Battery

By adopting laser welding technology and insulating layer design in the pole ear unit of lithium-ion battery, the length and position of the welding area are controlled, and the problem of increasing the thickness of the battery is solved by excessively wide welding parts, achieving high energy density and excellent battery Electrical performance.

CN222072123UActive Publication Date: 2024-11-26ZHUHAI COSMX BATTERY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420644111.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-29
Publication Date
2024-11-26
Estimated Expiration
2034-03-29

AI Technical Summary

Technical Problem

The welds of the soft and hard ear welding parts of the lithium-ion battery lead to an increase in the overall thickness of the battery, thereby reducing the energy density.

Method used

By laser welding using overlapping parts of the first bent section and the second bent section in the pole ear unit of the battery, a welding area is formed, and the extension length of the welding area is controlled to 0.3 to 0.8 of the length of the battery body, so as to Reduce the overall thickness of the battery while using an insulating layer and hot melt connection to avoid the impact of the welding area on the battery packaging.

Benefits of technology

It achieves the effect of small overall thickness of the battery and high energy density, and reduces the self-discharge phenomenon caused by metal dust, and improves the electrical performance of the battery cell.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222072123U_ABST
    Figure CN222072123U_ABST
Patent Text Reader

Abstract

The utility model provides a battery, and relates to the technical field of battery energy, the battery comprises a battery cell, the battery cell comprises a battery cell body and a tab unit, and the tab unit comprises a first tab and a second tab; the first tab comprises a first bending section, the second tab comprises a second bending section, the battery cell body, the first bending section and the second bending section are both located in the accommodating cavity, the first bending section is connected with the battery cell body and the second bending section, and the first bending section and the second bending section are at least partially overlapped; the overlapped parts of the first bending sections are welded and connected to form a welding area, and the extension length of the welding area along the first direction is greater than or equal to 0.3 of the extension length of the battery cell body along the first direction and less than or equal to 0.8 of the extension length of the battery cell body along the first direction. The battery disclosed by the utility model is relatively small in overall thickness and relatively high in energy density.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of battery energy technology, and in particular to a battery. Background Art

[0002] With the rapid development of 5G, people have higher and higher requirements for the battery life of electronic products, so high energy density is still one of the main development directions of lithium-ion batteries.

[0003] In the related art, a lithium-ion battery mainly includes a battery case, a battery cell and a tab assembly. The battery cell and the electrolyte are arranged in the battery case, and the current of the battery cell is conducted out through the tab assembly. The battery cell may include a positive electrode sheet, a diaphragm and a negative electrode sheet. The positive electrode sheet, the diaphragm and the negative electrode sheet are stacked in sequence and wound or laminated to form a battery cell. The tab assembly may include a soft tab and a hard tab. The soft tab is welded to the positive electrode sheet and the negative electrode sheet, and the hard tab is welded to the soft tab. Part of the hard tab is located outside the battery case to be connected to the device to be powered.

[0004] Since both the soft pole ear and the hard pole ear need to be bent after welding, if the weld between the soft pole ear and the hard pole ear is too wide, the bent part of the soft pole ear and the hard pole ear will exceed the thickness of the battery cell, thereby increasing the overall thickness of the battery, resulting in a lower energy density of the battery. Utility Model Content

[0005] Based on this, the present application provides a battery with a smaller overall thickness and higher energy density.

[0006] The present application provides a battery, including a battery cell, the battery cell including a battery cell body and a pole lug unit, the pole lug unit including a first pole lug and a second pole lug, the first pole lug including a first bending section, the second pole lug including a second bending section, the first bending section connecting the battery cell body and the second bending section;

[0007] The first bending section and the second bending section at least partially overlap, and the overlapping portion of at least a portion of the first bending section and at least a portion of the second bending section is welded to form a welding area;

[0008] An extension length of the welding area along the first direction is greater than or equal to 0.3 of an extension length of the battery cell body along the first direction, and less than or equal to 0.8 of an extension length of the battery cell body along the first direction;

[0009] The first direction is along the thickness direction of the battery cell body, and the second direction is perpendicular to the first direction.

[0010] In a possible implementation, the battery provided by the present application further includes a shell having a receiving cavity, the battery cell body, the first bent section, and the second bent section are all located in the receiving cavity, and the second pole ear further includes a straight section, the straight section is connected to an end of the second bent section away from the first bent section, and extends along the second direction to the outside of the receiving cavity;

[0011] At least part of the straight section and at least part of the shell are connected by heat melting to form a bonding area, and a first gap is formed between the welding area and the bonding area along the second direction.

[0012] In a possible implementation, in the battery provided in the present application, an extension length of the welding area along the second direction is greater than or equal to 0.1 of the first gap and less than or equal to 0.95 of the first gap.

[0013] In a possible implementation, in the battery provided by the present application, an extension length of the welding area along the second direction is greater than or equal to 85 μm and less than or equal to 300 μm;

[0014] And / or, the extension length of the battery cell body along the first direction is greater than or equal to 1 mm and less than or equal to 5 mm;

[0015] And / or, an extension length of the welding area along the first direction is greater than or equal to 0.3 mm and less than or equal to 0.8 mm.

[0016] In a possible implementation, in the battery provided by the present application, the distance between the two ends of the first bending section and the second bending section that are away from each other along the first direction is greater than or equal to 0.2 of the extension length of the battery body along the first direction, and less than or equal to the extension length of the battery body along the first direction;

[0017] And / or, the distance between two ends of the first bending section and the second bending section that are away from each other along the first direction is greater than or equal to 0.6 mm and less than or equal to 3 mm.

