Maintenance device for casting copper bush
Through the copper sleeve repair device with high-speed grinding and spray grinding fluid cooling, the problems of low precision and high cost of copper sleeve assembly in traditional methods are solved, and higher precision of copper sleeve repair and lower cost of use are achieved. Improved the quality of the casting billet.
Patent Information
- Application Number
- CN202323483159.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-20
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2033-12-20
AI Technical Summary
The traditional copper sleeve repair method results in low assembly accuracy between copper sleeves and graphite molds, large processing errors, limited use times and high cost, making it difficult to cast high-quality casting billets.
Copper sleeve repair device including workbench, fixed pressure plate, high-speed rotating drilling machine spindle, grinding head and spraying mechanism is adopted. The copper sleeve inner hole is accurately polished and reduced processing by cooling through high-speed grinding and spraying grinding fluid. Error and grinding amount.
The surface roughness and assembly accuracy of the copper sleeve are improved, the cost of use is reduced, the service life of the copper sleeve is extended, and the casting quality of the casting billet is improved.
Smart Images

Figure CN222095321U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of ingot casting equipment, in particular to a repairing device for a copper sleeve used for casting. Background Art
[0002] In the copper tube manufacturing process, the casting quality of the ingot is very important. In the casting process of the ingot, the assembly accuracy of the graphite mold and the copper sleeve directly affects the casting performance of the ingot.
[0003] The traditional copper sleeve repair method is to turn the inner hole after each use. The general turning size is 0.5mm~0.7mm, and the surface roughness is generally Ra3μm~4μm. Due to the long size of the copper sleeve, the circumference of the root and end of the copper sleeve will produce a processing error of 1μm~3μm, and the processing error is large, which leads to low assembly accuracy with the graphite mold and difficulty in casting high-quality ingots. At the same time, due to the limitation of the size of the graphite mold, the maximum allowable turning size of the inner hole of the copper sleeve is 5mm, and its processing size is limited. Using the traditional copper sleeve repair method, the copper sleeve will reach the scrap standard after 8~10 repairs. In this way, the cost of each use of the copper sleeve is about 400 yuan, which is relatively costly.
[0004] Therefore, the applicant has found a solution to the above-mentioned problem through beneficial exploration and research, and the technical solution to be introduced below is produced in this context. Utility Model Content
[0005] The technical problem to be solved by the utility model is: in view of the deficiencies in the prior art, a repair device for a copper sleeve for casting is provided, which can improve the surface roughness of the inner hole of the copper sleeve, reduce the processing errors of the circumferential size of the root and the end of the copper sleeve, reduce the turning amount, reduce the use cost, and improve the assembly accuracy of the copper sleeve and the graphite mold.
[0006] The technical problem to be solved by the present invention can be achieved by adopting the following technical solutions:
[0007] A repair device for a copper sleeve for casting, comprising:
[0008] Workbench;
[0009] A copper sleeve fixing pressure plate for fixing the copper sleeve on the workbench;
[0010] A drilling machine spindle is located directly above the copper sleeve and can move up and down in the vertical direction, the upper end of the drilling machine spindle is connected to the transmission mechanism of the drilling machine and is driven by the transmission mechanism of the drilling machine to rotate at a high speed;
[0011] a grinding head mounted on the lower end of the drilling machine spindle; and
[0012] A spraying mechanism is used for spraying grinding fluid on the grinding position of the copper sleeve.
[0013] In a preferred embodiment of the utility model, a copper sleeve supporting base for supporting the copper sleeve is fixedly arranged on the work surface of the workbench, and a grinding head accommodating groove is provided on the upper end surface of the copper sleeve supporting base.
[0014] In a preferred embodiment of the utility model, an L-shaped spindle support seat is arranged on the workbench, one end of the vertical part of the L-shaped spindle support seat is connected to the workbench, and the horizontal part thereof is located directly above the copper sleeve, and the drilling machine spindle passes through the horizontal part of the L-shaped spindle support seat.
[0015] In a preferred embodiment of the present invention, the rotation speed of the main shaft of the drilling machine is 200-220 rpm, and the grinding feed or grinding withdrawal speed is 700-900 mm / min.
[0016] In a preferred embodiment of the utility model, the top dead center position of the drilling machine spindle is the position where the grinding head completely exits the copper sleeve upward, and the bottom dead center position is the position where the distance between the lower end surface of the grinding head and the lower end surface of the copper sleeve is 4 cm to 5 cm after the grinding head passes through the copper sleeve downward.
