Cement drying shrinkage test mold
By designing the structure of limit blocks, installation blocks, clamping grooves and elastic pressing blocks in the cement dry-shrink test mold, the problem of easy loosening and falling off of the test nails is solved, and the measurement accuracy and stability of the test mold are improved.
Patent Information
- Application Number
- CN202420085714.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-12
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2034-01-12
AI Technical Summary
The existing cement dry shrink test nails are prone to loosening and falling off, resulting in experimental errors in the measurement of the length of the dry shrink test piece.
A cement dry-shrink test mold structure including limit blocks, mounting blocks, clamping grooves and elastic pressing blocks is designed. Through the fitting of the clamping grooves and groove bodies and the movement of the fasteners, the stability of the test nails is ensured and Accuracy.
It effectively avoids loosening and falling off of the test nails, improves measurement accuracy, and facilitates the disassembly and assembly process of the test mold.
Smart Images

Figure CN222105185U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of construction equipment, in particular to a cement shrinkage test mold. Background Art
[0002] In the concrete application process, the testing of concrete raw materials is very important. The testing involves the testing of cement strength and shrinkage performance. When testing the shrinkage performance, a cement shrinkage test mold with copper measuring nails is required. That is, first put the mixed cement mortar into the test mold, then use the vibration table to vibrate the cement slurry in the test mold, then scrape off the excess cement slurry on the test mold to ensure the neat shape of the test block, and finally take the mold.
[0003] However, since the existing test pins are smooth cylinders, the insertion or vibration during the molding process can easily cause the test pins to loosen. The copper test pins cannot be effectively fixed in the end plate limit holes, and are prone to displacement and falling off. The displacement of the copper test pins results in different lengths corresponding to different angles when measuring the length of the shrinkage specimen, resulting in certain experimental errors. Utility Model Content
[0004] The utility model aims to provide a cement shrinkage test mold to solve the problem that copper measuring pins are easily displaced and fall off.
[0005] In order to solve the above technical problems, the utility model adopts the following technical solutions.
[0006] The utility model provides a cement shrinkage test mold, which comprises: a base, comprising a limit block and a mounting block arranged oppositely; a first end plate, arranged on the side of the limit block facing the mounting block, the first end plate comprising a first plate body and a second plate body, the first plate body abutting against the limit block, the first plate body being provided with a clamping groove and a first groove body located on the inner side of the clamping groove, the second plate body abutting against the side of the first plate body facing away from the limit block, the second plate body being provided with a second groove body connected to the clamping groove; a second end plate, arranged on the side of the mounting block facing the limit block; a partition plate, clamped between the first end plate and the second end plate; a fastener , movably connected to the mounting block, the fastener can move in a direction close to or away from the limit block; a test nail, comprising a column and a clamping portion protruding along the radial direction of the column, and the clamping portion divides the column into a first column and a second column located on both sides of the clamping portion, and the end of the clamping portion is elastically connected to a pressing block; wherein, the first column is arranged in the first slot body, at least part of the clamping portion is arranged in the clamping slot, and the pressing block is elastically supported on the side wall of the clamping slot, the second column is arranged in the second slot body, and the size of the second slot body is configured to be able to pass the test nail.
[0007] In some embodiments of the present application, two ends of the clamping portion are elastically connected to the two pressing blocks respectively.
[0008] In some embodiments of the present application, two receiving grooves are provided at both ends of the clamping portion; the two pressing blocks are respectively installed in the two receiving grooves, and at least part of the pressing blocks protrude out of the receiving grooves; a limiting structure is also provided between the clamping portion and the pressing block, and the limiting structure prevents the pressing block from escaping from the receiving groove.
[0009] In some embodiments of the present application, the limiting structure includes a hook provided on the side wall of the accommodating groove and a slot provided on the side wall of the pressing block.
[0010] In some embodiments of the present application, a clearance groove is provided on the side wall of the accommodating groove, and an elastic arm is provided in the clearance groove, and the hook is provided at the end of the elastic arm.
[0011] In some embodiments of the present application, the test pin also includes a spring; a first plug post is protruding from the bottom of the accommodating groove; a second plug post is provided at the bottom of the pressing block and is arranged opposite to the first plug post; the spring is arranged in the accommodating groove, and the two ends of the spring are respectively sleeved on the first plug post and the second plug post.
