Smooth aluminum sheath power cable hot melt adhesive coating device

By designing an integrated heating coating device and a scraping mechanism, the problems of reducing the temperature of hot melt adhesive and air coating in the spraying system are solved, and higher adhesion and coating uniformity are achieved, and smooth aluminum protection is improved. Performance and safety and stability of cables.

CN222015132UActive Publication Date: 2024-11-15HANGZHOU CABLE
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323607151.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-28
Publication Date
2024-11-15
Estimated Expiration
2033-12-28

AI Technical Summary

Technical Problem

The existing smooth aluminum sheathed cable spraying system causes the temperature of the hot melt adhesive to decrease during the transportation and spraying process, affecting the viscosity, and there is air coating during spraying, forming tiny bubbles, affecting the safety and stability of the cable operation.

Method used

An integrated heating coating device is designed, including a hot melt cylinder, a temperature control device and a scraping mechanism. It adopts a wet coating and scraping device to ensure that the hot melt adhesive is attached at a stable temperature and passes through a spiral scraping structure. And the cold air mechanism reduces air coating and achieves uniform coating.

Benefits of technology

It effectively improves the adhesion and coating uniformity of hot melt adhesive, reduces bubbles on the coated surface, and improves the performance and operational safety and stability of the cable.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222015132U_ABST
    Figure CN222015132U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of power cables, in particular to a smooth aluminum sheath power cable hot melt adhesive coating device which comprises a rack, a bottom plate is arranged on the rack, a hot melting device is arranged on the bottom plate, the hot melting device comprises a hot melting cylinder for storing and heating hot melt adhesive, and the hot melting cylinder is provided with a heating device in a matched mode. Two opposite side walls of the hot melting cylinder are provided with a hot melting inlet and a hot melting outlet which are matched with a power cable; a wire supporting frame facilitating entering of a power cable is arranged outside the hot melting inlet, a die scraping mechanism is arranged on the outer side wall of the hot melting cylinder at the hot melting outlet, and the hot melting device further comprises a temperature control device electrically connected with the heating device. According to the hot melt adhesive coating device for the smooth aluminum sheath power cable, the problems of low adhesion, non-uniform coating, bubbles on the coating surface and the like when a smooth aluminum sheath is coated by spraying a hot melt adhesive in the current industry can be effectively solved, the coating process and mode are improved, and the performance of the smooth aluminum sheath cable is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of power cables, in particular to a hot melt adhesive coating device for a smooth aluminum sheathed power cable. Background Art

[0002] When bonding the metal sheath layer and the insulating outer sheath layer of the domestic smooth aluminum sheath high-voltage power cable, a layer of hot melt adhesive is applied to the outer layer of the metal sheath to increase the adhesion of the insulating outer sheath. In most cases, a spraying system and a scraping system are used. The hot melt adhesive with uniform adhesion can make the cable structure compact and increase the plasticity of the insulating outer sheath.

[0003] The smooth aluminum sheath layer and the insulating outer sheath layer are important components of high-voltage cables and play an important role in electrical performance and operational safety and stability.

[0004] At present, domestic smooth aluminum sheath cable manufacturers basically use split-type spraying systems, which are usually composed of a heating cylinder, an air pump, a rubber hose, and a nozzle. However, this spraying system also has some technical problems:

[0005] The spraying system uses an air pump to extract the heated hot melt adhesive, and then transports it through the adhesive guide tube to the nozzle for spraying. During the transportation and spraying process, the temperature will drop, affecting the viscosity of the hot melt adhesive.

[0006] The air pump extracts the hot melt adhesive, and there is encapsulated air when the nozzle sprays the hot melt adhesive, which forms tiny bubbles when adhering to the smooth surface of the aluminum sheath, affecting the safety and stability of the cable operation.

[0007] Therefore, in order to improve the spraying effect, it is necessary to improve the design of the spraying system. Utility Model Content

[0008] Based on the above problems, the present invention provides a hot melt adhesive coating device for a smooth aluminum sheathed power cable.

[0009] The technical solution adopted by the present invention to solve its technical problem is:

[0010] A hot melt adhesive coating device for a smooth aluminum sheathed power cable comprises a frame, a bottom plate is arranged on the frame, a hot melt device is arranged on the bottom plate, the hot melt device comprises a hot melt cylinder for storing and heating hot melt adhesive, and the hot melt cylinder is provided with a heating device, and hot melt inlets and hot melt outlets matching the power cable are provided on opposite side walls of the hot melt cylinder; a wire support frame is provided outside the hot melt inlet for facilitating the entry of the power cable, a scraping mold mechanism is provided on the outer side wall of the hot melt cylinder at the hot melt outlet, and a temperature control device is also provided, and the temperature control device is electrically connected to the heating device.

[0011] Preferably, a lifting device is provided on the frame, and the bottom plate is provided on the lifting device.