[0017] In a preferred embodiment of the utility model, the spray mechanism includes a spray pipe and a sprayer, the sprayer is added with grinding fluid and has a spray outlet, one end of the spray pipe is connected to the spray outlet of the sprayer, and the other end thereof extends to a position close to the copper sleeve being ground.
[0018] In a preferred embodiment of the present invention, the grinding fluid is kerosene, and its spray flow rate is 10 to 12 liters per minute.
[0019] Due to the adoption of the above technical solution, the beneficial effects of the utility model are:
[0020] 1. The surface roughness of the copper sleeve after grinding can reach Ra0.8μm;
[0021] 2. The machining error of the circumferential dimensions of the root and end of the copper sleeve of the utility model is reduced to 0.5-1 μm;
[0022] 3. The grinding amount of the utility model is only 0.1-0.15 mm, which is one fifth of the traditional turning, and can save the copper sleeve use cost of about 120,000 yuan a year;
[0023] 4. The grinding accuracy of the copper sleeve of the utility model is improved, the assembly accuracy of the copper sleeve and the graphite mold is improved, and the service life of the mold and the casting quality of the ingot are greatly improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0025] Figure 1 It is a structural schematic diagram of the utility model.
[0026] Figure 2 It is a partial structural sectional view of the utility model. DETAILED DESCRIPTION
[0027] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further described below with reference to specific illustrations.
[0028] Referring to the accompanying drawings, a repair device for a copper sleeve for casting is shown, which includes a workbench 100, a copper sleeve fixed pressure plate 200, a drilling machine spindle 300, a grinding head 400 and a spray mechanism (not shown in the drawings).
[0029] The workbench 100 has a work surface 110 , on which a copper sleeve supporting base 120 for supporting the copper sleeve 10 is fixedly arranged, and a grinding head accommodating groove 121 is provided on the upper end surface of the copper sleeve supporting base 120 .
[0030] The copper sleeve fixing platen 200 is used to fix the copper sleeve 10 on the copper sleeve supporting base 120 of the workbench 100. In this embodiment, the copper sleeve fixing platen 200 can be fixed by fasteners such as bolts. Of course, other fixing methods can also be used, as long as the copper sleeve fixing platen 200 can fix the copper sleeve 10 on the copper sleeve supporting base 120.
[0031] The drilling machine spindle 300 is located directly above the copper sleeve 10 and can move up and down in the vertical direction. The upper end of the drilling machine spindle 300 is connected to the transmission mechanism of the drilling machine and is driven by the transmission mechanism of the drilling machine to rotate at high speed. An L-shaped spindle support seat 130 is arranged on the workbench 100. One end of the vertical part of the L-shaped spindle support seat 130 is connected to the workbench 100, and its horizontal part is located directly above the copper sleeve 10. The drilling machine spindle 300 passes through the horizontal part of the L-shaped spindle support seat 130, which effectively limits the movement of the drilling machine spindle 300 and improves the grinding stability.
[0032] The grinding head 400 is mounted on the lower end of the drilling machine spindle 300 and is used for grinding the inner hole of the copper sleeve 10 .
[0033] The spray mechanism is used to spray the grinding fluid on the position where the copper sleeve 10 is ground, to ensure the discharge of the grinding coolant, and avoid affecting the grinding accuracy. The spray mechanism includes a spray pipe 500 and a sprayer, in which the grinding fluid is added and has a spray outlet, one end of the spray pipe 500 is connected to the spray outlet of the sprayer, and the other end thereof extends to the position close to the copper sleeve 10 being ground. Since copper metal is relatively sticky and difficult to remove chips, the grinding fluid used in the spray mechanism is kerosene, which ensures grinding cooling and chip removal, and avoids affecting the grinding accuracy.