[0018] In a possible implementation, the battery provided in the present application has at least one weld in the welding area, and the projection of the weld on the first bending section is linear, or the projection of the weld on the first bending section is point-shaped.

[0019] In a possible implementation, the battery provided by the present application, the weld includes a first connection area and a second connection area connected to each other, the first connection area is located in the first bending section, and the second connection area is located in the second bending section;

[0020] At least a portion of the first connection area protrudes from the first bending segment, and / or at least a portion of the second connection area protrudes from the second bending segment.

[0021] In a possible implementation, in the battery provided in the present application, an extension length of the first connection region along the first direction is smaller than an extension length of the second connection region along the first direction.

[0022] In a possible implementation, in the battery provided in the present application, the projection of the weld on the surface of the first electrode tab is curved.

[0023] In a possible implementation, in the battery provided in the present application, the tab unit further includes an insulating layer, which is disposed on two opposite sides of the welding area, and the projection of the insulating layer on the first bending section covers the welding area.

[0024] In a possible implementation, the battery provided in the present application has a welding area with at least two welds, and a second gap is provided between two adjacent welds.

[0025] In a possible implementation, in the battery provided in the present application, the second gap is greater than or equal to 0.3 of the extension length of the insulating layer along the first direction, and less than or equal to 0.9 of the extension length of the insulating layer along the first direction.

[0026] In a possible implementation, in the battery provided by the present application, the first bending section includes a first bending section of the positive electrode and a first bending section of the negative electrode, the second bending section includes a second bending section of the positive electrode and a second bending section of the negative electrode, and the second connection area includes a second connection area of ​​the positive electrode and a second connection area of ​​the negative electrode;

[0027] The second connection area of ​​the positive electrode protrudes from the second bending section of the positive electrode, and the height of the second connection area of ​​the positive electrode protruding from the second bending section of the positive electrode is less than or equal to 100 μm;

[0028] And / or, the second connection region of the negative electrode is recessed in the second bending section of the negative electrode, and the height of the second connection region of the negative electrode recessed in the second bending section of the negative electrode is less than or equal to 30 μm.

[0029] In a possible implementation, in the battery provided by the present application, the first connection region includes a first connection region of the positive electrode, and a height of the second connection region of the positive electrode protruding from the second bent section of the positive electrode is greater than a height of the first connection region of the positive electrode protruding from the first bent section of the positive electrode;

[0030] And / or, the height of the first connection region of the positive electrode protruding from the first bent section of the positive electrode is greater than or equal to 0.5 μm and less than or equal to 20 μm.

[0031] In a possible implementation, the battery provided by the present application, the weld includes a positive electrode weld connecting the first bent section of the positive electrode and the second bent section of the positive electrode, and a negative electrode weld connecting the first bent section of the negative electrode and the second bent section of the negative electrode;

[0032] The number of positive electrode welds is greater than or equal to the number of negative electrode welds and less than or equal to 5 of the number of negative electrode welds.

[0033] In a possible implementation, in the battery provided in the present application, the projection of the weld on the surface of the first bending section is curved, the weld has crests, and the spacing between adjacent crests is greater than 0.1 mm and less than or equal to 2 mm.

[0034] In a possible implementation, in the battery provided in the present application, the first bending section and the second bending section are laser welded.

[0035] In a possible implementation, the battery provided in the present application has a cell body including a pole piece and a diaphragm, the pole piece and the diaphragm are stacked in sequence, and the diaphragm is adjacent to the welding area along the second direction; or, the diaphragm and the welding area have a third gap along the second direction.

[0036] The battery provided by the present application includes a shell and a battery cell, the shell includes a receiving cavity, a battery cell body and a pole ear unit, the pole ear unit includes a first pole ear and a second pole ear, the first pole ear includes a first bending section, and the second pole ear includes a second bending section and a straight section. The battery cell body is provided to react with the electrolyte to generate current, the first bending section and the second bending section are provided to reduce the volume of the battery, and are used to connect the first pole ear and the second pole ear, a welding area is formed at the overlapping part of the first bending section and the second bending section, and the extension length of the welding area along the first direction is set to 0.3 to 0.8 of the extension length of the battery cell body along the first direction, so that the extension length of the welding area along the first direction is smaller, thereby avoiding the welding area being too wide and increasing the thickness of the battery cell. As a result, the overall thickness of the battery provided by the present application is smaller and the energy density is higher.

[0037] In addition to the technical problems solved by the embodiments of the present application described above, the technical features that constitute the technical solutions, and the beneficial effects brought about by the technical features of these technical solutions, other technical problems that can be solved by the battery provided by the present application, other technical features included in the technical solutions, and the beneficial effects brought about by these technical features will be further described in detail in the specific implementation methods. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, a brief introduction will be given below to the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0039] Figure 1 A schematic diagram of the structure of a battery provided in an embodiment of the present application;

[0040] Figure 2 for Figure 1 A partial enlarged view of the dotted box in the middle;

[0041] Figure 3 A schematic diagram of the structure of a battery cell in a battery provided in an embodiment of the present application;

[0042] Figure 4 Another schematic diagram of the structure of a battery cell in a battery provided in an embodiment of the present application;

[0043] Figure 5 A schematic diagram of the structure of a welding area in a battery provided in an embodiment of the present application;

[0044] Figure 6 A schematic diagram of the structure of a first bent section of a positive electrode, a second bent section of a positive electrode, and a weld in a battery provided in an embodiment of the present application;

[0045] Figure 7 A schematic structural diagram of the first bent section of the negative electrode, the second bent section of the negative electrode and the weld in the battery provided in an embodiment of the present application.

