NdFeB powder forming adjustable mold

By designing an adjustable neodymium iron boron powder molding mold, the combined structure of magnetic permeable plate and slider is used to adjust the mold size, the problems of frequent depressing deformation and mold replacement during the sintering of traditional neodymium iron boron magnets are solved, and the product qualification is improved rate and productivity.

CN222077957UActive Publication Date: 2024-11-29BAOTOU KETIAN MAGNET CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420388184.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-29
Publication Date
2024-11-29
Estimated Expiration
2034-02-28

AI Technical Summary

Technical Problem

Traditional neodymium iron boron magnets are prone to depressed and deformed in the middle and surface during sintering, resulting in low product qualification rate and frequent mold replacement affects production efficiency and increases costs.

Method used

A neodymium iron boron powder molding adjustable mold is designed, using parallel-arranged magnetic perforation plates and sliders. The slide movement is driven by the adjustment screw to adjust the mold size, reduce friction and improve molding accuracy.

Benefits of technology

It effectively reduces the depressed deformation of the magnet surface during sintering, shortens the mold replacement time, and improves production efficiency and product qualification rate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222077957U_ABST
    Figure CN222077957U_ABST
Patent Text Reader

Abstract

The utility model discloses an adjustable mold for neodymium iron boron powder forming. The adjustable mold comprises a first magnetic conductive plate and a second magnetic conductive plate which are arranged in parallel, the first sliding block and the second sliding block are arranged between the first magnetic conductive plate and the second magnetic conductive plate in a sliding manner; and the first adjusting screw rod and the second adjusting screw rod respectively drive the first sliding block and the second sliding block to move towards each other or move away from each other. According to the adjustable die, the fixing blocks and the adjusting screw rods are arranged, so that the die assembling time is shortened, and the forming production efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of NdFeB magnets, in particular to an adjustable mold for NdFeB powder molding. Background Art

[0002] The traditional production process of NdFeB magnets includes smelting process, molding process, sintering process, etc. The molding process includes: placing NdFeB powder into a mold, and then pressing it into NdFeB magnet blocks. Due to the bidirectional molding of the magnetic field molding press, large NdFeB magnets are prone to concave deformation in the middle and / or near the middle of the product during the sintering process, resulting in a lower product qualification rate, which directly affects the subsequent work and increases production costs. In addition, as the pressing depth increases, the friction between the mold cavity and the powder increases exponentially, and friction is an important reason affecting the appearance qualification rate of the molded product. At the same time, the specifications of NdFeB blank orders are relatively messy, the quantity of each order is small, and molding requires frequent mold changes, which directly affects production efficiency and increases production costs. Utility Model Content

[0003] In view of this, the purpose of the utility model is to provide an adjustable mold for NdFeB powder molding to shorten the time for molding and replacing the mold.

[0004] In order to achieve the above purpose, the technical solution adopted by the utility model is:

[0005] An adjustable mold for forming NdFeB powder, comprising:

[0006] A first magnetic conductive plate and a second magnetic conductive plate arranged in parallel;

[0007] A first slider and a second slider slidably arranged between the first magnetic conductive plate and the second magnetic conductive plate;

[0008] A first adjusting screw and a second adjusting screw are respectively driven to move the first slider and the second slider toward or away from each other.

[0009] The above-mentioned adjustable mold for forming NdFeB powder, wherein, further comprises:

[0010] A first fixing plate and a second fixing plate fixedly arranged between the first magnetic conductive plate and the second magnetic conductive plate;

[0011] Among them, the first adjusting screw passes through the first fixing plate and is connected to the first sliding block, the external thread of the first adjusting screw matches the internal thread of the first fixing plate, the second adjusting screw passes through the second fixing plate and is connected to the second sliding block, and the external thread of the second adjusting screw matches the internal thread of the second fixing plate.

[0012] The above-mentioned adjustable mold for forming NdFeB powder, wherein, further comprises:

[0013] A first connecting member that sequentially penetrates and fixes the first magnetic conductive plate, the first fixing plate, and the second magnetic conductive plate;

[0014] A second connecting piece sequentially penetrates and fixes the first magnetic conductive plate, the second fixing plate, and the second magnetic conductive plate.

