By setting a thin thickness and tightly fitting the support shell on the metal outer wall of the mold groove of the plastic product cooling mold, and using a solenoid valve to control the inflow and outflow of cold water, the problem of low cooling efficiency in the existing technology is solved, and efficient heat dissipation and Stable extrusion support.
Patent Information
- Application Number
- CN202421155272.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-24
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2034-05-24
AI Technical Summary
The cooling efficiency of existing plastic products cooling molds is poor, resulting in unsatisfactory heat dissipation effect.
By setting a thickness of 3-5mm on the metal outer wall of the mold groove and closely fitting the metal outer wall of the mold groove on the supporting shell to form a water injection cavity, the inlet and outlet solenoid valves are used to control the inlet and outflow of cold water to improve heat dissipation efficiency.
It improves the cooling and heat dissipation efficiency of plastic products, and provides stable extrusion support, ensuring the stability and shaping quality of the product in the mold groove.
Smart Images

Figure CN222039511U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of cooling and shaping molds, in particular to a cooling and shaping mold for plastic products. Background Art
[0002] The cooling shaping mold generally adds cooling equipment on the basis of the original shaping mold. For the cooling shaping mold of plastic products, generally, air cooling equipment or water cooling equipment is added on the basis of the original mold. The cooling shaping mold must not only maintain the original good shaping function, but also ensure a good cooling effect; as a result, many cooling shaping molds can also achieve cooling, but the cooling efficiency is poor. In order to solve the above problems, the utility model provides a cooling shaping mold for plastic products. Utility Model Content
[0003] In view of the above-mentioned technical deficiencies, the purpose of the utility model is to provide a cooling and shaping mold for plastic products, wherein the metal outer wall of the mold groove is set to 3-5mm, and the metal outer wall of the mold groove is tightly fitted to the supporting shell; after the supporting shell is separated from the metal outer wall of the mold groove, a water injection cavity is formed, and the water inlet solenoid valve and the water outlet solenoid valve are opened to realize cold water heat dissipation in the water injection cavity, thereby solving the technical problem of low cooling efficiency raised in the background technology.
[0004] In order to solve the above technical problems, the utility model adopts the following technical solutions: the utility model provides a cooling and shaping mold for plastic products, including a lower mold base and an upper pressing block; a mold groove is provided on the upper surface of the lower mold base; the upper pressing block matches the mold groove; when in use, the melted plastic is poured into the mold groove, and the upper pressing block first matches the mold groove under the drive of the second hydraulic rod, and then the upper pressing block presses the melted plastic to shape the product; an operating cavity is provided at the bottom of the lower mold base; a cooling ring cavity connected to the operating cavity is provided on the outside of the mold groove; in fact, the cooling ring cavity is located inside the lower mold base and surrounds the mold groove, so that cold water covers the outer periphery of the mold groove to realize cooling of the injection molded plastic product; the operating cavity is provided with a supporting shell; the supporting shell is matched and installed in the cooling ring cavity; generally In order to ensure the stability of the plastic product when it is extruded in the mold groove, the outer wall of the mold groove is relatively thick, and the thick outer wall also leads to slower cooling and heat dissipation; for this reason, in this embodiment, the metal outer wall of the mold groove is set to be relatively thin, generally 3-5mm, which can facilitate heat dissipation; at the same time, in order to ensure good support, the metal outer wall of the mold groove is tightly fitted to the support shell to provide stable extrusion support, which not only improves the heat dissipation efficiency but also provides stable support; a first hydraulic rod is installed at the bottom of the operating cavity; the output end of the first hydraulic rod is connected to the bottom of the support shell; the support shell and the metal outer wall of the mold groove are tightly fitted and separated by the extension and retraction of the first hydraulic rod; the left and right sides of the outside of the lower mold seat are respectively connected to the water inlet pipe and the water outlet pipe; the water inlet pipe and the water outlet pipe are both connected to the cooling ring cavity.
[0005] Preferably, the water inlet pipe is connected to the cold water outlet pipe of the chiller; the water outlet pipe is connected to the return pipe of the chiller; when the upper pressure block completes the extrusion of the plastic melt in the mold groove, the first hydraulic rod drives the support shell to separate from the metal outer wall of the mold groove. At this time, the support shell, the cooling ring cavity and the metal outer wall of the mold groove form a sealed water injection cavity, and the water inlet solenoid valve and the water outlet solenoid valve are opened to realize cold water heat dissipation in the water injection cavity, thereby improving the heat dissipation efficiency, which is convenient and efficient.
