Die for preventing sampling shrinkage cavity defect in spheroidal graphite casting molten iron component detection
By adopting the pouring riser feeding principle and the mold designed with copper material, the problems of shrinkage, shrinkage holes and graphitization aggregation of the ductile casting testing samples are solved, and more accurate detection and rapid cooling of the finished molten iron composition are achieved.
Patent Information
- Application Number
- CN202420447368.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-08
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-03-08
AI Technical Summary
The molten iron component testing samples of finished ductile graphite castings have defects such as shrinkage, shrinkage holes and surface graphitization accumulation, resulting in inaccurate testing of finished products.
The mold is designed using the pouring riser feeding principle, combined with copper material with excellent thermal conductivity, and connected to the sample cooling chamber through the feeding riser and feeding channel to achieve rapid cooling and prevent graphitization aggregation.
It effectively reduces the shrinkage and cavity problems of the test sample, improves the accuracy and cooling speed of the component detection of finished molten iron, and avoids detection deviations.
Smart Images

Figure CN221909700U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of casting, in particular to a mould for preventing shrinkage defects in molten iron component detection and sampling of ductile iron castings. Background Art
[0002] The finished molten iron composition test sample of ductile iron castings is formed by scooping molten iron from a spheroidizing ladle and pouring it into a brass or graphite mold to cool it. After the molten iron is cooled, the mold is pried open and samples are taken for inspection. However, the test samples obtained from traditional molds have shrinkage and shrinkage defects and surface graphitization aggregation. The above problems are the main reasons for the inaccuracy of the finished molten iron composition detection. Therefore, the inventors have developed a finished molten iron composition detection sampling mold made using the pouring riser shrinkage compensation principle to reduce the shrinkage and shrinkage problems of the test sample, and use copper with better thermal conductivity as the manufacturing material to increase the cooling rate and solve the problem of graphitization aggregation on the sample surface, ultimately making the finished molten iron composition detection of ductile castings more accurate. Utility Model Content
[0003] The utility model aims to provide a mold for preventing shrinkage defects in ductile iron castings during molten iron composition detection sampling, thereby greatly reducing the shrinkage, shrinkage and other defects of ductile iron castings that occur when preparing finished molten iron composition detection samples, and avoiding deviation in molten iron composition detection.
[0004] In order to achieve the above purpose, the utility model adopts the following technical solutions:
[0005] A mold for preventing shrinkage defects in sampling of molten iron composition detection of ductile iron castings, the mold is formed by butting and buckling two symmetrical structures, the butt-jointed mold comprises a feeding riser, a feeding channel, a sample cooling chamber, and a mold body, a sample cooling chamber is arranged at the center of the mold body, a feeding channel and a feeding riser are arranged in sequence on one side of the sample cooling chamber, the sample cooling chamber is connected to the outside of the mold body through the feeding channel and the feeding riser, the feeding riser is a funnel shape with a large outside and a small inside, and the feeding channel is a straight hole with the same minimum diameter as the feeding riser.
[0006] The outer wall of the mold body on the side opposite to the feeding riser is a plane.
[0007] The thickness of one monomer structure of the symmetrical structure is 35-55 mm.
[0008] The material of the mold body is copper.
[0009] The feeding channel has a diameter of 8 to 16 mm and a height of 4 to 10 mm.
[0010] The sample cooling chamber has a height of 7 to 20 mm and a shape of a circle with a diameter of 10 to 30 mm or a square with a side length of 10 to 30 mm.
[0011] The maximum diameter of the feeding riser is 20-60 mm, and the height of the feeding riser is 15-18 mm.
[0012] Compared with the prior art, the beneficial effects of the utility model are:
[0013] The utility model utilizes the pouring riser shrinkage compensation principle to manufacture a finished product molten iron composition detection sampling mold to reduce the shrinkage and shrinkage cavity problems of the detection sample, and uses copper with better thermal conductivity as a manufacturing material to increase the cooling speed and solve the graphitization aggregation problem on the sample surface, ultimately making the ductile iron composition detection of the finished product molten iron more accurate. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a three-dimensional schematic diagram of a single structure in the symmetrical structure of the sampling mold of the utility model.
[0015] Figure 2 It is a cross-sectional view of a single structure in the symmetrical structure of the sampling mold of the utility model.
[0016] In the figure: 1--die body, 2--feeding riser, 3--feeding channel, 4--sample cooling chamber. DETAILED DESCRIPTION
[0017] The following is a further description of the embodiments of the present invention in conjunction with the accompanying drawings:
[0018] See Figure 1 , Figure 2 A mold for preventing shrinkage defects in sampling of molten iron composition detection of ductile iron castings, wherein the mold is formed by butting and buckling two symmetrical structures, and the butt-jointed mold includes a feeding riser 2, a feeding channel 3, a sample cooling chamber 4, and a mold body 1. A sample cooling chamber 4 is arranged at the center of the mold body 1, and a feeding channel 3 and a feeding riser 2 are arranged in sequence on one side of the sample cooling chamber 4. The sample cooling chamber 4 is connected to the outside of the mold body 1 through the feeding channel 3 and the feeding riser 2. The feeding riser 2 is a funnel shape with a large outside and a small inside, and the feeding channel 3 is a straight hole with the same minimum diameter as the feeding riser 2.