[0012] In some embodiments of the present application, the depth of the clamping groove is less than the thickness of the clamping portion, so that a portion of the clamping portion is disposed in the clamping groove and another portion is disposed in the second groove body.
[0013] In some embodiments of the present application, the clamping groove and the first groove body constitute an installation groove; the first plate body is provided with a plurality of the installation grooves arranged side by side and spaced apart; the second plate body is provided with a plurality of the second groove bodies arranged side by side and spaced apart, and the second groove bodies are connected to the clamping groove one by one; a plurality of the partitions are arranged side by side and spaced apart, and a filling groove is formed between each two adjacent partitions; and the second groove bodies are also connected to the filling grooves one by one.
[0014] In some embodiments of the present application, the fastener includes a rod and a first handle connected to each other; the rod is screwed to the mounting block; the first handle is arranged on the side of the mounting block facing away from the limit block; the base also includes a second handle connected to the side of the limit block facing away from the mounting block.
[0015] In some embodiments of the present application, a plurality of first partition grooves arranged side by side and spaced apart are provided on the side of the second plate body facing the second end plate; a plurality of second partition grooves arranged side by side and spaced apart are provided on the side of the second end plate facing the second plate body; and both ends of the partition are respectively inserted into the first partition groove and the second partition groove.
[0016] It can be seen from the above technical solutions that the embodiments of the utility model have at least the following advantages and positive effects:
[0017] In the cement shrinkage test mold of the embodiment of the utility model, when installing the test nail, the first column of the test nail is inserted into the first slot, and the first column and the first slot can be matched with a small gap, which is convenient for the first column to be placed and can also prevent the first column from shaking in the first slot, thereby preventing the test nail from loosening. At least part of the clamping part is arranged in the clamping groove, and the pressing block elastically abuts against the side wall of the clamping groove. The elastic pressing of the pressing block prevents the clamping part from shaking in the clamping groove, thereby further preventing the test nail from loosening and improving the test accuracy.
[0018] The size of the second trough is configured so that the test nail used to embed the cement during molding can be demoulded and removed together with the cement test piece. The fastener moves in the direction close to the limit block to press the second end plate, the partition plate and the first end plate against the limit block, making the entire test mold structure more stable. The fastener moves in the direction away from the limit block and disengages from the second end plate, making demoulding easier. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] The various objects, features and advantages of the present invention will become more apparent by considering the following detailed description of the preferred embodiments of the present invention in conjunction with the accompanying drawings. The accompanying drawings are only exemplary illustrations of the present invention and are not necessarily drawn to scale. In the accompanying drawings, the same reference numerals always represent the same or similar parts. Among them:
[0020] Figure 1 It is a structural schematic diagram of a cement shrinkage test mold according to an embodiment of the utility model.
[0021] Figure 2 yes Figure 1 Schematic diagram of the structure from another angle.
[0022] Figure 3 yes Figure 1 Schematic diagram of the exploded structure of the first end plate and the test pin.
[0023] Figure 4 yes Figure 3 Schematic diagram of the decomposition structure.
[0024] Figure 5 yes Figure 4 Schematic diagram of the structure of the test nail.
[0025] Figure 6 yes Figure 5 Schematic diagram of the decomposition structure.
[0026] Figure 7 yes Figure 6 sectional view of .
[0027] Figure 8 yes Figure 1 Schematic diagram of the structure of the second end plate.
[0028] The accompanying drawings are marked as follows: 1. base; 11. limit block; 12. mounting block; 2. first end plate; 21. first plate body; 211. mounting groove; 2111. clamping groove; 2112. first groove body; 22. second plate body; 221. second groove body; 222. first partition groove; 3. second end plate; 31. second partition groove; 4. partition; 5. fastener; 51. rod; 52. first handle; 6. test nail; 61. column; 611. first column; 612. second column; 62. clamping part; 621. pressing block; 6211. slot; 6212. second plug column; 622. accommodating groove; 623. hook; 624. clearance groove; 625. elastic arm; 626. first plug column; 63. spring; 7. limit column. DETAILED DESCRIPTION
[0029] Although the present invention can be easily embodied as embodiments of different forms, only some of the specific embodiments are shown in the drawings and described in detail in this specification. It should be understood that this description should be regarded as an exemplary description of the principles of the present invention and is not intended to limit the present invention to that described herein.