[0006] Preferably, a water inlet solenoid valve is provided on the water inlet pipe; and a water outlet solenoid valve is provided on the water outlet pipe.
[0007] Preferably, four support columns are installed on the top of the lower mold base; a support plate is installed on the top of the support columns; a second hydraulic rod is fixedly installed on the bottom surface of the support plate; and the output end of the second hydraulic rod is fixedly connected to the upper part of the upper pressure block.
[0008] Preferably, vertical slide bars are symmetrically installed on the two opposite side walls of the cooling ring cavity; vertical slide grooves are symmetrically opened on the opposite outer side surfaces of the support shell; the vertical slide bars are slidably matched with the vertical slide grooves; through the slidably matching of the vertical slide bars and the vertical slide grooves, the stability of the support shell sliding up and down is ensured.
[0009] The beneficial effects of the utility model are:
[0010] 1. The utility model sets the metal outer wall of the mold groove to 3-5mm, and at the same time, the metal outer wall of the mold groove fits tightly with the support shell; after the support shell is separated from the metal outer wall of the mold groove, a water injection cavity is formed, and the water inlet solenoid valve and the water outlet solenoid valve are opened to realize cold water heat dissipation in the water injection cavity, thereby improving the heat dissipation efficiency, which is convenient and efficient.
[0011] 2. The utility model ensures the stability of the support shell 3 sliding up and down by sliding matching between the vertical slide bar and the vertical slide groove. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0013] Figure 1 A schematic structural diagram of a cooling and shaping mold for plastic products provided in an embodiment of the utility model.
[0014] Figure 2 for Figure 1 main view.
[0015] Figure 3 for Figure 1 Top view of the .
[0016] Figure 4 for Figure 3 Sectional view of AA.
[0017] Figure 5 It is a vertical cross-sectional view of the utility model when the supporting shell and the cooling ring cavity are separated.
[0018] Figure 6 for Figure 3 Cross-sectional view of BB.
[0019] Figure 7 It is a structural schematic diagram of the mutual installation of the supporting shell and the first hydraulic rod in the utility model.
[0020] Explanation of the accompanying drawings: 1-lower mold base, 11-mold groove, 12-operating cavity, 13-cooling ring cavity, 131-vertical slide, 14-support column, 2-upper pressure block, 21-support plate, 3-support shell, 31-vertical slide, 4-first hydraulic rod, 5-water inlet pipe, 51-water inlet solenoid valve, 6-water outlet pipe, 61-water outlet solenoid valve, 7-second hydraulic rod. DETAILED DESCRIPTION
[0021] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0022] Embodiment 1:
[0023] like Figures 1 to 7As shown, this embodiment provides a cooling and shaping mold for plastic products, including a lower mold base 1 and an upper pressing block 2; a mold groove 11 is provided on the upper surface of the lower mold base 1; the upper pressing block 2 matches the mold groove 11, and four support columns 14 are installed on the top of the lower mold base 1; a support plate 21 is installed on the top of the support column 14; a second hydraulic rod 7 is fixedly installed on the bottom surface of the support plate 21; the output end of the second hydraulic rod 7 is fixedly connected to the upper part of the upper pressing block 2, and when in use, the melted plastic is poured into the mold groove 11, and the upper pressing block 2 is first matched with the mold groove 11 under the drive of the second hydraulic rod 7, and then the upper pressing block 2 presses the melted plastic to shape the product. An operating cavity 12 is provided at the bottom of the lower mold base 1; a cooling ring cavity 13 connected to the operating cavity 12 is provided on the outside of the mold groove 11. In fact, the cooling ring cavity 13 is located inside the lower mold base 1 and surrounds the mold groove 11, so that cold water covers the periphery of the mold groove 11 to achieve cooling of the injection molded plastic product. The operating cavity 12 is provided with a support shell 3; generally, in order to ensure the stability of the plastic product when it is extruded in the mold groove 11, the outer wall of the mold groove 11 is relatively thick, and the thick outer wall also leads to slower cooling and heat dissipation; for this reason, in this embodiment, the metal outer wall of the mold groove 11 is set to be relatively thin, generally 3-5mm, which can facilitate heat dissipation; at the same time, in order to ensure good support, the metal outer wall of the mold groove 11 is tightly fitted with the support shell 3 to provide stable extrusion support, which