Joint structure

By designing multiple recesses and contact areas between conductive wires and pads in the metal-to-metal bonding structure, the problems of poor electrical performance and nanowire escapement are solved, achieving better electrical performance and cost reduction.

CN221783203UActive Publication Date: 2024-09-27ADVANCED SEMICON ENG INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323612188.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-28
Publication Date
2024-09-27
Estimated Expiration
2033-12-28

AI Technical Summary

Technical Problem

The existing metal-to-metal bonding structures have poor electrical performance, and nanowires are prone to leakage during bonding, resulting in electrical degradation. The cost is high and the implementation threshold is high.

Method used

Using multiple first conductive lines and second conductive lines and corresponding pad designs, the problem of solder is avoided by setting recesses and contact areas in the pads to achieve a larger contact area and stronger bonding strength, And provide better electrical performance by setting the bonding layer.

Benefits of technology

It achieves better electrical performance, reduces costs, avoids electrical degradation caused by nanowire migration, and provides stronger bonding strength.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221783203U
    Figure CN221783203U
Patent Text Reader

Abstract

The present application discloses a bonding structure. The bonding structure includes: a plurality of first conductive lines; a first pad under the plurality of first conductive lines and including a first recess to accommodate the plurality of first conductive lines, the first recess including a first opening having a first width in a horizontal direction; a plurality of second conductive lines horizontally overlapping the plurality of first conductive lines; a second pad under the plurality of second conductive lines and including a second recess to accommodate the plurality of second conductive lines, the second recess including a second opening having a second width in the horizontal direction; wherein the first width is different from the second width. According to the technical scheme, at least the problem of poor electrical performance caused by a joint structure in the prior art can be solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and more particularly, to a bonding structure. Background Art

[0002] like Figure 1 As shown in the figure, in the case of metal-to-metal (e.g., copper-to-copper) bonding, there is usually only a single point of contact between the surface of the metal pad (or through hole) 12, 14 and the tip edge of the metal conductive column 22, 24. Since such a contact area is always small, it leads to poor electrical performance. Further, in the metal-to-metal bonding, the conductive columns 22, 24 or pads 12, 14 formed by electroplating are generally limited by the coplanar uniformity (U%). If they are directly bonded, after the bonding force is released, the actual pads 12, 14 with different coplanarities often have connection errors, such as Figure 1 The conductive pillar 22 shown in the dotted line frame S1 is connected to the thicker pad 12, while the conductive pillar 24 shown in the dotted line frame S2 is not connected to the lower pad 14. Therefore, CMP (Chemical Mechanical Planarization) is usually used to level the bonding surface (for example, level the surfaces of the pads 12 and 14) and align them before butt bonding.

[0003] However, CMP is costly, has high restrictions on the docking environment, and has a high implementation threshold. Figure 2A As shown, the current nanowire technology forms multiple nanowires 70 on pads 52 (which may be referred to as mother pads 52) and pads 62 (which may be referred to as male pads 62) and directly connects them, and electrical connection can be completed without CMP. Figure 2B As shown, the process of docking multiple nanowires 70 will form an outward-flowing portion 75 due to mutual squeezing, so some nanowires 70 do not contact the opposite pad 52, pad 62, or opposite nanowire 70, resulting in poor electrical properties. Although this method provides a male pad 62, a female pad 52 and a nanowire 70 docking design, the width of the concave portion 52R on one side of the female pad 52 is greater than the width of the male pad 62, so some of the nanowires 70 after docking will still form an outward-flowing portion 75 and outward-flow to the side of the male pad 62, which may still cause a decrease in electrical properties. Utility Model Content

[0004] In view of the above problems, the present application proposes a bonding structure to at least solve the problem of poor electrical performance caused by the bonding structure in the prior art.

[0005] The technical solution of this application is implemented as follows:

[0006] According to one aspect of the present application, a bonding structure is provided, which includes: a plurality of first conductive wires; a first solder pad, located below the plurality of first conductive wires and including a first recess for accommodating the plurality of first conductive wires, the first recess including a first opening having a first width in a horizontal direction; a plurality of second conductive wires, horizontally overlapping with the plurality of first conductive wires; a second solder pad, located below the plurality of second conductive wires and including a second recess for accommodating the plurality of second conductive wires, the second recess including a second opening having a second width in a horizontal direction; wherein the first width is different from the second width.

[0007] In some embodiments, a thickness of the first pad in a vertical direction is smaller than a thickness of the second pad, and the first width is smaller than the second width.

[0008] In some embodiments, multiple first conductive wires contact each other in a first contact area within a first recess, and multiple second conductive wires contact each other in a second contact area within a second recess. In a vertical cross-sectional perspective or a top-down perspective, the area of ​​the first contact area is smaller than the area of ​​the second contact area.

