Atomic layer deposition equipment
By using positioning components and a flow control ring made of ceramic or quartz in the atomic layer deposition equipment, the problems of difficulty in installing the flow control ring and insufficient centering accuracy in the equipment are solved, and the uniformity of the deposition process and product quality are improved. Reduces maintenance costs and impurity generation.
Patent Information
- Application Number
- CN202323665432.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-29
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2033-12-29
AI Technical Summary
In existing atomic layer deposition equipment, it is difficult to install the flow control ring and the centering accuracy is difficult to meet the requirements, which affects the uniformity of the deposition process and product quality.
An atomic layer deposition device including a reaction chamber and a flow control ring is designed. By providing a positioning assembly on the second chamber and a positioning hole on the flow control ring, the installation difficulty is reduced and the installation accuracy is improved. The positioning assembly includes a fixing member and an adjusting member, the adjusting member is an eccentric ring, the flow control ring is made of ceramic or quartz, and the reaction contact surface is set to a rough surface to improve the stability of the deposited layer.
It realizes simple installation and high-precision positioning of the flow control ring, improves the uniformity of the deposition process and product quality, reduces maintenance costs and impurity generation, and enhances the stability of the equipment and the uniformity of the reaction products.
Smart Images

Figure CN222008036U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of semiconductor equipment, and in particular to an atomic layer deposition equipment. Background Art
[0002] Atomic layer deposition is one of the methods for manufacturing integrated circuits. Atomic layer deposition requires that the reactants be generated layer by layer in the form of a single atomic film by introducing precursors into the reaction chamber. The interior of the reaction chamber is divided into an upper chamber and a lower chamber, and atomic layer deposition is performed in the upper chamber. In order for the precursor to enter the lower chamber and react in the lower chamber, a narrow slit non-contact seal is used in the prior art to seal the flow control ring and the non-reactive area below. However, general flow control rings have problems such as difficulty in installation and difficulty in meeting the centering accuracy requirements. Utility Model Content
[0003] In order to solve the above problems, the present application provides an atomic layer deposition device with simple flow control installation and high centering accuracy.
[0004] To achieve the above objectives, the technical solutions adopted in this application are as follows:
[0005] An embodiment of the present application provides an atomic layer deposition device, which includes a reaction chamber and a flow control ring; the reaction chamber includes a first chamber and a second chamber, the second chamber is provided with a positioning assembly, the positioning assembly includes a fixing part and an adjustment part sleeved on the outside of the fixing part; the flow control ring, the flow control ring is fixed to the second chamber, the flow control ring is provided with a positioning hole, the positioning hole and the positioning assembly cooperate with each other, and the positioning hole is sleeved on the outside of the adjustment part.
[0006] Further, in the positioning assembly, the fixing member is detachably connected to the top of the second chamber, and the adjusting member is an eccentric ring.
[0007] Furthermore, the second chamber is provided with three positioning components evenly distributed along the circumference, the flow control ring is provided with three positioning holes matched with the positioning components, and the three positioning holes are evenly distributed on the flow control ring along the circumference.
[0008] Furthermore, the size of the positioning hole is greater than or equal to the size of the adjusting member.
[0009] Further, when the size of the positioning hole is equal to the size of the adjusting member, the tolerance of the size of the positioning hole is set to a positive tolerance, and the tolerance of the size of the adjusting member is set to a negative tolerance.
[0010] Furthermore, the positioning hole is a semi-waist-shaped hole arranged on the edge of the flow control ring.
[0011] Furthermore, the flow control ring is made of a ceramic ring material or a quartz ring material.
[0012] Furthermore, the surface of the flow control ring exposed in the reaction chamber is defined as a reaction contact surface, and the reaction contact surface is a rough surface.
[0013] Furthermore, the roughness Ra of the reaction contact surface is 0.5-10 μm.
[0014] Furthermore, the roughness Ra of the reaction contact surface is 1-8 μm.
