple connecting grooves disposed in the connecting body. In step S3, the multiple crack guide strips 100 to be connected are first inserted one-to-one into the multiple connecting grooves of the connecting body, and the crack guide strips 100 are bonded to the groove walls; then, the pressing structure 200 is used to embed the multiple crack guide strips 100 and the multiple connecting joints 300 together into the concrete. The connecting joints 300 are used to connect adjacent multiple crack guide strips 100, which is convenient and quick to operate.
[0074] When the connecting joint 300 is anchored into the concrete, the upper surface of the connecting joint 300 is flush with the upper surface of the plain concrete layer 10.
[0075] Specifically, when the connecting body has two connecting grooves, the cross-sectional shape of the connecting body is L-shaped, which can connect two mutually perpendicular crack guide strips 100; when the connecting body has three connecting grooves, the cross-sectional shape of the connecting body is T-shaped, which can connect three crack guide strips 100; when the connecting body has four connecting grooves, the cross-sectional shape of the connecting body is cross-shaped, which can connect four crack guide strips 100.
[0076] For example, the connecting body is made of rigid polyvinyl chloride, the groove depth is 50 mm, and the cross-sectional shape of the connecting groove is the same as the cross-sectional shape of the crack guide strip 100.
[0077] Specifically, the connecting body is provided with a guide hole located at the opening of the connecting groove. The wall of the guide hole is inclined relative to the insertion direction of the crack guide strip 100 and the connecting groove, and the diameter of the guide hole at the end away from the opening of the connecting groove is larger than the diameter of the end connected to the connecting groove. The end of the crack guide strip 100 can enter the connecting groove through the guide hole. This design makes the guide hole a funnel-shaped hole, which helps to improve the convenience of inserting the crack guide strip 100 into the connecting body and facilitates on-site operation.
[0078] Specifically, several grooves are provided on the side wall of the connecting groove. In step S3, before the crack guide strip 100 is inserted into the connecting groove, the step of applying sealant to a portion of the surface of the crack guide strip 100 is also included. When the crack guide strip 100 is inserted into the connecting groove, there is a gap fit between the surface of the crack guide strip 100 and the groove wall of the connecting groove. The sealant is squeezed into the grooves and gaps, so that the crack guide strip 100 can adhere to the groove wall of the connecting groove. The crack guide strip 100 can be reliably inserted into the connecting groove, and the sealing of the connection is ensured, which helps to prevent moisture and cracks from rising from the connection between two adjacent crack guide strips 100.
[0079] For example, the sealant is a polyvinyl chloride-specific adhesive or a neutral silicone sealant.
[0080] Specifically, a snap-fit part is provided on the side wall of the connecting groove, the anchoring part 112 is inclined upward and the snap-fit part is inclined downward. After the anchoring part 112 enters the connecting groove, the anchoring part 112 can engage with the snap-fit part to prevent the guide 110 from disengaging from the connecting groove and improve the stability of the connection.
[0081] Specifically, the connecting groove has a protruding conductive part on its wall, forming a conductive groove between the conductive part and the groove wall. The conductive grooves of multiple connecting grooves are interconnected, and the conductive part can fit against the lower end of the guide 110. This design allows the shrinkage stress of the concrete to be conducted through the guide 110 to the connecting joint 300 and concentrated and released at the conductive groove, ensuring that the cracks at the junction of the two crack guide strips 100 can be regularly connected, and reducing irregular diagonal cracks around the connecting joint 300.
[0082] Optionally, after step S3 and before step S4, the following steps are also included: After the crack guide strip 100 is installed, the limiting structure is snapped into the crack guide strip 100 and anchored in the concrete; when the concrete has fully set or the crack guide strip 100 no longer moves in the concrete, the limiting structure is removed from the concrete and separated from the crack guide strip 100. This operation ensures that before the concrete strength reaches the required level, the limiting structure can effectively constrain the position of the crack guide strip 100 in the concrete, improving the installation accuracy of the crack guide strip 100.
