Seawater desalination and recovery integrated device based on self-floating solar photo-thermal evaporator

Through the three-dimensional evaporator of MXene precipitate/polyvinyl alcohol/sodium alginate composite aerogel, the problems of high cost, low efficiency and poor salt resistance in seawater desalination are solved, and efficient and stable seawater desalination is achieved. Suitable for remote areas.

CN222034673UActive Publication Date: 2024-11-22QINGDAO UNIV
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202420248441.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-01
Publication Date
2024-11-22
Estimated Expiration
2034-02-01

AI Technical Summary

Technical Problem

In the existing seawater desalination technology, the evaporator has high cost, low photothermal conversion efficiency, poor salt resistance, and low MXene preparation process efficiency, resulting in the failure of MXene precipitates to be effectively applied to seawater desalination.

Method used

Using MXene precipitate/polyvinyl alcohol/sodium alginate composite aerogel as photothermal material, a three-dimensional evaporator with vertical porous channel structure is prepared by directed freezing, and a cotton swab is combined as a water transmission channel to realize a self-floating solar photothermal evaporator seawater desalination and recycling integrated device.

Benefits of technology

It improves the photothermal conversion efficiency, evaporation rate and salt resistance, reduces costs, and achieves effective seawater desalination in remote mountainous areas and islands, while maintaining stable performance in oil pollution and extreme environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222034673U_ABST
    Figure CN222034673U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of seawater desalination, in particular to a seawater desalination and recovery integrated device based on a self-floating solar photo-thermal evaporator, which comprises a collecting box and a water guide plate obliquely arranged at the top of the collecting box, and a partition plate for dividing the collecting box into a seawater containing area and a fresh water collecting area is arranged in the collecting box. The MXene sediment / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator is arranged in the seawater containing area, the MXene sediment is used as a photo-thermal material, the raw material of MXene is fully utilized, excellent photo-thermal conversion efficiency, evaporation rate, salt resistance and biological / oil stain / special environment resistance are achieved in actual seawater desalination, and the cost is also reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of seawater desalination, in particular to a seawater desalination and recovery integrated device based on a self-floating solar thermal evaporator. Background Art

[0002] Freshwater shortage is a problem that humans have always faced, especially in remote mountainous areas and islands where electricity is scarce. Solar desalination technology is of great significance in solving the problem of freshwater shortage on islands and the desalination of brackish water in remote water-scarce areas where electricity is not accessible. With the rapid development of the world economy, the increasing population and urban expansion, poor management of freshwater resources and water pollution have caused a shortage of freshwater resources. Desalination and collection of seawater is one of the most important and effective ways to obtain fresh water.

[0003] At present, the water purification products on the market mainly use filtration to separate and obtain pure water. The filter membranes are mainly divided into: ion exchange membrane, RO reverse osmosis membrane and ultrafiltration membrane. The filter element components with the filter membrane as the core usually need to be replaced after a period of use (3-24 months). This kind of filtration method of water purifier not only has expensive filter consumables, but also requires external electric energy to assist in operation. Therefore, there is an urgent need for a green and environmentally friendly water purifier to meet the demand for pure drinking water in remote mountainous areas, independent islands and outdoor travel. In recent years, solar-driven interfacial water evaporation technology has attracted widespread attention from academia and industry. It can achieve eco-friendly, low-cost, safe, and independent of electricity desalination of seawater, and is considered to be an excellent choice for producing pure water, becoming one of the most promising ways to alleviate the imminent freshwater shortage crisis.

[0004] For interfacial solar evaporation systems, researchers usually focus on the selection of evaporator materials, water transport channels and evaporator structure design. The development of interfacial solar evaporator materials is diverse, and the research on materials such as nanofiber membranes, fabrics, sponges, hydrogels, and aerogels has been vigorously developed. Among them, aerogel-based materials are one of the emerging materials for solar steam. The ultra-high porosity can make the gas captured in the polymer network inhibit the collapse of the three-dimensional structure, thus having high mechanical strength. At the same time, the advantages of high specific surface area, low packing density and extremely low thermal conductivity make aerogel an ideal choice for evaporators in interfacial solar evaporation systems. However, the disordered pores in aerogels are not conducive to water transport by capillary force, and the mechanical brittleness of aerogels also hinders its development. Water transport channels play a key role in achieving efficient and continuous water evaporation in interfacial solar evaporators. The disordered and interconnected porous structure in the traditional three-dimensional water transport channel uses capillary force as a driving force to transport water to the surface of the evaporation layer. However, since the three-dimensional water channel is directly connected to the water body, it is difficult to avoid energy loss during the transmission process, which greatly weakens the thermal localization effect.

[0005] Photothermal materials, as materials for absorbing and converting solar energy, have been widely studied by scientific researchers in recent years, mainly including semiconductors, metal nanoparticles, carbon-based composites and organic conjugated polymers. The photothermal mechanisms of these materials can be divided into electron-hole generation and relaxation, plasma localized heating and molecular thermal vibration. However, many materials still have problems such as low photothermal conversion efficiency, insufficient energy management and poor hydrophilicity that plague researchers. The two-dimensional nanomaterial MXene has the advantages of good mechanical stability, rich types, adjustable thermal radiation loss and easy control of optical properties. However, the preparation or processing of MXene has problems such as high cost, low yield or additional functional treatment, which limits its application in seawater desalination.