[0046] Description of reference numerals:

[0047] 100-housing; 110-accommodating cavity;

[0048] 200-battery cells;

[0049] 210-battery cell body;

[0050] 220-ear unit;

[0051] 221-first pole ear; 2211-first bending section; 2211a-first bending section of the positive electrode; 2211b-first bending section of the negative electrode;

[0052] 222-second pole ear; 2221-second bending section; 2221a-second bending section of the positive electrode; 2221b-second bending section of the negative electrode; 2222-straight section;

[0053] 223-welding area; 2231-welding seam; 2231a-first connection area; 2231b-second connection area;

[0054] 224-insulation layer;

[0055] 300 - bonding area. DETAILED DESCRIPTION

[0056] In order to make the purpose, technical scheme and advantages of the present application clearer, the technical scheme in the embodiment of the present application will be described in more detail below in conjunction with the drawings in the preferred embodiments of the present application. In the drawings, the same or similar reference numerals throughout represent the same or similar parts or parts with the same or similar functions. The described embodiments are part of the embodiments of the present application, not all of the embodiments. The embodiments described below with reference to the drawings are exemplary and are intended to be used to explain the present application, and should not be construed as limitations on the present application. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present application. The embodiments of the present application are described in detail below in conjunction with the drawings.

[0057] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, or it can be an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0058] In the description of the present application, it should be understood that the terms "upper", "lower", "front", "back", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are orientations or positional relationships based on the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0059] The terms "first", "second", "third" (if any) in the specification and claims of this application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the numbers used in this way can be interchanged where appropriate, so that the embodiments of the application described herein can be implemented in an order other than those illustrated or described herein, for example.

[0060] In addition, the terms "comprises," "comprising," and "having," and any variations thereof, are intended to cover a non-exclusive inclusion, for example, a process, method, system, product, or display comprising a series of steps or elements is not necessarily limited to those steps or elements explicitly listed, but may include other steps or elements not explicitly listed or inherent to such process, method, product, or display.

[0061] In the related art, a lithium-ion battery mainly includes a battery case, a battery cell and a tab assembly. The battery cell and the electrolyte are arranged in the battery case, and the current of the battery cell is conducted out through the tab assembly. The battery cell may include a positive electrode sheet, a diaphragm and a negative electrode sheet. The positive electrode sheet, the diaphragm and the negative electrode sheet are stacked in sequence and wound or laminated to form a battery cell. The tab assembly may include a soft tab and a hard tab. The soft tab is welded to the positive electrode sheet and the negative electrode sheet, and the hard tab is welded to the soft tab. Part of the hard tab is located outside the battery case to be connected to the device to be powered.

[0062] Since both the soft pole ear and the hard pole ear need to be bent, and the welds at the welding parts of the soft pole ear and the hard pole ear are too wide, the bent parts of the soft pole ear and the hard pole ear will exceed the thickness of the battery cell, thereby increasing the overall thickness of the battery, resulting in a lower energy density of the battery.

[0063] The embodiment of the present application connects the first bending section and the second bending section by welding, so that a welding area is formed at the overlapping portion of the first bending section and the second bending section, and the extension length of the welding area along the first direction is set to 0.3 to 0.8 of the extension length of the battery body along the first direction, so that the dimensions of the welding area and the battery body in the first direction can overlap, thereby reducing the overall thickness of the battery and improving the energy density of the battery.

[0064] The specific implementation of the battery provided in the embodiments of the present application is explained and illustrated in detail below with reference to the accompanying drawings.

[0065] Reference Figures 1 to 4 As shown, the battery provided in the embodiment of the present application includes a housing 100 and a battery cell 200 , the housing 100 has a receiving cavity 110 , the battery cell 200 includes a battery cell body 210 and a tab unit 220 , and the tab unit 220 includes a first tab 221 and a second tab 222 .

[0066] The first pole ear 221 includes a first bending section 2211, and the second pole ear 222 includes a second bending section 2221 and a straight section 2222. The battery cell body 210, the first bending section 2211 and the second bending section 2221 are all located in the accommodating cavity 110. The first bending section 2211 and the second bending section 2221 both extend along the first direction. The first bending section 2211 is connected between the battery cell body 210 and the second bending section 2221. The straight section 2222 is connected to one end of the second bending section 2221 away from the first bending section 2211, and extends to the outside of the accommodating cavity 110 along the second direction. The first bending section 2211 and the second bending section 2221 at least partially overlap, and the overlapping parts of the first bending section 2211 and the first bending section 2211 are connected by laser welding to form a welding area 223.

[0067] The first direction is along the thickness direction of the battery cell body 210 , and the second direction is perpendicular to the first direction.

[0068] In the present application, the battery cell body 210 can react with the electrolyte to generate current, and the first pole ear 221 is used to be directly connected to the battery cell body 210 to lead the current of the battery cell body 210, and the first pole ear 221 is connected between the battery cell body 210 and the second pole ear 222, and the second pole ear 222 is used to lead the current out of the housing 100 to transmit current between the battery and the device to be powered.

[0069] It is understandable that in order to reduce the overall volume of the battery, after the first pole ear 221 and the second pole ear 222 are connected, the first pole ear 221 and the second pole ear 222 need to be bent to make the battery structure more compact. Therefore, the first pole ear 221 is bent to form a first bending section 2211, and the second pole ear 222 is bent to form a second bending section 2221. The first bending section 2211 and the second bending section 2221 are both along the thickness of the battery body 210, that is, the first direction. Specifically, the first direction can refer to the X direction in the accompanying drawings, and the second direction can refer to the Y direction in the accompanying drawings.

