Copper foil composite heat insulation pressing equipment

By using correction and clamping components in copper foil composite thermal insulation pressing equipment, the misalignment and slip problems caused by skewed angle of copper foil during the hot pressing process are solved, and the stable clamping and high-quality hot pressing effect of copper foil is achieved. .

CN222077783UActive Publication Date: 2024-11-29CHANGDE KE RUIFEI ELECTRONIC TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420067932.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-10
Publication Date
2024-11-29
Estimated Expiration
2034-01-10

AI Technical Summary

Technical Problem

During the hot pressing of copper foil, the copper foil and materials may experience angular skew after long distance displacement on the equipment, resulting in problems such as misalignment, slippage, and wrinkles.

Method used

A copper foil composite heat-insulating pressing equipment is designed, including a calibration assembly, a clamping assembly and a pressing assembly. The copper foil is angled and clamped through a clamping and traction mechanism driven by an electric slide rail and a motor. Ensure the stability of the material during the hot pressing process.

Benefits of technology

It effectively avoids the misalignment, slip and wrinkle problems caused by angle skew during the hot pressing process, ensuring the flatness of the copper foil and the high-quality hot pressing effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222077783U_ABST
    Figure CN222077783U_ABST
Patent Text Reader

Abstract

The utility model relates to the field of copper foil processing, in particular to copper foil composite heat insulation pressing equipment. The technical problems that in the copper foil hot-pressing process, after the copper foil and a material are subjected to long-distance displacement on equipment, the angles of the copper foil and the material possibly incline slightly, and therefore the hot-pressed copper foil possibly has the problems of dislocation, slippage, wrinkles and the like are solved. According to the technical scheme, the copper foil composite heat insulation pressing equipment comprises a correcting assembly, a clamping assembly and a pressing assembly. By arranging the correcting mechanism and the clamping traction mechanism, the angle of a material is corrected before the material is clamped, and the material can be clamped after the angle is corrected, so that the material is not easy to incline when the material is pulled, and the problem that in the copper foil hot-pressing process, after the copper foil and the material are subjected to long-distance displacement on equipment, the copper foil and the material cannot incline easily is solved to a certain extent. And the angle of the hot-pressed copper foil can slightly incline, so that the hot-pressed copper foil can have the problems of dislocation, slippage, wrinkles and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of copper foil processing, in particular to a copper foil composite heat insulation pressing device. Background Art

[0002] With the continuous development of science and technology, the performance requirements for electronic products are getting higher and higher, especially the demand for thin, high-performance electronic products is increasing. Copper foil, as an important electronic material, is widely used in the manufacture of electronic products. Copper foil has excellent electrical conductivity, electromagnetic shielding performance and high strength, and is widely used in the conductive layer, electromagnetic shielding layer and structural support of electronic circuits. However, after the copper foil and materials have been displaced over a long distance on the equipment, their own angles may be slightly skewed, which may cause the hot-pressed copper foil to have problems such as dislocation, slippage, and wrinkles. Utility Model Content

[0003] In order to overcome the problem that during the hot pressing process of copper foil, the angles of the copper foil and materials may be slightly skewed after a long distance displacement on the equipment, which may cause the hot pressed copper foil to be misaligned, slipped, wrinkled, etc.

[0004] The technical solution of the utility model is: a copper foil composite heat insulation pressing device, comprising a correction component, a clamping component, and a pressing component; the rear end of the correction component is provided with a clamping component for clamping the copper foil; the rear end of the clamping component is provided with a pressing component for pressing the copper foil.

[0005] Preferably, the correction component is used to correct the copper foil, the clamping component is used to clamp the copper foil, and the pressing component is used to press the copper foil.

[0006] Preferably, the correction assembly includes a base plate, a first electric slide rail, a first electric slider, and a correction plate; the first electric slide rail is disposed at the front end of the base plate; the first electric slide rail is electrically connected to the first electric slider; the correction plate is fixed to the first electric slider. The first electric slider slides in the first electric slide rail to slide the correction plate, so that the correction plate with adjusted position can correct the angle of the copper foil.