[0083] In this embodiment, the limiting structure includes multiple U-shaped clamps, which are arranged at intervals along the extension direction of the crack guide strip 100. The crack guide strip 100 is inserted into the U-shaped groove of the U-shaped clamp, and both ends of the U-shaped clamp are inserted into the concrete.
[0084] For example, the U-shaped clamps are arranged every 1.0m to 1.5m, and the depth of the U-shaped clamps inserted into the concrete is 5mm to 10mm.
[0085] Optionally, after step S3 and before step S4, the following steps are also included: before the initial setting of the concrete, perform secondary troweling; and after the final setting of the concrete, cover it with geotextile and water it for curing for no less than 7 days.
[0086] The secondary troweling and curing of concrete are existing technologies in this field and will not be described in detail here.
[0087] Optionally, the seal 130 includes a sealing portion 132, on which a protective layer is detachably connected.
[0088] In step S3, before embedding the crack guide strip 100 into the concrete, the protective layer is separated from the sealing part 132 so that the bonding surface of the sealing part 132 is exposed; subsequently, during the concrete setting process, the sealing part 132 bonds with the concrete and is sealed to the plain concrete layer 10.
[0089] Specifically, in step S3, the crack guide strip 100 is first snapped into the press-in part 220; then, the protective layer is peeled off from the sealing part 132; next, the crack guide strip 100 is pressed into the concrete before initial setting using the press-in structure 200. During the pressing process, the sealing part 132 is in full contact with the concrete, thereby achieving reliable adhesion and sealing connection between the sealing part 132 and the concrete.
[0090] Optionally, the crack guide strip 100 also includes crack-resistant mesh. The steps following step S3 and before step S4 are as follows: After concrete curing, the crack-resistant mesh is laid on the sealant 130 and the upper surface of the plain concrete layer 10, and the crack-resistant mesh is connected to the sealant 130.
[0091] In this embodiment, the laying of the crack-resistant mesh fabric specifically includes the following steps: applying an interface agent to the upper surface of the plain concrete layer 10 on the surface of the sealant 130, and laying the crack-resistant mesh fabric in the center on the upper surface of the sealant 130, with the extended section of the crack-resistant mesh fabric fixedly connected to the upper surface of the plain concrete layer 10; at the same time, embedding the fastened section of the crack-resistant mesh fabric into the corresponding first mounting groove 133, and keeping the loosened section of the crack-resistant mesh fabric loose.
[0092] S4. After the concrete curing is completed, pour material on the surface of the plain concrete layer 10 to form the leveling layer 20. While pouring the material, ensure that the material is poured symmetrically and synchronously on both sides of the crack guide strip 100.
[0093] The materials include, but are not limited to, concrete and cement mortar. The pouring process of the materials is existing technology in this field and will not be described in detail here.
[0094] The construction method for the building structure surface layer provided in this embodiment allows the material to be poured symmetrically and synchronously on both sides of the crack guide strip 100 when the leveling layer 20 is formed. This enables the material on both sides of the crack guide strip 100 to shrink and harden synchronously and be subjected to balanced force, effectively avoiding the displacement of the crack guide strip 100 due to unilateral shrinkage, and ensuring that cracks can only occur in the set position.
[0095] Furthermore, compared to existing technologies that involve cutting expansion joints, subsequent grouting repairs, and finishing rework, the construction method for building structure surface layers in this embodiment can significantly reduce construction costs and improve construction economy.
[0096] Optionally, when the building structure surface layer is a subfloor of floor tiles, the building structure surface layer also includes a bonding layer 40, a floor slab 30 with a thickness of 60mm, a plain concrete layer 10 with a thickness of 40mm made of lightweight aggregate concrete, a leveling layer 20 with a thickness of 20mm made of fine stone concrete, and a bonding layer 40 with a thickness of 10mm made of dry-hardened cement mortar.
