Sodium-ion battery electrode current collector with good adhesion and binding force

By forming an etched structure layer on the surface of aluminum foil, the problems of sagging and peeling during the coating process of sodium-ion battery cathode materials are solved, achieving the effects of high adhesion, low cost and simplified process.

CN221928138UActive Publication Date: 2024-10-29SHENZHEN JANAENERGY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323454201.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-19
Publication Date
2024-10-29
Estimated Expiration
2033-12-19

AI Technical Summary

Technical Problem

Sodium-ion battery cathode materials suffer from sagging and film detachment during coating. Existing methods, such as cleaning foil and carbon-coated foil, have problems with low film peel strength and high cost.

Method used

A 0.5-3μm thick corrosion structure layer is formed on the surface of aluminum foil. Irregular uneven texture structure is formed by corrosion with dilute sulfuric acid, dilute hydrochloric acid, carbonic acid or citric acid to increase the contact area between the active material and the current collector. Multi-level structure is formed by secondary or multiple acid corrosion.

Benefits of technology

It improves the adhesion of sodium-ion battery cathode materials, reduces production costs, simplifies process operations, and enhances electrode yield and electrode stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221928138U_ABST
    Figure CN221928138U_ABST
Patent Text Reader

Abstract

The utility model discloses a sodium ion battery electrode current collector with good adhesion and binding force, which comprises a current collector body, and a corrosion structure layer is arranged on one side or two sides of the current collector body; the thickness of the corrosion structure layer is 0.5-3 [mu] m; and the thickness of the current collector is 6-25 [mu] m. The sodium ion battery electrode current collector with good adhesion and binding force has the characteristics of strong adhesion capability, low cost and simple process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of sodium ion batteries, in particular to a sodium ion battery electrode current collector with good adhesion and bonding force. Background Art

[0002] The processing technology of sodium-ion batteries is basically the same as that of lithium-ion batteries. The positive electrode uses aluminum foil as the current collector. The aluminum foil is made by rolling aluminum ingots. During the rolling process, in order to make the aluminum foil and the roller press fall off smoothly, an oily substance needs to be added between the two. The oily substance is generally an organic fatty acid or fatty alcohol. The oily substance remains on the surface of the aluminum foil after rolling. In the coating process of the lithium battery positive electrode, aluminum foil with oily substances (that is, conventional plain foil) is used for coating, and the lithium battery raw materials can adhere well to the surface of the foil.

[0003] Specifically, when the raw materials for the positive electrode of sodium-ion batteries are coated with traditional plain foil, there is a "sagging" phenomenon during the coating process, that is, the slurry cannot adhere well to the surface of the foil and partially flows down from the foil before drying. Or, after normal coating, during the rolling stage, the membrane is very easy to fall off the current collector. Both of the above will cause the pole piece to be scrapped.

[0004] In the prior art, the main methods for solving the problems existing in the coating and rolling processes include: for example, cleaning the plain foil and removing the oily substances on the surface to obtain the cleaned foil, which can solve the above problems; for example, using carbon-coated aluminum foil, that is, pre-constructing a carbon layer on the surface of the plain foil, which can solve the above problems. However, the above methods all have the problem of low film peeling force. In addition, the cleaning process of the cleaned foil is not thorough, and it is impossible to achieve 100% cleaning, and the smooth surface cannot provide sufficient adhesion; the carbon-coated foil has a high price, which is 1.5 to 2 times that of ordinary plain foil. For the surface morphology of plain foil and carbon-coated foil, please refer to Figure 1-2 The SEM image shows that the cleaned foil is only degreased for the smooth foil, and its surface morphology is basically the same as that of the smooth foil. Utility Model Content

[0005] The utility model aims to provide a sodium ion battery electrode current collector with good adhesion and bonding force, which has the characteristics of strong adhesion, low cost and simple process.

[0006] The utility model can be realized by the following technical solutions:

[0007] The utility model discloses a sodium ion battery electrode current collector with good adhesion and bonding force, comprising a current collector body 1, one side or both sides of the current collector body 1 are provided with a corrosion structure layer 2.