[0019] The outer wall of the mold body 1 on the side opposite to the feeding riser 2 is a plane.
[0020] The thickness of one monomer structure of the symmetrical structure is H=35-55 mm, which can ensure the rapid and extreme cooling effect of the molten iron.
[0021] The mold body 1 is made of copper.
[0022] The radius E of the feeding channel 3 is 4-8 mm, the diameter is 8-16 mm, and the height is C=4-10 mm, so as to ensure that the sample cooling chamber 4 is quickly filled with molten iron after being poured in.
[0023] The height of the sample cooling chamber 4 is D=7-20 mm, and the shape is circular with a diameter of 10-30 mm or square with a side length of 10-30 mm, to ensure that the test sample has sufficient grinding removal. The diameter or side length of the sample cooling chamber 4 can be adjusted accordingly according to the size of the sample carrier platform of the spectrometer.
[0024] The maximum diameter of the feeding riser 2 is 20-60 mm (i.e., the mold pouring port), and the height of the feeding riser is 15-18 mm, which can effectively replenish the molten iron in the sample cooling chamber 4 and prevent shrinkage and shrinkage cavities.
[0025] Embodiment 1:
[0026] The processing dimensions of the embodiment mold are as follows: the thickness of the mold body 1 is H=50mm; the height of the feeding channel 3 is C=8mm and the radius is E=6mm; the sample cooling chamber 4 is a round shape with a thickness of D=10mm and a diameter of 20mm; after the mold is combined, the maximum diameter of the feeding riser 2 (i.e., the mold pouring port) is 30mm and the height is 16mm. The production and use methods are as follows:
[0027] 1) Use copper rods as the base material and process and saw according to the sample drawing;
[0028] 2) Drill a hole on the surface of the sawn bar, the hole depth is to the center of the bar, and then turn a "funnel-shaped" radial from the large diameter to the small diameter from the surface of the bar with the drilled hole as the center as the feeding riser 2. The minimum diameter of the feeding riser 2 is the same as the drilled hole;
[0029] 3) Mill a plane on the opposite side of the rod hole to serve as the sampling mold placement plane;
[0030] 4) Sawing along the center axis of the drill hole and perpendicular to the center axis of the bar to saw the processed bar into two parts;
[0031] 5) Milling a circular groove on the cross section of the sawn bar, and the milled circular groove is connected to the initial drilled hole;
[0032] 6) When in use, the two sampling molds after processing are relatively merged, the round grooves are combined with the round grooves to form a sample cooling chamber 4, the half holes are combined with the half holes to form a feeding channel 3, and the half "funnel riser" is combined with the half "funnel riser" to form a feeding riser 2. After the merging is completed, the molten iron can be poured into the funnel, and samples can be taken for testing after the molten iron has cooled.
Claims
1. A mold for preventing shrinkage defects in ductile iron casting molten iron composition detection sampling, characterized in that: The mold is formed by butting and buckling two symmetrical structures, and the butt-jointed mold includes a feeding riser, a feeding channel, a sample cooling chamber, and a mold body. The sample cooling chamber is arranged at the central part of the mold body, and a feeding channel and a feeding riser are arranged in sequence on one side of the sample cooling chamber. The sample cooling chamber is connected to the outside of the mold body through the feeding channel and the feeding riser. The feeding riser is a funnel shape with a larger outside and a smaller inside, and the feeding channel is a straight hole with the same minimum diameter as the feeding riser.
2. A mold for preventing shrinkage defects in molten iron composition detection sampling of ductile iron castings according to claim 1, characterized in that: The outer wall of the mold body on the side opposite to the feeding riser is a plane.
3. A mold for preventing shrinkage defects in molten iron composition detection sampling of ductile iron castings according to claim 1, characterized in that: The thickness of one monomer structure of the symmetrical structure is 35-55 mm.
4. A mold for preventing shrinkage defects in ductile iron casting molten iron composition detection sampling according to claim 1, characterized in that: The material of the mold body is copper.
5. A mold for preventing shrinkage defects in molten iron composition detection sampling of ductile iron castings according to claim 1, characterized in that: The feeding channel has a diameter of 8 to 16 mm and a height of 4 to 10 mm.
6. A mold for preventing shrinkage defects in molten iron composition detection sampling of ductile iron castings according to claim 1, characterized in that: The sample cooling chamber has a height of 7 to 20 mm and a shape of a circle with a diameter of 10 to 30 mm or a square with a side length of 10 to 30 mm.
7. A mold for preventing shrinkage defects in molten iron composition detection sampling of ductile iron castings according to any one of claims 1 to 6, characterized in that: The maximum diameter of the feeding riser is 20-60 mm, and the height of the feeding riser is 15-18 mm.