[0070] If the ultrasonic welding in the prior art is used to weld the first pole ear 221 and the second pole ear 222, the ultrasonic welding area formed after the two are welded has a longer extension length along the first direction. Since the ultrasonic welding area cannot be bent, in order to avoid the ultrasonic welding area, when the first pole ear 221 and the second pole ear 222 are subsequently bent, it is necessary to make the first bending section 2211 and the second bending section 2221 extend longer along the first direction, so that the overlapping portion of the first bending section 2211 and the second bending section 2221 extends longer along the first direction. The length of the first bending section 2211 and the second bending section 2221 is longer, so that the extension length of the first bending section 2211 and the second bending section 2221 along the first direction is increased more, and the distance between the end of the first bending section 2211 away from the second bending section 2221 and the end of the second bending section 2221 away from the first bending section 2211 is longer, thereby making the distance between the end of the first bending section 2211 away from the second bending section 2221 and the end of the second bending section 2221 away from the first bending section 2211 exceed the thickness of the battery body 210, thereby increasing the overall thickness of the battery.

[0071] Therefore, in this embodiment, the first bending segment 2211 and the second bending segment 2221 are welded by laser, and a welding area 223 is formed at the overlapping portion of the first bending segment 2211 and the second bending segment 2221. The first pole ear 221 and the second pole ear 222 are welded by laser welding, so that the extension length of the welding area 223 in the first direction is smaller, thereby avoiding the sum of the extension lengths of the first bending segment 2211 and the second bending segment 2221 along the first direction exceeding the thickness of the battery body 210, thereby avoiding increasing the overall thickness of the battery, thereby improving the energy density of the battery.

[0072] In addition, when laser welding is used, less metal dust is generated, thereby reducing the self-discharge of the battery cell 200 caused by the metal dust, thereby improving the electrical performance of the battery cell 200 .

[0073] The battery provided in the embodiment of the present application includes a shell 100 and a battery cell 200, the shell 100 includes a accommodating cavity 110, a battery cell body 210 and a pole lug unit 220, the pole lug unit 220 includes a first pole lug 221 and a second pole lug 222, the first pole lug 221 includes a first bent section 2211, and the second pole lug 222 includes a second bent section 2221 and a straight section 2222. The accommodating cavity 110 is provided to accommodate the battery cell body 210 and the electrolyte, the battery cell body 210 is provided to react with the electrolyte to generate current, the first bending section 2211 and the second bending section 2221 are provided to reduce the volume of the battery and to connect the first pole ear 221 and the second pole ear 222, and laser welding is performed at the overlapping portion of the first bending section 2211 and the second bending section 2221 to form a welding area 223, thereby making the extension length of the welding area 223 along the first direction shorter, thereby preventing the sum of the extension lengths of the first bending section 2211 and the second bending section 2221 along the first direction from exceeding the thickness of the battery cell body 210. Therefore, the battery provided in the embodiment of the present application has a smaller overall thickness and a higher energy density. Figures 2 to 4 As shown, in a possible implementation, the tab unit 220 may further include an insulating layer 224 , which is disposed on two opposite sides of the welding region 223 along the first direction, and a projection of the insulating layer 224 on the first bending section 2211 covers the welding region 223 .

[0074] It should be noted that the insulating layer 224 covering the two opposite sides of the welding area 223 is used to insulate and isolate the welding area 223 to prevent the first pole ear 221 or the second pole ear 222 of the welding area 223 from directly contacting the battery body 210, thereby causing a battery short circuit, and the insulating layer 224 will not extend to the straight section 2222 to avoid affecting the battery packaging.

[0075] It is understandable that when the shell 100 is made of aluminum-plastic film, the aluminum-plastic film has a hot-melt adhesive layer, and the two aluminum-plastic films can be hot-melt connected by hot pressing. If the insulating layer 224 extends to the straight section 2222, the two hot-melt adhesive layers cannot be completely bonded together when the two aluminum-plastic films are hot-melt connected, thereby causing poor packaging of the shell 100. At least part of the straight section 2222 and at least part of the shell 100 are hot-melt connected to form a bonding area 300, and the welding area 223 and the bonding area 300 have a first gap along the second direction. The extension length of the welding area 223 along the second direction is greater than or equal to 0.1 of the first gap and less than or equal to 0.95 of the first gap. In this way, when the insulating layer 224 is subsequently pasted, sufficient distance can be provided to the insulating layer 224, thereby preventing the insulating layer 224 from extending to the straight section 2222 to avoid affecting the battery packaging.

[0076] Among them, the extension length of the welding area 223 along the second direction can be any value of 85-300μm, therefore, the first gap can be any value of 86-3000μm, for example, the extension length of the welding area 223 along the second direction can be any value of 85μm, 100μm, 200μm, 300μm or within any two numerical ranges, and the first gap can be any value of 86μm, 120μm, 1000μm, 3000μm or within any two numerical ranges.

[0077] Specifically, the first gap can refer to Figure 2 G1 in.

[0078] In a possible implementation, an extension length of the battery cell body 210 along the first direction is greater than or equal to 1 mm and less than or equal to 5 mm.