[0006] CN111422873B discloses a MXene / sodium alginate derived carbon three-dimensional aerogel and its preparation method and application. The preparation method of the MXene / sodium alginate derived carbon three-dimensional aerogel provided by the present invention comprises the following steps: mixing a MXene dispersion and a sodium alginate aqueous solution in liquid phase to obtain a MXene / sodium alginate mixed solution; adding a calcium chloride solution to the MXene / sodium alginate mixed solution to gel the sodium alginate to obtain a MXene / sodium alginate hydrogel; carbonizing the sodium alginate by high temperature treatment, and then washing with 1-3 mol / L hydrochloric acid and deionized water to obtain a MXene / sodium alginate derived carbon three-dimensional aerogel material. The MXene / sodium alginate derived carbon three-dimensional aerogel material provided by the above patent has good electrochemical performance when used in the field of supercapacitors. However, due to the common problem of low efficiency in the production process of MXene on the market, some MXene precipitate "garbage" is produced. These MXene precipitates (MS) are composed of unetched MAX and unpeeled multilayer MXene (m-MXene) and a small amount of residual single-layer / few-layer MXene. Currently, MXene precipitates have been widely studied in supercapacitors, electromagnetic shielding and smart wearables. It is worth noting that these "junk" MS are also excellent photothermal conversion materials, but there is no research on their application in seawater desalination.

[0007] CN110655135A discloses a water collection device integrating seawater desalination and atmospheric water collection, including a super-affinity absorber, a seawater container, a fresh water container, a transparent cover and a bracket; the surface of the super-affinity absorber is a super-affinity pattern composed of a super-hydrophilic area and a super-hydrophobic area; when used for seawater desalination, the super-affinity absorber floats on the seawater surface of the seawater container, and the transparent cover covers the seawater container, the fresh water container and the super-affinity absorber; the top of the transparent cover is set as an inclined surface, and the height of the top of the transparent cover above the fresh water container is lower than the height of the top of the transparent cover above the seawater container; when used for atmospheric water collection, the super-affinity absorber is fixed on the bracket, and the fresh water container is located below the super-affinity absorber. The above patent integrates the dual functions of seawater desalination and atmospheric water collection, and can realize the all-weather wide-area operation of fresh water collection, which is expected to enable people to obtain fresh water in various regions and climates, and to a certain extent alleviate the fresh water crisis in today's society. However, the long-term stability of the evaporator in a complex environment is the key to realizing the large-scale practical application of solar evaporation technology. The excellent salt and oil resistance of the evaporator is the key factor that determines the long-term stable evaporation of the evaporator. Therefore, how to solve the problems of reducing costs, increasing light-to-heat conversion efficiency, improving water evaporation efficiency and salt resistance, and realizing industrial application, is an urgent problem that plagues technicians in the field of seawater desalination and sewage treatment. Summary of the invention

[0008] In view of the shortcomings of the above-mentioned prior art, an integrated seawater desalination and recovery device based on a self-floating solar thermal evaporator is provided. MXene precipitates are used as photothermal materials, which fully utilizes the raw materials of MXene. In actual seawater desalination, excellent photothermal conversion efficiency, evaporation rate, salt resistance and resistance to biological / oil pollution / special environments are achieved, and costs are also reduced.

[0009] In order to solve the above technical problems, the technical solution adopted by the utility model is a seawater desalination and recovery integrated device based on a self-floating solar thermal evaporator, comprising a collecting box and a water guide plate inclined at the top of the collecting box, a partition plate for partitioning the collecting box into a seawater holding area and a fresh water collection area is provided in the collecting box, a MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator is provided in the seawater holding area, the MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator comprises a heat-insulating carrier for floating on the surface of seawater, a high evaporation rate, salt-resistant three-dimensional aerogel body composed of continuous vertically arranged porous channels formed by directional freezing of polyvinyl alcohol, sodium alginate and MXene precipitates, the side temperature of which is lower than the ambient temperature and the surface of which has a stable water film layer is provided on the upper surface of the heat-insulating carrier, holes are arrayed on the heat-insulating carrier, and a water guide for contacting the three-dimensional aerogel body is provided in each hole.

[0010] In the above-mentioned integrated seawater desalination and recovery device based on the self-floating solar thermal evaporator, the three-dimensional aerogel body has polygonal pores with an average pore size of about 10-70 μm.

[0011] The above-mentioned integrated seawater desalination and recovery device based on the self-floating solar thermal evaporator is characterized in that the channel wall thickness of the porous channel is 0.5-2 μm.

[0012] The above-mentioned integrated desalination and recovery device based on the self-floating solar thermal evaporator has a vertically arranged channel with a width of 30-100 μm.

[0013] In the above-mentioned integrated seawater desalination and recovery device based on the self-floating solar thermal evaporator, the heat insulation carrier is made of polypropylene material, and the diameter of the hole is 0.5 cm.

[0014] In the above-mentioned integrated desalination and recovery device based on the self-floating solar thermal evaporator, the heat insulation carrier has a density of 0.9g / cm 3 Polypropylene material.

[0015] In the above-mentioned integrated seawater desalination and recovery device based on the self-floating solar thermal evaporator, the height of the three-dimensional aerogel body is 2.5 cm-3.5 cm.

[0016] In the above-mentioned integrated seawater desalination and recovery device based on the self-floating solar thermal evaporator, the water guide member is a cotton swab.

