Adhesive tape

By designing a multi-layer structure in the tape, including the identification printing layer and the acrylic adhesive layer, the problems of insufficient adhesive performance and residual glue pollution are solved, efficient pasting and significant identification of the tape are achieved, and the use of electronic equipment is met. need.

CN222064414UActive Publication Date: 2024-11-26NITTO DENKO SHANGHAI SONGJIANG +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420561570.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-21
Publication Date
2024-11-26
Estimated Expiration
2034-03-21

AI Technical Summary

Technical Problem

The existing tapes are insufficient in the electronics industry and are prone to residual glue contamination, affecting the appearance of the adhered, and the product identification is not significant, resulting in difficulty in identifying consumers.

Method used

A tape including a first pressure-sensitive adhesive layer, a foamed resin layer, a second pressure-sensitive adhesive layer, a first release layer, a base material layer and a second release layer are designed in sequence from top to bottom, and foaming A marking printing layer is provided on the resin layer, and the surface area of ​​the marking printing layer accounts for 5 to 30% of the foamed resin layer. An acrylic adhesive and a silicone resin release layer are used to ensure adhesive performance and identification significance.

Benefits of technology

The tape is kept pasted at a predetermined position, and is easy to remove after use, without causing residual glue contamination, and the product identification is significant, making it easy for consumers to identify.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222064414U_ABST
    Figure CN222064414U_ABST
Patent Text Reader

Abstract

The utility model relates to an adhesive tape which comprises a first pressure-sensitive adhesive layer, a foaming resin layer, a second pressure-sensitive adhesive layer, a first release layer, a base material layer and a second release layer which are sequentially adjacently connected from top to bottom, a mark printing layer is arranged on one surface of the foaming resin layer, which is adjacently connected with the first pressure-sensitive adhesive layer, and a mark printing layer is arranged on the other surface of the foaming resin layer. The surface area of the identification printing layer accounts for 5-30% of the surface area of the foaming resin layer. The adhesive tape disclosed by the utility model has high identification degree and wide application in the aspects of bonding electronic equipment and the like. And when the adhesive tape is used or stripped, the adhesive tape can maintain the permanent existence of the mark.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the field of adhesive tapes, and in particular relates to an adhesive tape used for electronic equipment. Background Art

[0002] At present, in industries such as the electronics industry, a method of applying an adhesive tape is generally used for fixing, protecting a forming surface, or preventing contamination of the forming surface.

[0003] However, current conventional adhesive tapes have insufficient adhesive properties, or are prone to residual adhesive contamination on the adherend, affecting the appearance of the adherend; the product logo is not obvious, resulting in consumers being unable to identify it. Utility Model Content

[0004] Problems to be solved by utility models

[0005] The utility model aims to provide an adhesive tape which is convenient to use, has excellent bonding performance and has obvious product identification.

[0006] Solutions for solving problems

[0007] In order to achieve the above-mentioned object, the utility model provides an adhesive tape, which is specifically as follows.

[0008] A tape comprises a first pressure-sensitive adhesive layer, a foamed resin layer, a second pressure-sensitive adhesive layer, a first release layer, a substrate layer and a second release layer which are adjacent to each other from top to bottom. The tape is characterized in that a logo printing layer is provided on a surface of the foamed resin layer adjacent to the first pressure-sensitive adhesive layer, and the surface area of ​​the logo printing layer accounts for 5 to 30% of the surface area of ​​the foamed resin layer.

[0009] Among them, the thickness of the first pressure-sensitive adhesive layer is 15 to 100 μm, the thickness of the foamed resin layer is 100 to 400 μm, the thickness of the second pressure-sensitive adhesive layer is 15 to 100 μm, the thickness of the first release layer is 0.2 to 2 μm, the thickness of the substrate layer is 5 to 100 μm, and the thickness of the second release layer is 0.2 to 2 μm.

[0010] Wherein, the logo on the logo printing layer is one of NITTO, Nitto, NITTO TAPE or Nitto tape.

[0011] The foamed resin layer contains a foamed resin having pores with a height of 150 μm or less and lengths of 500 μm or less in the MD and TD directions, respectively.

[0012] Wherein, the first pressure-sensitive adhesive layer and the second pressure-sensitive adhesive layer are acrylic adhesive layers.

[0013] Wherein, the foamed resin layer comprises one of polyurethane foamed resin, polyester foamed resin, phenolic foamed resin and polyolefin foamed resin.

[0014] Wherein, the first release layer and the second release layer are silicone resin release layers.

[0015] Wherein, the substrate layer is a polyimide film, a polyester film, a polynaphthyl ester film, a polyamide film or a polyolefin film.

[0016] Wherein, the logo protrusion thickness of the logo printing layer is less than 0.8 μm.

[0017] Effect of utility model

[0018] The adhesive tape of the utility model can be kept adhered to the predetermined pasting position of the adherend, has excellent adhesive performance, is easy to remove after use, does not cause residual adhesive pollution to the adherend, and has a clear product mark. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a schematic cross-sectional view of an adhesive tape according to an embodiment of the present utility model.

[0020] Figure 2 This is a scanning electron microscope (SEM) photograph of the foamed resin layer.

[0021] Description of Reference Numerals

[0022] 1. First pressure-sensitive adhesive layer

[0023] 2 Foam resin layer

[0024] 3 Second pressure-sensitive adhesive layer

[0025] 4 First release layer

[0026] 5. Substrate layer

[0027] 6 Second release layer

[0028] 7 Logo printing layer

[0029] 100 Tape DETAILED DESCRIPTION

[0030] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0031] like Figure 1As shown, the adhesive tape 100 of the utility model includes a first pressure-sensitive adhesive layer 1, a foamed resin layer 2, a second pressure-sensitive adhesive layer 3, a first release layer 4, a substrate layer 5 and a second release layer 6 which are adjacent to each other from top to bottom, wherein a logo printing layer 7 is provided on the surface of the foamed resin layer 2 adjacent to the first pressure-sensitive adhesive layer 1, and the surface area of ​​the logo printing layer 7 accounts for 5 to 30% of the surface area of ​​the foamed resin layer 2, preferably 10 to 20%, and more preferably 12 to 18%.