[0097] The construction method for the building structure surface layer in this embodiment specifically includes the following steps: S11. Clean the surface of floor slab 30 and divide the surface of floor slab 30 into a 3m×3m grid. The distance from the outermost edge of the grid to the wall is 150mm. S21. Pour lightweight aggregate concrete mixed with polypropylene coarse fiber and calcium sulfoaluminate expansion agent onto the surface to be constructed to form plain concrete layer 10. S31. Before the concrete initially sets, the protective layer is separated from the sealing part 132, and multiple crack guide strips 100 are embedded in the concrete using the pressing structure 200 along multiple grid edges. At the same time, two adjacent crack guide strips 100 are connected using the connecting joint 300. Subsequently, secondary troweling and curing are performed. Next, the crack-resistant mesh is installed onto the sealing part 130 and the plain concrete layer 10.
[0098] S41. After the concrete curing is completed, fine stone concrete is poured on the surface of plain concrete layer 10 to form leveling layer 20. S51. After the leveling layer 20 has dried, the bonding layer 40 shall be constructed on top of the leveling layer 20. S61. Construct the floor tile layer 50 above the bonding layer 40. Fill the tile joints that coincide with the grid edge with neutral silicone sealant, and fill the tile joints that do not coincide with the grid edge with ordinary grout.
[0099] In this embodiment, the sealing part 132, the crack-resistant mesh part, and the neutral silicone sealant can form three layers of protection from bottom to top, effectively blocking the transmission of cracks to the floor tile layer 50, and significantly improving the water resistance and crack resistance of the building structure surface layer.
[0100] Optionally, when the building structure surface layer is a subfloor of rubber flooring, the floor slab is 30mm thick and 60mm thick, the plain concrete layer is 10mm thick and 40mm thick, made of lightweight aggregate concrete, and the leveling layer is 20mm thick and 20mm thick, made of fine stone concrete.
[0101] The construction method for the building structure surface layer in this embodiment specifically includes the following steps: S12. Clean the surface of floor slab 30 and divide the surface of floor slab 30 into a 3m×3m grid; S22. Pour lightweight aggregate concrete onto the surface to be constructed to form a plain concrete layer 10. S32. Before the concrete sets, the protective layer is separated from the sealing part 132, and multiple crack guide strips 100 are embedded in the concrete along multiple grid edges using the press-in structure 200. At the same time, two adjacent crack guide strips 100 are connected using the connecting joint 300. Then, a second troweling and curing are performed. Next, the crack-resistant mesh is installed on the sealing part 130 and the plain concrete layer 10.
[0102] S42. After the concrete curing is completed, fine stone concrete is poured on the surface of plain concrete layer 10 to form leveling layer 20. S52. After the moisture content of the leveling layer 20 drops to no more than 4.5%, first apply a 200mm wide layer of elastic polyurethane to the leveling layer 20, with the elastic polyurethane positioned directly above the crack guide strip 100. Then, apply self-leveling cement to the entire surface of the leveling layer 20. After the cement dries, fully adhere a 2mm thick layer of floor adhesive to the cement surface. When fully adhering the floor adhesive, use hot-melt welding at the joints where the floor adhesive coincides with the grid edge, ensuring that the weld can withstand minor deformations of the underlying structure without tearing.
[0103] Optionally, when the building structure surface layer is a thick plain concrete cushion layer, the plain concrete layer 10 is 100mm thick C15 plain concrete or 150mm thick C20 concrete, and the C20 concrete contains a steel mesh.
[0104] When the plain concrete layer 10 is 100mm thick C15 plain concrete, the construction method for the building structure surface layer in this embodiment can be performed according to steps S11, S21, and S31. When the plain concrete layer 10 is 150mm thick C20 concrete, the construction method for the building structure surface layer in this embodiment specifically includes the following steps: S13. Clean the surface of floor slab 30 and divide the surface of floor slab 30 into a 3m×3m grid; S23. Pour concrete onto the surface to be constructed and install the steel mesh into the concrete. When installing the steel mesh, it is necessary to break the steel mesh 50mm away from the crack guide strip 100. The broken end of the steel mesh should be anchored into the concrete to avoid rigid force transmission of the steel bars at this point.