[0030] Thus, a feature indicated in this specification will be used to illustrate one of the features of an embodiment of the utility model, rather than implying that each embodiment of the utility model must have the described feature. In addition, it should be noted that this specification describes many features. Although some features can be combined together to illustrate possible system designs, these features can also be used in other combinations that are not explicitly described. Thus, unless otherwise stated, the described combinations are not intended to be limiting.
[0031] In the embodiments shown in the drawings, the indications of directions (such as up, down, left, right, front and back) used to explain the structure and movement of various elements of the utility model are not absolute but relative. These descriptions are appropriate when these elements are in the positions shown in the drawings. If the descriptions of the positions of these elements change, the indications of these directions also change accordingly.
[0032] See also Figures 1 to 8 A cement shrinkage test mold provided by an embodiment of the utility model includes a base 1, a first end plate 2, a second end plate 3, a partition 4, a fastener 5 and a test nail 6.
[0033] The base 1 includes a limiting block 11 and a mounting block 12 that are arranged opposite to each other. The first end plate 2 is arranged on the side of the limiting block 11 facing the mounting block 12, and the first end plate 2 includes a first plate body 21 and a second plate body 22. The first plate body 21 abuts against the limiting block 11, and the first plate body 21 is provided with a clamping groove 2111 and a first groove body 2112 located inside the clamping groove 2111, and the second plate body 22 abuts against the side of the first plate body 21 facing away from the limiting block 11, and the second plate body 22 is provided with a second groove body 221 connected to the clamping groove 2111. The second end plate 3 is arranged on the side of the mounting block 12 facing the limiting block 11. The partition plate 4 is clamped between the first end plate 2 and the second end plate 3. The fastener 5 is movably connected to the mounting block 12, and the fastener 5 can move in a direction close to or away from the limiting block 11.
[0034] The test nail 6 includes a column 61 and a clamping portion 62 protruding along the radial direction of the column 61, and the clamping portion 62 divides the column 61 into a first column 611 and a second column 612 located on both sides of the clamping portion 62, and the end of the clamping portion 62 is elastically connected to a pressing block 621.
[0035] Among them, the first column 611 is arranged in the first groove 2112, at least part of the clamping portion 62 is arranged in the clamping groove 2111, and the pressing block 621 elastically abuts against the side wall of the clamping groove 2111, the second column 612 is arranged in the second groove 221, and the size of the second groove 221 is configured to be able to pass the test nail 6.
[0036] Through the above structural design, when installing the test nail 6, the first column 611 of the test nail 6 is inserted into the first slot 2112, and the first column 611 and the first slot 2112 can be matched with a small gap, which is convenient for the first column 611 to be inserted and can also prevent the first column 611 from shaking in the first slot 2112, thereby preventing the test nail 6 from loosening. At least part of the clamping portion 62 of the clamping portion 62 is arranged in the clamping groove 2111, and the pressing block 621 elastically abuts against the side wall of the clamping groove 2111. Through the elastic compression of the pressing block 621, the clamping portion 62 is prevented from shaking in the clamping groove 2111, thereby further preventing the test nail 6 from loosening and improving the test accuracy.
[0037] The size of the second slot 221 is configured so that the test nail 6 used to embed the cement during molding can be demolded and removed together with the cement test piece. The fastener 5 moves toward the direction close to the limit block 11 to press the second end plate 3, the partition 4 and the first end plate 2 against the limit block 11, making the entire test mold structure more stable. The fastener 5 moves away from the limit block 11 and breaks contact with the second end plate 3, making demolding easier.
[0038] It is worth mentioning that since the pressing block 621 is elastically connected to the clamping part 62, when the test nail 6 passes through the second groove body 221, the pressing block 621 also elastically presses against the inner wall of the second groove body 221, rather than rigidly contacting the inner wall of the second groove body 221. Therefore, it is also more convenient for the test nail 6 to pass through the second groove body 221 along with the cement block for demolding.
[0039] The depth of the clamping groove 2111 is less than the thickness of the clamping portion 62, so that a part of the clamping portion 62 is disposed in the clamping groove 2111, and the other part is disposed in the second groove body 221. That is to say, when the test nail 6 is installed on the first plate body 21, the other part of the test nail 6 is located outside the clamping groove 2111, providing a position for holding the test nail 6, and facilitating the installation of the test nail 6. At the same time, during demoulding, since a part of the test nail 6 is disposed in the second groove body 221, it is more convenient for the test nail 6 to be demoulded and removed together with the cement block through the second groove body 221.
