Polymer composite reinforcing film
By introducing a middle buffer layer, a lower composite reinforcement layer and an upper composite reinforcement layer into the reinforcement film, nano-rubber and fiberglass materials are used, combined with a wear-resistant layer and a tear-resistant adhesive layer, the reinforcement film is solved by not resistant to corrosion and at high temperatures. The problem of lower viscosity achieves higher durability and safety.
Patent Information
- Application Number
- CN202323636693.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-29
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2033-12-29
AI Technical Summary
Existing reinforcement films are not corrosion-resistant and can easily reduce viscosity in high temperature weather, affecting their service life, and are not safe and durable.
A polymer composite reinforcement film was designed, including a middle buffer layer, a lower composite reinforcement layer and an upper composite reinforcement layer. It is made of nano-rubber material and glass fiber cloth material, equipped with a lower wear-resistant layer and an upper wear-resistant layer, and uses epoxy The resin composite material and the resin-type pressure-sensitive adhesive are provided with a tear-apart tear-a-surface layer.
It improves moisture-proof viscosity, climate resistance, chemical corrosion resistance and UV resistance, enhances heat resistance and electrical insulation, is safer and more reliable in use, and simplifies the pasting process.
Smart Images

Figure CN222099849U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of reinforcing films, in particular to a polymer composite reinforcing film. Background Art
[0002] In automobile design and production, manufacturers reduce the weight of the car by reducing the thickness of materials and hollowing out structural parts. However, the above solutions will also bring new problems: thinning steel plates will reduce the rigidity of the car body, especially the inner door panels, door handles, the inside of the hood, the roof, wheel covers, side panels and other parts are prone to noise and resonance during driving. When an accidental collision occurs, the impact energy absorption becomes smaller, which is easy to injure the occupants; hollowing out of structural parts reduces the strength, sound insulation and vibration prevention of steel plates, shortening the service life of automobile steel plates. To overcome the above defects, most merchants use reinforcing films to strengthen the door panels of cars.
[0003] In the specification of a composite fiber reinforcing film in the prior art (publication number CN206749186U), it is mentioned that "the reinforcing layer includes: a composite fiber material layer, which is a composite fiber made of polypropylene fiber, glass fiber, carbon fiber and asbestos fiber by conventional needle punching and blending; the upper surface of the composite fiber material layer is provided with a plurality of vertically arranged cylindrical first grooves, and the lower surface is provided with a plurality of vertically arranged cylindrical second grooves, and any first groove and the second groove do not overlap in the vertical direction", but the reinforcing film in the prior art is not corrosion-resistant, and its viscosity is easily reduced in high temperature weather, which affects its service life, and is even less safe and durable. Utility Model Content
[0004] In order to overcome the defects of the prior art, a polymer composite reinforcing film is now provided to solve the problem that the reinforcing film in the prior art is not corrosion-resistant, easily reduces viscosity in high temperature weather, affects its service life, and is not safe and durable.
[0005] To achieve the above-mentioned purpose, a polymer composite reinforcing film is provided, including a reinforcing film, a middle buffer layer is arranged at the center of the reinforcing film, and a lower composite reinforcing layer is arranged on the lower side of the middle buffer layer, an upper composite reinforcing layer is arranged on the upper side of the middle buffer layer, and an upper wear-resistant layer is arranged on the upper side of the upper composite reinforcing layer, and multiple groups of fiber filaments are passed through the lower composite reinforcing layer, the middle buffer layer and the upper composite reinforcing layer.
[0006] Furthermore, the middle buffer layer adopts a honeycomb structure of nano rubber material.
[0007] Furthermore, the thickness of the lower composite reinforcement layer and the upper composite reinforcement layer are set to be consistent, and the lower composite reinforcement layer and the upper composite reinforcement layer are both made of glass fiber cloth.
[0008] Furthermore, a lower wear-resistant layer is arranged on the lower side of the lower composite reinforcement layer, and the thickness of the lower wear-resistant layer and the upper wear-resistant layer are set to be the same, and the lower wear-resistant layer and the upper wear-resistant layer are both made of epoxy resin composite material.
[0009] Furthermore, an adhesive layer is provided on the lower side of the lower wear-resistant layer, and the adhesive layer adopts a resin-type pressure-sensitive adhesive.