[0015] In the present application, a positioning component with a certain adjustment range is arranged in the second chamber of the atomic layer deposition equipment, and a positioning hole matching the positioning component is arranged on the flow control ring. Through the mutual cooperation of the positioning component and the positioning hole, the installation difficulty between the flow control ring and the second chamber is reduced, and the installation accuracy between the flow control ring and the second chamber is improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 A longitudinal cross-sectional schematic diagram of a reaction chamber portion of an atomic deposition device in one embodiment of the present application;
[0017] Figure 2 This is a schematic top view of the second chamber in one embodiment of the present application;
[0018] Figure 3 for Figure 2 The enlarged schematic diagram of point A in the middle;
[0019] Figure 4 This is a schematic top view of a flow control ring in one embodiment of the present application;
[0020] Figure 5 This is a schematic top view of a partial structure of a reaction chamber in one embodiment of the present application;
[0021] Figure 6 This is a schematic top view of a flow control ring in another embodiment of the present application.
[0022] In the figure: atomic layer deposition equipment 100, reaction chamber 11, first chamber 111, second chamber 112, positioning assembly 1121, fixing member 1121a, adjusting member 1121b, flow control ring 12, positioning hole 121, reaction contact surface 122, sealing ring 13, spray plate 14, heating base 15. DETAILED DESCRIPTION
[0023] In order to enable those skilled in the art to better understand the solution of the present application, the technical solution in the specific implementation manner of the present application will be clearly and completely described below in conjunction with the drawings in the implementation manner of the present application.
[0024] This application provides a Figure 1The atomic layer deposition device 100 shown in the figure includes a reaction chamber 11, a flow control ring 12, a sealing ring 13, a spray plate 14 and a heating base 15. The reaction chamber serves as the main place for precursors to form semiconductor materials through atomic layer deposition. The heating base 15 serves as a carrier for atomic layer deposition. At the same time, the heating base 15 divides the reaction chamber 11 into a first chamber 111 and a second chamber 112. The reaction of the precursor inside the reaction chamber 11 is confined to the first chamber 111. The spray plate 14 is used to input the precursor into the first chamber 111. The sealing ring 13 is sleeved on the outside of the heating base 15, and the flow control ring 12 is fixed to the second chamber 112. The sealing ring 13 and the flow control ring 12 cooperate with each other to form a sealing structure, which isolates the first chamber 111 and the second chamber 112 and prevents the precursor from entering the second chamber 112. As shown Figure 2 and Figure 3 As shown, the second chamber 112 is provided with a positioning assembly 1121, which includes a fixing member 1121a and an adjusting member 1121b. The fixing member 1121a is connected to the second chamber 112, and the adjusting member 1121b is sleeved on the outside of the fixing member 1121a. The adjusting member 1121b can rotate around the fixing member 1121a. During the rotation around the fixing member 1121a, the adjusting member 1121b can adjust its position within a certain range. Figure 4 As shown, the flow control ring 12 is provided with a positioning hole 121, and the positioning hole 121 and the positioning component 1121 are matched with each other. Figure 5 As shown, after the positioning hole 121 and the positioning component 1121 cooperate with each other, the flow control ring 12 can be fixed to the second chamber 112. At the same time, the installation accuracy between the flow control ring 12 and the second chamber 112 can be improved by the mutual cooperation of the positioning hole 121 and the positioning component 1121. Specifically, the positioning hole 121 and the adjustment member 1121b match each other, and the positioning hole 121 can be sleeved to the outside of the adjustment member 1121b. The adjustment member 1121b can adjust its own position within a certain range, can better adapt to the flow control ring 12, and thus can reduce the difficulty of installing the flow control ring 12 to the second chamber 112. After reducing the installation difficulty of the flow control ring 12 and the second chamber 112 and improving the installation accuracy through the above-mentioned settings, the uniformity of the reaction products generated in the atomic layer deposition equipment 100 can be improved.
[0025] As an embodiment, the fixing member 1121a in the positioning assembly 1121 is detachably connected to the top of the second chamber 112, and the adjusting member 1121b is an eccentric ring. The detachably connected fixing member 1121a facilitates the selection of fixing members 1121a and corresponding adjusting members 1121b of corresponding shapes and sizes according to the specific structure of the flow control ring 12. At the same time, when the fixing member 1121a and the adjusting member 1121b are damaged, the fixing member 1121a and the adjusting member 1121b can be replaced more conveniently, which can reduce the later maintenance cost of the atomic layer deposition equipment 100. The adjusting member 1121b with an eccentric ring structure can realize the fine adjustment of the position of the positioning assembly 1121, so that the positioning assembly 1121 can better adapt to the flow control ring 12, reduce the installation difficulty of the flow control ring 12 and improve the installation accuracy of the flow control ring 12.