[0040] The two ends of the clamping portion 62 are elastically connected to two pressing blocks 621. The two pressing blocks 621 are elastically pressed against two opposite side walls of the clamping groove 2111, so that the clamping portion 62 can be more stably installed in the clamping groove 2111 to prevent the test nail 6 from loosening.
[0041] Two receiving grooves 622 are provided at both ends of the clamping portion 62. Two pressing blocks 621 are respectively installed in the two receiving grooves 622, and at least part of the pressing block 621 protrudes out of the receiving groove 622. A limiting structure is also provided between the clamping portion 62 and the pressing block 621, and the limiting structure prevents the pressing block 621 from escaping from the receiving groove 622.
[0042] The portion of the pressing block 621 protruding out of the receiving groove 622 is used to elastically abut against the side wall of the clamping groove 2111. The limiting structure prevents the pressing block 621 from escaping from the receiving groove 622 to ensure the connection stability between the clamping portion 62 and the pressing block 621.
[0043] The limiting structure includes a hook 623 disposed on the side wall of the receiving groove 622 and a slot 6211 disposed on the side wall of the pressing block 621. The hook 623 is engaged with the slot 6211 to prevent the pressing block 621 from escaping from the receiving groove 622.
[0044] A clearance groove 624 is provided on the side wall of the receiving groove 622, and an elastic arm 625 is provided in the clearance groove 624, and a hook 623 is provided at the end of the elastic arm 625. The elastic arm 625 is opened outward to facilitate the installation of the pressing block 621 into the receiving groove 622, and then the elastic arm 625 rebounds inward under its own elastic force and is engaged with the clamping groove 6211, which facilitates the installation of the pressing block 621.
[0045] The test pin 6 also includes a spring 63. A first plug 626 is protruding from the bottom of the receiving groove 622. A second plug 6212 is provided at the bottom of the pressing block 621 and is arranged opposite to the first plug 626. The spring 63 is arranged in the receiving groove 622, and the two ends of the spring 63 are respectively sleeved on the first plug 626 and the second plug 6212.
[0046] The spring 63 provides elastic force to make the pressing block 621 elastically abut against the side wall of the clamping groove 2111. The first plug post 626 and the second plug post 6212 can prevent the spring 63 from shifting.
[0047] The clamping groove 2111 and the first groove body 2112 form a mounting groove 211. The first plate body 21 is provided with a plurality of mounting grooves 211 arranged side by side and at intervals. The second plate body 22 is provided with a plurality of second groove bodies 221 arranged side by side and at intervals, and the second groove bodies 221 are connected to the clamping groove 2111 one by one. A plurality of partitions 4 are arranged side by side and at intervals, and a filling groove is formed between each two adjacent partitions 4. The second groove bodies 221 are also connected to the filling grooves one by one.
[0048] The filling slot is used to fill cement slurry. Each set of mounting slots 211 and second slot body 221 can be installed on a test nail 6, and each test nail 6 corresponds to a filling slot. The cement shrinkage test mold can form multiple cement blocks at one time.
[0049] The fastener 5 includes a rod 51 and a first handle 52 connected to each other. The rod 51 is screwed to the mounting block 12. The first handle 52 is arranged on the side of the mounting block 12 facing away from the limit block 11. The base 1 also includes a second handle connected to the side of the limit block 11 facing away from the mounting block 12.
[0050] By rotating the rod 51 through the first handle 52, the fastener 5 can be moved toward or away from the limit block 11. The first handle 52 and the second handle are convenient for holding and fixing the cement shrinkage test mold, preventing the cement shrinkage test mold from shaking during vibration molding, which is conducive to molding, more convenient operation, and improved operating efficiency.
[0051] A plurality of first partition grooves 222 arranged side by side and spaced are also provided on the side of the second plate body 22 facing the second end plate 3. A plurality of second partition grooves 31 arranged side by side and spaced are also provided on the side of the second end plate 3 facing the second plate body 22. Both ends of the partition 4 are respectively inserted into the first partition groove 222 and the second partition groove 31. The first partition groove 222 and the second partition groove 31 prevent the partition 4 from shifting.
[0052] The base 1 further includes a limiting column 7, which is disposed between the limiting block 11 and the mounting block 12 and close to the side of the base 1. One side of the partition 4 can abut against the limiting column 7 to fix the positions of the assembled first end plate 2, the second end plate 3 and the plurality of partitions 4.
