Slurry pump impeller evanescent mode and production mold
By adjusting the parting surface of the impeller lost foam and setting a lightweight movable block, the problem of blade breakage caused by excessive movable block weight in the production of large slurry pump impellers was solved, achieving smooth demolding and improved production efficiency.
Patent Information
- Application Number
- CN202420311289.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-20
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-02-20
AI Technical Summary
During the production of lost foam casting for large slurry pump impellers, the blades are easily torn off due to the excessive weight of the live block, and the operation is difficult.
The parting surface of the impeller lost foam is adjusted to the center of the outlet flow channel. The first and second molds are made of high-hardness metal. Lightweight first and second movable blocks are set, and weight-reducing cavities are provided in the movable blocks to ensure that the upper and lower mold halves can be demolded smoothly.
This avoids the problem of blade breakage caused by excessive weight of the live block, reduces the difficulty of operation, and ensures the integrity and production efficiency of the lost foam casting of large slurry pump impellers.
Smart Images

Figure CN222058766U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of casting parts of slurry pumps, in particular to a lost foam and a production mold for a slurry pump impeller. Background Art
[0002] Slurry pump is an important equipment used for conveying abrasive slurry in industrial production. Its impeller is made of wear-resistant materials. The impeller blank is cast. In order to improve production efficiency and production quality, more and more slurry pump impellers are produced by lost foam casting.
[0003] When producing impeller blanks, you first need to use foam plastic to make an impeller lost mold (commonly known as a white mold because of its white color) that is similar in size and shape to the impeller blank. After applying refractory paint and drying, bury it in dry quartz sand for vibration shaping and pouring under negative pressure to vaporize the impeller lost mold. The liquid metal occupies the position of the impeller lost mold and forms the impeller blank after solidification and cooling.
[0004] The impeller lost foam is made of a mold. If the impeller lost foam adopts an integral demoulding method, it is difficult to completely demould the blades of the impeller lost foam as the blade shape is a spatial distortion, and it is difficult to design a live block of the mold, which is not advisable.
[0005] At present, when designing the production mold of the impeller lost foam, the junction between the rear cover and the blade is usually used as the parting surface. The impeller lost foam is divided into two parts and the molds are made separately. Then, the upper mold and the lower mold are made separately. After the upper mold and the lower mold are bonded, a complete impeller lost foam is formed.
[0006] The mold made using this solution also cannot be taken out of the mold directly because the blade shape is a spatially distorted shape. Therefore, a loose block is provided at the blade position of the mold so that the loose block and the upper mold, and the loose block and the lower mold can be removed from the mold together, and then the loose block can be removed and put back into the mold for reuse.
[0007] This is not a problem for the production of small slurry pump impellers, but when used for the production of large slurry pump impellers (such as impellers with a diameter greater than 500mm), the weight of the loose piece will be too large, making it difficult to remove the loose piece from the mold together with the lower mold. Since the lower mold is made of foam plastic, the excessive weight of the loose piece will cause the blades to be pulled too hard when they are removed from the mold, which will easily cause the blades to be torn off. At the same time, the excessive weight of the loose piece will also cause difficulty in operation. Utility Model Content
[0008] The technical problem to be solved by the utility model is to provide a lost foam and production mold for a slurry pump impeller, which are used to solve the problem that the impeller lost foam of a large slurry pump is easily torn off due to the excessive weight of the live block during production.
[0009] In order to solve the above technical problems, the technical solution adopted by the utility model is:
[0010] A slurry pump impeller lost mold, the parting surface of the impeller lost mold is a plane passing through the center of the impeller lost mold outlet flow channel, the plane is perpendicular to the axis of the impeller lost mold, and the plane divides the impeller lost mold into two parts, namely an upper half mold and a lower half mold spliced to each other.
[0011] Furthermore, the shapes of the upper blades of the upper half mold and the lower blades of the lower half mold are both spatially distorted shapes.
[0012] A production mold for a slurry pump impeller lost foam, used for producing a slurry pump impeller lost foam, includes a first mold for producing an upper half mold and a second mold for producing a lower half mold, wherein the shapes on both sides of a first blade reverse mold section of the first mold respectively correspond to the corresponding side shapes of the upper blade, and the shapes on both sides of a second blade reverse mold section of the second mold respectively correspond to the corresponding side shapes of the lower blade.
[0013] Furthermore, the first blade anti-module includes a first blade anti-module main body and an arc-shaped first movable block movably connected to the concave side of the first blade anti-module main body; the side of the first movable block corresponding to the first blade anti-module main body is perpendicular to the rear cover plate of the upper mold, and this side of the first movable block is tightly attached to the concave side of the first blade anti-module main body, and the shape of the other side of the first movable block corresponds to the shape of the corresponding side of the upper blade.