[0015] The above-mentioned adjustable mold for forming NdFeB powder, wherein, further comprises:

[0016] A first hard alloy plate is attached to the inner wall of the first magnetic conductive plate, and a second hard alloy plate is attached to the inner wall of the second magnetic conductive plate, wherein the first slider and the second slider are both located between the first hard alloy plate and the second hard alloy plate.

[0017] The above-mentioned adjustable mold for forming NdFeB powder, wherein a receiving cavity for receiving magnetic powder to be pressed and formed is formed between the first cemented carbide plate and the second cemented carbide plate.

[0018] The above-mentioned NdFeB powder molding adjustable mold, wherein each of the two sides of the first magnetic conductive plate and each of the two sides of the second magnetic conductive plate are provided with a positioning groove, and both ends of the first fixed plate and both ends of the second fixed plate are arranged in the positioning groove.

[0019] The above-mentioned adjustable mold for forming NdFeB powder, wherein the first fixing plate and the second fixing plate are both in a "convex" shape.

[0020] The above-mentioned NdFeB powder molding adjustable mold, wherein the first magnetic conductive plate and the second magnetic conductive plate are arranged in a first direction, the first slider and the second slider are arranged in a second direction perpendicular to the first direction, and are open in a third direction perpendicular to the first direction and the second direction.

[0021] The above-mentioned NdFeB powder molding adjustable mold, wherein the size in the first direction is determined by the first magnetic conductive plate and the second magnetic conductive plate, the size in the second direction is determined by the first slider and the second slider, and bidirectional molding is performed in the third direction by a magnetic field molding press.

[0022] The above-mentioned adjustable mold for forming NdFeB powder, wherein the first connecting member and the second connecting member are both threaded connecting members;

[0023] One of the first magnetic conductive plate and the second magnetic conductive plate is provided with a countersunk hole, and the other of the first magnetic conductive plate and the second magnetic conductive plate is correspondingly arranged with a threaded hole.

[0024] The above-mentioned NdFeB powder molding adjustable mold, wherein the first magnetic conductive plate and the second magnetic conductive plate are both made of magnetic conductive Cr12;

[0025] The first slider and the second slider are both made of non-magnetic G60 steel.

[0026] Due to the adoption of the above technology, the utility model has the following positive effects compared with the prior art:

[0027] (1) The adjustable mold of the utility model reduces the mold assembly time and improves the molding production efficiency by providing a fixed block and an adjusting screw.

[0028] (2) The utility model can reduce the occurrence of concave deformation on the surface of the magnet during the sintering process. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 It is a schematic diagram of the adjustable mold for forming NdFeB powder of the utility model.

[0030] Figure 2 It is a schematic diagram of a fixed mold in the prior art.

[0031] In the accompanying drawings: 11, first fixed plate; 12, second fixed plate; 13, first magnetic conductive plate; 14, second magnetic conductive plate; 15, first carbide plate; 16, second carbide plate; 17, first slider; 18, second slider; 21, first adjusting screw; 22, second adjusting screw; 23, first connecting member; 24, second connecting member. DETAILED DESCRIPTION

[0032] The technical solution of the utility model will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0033] In the description of the present invention, it is necessary to understand that the directions or positional relationships indicated by terms such as “upper”, “lower”, “left”, “right”, “inside”, “outside”, “front”, “back”, “lateral” and “vertical” are based on the directions or positional relationships shown in the accompanying drawings and are only for the convenience of describing the present invention. They do not indicate or imply that the device or component referred to must have a specific direction and therefore should not be understood as a limitation on the present invention.

[0034] It should be specially explained that the terms “horizontal” and “vertical” in the present invention are used to illustrate a rough positional relationship, rather than a strict “horizontal plane” or “vertical plane”.

[0035] See also Figure 1 As shown, a preferred embodiment of an adjustable mold for forming NdFeB powder is shown, including: a first magnetic conductive plate 13 and a second magnetic conductive plate 14 arranged in parallel, a first slider 17 and a second slider 18 slidably arranged between the first magnetic conductive plate 13 and the second magnetic conductive plate 14, and a first adjusting screw 21 and a second adjusting screw 22 respectively driving the first slider 17 and the second slider 18 to move toward or away from each other.

[0036] The distance between the first magnetic conductive plate 13 and the second magnetic conductive plate 14 is adjustable and fixed, and the distance between the first sliding block 17 and the second sliding block 18 is adjustable.

[0037] Preferably, the demoulding angle of the adjustable mold for NdFeB powder molding is 1 to 5°, preferably 1 to 3°.