[0009] In some embodiments, multiple first conductive lines include a portion that is not in contact with each other, one of the multiple portions of the multiple first conductive lines has a first length, multiple second conductive lines include a portion that is not in contact with each other, one of the multiple portions of the multiple second conductive lines has a second length, and the first length is longer than the second length.

[0010] In some embodiments, a portion of the surface of the first recess is separated from the plurality of first conductive lines.

[0011] In some embodiments, a first conductive line among the plurality of first conductive lines has a first bend angle.

[0012] In some embodiments, at least two first conductive lines among the plurality of first conductive lines include different bend angles from each other.

[0013] According to another aspect of the present application, a bonding structure is provided, which includes: a plurality of first conductive wires; a first solder pad, located below the plurality of first conductive wires and having a first top surface facing the plurality of first conductive wires, the first top surface having a first recess for accommodating the plurality of first conductive wires; a plurality of second conductive wires, horizontally overlapping with the plurality of first conductive wires; a second solder pad, located below the plurality of second conductive wires and having a second top surface facing the plurality of second conductive wires, the second top surface having a second recess for accommodating the plurality of second conductive wires; wherein the first top surface is not flush with the second top surface, and the bottom of the first recess is not flush with the bottom of the second recess.

[0014] In some embodiments, the first recess includes a first opening having a first width, and the second recess includes a second opening having a second width, wherein the first width is smaller than the second width, and the second top surface is higher than the first top surface.

[0015] In some embodiments, a plurality of first conductive lines contact each other at a first contact region in the first recess, a plurality of second conductive lines contact each other at a second contact region in the second recess, and a thickness of the first contact region is less than a thickness of the second contact region.

[0016] The above technical solution of the present application can achieve direct interconnection and bonding by using multiple first nanowires, second nanowires and first pads and second pads to achieve direct interconnection and bonding, so as to obtain a shorter path with better electrical performance. Since solder is not required for interconnection, the overall structure thickness can be reduced at low cost and thinned, and some solder problems can be avoided. In addition, by providing a first recess and a second recess in the first pad and the second pad to concentrate and accommodate the first nanowire and the second nanowire, more contact area can be provided, which is not restricted by coplanarity, provides better electrical performance, and avoids the problem of electrical degradation caused by the outflow of nanowires in the prior art. In addition, by providing a first bonding layer and a second bonding layer, a stronger bonding strength can be provided between the first nanowire and the first bonding layer, and between the second nanowire and the second bonding layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0018] Figure 1 It is a cross-sectional schematic diagram of a bonding structure in the prior art.

[0019] Figure 2A and Figure 2B They are schematic cross-sectional views of a bonding structure using nanowires in the prior art before and after bonding.

[0020] Figure 3 is a schematic cross-sectional view of a bonding structure according to an embodiment of the present application.

[0021] Figure 4A Shows Figure 3 A locally enlarged schematic diagram of multiple first nanowires and a first pad.

[0022] Figure 4B Shows Figure 3 A local enlarged schematic diagram of multiple second nanowires and second pads.

[0023] Figure 4C It is a partially enlarged schematic diagram after two second nanowires are bonded to the second bonding layer.

[0024] FIG. 5A to FIG. 5S is formed Figure 3 Schematic cross-sectional view of the multiple step stages of the bonding structure shown.

[0025] Figure 6 , 7A to 7C ,and Figures 8 to 11 Each of them is a schematic cross-sectional view of a bonding structure according to another embodiment of the present application.

[0026] Fig. 12A It is a cross-sectional schematic diagram when a plurality of first nanowires and second nanowires are placed upward according to an embodiment of the present application.

[0027] FIG. 12B to FIG. 12F According to different embodiments Figure 2A A schematic top view from a top-down perspective is shown. DETAILED DESCRIPTION

[0028] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field belong to the scope of protection of this application.

[0029] The following disclosure provides many different embodiments or examples for realizing different features of the provided subject matter. Specific examples of components and arrangements will be described below to simplify the present invention. Of course, these are merely examples and are not intended to limit the present invention. For example, in the following description, forming a first component above or on a second component may include an embodiment in which the first component and the second component are in direct contact, and may also include an embodiment in which an additional component is formed between the first component and the second component so that the first component and the second component may not be in direct contact. Moreover, the present invention may repeatedly refer to numbers and / or letters in various examples. This repetition is only for simplicity and clarity, and does not itself represent the relationship between the various embodiments and / or configurations discussed.

[0030] In addition, the embodiments and features in the embodiments of the present application may be combined with each other without conflict. The present application will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.