[0017] The beneficial effect of the integrated desalination and recovery device based on the self-floating solar thermal evaporator of the utility model is that a three-dimensional aerogel evaporator with vertical multi-sized pores composited with polyvinyl alcohol / sodium alginate (PVA / SA) and MXene precipitates is innovatively prepared, and a solar "self-floating steam condensation recovery device" is further designed and assembled. Cotton swabs are used as water transmission channels, and polypropylene is used as the support of the evaporator to float on the sea surface to ensure the normal operation of the evaporator. The photothermal water evaporation system with MXene precipitates as the main substrate can ensure long-term stable evaporation due to its strong water absorption. In addition, since the three-dimensional aerogel has a certain height, during the evaporation process, the side of the aerogel is used as a cold evaporation surface, and energy can be obtained from the environment through the temperature difference with the surrounding environment, further improving the evaporation rate and energy conversion efficiency of the evaporator. When the exposure height of the evaporator is 2.5 cm, the evaporation rate under one sun is as high as 3.6 kg m -2 h -1 , outdoor continuous 7-hour test can achieve 18.37kg m -2The evaporation amount. Through directional freezing, a solar evaporator with an anisotropic vertical channel structure was designed to support high-speed water transmission and promote bidirectional salt ion diffusion. Under natural light conditions, evaporation continued for 14 days without salt crystallization on the evaporator surface, showing excellent salt resistance. In addition, the superhydrophilicity imparted by SA and MXene forms a water film layer on its surface, giving the evaporator good oleophobic properties, and it can still maintain long-term stable evaporation performance even in oily seawater. In short, the vertical channel aerogel evaporator has the advantages of excellent evaporation performance, long-term stability in various environments, and waste resource utilization. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a structural schematic diagram of the utility model. DETAILED DESCRIPTION

[0019] The utility model is described in detail below with reference to the accompanying drawings and specific embodiments.

[0020] like Figure 1 As shown, an integrated desalination and recovery device based on a self-floating solar thermal evaporator comprises a collecting box 1, and a water guide plate 2 obliquely arranged on the top of the collecting box 1, a partition plate 5 for partitioning the collecting box 1 into a seawater receiving area 3 and a freshwater collecting area 4 is arranged in the collecting box, a MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator is arranged in the seawater receiving area 3, and the MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator comprises a heat-insulating carrier 7 for floating on the surface of seawater, a high evaporation rate and salt-resistant three-dimensional aerogel body 6 composed of continuous vertically arranged porous channels formed by directional freezing of polyvinyl alcohol, sodium alginate and MXene precipitates, the side temperature of which is lower than the ambient temperature and the surface of which has a stable water film layer is arranged on the upper surface of the heat-insulating carrier 7, holes are arrayed on the heat-insulating carrier 7, and a water guide 8 for contacting the three-dimensional aerogel body 6 is arranged in each hole.

[0021] Example 1

[0022] The same parts as those in Example 1 are not described in detail here. The difference between the present embodiment and Example 1 is that the preparation method of the above-mentioned integrated desalination and recovery device based on the self-floating solar thermal evaporator comprises the following steps:

[0023] (1) Dissolve 3.0 g LiF in 50 mL HCl solution and stir at room temperature for 10 min;

[0024] (2) 2.5 g Ti 3 AlC 2 The powder was slowly added to the above mixture solution and stirred at 40 °C for 24 h;

[0025] (3) The etching solution was washed 7 times with deionized water, and the mixed solution was separated and centrifuged to make the pH value of the supernatant reach 6, and a clay-like precipitate was obtained on the inner wall of the centrifuge tube; the remaining clay-like precipitate on the inner wall of the centrifuge tube was mainly unetched MAX and unpeeled multilayer MXene (m-MXene) and residual single-layer / few-layer MXene, etc. These discarded precipitates were used as photothermal materials for preparing aerogel evaporators;

[0026] (4) Disperse it in 150 ml of deionized water, treat it with ultrasound, and centrifuge it at 3500 rpm for 1.1 hours. The supernatant is Ti 3 C 2 Tx;

[0027] (5) Stir 5 mL of 1 wt% PVA solution and 15 mL of 1 wt% SA solution at room temperature for 5 min, disperse 3.6 g of MXene precipitate in 20 mL of deionized water, then add it to the mixed solution, and drop 0.4 g of cross-linking agent. After mixing, stir magnetically for 3 h, and perform ultrasonic degassing after stirring.

[0028] (6) Pour the mixed solution into a customized mold and prepare a MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator by liquid nitrogen directional freezing;

[0029] (7) A collection box is made, a transparent plate is used as a water guide plate, and the water guide plate is tiltedly set on the top of the collection box. A partition plate is set in the collection box to divide the collection box into a seawater receiving area and a fresh water collection area. The MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator is placed on one side of the seawater receiving area.

[0030] In order to characterize the technical effect of the present invention, the above-mentioned product is recorded as PSMS-1, and PVA / SA composite aerogels, 2wt%-4wt% (PSMS-2, PSMS-3, PSMS-4) and composite aerogels with MXene precipitate content of 2.6g (PSMS-5) and 4.6g (PSMS-6) were prepared according to the same method as above.

[0031]

[0032] like Figure 1As shown, the evaporation device is composed of a water guide, a heat insulation carrier, and a three-dimensional aerogel body, wherein the water guide is a cotton swab. The cotton swab can ensure that the three-dimensional aerogel body can be adequately supplied with water, and it can be used as a one-dimensional water channel to transfer water to the three-dimensional aerogel body. Considering the heat loss during water transfer, the water transfer channel and the thermal management structure are separated. The application of the one-dimensional water channel greatly reduces the thermal radiation, thermal convection, and heat loss of water during the transfer process.

[0033] The heat insulation carrier has a density of only 0.9 g / cm 3 The polypropylene material is a non-woven fabric that can be used as an aerogel support to float on the water surface. Holes with a diameter of 0.5 cm are formed in an array in the polypropylene material, and cotton swabs are assembled in the holes. Finally, the three-dimensional aerogel is placed on the polypropylene material to contact the cotton swab to ensure that the aerogel can get sufficient water supply.