not only improves the heat dissipation efficiency but also provides stable support. The support shell 3 is matched and installed in the cooling ring cavity 13; the first hydraulic rod 4 is installed at the bottom of the operating cavity 12; the output end of the first hydraulic rod 4 is connected to the bottom of the support shell 3; the support shell 3 is tightly fitted and separated from the metal outer wall of the mold groove 11 by the extension and contraction of the first hydraulic rod 4. The left and right sides of the outer side of the lower mold seat 1 are respectively connected to the water inlet pipe 5 and the water outlet pipe 6; the water inlet pipe 5 and the water outlet pipe 6 are both connected to the cooling ring cavity 13. Specifically, the water inlet pipe 5 is connected to the cold water outlet pipe of the chiller; the water outlet pipe 6 is connected to the return pipe of the chiller, and a water inlet solenoid valve 51 is arranged on the water inlet pipe 5; a water outlet solenoid valve 61 is arranged on the water outlet pipe 6; in actual use, when the upper pressure block 2 completes the extrusion of the plastic melt in the mold groove 11, the first hydraulic rod 4 drives the support shell 3 to separate from the metal outer wall of the mold groove 11, and at this time, the support shell 3, the cooling ring cavity 13 and the metal outer wall of the mold groove 11 form a sealed water injection cavity, and the water inlet solenoid valve 51 and the water outlet solenoid valve 61 are opened to realize cold water heat dissipation in the water injection cavity, thereby improving the heat dissipation efficiency, which is convenient and efficient.
[0024] Embodiment 2:
[0025] See also Figures 5 to 7As shown, on the basis of retaining all the technical features in the specific embodiment 1, the cooling ring cavity 13 has vertical slide bars 131 symmetrically installed on the two opposite side walls; the support shell 3 has vertical slide grooves 31 symmetrically opened on the opposite outer side; the vertical slide bars 131 and the vertical slide grooves 31 are slidably matched, and the vertical slide bars 131 and the vertical slide grooves 31 are tightly matched and will not leak cold water. In actual use, the vertical slide bars 131 and the vertical slide grooves 31 are slidably matched to ensure the stability of the support shell 3 sliding up and down.
[0026] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A cooling and shaping mold for plastic products, characterized in that: It comprises a lower mold base (1) and an upper pressing block (2); a mold groove (11) is provided on the upper surface of the lower mold base (1); the upper pressing block (2) matches the mold groove (11); an operating cavity (12) is provided at the bottom of the lower mold base (1); a cooling ring cavity (13) connected to the operating cavity (12) is provided outside the mold groove (11); the operating cavity (12) is provided with a supporting shell (3); the supporting shell (3) is matched and installed in the cooling ring cavity (13); a first hydraulic rod (4) is installed at the bottom of the operating cavity (12); the output end of the first hydraulic rod (4) is connected to the bottom of the supporting shell (3); The left and right sides of the exterior of the lower mold base (1) are respectively connected to a water inlet pipe (5) and a water outlet pipe (6); the water inlet pipe (5) and the water outlet pipe (6) are both in communication with the cooling ring cavity (13).
2. The cooling and shaping mold for plastic products according to claim 1, characterized in that: The water inlet pipe (5) is connected to the cold water outlet pipe of the chiller; the water outlet pipe (6) is connected to the return water pipe of the chiller.
3. The cooling and shaping mold for plastic products according to claim 2, characterized in that: The water inlet pipe (5) is provided with a water inlet solenoid valve (51); and the water outlet pipe (6) is provided with a water outlet solenoid valve (61).
4. The cooling and shaping mold for plastic products according to claim 3, characterized in that: Four support columns (14) are installed on the top of the lower mold base (1); a support plate (21) is installed on the top of the support columns (14); a second hydraulic rod (7) is fixedly installed on the bottom surface of the support plate (21); the output end of the second hydraulic rod (7) is fixedly connected to the upper part of the upper pressing block (2).
5. The cooling and shaping mold for plastic products according to claim 4, characterized in that: The cooling ring cavity (13) has vertical slide bars (131) symmetrically installed on the two side walls thereof; the supporting shell (3) has vertical slide grooves (31) symmetrically opened on the outer side surfaces thereof; the vertical slide bars (131) are slidably matched with the vertical slide grooves (31).