[0032] The thickness of the first pressure-sensitive adhesive layer 1 is 15-100 μm, preferably 25-75 μm, the thickness of the foamed resin layer 2 is 100-400 μm, preferably 150-300 μm, the thickness of the second pressure-sensitive adhesive layer 3 is 15-100 μm, preferably 25-75 μm, the thickness of the first release layer 4 is 0.2-2 μm, the thickness of the substrate layer 5 is 5-100 μm, preferably 35-75 μm, and the thickness of the second release layer 6 is 0.2-2 μm, preferably 0.2-1 μm. The logo protrusion thickness of the logo printing layer is less than 0.8 μm, preferably 0.2-0.8 μm. As a test method for the thickness of each layer, various known layer thickness test methods can be used, such as a scanning electron microscope (SEM) with a magnification of hundreds to tens of thousands of times.

[0033] In the present invention, the logo on the logo printing layer 7 is one of NITTO, Nitto, NITTO TAPE or Nittotape. When the adhesive tape is applied to electronic devices, the first pressure-sensitive adhesive layer 1 can be peeled off to expose the logo on the logo printing layer 7 to help consumers identify it.

[0034] The foamed resin layer 2 contains a foamed resin having a hole with a height of 150 μm or less (preferably 120 μm or less) and a length of 500 μm or less (preferably 300 μm or less) in the MD and TD directions. There is no particular restriction on the foamed resin contained in the foamed resin layer, which can be one of a polyurethane foamed resin, a polyester foamed resin, a phenolic foamed resin, and a polyolefin foamed resin. The foamed resin layer 2 can be subjected to a conventional surface treatment, such as a conventional corona treatment, an ionizing radiation treatment, a sodium-naphthalene treatment, etc.

[0035] The first pressure-sensitive adhesive layer 1 and the second pressure-sensitive adhesive layer 3 are acrylic adhesive layers.

[0036] The first release layer 4 and the second release layer 6 are silicone release layers. The release layers can also be subjected to conventional electrostatic treatment.

[0037] The type of the substrate layer 5 is not particularly limited, and may be a polyimide film, a polyester film, a polynaphthyl ester film, a polyamide film, or a polyolefin film.

[0038] As a method for forming each layer, any appropriate method may be adopted, and examples thereof include roll coating, spin coating, wire bar coating, dip coating, die coating, curtain coating, spray coating, knife coating, and micro-gap coating printing.

[0039] In the present invention, the materials contained in each layer are all materials of known types.

[0040] The following examples are merely illustrative and are not intended to limit the present invention.

[0041] Example

[0042] A foamed resin film with a thickness of 200 μm (manufactured by Sekisui Chemical Co., Ltd., wherein the height of the holes in the foamed resin is less than 120 μm and the lengths in the MD and TD directions are respectively less than 300 μm) was subjected to double-sided corona treatment. The five letters of NITTO were printed on one side as a logo using micro-gravure printing, and the area occupied by the five letters after printing was 15% of the surface of the foamed resin layer.

[0043] An acrylic adhesive layer was coated on both sides of the treated foamed resin film to form a first pressure-sensitive adhesive layer with a thickness of 50 μm and a second pressure-sensitive adhesive layer with a thickness of 50 μm, respectively.

[0044] A release film with silicone resin coated on both sides of polyethylene terephthalate (PET) with a thickness of 75 μm (the thickness of the silicone resin on both sides is 0.3 μm) is laminated to the second pressure-sensitive adhesive layer and rolled up to form an adhesive tape.

Claims

1. An adhesive tape comprising a first pressure-sensitive adhesive layer, a foamed resin layer, a second pressure-sensitive adhesive layer, a first release layer, a substrate layer and a second release layer, which are adjacent to each other from top to bottom, characterized in that: A logo printing layer is arranged on one surface of the foamed resin layer adjacent to the first pressure-sensitive adhesive layer, and the surface area of ​​the logo printing layer accounts for 5-30% of the surface area of ​​the foamed resin layer.

2. The adhesive tape according to claim 1, characterized in that The thickness of the first pressure-sensitive adhesive layer is 15 to 100 μm, the thickness of the foamed resin layer is 100 to 400 μm, the thickness of the second pressure-sensitive adhesive layer is 15 to 100 μm, the thickness of the first release layer is 0.2 to 2 μm, the thickness of the substrate layer is 5 to 100 μm, and the thickness of the second release layer is 0.2 to 2 μm.

3. The adhesive tape according to claim 1 or 2, characterized in that: The foamed resin layer contains a foamed resin having pores with a height of 150 μm or less and lengths in the MD and TD directions of 500 μm or less, respectively.

4. The adhesive tape according to claim 1 or 2, characterized in that: The first pressure-sensitive adhesive layer and the second pressure-sensitive adhesive layer are acrylic adhesive layers.

5. The adhesive tape according to claim 1 or 2, characterized in that: The foamed resin layer includes one of polyurethane foamed resin, polyester foamed resin, phenolic foamed resin and polyolefin foamed resin.

6. The adhesive tape according to claim 1 or 2, characterized in that: The first release layer and the second release layer are silicone release layers.

7. The adhesive tape according to claim 1 or 2, characterized in that: The substrate layer is a polyimide film, a polyester film, a polynaphthyl ester film, a polyamide film or a polyolefin film.