[0014] Furthermore, a weight reduction cavity is provided on a side of the first movable block corresponding to the first blade counter-module body.
[0015] Furthermore, the second blade anti-module includes a second blade anti-module main body and an arc-shaped second movable block movably connected to the concave side of the second blade anti-module main body; the side of the second movable block corresponding to the second blade anti-module main body is perpendicular to the front cover plate of the lower half mold, and this side of the second movable block is tightly attached to the concave side of the second blade anti-module main body, and the shape of the other side of the second movable block corresponds to the shape of the corresponding side of the lower blade.
[0016] Furthermore, a weight reduction cavity is provided on a side of the second movable block corresponding to the second blade counter-module body.
[0017] Furthermore, the first mold and the second mold are both made of high-hardness metal, and the material grade is ZL104.
[0018] The positive effects of the utility model are:
[0019] 1. The utility model improves the position of the existing impeller lost mold parting surface, adjusts the parting surface to the center position of the impeller lost mold outlet flow channel, and accordingly improves the first mold and the second mold, arranges a first loose block in the first mold, and arranges a second loose block in the second mold, thereby ensuring that the upper and lower molds of the impeller lost mold can be smoothly demolded. The weight of the first and second loose blocks is much smaller than the weight of the existing loose blocks, thereby avoiding the upper blades of the upper mold or the lower blades of the lower mold being torn off due to the excessive weight of the loose blocks when producing the impeller lost mold of a large slurry pump.
[0020] 2. A weight-reducing cavity is provided in both the first movable block and the second movable block, which can further reduce the weight of the first movable block and the second movable block, reduce the contact area between the first movable block and the first blade anti-module body and between the second movable block and the second blade anti-module body, make it easier for the first movable block and the first blade anti-module body and between the second movable block and the second blade anti-module body to stick tightly, reduce the difficulty of processing the matching surface between the first movable block and the first blade anti-module body and between the second movable block and the second blade anti-module body, and prevent the generation of gaps that cause foam plastic to enter between the first movable block and the first blade anti-module body or between the second movable block and the second blade anti-module body, thereby affecting the demolding of the upper mold or the lower mold. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 is a three-dimensional diagram of the first mold;
[0022] Figure 2 This is a schematic diagram of the upper half mold when it is ejected from the mold;
[0023] Figure 3 It is a stereogram of the first live block;
[0024] Figure 4 It is a three-dimensional picture of the impeller lost foam;
[0025] Figure 5 It is an exploded view of the impeller lost foam in the utility model;
[0026] Figure 6 is a three-dimensional diagram of the second mold;
[0027] Figure 7 This is a schematic diagram of the lower half mold when it is ejected from the mold;
[0028] Figure 8 It is a stereogram of the second live block;
[0029] Fig. 9 is a three-dimensional diagram of a second mold in the prior art;
[0030] Fig.10 It is a schematic diagram of the lower half mold being ejected in the prior art;
[0031] Fig.11 It is a stereogram of a live block in the prior art;
[0032] Fig.12 It is an exploded view of the impeller lost foam in the prior art;
[0033] In the figure:
[0034] 1. Rear cover; 2. Upper mold; 3. Lower mold; 4. Hub; 5. Blade; 6. Upper blade; 7. Lower blade; 8. First movable block; 9. First lower mold; 10. First upper mold; 11. Second lower mold; 12. Second upper mold; 13. Second movable block; 14. Weight reduction cavity; 15. First blade anti-module body; 16. Second blade anti-module body; 17. Front cover; 18. Loose block. DETAILED DESCRIPTION
[0035] like Fig.12 As shown in the figure, the impeller lost mold currently used to produce the impeller of the slurry pump consists of two parts, namely, the upper half mold 2 and the lower half mold 3. The parting surface is located at the rear cover plate 1 of the impeller lost mold. The upper half mold 2 includes the rear cover plate 1 and the hub, and the lower half mold 3 includes the front cover plate 17 and the blades 5. The center of the front cover plate 17 is the water inlet 14. After the upper half mold 2 and the lower half mold 3 are buckled and bonded, a shape as shown in the figure is formed. Figure 4 The impeller lost foam is shown.
[0036] The upper mold 2 has a simple shape and no space-distorted shape, so the first mold used for its production is not provided with a loose block. The lower mold 3 has a loose block 18 because its blade 5 is space-distorted. The shape of the loose block 18 is as follows: Fig.11 As shown. The lower half mold 3 adopts Fig. 9 The second mold shown in the figure is produced, and the second mold includes a second lower mold 11 and a second upper mold 12. Five second blade reverse mold bodies 16 are evenly distributed in the second lower mold 11 along the circumferential direction, and the movable block 18 is arranged on the second reverse mold body 16. Fig.10 As shown, when demolding, the water outlet 14 of the lower mold half 3 faces upward, and the movable block 18 is separated from the second lower mold 11 together with the lower mold half 3.
