Ionic liquid gating device for regulating and controlling oxygen content of oxide film
Through the ionic liquid gate control device, the electric field is formed by using electrochemical reactions, which solves the problem of poor controllability of the oxygen content regulation of the oxide film, and achieves the accurate, deep, wide range, fast speed and good reversibility of the oxygen content, satisfying the Different application requirements.
Patent Information
- Application Number
- CN202420384236.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-29
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The prior art cannot effectively realize the precise regulation of the oxygen content of oxide films, and the controllability and limited depth are poor, so it cannot meet the needs of different application.
Using an ionic liquid gate control device, the bottom plate, working electrode, top electrode and ionic liquid are installed in the oxide film, the gate voltage is applied using an external power supply to control the oxygen content, and the liquid-solid electrochemical reaction is used to form an electric field to achieve oxygen ions. migrate.
It realizes accurate regulation of the oxygen content of oxide films, with large depth of regulation, wide range, fast speed and good reversibility, meets different application needs, is easy to operate, and is easy to batch preparation and application.
Smart Images

Figure CN221988694U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of thin film material regulating devices, in particular to an ionic liquid gating device for regulating the oxygen content of an oxide film. Background Art
[0002] Oxide thin film materials have broad application prospects in the fields of information storage, sensing, and optoelectronic devices due to their excellent magnetic, electrical, and optical properties. The oxygen content in oxide thin films is closely related to their performance. For example, oxygen vacancies in perovskite structured oxides affect the conductivity of the material, and changes in the oxygen content in transition metal oxides can cause changes in the metal valence state, thereby changing the magnetic and electrical properties of the material. Therefore, achieving precise control of the oxygen content of oxide thin films is of great significance for optimizing and expanding the functions of oxide thin film materials.
[0003] At present, the regulation of the oxygen content of oxide films is mainly carried out by changing the film-forming conditions of the oxide, such as temperature, oxygen partial pressure, and subsequent annealing oxidation. However, the controllability of these methods is poor, the change of oxygen content is relatively random, and it is impossible to achieve real-time monitoring of the change process of oxygen content. In recent years, by constructing an oxide thin film field effect transistor structure, the gate voltage is used to control the conductivity of the film to achieve the regulation of oxygen content. However, this method has limited control depth and the adjustment range of the oxygen content of the film is small.
[0004] Therefore, there is an urgent need for a new device that can easily and precisely control the oxygen content of oxide films. Utility Model Content
[0005] In order to solve the problems of the prior art, the embodiment of the utility model provides an ionic liquid gating device for regulating the oxygen content of an oxide film. The technical solution is as follows:
[0006] On the one hand, an ionic liquid gating device for regulating the oxygen content of an oxide film is provided, comprising a base plate, an oxide film working electrode arranged on the base plate, a top electrode arranged above the oxide film working electrode, an ionic liquid arranged between the oxide film working electrode and the top electrode, and an external power supply connecting the working electrode and the top electrode, wherein the lower surface of the oxide film working electrode is attached to the base plate, the top electrode is an aluminum foil, the three edges of the oxide film working electrode are covered by the aluminum foil, a gap for placing the ionic liquid is formed between the aluminum foil and the oxide film working electrode, and the external power supply applies a gate voltage to the aluminum foil to regulate the oxygen content in the oxide film working electrode.
[0007] Furthermore, the material of the oxide thin film working electrode is a perovskite structure oxide material.
[0008] Furthermore, the ionic liquid is composed of positive ion N,N-diethyl-N-(2-methoxyethyl)-N-methylammonium and negative ion bis(trifluoromethanesulfonyl)imide.
[0009] Furthermore, the external power supply is a constant power supply.
[0010] Furthermore, the thickness of the oxide thin film working electrode is 50 nanometers to 500 nanometers.
[0011] Furthermore, the height of the aluminum foil covering the three edges of the oxide film working electrode is equal to or exceeds the thickness of the oxide film.
[0012] Furthermore, it also includes a chip holder arranged below the bottom plate, and the oxide film working electrode is adhered to the chip holder by double-sided adhesive.
[0013] Furthermore, a groove is formed on the chip holder, and the connecting wire constituting the external power supply is inserted into the groove and electrically connected to the oxide film working electrode and the top electrode.
[0014] Furthermore, the gate voltage output by the external power supply is -10 to 10 volts.
[0015] Furthermore, the material of the oxide thin film working electrode is strontium cobaltate SrCoO3.
[0016] The beneficial effects brought by the technical solution provided by the embodiment of the utility model are:
[0017] The precise regulation of the oxygen content of the oxide film is achieved, and the oxygen content of the oxide film can be continuously and controllably changed to meet the needs of different applications.
[0018] The control method is simple. The oxygen content can be adjusted by changing the voltage direction and size of the external power supply without the need to introduce different gases.