[0007] Preferably, the clamping assembly includes a first fixed frame, a lower fixed roller, a first motor, a second electric slide rail, a second electric slider, a slide, an upper fixed roller, and a second motor; the first fixed frame is fixedly connected to the upper end surface of the rear end of the first electric slider and the rear end of the bottom plate; the lower fixed roller is rotatably connected to the first fixed frame; one side of the lower fixed roller is rotatably connected to the first motor fixed to the first fixed frame through a coupling; the upper end of the first fixed frame is fixedly connected to the second electric slide rail; the second electric slider is electrically connected to the second electric slide rail; the slide is fixedly connected to the second electric slider; the upper fixed roller is rotatably connected to the slide; one side of the upper fixed roller is rotatably connected to the second motor fixed to the slide through a coupling. The first motor rotates the lower fixed roller clockwise, the second motor rotates the upper fixed roller counterclockwise, and the second electric slider slides downward on the second electric slide rail, which can cause the upper fixed roller to move downward, so that the upper fixed roller and the lower fixed roller clamp and pull the copper foil.

[0008] Preferably, the pressing assembly includes a second fixed frame, a third fixed frame, a fourth fixed frame, a first heating roller, a third motor, a gear, a second heating roller, a fourth motor, a fan, a hydraulic cylinder, a sleeve, a guide rod, a spring, a connecting block, a third heating roller, a heating ring, a heat insulation layer, and a fifth motor; the rear end of the first fixed frame is provided with a second fixed frame; the rear end of the second fixed frame is provided with a third fixed frame; the third fixed frame is fixedly connected to the fourth fixed frame; the second fixed frame is rotatably connected to two first heating rollers; one side of the first heating roller at the front end is rotatably connected to the third motor through a coupling; the other sides of the two first heating rollers are fixedly connected to mutually meshing gears. The third motor causes the first heating roller at the front end to rotate clockwise, and the first heating roller at the front end rotates counterclockwise through the gear, and the heating ring in the first heating roller preheats the copper foil.

[0009] Preferably, the third fixed frame is rotatably connected to a second heating roller; one side of the second heating roller is rotatably connected to a fourth motor via a coupling; a fan fixed to the bottom plate is provided at the rear end of the second heating roller. The fourth motor rotates the second heating roller clockwise, and the fan cools the copper foil after hot pressing.

[0010] Preferably, a hydraulic cylinder is fixedly connected to the fourth fixed frame; a sleeve is fixedly connected to the lower end of the hydraulic cylinder; a guide rod is slidably connected in the sleeve; a spring is arranged outside the lower end of the guide rod; a connecting block is fixedly connected to the lower end of the guide rod; a third heating roller is rotatably connected to the connecting block; a fifth motor is rotatably connected to one side of the third heating roller through a coupling. The hydraulic cylinder moves the third heating roller downward so that the third heating roller and the second heating roller can press the copper foil, and the fifth motor rotates the third heating roller counterclockwise so that the copper foil is pulled.

[0011] Preferably, the first heating roller, the second heating roller and the third heating roller are all fixedly connected with heating rings, and the heating power of the heating ring inside the first heating roller is relatively low; the outer sides of the second heating roller and the third heating roller are provided with heat insulation layers. The heating rings are used to heat the copper foil, and the heat insulation layers are used to prevent the high temperature on the surfaces of the second heating roller and the third heating roller from damaging the processed copper foil.

[0012] Beneficial effects of the utility model:

[0013] 1. By setting up a correction mechanism and a clamping and pulling mechanism, the material is first corrected before being clamped. After the angle is corrected, the material can be clamped so that the angle is not easy to tilt when the material is pulled. This solves the problem that during the hot pressing of copper foil, the copper foil and the material may be slightly skewed after a long distance displacement on the equipment, which may cause the hot pressed copper foil to be dislocated, slipped, wrinkled, etc.

[0014] 2. The correction plate is slid by the first electric slider in the first electric slide rail until the distance between the two correction plates is just equal to the width of the material, and the material is passed through the middle of the two correction plates, so that the correction plates with adjusted positions can correct the angle of the copper foil;

[0015] 3. The lower fixed roller is rotated clockwise by the first motor, and the upper fixed roller is rotated counterclockwise by the second motor. The second electric slider slides downward on the second electric slide rail, so that the upper fixed roller can be displaced downward, so that the upper fixed roller and the lower fixed roller can clamp and pull the copper foil passing through the middle of the upper fixed roller and the lower fixed roller, thereby preventing the material from being skewed during displacement. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 What is shown is a schematic diagram of the overall structure of the utility model;

[0017] Figure 2 Shown is a schematic diagram of the second electric slide structure of the utility model;

[0018] Figure 3 What is shown is a schematic diagram of the gear structure of the utility model;

[0019] Figure 4 What is shown is a schematic diagram of the guide rod structure of the utility model.