[0031] Figure 3 is a schematic cross-sectional view of a bonding structure 100 according to an embodiment of the present application. Figure 3As shown, the bonding structure 100 includes a plurality of first nanowires 112 and a first pad 130 located below the plurality of first nanowires 112. The first pad 130 includes a first recess 130R for accommodating the plurality of first nanowires 112. The bonding structure 100 also includes a plurality of second nanowires 114 and a second pad 140 located below the plurality of second nanowires 114. The plurality of second nanowires 114 overlap with the plurality of first nanowires 112 in a horizontal direction. The second pad 140 includes a second recess 140R for accommodating the plurality of second nanowires 114.

[0032] The first recess 130R has a first opening 132, which is one end of the first recess 130R facing the plurality of first nanowires 112. The first opening 132 has a first width W1 in the horizontal direction. The second recess 140R has a second opening 142, which is one end of the second recess 140R facing the plurality of second nanowires 114. The second opening 142 has a second width W2 in the horizontal direction that is different from the first width W1. The plurality of first nanowires 112 may have a width W3, and the plurality of second nanowires 114 may have a width W4. The first width W1 of the first opening 132 may be greater than the width W3 of the plurality of first nanowires 112, so that the first recess 130R may accommodate the plurality of first nanowires 112. The second width W2 of the second opening 142 may be greater than the width W4 of the plurality of second nanowires 114, so that the second recess 140R may accommodate the plurality of second nanowires 114.

[0033] In some embodiments, the width W3 of the plurality of first nanowires 112 may be in the range of 3 μm to 30 μm, and the width W4 of the plurality of second nanowires 114 may be in the range of 3 μm to 30 μm. In some embodiments, the width of a single first nanowire 112 may be in the range of several nanometers to several hundred nanometers, and the width of a single second nanowire 114 may be in the range of several nanometers to several hundred nanometers.

[0034] It should be understood that although the technical solution of the present application is described with a plurality of first nanowires 112 and a plurality of second nanowires 114 , the plurality of first nanowires 112 and the plurality of second nanowires 114 may also be other types of conductive wires extending in the vertical direction.

[0035] The above technical solution of the present application realizes direct interconnection and bonding by connecting a plurality of first nanowires 112 and second nanowires 114 with first pads 130 and second pads 140, and can obtain a shorter path to have better electrical performance. Since solder is not required for interconnection, the overall structure thickness can be reduced at a low cost, and some solder problems such as cracks, cold joints, bridging at small pitches, and delamination can be avoided. Furthermore, by providing a first recess 130R and a second recess 140R in the first pad 130 and the second pad 140 to concentrate and accommodate a plurality of first nanowires 112 and second nanowires 114, after the first nanowire 112 and the second nanowire 114 enter the corresponding first recess 130R and the second recess 140R, the first nanowire 112 and the second nanowire 114 will rotate and slide along the surface of the first recess 130R and the second recess 140R and be connected to the corresponding first pad 130 and the second pad 140, thereby having more contact area, not being restricted by coplanarity, providing better electrical performance, and avoiding the problem of electrical degradation due to the outward leakage of nanowires in the prior art.

[0036] Continue to refer Figure 3 As shown, in this embodiment, the bonding structure 100 is connected between the bottom device 1100 and the top device 1200. The first pad 130 and the second pad 140 are located on the bottom device 1100. The first nanowire 112 and the second nanowire 114 are connected to the top device 1200. In some embodiments, the bottom device 1100 can be any one of a substrate, a wafer or a chip. In some embodiments, the top device 1200 can be any one of a substrate, a wafer or a chip. In some embodiments, the bottom device 1100 and the top device 1200 may include a layer formed of a dielectric material, which may use an organic dielectric material (such as PI (Polyimide, polyimide), epoxy resin, ABF (Ajinomoto Build-up Film, Ajinomoto Build-up Film), PP (Polypropylene, polypropylene) or / and acrylic acid, etc.), and / or a non-organic dielectric material (such as ceramics, silicon, glass, quartz and / or GaAs (gallium arsenide), etc.). In some embodiments, the dielectric materials in the bottom device 1100 and the top device 1200 may use organic photosensitive liquids or / and dry film materials, or / and, organic non-photosensitive liquids or / and dry film materials.

[0037] In this embodiment, the first recess 130R and the second recess 140R both have a trapezoidal cross section. Specifically, the first recess 130R and the second recess 140R both have a flat bottom surface and a side surface connected to the bottom surface and tilted outward in an upward direction. However, it should be understood that the present application does not limit the shapes of the first recess 130R and the second recess 140R.

[0038] The bonding structure 100 may further include a third pad 150 and a fourth pad 160 connected to the top device 1200. The third pad 150 is connected to one end of the plurality of first nanowires 112 opposite to the first pad 130, that is, connected to the top of the plurality of first nanowires 112. The fourth pad 160 is connected to one end of the plurality of second nanowires 114 opposite to the second pad 140, that is, connected to the top of the plurality of second nanowires 114. In some embodiments, the thickness of the third pad 150 and the fourth pad 160 may be the same. A top seed layer 202 may be provided between the third pad 150 and the first nanowire 112, and between the fourth pad 160 and the second nanowire 114, respectively. In some embodiments, the material of the top seed layer 202 may be any one of Cu, Au, Ag, Al, Pd (palladium), Pt (platinum), and Ni (nickel), or any alloy of multiple thereof.

