Diamond thinning pad
By designing the combination structure of chip removal groove and through holes on the diamond thinning pad, the problem of debris accumulation in diamond abrasive material is solved, and the smooth discharge of debris and the improvement of grinding and polishing efficiency is achieved. At the same time, the PC board is used to improve material performance .
Patent Information
- Application Number
- CN202223532286.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-29
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2032-12-29
AI Technical Summary
The existing diamond abrasive substrate lacks chip removal structural design, which leads to the inability to discharge processed debris in time, causing accumulation to affect the grinding and polishing effect.
A diamond thinning pad is designed, including a substrate and a base glue layer. A matrix-arranged cylindrical abrasive particles and through holes are provided on the substrate. The through holes penetrate the substrate and connect the chip discharge groove to ensure that the debris can be discharged smoothly.
Through the combined design of chip drain and through holes, debris accumulation is avoided, grinding and polishing efficiency is improved, and the substrate made of PC boards improves the lightweight, weather resistance and super-strong performance of the material.
Smart Images

Figure CN221953076U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of grinding materials, in particular to a diamond thinning pad. Background Art
[0002] With the development of materials science, the hardness of materials used in the field of 3C technology is getting higher and higher. The materials used in products such as sapphire substrates, sapphire glass, ceramic mobile phone back covers, ceramic fingerprint recognition sheets and tempered glass are all materials with a Mohs hardness of 9. During the production process, abrasive tools are often required to grind and polish the surfaces of these products.
[0003] The widespread use of superhard materials has put forward higher requirements for processing. Ordinary abrasives have low hardness and are not suitable for grinding and polishing operations of products with very high hardness. In this case, special abrasives with large cutting force, high self-sharpening and continuous grinding force are required, such as diamond abrasives. The existing diamond abrasive material structure usually includes a substrate, a grinding layer arranged on the substrate and a grinding protrusion arranged on the grinding layer. Although it can achieve high-requirement grinding and polishing, its substrate lacks a chip removal structure design, resulting in the inability to discharge the debris in time, causing the processing debris to accumulate in the chip removal groove and affect the grinding and polishing phenomenon.
[0004] Therefore, it is necessary to develop a new technology to solve the above problems. Utility Model Content
[0005] In view of this, the utility model aims to solve the defects in the prior art, and its main purpose is to provide a diamond thinning pad, which avoids the phenomenon that machining debris accumulates in the chip groove and affects the grinding and polishing.
[0006] In order to achieve the above purpose, the utility model adopts the following technical solutions:
[0007] A diamond thinning pad comprises a substrate and a base glue layer connected to the upper surface of the substrate, wherein the substrate is made of a PC board, a plurality of abrasive particles are convexly provided on the upper surface of the base glue layer, the plurality of abrasive particles are arranged in a matrix, the abrasive particles are in a cylindrical structure, a chip groove is formed between two adjacent abrasive particles, the substrate is provided with a through hole, the through hole extends in the up-down direction and passes through the upper and lower surfaces of the substrate, the through hole passes through the base glue layer and is connected to the chip groove.
[0008] As a preferred solution, a chamfer is provided at the upper opening of the through hole, and the chamfer extends obliquely upward and outward along the circumference of the through hole.
[0009] As a preferred embodiment, the abrasive particles have two parallel bottom surfaces, which are respectively defined as an upper bottom surface and a lower bottom surface, the upper bottom surface and the lower bottom surface are connected by a side surface, the upper bottom surface is the abrasive surface, and the lower bottom surface is connected to the upper surface of the base glue layer.
[0010] As a preferred solution, the upper bottom surface and the lower bottom surface are both circular structures, the diameters of the upper bottom surface and the lower bottom surface are both 1-100 mm, and the height of the side surface in the up and down directions is 1-30 mm.
[0011] As a preferred solution, the distance between two adjacent abrasive particles is 0.5-30 mm.
[0012] As a preferred solution, the cross section of the substrate is an annular structure, and correspondingly, the cross section of the primer layer is an annular structure.
[0013] As a preferred solution, the cross-sections of the substrate and the primer layer are both rectangular structures.
[0014] As a preferred solution, the lower surface of the primer layer is bonded to the upper surface of the substrate.
[0015] Compared with the prior art, the utility model has obvious advantages and beneficial effects. Specifically, it can be seen from the above technical scheme that it mainly combines the chip groove and the through hole to enable the chips generated by processing to be smoothly discharged through the chip groove and the through hole. In this way, the phenomenon that the processing chips accumulate in the chip groove and affect the grinding and polishing is avoided. In addition, the base plate made of PC board can have better performance, so that it has the properties of light weight, weather resistance, super strength, etc.
[0016] In order to more clearly illustrate the structural features, technical means and specific purposes and functions achieved by the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a cross-sectional view of the first embodiment of the utility model;
[0018] Figure 2 It is a top view of the first embodiment of the utility model;
[0019] Figure 3 It is a top view of the second embodiment of the present utility model.