[0026] As an embodiment, the second chamber 112 is provided with three positioning components 1121 evenly distributed along the circumference, and the flow control ring 12 is provided with three positioning holes 121 that match the positioning components 1121, and the three positioning holes 121 are evenly distributed on the flow control ring 12 along the circumference. The three positioning components 1121 and the three positioning holes 121 constitute a three-point fixed structure, which can uniquely determine the posture and position of the flow control ring 12, realize the precise positioning of the installation position of the flow control ring 12, and meet the centering accuracy requirements. The three-point fixed structure can also play a good fixing effect, enhance the stability and rigidity of the fixed structure, and improve the connection reliability between the flow control ring 12 and the second chamber 112. The three-point fixed structure can also prevent the flow control ring 12 from being displaced during the use of the atomic layer deposition device 100. The three positioning components 1121 and the three positioning holes 121 are evenly distributed along the circumference, and can limit the installation position of the flow control ring 12 from all directions, improve the installation accuracy between the flow control ring 12 and the second chamber 112, and make the axis of the flow control ring 12 completely aligned with the axis of the second chamber 112, so as to achieve the centering installation of the flow control ring 12 and the second chamber 112. In addition, the provision of the three positioning components 1121 and the three positioning holes 121 can also avoid the adverse effects on the generation of reaction products in the atomic layer deposition device 100 due to the excessive number of positioning components 1121 and positioning holes 121, and improve the uniformity of the reaction products generated in the atomic layer deposition device 100.
[0027] As an implementation mode, the size of the positioning hole 121 is greater than or equal to the size of the adjustment member 1121b. When the size of the positioning hole 121 is equal to the size of the adjustment member 1121b, the flow control ring 12 can be installed on the positioning component 1121 of the second cavity through the positioning hole 121, so as to achieve accurate installation of the flow control ring 12. When the size of the positioning hole 121 is greater than the size of the adjustment member 1121b, a certain adjustment margin is reserved between the positioning hole 121 and the adjustment member 1121b, which can increase the installation flexibility and convenience of the flow control ring 12 to a certain extent, can reduce the installation of the flow control ring 12, and better improve the installation accuracy and centering accuracy of the flow control ring 12.
[0028] As an implementation mode, when the size of the positioning hole 121 is equal to the size of the adjusting member 1121b, the tolerance of the size of the positioning hole 121 is set to a positive tolerance, and the tolerance of the size of the adjusting member 1121b is set to a negative tolerance. When the size of the positioning hole 121 is equal to the size of the adjusting member 1121b, the tolerance of the size of the positioning hole 121 is controlled to be a positive tolerance, and the size of the adjusting member 1121b is controlled to be a negative tolerance, so that there is a margin between the size of the positioning hole 121 and the size of the adjusting member 1121b, that is, there is a margin for position adjustment between the positioning hole 121 and the adjusting member 1121b, which is convenient for adjusting the installation position of the flow control ring 12 and improving the installation convenience of the flow control ring 12. After adjusting the position of the adjusting member 1121b, installing the flow control ring 12 can ensure the installation accuracy of the flow control ring 12, so that the flow control ring 12 is accurately fixed to the second cavity.
[0029] As an implementation method, Figure 6 As shown, the positioning hole 121 is a semi-waist-shaped hole set on the edge of the flow control ring 12. In the embodiment of the present application, there is no special requirement for the specific shape of the positioning hole 121. However, setting the positioning hole 121 as a semi-waist-shaped hole with an opening can further reduce the difficulty of matching between the positioning hole 121 and the positioning component 1121, and can better reduce the difficulty of installing the flow control ring 12.