[0105] Optionally, when the building structure surface layer is a roof slope-finding layer, the building structure surface layer also includes a protective layer 80, which is 40mm thick and made of C20 fine stone concrete; a plain concrete layer 10 of varying thickness, with the thinnest part being 50mm thick and the thickest part being approximately 250mm~300mm, with a slope of 2%, and the plain concrete layer 10 is made of lightweight aggregate concrete; and a leveling layer 20 of 20mm thickness, made of cement mortar.
[0106] The construction method for the building structure surface layer in this embodiment specifically includes the following steps: S14. Divide the surface of the floor slab into a 3m×3m grid; S24. Pour lightweight aggregate concrete onto the surface to be constructed to form a plain concrete layer with a slope 10. S34. Before the initial setting of the concrete, the protective layer is separated from the sealing part 132, and multiple crack guide strips 100 are embedded in the concrete along multiple grid edges using the pressing structure 200. At the same time, adjacent crack guide strips 100 are connected using the connecting joint 300. The thickest part of the plain concrete layer 10 uses crack guide strips 100 with a length of 180mm along the thickness direction of the plain concrete layer 10, and the part of the plain concrete layer 10 with a thickness of less than 100mm uses crack guide strips 100 with a length of 65mm or 45mm along the thickness direction of the plain concrete layer 10. Subsequently, secondary troweling and curing are performed.
[0107] S44. After the concrete curing is completed, cement mortar is poured on the surface of the plain concrete layer 10 to form a leveling layer 20. S54. After the leveling layer 20 dries, the waterproof membrane, the insulation layer 70, and the protective layer 80 are laid on top of the leveling layer 20 in the order from bottom to top.
[0108] The protective layer 80 is provided with a steel mesh, and the treatment of the steel mesh is the same as in step S23, so it will not be described again here.
[0109] In this embodiment, polyethylene foam rods, polyethylene foam boards, and weather-resistant silicone sealant are sequentially arranged from bottom to top at the break in the reinforcing mesh. Polyethylene foam rods, polyethylene foam boards, and weather-resistant silicone sealant are all existing technologies in the art and will not be described in detail here.
[0110] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the implementation of the present invention. Those skilled in the art will be able to make various obvious changes, readjustments, and substitutions without departing from the scope of protection of the present invention. It is neither necessary nor possible to exhaustively describe all embodiments here. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the scope of protection of the claims of the present invention.
Claims
1. A crack guide strip, characterized in that, include: The guide (110) can be anchored in the plain concrete layer (10). The guide (110) is provided with a guide slope (111) that is angled to the thickness direction of the plain concrete layer (10) so that the cross-sectional width of the upper end of the guide (110) is greater than the cross-sectional width of the lower end of the guide (110), and the crack starts from the lower end of the guide (110). A flexible energy dissipation component (120) is disposed on the top of the guide (110), and the flexible energy dissipation component (120) is provided with an arc-shaped curved energy dissipation surface (121). A sealing element (130) is disposed on the top of the flexible energy dissipation element (120) and can be sealed to the plain concrete layer (10). The guide element (110), the flexible energy dissipation element (120) and the sealing element (130) are arranged coaxially along the thickness direction of the plain concrete layer (10).
2. The crack guide strip according to claim 1, characterized in that, The flexible energy dissipation component (120) includes a plurality of arc-shaped protrusions (122) and a plurality of arc-shaped recesses (123). The arc-shaped protrusions (122) and the arc-shaped recesses (123) extend circumferentially along the flexible energy dissipation component (120). The arc-shaped protrusions (122) and the arc-shaped recesses (123) are alternately arranged vertically. The energy dissipation surface (121) is formed on the surface of the arc-shaped protrusions (122) and the arc-shaped recesses (123).