[0034] Solar steam generation testing

[0035] Solar radiation was simulated using a solar simulator (CEL-PE300L-3A, xenon lamp) with an AM1.5G filter, and the light density of the solar irradiation was determined using an auxiliary detector (CEL-NP2000, optical power meter, China). The light density on the sample was adjusted by controlling the power and light distance of the solar simulator. The size of the spot was controlled by the aperture to ensure that the size of the spot was equal to the size of the sample. Each sample was irradiated for 60 minutes, and the mass change was measured in real time using a computer-connected electronic balance (accuracy 0.1 mg), and the temperature was measured using an infrared camera. The experiment was carried out at an ambient temperature of 24°C to 25°C and a humidity of 55% to 60%. The water evaporation rate under one sun irradiation was calculated by the change in real-time water evaporation mass recorded by the balance (Table 2). Generally, the evaporation area (Ae) of a material is equal to the light projection area (Ap). Therefore, the evaporation rate V can be calculated by the following formula:

[0036]

[0037] Where m is the mass of evaporated water and t is the illumination time. M is the mass of evaporated water, expressed as the slope of the mass loss curve obtained by linear fitting at steady state.

[0038] Sample characterization

[0039] The morphology and surface chemical composition of the composite aerogel were studied by scanning electron microscopy (SEM). The chemical structure of the prepared samples was characterized by X-ray diffractometer. The water contact angle of the aerogel was measured by contact angle meter. The optical transmittance and reflectance spectra of the fabric were measured using UV-Vis-NIR spectrometer (UV-3600) with an integrating sphere. According to Kirchhoff's law, the absorbance (A) was calculated from the reflectance (R) and transmittance (T), and the calculation formula was A=1-RT.

[0040] Structural characterization of MXene precipitate composite aerogel evaporator

[0041] Inspired by the transpiration of natural wood, a three-dimensional evaporator ( Figure 1 ). In the process of preparing MXene, Ti 3 AlC 2 After etching, centrifugation and ultrasonic treatment, high-quality single-layer / multilayer Ti 3 C 2 T x MXene nanosheets (supernatant), a large amount of sediment will still remain at the bottom. Through transmission electron microscopy (TEM), we found that MS contains unetched MAX phase, as well as multilayer and single-layer MXene nanosheets after etching, proving the coexistence of MAX phase, m-MXene and MXene layers in MS. MXene precipitates with broadband light absorption ability can effectively increase the absorption of sunlight as photothermal materials and convert it into heat. PVA and SA make the aerogel have better mechanical properties and hydrophilicity. PSMS aerogel was prepared by directional freezing with liquid nitrogen and then freeze drying. During the directional freezing process, a large number of ice crystals grow vertically from the bottom of the mold to the top, the suspension squeezes each other at the interface of the ice crystals, and water molecules as pore formers and spacers spontaneously assemble into a porous structure. The vertically arranged porous channels not only reduce the heat loss of water during transmission and improve the efficiency of photothermal conversion, but also enable the rapid evaporation of water vapor at the interface.

[0042] The morphology of the prepared PSMS aerogel was observed by scanning electron microscopy (SEM). Unlike the disordered and interconnected porous structures of previously reported aerogels, the PSMS aerogel has a clear layered and orderly structure. The SEM image shows that the aerogel has polygonal pores with an average pore size of about 10-70μm. The MXene precipitate, sodium alginate and viscous PVA polymer interweave to form a channel wall of 0.5-2μm. The formation of its morphology is due to the combined effect of the two-dimensional structure of the MXene precipitate and the extrusion of ice crystals during the freezing process. The PSMS aerogel also forms vertically arranged channels with a width of 30-100μm during the freeze-drying process. These parallel lamellar channel walls form short-range ordered micro-regions. This may be due to the unidirectional growth of ice crystals during the freezing process. The MXene precipitate flakes are arranged vertically along the growth direction of the ice crystals by mechanically shearing the MS disc-like lamellar liquid crystal phase. The cross-linked areas in the center of these micro-regions are composed of interconnected pore walls, PVA and SA bonding points, which are connected to form a continuous vertically arranged microchannel structure. EDS images show that C, O, Ti, and F are distributed on the fiber surface. C and O elements come from MXene precipitates, PVA, and SA, while Ti and F elements only come from MXene precipitates. The uniform distribution of C, O, Ti, and F elements in the entire area verifies the uniform distribution of MXene precipitates in the porous PVA and SA network structure. 3 AlC 2 Phase, Ti 3 C 2 T x , XRD patterns of MXene precipitates and PSMS-3 aerogel, Ti 3 AlC 2 The phase has two strong characteristic peaks at 9.45° and 38.89°. After etching, Ti 3 AlC 2 The characteristic peak of 38.89° changes from 9.45° to 6.78°, and the characteristic peak of 38.89° almost disappears, indicating that the Al layer in the MAX phase is etched away to form Ti 3 C 2 T x (MXene). The remaining precipitate after the successful preparation of MXene is MXene precipitate, which has characteristic peaks at 6.78°, 9.53° and 39°, further verifying that the remaining incompletely peeled multilayer Ti in the precipitate 3 C 2 T x, unetched MAX phase, MXene, etc. PSMS aerogel was prepared by compounding MXene precipitate with PVA and SA. The characteristic peak at 6.78° disappeared after the addition of SA and PVA, and the characteristic peak intensity at 39° weakened, indicating that the MXene precipitate has been evenly compounded in the aerogel. The ultra-light property of PSMS is that the aerogel with a diameter of 2cm and a height of 2.5cm stays on the wheat awn without causing any deformation. At the same time, the weight comparison before and after the aerogel absorbs water shows that PSMS aerogel has the excellent characteristics of low density and high porosity.

[0043] Hydrophilicity, light absorption and thermal management properties of MXene precipitate composite aerogel evaporator

[0044] During the evaporation process, the wettability of the material and the efficient water transport play an important role in the generation of solar-driven interfacial steam. It only takes 2.5s for the water droplets to be completely absorbed by the PSMS composite aerogel (Fig. 3a). This is because SA contains a large number of carboxyl and hydroxyl groups, and the hydrogen bonding between SA and PVA further improves the water absorption performance of the aerogel. In addition, the MXene precipitate also has good hydrophilicity, and the loose vertical pores in the aerogel form a good wicking effect, which can improve the water transport capacity of the aerogel. In order to highlight the effect of the channel structure on the water transport performance in this study, aerogels with disordered channels were made for comparison. According to the transport height of dyed water within 8s, the water transport height of the vertical channel aerogel frozen by liquid nitrogen is significantly higher than that of the disordered channel aerogel frozen by a refrigerator. Therefore, the PSMS composite aerogel can quickly transport water to the upper surface of the evaporator, thereby ensuring efficient water supply during the evaporation process.