[0039] In some embodiments, the metal material of the first pad 130, the second pad 140, the third pad 150 and the fourth pad 160 may be any one of Cu (copper), Au (gold), Ag (silver) and Al (aluminum) or any alloy thereof. In some embodiments, the material of the first nanowire 112 and the second nanowire 114 may be any one of Cu, Au, Ag and Al or any alloy thereof. In some embodiments, the interval GI between the bottom device 1100 and the top device 1200 may be in the range of 20 μm to 100 μm.

[0040] The plurality of first nanowires 112, the plurality of second nanowires 114, the first pads 130, and the second pads 140 may be covered by a protective layer 290. In some embodiments, the material of the protective layer 290 may be, for example, an underfill material or a molding material. In some embodiments, the material of the protective layer 290 may be an organic material, such as PI, epoxy resin, ABF, PP, or / and acrylic acid. In some embodiments, the material of the protective layer 290 may be an organic photosensitive liquid or / and a dry film material, or / and, an organic non-photosensitive liquid or / and a dry film material.

[0041] In the present embodiment, the thickness T1 of the first pad 130 in the vertical direction is smaller than the thickness T2 of the second pad 140, and the first width W1 of the first opening 132 may be smaller than the second width W2 of the second opening 142. In some embodiments, the first pad 130 and the second pad 140 may be formed by an electroplating process. According to the difference in thickness T1 and T2 of the electroplated first pad 130 and the second pad 140, the first width W1 of the first opening 132 of the first pad 130 and the second width W2 of the second opening 142 of the second pad 140 may be adjusted to be different.

[0042] In the case where the thickness T1 of the first pad 130 is less than the thickness T2 of the second pad 140, the first nanowire 112 and the second nanowire 114 can be pressed down into the first recess 130R and the second recess 140R to be bonded with the first pad 130 and the second pad 140. After bonding, for the first pad 130 with a smaller thickness T1, a portion of the surface of the first recess 130R can be separated from the plurality of first nanowires 112 by the gap GP, but since the portion of the first nanowire 112 located in the first recess 130R can be connected to the first pad 130, better electrical performance is also provided for the lower first pad 130. Therefore, it is possible not to be limited by the coplanarity of the first pad 130 and the second pad 140. In some embodiments, the gap GP can be filled with a protective layer 290.

[0043] The bonding structure 100 may further include a first bonding layer 181 conformally located in the first recess 130R and a second bonding layer 182 conformally located in the second recess 140R. The first bonding layer 181 is in physical contact with the plurality of first nanowires 112. The second bonding layer 182 is in physical contact with the plurality of second nanowires 114. By providing the first bonding layer 181 and the second bonding layer 182, a stronger bonding strength can be provided between the first nanowire 112 and the first bonding layer 181, and between the second nanowire 114 and the second bonding layer 182, while having a larger contact area, and the depth of the first nanowire 112 and the second nanowire 114 being pressed down can also be larger.

[0044] A first bottom seed layer 191 may be further disposed between the first bonding layer 181 and the first pad 130, and a second bottom seed layer 192 may be further disposed between the second bonding layer 182 and the second pad 140. In some embodiments, the materials of the first bonding layer 181 and the second bonding layer 182 may be any one of Cu, Au, Ag, and Al, or any alloys thereof. In some embodiments, the materials of the first bottom seed layer 191 and the second bottom seed layer 192 may be any one of Cu, Au, Ag, Al, Pd, Pt, and Ni, or any alloys thereof.

[0045] After the first nanowire 112 contacts the first bonding layer 181, it can rotate along the surface of the first bonding layer 181, so that the first nanowires 112 contact each other in the first contact area 112c in the first recess 130R. Similarly, the second nanowires 114 contact each other in the second contact area 114c in the second recess 140R. Figure 3 In the cross-sectional view shown, the area of ​​the first contact region 112c may be smaller than the area of ​​the second contact region 114c. In another embodiment, in the vertical top view, the area of ​​the first contact region 112c may be smaller than the area of ​​the second contact region 114c.

[0046] The first contact region 112c may be separated from the first pad 130. Specifically, the first contact region 112c is separated from the first bonding layer 181 on the first pad 130 by a gap GP. The second contact region 114c may at least fill the bottom of the second recess 140R. Figure 4B As shown, in some other embodiments, the second contact region 114 c may also be separated from the second bonding layer 182 on the second pad 140 .