[0012] Preferably, the hot melt cylinder is provided with a disengagement mechanism for disengaging the power cable from the hot melt adhesive between the hot melt inlet and the hot melt outlet. The disengagement mechanism is arranged in the hot melt cylinder, and a disengagement outlet for outputting the power cable from the hot melt cylinder and a disengagement inlet for re-entering the hot melt cylinder from the disengagement mechanism are arranged on the side wall of the disengagement mechanism.

[0013] Preferably, the scraper mechanism comprises a body, a scraper hole is formed on the body, the scraper hole has a multi-section structure, and the scraper opening is reduced in sections or gradually from the inside to the outside.

[0014] Preferably, a spiral structure is provided in the front half of the scraper die hole.

[0015] Preferably, a cold air mechanism is provided outside the hot melt outlet.

[0016] The solution of the present application adopts an integrated heating coating device to allow the hot melt adhesive to adhere to the smooth aluminum jacket layer at a stable temperature and exert the best viscosity;

[0017] Wet coating is used to completely immerse the smooth aluminum sheath layer in the completely melted hot melt adhesive to achieve air isolation effect;

[0018] Use a scraping device to adjust the scraper mold size according to the wire diameter, and scrape off excess hot melt adhesive when the wire is coming out to ensure uniform coating.

[0019] The main structures of this design are: scraping part, adjustment part, temperature control part. The design and operation ideas are as follows: fill the cylinder with hot melt adhesive, and use the temperature control box to control the heating device for heating and insulation. Adjust the scraping mold and center height according to the size of the cable; the cable enters the cylinder and adheres to the hot melt adhesive, passes through the outlet scraping mold, and scrapes off the excess hot melt adhesive; fine-tune the center height to ensure uniform coating thickness.

[0020] Compared with the prior art, the present invention has the following beneficial effects:

[0021] The hot melt adhesive coating device for smooth aluminum sheathed power cable of the present application can effectively solve the problems of low adhesion, uneven coating, and bubbles on the coating surface when smooth aluminum sheath is coated with spray hot melt adhesive in the current industry, improves the coating process and method, and enhances the performance of smooth aluminum sheathed cables. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 A structural schematic diagram of the utility model is provided.

[0023] Figure 2 A schematic structural diagram of the improved hot melt cylinder of Example 2 of the present utility model is given.

[0024] Figure 3 A mold scraping mechanism according to an embodiment of the utility model is provided.

[0025] In the figure: 1 frame, 2 bottom plate, 3 hot melt device, 4 hot melt cylinder, 5 heating device, 6 hot melt inlet, 7 hot melt outlet, 8 wire support frame, 9 scraper mechanism, 10 temperature control device, 11 lifting device, 12 disengagement mechanism, 13 disengagement outlet, 14 disengagement inlet, 15 body, 16 scraper hole, 17 spiral structure. DETAILED DESCRIPTION

[0026] The technical solution of the present application is further described in detail below through specific embodiments. In the present invention, unless otherwise specified, the raw materials and equipment used can be purchased from the market or are commonly used in the art. The methods in the following embodiments, unless otherwise specified, are all conventional methods in the art.

[0027] Embodiment 1: Based on the current domestic smooth aluminum sheath cable manufacturers, the split-type spraying system is basically adopted, which is usually composed of a heating cylinder, an air pump, a rubber guide tube, and a nozzle. This spraying system also has many technical problems. Mainly reflected in: 1. The spraying system device extracts the heated hot melt adhesive by the air pump, and then transports it through the rubber guide tube to the nozzle for spraying. During the transportation and spraying process, the temperature will be reduced, affecting the viscosity of the hot melt adhesive; 2. When the air pump extracts the hot melt adhesive, there is air when the nozzle sprays the hot melt adhesive, which forms tiny bubbles when it adheres to the surface of the smooth aluminum sheath, affecting the safety and stability of the cable operation.

[0028] Therefore, our company has designed a hot melt adhesive coating device for smooth aluminum sheathed power cables, through which the coating operation for smooth aluminum sheathed power cables can be improved.

[0029] The coating device includes a frame, a bottom plate is arranged on the frame, a hot melt device is arranged on the bottom plate, the hot melt device includes a hot melt cylinder for storing and heating hot melt adhesive, and the hot melt cylinder is equipped with a heating device, and the hot melt cylinder has two opposite side walls with hot melt inlet and hot melt outlet matching with the power cable; a wire support frame is arranged outside the hot melt inlet for convenient entry of the power cable, and a scraping mechanism is arranged on the outer side wall of the hot melt cylinder at the hot melt outlet, and also includes a temperature control device, which is electrically connected to the heating device. In order to facilitate the adjustment of the entry and exit height of the power cable, a lifting device is arranged on the frame, and the bottom plate is arranged on the lifting device.