[0038] In the utility model, the pressed magnet can be a square magnet, such as a large square magnet. In the magnetic powder molding process, the size of the mold can be quickly adjusted by the first adjusting screw 21 and the second adjusting screw 22 according to the different performance shrinkage, which basically does not affect the molding production efficiency. At the same time, in the magnetic powder pressing molding process, on the one hand, it is necessary to ensure that the magnetic properties of the obtained magnet are not affected. On the other hand, due to the large volume of the magnet, the surface of the middle part of the magnet is prone to concave deformation during the sintering process. The use of the pressing mold of the utility model can greatly reduce the generation of concave deformation.

[0039] Further, as a preferred embodiment, the adjustable mold for forming neodymium iron boron powder also includes: a first fixed plate 11 and a second fixed plate 12 fixedly arranged between the first magnetic conductive plate 13 and the second magnetic conductive plate 14; wherein, the first adjusting screw 21 passes through the first fixed plate 11 and is connected to the first slider 17, and the external thread of the first adjusting screw 21 matches the internal thread of the first fixed plate 11, and the second adjusting screw 22 passes through the second fixed plate 12 and is connected to the second slider 18, and the external thread of the second adjusting screw 22 matches the internal thread of the second fixed plate 12.

[0040] Specifically, by rotating the first adjusting screw 21, the first adjusting screw 21 rotates relative to the first fixing plate 11, so that the first adjusting screw 21 moves relative to the first fixing plate 11, thereby driving the first slider 17 to move. More specifically, the second adjusting screw 22 operates in the same manner.

[0041] Specifically, the end of the first adjusting screw 21 abuts against the first slider 17 to push the first slider 17 to move.

[0042] The size of the mold can be adjusted by adjusting the screw to push the slider back and forth, which reduces the mold assembly time and improves production efficiency.

[0043] Furthermore, as a preferred embodiment, the adjustable mold for forming NdFeB powder also includes: a first connecting member 23 that sequentially penetrates and fixes the first magnetic conductive plate 13, the first fixed plate 11, and the second magnetic conductive plate 14, and a second connecting member 24 that sequentially penetrates and fixes the first magnetic conductive plate 13, the second fixed plate 12, and the second magnetic conductive plate 14.

[0044] Furthermore, as a preferred embodiment, the adjustable mold for forming NdFeB powder also includes: a first carbide plate 15 attached to the inner wall of the first magnetic conductive plate 13, and a second carbide plate 16 attached to the inner wall of the second magnetic conductive plate 14, wherein the first slider 17 and the second slider 18 are both located between the first carbide plate 15 and the second carbide plate 16.

[0045] Further, as a preferred embodiment, a receiving cavity for receiving magnetic powder to be pressed is formed between the first cemented carbide plate 15 and the second cemented carbide plate 16 .

[0046] Preferably, the roughness of the inner surface of the accommodating cavity is less than or equal to 0.2 μm. Surface roughness refers to the unevenness of the small spacing and tiny peaks and valleys of the processed surface. This is conducive to reducing the friction between the inner surface of the accommodating cavity of the pressing mold and the magnet powder to be pressed, which is conducive to smooth demoulding.

[0047] Preferably, the thickness of the first cemented carbide plate 15 and the second cemented carbide plate 16 is 2-5 mm.

[0048] The arrangement of the first cemented carbide plate 15 and the second cemented carbide plate 16 is conducive to reducing the occurrence of surface concave deformation of the magnet, making the density of the magnet more uniform and improving the product qualification rate.

[0049] Furthermore, as a preferred embodiment, each of the two sides of the first magnetic conductive plate 13 and each of the two sides of the second magnetic conductive plate 14 are provided with positioning grooves, and both ends of the first fixed plate 11 and both ends of the second fixed plate 12 are arranged in the positioning grooves.

[0050] Furthermore, as a preferred embodiment, the first fixing plate 11 and the second fixing plate 12 are both in a "convex" shape.

[0051] Further, as a preferred embodiment, the first magnetic conductive plate 13 and the second magnetic conductive plate 14 are arranged in a first direction, the first slider 17 and the second slider 18 are arranged in a second direction perpendicular to the first direction, and are open in a third direction perpendicular to the first direction and the second direction.