[0047] Figure 4A Shows Figure 3 A partial enlarged schematic diagram of the plurality of first nanowires 112 and the first pad 130 in FIG. Figure 4A As shown, the middle area of ​​the upper surface of the first contact area 112c may be lower than the edge area. In some embodiments, the thickness of the second bonding layer 182 may be in the range of 0.1 μm to 5 μm. In some embodiments, the angle θ1 between the side wall of the first recess 130R and the extension line of the bottom surface of the first recess 130R may be in the range of 3° to 85°. In some embodiments, the interval GB between the first pad 130 and the third pad 150 may be in the range of 1 μm to 20 μm.

[0048] Figure 4B Shows Figure 3 A local enlarged schematic diagram of the plurality of second nanowires 114 and the second pad 140 in FIG. Figure 4B As shown, the middle area of ​​the upper surface of the second contact area 114c may be lower than the edge area. In some embodiments, the thickness of the second bonding layer 182 may be in the range of 0.1 μm to 5 μm. In some embodiments, the depth VD of the second recess 140R may be in the range of 0.1 μm to 20 μm. In some embodiments, the angle θ2 between the side wall of the second recess 140R and the extension line of the bottom surface may be in the range of 3° to 85°.

[0049] Join reference Figure 4A and Figure 4BAs shown, the plurality of first nanowires 112 include a portion that is not in contact with each other, that is, a portion of the first nanowire 112 above the first contact region 112c, and a first nanowire (such as the first nanowire 112a) in the portion that is not in contact with each other may have a first length L1. The region of the plurality of first nanowires 112 above the first contact region 112c that is not in contact with each other may be referred to as a spacing region of the plurality of first nanowires 112. The plurality of second nanowires 114 also include a portion that is not in contact with each other, that is, a portion of the second nanowire 114 above the second contact region 114c, and a second nanowire (such as the second nanowire 114a) in the portion that is not in contact with each other may have a second length L2. In some embodiments, the first length L2 may be longer than the second length L1. This is because the thickness of the first pad 130 is less than that of the second pad 140, so that the depth of the plurality of first nanowires 112 entering the first recess 130R is smaller, so the length of the portion of the first nanowire 112 that is not in contact with each other is longer.

[0050] Figure 4C FIG. 1 is a partial enlarged schematic diagram of two second nanowires 114 bonded to the second bonding layer 182 according to an embodiment of the present application. Figure 4C As shown, when the second nanowire (such as Figure 4C After the two second nanowires 114a and 114b shown in FIG. 1 contact the second bonding layer 182, they rotate and slide along the side of the second bonding layer 182, so that the second nanowires 114a and 114b may have a fold angle, for example, the second nanowire 114a located on the outside has a first fold angle β1, and the next second nanowire 114b to the inside has a second fold angle β2. The second nanowire 114a specifically includes a portion 114a1 that contacts the second nanowire 114b, and a portion 114a2 that is spaced apart from the second nanowire 114b, and the first fold angle β1 is defined by the portion 114a1 and the portion 114a2. The second nanowire 114b specifically includes a portion 114b1 that contacts the second nanowire 114a, and a portion 114b2 that is spaced apart from the second nanowire 114a, and the second fold angle β2 is defined by the portion 114b1 and the portion 114b2. In some embodiments, the fold angle of the second fold angle β2 is different from the first fold angle β1. In some embodiments, the first bending angle β1 of the second nanowire 114 a located on the outside may be greater than the second bending angle β2 of the second nanowire 114 b located on the inside.

[0051] Refer to Figure 3 , and the above reference Figure 4CSimilar to the description, after the first nanowire 112 contacts the first bonding layer 181, it rotates and slides along the surface of the first bonding layer 181, so that the first nanowire 112 among the plurality of first nanowires 112 may have a fold angle defined by a portion contacting each other in the first contact region 112c and a portion spaced apart from each other in the spacer region (the region above the first contact region 112c). In some embodiments, the first fold angle of one first nanowire 112 among the plurality of first nanowires 112 may be different from the second fold angle of another first nanowire 112.

[0052] The embodiments of the present application also provide a method for forming Figure 3 A method of joining structure 100 is shown. FIG. 5A to FIG. 5S is formed Figure 3 The cross-sectional views of the bonding structure 100 are schematically shown at various stages.

[0053] refer to Figure 5A As shown, a top device 1200 (such as a chip or a wafer, etc.) is provided, and the third pad 150 and the fourth pad 160 mentioned above are bonded to the top device 1200. In some embodiments, the third pad 150 and the fourth pad 160 can be formed by any one of PVD (Physical Vapor Deposition, physical vapor deposition), electroplating, chemical plating, printing and potting metal processes. The third pad 150 and the fourth pad 160 can also be called micro pads. Then refer to Figure 5B As shown, the top seed layer 202 conformally covers the top device 1200, the third pad 150 and the fourth pad 160. In some embodiments, the top seed layer 202 can be formed by any one of PVD, electroplating, chemical plating, printing and potting metal processes.