[0045] In order to evaluate the light absorption capacity of MXene precipitate composite aerogels, the absorption spectra of aerogels prepared with different contents of MXene precipitates in the ultraviolet visible near infrared (UV-Vis-NiR) range were compared. The wet MXene precipitate composite aerogels showed low transmittance (≈0%) and reflectivity in the range of 300nm-2500nm. Among them, the PSMS-5 evaporator with the lowest precipitate content had a light absorption rate of 96%; the PSMS-6 MXene precipitate aerogel with the highest content had an absorbance of up to 98%. The excellent light absorption of PSMS is the combined effect of the strong absorption of MXene precipitates and vertical porous channels. The MXene precipitates on the surface of the aerogel can induce light to reflect or transmit, and absorb the internal light into the vertically arranged channels.

[0046] Efficient photothermal conversion is very important for the evaporation performance of solar evaporators. Subsequently, the photothermal conversion performance of aerogels was tested and studied. The excellent sunlight absorption and photothermal conversion capabilities of MXene precipitates enable them to generate a large amount of heat under sunlight. At the same time, the design of the directional frozen porous structure can better limit the heat on the surface of the evaporator, further improving the efficiency of photothermal conversion. The infrared thermal imager measured 1kW m -2 The surface temperature of the aerogel in dry and wet states under illumination. It can be observed that the surface temperature of the evaporator rises rapidly in the dry state, reaching 68.5°C within 210s; in the wet state, the composite aerogel reaches 26.7°C within 200s, indicating that the excellent light absorption performance of the evaporator and the plasma localized heating effect of MS give it good photothermal conversion performance. More importantly, the evaporator works in a wet state during the evaporation process. The side temperature of the PSMS aerogel in a wet state is only 16.2°C, which is much lower than the ambient temperature of 22.6°C. Therefore, the process of water transport from bottom to top not only eliminates the impact of heat loss, but also absorbs heat in the environment. This energy mainly comes from the heat transfer of air convection and radiation coupling, which shows that the PSMS aerogel evaporator has excellent thermal management performance.

[0047] In the dry state, the thermal conductivity of the horizontal and vertical sections is 0.0404 W m -1 k -1 and 0.0445W m -1 k -1 , but after wetting they increase to 0.1786 W m -1 k -1 and 0.1829W m -1 k -1This is because the medium in the pores changes from air to water, so the thermal conductivity increases. The lower thermal conductivity in the dry and wet states indicates that this study has excellent thermal insulation, which is conducive to the formation of "local heating" during the evaporation process. The dry aerogel evaporator was placed on a hot plate at 80°C for 1h. As time goes by, the temperature at the top of the aerogel has been maintained at around 28°C, and the temperature difference between the bottom and top of the aerogel is around 52°C, indicating that the evaporator has good thermal insulation and excellent thermal localization. In actual seawater desalination applications, the sun will rotate over time, so the absorption capacity of sunlight at different incident angles is another important factor in the preparation of high-efficiency solar evaporators. Under 1 simulated sunlight, according to the infrared image of the surface temperature of the evaporator at different incident angles, it can be observed that as the angle between the vertical direction of the aerogel and the incident direction of the sunlight increases from 30° to 70°, the surface temperature of the evaporator does not change much and stabilizes between 50°C and 60°C. At a larger incident angle, the surface temperature of the composite aerogel decreases slightly, which is caused by the gradual reduction of the illumination projection area, indicating that the PSMS evaporator has low dependence on the illumination direction and has good photothermal conversion stability. In addition, in order to verify the accuracy of the heat transfer model, COMSOL Multiphysics simulated the rapid heating process of the dry and wet PSMS-1 evaporator surface within 5 minutes (Fig.3f, Fig.). The numerical model is in good agreement with the experimental data, proving the accuracy of the heat transfer model. The above results show that the PSMS3D aerogel evaporator in this study has excellent thermal localization and thermal barrier properties, which will reduce the heat loss of water during evaporation and improve the energy utilization of photothermal conversion.

[0048] Study on the photothermal water evaporation performance of MXene precipitate composite aerogel evaporator

[0049] For a three-dimensional evaporator, the evaporation rate is affected by many factors. An electronic balance (accuracy 0.1 mg) connected to a computer is used to measure the mass change in real time. The water mass change during the evaporation process of the same content of MXene precipitate and different concentrations of aerogel under 1 sun irradiation. The evaporation rate of the PSMS-4 evaporator is 3.2 kg m -2 h -1 The evaporation rate of PSMS-3 evaporator reached 3.35 kg m -2 h -1 The evaporation rate of PSMS-2 evaporator is 3.5 kg m -2 h -1 The evaporation rate of PSMS-1 evaporator is 3.6 kg m -2. As the aerogel concentration decreases, the evaporation rate actually increases. This is because as the aerogel concentration decreases, the water content in the solution increases. During the liquid nitrogen directional freezing process, ice crystals grow vertically from bottom to top. The more water acts as a spacer, the larger the pore size inside the aerogel evaporator after freeze-drying. These pores provide good conditions for water transfer and thermal radiation conduction inside the evaporator, resulting in increased evaporation. Next, the water mass changes of evaporators with different contents of MXene precipitates under 1 sun irradiation were investigated. Under simulated solar irradiation, the evaporation rates of evaporators with MS contents of 2.6, 3.6, and 4.6 g were 3.4, 3.6, and 3.9 kg m, respectively. -2 h -1 , which indicates that the higher the MS content, the better the evaporation effect. This is attributed to the fact that MXene precipitates have rich active groups and high specific surface area, which can efficiently absorb sunlight and convert it into heat, improving the thermal localization effect on the surface of the evaporator. Therefore, the stronger the photothermal conversion ability, the higher the evaporation rate. It can be found that the relationship between the evaporation rate and the MXene precipitate is not a linear growth. Therefore, while ensuring the evaporation rate, in order to save the manufacturing cost of the evaporator, the aerogel with a MXene precipitate content of 3.6g was selected as the subsequent experimental concentration.