[0020] Description of reference numerals: 1. correction assembly; 2. clamping assembly; 3. pressing assembly; 101. bottom plate; 102. first electric slide rail; 103. first electric slider; 104. correction plate; 201. first fixed frame; 202. lower fixed roller; 203. first motor; 204. second electric slide rail; 205. second electric slider; 206. slide frame; 207. upper fixed roller; 208. second motor; 301. second fixed frame Fixed frame; 302, third fixed frame; 303, fourth fixed frame; 304, first heating roller; 305, third motor; 306, gear; 307, second heating roller; 308, fourth motor; 309, fan; 310, hydraulic cylinder; 311, sleeve; 312, guide rod; 313, spring; 314, connecting block; 315, third heating roller; 316, heating ring; 317, thermal insulation layer; 318, fifth motor. DETAILED DESCRIPTION

[0021] The utility model is further described below in conjunction with the accompanying drawings and embodiments.

[0022] See also Figure 1-2The utility model provides an embodiment: a copper foil composite heat insulation pressing device, comprising a correction component 1, a clamping component 2, and a pressing component 3; the rear end of the correction component 1 is provided with a clamping component 2 for clamping the copper foil; the rear end of the clamping component 2 is provided with a pressing component 3 for pressing the copper foil. The correction component 1 is used to correct the copper foil, the clamping component 2 is used to clamp the copper foil, and the pressing component 3 is used to press the copper foil. The correction component 1 comprises a bottom plate 101, a first electric slide rail 102, a first electric slider 103, and a correction plate 104; the front end of the bottom plate 101 is provided with a first electric slide rail 102; the first electric slider 103 is electrically connected to the first electric slide rail 102; the correction plate 104 is fixed to the first electric slider 103. The first electric slider 103 slides in the first electric slide rail 102 to slide the correction plate 104, so that the correction plate 104 with the adjusted position can correct the angle of the copper foil. The clamping assembly 2 includes a first fixed frame 201, a lower fixed roller 202, a first motor 203, a second electric slide rail 204, a second electric slider 205, a slide 206, an upper fixed roller 207, and a second motor 208; the first fixed frame 201 is fixedly connected to the rear end of the first electric slider 103 and the upper end surface of the rear end of the bottom plate 101; the first fixed frame 201 is rotatably connected to the lower fixed roller 202; one side of the lower fixed roller 202 is rotatably connected to the first motor 203 fixed to the first fixed frame 201 through a coupling; the second electric slide rail 204 is fixed to the upper end of the first fixed frame 201; the second electric slider 205 is electrically connected to the second electric slide rail 204; the slide 206 is fixed to the second electric slider 205; the upper fixed roller 207 is rotatably connected to the slide 206; one side of the upper fixed roller 207 is rotatably connected to the second motor 208 fixed to the slide 206 through a coupling. The first motor 203 rotates the lower fixed roller 202 clockwise, the second motor 208 rotates the upper fixed roller 207 counterclockwise, and the second electric slider 205 slides downward on the second electric slide rail 204 to move the upper fixed roller 207 downward, so that the upper fixed roller 207 and the lower fixed roller 202 clamp and pull the copper foil.