[0030] As an embodiment, the flow control ring 12 is made of ceramic or quartz. Both ceramic and quartz materials have low thermal conductivity, which can prevent the heat in the first chamber 111 from being transferred to the second chamber 112 during the atomic layer deposition reaction, prevent the heat in the first chamber 111 from being lost, improve the temperature stability in the first chamber 111, and also prevent the durability of the components in the second chamber 112 from being reduced due to high temperature.
[0031] As an embodiment, the surface of the flow control ring 12 exposed in the reaction chamber 11 is defined as a reaction contact surface 122, and the reaction contact surface 122 is a rough surface. During the atomic layer deposition reaction process, the reaction contact surface 122 of the flow control ring 12 exposed in the reaction chamber 11 will inevitably undergo a deposition reaction and form a reactant deposition layer on the reaction contact surface 122. In the present application, the reaction contact surface 122 is set as a rough surface, so that the reactants generated on the reaction contact surface 122 during the reaction process can be firmly adsorbed on the reaction contact surface 122 to form a stable reactant deposition layer. The formation of a stable reactant deposition layer can prevent the reactants deposited on the reaction contact surface 122 from falling off due to the drastic temperature and flow changes such as high temperature and exhaust, forming particulate impurities, and avoid increasing the concentration of particulate matter in the reaction chamber 11, which can reduce impurities in the atomic layer deposition reaction process and improve the quality of the thin film deposition reaction. In addition, the stable reactant deposition layer formed on the reaction contact surface 122 can also protect the flow control ring 12, increase the service life of the flow control ring 12, and reduce the maintenance frequency of the atomic layer deposition device 100.
[0032] As an embodiment, the roughness Ra of the reaction contact surface 122 is 0.5-10 μm. When the roughness Ra of the reaction contact surface 122 is 0.5-10 μm, the roughness of the reaction contact surface 122 is moderate, which can avoid the problem that the reactant deposition layer cannot be formed due to the reaction base surface being too smooth, and can also avoid the problem that the reactant deposition layer is too rough and has poor adhesion and is easy to fall off. Further, the roughness Ra of the reaction contact surface 122 is 1-8 μm.
[0033] It should be understood that those skilled in the art can make improvements or changes based on the above description, and all these improvements and changes should fall within the scope of protection of the claims attached to this application.
Claims
1. An atomic layer deposition device, characterized in that: include: A reaction chamber, the reaction chamber comprising a first chamber and a second chamber, the second chamber being provided with a positioning assembly, the positioning assembly comprising a fixing member and an adjusting member sleeved outside the fixing member; A flow control ring is fixed to the second chamber, a positioning hole is provided on the flow control ring, the positioning hole cooperates with the positioning assembly, and the positioning hole is sleeved on the outside of the adjusting member.
2. The atomic layer deposition apparatus according to claim 1, characterized in that: In the positioning assembly, the fixing member is detachably connected to the top of the second chamber, and the adjusting member is an eccentric ring.
3. The atomic layer deposition apparatus according to claim 1, characterized in that: The second chamber is provided with three positioning components evenly distributed along the circumference, the flow control ring is provided with three positioning holes matched with the positioning components, and the three positioning holes are evenly distributed on the flow control ring along the circumference.
4. The atomic layer deposition apparatus according to claim 1, characterized in that: The size of the positioning hole is greater than or equal to the size of the adjusting member.
5. The atomic layer deposition apparatus according to claim 4, characterized in that: When the size of the positioning hole is equal to the size of the adjusting member, the tolerance of the size of the positioning hole is set to a positive tolerance, and the tolerance of the size of the adjusting member is set to a negative tolerance.
6. The atomic layer deposition apparatus according to claim 1, characterized in that: The positioning hole is a semi-waist-shaped hole arranged on the edge of the flow control ring.
7. The atomic layer deposition apparatus according to claim 1, characterized in that: The flow control ring is made of ceramic ring material or quartz ring material.
8. The atomic layer deposition apparatus according to claim 1, characterized in that: The surface of the flow control ring exposed in the reaction chamber is defined as a reaction contact surface, and the reaction contact surface is a rough surface.
9. The atomic layer deposition apparatus according to claim 8, characterized in that: The roughness Ra of the reaction contact surface is 0.5-10 μm.