[0050] For 3D evaporators, the side area also plays a crucial role in the evaporation rate of seawater desalination. PSMS evaporators with a diameter of 0.75 cm, 1.5 cm, 2.5 cm, and 3.5 cm were designed with a concentration of 1 wt% and a content of 3.6 g MS, and the water evaporation rate under one sun irradiation was measured. With the increase of height, the evaporation rate increased from 3.1 kg m -2 h -1 Increased to 4.0kgm -2 h -1 . This is mainly because the side wall area of ​​the 3D evaporator provides an additional water / air interface while maintaining the same projected area. The evaporation of the side surface of the evaporator in a wet state causes its temperature to be lower than the ambient temperature, which is beneficial for obtaining additional energy from the surrounding environment. At the same time, the side surface of the PSMS evaporator can also reduce the average temperature of the top surface, greatly reducing the heat loss from top convection and thermal radiation. In order to save manufacturing costs, an evaporator with a height of 2.5 cm was further selected to investigate the water evaporation rate of the PSMS aerogel under different light intensities. The evaporation rates of the PSMS aerogel under 1, 2, 3, and 4 suns were 3.6, 5.9, 7.8, 9.7, and 11 kg m, respectively. -2 h -1The experimental results show that the evaporation rate increases with the increase of light intensity. Even under high sunlight, the evaporator has a stable and excellent evaporation rate. The durability and long-term stability of the PSMS evaporator were tested. Obviously, the prepared evaporator showed excellent recyclability and strong durability. Even under 10 light cycles, its evaporation rate was basically stable at 3.6 kg m -2 h -1 about.

[0051] In the application of seawater desalination, the salt deposition layer not only increases the reflection of sunlight, blocks the transmission speed of water, and causes the evaporation rate to decrease, but also seriously affects the service life of the evaporator. Therefore, the salt resistance of the evaporator is crucial in the application process, and it is also the key to the long-term efficient and stable operation of the evaporator. Large-scale preparation, continuous steam generation, and high-productivity evaporation systems are still a challenge. Therefore, the design of a new type of solar evaporator with salt resistance is very necessary for the interfacial solar desalination evaporation system technology. In order to study the salt resistance of the evaporator, PSMS-1 aerogel was used to test the evaporation rate at different salt concentrations. The evaporation rate of PSMS1 aerogel in pure water, 3.5%wt seawater and 20%wt salt solution can be maintained at approximately 3.5kg m -2 h -1 Under one sun, the evaporator was cycled 10 times in 3.5%wt seawater and 20%wt salt solution, and the evaporation rate remained stable at 3.3 kg m -2 h -1The above. Outdoor tests with natural seawater found that no salt crystals precipitated on the surface of the evaporator under 14 days of natural light. The above results show that the evaporator has a stable evaporation rate and excellent salt resistance even under long-term high salinity conditions. The salt resistance of the evaporator can be attributed to the vertically ordered microchannel structure formed by directional freezing, which enables the PSMS aerogel to continuously transport water to the evaporator surface as a supporting matrix under capillary action, while the anisotropic structure increases the ion exchange capacity between the channels. The liquid vapor on the surface of the evaporator evaporates under the action of efficient photothermal conversion to produce a concentration gradient, and gradually reaches saturation as the effective evaporation proceeds. The salt ions dissolved in the saturated solution will gradually flow back into the seawater along the water transport channel in the PSMS, which may be driven by the chemical potential difference between the saturated solution and the simulated seawater. When the whole system is combined, it can reach the equilibrium of a high-concentration salt solution and inhibit the precipitation of salt crystals. By comparison, the evaporation rate of the PSMS three-dimensional evaporator designed in this paper is significantly higher than that of most MXene three-dimensional evaporators reported so far. This is mainly attributed to its well-integrated structure, excellent thermal confinement, and timely upward water convection. It also proves the reliability and practicality of using "garbage" material MXene precipitates in the preparation of seawater desalination evaporators.

[0052] Application of MXene precipitate composite aerogel evaporator

[0053] The presence of organic pollutants such as oil in seawater is inevitable. In this case, oil may adhere to the surface of the evaporator to a certain extent, blocking the transmission channel of seawater and reducing the actual evaporation performance of the evaporator. Vegetable oil is used to simulate oil in seawater, and the contact angle with the evaporator underwater is 148°, showing excellent underwater superoleophobic properties. When vegetable oil is injected on the surface of the PSMS evaporator, it will immediately escape from the surface of the aerogel, and no oil droplets will adhere, which further proves the excellent anti-oil property of the PSMS evaporator. The superoleophobic property of the evaporator is because the superhydrophilic properties of SA and MXene in the PSMS aerogel form a highly stable water film layer on its surface, preventing oil from entering the aerogel. At the same time, the evaporation rate of the evaporator in extreme environments was also tested, using acidic, alkaline and oil-in-water emulsions to simulate domestic wastewater and industrial wastewater discharged into seawater. It can be found that the evaporation rates of the corrosion solutions with pH = 1 and pH = 12 are 3.2 and 3.3 respectively, and the evaporation rate of the emulsion is close to 3.6 with pure water, and no oil droplets appear in the purified condensed water. This shows that even under some harsh seawater conditions, PSMS can maintain stable evaporation performance and achieve efficient water purification. In order to avoid various epidemics caused by microorganisms such as bacteria, we selected representative Staphylococcus aureus and Escherichia coli to test the antibacterial effect of the evaporator. There was almost no bacterial growth on the solid agar plate of PSMS, indicating that it has superior antibacterial activity, and the antibacterial rate is higher than 99.9%. This is because the single-layer and multi-layer nanosheets in MS have hydrophilic and negatively charged surface properties, which increase the chance of contact with the cell membrane. The sharp edges of the nanosheets will destroy the bacterial membrane, causing the bacteria to die due to the leakage of a large amount of cytoplasmic components. Therefore, MS can effectively prevent the evaporator from being contaminated and corroded by microorganisms during long-term use.