[0023] See also Figure 3-4In this embodiment, as a preference, the pressing assembly 3 includes a second fixed frame 301, a third fixed frame 302, a fourth fixed frame 303, a first heating roller 304, a third motor 305, a gear 306, a second heating roller 307, a fourth motor 308, a fan 309, a hydraulic cylinder 310, a sleeve 311, a guide rod 312, a spring 313, a connecting block 314, a third heating roller 315, a heating ring 316, an insulating layer 317, and a fifth motor 318; the rear end of the first fixed frame 201 is provided with a second fixed frame 301; the rear end of the second fixed frame 301 is provided with a third fixed frame 302; the third fixed frame 302 is fixedly connected to the fourth fixed frame 303; the second fixed frame 301 is rotatably connected to two first heating rollers 304; one side of the first heating roller 304 at the front end is rotatably connected to the third motor 305 through a coupling; the other sides of the two first heating rollers 304 are fixedly connected to mutually meshing gears 306. The third motor 305 rotates the first heating roller 304 at the front end in a clockwise direction, and the first heating roller 304 at the front end rotates the first heating roller 304 at the rear end in a counterclockwise direction through the gear 306, and at the same time, the heating ring 316 in the first heating roller 304 preheats the copper foil. The second heating roller 307 is rotatably connected to the third fixed frame 302; one side of the second heating roller 307 is rotatably connected to the fourth motor 308 through a coupling; the rear end of the second heating roller 307 is provided with a fan 309 fixed to the bottom plate 101. The fourth motor 308 rotates the second heating roller 307 in a clockwise direction, and the fan 309 cools the copper foil after the hot pressing. A hydraulic cylinder 310 is fixedly connected to the fourth fixed frame 303; a sleeve 311 is fixedly connected to the lower end of the hydraulic cylinder 310; a guide rod 312 is slidably connected in the sleeve 311; a spring 313 is arranged on the outer side of the lower end of the guide rod 312; a connecting block 314 is fixedly connected to the lower end of the guide rod 312; a third heating roller 315 is rotatably connected to the connecting block 314; a fifth motor 318 is rotatably connected to one side of the third heating roller 315 through a coupling. The hydraulic cylinder 310 moves the third heating roller 315 downward so that the third heating roller 315 and the second heating roller 307 can press the copper foil, and the fifth motor 318 rotates the third heating roller 315 counterclockwise, so that the copper foil is pulled. The first heating roller 304, the second heating roller 307 and the third heating roller 315 are all fixedly connected with a heating ring 316, and the heating power of the heating ring 316 inside the first heating roller 304 is relatively low; the outer sides of the second heating roller 307 and the third heating roller 315 are provided with a heat insulating layer 317. The heating ring 316 is used to heat the copper foil, and the heat insulating layer 317 is used to prevent the high temperature on the surface of the second heating roller 307 and the third heating roller 315 from damaging the processed copper foil.

[0024] When working, the first electric slider 103 slides in the first electric slide rail 102 to slide the correction plate 104 until the distance between the two correction plates 104 is just equal to the width of the material, and the material is allowed to pass through the middle of the two correction plates 104, so that the correction plates 104 with adjusted positions can correct the angle of the copper foil, and then the material and the copper foil are pulled between the upper fixed roller 207 and the lower fixed roller 202;

[0025] Subsequently, the first motor 203 rotates the lower fixed roller 202 in a clockwise direction, the second motor 208 rotates the upper fixed roller 207 in a counterclockwise direction, and the second electric slider 205 slides downward on the second electric slide rail 204, so that the upper fixed roller 207 can be displaced downward, so that the upper fixed roller 207 and the lower fixed roller 202 can clamp and pull the copper foil passing through the upper fixed roller 207 and the lower fixed roller 202, thereby preventing the material from being skewed during displacement;

[0026] Next, the material passes through the middle of the two first heating rollers 304, and the third motor 305 makes the front first heating roller 304 rotate clockwise, while the front first heating roller 304 passes through the gear 306 to make the rear first heating roller 304 rotate counterclockwise, and at the same time, the heating ring 316 in the first heating roller 304 preheats the copper foil;

[0027] Next, the copper foil and the material are passed through the middle of the second heating roller 307 and the third heating roller 315, and then the hydraulic cylinder 310 moves the third heating roller 315 downward so that the third heating roller 315 and the second heating roller 307 can press the copper foil, and at the same time the fifth motor 318 rotates the third heating roller 315 counterclockwise, and the fourth motor 308 rotates the second heating roller 307 clockwise, and the heating ring 316 is used to heat the copper foil, and the heat insulation layer 317 is used to prevent the high temperature on the surface of the second heating roller 307 and the third heating roller 315 from damaging the processed copper foil, so as to heat-press the material;

[0028] Finally, the upper fixed roller 207 and the lower fixed roller 202 at the rear end of the equipment clamp and pull the copper foil passing through the middle of the upper fixed roller 207 and the lower fixed roller 202 to pull the hot-pressed copper foil to other equipment, and the fan 309 cools the hot-pressed copper foil.

[0029] Through the above steps, the correction mechanism and the clamping and pulling mechanism are set so that the angle of the material can be corrected before being clamped. After the angle is corrected, the material can be clamped so that the angle is not easy to tilt when the material is pulled, thereby solving to a certain extent the problem that during the hot pressing process of the copper foil, the copper foil and the material may be slightly skewed after a long distance displacement on the equipment, which may cause the hot pressed copper foil to be misaligned, slipped, wrinkled and other problems.