[0010] Furthermore, a tearing layer is attached to the lower side of the adhesive layer, and the tearing layer is made of release paper and has a tearable structure.
[0011] The beneficial effects of the utility model are:
[0012] 1. The middle buffer layer arranged in the center of the reinforcing film of the utility model has high moisture-proof viscosity, which not only connects the lower composite reinforcement layer and the upper composite reinforcement layer tightly and firmly, but also enhances the moisture-proof, waterproof and shock-absorbing effects.
[0013] 2. The lower composite reinforcement layer and the upper composite reinforcement layer of the utility model have strong weather resistance, and are resistant to chemical corrosion, strong acid and strong alkali, and have good insulation and UV resistance, making them safer and more reliable to use.
[0014] 3. The lower wear-resistant layer and the upper wear-resistant layer of the utility model are arranged with the characteristics of longitudinal stretching and transverse compression, and also have good heat resistance and electrical insulation, and are safer and more durable.
[0015] 4. The tearing surface layer outside the adhesive layer on the lower side of the reinforcing film of the utility model is easy to tear off, and after the adhesive layer is exposed, it can be pasted on the area where it is needed. The method of use is simple and convenient, and it is more convenient and practical. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 This is a schematic diagram of the effect of an embodiment of the utility model;
[0017] Figure 2 It is a top view schematic diagram of an embodiment of the utility model;
[0018] Figure 3 It is a schematic diagram of the internal structure of an embodiment of the utility model;
[0019] Figure 4 This is a schematic diagram of fiber filaments according to an embodiment of the utility model.
[0020] In the figure: 1, reinforcing film; 10, tear surface layer; 11, adhesive layer; 12, lower wear-resistant layer; 13, lower composite reinforcement layer; 14, middle buffer layer; 15, upper composite reinforcement layer; 16, upper wear-resistant layer; 17, fiber filaments. DETAILED DESCRIPTION
[0021] In order to make the technical problems, technical solutions and beneficial effects to be solved by the utility model clearer, the utility model is further described in detail in combination with the accompanying drawings and embodiments. The specific embodiments described herein are only used to explain the utility model, and are not used to limit the utility model. Specific details such as specific system structures and technologies are proposed in order to more thoroughly understand the embodiments of the utility model. The described embodiments are part of the embodiments of the present disclosure, rather than all of the embodiments. However, it should be clear to those skilled in the art that the utility model can also be implemented in other embodiments without these specific details. Based on the embodiments in the present disclosure, all other embodiments obtained by those skilled in the art without making creative work are within the scope of protection of the present disclosure.
[0022] The specific implementation of the utility model is described in detail below with reference to the accompanying drawings.
[0023] Figure 1 The effect diagram of the embodiment of the utility model is shown in FIG. Figure 2 A schematic top view of an embodiment of the utility model, Figure 3 The internal structure of the embodiment of the utility model is shown and Figure 4 This is a schematic diagram of fiber filaments according to an embodiment of the utility model.
[0024] Reference Figures 1 to 4 As shown, the utility model provides a polymer composite reinforcing film, including a reinforcing film 1, a middle buffer layer 14 is arranged at the center of the reinforcing film 1, and a lower composite reinforcing layer 13 is arranged on the lower side of the middle buffer layer 14, an upper composite reinforcing layer 15 is arranged on the upper side of the middle buffer layer 14, and an upper wear-resistant layer 16 is arranged on the upper side of the upper composite reinforcing layer 15, and multiple groups of fiber filaments 17 penetrate between the lower composite reinforcing layer 13, the middle buffer layer 14 and the upper composite reinforcing layer 15.
[0025] In this embodiment, the middle buffer layer 14 adopts a honeycomb structure of nano rubber material.
[0026] As a preferred embodiment, the middle buffer layer 14 arranged in the center of the reinforcing film 1 of the utility model has high moisture-proof viscosity, which not only connects the lower composite reinforcement layer 13 and the upper composite reinforcement layer 15 tightly and firmly, but also enhances the moisture-proof, waterproof and shock-absorbing effects.
[0027] In this embodiment, the thickness of the lower composite reinforcement layer 13 and the upper composite reinforcement layer 15 are set to be consistent, and the lower composite reinforcement layer 13 and the upper composite reinforcement layer 15 are both made of glass fiber cloth.