[0079] That is to say, the thickness of the battery cell body 210 is 1mm-5mm. For example, the thickness of the battery cell body 210 is any one of 1mm, 2mm, 1mm, 4mm, and 5mm or is within any two numerical ranges. The thickness of the battery cell body 210 is relatively thin. For thin batteries with a relatively small thickness, the connection portion between the first pole tab 221 and the second pole tab 222 should be narrower, that is, the extension length of the welding area 223 along the first direction should not be too large, so that after the pole tabs are folded, the overall thickness of the battery cell 200 will not be affected by the larger width of the connection portion between the first pole tab 221 and the second pole tab 222. On the one hand, due to the width limitation of the welding area 223, the welding depth of the welding area 223 is also reduced, making it difficult to connect all the first pole tab 221 and the second pole tab 222, and the pole tab unit 220 cannot achieve effective output of electrons. On the other hand, due to the constraint of the width of the welding area 223, the welding strength of the conventional welding method is also relatively low. If conventional ultrasonic welding is used, it is impossible to effectively reduce the overall thickness of the battery and improve the connection strength of the tab unit 220 at the same time.

[0080] In some embodiments, an extension length of the welding region 223 along the first direction is greater than or equal to 0.3 of an extension length of the cell body 210 along the first direction, and less than or equal to 0.8 of an extension length of the cell body 210 along the first direction.

[0081] It can be understood that the welding area 223 should reliably connect the first bending section 2211 and the second bending section 2221. If the extension length of the welding area 223 along the first direction is small, the connection strength of the welding area 223 is insufficient and the welding area 223 cannot reliably connect the first bending section 2211 and the second bending section 2221. Therefore, the extension length of the welding area 223 along the first direction is greater than or equal to 0.3 of the extension length of the battery cell body 210 along the first direction.

[0082] If the extension length of the welding area 223 along the first direction is large, correspondingly, the extension length of the insulating layer 224 along the first direction is also large, and the thickness of the battery cell will also increase. In order to avoid the insulating layer 224 extending to the straight section 2222, and to reduce the thickness of the battery cell and improve the energy density of the battery, the extension length of the welding area 223 along the first direction should be less than or equal to 0.8 of the extension length of the battery cell body 210 along the first direction.

[0083] For example, the extension length of the welding area 223 along the first direction may be 0.3, 0.4, 0.6, or 0.8 of the extension length of the battery cell body 210 along the first direction.

[0084] It is understood that when the thickness of the battery cell body 210 is 1mm-5mm, the extension length of the welding area 223 along the first direction is 0.3-0.8mm. For example, the extension length of the welding area 223 along the first direction is any one of 0.3mm, 0.4mm, 0.5mm, 0.8mm or within any two value ranges.

[0085] In some embodiments, the projections of the first bending section 2211 and the second bending section 2221 in the first direction are located inside the battery cell body 210. That is, the extension length of the first bending section 2211 along the first direction is less than or equal to the extension length of the battery cell body 210 along the first direction, and the extension length of the second bending section 2221 along the first direction is less than or equal to the extension length of the battery cell body 210 along the first direction. After the first bending section 2211 and the second bending section 2221 partially or completely overlap, the sum of the extension lengths of the first bending section 2211 and the second bending section 2221 along the first direction is less than or equal to the thickness of the battery cell body 210. In this way, the first bending section 2211 and the second bending section 2221 can overlap with the size of the battery cell body 210 in the first direction, so that the first bending section 2211 and the second bending section 2221 do not occupy additional thickness of the battery, so as to avoid increasing the overall thickness of the battery.

[0086] In order to form a welding area 223 at the overlapping portion of the first bending section 2211 and the second bending section 2221, and in order to avoid increasing the thickness of the battery, the distance between the two ends of the first bending section 2211 and the second bending section 2221 that are opposite to each other along the first direction is greater than or equal to 0.2 of the extension length of the battery cell body 210 along the first direction, and less than or equal to the extension length of the battery cell body 210 along the first direction.

[0087] For example, the distance between the two ends of the first bending section 2211 and the second bending section 2221 that are opposite to each other along the first direction may be 0.2, 0.3, 0.5, 0.8, 1, etc. of the extension length of the battery cell body 210 along the first direction.

[0088] And / or, the distance between the two ends of the first bending segment and the second bending segment that are separated from each other along the first direction is greater than or equal to 0.6 mm and less than or equal to 3 mm. For example, the distance between the two ends of the first bending segment 2211 and the second bending segment 2221 that are separated from each other can be any one of 0.6 mm, 0.8 mm, 1.2 mm, 2 mm, and 3 mm, or be within any two numerical ranges.

[0089] Reference Figure 5 As shown, in a possible implementation, the welding area 223 has at least one welding seam 2231 , the projection of the welding seam 2231 on the surface of the first electrode tab 221 is linear, and the welding seam 2231 extends along the third direction.

[0090] It should be noted that the first direction and the second direction are both perpendicular to the third direction, and the third direction can refer to the Z direction in the accompanying drawings.

[0091] That is to say, when laser welding is used to weld the first pole ear 221 and the second pole ear 222, the movement path of the laser beam can be a straight line or a curve, and the heat of the laser beam can dissolve the metal material of the first pole ear 221 and the second pole ear 222, thereby forming a linear weld 2231 between the first pole ear 221 and the second pole ear 222, thereby connecting the first pole ear 221 and the second pole ear 222.

[0092] Illustratively, the weld 2231 may be a straight line, a sinusoidal line or a spiral line. The linear weld 2231 can provide a larger contact area between the first pole tab 221 and the second pole tab 222, thereby increasing the flow conduction area of ​​the pole tab unit 220, improving the welding strength and reducing the welding internal resistance.

[0093] In some embodiments, the projection of the weld 2231 on the surface of the first bending section 2211 is curved, the weld 2231 has wave crests, and the spacing between adjacent wave crests is greater than 0.1 mm and less than or equal to 2 mm.