[0054] In order to further evaluate the practical application of PSMS aerogel evaporator in seawater desalination under natural light, a collection box, a water guide plate and a partition plate were made of transparent acrylic plates, and then the collection box, the water guide plate and the partition plate were combined to form a condensation device. The water guide plate is detachably connected to the top of the collection box. Of course, it can also be made of glass or other transparent materials, or a condensation plate can be set on the bottom surface of the water guide plate to condense water vapor and guide water. The seawater evaporation effect of a PSMS evaporator with a height of 3.5 cm under outdoor natural sunlight was tested, and the surface temperature of the evaporator was recorded with an infrared camera. When the evaporator is working, the steam will condense into water droplets at the top and flow into the other side of the partition plate for collection. The PSMS evaporator was placed in the condensation device. The experimental time was 10:00-18:00. The test recorded the changes in ambient temperature, evaporator surface temperature, sunlight intensity and water quality. It can be observed that the surface temperature of the evaporator changes with the change of sunlight intensity. The sunlight intensity changes from 0.47kW m at 10 o'clock in the morning to 0.47kW m at 10 o'clock in the morning. -2The solar intensity gradually increased from 12 noon to 14 o'clock in the afternoon, and remained at 0.6 kW m -2 The surface temperature of the evaporator also increases with the increase of sunlight intensity, and then maintains at around 35°C, which is much higher than the actual ambient temperature. From 10:00 to 17:00, the total amount of fresh water collected by the PSMS evaporator condensation device is 18.37 kg m -2 . Real seawater was evaporated by PSMS evaporator and collected by condensation device. Due to the weak solar intensity, the evaporation rate was not as high as that measured in the laboratory. Water quality was directly evaluated by simple resistance value. The electrode distance was fixed and the ohm value was measured with a multimeter. The resistance values ​​of real seawater, domestic water and purified water were 0.07, 5.12 and 1.07 MΩ respectively, indicating that PSMS has excellent ability to purify seawater. Ca was tested before and after seawater purification using ICP-OES 2+ , K + Mg 2+ and Na + The concentration of metal ions after purification has dropped significantly, reaching the standards of the World Health Organization (WHO) and the U.S. Environmental Protection Agency (EPA) for drinking water salt content. This further shows that the purification system of the PSMS evaporator can obtain clean drinking water from seawater using photothermal interface evaporation technology, providing a new and effective way to solve the shortage of fresh water resources.

[0055] In summary, considering the problem of resource waste in the preparation process of MXene photothermal materials, this application designed and developed a PSMS three-dimensional evaporator using MXene precipitates as raw materials, and further assembled a condensed water collection device. In actual seawater desalination, excellent photothermal conversion efficiency, evaporation rate, salt resistance, and resistance to biological / oil pollution / special environments were achieved. The ordered porous structure of directional freezing is not only conducive to water transmission, but also can absorb light into the channel, maximizing the efficiency of photothermal conversion. The design of the three-dimensional structure increases the vapor diffusion at the air / water interface, and the side temperature is lower than the ambient temperature, which can absorb more heat in the environment and increase the dark evaporation on the side. The evaporation rate of the evaporator under 1 sun is 3.6 kg m -2 h -1 The evaporation capacity of the condensation collection device in the open air for 7 hours is as high as 21.87 kg m -2. At the same time, the unique anisotropic structure drives the chemical potential difference between the saturated solution and the simulated seawater to achieve the equilibrium of the high-concentration salt solution, promote convection and diffusion, and inhibit the precipitation of salt crystals. In addition, the water film layer on the surface of the PSMS aerogel prevents oil from entering the aerogel. The evaporator also has excellent antibacterial properties and can still maintain stable evaporation performance in seawater in extreme environments. Finally, the self-floating device is combined with the condensation collection device to solve the collection problem of seawater desalination. The purified water collected by condensation meets the standards of WHO and EPA, proving that the PSMS evaporator is a new way to develop a sustainable salt-resistant and efficient freshwater resource recovery device. Using MXene precipitates as photothermal materials makes full use of the raw materials of MXene, and in the future, the development of MXene precipitate-based evaporators will be expanded in the field of interfacial solar desalination evaporators.