[0008] Furthermore, the thickness of the corrosion structure layer is 0.5-3 μm, and the thickness of the current collector is 6-25 μm. The verified thickness of the corrosion structure layer is beneficial to processing control while ensuring the bonding force, and also avoids the waste of energy density due to excessive increase in the thickness of the current collector.

[0009] Furthermore, the current collector body is aluminum foil, and the aluminum foil is single-sided smooth aluminum foil or double-sided smooth aluminum foil, which is applicable to a variety of aluminum foils, effectively reducing the manufacturing cost of sodium ion batteries.

[0010] Furthermore, the corrosion structure layer is formed on the surface of the current collector body by one-piece corrosion using acid solution, which is simple to process and does not cause bonding problems between the corrosion structure layer and the current collector body.

[0011] Furthermore, the acid solution is dilute sulfuric acid, dilute hydrochloric acid, carbonic acid and / or citric acid, which has a wide source and a simple process.

[0012] Furthermore, an irregular concave-convex texture structure is formed on the surface of the corrosion structure layer, which effectively increases the contact surface area between the active material and the current collector and improves the bonding strength.

[0013] Furthermore, the corrosion structure layer is formed by two or more acid corrosions, and a second-order or multi-order structure is formed inside the corrosion structure layer, forming a richer surface texture and increasing the bonding depth and surface area.

[0014] Furthermore, the aperture gap of the second-order or multi-order structure inside the corrosion structure layer changes gradually from the inside to the outside, forming a multi-level, multi-angle and multi-dimensional combination to enhance the bonding strength.

[0015] Furthermore, the sodium ion battery includes a positive electrode material layer coated on a current collector, wherein the positive electrode material layer is a layered oxide material layer, a polyanion material layer or a Prussian blue material layer, which meets the use requirements of different types of sodium ion batteries.

[0016] Furthermore, the length of the positive electrode material layer is smaller than the length of the corrosion structure layer, and the width of the positive electrode material layer is smaller than the width of the corrosion structure layer, which effectively ensures that the positive electrode material layer is fully and effectively combined with the surface of the current collector.

[0017] The utility model discloses a sodium ion battery electrode current collector with good adhesion and bonding force, which has the following beneficial effects:

[0018] First, the adhesion ability is good. In the present invention, a structural corrosion layer is formed on the surface of the current collector body to form a rough texture on the surface. When the active material is coated on the surface, the rough texture increases the bonding contact surface between the active material and the current collector, thereby improving the adhesion.

[0019] Second, the cost is low. The current collector of the utility model only needs to form a corrosion structure layer on the current collector body to ensure the binding force of the active material layer, and no carbon coating is required, which effectively reduces its manufacturing and processing costs;

[0020] Third, the process is simple. The structural corrosion layer on the surface of the current collector body of the utility model is directly formed by corrosion. During use, there is no need to use complex oil removal operations to meet the bonding requirements, which effectively simplifies the process operation process. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is the SEM image of the prior art aluminum foil (magnification is 30,000 times);

[0022] Figure 2 This is a SEM image of the existing carbon-coated foil (magnification is 30,000 times);

[0023] Figure 3 This is a SEM image (magnification is 30,000 times) of a sodium ion battery electrode current collector (corrosion foil) with good adhesion and bonding force in the utility model;

[0024] Figure 4 This is a schematic structural diagram of a sodium ion battery electrode current collector with good adhesion and bonding strength provided with a corrosion structure layer on one side of the utility model;

[0025] Figure 5 This is a schematic structural diagram of a sodium ion battery electrode current collector with good adhesion and bonding strength provided with corrosion structure layers on both sides of the utility model;

[0026] Figure 6 This is a comparison chart of the peeling force of films coated with different foils;

[0027] The markings in the accompanying drawings include: 1. current collector body; 2. corrosion structure layer. DETAILED DESCRIPTION

[0028] In order to enable those skilled in the art to better understand the technical solution of the present invention, the present invention is further described in detail below in conjunction with embodiments.