[0052] The size in the first direction is determined by the first magnetic conductive plate 13 and the second magnetic conductive plate 14 , the size in the second direction is determined by the first slider 17 and the second slider 18 , and bidirectional forming is performed in the third direction by a magnetic field forming press.

[0053] For details, see Figure 1 As shown, the first direction is Figure 1 The up and down directions in the second direction are Figure 1 The left and right directions in the third direction are Figure 1 The direction perpendicular to the paper surface.

[0054] Among them, the second direction is the non-directional in this field, the first direction is the directional in this field, and the third direction is the compressive direction in this field.

[0055] Preferably, the NdFeB magnet forming adjustable mold of this embodiment has a non-axial diameter of 65-78 mm (adjustable), a compression diameter of 30-62 mm (adjustable), and an orientation diameter of 45-52 mm (adjustable). The density of the pressed magnet can reach 4.0-4.2 g / cm3.

[0056] More preferably, in certain specific embodiments, the adjustable mold for forming the NdFeB magnet has a non-axial length of 76 mm, a compression length of 61.5 mm, and an orientation length of 48 mm.

[0057] In other specific embodiments, the adjustable mold for forming NdFeB magnets has a non-directional diameter of 76.5 mm, a compressive diameter of 61.5 mm, and an oriented diameter of 50.7 mm.

[0058] Further, as a preferred embodiment, the first connecting member 23 and the second connecting member 24 are both threaded connecting members, especially adjustable screws.

[0059] Specifically, the distance between the first magnetic conductive plate 13 and the second magnetic conductive plate 14 is adjusted by the first connecting member 23 and the second connecting member 24 .

[0060] Further, as a preferred embodiment, one of the first magnetic conductive plate 13 and the second magnetic conductive plate 14 is provided with a countersunk hole, and the other of the first magnetic conductive plate 13 and the second magnetic conductive plate 14 is correspondingly arranged with a threaded hole.

[0061] Specifically, the countersunk hole and the threaded hole are matched with the first connecting member 23 and the second connecting member 24 .

[0062] Further, as a preferred embodiment, the first connecting member 23 and the second connecting member 24 are respectively located on both sides of the first cemented carbide plate 15 and the second cemented carbide plate 16 .

[0063] Furthermore, as a preferred embodiment, the first magnetic conductive plate 13 and the second magnetic conductive plate 14 are both made of magnetic conductive Cr12.

[0064] Furthermore, as a preferred embodiment, the first slider 17 and the second slider 18 are both made of non-magnetic G60 steel.

[0065] Furthermore, as a preferred embodiment, the first cemented carbide plate 15 and the second cemented carbide plate 16 are both made of non-magnetic G60 steel.

[0066] Preferably, the thickness of the first cemented carbide plate 15 and the second cemented carbide plate 16 may be 2 to 5 mm, preferably 3 to 5 mm.

[0067] Furthermore, as a preferred embodiment, the first fixing plate 11 and the second fixing plate 12 are both made of 304 stainless steel.

[0068] See also Figure 2 As shown, Figure 2 A schematic diagram of a fixed mold of the prior art is shown, which includes a first magnetic conductive plate located on the upper side, a second magnetic conductive plate located on the lower side, two non-adjustable parallel fasteners connecting the first magnetic conductive plate and the second magnetic conductive plate, and two pressure plates respectively located on the left and right sides and penetrated by the two fasteners.

[0069] Wherein, an accommodating cavity is formed between the first magnetic conductive plate, the second magnetic conductive plate and two pressing plates with a fixed interval.

[0070] use Figure 1 The adjustable mold for forming NdFeB powder of the utility model is used to press and sinter the magnetic powder to be pressed and formed. The surface roughness of the accommodating cavity is 0.25 μm. The non-directional diameter of the mold is 72 mm, the compression direction is 64 mm, and the orientation direction is 52 mm, thereby obtaining Example 1.

[0071] use Figure 1 The adjustable mold for forming NdFeB powder of the utility model is used to press and sinter the magnetic powder to be pressed and formed. The surface roughness of the accommodating cavity is 0.25 μm. The non-directional diameter of the mold is 74 mm, the compression direction is 45 mm, and the orientation direction is 50 mm, thereby obtaining Example 2.

[0072] use Figure 1 The adjustable mold for forming NdFeB powder of the utility model is used to press and sinter the magnetic powder to be pressed and formed. The surface roughness of the accommodating cavity is 0.25 μm. The non-directional diameter of the mold is 66 mm, the compression direction is 50 mm, and the orientation direction is 50 mm, thereby obtaining Example 3.