[0020] Description of the accompanying drawings:
[0021] 10. Substrate 20. Base glue layer
[0022] 30. Abrasive particles 40. Chip removal groove
[0023] 50. Through hole. DETAILED DESCRIPTION
[0024] Please refer to Figures 1 to 3 As shown, it shows the specific structure of two embodiments of the utility model; it is mainly used for grinding and polishing sapphire, ceramics, glass, metal, etc., but is not limited to this.
[0025] A diamond thinning pad includes a substrate 10 and a primer layer 20 connected to the upper surface of the substrate 10. Preferably, the lower surface of the primer layer 20 is bonded to the upper surface of the substrate 10. A plurality of abrasive particles 30 are convexly arranged on the upper surface of the primer layer 20. The abrasive particles 30 are used for grinding and polishing. The plurality of abrasive particles 30 are arranged in a matrix. The abrasive particles 30 are cylindrical in structure. The abrasive particles 30 have two parallel bottom surfaces, which are respectively defined as an upper bottom surface and a lower bottom surface. The upper bottom surface and the lower bottom surface are connected through a side surface. The upper bottom surface is an abrasive surface, and the lower bottom surface is connected to the upper surface of the primer layer 20. The upper bottom surface and the lower bottom surface are both circular structures. The diameters of the upper bottom surface and the lower bottom surface are both 1-100 mm, and the height of the side surface in the up-down direction is 1-30 mm.
[0026] Preferably, the substrate 10 is made of PC board, which has excellent properties such as light weight, weather resistance, super strength, flame retardancy, and sound insulation compared to laminated glass, tempered glass, and hollow glass. In this way, the substrate 10 made of PC board can have better performance, thereby making it have properties such as light weight, weather resistance, and super strength.
[0027] A chip groove 40 is formed between two adjacent abrasive particles 30. Preferably, the spacing between two adjacent abrasive particles 30 is 0.5-30 mm. The substrate 10 is provided with a through hole 50, which extends in the up-down direction and penetrates the upper and lower surfaces of the substrate 10. The through hole 50 passes through the primer layer 20 and is connected to the chip groove 40. A chamfer is provided at the upper opening of the through hole 50, and the chamfer extends obliquely upward outward along the circumference of the through hole 50. In this way, the setting of the chamfer can facilitate the debris in the chip groove 40 to flow smoothly into the through hole 50 through the chamfer for discharge, making the chip discharge smoother. Here, through the combined design of the chip groove 40 and the through hole 50, the debris generated by the processing can be discharged smoothly through the chip groove 40 and the through hole 50, so as to avoid the phenomenon that the processing debris accumulates in the chip groove 40 and affects the grinding and polishing.
[0028] like Figure 1 , 2 As shown, in the first embodiment, the cross section of the substrate 10 is an annular structure, and correspondingly, the cross section of the primer layer 20 is an annular structure. In this way, the whole structure can be annular.
[0029] like Figure 3 As shown, in the second embodiment, the cross sections of the substrate 10 and the primer layer 20 are both rectangular structures. In this way, the whole structure can be rectangular.
[0030] To sum up, the design focus of the utility model is that it mainly combines the chip groove and the through hole to enable the chips generated by processing to be smoothly discharged through the chip groove and the through hole. In this way, the phenomenon that the processing chips accumulate in the chip groove and affect the grinding and polishing is avoided, and the substrate made of PC board can have better performance, so that it has the properties of light weight, weather resistance, and super strength.
[0031] The above description is only a preferred embodiment of the present invention and does not limit the technical scope of the present invention. Therefore, any slight modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention are still within the scope of the technical solution of the present invention.
Claims
1. A diamond thinning pad, Features: The invention comprises a substrate and a primer layer connected to the upper surface of the substrate, wherein the substrate is made of a PC board, a plurality of abrasive particles are convexly arranged on the upper surface of the primer layer, the plurality of abrasive particles are arranged in a matrix, the abrasive particles are in a cylindrical structure, a chip groove is formed between two adjacent abrasive particles, the substrate is provided with a through hole, the through hole extends in the up-down direction and passes through the upper and lower surfaces of the substrate, the through hole passes through the primer layer and is connected to the chip groove; a chamfer is provided at the upper opening of the through hole, the chamfer extends obliquely upward outward along the circumference of the through hole; the cross section of the substrate is annular, and correspondingly, the cross section of the primer layer is annular; the lower surface of the primer layer is bonded to the upper surface of the substrate; The abrasive particles have two parallel bottom surfaces, which are respectively defined as an upper bottom surface and a lower bottom surface, the upper bottom surface and the lower bottom surface are connected by a side surface, the upper bottom surface is an abrasive surface, and the lower bottom surface is connected to the upper surface of the base glue layer; the upper bottom surface and the lower bottom surface are both circular structures, the diameters of the upper bottom surface and the lower bottom surface are both 1-100 mm, and the height of the side surface in the up and down direction is 1-30 mm; The distance between two adjacent abrasive particles is 0.5-30 mm.