[0030] The embodiments of the present invention are described in detail above in conjunction with the accompanying drawings, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of those skilled in the art without departing from the purpose of the present invention.

Claims

1. A copper foil composite heat insulation pressing device, comprising a correction component (1); Features: It also comprises a clamping component (2) and a pressing component (3); the rear end of the correction component (1) is provided with a clamping component (2) for clamping the copper foil; the rear end of the clamping component (2) is provided with a pressing component (3) for pressing the copper foil.

2. A copper foil composite heat insulation pressing device according to claim 1, Features: The correction component (1) comprises a base plate (101), a first electric slide rail (102), a first electric slider (103), and a correction plate (104); the first electric slide rail (102) is arranged at the front end of the base plate (101); the first electric slide rail (102) is electrically connected to the first electric slider (103); and the correction plate (104) is fixedly connected to the first electric slider (103).

3. A copper foil composite heat insulation pressing device according to claim 2, Features: The clamping assembly (2) comprises a first fixed frame (201), a lower fixed roller (202), a first motor (203), a second electric slide rail (204), a second electric slider (205), a slide frame (206), an upper fixed roller (207), and a second motor (208); the first fixed frame (201) is fixedly connected to the rear end of the first electric slider (103) and the upper end surface of the rear end of the bottom plate (101); the first fixed frame (201) is rotatably connected to the lower fixed roller (202); one side of the lower fixed roller (202) is connected to the lower fixed roller (207) by a coupling. The device is rotatably connected to a first motor (203) fixedly connected to a first fixed frame (201); a second electric slide rail (204) is fixedly connected to the upper end of the first fixed frame (201); a second electric slider (205) is electrically connected to the second electric slide rail (204); a slide frame (206) is fixedly connected to the second electric slider (205); an upper fixed roller (207) is rotatably connected to the slide frame (206); one side of the upper fixed roller (207) is rotatably connected to a second motor (208) fixedly connected to the slide frame (206) through a coupling.

4. A copper foil composite insulation pressing device according to claim 3, Features: The pressing assembly (3) comprises a second fixing frame (301), a third fixing frame (302), a fourth fixing frame (303), a first heating roller (304), a third motor (305), a gear (306), a second heating roller (307), a fourth motor (308), a fan (309), a hydraulic cylinder (310), a sleeve (311), a guide rod (312), a spring (313), a connecting block (314), a third heating roller (315), a heating ring (316), a heat insulating layer (317), and a fifth motor (31 8); a second fixing frame (301) is arranged at the rear end of the first fixing frame (201); a third fixing frame (302) is arranged at the rear end of the second fixing frame (301); a fourth fixing frame (303) is fixedly connected to the third fixing frame (302); two first heating rollers (304) are rotatably connected to the second fixing frame (301); one side of the first heating roller (304) at the front end is rotatably connected to a third motor (305) via a coupling; and the other sides of the two first heating rollers (304) are fixedly connected to mutually meshing gears (306).

5. A copper foil composite heat insulation pressing device according to claim 4, Features: A second heating roller (307) is rotatably connected to the third fixed frame (302); one side of the second heating roller (307) is rotatably connected to a fourth motor (308) via a coupling; a fan (309) fixedly connected to the bottom plate (101) is provided at the rear end of the second heating roller (307).

6. A copper foil composite heat insulation pressing device according to claim 4, Features: A hydraulic cylinder (310) is fixedly connected to the fourth fixed frame (303); a sleeve (311) is fixedly connected to the lower end of the hydraulic cylinder (310); a guide rod (312) is slidably connected inside the sleeve (311); a spring (313) is arranged on the outer side of the lower end of the guide rod (312); a connecting block (314) is fixedly connected to the lower end of the guide rod (312); a third heating roller (315) is rotatably connected to the connecting block (314); and a fifth motor (318) is rotatably connected to one side of the third heating roller (315) via a coupling.

7. The copper foil composite heat insulation pressing device according to claim 4, Features: The first heating roller (304), the second heating roller (307) and the third heating roller (315) are all fixedly connected with a heating ring (316) inside, and the heating power of the heating ring (316) inside the first heating roller (304) is relatively low; A heat insulating layer (317) is provided on the outer sides of the second heating roller (307) and the third heating roller (315).