[0073] use Figure 2 The fixed mold of the prior art shown is used to press and sinter the magnetic powder to be pressed, thereby obtaining Comparative Example 1.

[0074] Examples 1 to 3 and Comparative Example 1 were analyzed, and the results are shown in Table 1.

[0075] Table 1

[0076] serial number Mold time Deformation rate / % Example 1 0.1h 0.2 Example 2 0.1h 0.1 Example 3 0.15h 0.18 Comparative Example 1 0.45h 1.5

[0077] It can be seen from Table 1 that, compared with Comparative Example 1, the mold replacement time of the adjustable mold for forming the NdFeB magnets of Examples 1 to 3 is significantly reduced, the deformation rate of the product is significantly reduced, the product qualification rate is significantly improved, and the production efficiency is improved.

[0078] The above description is only a preferred embodiment of the present invention, and does not limit the implementation mode and protection scope of the present invention. For those skilled in the art, it should be aware that all solutions obtained by equivalent substitutions and obvious changes made using the description and illustrations of the present invention should be included in the protection scope of the present invention.

Claims

1. An adjustable mold for forming NdFeB powder, characterized in that: include: A first magnetic conductive plate and a second magnetic conductive plate arranged in parallel; A first slider and a second slider slidably arranged between the first magnetic conductive plate and the second magnetic conductive plate; A first adjusting screw and a second adjusting screw are respectively driven to move the first slider and the second slider toward or away from each other.

2. The adjustable mold for forming NdFeB powder according to claim 1, characterized in that: Also includes: A first fixing plate and a second fixing plate fixedly arranged between the first magnetic conductive plate and the second magnetic conductive plate; Among them, the first adjusting screw passes through the first fixing plate and is connected to the first sliding block, the external thread of the first adjusting screw matches the internal thread of the first fixing plate, the second adjusting screw passes through the second fixing plate and is connected to the second sliding block, and the external thread of the second adjusting screw matches the internal thread of the second fixing plate.

3. The adjustable mold for forming NdFeB powder according to claim 2, characterized in that: Also includes: A first connecting member that sequentially penetrates and fixes the first magnetic conductive plate, the first fixing plate, and the second magnetic conductive plate; A second connecting piece sequentially penetrates and fixes the first magnetic conductive plate, the second fixing plate, and the second magnetic conductive plate.

4. The adjustable mold for forming NdFeB powder according to claim 3, characterized in that: Also includes: A first hard alloy plate is attached to the inner wall of the first magnetic conductive plate, and a second hard alloy plate is attached to the inner wall of the second magnetic conductive plate, wherein the first slider and the second slider are both located between the first hard alloy plate and the second hard alloy plate.

5. The adjustable mold for forming NdFeB powder according to claim 4, characterized in that: A receiving cavity for receiving magnetic powder to be pressed and formed is formed between the first cemented carbide plate and the second cemented carbide plate.

6. The adjustable mold for forming NdFeB powder according to claim 2, characterized in that: Each of the two sides of the first magnetic conductive plate and each of the two sides of the second magnetic conductive plate are provided with positioning grooves, and both ends of the first fixing plate and both ends of the second fixing plate are arranged in the positioning grooves.

7. The adjustable mold for forming NdFeB powder according to claim 5, characterized in that: The first fixing plate and the second fixing plate are both in a "convex" shape.

8. The adjustable mold for forming NdFeB powder according to claim 1, characterized in that: The first magnetic conductive plate and the second magnetic conductive plate are arranged in a first direction, the first slider and the second slider are arranged in a second direction perpendicular to the first direction, and are open in a third direction perpendicular to the first direction and the second direction.

9. The adjustable mold for forming NdFeB powder according to claim 3, characterized in that: The first connecting member and the second connecting member are both threaded connecting members; One of the first magnetic conductive plate and the second magnetic conductive plate is provided with a countersunk hole, and the other of the first magnetic conductive plate and the second magnetic conductive plate is correspondingly arranged with a threaded hole.

10. The adjustable mold for forming NdFeB powder according to claim 1, characterized in that: The first magnetic conductive plate and the second magnetic conductive plate are both made of magnetic conductive Cr12; The first slider and the second slider are both made of non-magnetic G60 steel.