[0094] In this way, the conduction density of the welding area 223 can be reduced, and the temperature rise of the welding area 223 when the battery cell 200 is working can be reduced, thereby preventing the tab unit 220 from contacting the battery cell body 210 due to the melting of the insulating layer 224, thereby avoiding a short circuit in the battery cell 210.

[0095] The extension length of the weld 2231 along the second direction should be greater than or equal to 85 μm and less than or equal to 300 μm. The weld 2231 is also at a distance from the bonding area 300 to provide a sufficient distance for the insulating layer 224, thereby preventing the insulating layer 224 from extending to the straight section 2222, thereby preventing the insulating layer 224 from affecting the packaging of the housing 100.

[0096] It can be understood that since the first pole ear 221 has different thicknesses in different types of batteries, and the second pole ear 222 has different thicknesses in different types of batteries, in order to ensure that the weld 2231 effectively connects the first bending section 2211 and the second bending section 2221, the extension length of the weld 2231 along the second direction should be greater than the sum of the thicknesses of the first bending section 2211 and the second bending section 2221.

[0097] For example, along the second direction, the distance from the weld 2231 to the bonding area 300 is 0.1 to 0.95 of the extension length of the weld 2231 along the second direction.

[0098] Alternatively, in some embodiments, the weld 2231 may also be in a point shape, such as a spiral point shape, that is, a plurality of weld points are connected in sequence to form a spiral line.

[0099] Specifically, the weld 2231 may include a first connection area 2231a and a second connection area 2231b connected to each other along the second direction, wherein the first connection area 2231a is located at the first bending section 2211, and the second connection area 2231b is located at the second bending section 2221. The first connection area 2231a protrudes from the first bending section 2211, and / or the second connection area 2231b protrudes from the second bending section 2221.

[0100] In order to make the welding area 223 reliably connect the first bending section 2211 and the second bending section 2221, when performing laser welding, the laser beam is irradiated on the side of the second bending section 2221 away from the first bending section 2211, and the heat of the laser beam should be able to ensure that the first bending section 2211 and the second bending section 2221 can be welded through, and after the weld 2231 is formed, the weld 2231 will protrude from the first bending section 2211, or the weld 2231 will protrude from the second bending section 2221, or the weld 2231 will protrude from the first bending section 2211 and the second bending section 2221 at the same time.

[0101] The extension length of the first connection region 2231a along the first direction is smaller than the extension length of the second connection region 2231b along the first direction.

[0102] That is to say, the weld 2231 includes two parts, one part is located in the first bending section 2211, namely the first connection area 2231a, and the other part is located in the second bending section 2221, namely the second connection area 2231b. In order to avoid excessive heat input causing damage to the first pole ear 221 and the second pole ear 222, affecting the conductivity of the first pole ear 221 and the second pole ear 222, the heat of the laser beam should not be too large. When the heat of the laser beam can just weld through the first bending section 2211 and the second bending section 2221, in the formed weld 2231, the first connection area 2231a is wider and the second connection area 2231b is narrower, forming a weld 2231 structure similar to an inverted triangle. In this way, the temperature rise of the welding area 223 when the battery cell 200 is working can be reduced, and the melting of the insulating layer 224 can be avoided, which causes the first pole ear 221 or the second pole ear 222 to contact the battery cell body 210, thereby avoiding a short circuit in the battery cell 200.

[0103] In a possible implementation, the projection of the weld 2231 on the surface of the first bending segment 2211 is a curve.

[0104] For example, the weld 2231 can be a sinusoidal line or a spiral line. When the extension length of the first bending section 2211 along the third direction is the same, the weld 2231 extending along the curve can increase the overall length of the weld 2231 relative to the weld 2231 extending along a straight line, thereby increasing the connection area between the first bending section 2211 and the second bending section 2221, thereby increasing the diversion area, improving the welding strength and reducing the welding internal resistance.

[0105] In order to increase the connection area between the first bending section 2211 and the second bending section 2221, in a possible implementation, the welding area 223 has at least two welds 2231, and a second gap is provided between two adjacent welds 2231, and the second gap is greater than or equal to 0.3 of the extension length of the insulating layer 224 along the first direction, and less than or equal to 0.9 of the extension length of the insulating layer 224 along the first direction.

[0106] In this way, the insulating layer 224 can cover all the welds 2231 of the welding area 223 to prevent the welding area 223 from contacting the battery cell body 210 and causing a short circuit in the battery cell 200 .

[0107] The second gap can be referred to Figure 5 In G2, the second gap may be in the range of 0.1-0.5 mm. For example, the second gap may be any one of 0.1 mm, 0.3 mm, 0.4 mm, and 0.5 mm or may be within the range of any two values.

[0108] It can be understood that, in a specific implementation, the first pole ear 221 may include a first pole ear of the positive electrode and a first pole ear of the negative electrode, the second pole ear 222 may include a second pole ear of the positive electrode and a second pole ear of the negative electrode, the battery cell body 210 may include a positive electrode sheet, a separator and a negative electrode sheet, the first pole ear of the positive electrode is connected between the positive electrode sheet and the second pole ear of the positive electrode, and the first pole ear of the negative electrode is connected between the negative electrode sheet and the second pole ear of the negative electrode.

[0109] Corresponding, refer to Figure 6 and Figure 7 As shown, the first bending segment 2211 may include a first bending segment 2211a of the positive electrode and a first bending segment 2211b of the negative electrode, the second bending segment 2221 may include a second bending segment 2221a of the positive electrode and a second bending segment 2221b of the negative electrode, the first bending segment 2211a of the positive electrode and the second bending segment 2221a of the positive electrode are welded, and the first bending segment 2211b of the negative electrode and the second bending segment 2221b of the negative electrode are welded.