3. The crack guide strip according to claim 1, characterized in that, The crack guide strip (100) also includes crack-resistant mesh fabric, which includes a relaxation section, two fastening sections and two extension sections. The relaxation section is laid on the upper surface of the sealant (130) in a relaxed state. The two fastening sections are located on both sides of the relaxation section. The two extension sections correspond one-to-one with the two fastening sections. One end of the fastening section is connected to the relaxation section and the other end is connected to the corresponding extension section. The fastening section is fixedly connected to the sealant (130), and the extension section is fixedly laid on the upper surface of the plain concrete layer (10).
4. The crack guide strip according to claim 3, characterized in that, The upper surface of the seal (130) is provided with a first mounting groove (133) corresponding to the two fastening sections, and the fastening sections are embedded in the corresponding first mounting groove (133).
5. The crack guide strip according to claim 1, characterized in that, The sealing element (130) includes a connecting plate (131) and a sealing part (132) disposed on the connecting plate (131). The connecting plate (131) is connected to the flexible energy dissipation element (120) and is flush with the upper surface of the plain concrete layer (10). The sealing part (132) is provided with a protective layer that can be detachably connected to it. When the protective layer is separated from the sealing part (132), the sealing part (132) can adhere to and seal the plain concrete layer (10).
6. The crack guide strip according to claim 1, characterized in that, The guide (110) is provided with an anchoring part (112), the extension direction of the anchoring part (112) is set at an angle to the thickness direction of the plain concrete layer (10), so that the anchoring part (112) can be anchored in the plain concrete layer (10).
7. A construction method for a building structural surface layer, wherein the building structural surface layer comprises a plain concrete layer (10) and a leveling layer (20) stacked on top of the plain concrete layer (10), characterized in that, The construction method for the building structure surface layer is applicable to the crack guide strip (100) as described in any one of claims 1-6, and includes the following steps: S1. Divide the surface to be constructed into a grid to form multiple grid edges; S2. Pour concrete onto the surface to be constructed to form the plain concrete layer (10). S3. Before the concrete sets, along the multiple grid edges, multiple crack guide strips (100) are embedded into the concrete to a predetermined depth using a pressing structure (200), and adjacent crack guide strips (100) are connected using a connecting joint (300). S4. After the concrete curing is completed, pour material on the surface of the plain concrete layer (10) to form the leveling layer (20); while pouring the material, make the material symmetrical and synchronously constructed on both sides of the crack guide strip (100).
8. The construction method for the surface layer of a building structure according to claim 7, characterized in that, The press-in structure (200) includes a mounting base (210) and a press-in member (220). The press-in member (220) is movably disposed on the mounting base (210) along the thickness direction of the plain concrete layer (10) and can engage with the sealing member (130) of the crack guide strip (100). When installing the crack guide strip (100) into the concrete in step S3, the following steps are included: Engage the press-in component (220) with the crack guide strip (100) and move the press-in structure (200) along the thickness direction of the plain concrete layer (10) until the mounting base (210) is in contact with the upper surface of the plain concrete layer (10); then, drive the press-in component (220) to move relative to the mounting base (210) along the thickness direction of the plain concrete layer (10), and the press-in component (220) drives the connected crack guide strip (100) to move into the concrete until the upper surface of the seal (130) of the crack guide strip (100) is flush with the upper surface of the plain concrete layer (10).
9. The construction method for the surface layer of a building structure according to claim 7, characterized in that, The connector (300) includes a connecting body and a plurality of connecting grooves disposed in the connecting body; In step S3, the multiple crack guide strips (100) to be connected are first inserted into the multiple connecting grooves of the connecting body one by one, and the crack guide strips (100) are bonded to the groove wall of the connecting groove; then, the multiple crack guide strips (100) and the multiple connecting joints (300) are buried together in the concrete using the pressing structure (200).
10. The construction method for the surface layer of a building structure according to claim 7, characterized in that, The sealing element (130) includes a sealing part (132), on which a protective layer is provided that can be detachably connected; In step S3, before embedding the crack guide strip (100) into the concrete, the protective layer is separated from the sealing part (132); during the concrete setting process, the sealing part (132) adheres to the concrete.