[0054] refer to Figure 5C As shown, a photoresist layer 501 is laminated on the top seed layer 202, and a photolithography process is performed on the photoresist layer 501. Through the photolithography process, an opening 512 exposing the third pad 150 and the fourth pad 160 can be formed in the photoresist layer 501, as shown in FIG. Figure 5D A metal material is formed in the opening 512 to form a first metal column 112' and a second metal column 114' (also referred to as a metal bump) on the third pad 150 and the fourth pad 160, respectively. In some embodiments, the first metal column 112' and the second metal column 114' can be formed by any one of PVD, electroplating, chemical plating, printing, and potting metal processes.

[0055] Then remove the photoresist layer 501, refer to Figure 5EAs shown, the exposed top seed layer 202 is subjected to an etching process 531. The etching process 531 can remove the top seed layer 202 outside the area below the first metal column 112' and the second metal column 114', that is, only the top seed layer 202 below the first metal column 112' and the second metal column 114' is retained. Fig. 5F As shown. Then, the first metal column 112' and the second metal column 114' are subjected to an etching process 531. After the etching process 531, as shown Figure 5G As shown, a plurality of first nanowires 112 are formed on the top seed layer 202 on the third pad 150, and a plurality of second nanowires 114 are formed on the top seed layer 202 on the fourth pad 160. Thus, by referring to the above FIG. 5A to FIG. 5G The described process forms a first intermediate structure 551 including a plurality of first nanowires 112 and second nanowires 114 connected to third and fourth pads 150 and 160, respectively.

[0056] Then refer to Figure 5H As shown, a bottom device 1100 (such as a substrate or a wafer) is provided, and a first pad 130 and a second pad 140 having different thicknesses are bonded to the bottom device 1100, wherein the thickness of the first pad 130 is less than that of the second pad 140. In some embodiments, the first pad 130 and the second pad 140 can be formed by any one of PVD, electroplating, chemical plating, printing, and potting metal processes. Fig.5I As shown, a photoresist layer 502 is laminated on the bottom device 1100, the first pad 130 and the second pad 140, and then a photolithography process is performed on the photoresist layer 502. Figure 5J As shown, an opening 514 exposing the first pad 130 and the second pad 140 is formed in the photoresist layer 502 by a photolithography process. An etching process 532 is performed on the first pad 130 and the second pad 140 through the opening 514.

[0057] The first and second recesses 130R and 140R are formed in the first and second pads 130 and 140 by etching process 532. Figure 5K As shown. Afterwards, the bottom seed layer 190 is conformally covered on the bottom device 1100, the first pad 130 and the second pad 140. In some embodiments, the bottom seed layer 190 can be formed by any one of PVD, electroplating, chemical plating, printing and encapsulation metal processes. Figure 5L As shown, a photoresist layer 503 is laminated on the bottom seed layer 190 and a photolithography process is performed on the photoresist layer 503 .

[0058] refer to Figure 5MAs shown, an opening 516 exposing the first recess 130R and the second recess 140R may be formed in the photoresist layer 503 through a photolithography process. Furthermore, the first bonding layer 181 and the second bonding layer 182 are conformally formed in the first recess 130R and the second recess 140R through the opening 516. In some embodiments, the first bonding layer 181 and the second bonding layer 182 may be formed by any one of PVD, electroplating, chemical plating, printing, and potting metal processes.

[0059] Then remove the photoresist layer 503, as Figure 5N Subsequently, the bottom seed layer 190 exposed by the first bonding layer 181 and the second bonding layer 182 is removed by, for example, an etching process 533, and only the bottom seed layer 190 below the first bonding layer 181 and the second bonding layer 182 is retained, as shown in FIG. Fig.5O As shown, a first bottom seed layer 191 located below the first bonding layer 181 and a second bottom seed layer 192 located below the second bonding layer 182 are formed. FIG. 5H to FIG. 5O The described process forms the second intermediate structure 552 including the first pad 130 with the first recess 130R and the second pad 140 with the second recess 140R. It should be understood that the first intermediate structure 551 may also be formed after the second intermediate structure 552 is formed.

[0060] Later reference Figure 5P As shown, provide Figure 5G The first intermediate structure 551 formed at Fig.5O A second intermediate structure 552 is formed at the position where the first pad 130 is placed under the first nanowire 112 and the second pad 140 is placed under the second nanowire 114.