[0030] The scraper mechanism comprises a body, a scraper hole is provided on the body, the scraper hole is a multi-section structure, and the scraper opening is reduced in sections or gradually from the inside to the outside.

[0031] Embodiment 2: In order to improve the bonding between the hot melt adhesive and the power cable, a disengagement mechanism for disengaging the power cable from the hot melt adhesive is provided between the hot melt inlet and the hot melt outlet of the hot melt cylinder. The disengagement mechanism is provided in the hot melt cylinder, and a disengagement outlet for the power cable to be output from the hot melt cylinder and a disengagement inlet for the power cable to re-enter the hot melt cylinder are provided on the side wall of the disengagement mechanism. The disengagement mechanism is used to divide the coating of the power cable into two stages, and the two-stage coating is used to improve the firmness and flatness of the attached drawing.

[0032] At the same time, the scraping mechanism is improved and designed, specifically, a spiral structure is set in the front half of the scraping hole. The spiral mechanism is used to homogenize the surface of the power cable that is about to leave the hot melt cylinder. Finally, a cold air mechanism is set outside the hot melt outlet to use cold air to reduce the temperature of the coating on the power cable and accelerate the molding.

[0033] Comparative Example:

[0034] Use spraying equipment to spray.

[0035] Then the samples of Example 1 and the comparative example were tested.

[0036] Appearance test:

[0037] The spraying equipment in the comparative example is filamentous when spraying and white after spraying, with visible tiny bubbles.

[0038] The coating device of this embodiment shows the original color after coating without tiny bubbles.

[0039] Bond strength test comparison:

[0040] 1. Take a 30cm cable sprayed with hot melt adhesive and put it into a 70℃ aging box. After 8 hours, take it out and place it in a room temperature environment for 16 hours to cool naturally. Cut the sheath together with the flat aluminum sheath longitudinally, take 3 narrow strips with a width of 10mm along the longitudinal direction of the sheath, and mark them as A1, A2, and A3 samples;

[0041] 2. Take a 30cm cable coated with hot melt adhesive and put it into a 70℃ aging box. After 8 hours, take it out and place it in room temperature for 16 hours to cool naturally. Repeat this operation 10 times. After 10 times, prepare samples according to the requirements of step 1 and mark them as B1, B2, and B3 samples.

[0042] 3. Sheath peel strength test:

[0043]

[0044] By comparison, it can be seen that after the hot melt adhesive is coated using the device of the present application, the smooth aluminum sheath and the non-metallic outer sheath are more fully bonded, and the bonding strength is increased.

[0045] It is obvious to those skilled in the art that the above embodiments are not intended to be exhaustive or limit the embodiments to the specific precise forms disclosed. It is obvious to those skilled in the art that certain modifications, combinations and variations can be made based on the above teachings.

Claims

1. A hot melt adhesive coating device for a smooth aluminum sheathed power cable, characterized in that: It includes a frame, a bottom plate is arranged on the frame, a hot melt device is arranged on the bottom plate, the hot melt device includes a hot melt cylinder for storing and heating hot melt adhesive, and the hot melt cylinder is equipped with a heating device, and hot melt inlets and hot melt outlets matching power cables are provided on opposite side walls of the hot melt cylinder; a wire support rack is arranged outside the hot melt inlet for convenient entry of power cables, a scraping mold mechanism is arranged on the outer side wall of the hot melt cylinder at the hot melt outlet, and a temperature control device is also included, and the temperature control device is electrically connected to the heating device.

2. According to claim 1, a hot melt adhesive coating device for a smooth aluminum sheathed power cable is characterized in that: The frame is provided with a lifting device, and the bottom plate is provided on the lifting device.

3. The hot melt adhesive coating device for a smooth aluminum sheathed power cable according to claim 1, characterized in that: The hot melt cylinder is provided with a disengagement mechanism between the hot melt inlet and the hot melt outlet for disengaging the power cable from the hot melt adhesive. The disengagement mechanism is arranged in the hot melt cylinder, and a disengagement outlet for the power cable to be output from the hot melt cylinder and a disengagement inlet for the disengagement mechanism to re-enter the hot melt cylinder are arranged on the side wall of the disengagement mechanism.

4. A hot melt adhesive coating device for a smooth aluminum sheathed power cable according to claim 1, characterized in that: The scraper mechanism comprises a body, a scraper hole is provided on the body, the scraper hole is a multi-section structure, and the scraper opening is reduced in sections or gradually from the inside to the outside.

5. A hot melt adhesive coating device for a smooth aluminum sheathed power cable according to claim 4, characterized in that: A spiral structure is arranged in the front half of the scraper die hole.

6. A hot melt adhesive coating device for a smooth aluminum sheathed power cable according to claim 1, characterized in that: A cold air mechanism is arranged outside the hot melt outlet.