[0029] like Figures 4-5 As shown, the utility model discloses a sodium ion battery electrode current collector with good adhesion and bonding force, comprising a current collector body, one side or both sides of the current collector body are provided with a corrosion structure layer.

[0030] To ensure energy density, the thickness of the corrosion structure layer is 0.5-3 μm, and the thickness of the current collector is 6-25 μm. Specifically, the current collector body is aluminum foil, and the aluminum foil is single-sided smooth aluminum foil or double-sided smooth aluminum foil.

[0031] To achieve process feasibility, the corrosion structure layer is formed on the surface of the current collector body by one-piece corrosion using acid solution. Specifically, the acid solution is dilute sulfuric acid, dilute hydrochloric acid, carbonic acid and / or citric acid.

[0032] like Figure 3 As shown, an irregular concave-convex texture structure is formed on the surface of the corrosion structure layer. At the same time, in order to expand and enhance its bonding strength, the corrosion structure layer is formed by secondary or multiple acid corrosion, and a second-order or multi-level structure is formed inside the corrosion structure layer; the aperture gap of the second-order or multi-level structure inside the corrosion structure layer changes from inside to outside.

[0033] In terms of active material applicability, the sodium ion battery includes a positive electrode material layer coated on a current collector, and the positive electrode material layer is a layered oxide material layer, a polyanion material layer or a Prussian blue material layer. Specifically, the length of the positive electrode material layer is less than the length of the corrosion structure layer, and the width of the positive electrode material layer is less than the width of the corrosion structure layer.

[0034] In order to fully verify the technical effect of the utility model, the positive electrode coating was carried out using plain foil, cleaned foil, carbon-coated foil and the corrosion foil of the utility model. The positive electrode formula is NFPP (composite sodium pyrophosphate) 95%: SP 1.5%: KS6 0.5%: PVDF5130 3%, and the single-sided surface density of the coating is 150g / m 2 , compacted density 2.0g / cm 3 The above electrodes were subjected to peeling force test, and the test results are as follows: Figure 6 As shown, the test results show that the corrosion foil is the best, about twice that of other foils. The test results show that the current collector of the utility model has better electrode adhesion, can improve the yield rate of the electrode, improve the electrode stability and thus improve the long-term electrochemical performance.

[0035] The above embodiments are only specific embodiments of the present invention, and their descriptions are relatively specific and detailed, but they cannot be understood as limiting the scope of the present invention. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the present invention, and these obvious replacement forms all belong to the protection scope of the present invention.

Claims

1. A sodium ion battery electrode current collector with good adhesion, comprising a current collector body, characterized in that: A corrosion structure layer is arranged on one or both sides of the current collector body; an irregular concave-convex texture structure is formed on the surface of the corrosion structure layer; the corrosion structure layer is formed by secondary or multiple acid corrosion, and a second-order or multi-order structure is formed inside the corrosion structure layer.

2. The sodium ion battery electrode current collector with good adhesion according to claim 1, characterized in that: The thickness of the corrosion structure layer is 0.5-3 μm; the thickness of the current collector is 6-25 μm.

3. The sodium ion battery electrode current collector with good adhesion according to claim 2, characterized in that: The current collector body is aluminum foil, and the aluminum foil is single-sided smooth aluminum foil or double-sided smooth aluminum foil.

4. The sodium ion battery electrode current collector with good adhesion according to claim 3, characterized in that: The corrosion structure layer is formed on the surface of the current collector body by one-piece corrosion using acid solution.

5. The sodium ion battery electrode current collector with good adhesion according to claim 4, characterized in that: The aperture gap of the second-order or multi-order structure inside the corrosion structure layer changes gradually from the inside to the outside.

6. The sodium ion battery electrode current collector with good adhesion according to claim 5, characterized in that: The sodium ion battery comprises a positive electrode material layer coated on a current collector, wherein the positive electrode material layer is a layered oxide material layer, a polyanion material layer or a Prussian blue material layer.

7. The sodium ion battery electrode current collector with good adhesion according to claim 6, characterized in that: The length of the positive electrode material layer is smaller than the length of the corrosion structure layer, and the width of the positive electrode material layer is smaller than the width of the corrosion structure layer.