[0053] Although the utility model has been described with reference to several typical embodiments, it should be understood that the terms used are illustrative and exemplary, rather than restrictive. Since the utility model can be implemented in a variety of forms without departing from the spirit or essence of the utility model, it should be understood that the above-mentioned embodiments are not limited to any of the aforementioned details, but should be widely interpreted within the spirit and scope defined by the attached claims, so all changes and modifications falling within the scope of the claims or their equivalents should be covered by the attached claims.
Claims
1. A cement shrinkage test mold, characterized in that: include: A base, comprising a limiting block and a mounting block which are arranged opposite to each other; A first end plate is arranged on the side of the limit block facing the mounting block, the first end plate comprises a first plate body and a second plate body, the first plate body abuts against the limit block, a clamping groove and a first groove body located inside the clamping groove are provided on the first plate body, the second plate body abuts against the side of the first plate body facing away from the limit block, and a second groove body communicating with the clamping groove is provided on the second plate body; A second end plate, arranged on a side of the mounting block facing the limit block; a partition plate, sandwiched between the first end plate and the second end plate; A fastener, movably connected to the mounting block, wherein the fastener can move toward or away from the limiting block; The test nail comprises a column and a clamping portion protruding in the radial direction of the column, wherein the clamping portion divides the column into a first column and a second column located on both sides of the clamping portion, and the end of the clamping portion is elastically connected to a pressing block; The first column is disposed in the first slot, at least part of the clamping portion is disposed in the clamping slot, and the pressing block elastically abuts against the side wall of the clamping slot, the second column is disposed in the second slot, and the size of the second slot is configured to be able to pass the test pin.
2. The cement shrinkage test mold according to claim 1, characterized in that: The two ends of the clamping part are elastically connected to the two pressing blocks respectively.
3. The cement shrinkage test mold according to claim 2, characterized in that: Two accommodating grooves are provided at both ends of the clamping portion; The two pressing blocks are respectively installed in the two receiving grooves, and at least a portion of the pressing blocks protrudes out of the receiving grooves; A limiting structure is further provided between the clamping portion and the pressing block, and the limiting structure prevents the pressing block from escaping from the accommodating groove.
4. The cement shrinkage test mold according to claim 3, characterized in that: The limiting structure includes a hook arranged on the side wall of the accommodating groove and a slot arranged on the side wall of the pressing block.
5. The cement shrinkage test mold according to claim 4, characterized in that: A clearance groove is arranged on the side wall of the accommodation groove, and an elastic arm is arranged in the clearance groove, and the hook is arranged at the end of the elastic arm.
6. The cement shrinkage test mold according to claim 3, characterized in that: The test nail also includes a spring; A first plug post is protruding from the bottom of the accommodating groove; A second plug post is disposed at the bottom of the pressing block and is arranged opposite to the first plug post; The spring is arranged in the accommodating groove, and two ends of the spring are respectively sleeved on the first plug post and the second plug post.
7. The cement shrinkage test mold according to claim 1, characterized in that: The depth of the clamping groove is smaller than the thickness of the clamping portion, so that a portion of the clamping portion is disposed in the clamping groove and another portion is disposed in the second groove body.
8. The cement shrinkage test mold according to claim 1, characterized in that: The clamping groove and the first groove body form a mounting groove; The first plate body is provided with a plurality of the mounting grooves arranged side by side and at intervals; The second plate body is provided with a plurality of second slot bodies arranged side by side and spaced apart from each other, and the second slot bodies are connected to the clamping slots one by one correspondingly; A plurality of partitions are arranged side by side and spaced apart, and a filling groove is formed between each two adjacent partitions; The second tank bodies are also connected to the filling tanks in a one-to-one correspondence.
9. The cement shrinkage test mold according to claim 1, characterized in that: The fastener includes a rod portion and a first handle connected to each other; The rod portion is screwed to the mounting block; The first handle is arranged on a side of the mounting block facing away from the limiting block; The base also includes a second handle connected to a side of the limiting block facing away from the mounting block.
10. The cement shrinkage test mold according to claim 1, characterized in that: The second plate body is also provided with a plurality of first partition grooves arranged side by side and at intervals on the side facing the second end plate; The second end plate is also provided with a plurality of second partition grooves arranged side by side and at intervals on the side facing the second plate body; Two ends of the partition are respectively inserted into the first partition groove and the second partition groove.