[0061] Press the first intermediate structure 551 downward toward the second intermediate structure 552, referring to Figure 5Q As shown, the plurality of first nanowires 112 and the plurality of second nanowires 114 enter the first recess 130R and the second recess 140R, respectively. Then, a heating process may be performed, through which the first nanowires 112 and the first bonding layer 181 may be sintered together, and the second nanowires 114 and the second bonding layer 182 may be sintered together. Furthermore, the plurality of first nanowires 112 may be brought into contact with each other at the first contact region 112c, and the plurality of second nanowires 114 may be brought into contact with each other at the second contact region 114c. After the heating process, the bonding structure 100 is formed. Then, refer to Figure 5R As shown, a bottom filling material 290' is filled between the bottom device 1100 and the top device 1200 to form a protection layer 290, such as Figure 5SThe protection layer 290 may fill the gap between the bottom device 1100 and the top device 1200 .

[0062] Figures 6 to 11 Each of them is a schematic cross-sectional view of a bonding structure according to another embodiment of the present application. Figures 6 to 11 Many aspects of the illustrated embodiments can be compared with those described above. Figure 3 The same or similar as described above, so for the sake of brevity, only Figures 6 to 11 The differences between the embodiments shown.

[0063] refer to Figure 6 As shown, Figure 3 The plurality of first nanowires 112 shown are different from a single bundle of nanowires. Figure 6 In the illustrated bonding structure 200, the plurality of first nanowires 112 may include a plurality of bundles of first nanowires 112. Figure 6 1 and 130R. Two bundles of first nanowires 112G1 and 112G2 are shown. Each bundle of first nanowires 112G1 and 112G2 may include any number of multiple first nanowires 112. There may be a gap GS between the two bundles of first nanowires 112G1 and 112G2. The two bundles of first nanowires 112G1 and 112G2 may contact their respective first contact regions 112c1 and 112c2, respectively, and each first contact region 112c1 and 112c2 may be in physical contact with the first bonding layer 181. The first contact regions 112c1 and 112c2 may not contact each other in the first recess 130R, or may contact each other.

[0064] 7A to 7C Many aspects of the embodiments shown may be the same, and for the sake of simplicity, only the following description will be given. 7A to 7C The differences between the embodiments shown. Fig. 7A As shown, in the bonding structure 300A, the same third pad 150 may be connected to a plurality of first nanowire bundles 112, and a plurality of first pads 130 may be provided respectively under each first nanowire bundle 112. Fig. 7A In the embodiment, two bundles of first nanowires 112 are connected to the same third pad 150, and two first pads 130 are respectively located under the two bundles of first nanowires 112. The two first pads 130 are used to bond the two bundles of first nanowires 112, respectively.

[0065] refer to Figure 7BAs shown, in the bonding structure 300B, each bundle of first nanowires 112 is connected to two different, separate third pads 150. And in this embodiment, the two bundles of first nanowires 112 are located above the same first pad 130. The first pad 130 has two separate first recesses 130R. The two first recesses 130R are respectively located under the two bundles of first nanowires 112, and are used to accommodate the two bundles of first nanowires 112, respectively.

[0066] refer to Figure 7C As shown, in the bonding structure 300C, two bundles of first nanowires 112 are connected to the same third pad 150, and the two bundles of first nanowires 112 are located above the same first pad 130. The first pad 130 has two separate first recesses 130R. The two first recesses 130R are respectively located below the two bundles of first nanowires 112 and are used to accommodate the two bundles of first nanowires 112.

[0067] refer to Figure 8 As shown, the bonding structure 400 may include a first conductive pillar 412 connected between the plurality of first nanowires 112 and the third pad 150, and a second conductive pillar 414 connected between the plurality of second nanowires 114 and the fourth pad 160. In some embodiments, the thickness of the first conductive pillar 412 and the second conductive pillar 414 may be the same. More specifically, a top seed layer 204 may be disposed between the first conductive pillar 412 and the third pad 150, and between the second conductive pillar 414 and the fourth pad 160. A top seed layer 206 may be disposed between the first conductive pillar 412 and the plurality of first nanowires 112, and between the second conductive pillar 414 and the plurality of second nanowires 114.

[0068] Fig. 9 yes Figure 8 Another embodiment of the first recess 130R in the joint structure 400 is shown. Fig. 9 , which shows a first recess 130R' having a curved cross-section. The first bonding layer 181 is conformally located in the first recess 130R', and thus the first bonding layer 181' located in the first recess 130R' also has a curved surface. In some embodiments, the plurality of first nanowires 112 may all be in physical contact with the first bonding layer 181, that is, there is no spacing between the plurality of first nanowires 112 and the first bonding layer 181. In some embodiments, the second recess 140R (e.g., see Figure 3 ) can also have a curved cross-section.