[0019] The regulation depth is large. Based on the liquid-solid electrochemical reaction, a strong electric field can be formed inside the oxide film, and the oxygen ion migration depth is large.
[0020] The regulation range is wide, and the oxygen content in the oxide film can be increased or decreased to meet the regulation needs in different directions.
[0021] The regulation speed is fast, and the oxygen ions migrate quickly between the liquid and the solid, achieving real-time control of the oxide film properties.
[0022] The regulation has good reversibility, and oxygen ions can be repeatedly inserted and extracted by changing the voltage direction, thus achieving reversible regulation of oxygen content.
[0023] Precise control: By using electrochemical means, the migration of oxygen ions can be precisely controlled to achieve precise regulation of oxygen content.
[0024] The operation is simple, the experimental equipment is simple, and it is easy to prepare and apply in batches. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0026] Figure 1 This is a schematic diagram of a module of an ionic liquid gating device for regulating the oxygen content of an oxide film according to an embodiment of the utility model;
[0027] Figure 2 It is a schematic diagram of an ionic liquid gating device for regulating the oxygen content of an oxide film according to an embodiment of the utility model;
[0028] Figure 3 This is a schematic diagram of an ionic liquid gating device for regulating the oxygen content of an oxide film according to an embodiment of the utility model, which is arranged in an ionic liquid electrical measurement box;
[0029] Figure 4 This is a schematic diagram of the principle of regulating oxide film in an embodiment of the utility model. DETAILED DESCRIPTION
[0030] In order to make the purpose, technical solution and advantages of the present invention more clear, the implementation mode of the present invention will be further described in detail below with reference to the accompanying drawings.
[0031] The utility model provides an ionic liquid gating device for regulating the oxygen content of an oxide film.
[0032] Reference Figure 1 and 2 , which is a specific embodiment of the utility model, includes a base plate 1, an oxide film working electrode 2 arranged on the base plate 1, an aluminum foil top electrode 3 arranged above the working electrode 2, an ionic liquid arranged between the working electrode 2 and the top electrode 3, and an external power supply 5 connecting the working electrode 2 and the top electrode 3.
[0033] The working electrode 2 is prepared by magnetron sputtering or pulsed laser deposition, and the material is preferably an oxide film of strontium ferrite or strontium cobaltate with a perovskite structure. The thickness of the working electrode 2 is preferably 50-500nm. The lower surface of the working electrode 2 is directly attached to the bottom plate 1. The material of the bottom plate 1 is preferably PVC, mica, glass, etc. with good insulation to prevent short circuit between the electrode and the chip slot.
[0034] The top electrode 3 is an aluminum foil, covering three edges of the working electrode 2. The height of the top electrode 3 covering the edge of the working electrode 2 is not less than the thickness of the working electrode 2. A gap for placing the ionic liquid is formed between the top electrode 3 and the working electrode 2. The width of the gap is greater than 300 microns.
[0035] The ionic liquid is preferably a combination of N, N-diethyl-N-(2-methoxyethyl)-N-methylammonium and bis(trifluoromethanesulfonyl)imide. The ionic liquid has good conductivity and a wide liquid temperature range (-4°C to 200°C), which meets the working requirements of the equipment.
[0036] The external power supply 5 is a constant power supply, which outputs a stable DC voltage. The output voltage range is -10 to 10 V. The external power supply 5 controls the migration of oxygen ions in the ionic liquid to the working electrode 2 by changing the output gate voltage, so as to increase or decrease the oxygen content of the working electrode 2.
[0037] In addition, in order to facilitate connection with the external power supply 5, a chip holder 6 can be arranged below the bottom plate 1, and the working electrode 2 and the top electrode 3 are electrically connected to the connection slots on the chip holder 6 through gold wires.
[0038] When set to the ionic liquid electrical measurement box 4, see Figure 3 , the external power supply 5 is arranged on the ionic liquid electrical measurement box 4 .
[0039] In this embodiment, a large electric field can be formed by utilizing ionic liquid to control the reversible migration of oxygen ions between the working electrode 2 and the liquid, thereby achieving precise regulation of the oxygen content of the oxide film and overcoming the disadvantage of limited regulation capability of the prior art.
[0040] The working principle of the utility model is:
[0041] An ionic liquid is sandwiched between the working electrode 2 and the top electrode 3 to form a three-electrode electrochemical cell structure.
[0042] When the external power source 5 applies voltage, the negative oxygen ions in the ionic liquid will migrate to the surface of the working electrode 2, and the positive ions will migrate to the surface of the top electrode 3, forming an electric double layer structure at the interface.
[0043] When a positive voltage is applied, negative oxygen ions flow from the working electrode 2 into the ionic liquid, which is equivalent to extracting oxygen ions from the oxide film; when a negative voltage is applied, oxygen ions are inserted from the ionic liquid into the working electrode 2, which is equivalent to inserting oxygen ions into the oxide film.