[0056] Example 2

[0057] The preparation method of the above-mentioned integrated desalination and recovery device based on the self-floating solar thermal evaporator comprises the following steps:

[0058] (1) Dissolve 1 g of LiF in 2 mL of HCl solution and stir at room temperature for 5 min;

[0059] (2) 1gTi 3 AlC 2 The powder was slowly added to the above mixture solution and stirred at 20 °C for 10 h;

[0060] (3) The etching solution was washed 5 times with deionized water, and the mixed solution was separated and centrifuged to make the pH value of the supernatant reach 6, and a clay-like precipitate was obtained on the inner wall of the centrifuge tube; the remaining clay-like precipitate on the inner wall of the centrifuge tube was mainly unetched MAX and unpeeled multilayer MXene (m-MXene) and residual single-layer / few-layer MXene, etc. These discarded precipitates were used as photothermal materials for preparing aerogel evaporators;

[0061] (4) Disperse it in 50 ml of deionized water, treat it with ultrasound, and centrifuge it at 1000 rpm for 1 hour. The supernatant is Ti 3 C 2 Tx;

[0062] (5) Stir 1 mL of 1 wt% PVA solution and 5 mL of 1 wt% SA solution at room temperature for 2 min, disperse 2 g of MXene precipitate in 5 mL of deionized water, then add it to the mixed solution, and drop 0.2 g of cross-linking agent, mix and stir magnetically for 1 h, and perform ultrasonic degassing after stirring;

[0063] (6) Pour the mixed solution into a customized mold and prepare a MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator by liquid nitrogen directional freezing;

[0064] (7) A collection box is made, a transparent plate is used as a water guide plate, and the water guide plate is tiltedly set on the top of the collection box. A partition plate is set in the collection box to divide the collection box into a seawater receiving area and a fresh water collection area. The MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator is placed on one side of the seawater receiving area.

[0065] Example 3

[0066] The same parts as those in Example 1 are not described in detail here. The difference between the present embodiment and Example 1 is that the preparation method of the above-mentioned integrated desalination and recovery device based on the self-floating solar thermal evaporator comprises the following steps:

[0067] (1) Dissolve 5 g LiF in 2-1000 mL HCl solution and stir at room temperature for 50 min;

[0068] (2) 5gTi 3 AlC 2 The powder was slowly added to the above mixture solution and stirred at 60 °C for 30 h;

[0069] (3) The etching solution was washed 10 times with deionized water, and the mixed solution was separated and centrifuged to make the pH value of the supernatant reach 6, and a clay-like precipitate was obtained on the inner wall of the centrifuge tube; the remaining clay-like precipitate on the inner wall of the centrifuge tube was mainly unetched MAX and unpeeled multilayer MXene (m-MXene) and residual single-layer / few-layer MXene, etc. These discarded precipitates were used as photothermal materials for preparing aerogel evaporators;

[0070] (4) Disperse it in 200 ml of deionized water, treat it with ultrasound, and centrifuge it at 5000 rpm for 3 hours. The supernatant is Ti 3 C 2 Tx;

[0071] (5) Stir 10 mL of 1 wt% PVA solution and 30 mL of 1 wt% SA solution at room temperature for 10 min, disperse 6 g of MXene precipitate in 40 mL of deionized water, then add it to the mixed solution, and drop 0.8 g of cross-linking agent, mix and stir magnetically for 6 h, and perform ultrasonic degassing after stirring;

[0072] (6) Pour the mixed solution into a customized mold and prepare a MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator by liquid nitrogen directional freezing;

[0073] (7) A collection box is made, a transparent plate is used as a water guide plate, and the water guide plate is tiltedly set on the top of the collection box. A partition plate is set in the collection box to divide the collection box into a seawater receiving area and a fresh water collection area. The MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator is placed on one side of the seawater receiving area.

[0074] Of course, the above description is not a limitation of the present invention, and the present invention is not limited to the above examples. Any changes, modifications, additions or substitutions made by ordinary technicians in this technical field within the essential scope of the present invention should also fall within the protection scope of the present invention.

Claims

1. An integrated desalination and recovery device based on a self-floating solar thermal evaporator, characterized by: The invention comprises a collecting box and a water guide plate obliquely arranged on the top of the collecting box, wherein a partition plate for partitioning the collecting box into a seawater receiving area and a freshwater collecting area is arranged in the collecting box, and a MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator is arranged in the seawater receiving area, wherein the MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator comprises a heat-insulating carrier for floating on the surface of seawater, and a high evaporation rate and salt-resistant three-dimensional aerogel body composed of continuous vertically arranged porous channels formed by directional freezing of polyvinyl alcohol, sodium alginate and MXene precipitates, with a side temperature lower than the ambient temperature and a stable water film layer on the surface is arranged on the upper surface of the heat-insulating carrier, and holes are arranged in an array on the heat-insulating carrier, and a water guide for contacting the three-dimensional aerogel body is arranged in each hole.

2. The integrated desalination and recovery device based on the self-floating solar thermal evaporator according to claim 1 is characterized in that: The three-dimensional aerogel body has polygonal pores with an average pore diameter of about 10-70 μm.

3. The integrated desalination and recovery device based on the self-floating solar thermal evaporator according to claim 2 is characterized in that: The thickness of the channel wall of the porous channel is 0.5-2 μm.

4. The integrated desalination and recovery device based on the self-floating solar thermal evaporator according to claim 3 is characterized in that: The width of the vertically aligned channels is 30-100 μm.

5. The integrated desalination and recovery device based on the self-floating solar thermal evaporator according to claim 4 is characterized in that: The heat insulation carrier is made of polypropylene material, and the diameter of the holes is 0.5 cm.

6. The integrated desalination and recovery device based on the self-floating solar thermal evaporator according to claim 5 is characterized in that: The thermal insulation carrier has a density of 0.9 g / cm 3 Polypropylene material.

7. The integrated desalination and recovery device based on the self-floating solar thermal evaporator according to claim 5 is characterized in that: The height of the three-dimensional aerogel body is 2.5 cm-3.5 cm.

8. The integrated desalination and recovery device based on the self-floating solar thermal evaporator according to claim 5 is characterized in that: The water guide is a cotton swab.

Citation Information

Cited By

  • Seawater desalination and collection device based on MXene precipitate / polyvinyl alcohol / sodium alginate composite aerogel three-dimensional evaporator and preparation method of seawater desalination and collection device

    CN117861571A

  • Photo-thermal composite hydrogel solar evaporator and preparation method thereof

    CN120383356A