[0037] Example 1
[0038] This embodiment is improved on the basis of the above existing impeller lost foam, the parting surface of the impeller lost foam is moved downward, and the mold is also improved accordingly, as follows:
[0039] like Figure 4 and Figure 5As shown, a lost mold for an impeller of a slurry pump is provided. The parting surface of the lost mold for the impeller is a plane passing through the center of the water outlet flow channel of the lost mold for the impeller, and the plane is perpendicular to the axis of the lost mold for the impeller. The plane divides the lost mold for the impeller into two parts, namely, an upper mold 2 and a lower mold 3 which are spliced to each other. The upper mold 2 includes a rear cover plate 1, a hub 4 arranged at the top center of the rear cover plate 1, and five upper blades 6 evenly distributed on the bottom of the rear cover plate 1. The lower mold 2 includes a front cover plate 17 and five lower blades 7 evenly distributed on the front cover plate 17, and the shapes of the upper blades 6 and the lower blades 7 are both spatially distorted. The upper blades 6 and the lower blades 7 are correspondingly buckled and bonded to form a shape as shown in the figure. Figure 4 The complete impeller lost foam is shown.
[0040] like Figures 1 to 3 , Figures 6 to 8 As shown, a production mold of a slurry pump impeller lost foam is used to produce the above-mentioned slurry pump impeller lost foam, including a first mold for producing an upper half mold 2 and a second mold for producing a lower half mold 3. The shapes of both sides of the first blade reverse mold of the first mold correspond to the corresponding side shapes of the upper blade 6, and the shapes of both sides of the second blade reverse mold of the second mold correspond to the corresponding side shapes of the lower blade 7. The first mold and the second mold are both made of high-hardness metal, and the material grade is ZL104.
[0041] The first blade reverse module includes a first blade reverse module body 15 and an arc-shaped first movable block 8 movably connected to the concave side of the first blade reverse module body 15; the side of the first movable block 8 corresponding to the first blade reverse module body 15 is perpendicular to the rear cover plate 1 of the upper half mold 2, and this side of the first movable block 8 is tightly attached to the concave side of the first blade reverse module body 15, and the shape of the other side of the first movable block 8 corresponds to the shape of the corresponding side of the upper blade 6.
[0042] The first mold is composed of a first upper mold 10 and a first lower mold 9 which are buckled with each other, the buckling plane is located at the rear cover plate 1 , and the first blade counter-module body 15 is located in the first lower mold 9 .
[0043] The second blade anti-module comprises a second blade anti-module main body 16 and an arc-shaped second movable block 13 movably connected to the concave side of the second blade anti-module main body 16; the side of the second movable block 13 corresponding to the second blade anti-module main body 16 is perpendicular to the front cover plate 17 of the lower half mold 3, and this side of the second movable block 13 is tightly attached to the concave side of the second blade anti-module main body 16, and the shape of the other side of the second movable block 13 corresponds to the shape of the corresponding side of the lower blade 7.
[0044] The second mold is composed of a second upper mold 12 and a second lower mold 11 that are buckled with each other. The buckling plane is located at the front cover plate 17 , and the second blade counter-module body 16 is located in the second lower mold 11 .
[0045] Since the upper blade 6 of the upper mold 2 and the lower blade 7 of the lower mold 3 are both spatially distorted, in this embodiment, a first movable block 8 is provided in the first mold and a second movable block 13 is provided in the second mold, thereby ensuring that the upper mold 2 and the lower mold 3 can be smoothly demolded. The weight of the first movable block 8 and the second movable block 13 is much smaller than the weight of the existing movable block 18, thereby avoiding the upper blade 6 or the lower blade 7 being torn off due to the excessive weight of the movable block when producing the impeller lost mold of a large slurry pump.
[0046] Example 2
[0047] This embodiment is improved on the basis of embodiment 1, specifically:
[0048] like Figure 8 As shown, a weight reduction cavity 14 is provided on the side of the first movable block 8 corresponding to the first blade anti-module body 15, and the shape of the weight reduction cavity 14 corresponds to the shape of the first movable block 8, so that the first movable block 8 forms a thin-walled part, which can further reduce the weight of the first movable block 8, reduce the contact area between the first movable block 8 and the first blade anti-module body 15, make the first movable block 8 and the first blade anti-module body 15 more easily fit together, reduce the processing difficulty of the matching surface of the first movable block 8 and the first blade anti-module body 15, and prevent the generation of gaps that cause foam plastic to enter between the first movable block 8 and the first blade anti-module body 15.