[0034] The working principle of the repairing device of the copper sleeve for casting of the utility model is as follows:
[0035] Step S10, install a φ1mm positioning drill bit on the lower end of the drilling machine spindle 300, start the drilling machine, and control the drilling machine spindle 300 to move downward close to the copper sleeve supporting base 120 of the workbench 100, and determine the center point on the copper sleeve supporting base 120 of the workbench 100 according to the positioning drill bit on the drilling machine spindle 300 and mark the center point;
[0036] Step S20, placing the copper sleeve 10 on the copper sleeve supporting base 120 of the workbench 100, and adjusting the position of the copper sleeve 10 so that the central axis of the inner hole of the copper sleeve 10 coincides with the center point of the mark, and fixing the copper sleeve 10 on the copper sleeve supporting base 120 of the workbench 100 by using the copper sleeve fixing plate 200;
[0037] Step S30, remove the positioning drill bit from the drilling machine spindle 300, and install the grinding head 400 on the lower end of the drilling machine spindle 300; the rotation speed of the drilling machine spindle 300 and the speed of grinding feed or grinding withdrawal directly affect the grinding accuracy. In this embodiment, the rotation speed of the drilling machine spindle 300 is controlled at 200-220 rpm, and its grinding feed or grinding withdrawal speed is 700-900 mm / min; at the same time, the top dead center position of the drilling machine spindle 300 is the position where the grinding head 400 completely withdraws from the copper sleeve 10 upward, and the bottom dead center position is the position where the grinding head 40 passes through the copper sleeve 10 downward and enters the grinding head accommodating groove 121 of the copper sleeve supporting base 120, and the distance between its lower end surface and the lower end surface of the copper sleeve 10 is 4 cm to 5 cm;
[0038] Step S40, start the drilling machine and the spraying mechanism, the drilling machine drives the drilling machine spindle 300 to rotate through the transmission mechanism, and moves the drilling machine spindle 300 in the vertical direction according to the upper and lower dead point positions of the drilling machine spindle 300 for grinding. During the grinding process, the spraying mechanism sprays the grinding fluid to the grinding position of the copper sleeve, and the spraying flow rate is 10 to 12 liters / minute. Generally, the copper sleeve 10 can be ground after 15 to 20 minutes of grinding.
[0039] The above shows and describes the basic principle and main features of the utility model and the advantages of the utility model. Those skilled in the art should understand that the utility model is not limited by the above embodiments. The above embodiments and descriptions are only for explaining the principle of the utility model. Without departing from the spirit and scope of the utility model, the utility model may have various changes and improvements, which fall within the scope of the utility model to be protected. The scope of protection claimed by the utility model is defined by the attached claims and their equivalents.
Claims
1. A repair device for a copper sleeve for casting, characterized in that: include: Workbench; A copper sleeve fixing pressure plate for fixing the copper sleeve on the workbench; A drilling machine spindle is located directly above the copper sleeve and can move up and down in the vertical direction, the upper end of the drilling machine spindle is connected to the transmission mechanism of the drilling machine and is driven by the transmission mechanism of the drilling machine to rotate at a high speed; a grinding head mounted on the lower end of the drilling machine spindle; and A spraying mechanism is used for spraying grinding fluid on the grinding position of the copper sleeve.
2. The repairing device for the copper sleeve for casting according to claim 1, characterized in that: A copper sleeve supporting base for supporting the copper sleeve is fixedly arranged on the working table surface of the workbench, and a grinding head accommodating groove is provided on the upper end surface of the copper sleeve supporting base.
3. The repairing device for the copper sleeve for casting according to claim 1, characterized in that: An L-shaped spindle support seat is arranged on the workbench, one end of the vertical part of the L-shaped spindle support seat is connected to the workbench, and the horizontal part of the L-shaped spindle support seat is located directly above the copper sleeve, and the drilling machine spindle passes through the horizontal part of the L-shaped spindle support seat.
4. The repairing device for the copper sleeve for casting according to claim 1, characterized in that: The rotation speed of the main shaft of the drilling machine is 200-220 rpm, and the grinding feed or grinding withdrawal speed is 700-900 mm / min.
5. The repairing device for the copper sleeve for casting according to claim 1, characterized in that: The top dead center position of the drilling machine spindle is the position where the grinding head completely exits the copper sleeve upward, and the bottom dead center position is the position where the distance between the lower end surface of the grinding head and the lower end surface of the copper sleeve is 4cm to 5cm after the grinding head passes through the copper sleeve downward.
6. The repairing device for a copper sleeve for casting according to any one of claims 1 to 5, characterized in that: The spray mechanism includes a spray pipe and a sprayer, the sprayer is filled with grinding fluid and has a spray outlet, one end of the spray pipe is connected to the spray outlet of the sprayer, and the other end thereof extends to a position close to the grinding position of the copper sleeve.
7. The repairing device for the copper sleeve for casting according to claim 6, characterized in that: The grinding fluid is kerosene, and its spraying flow rate is 10 to 12 liters per minute.
Citation Information
Cited By
Maintenance device and method for casting copper bush
CN117798678A