[0044] By controlling the magnitude and direction of the output voltage of the external power supply 5, the oxygen content in the oxide film working electrode 2 can be controlled, thereby achieving regulation of the performance of the oxide film.
[0045] Compared with the existing gate electric field effect, the utility model is based on liquid-solid interface electrochemical reaction, which can form a larger electric field inside the oxide film, a greater oxygen ion migration depth, and a more obvious control effect.
[0046] See also Figure 4 , and also provided the principle diagram of regulating oxide film: (a) Schematic diagram of ionic liquid gate device of SCO film; (b) Negative gate voltage and (c) positive gate voltage induced ionic liquid gate device working principle. SCO represents SrCoO3 oxide film, STO represents SrTiO3 substrate, TFSI- and DEME+ are positive and negative ions of ionic liquid, and the positive and negative ions can form opposite electric fields after the positive and negative voltages are applied, which in turn regulates the O in SrCoO3 oxide film. 2- Insertion or extraction, that is, reversible regulation of oxygen ions in oxide films, thereby regulating various magneto-optical and other properties.
[0047] An application example of the utility model is:
[0048] The device was used to control the strontium cobalt oxide (SrCoO 3-δ )The oxygen content of the film can be used to regulate its resistance.
[0049] Strontium cobalt oxide is a typical transition metal oxide, and its resistance is strongly dependent on the oxygen content. The more oxygen defects in the strontium cobalt oxide film, the greater the resistance.
[0050] The steps are:
[0051] Depositing a strontium cobalt oxide thin film on a substrate as a working electrode;
[0052] Aluminum foil was placed on top of the film as the top electrode;
[0053] Inject DEME-TFSI ionic liquid between the two;
[0054] Connect an external power supply, apply a positive voltage, and extract oxygen ions from the film;
[0055] The increase in the resistance of the strontium cobalt oxide film was measured as the oxygen content decreased;
[0056] When a negative voltage is applied in the reverse direction, oxygen ions are inserted and the resistance of the strontium cobalt oxide film decreases.
[0057] Specifically, an oxide thin film working electrode is prepared on a substrate by magnetron sputtering or pulsed laser deposition;
[0058] The oxide film working electrode is adhered to the bottom plate, and then the bottom plate is adhered to the chip holder;
[0059] Use aluminum foil as the top electrode to cover the three edges of the oxide film working electrode, leaving a gap between the top of the aluminum foil and the film, then use a syringe to fill the uncoated side with ionic liquid, and finally insert the chip holder into the slot of the control device;
[0060] Use gold wire to connect the oxide film working electrode and the aluminum foil top electrode to the corresponding chip holder slot, and the slot is connected to an external power supply.
[0061] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. An ionic liquid gating device for regulating the oxygen content of an oxide film, characterized in that: It includes a bottom plate, an oxide film working electrode arranged on the bottom plate, a top electrode arranged above the oxide film working electrode, an ionic liquid arranged between the oxide film working electrode and the top electrode, and an external power supply connecting the oxide film working electrode and the top electrode. The lower surface of the oxide film working electrode is attached to the bottom plate, the top electrode is an aluminum foil, the three edges of the oxide film working electrode are covered by the aluminum foil, a gap for placing the ionic liquid is formed between the aluminum foil and the oxide film working electrode, and the external power supply applies a gate voltage to the aluminum foil to regulate the oxygen content in the oxide film working electrode.
2. The device according to claim 1, characterized in that The material of the oxide thin film working electrode is a perovskite structure oxide material.
3. The device according to claim 1, characterized in that The ionic liquid consists of positive ion N,N-diethyl-N-(2-methoxyethyl)-N-methylammonium and negative ion bis(trifluoromethanesulfonyl)imide.
4. The device according to claim 1, characterized in that The external power supply is a constant power supply.
5. The device according to claim 1, characterized in that The thickness of the oxide film working electrode is 50 nanometers to 500 nanometers.
6. The device according to claim 1, characterized in that The height of the aluminum foil covering the three edges of the oxide film working electrode is equal to or greater than the thickness of the oxide film.
7. The device according to claim 1, characterized in that It also includes a chip holder arranged below the bottom plate, and the oxide film working electrode is adhered to the chip holder by double-sided adhesive.
8. The device according to claim 7, characterized in that The chip holder is provided with a groove, and a connecting wire constituting an external power source is inserted into the groove and electrically connected to the oxide film working electrode and the top electrode.
9. The device according to claim 1, characterized in that The gate voltage output by the external power supply is -10 to 10 volts.
10. The device according to claim 1, characterized in that The material of the oxide film working electrode is strontium cobaltate SrCoO3.