[0110] Since the first pole ear and the second pole ear of the positive electrode are made of aluminum foil, and the thermal expansion coefficient of the aluminum foil is relatively large, in the formed weld 2231, the second connection area 2231b of the positive electrode protrudes from the second bending section 2221a of the positive electrode, and the first pole ear and the second pole ear of the negative electrode are made of copper foil, and the thermal expansion coefficient of the copper foil is relatively small, therefore, in the formed weld 2231, the second connection area 2231b of the negative electrode is recessed in the second bending section 2221b of the negative electrode.

[0111] In one possible implementation, the first connection area 2231a of the positive electrode protrudes from the first bending section 2211a of the positive electrode, and the height of the second connection area 2231b of the positive electrode protruding from the second bending section 2221a of the positive electrode is greater than the height of the first connection area 2231a of the positive electrode protruding from the first bending section 2211a of the positive electrode.

[0112] Since the expansion coefficients of the first pole ear and the second pole ear of the positive electrode are relatively large, the weld 2231 will protrude from the first bending section 2211a and the second bending section 2221a of the positive electrode at the same time, that is, the first connection area 2231a of the positive electrode protrudes from the first bending section 2211a of the positive electrode, and the second connection area 2231b of the positive electrode protrudes from the second bending section 2221a of the positive electrode. The welding protrusion of the weld 2231 as a whole can make the welding area 223 form a smooth and thinner thickness, thereby avoiding the waste of space in the accommodating cavity 110, thereby improving the energy density of the battery.

[0113] The height of the second connection area 2231b of the positive electrode protruding from the second bending section 2221a of the positive electrode is in the range of 0-100 μm, and the height of the first connection area 2231a of the positive electrode protruding from the first bending section 2211a of the positive electrode is in the range of 0.5-20 μm.

[0114] For example, the height of the second connection area 2231b of the positive electrode protruding from the second bending section 2221a of the positive electrode is any one of 5μm, 10μm, 30μm, 50μm, 65μm, and 100μm, or is within any two numerical ranges, and the height of the first connection area 2231a of the positive electrode protruding from the first bending section 2211a of the positive electrode is any one of 0.5μm, 1μm, 5μm, 10μm, 15μm, and 20μm, or is within any two numerical ranges.

[0115] In some embodiments, the first connection region 2231a of the negative electrode may be flush with the first bending section 2211b of the negative electrode, or the first connection region 2231a of the negative electrode may slightly protrude from the first bending section 2211b of the negative electrode.

[0116] In order to solve the problem of large welding protrusions in the welding area 223, in a possible implementation, the height of the second connection area 2231b of the positive electrode protruding from the second bending section 2221a of the positive electrode is less than or equal to 100um. The height of the second connection area 2231b of the negative electrode recessed in the second bending section 2221b of the negative electrode is less than or equal to 30um.

[0117] That is, the height of the second connection area 2231b of the positive electrode protruding relative to the second bending section 2221a of the positive electrode ranges from 0 to 100 μm, and the height of the second connection area 2231b recessed relative to the second bending section 2221b of the negative electrode ranges from 0 to 30 μm.

[0118] For example, the height of the second connection area 2231b of the positive electrode protruding from the second bending section 2221a of the positive electrode is any one of 1um, 5um, 10um, 20μm, 55μm, 65μm, 100μm or within any two numerical ranges, and the height of the second connection area 2231b of the negative electrode recessed in the second bending section 2221b of the negative electrode can be any one of 2um, 6um, 10um, 20μm, 30um or within any two numerical ranges.

[0119] In this way, the welding area 223 can achieve a lower welding protrusion, prevent the welding protrusion from piercing the insulating layer 224, and further avoid the first pole ear 221 or the second pole ear 222 from contacting the pole piece, thereby improving the safety performance of the battery cell 200.

[0120] It should be noted that since the first pole ear of the positive electrode and the second pole ear of the positive electrode are made of aluminum foil, the surface of the aluminum foil has an oxide layer. Therefore, when laser welding the first pole ear of the positive electrode and the second pole ear of the positive electrode, a large number of welds 2231 are required, so as to improve the welding strength between the first pole ear of the positive electrode and the second pole ear of the positive electrode through multiple heat accumulation, and avoid damage to the pole ear unit 220 due to cold welding and exploded welding.

[0121] Specifically, the weld 2231 includes a positive electrode weld for connecting the first bending section 2211a of the positive electrode and the second bending section 2221a of the positive electrode, and a negative electrode weld for connecting the first bending section 2211b of the negative electrode and the second bending section 2221b of the negative electrode.

[0122] Among them, the number of positive electrode welds is greater than or equal to the number of negative electrode welds, and less than or equal to 5 of the number of negative electrode welds.

[0123] For example, when laser welding the first electrode tab and the second electrode tab of the negative electrode, the number of positive electrode welds can be one, and when laser welding the first electrode tab and the second electrode tab of the positive electrode, the number of negative electrode welds can be any number from one to five.

[0124] In a possible implementation, the battery cell body may include a pole piece and a diaphragm, which are stacked in sequence along a first direction, and the diaphragm is adjacent to the welding area 223 along a second direction, or the diaphragm and the welding area 223 have a third gap along the second direction.

[0125] That is to say, the diaphragm will not contact the welding area 223, thereby preventing the diaphragm from intervening in the welding area 223 to cause a cold weld, thereby preventing the diaphragm from affecting the welding strength of the welding area 223, thereby ensuring that the welding area 223 has a higher welding strength.

