Double seal of indissolvable metal composite plate chemical container
By adding a sealing cover plate and a leakage hole to the double-pass sealing structure of the chemical container, the risk of corrosive medium penetration under the single-pass sealing structure is solved, the safety and service life of the container are improved, and timely detection of corrosion is ensured. Handling and Safeguarding.
Patent Information
- Application Number
- CN202420546392.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-20
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2034-03-20
AI Technical Summary
The single-channel sealing structure of existing refractory metal composite plate chemical containers can easily cause corrosive media to penetrate the corrosion-resistant cladding to the non-corrosion-resistant base layer under extreme conditions, leading to the risk of equipment failure accidents.
Adopting a double-channel sealing structure, a sealing cover is added between the cladding plate and the cover plate to form a sealed cavity, and leakage holes are set on the backing plate and cover plate to detect and handle in time when corrosive media penetrates. .
It improves the safety and service life of chemical containers and ensures timely detection and treatment when corrosive media penetrates, thereby reducing the probability of safety accidents and ensuring equipment and personal safety.
Smart Images

Figure CN221824784U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of chemical containers, in particular to a double-pass seal of a chemical container made of a refractory metal composite plate. Background Art
[0002] The double-pass seal of the chemical container with refractory metal composite plate refers to setting up a two-layer sealing structure on the container cover to ensure that the medium inside the container can maintain a high degree of sealing performance under extreme working conditions. This design is usually used in occasions requiring high safety and high reliability.
[0003] Refractory metals such as zirconium and titanium have excellent corrosion resistance and are often used to make various chemical containers, but they are expensive and have low strength. In order to reduce investment costs, an economical composite plate structure is often used, and the corrosion-resistant composite layer is made of zirconium, titanium and other materials, while the strength-bearing base layer is made of cheap iron-based materials. Due to the difference between the two materials, the material between the composite layer and the base layer cannot be melt-welded, so in local areas such as longitudinal and circumferential welds, a special loose lining structure is required to form a complete corrosion-resistant protective layer. Therefore, the present application proposes a double-pass seal for a refractory metal composite plate chemical container to solve the above technical problems. Summary of the invention
[0004] 1. Technical issues to be resolved
[0005] In view of the shortcomings of the prior art, the utility model provides a double-pass seal for a chemical container made of a refractory metal composite plate, which has the advantages of improving safety of use, etc., and solves the problem that the prior art uses a single-pass seal. If there are deficiencies in materials and welding, the corrosive medium in the chemical container can easily penetrate the corrosion-resistant composite layer to the non-corrosion-resistant base layer, thereby causing equipment failure accidents.
[0006] In order to achieve the above-mentioned purpose of improving the safety of use, the utility model provides the following technical solutions: a double-channel seal of a chemical container of a refractory metal composite plate, comprising a first pipeline and a second pipeline, the outer sides of the first pipeline and the second pipeline are both fixedly installed with a composite plate, and the outer side of the composite plate is fixedly installed with a sealing cover plate;
[0007] A cover plate is fixedly installed on the outer side of the sealing cover plate, and a number of gasket leak indication holes are arranged on the first pipeline and the second pipeline, and a number of cover leak indication holes are arranged on the first pipeline and the second pipeline.
[0008] Preferably, the composite plate is welded to the outside of the first pipe or the second pipe by silver brazing.
[0009] Preferably, a closed cavity is formed between the composite plate and the sealing cover plate.
[0010] Preferably, a closed cavity is formed between the cover plate and the sealing cover plate.
[0011] Preferably, one end of the leakage hole of the pad is in contact with the inner wall of the composite plate.
[0012] Preferably, one end of the cover plate leak hole is in contact with the inner side wall of the sealing cover plate.
[0013] Compared with the prior art, the utility model provides a double-pass seal for a chemical container made of a refractory metal composite plate, which has the following beneficial effects:
[0014] The double-pass seal of the chemical container made of refractory metal composite plate can form a sealed cavity by adding a sealing cover plate between the composite plate and the cover plate, so that when the corrosive medium in the chemical container penetrates the corrosion-resistant composite plate, it can be blocked by the sealing cover plate, ensuring that the chemical container can still operate safely for a period of time, and through the gasket plate leak indication hole and the cover plate leak indication hole, when the layered plate is penetrated by the corrosive medium in the chemical container, it can be detected in time, so that there is time to deal with the chemical container, thereby improving the safety of the equipment and ensuring the personal safety of the staff. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic diagram of the overall structure of the utility model;
[0016] Figure 2 It is a partial cross-sectional schematic diagram of the utility model;
[0017] Figure 3 It is a schematic diagram of a partially enlarged structure of the utility model.