[0049] Since the contact area between the first blade counter-module bodies 15 is reduced, it is easier to demold the upper half mold 2.
[0050] Example 3
[0051] This embodiment is improved on the basis of embodiment 2, specifically:
[0052] A weight reduction cavity 14 is also provided on a side of the second movable block 13 corresponding to the second blade counter-module body 16 .
[0053] The shape of the weight reduction cavity 14 corresponds to the shape of the second movable block 13, so that the second movable block 13 forms a thin-walled part, which can further reduce the weight of the second movable block 13 and the contact area between the second movable block 13 and the second blade anti-module body 16, making it easier for the second movable block 13 and the second blade anti-module body 16 to fit tightly, reducing the processing difficulty of the matching surface between the second movable block 13 and the second blade anti-module body 16, and preventing the generation of gaps that cause foam plastic to enter between the second movable block 13 and the second blade anti-module body 16.
[0054] Since the contact area between the second blade counter-module bodies 16 is reduced, it is easier to demold the lower half mold 3.
[0055] The above-mentioned embodiments describe the content in a relatively detailed and specific manner, expressing the preferred embodiments of the utility model, and are only used to illustrate the technical ideas and features of the utility model. The purpose is to enable technicians in the field to understand the content of the utility model and implement it accordingly, but it is not limited to the utility model. The patent scope of the utility model cannot be limited only by this embodiment, that is, any equivalent changes or modifications made to the spirit disclosed by the utility model, for researchers or technicians in the field, within the structure of the utility model, the local improvements within the system and the changes and transformations between subsystems are still within the patent scope of the utility model. At present, the technical solution of this application has been pilot-tested, that is, a small-scale experiment of the product before large-scale mass production; after the pilot test, a user survey was conducted in a small range, and the survey results showed that the user satisfaction was high; now it is preparing for the formal production of the product for industrialization, including intellectual property risk warning surveys.
Claims
1. A lost foam mold for a slurry pump impeller, characterized in that: The parting surface of the impeller lost mold is a plane passing through the center of the impeller lost mold outlet flow channel, which is perpendicular to the axis of the impeller lost mold and divides the impeller lost mold into two parts, namely an upper half mold (2) and a lower half mold (3) which are spliced to each other.
2. The lost foam mold of a slurry pump impeller according to claim 1, characterized in that: The shapes of the upper blade (6) of the upper half mold (2) and the lower blade (7) of the lower half mold (3) are both spatially distorted shapes.
3. A production mold for a slurry pump impeller lost foam, used for producing a slurry pump impeller lost foam according to claim 2, characterized in that: It comprises a first mould for producing an upper half mould (2) and a second mould for producing a lower half mould (3), wherein the shapes of two sides of a first blade reverse mould block of the first mould respectively correspond to the corresponding side shapes of an upper blade (6), and the shapes of two sides of a second blade reverse mould block of the second mould respectively correspond to the corresponding side shapes of a lower blade (7).
4. The lost foam production mold for a slurry pump impeller according to claim 3, characterized in that: The first blade reverse module comprises a first blade reverse module body (15) and an arc-shaped first movable block (8) movably connected to a concave side of the first blade reverse module body (15); a side of the first movable block (8) corresponding to the first blade reverse module body (15) is perpendicular to the rear cover plate (1) of the upper half mold (2), the side of the first movable block (8) is tightly attached to the concave side of the first blade reverse module body (15), and the shape of the other side of the first movable block (8) corresponds to the shape of a side corresponding to the upper blade (6).
5. The lost foam production mold for a slurry pump impeller according to claim 4, characterized in that: A weight reduction cavity (14) is provided on a side of the first movable block (8) corresponding to the first blade counter-module body (15).
6. The lost foam production mold for a slurry pump impeller according to claim 3, characterized in that: The second blade reverse module comprises a second blade reverse module body (16) and an arc-shaped second movable block (13) movably connected to a concave side of the second blade reverse module body (16); a side of the second movable block (13) corresponding to the second blade reverse module body (16) is perpendicular to the front cover plate (17) of the lower half mold (3), the side of the second movable block (13) is tightly attached to the concave side of the second blade reverse module body (16), and the shape of the other side of the second movable block (13) corresponds to the shape of the corresponding side of the lower blade (7).
7. The lost foam production mold for a slurry pump impeller according to claim 6, characterized in that: A weight reduction cavity (14) is provided on one side of the second movable block (13) corresponding to the second blade counter-module body (16).
8. The lost foam production mold for a slurry pump impeller according to claim 3, characterized in that: The first mold and the second mold are both made of high-hardness metal, and the material grade is ZL104.
Citation Information
Cited By
Ceramic slurry pump impeller compression molding device and molding process
CN120902087A