[0028] As a preferred embodiment, the lower composite reinforcement layer 13 and the upper composite reinforcement layer 15 of the utility model have strong weather resistance, are resistant to chemical corrosion, strong acids and alkalis, have good insulation and UV resistance, and are safer and more reliable to use.
[0029] In this embodiment, a lower wear-resistant layer 12 is provided on the lower side of the lower composite reinforcement layer 13, and the thickness of the lower wear-resistant layer 12 and the upper wear-resistant layer 16 are set to be the same, and the lower wear-resistant layer 12 and the upper wear-resistant layer 16 are both made of epoxy resin composite materials.
[0030] As a preferred embodiment, the lower wear-resistant layer 12 and the upper wear-resistant layer 16 of the utility model are arranged with the characteristics of longitudinal stretching and transverse compression, and also have good heat resistance and electrical insulation, and are safer and more durable.
[0031] In this embodiment, an adhesive layer 11 is provided on the lower side of the lower wear-resistant layer 12, and the adhesive layer 11 adopts a resin-type pressure-sensitive adhesive; a tear layer 10 is attached to the lower side of the adhesive layer 11, and the tear layer 10 adopts release paper, and the tear layer 10 is a tearable structure.
[0032] As a preferred embodiment, the tearing surface layer 10 outside the adhesive layer 11 on the lower side of the reinforcing film 1 in the utility model is easy to tear off, and after the adhesive layer 11 is exposed, it can be pasted on the area where it is needed. The method of use is simple and convenient, and it is more convenient and practical.
[0033] The utility model can effectively solve the problems in the prior art that the reinforcing film is not corrosion-resistant, easily reduces viscosity in hot weather, affects its service life, and is not safe and durable. The utility model has good resistance to strong acids and alkalis and high temperatures, so that it can be tightly and firmly adhered and installed for a long time, is more durable, and is safe and reliable.
[0034] The above embodiments are used to explain the present invention rather than to limit the present invention. Any modifications and changes made to the present invention within the spirit of the present invention and the scope of the claims for protection shall be included in the protection scope of the present invention.
Claims
1. A polymer composite reinforcing film, characterized in that: The invention comprises a reinforcing film (1), wherein a middle buffer layer (14) is arranged at the center of the reinforcing film (1), and a lower composite reinforcing layer (13) is arranged on the lower side of the middle buffer layer (14), an upper composite reinforcing layer (15) is arranged on the upper side of the middle buffer layer (14), and an upper wear-resistant layer (16) is arranged on the upper side of the upper composite reinforcing layer (15), and a plurality of groups of fiber filaments (17) are interlaced between the lower composite reinforcing layer (13), the middle buffer layer (14) and the upper composite reinforcing layer (15).
2. A polymer composite reinforcing film according to claim 1, characterized in that: The middle buffer layer (14) adopts a honeycomb structure of nano rubber material.
3. A polymer composite reinforcing film according to claim 1, characterized in that: The thickness of the lower composite reinforcement layer (13) and the upper composite reinforcement layer (15) are set to be consistent, and the lower composite reinforcement layer (13) and the upper composite reinforcement layer (15) are both made of glass fiber cloth.
4. A polymer composite reinforcing film according to claim 1, characterized in that: A lower wear-resistant layer (12) is arranged on the lower side of the lower composite reinforcement layer (13), and the thickness of the lower wear-resistant layer (12) and the upper wear-resistant layer (16) are set to be the same, and the lower wear-resistant layer (12) and the upper wear-resistant layer (16) are both made of epoxy resin composite material.
5. A polymer composite reinforcing film according to claim 4, characterized in that: An adhesive layer (11) is provided on the lower side of the lower wear-resistant layer (12), and the adhesive layer (11) is made of a resin-type pressure-sensitive adhesive.
6. A polymer composite reinforcing film according to claim 5, characterized in that: A tearing layer (10) is attached to the lower side of the adhesive layer (11), and the tearing layer (10) is made of release paper, and the tearing layer (10) is a tearable structure.
Citation Information
Cited By
High-wear-resistance and high-elasticity EPDM (ethylene-propylene-diene monomer) sheet and preparation method thereof