[0018] In the figure: 1. first pipeline; 2. second pipeline; 3. composite plate; 4. sealing cover plate; 5. cover plate; 6. gasket plate indicating leakage hole; 7. cover plate indicating leakage hole. DETAILED DESCRIPTION
[0019] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0020] See also Figure 1-3The double-channel seal of the refractory metal composite plate chemical container includes a first pipeline 1 and a second pipeline 2. The first pipeline 1 and the second pipeline 2 are both fixedly installed on the outside of the chemical container. A composite plate 3 is fixedly installed on the outside of the first pipeline 1 and the second pipeline 2. The composite plate 3 is welded to the outside of the first pipeline 1 or the second pipeline 2 by silver brazing. A sealing cover plate 4 is fixedly installed on the outside of the composite plate 3, and a closed cavity is formed between the composite plate 3 and the sealing cover plate 4.
[0021] A cover plate 5 is fixedly installed on the outside of the sealing cover plate 4, and a closed cavity is formed between the cover plate 5 and the sealing cover plate 4. A number of gasket leak holes 6 are provided on the first pipeline 1 and the second pipeline 2, and one end of the gasket leak hole 6 is in contact with the inner wall of the composite plate 3. When the composite plate 3 fails, the staff can take action in time, thereby reducing the probability of safety accidents and improving the safety of the equipment. A number of cover leak holes 7 are provided on the first pipeline 1 and the second pipeline 2, and one end of the cover leak hole 7 is in contact with the inner wall of the sealing cover plate 4. When the sealing cover plate 4 fails, the staff can take action in time, thereby reducing the probability of safety accidents and improving the safety of the equipment.
[0022] In summary, the double-pass sealing of the chemical container made of refractory metal composite plate can form a sealed cavity by adding a sealing cover plate 4 between the composite plate 3 and the cover plate 5, so that when the corrosive medium in the chemical container penetrates the corrosion-resistant composite plate 3, it will be blocked by the sealing cover plate 4, ensuring that the chemical container can still operate safely for a period of time, and through the gasket leak hole 6 and the cover plate leak hole 7, when the layered plate is penetrated by the corrosive medium in the chemical container, it can be timely detected, so that there is time to deal with the chemical container, thereby improving the safety of the equipment and ensuring the personal safety of the staff.
[0023] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.
[0024] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A double-channel seal for a chemical container made of a refractory metal composite plate, comprising a first pipeline (1) and a second pipeline (2), characterized in that: A composite plate (3) is fixedly mounted on the outer sides of the first pipe (1) and the second pipe (2), and a sealing cover plate (4) is fixedly mounted on the outer sides of the composite plate (3); A cover plate (5) is fixedly mounted on the outer side of the sealing cover plate (4); a number of gasket plate leak indication holes (6) are provided on the first pipe (1) and the second pipe (2); and a number of cover plate leak indication holes (7) are provided on the first pipe (1) and the second pipe (2).
2. The double-pass seal of the refractory metal composite plate chemical container according to claim 1 is characterized by: The composite plate (3) is welded to the outside of the first pipe (1) or the second pipe (2) by silver brazing.
3. The double-pass seal of the refractory metal composite plate chemical container according to claim 1 is characterized by: A closed cavity is formed between the composite plate (3) and the sealing cover plate (4).
4. The double-pass seal of the refractory metal composite plate chemical container according to claim 1 is characterized by: A closed cavity is formed between the cover plate (5) and the sealing cover plate (4).
5. The double-pass seal of the refractory metal composite plate chemical container according to claim 1 is characterized by: One end of the gasket plate leak hole (6) contacts the inner side wall of the composite plate (3).
6. The double-pass seal of the refractory metal composite plate chemical container according to claim 1 is characterized by: One end of the cover plate leak hole (7) contacts the inner side wall of the sealing cover plate (4).