[0126] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present application.

Claims

1. A battery, characterized in that: A battery cell is provided, wherein the battery cell comprises a battery cell body and a tab unit, wherein the tab unit comprises a first tab and a second tab, wherein the first tab comprises a first bending section, and the second tab comprises a second bending section, wherein the first bending section connects the battery cell body and the second bending section; The first bending section and the second bending section at least partially overlap, and at least a portion of the first bending section and at least a portion of the second bending section overlapping each other are welded to form a welding area; The extending length of the welding area along the first direction is greater than or equal to 0.3 of the extending length of the battery body along the first direction, and less than or equal to 0.8 of the extending length of the battery body along the first direction; The first direction is along the thickness direction of the battery cell body, and the second direction is perpendicular to the first direction.

2. The battery according to claim 1, characterized in that The battery cell body, the first bending section and the second bending section are all located in the accommodating cavity. The second pole ear also includes a straight section, which is connected to an end of the second bending section away from the first bending section and extends along a second direction to the outside of the accommodating cavity. At least a portion of the straight section and at least a portion of the shell are heat-melted to form a bonding area, and a first gap is formed between the welding area and the bonding area along the second direction.

3. The battery according to claim 2, characterized in that An extension length of the welding area along the second direction is greater than or equal to 0.1 of the first gap and less than or equal to 0.95 of the first gap.

4. The battery according to claim 1, characterized in that The extension length of the welding area along the second direction is greater than or equal to 85 μm and less than or equal to 300 μm; And / or, the extension length of the battery cell body along the first direction is greater than or equal to 1 mm and less than or equal to 5 mm; And / or, an extension length of the welding area along the first direction is greater than or equal to 0.3 mm and less than or equal to 0.8 mm.

5. The battery according to claim 1, characterized in that The distance between the two ends of the first bending section and the second bending section that are away from each other along the first direction is greater than or equal to 0.2 of the extension length of the battery cell body along the first direction, and less than or equal to the extension length of the battery cell body along the first direction; And / or, a distance between two ends of the first bending section and the second bending section that are away from each other along the first direction is greater than or equal to 0.6 mm and less than or equal to 3 mm.

6. The battery according to claim 1, characterized in that The welding area has at least one welding seam, and the projection of the welding seam on the first bending section is linear, or the projection of the welding seam on the first bending section is point-shaped.

7. The battery according to claim 6, characterized in that The weld includes a first connection area and a second connection area connected to each other, the first connection area is located in the first bending section, and the second connection area is located in the second bending section; At least a portion of the first connection area protrudes from the first bending section, and / or at least a portion of the second connection area protrudes from the second bending section.

8. The battery according to claim 7, characterized in that An extension length of the first connection region along the first direction is shorter than an extension length of the second connection region along the first direction.

9. The battery according to claim 6, characterized in that The projection of the weld on the surface of the first electrode tab is in a curved shape.

10. The battery according to claim 6, characterized in that The tab unit further includes an insulating layer, which is disposed on two opposite sides of the welding area, and a projection of the insulating layer on the first bending section covers the welding area.

11. The battery according to claim 10, characterized in that The welding area has at least two welding seams, and a second gap is provided between two adjacent welding seams.

12. The battery according to claim 11, characterized in that The second gap is greater than or equal to 0.3 of an extension length of the insulating layer along the first direction, and less than or equal to 0.9 of an extension length of the insulating layer along the first direction.

13. The battery according to claim 7 or 8, characterized in that: The first bending section includes a first bending section of the positive electrode and a first bending section of the negative electrode, the second bending section includes a second bending section of the positive electrode and a second bending section of the negative electrode, and the second connecting area includes a second connecting area of ​​the positive electrode and a second connecting area of ​​the negative electrode; The second connection area of ​​the positive electrode protrudes from the second bending section of the positive electrode, and the height of the second connection area of ​​the positive electrode protruding from the second bending section of the positive electrode is less than or equal to 100 μm; And / or, the second connection region of the negative electrode is recessed in the second bending section of the negative electrode, and the height of the second connection region of the negative electrode recessed in the second bending section of the negative electrode is less than or equal to 30 μm.

14. The battery according to claim 13, characterized in that The first connection area includes a first connection area of ​​the positive electrode, and the height of the second connection area of ​​the positive electrode protruding from the second bending section of the positive electrode is greater than the height of the first connection area of ​​the positive electrode protruding from the first bending section of the positive electrode; And / or, the height of the first connection area of ​​the positive electrode protruding from the first bending section of the positive electrode is greater than or equal to 0.5 μm and less than or equal to 20 μm.

15. The battery according to claim 13, characterized in that The weld includes a positive electrode weld connecting the first bending section of the positive electrode and the second bending section of the positive electrode, and a negative electrode weld connecting the first bending section of the negative electrode and the second bending section of the negative electrode; The number of the positive electrode welds is greater than or equal to the number of the negative electrode welds, and less than or equal to 5 of the number of the negative electrode welds.

16. The battery according to claim 6, characterized in that The projection of the weld on the surface of the first bending section is curved, the weld has wave crests, and the spacing between adjacent wave crests is greater than 0.1 mm and less than or equal to 2 mm.

17. The battery according to any one of claims 1 to 8, characterized in that: The first bending section and the second bending section are laser welded.

18. The battery according to any one of claims 1 to 8, characterized in that: The battery cell body comprises a pole piece and a diaphragm, the pole piece and the diaphragm are stacked in sequence, the diaphragm is adjacent to the welding area along the second direction; or, the diaphragm and the welding area have a third gap along the second direction.