[0069] refer to Fig.10As shown, the first pad 130 and the second pad 140 may be embedded in the bottom device 1100 (for example, it may be a substrate). The top surfaces of the first pad 130 and the second pad 140 may be flush with each other and may be flush with the surface of the bottom device 1100. In this embodiment, the plurality of first nanowires 112 and the plurality of second nanowires 114 may enter the first recess 130R and the second recess 140R to substantially the same depth. The first contact region 112c of the plurality of first nanowires 112 and the second contact region 114c of the plurality of second nanowires 114 may be spaced apart from the bottom surfaces of the first recess 130R and the second recess 140R, respectively. The areas of the first contact region 112c and the second contact region 114c may be substantially the same.

[0070] refer to Fig.11 As shown, different from Figure 3 The first pad 130 and the second pad 140 are shown as rectangular shapes, but the first pad 130 ′ and the second pad 140 ′ may have non-rectangular shapes. Specifically, the sidewalls of the first pad 130 and the second pad 140 are convex curved surfaces.

[0071] Fig. 12A It is a cross-sectional schematic diagram when a plurality of first nanowires 112 and second nanowires 114 are placed upward. FIG. 12B to FIG. 12F According to different embodiments Figure 2A The top view diagram is shown in the top view perspective. FIG. 12B to FIG. 12F As shown, the region where the plurality of first nanowires 112 and / or the plurality of second nanowires 114 are located may have a variety of applicable top-view shapes. Fig. 12B As shown, the top view shape of the region where the plurality of first nanowires 112 and / or the plurality of second nanowires 114 are located may be a square, and in this embodiment, the top view shape of the third pad 150 and / or the fourth pad 160 may be a square. Fig. 12C As shown, the top view shape of the region where the plurality of first nanowires 112 and / or the plurality of second nanowires 114 are located may be circular, and in this embodiment, the top view shape of the third pad 150 and / or the fourth pad 160 may be circular. For another example, the top view shape of the region where the plurality of first nanowires 112 and / or the plurality of second nanowires 114 are located, and the third pad 150 and / or the fourth pad 160 may also be polygonal (e.g. Fig.12D pentagons as shown), irregular shapes (such as Fig.12E ), rectangle (such as Fig.12F )wait.

[0072] The above description is only a preferred embodiment of the present application and is not intended to limit the present application. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present application should be included in the protection scope of the present application.

Claims

1. A joining structure, characterized in that: include: a plurality of first conductive lines; A first pad, located below the plurality of first conductive lines, and comprising a first recess for accommodating the plurality of first conductive lines, wherein the first recess comprises a first opening having a first width in a horizontal direction; a plurality of second conductive lines horizontally overlapping the plurality of first conductive lines; A second pad is located below the plurality of second conductive lines and includes a second recess for accommodating the plurality of second conductive lines, wherein the second recess includes a second opening having a second width in a horizontal direction; The first width is different from the second width.

2. The joining structure according to claim 1, characterized in that: A thickness of the first pad in a vertical direction is smaller than a thickness of the second pad, and the first width is smaller than the second width.

3. The joining structure according to claim 2, characterized in that: The multiple first conductive wires contact each other at a first contact area in the first recess, and the multiple second conductive wires contact each other at a second contact area in the second recess. In a vertical cross-sectional perspective or a top view, an area of ​​the first contact area is smaller than an area of ​​the second contact area.

4. The joining structure according to claim 2, characterized in that: The plurality of first conductive lines include a portion that is not in contact with each other, one of the plurality of the portions of the plurality of first conductive lines has a first length, the plurality of second conductive lines include a portion that is not in contact with each other, one of the plurality of the portions of the plurality of second conductive lines has a second length, and the first length is longer than the second length.

5. The joining structure according to claim 1, characterized in that: A portion of the surface of the first recess is spaced apart from the plurality of first conductive lines.

6. The joining structure according to claim 1, characterized in that: One of the plurality of first conductive lines has a first fold angle.

7. The joining structure according to claim 1, characterized in that: At least two first conductive lines among the plurality of first conductive lines include different bend angles from each other.

8. A joining structure, characterized in that: include: a plurality of first conductive lines; A first pad is located below the plurality of first conductive lines and has a first top surface facing the plurality of first conductive lines, wherein the first top surface has a first recess for accommodating the plurality of first conductive lines; a plurality of second conductive lines horizontally overlapping the plurality of first conductive lines; A second pad is located below the plurality of second conductive lines and has a second top surface facing the plurality of second conductive lines, wherein the second top surface has a second recess for accommodating the plurality of second conductive lines; The first top surface is not flush with the second top surface, and the bottom of the first recess is not flush with the bottom of the second recess.

9. The joining structure according to claim 8, characterized in that: The first recess includes a first opening having a first width, and the second recess includes a second opening having a second width, wherein the first width is smaller than the second width, and the second top surface is higher than the first top surface.

10. The joining structure according to claim 8, characterized in that: The first conductive lines contact each other at a first contact region in the first recess, and the second conductive lines contact each other at a second contact region in the second recess. The thickness of the first contact region is smaller than that of the second contact region.